High-temperature-resistant nylon material and preparation method thereof
By coating the modified magnesium aluminate fiber membrane with phenolic resin to form a porous carbon film, the problems of low heat resistance and elastic modulus of nylon 66 material are solved, and its high temperature resistance and mechanical properties are improved.
Patent Information
- Application Number
- CN202411074475.5
- Authority / Receiving Office
- CN · China
- Patent Type
- Applications(China)
- Current Assignee / Owner
- Filing Date
- 2024-08-07
- Publication Date
- 2024-11-08
AI Technical Summary
Nylon 66 material has poor heat resistance and low elastic modulus, and it is difficult for existing modification methods to improve its heat resistance and flexibility at the same time.
The modified magnesium aluminate fiber membrane is coated with phenolic resin to form a porous carbon film, which is prepared by electrospinning technology and combined with the same-direction twin screw extrusion process to enhance the mechanical properties and high temperature resistance of nylon 66.
It significantly improves the high temperature resistance and mechanical properties of nylon 66, enhances its thermal stress buffering ability under rapid temperature changes, and avoids the uneven distribution and agglomeration problems of conventional particulate materials.
Abstract
Description
Technical Field
[0001] The invention relates to the technical field of functional materials, and in particular to a high temperature resistant nylon material and a preparation method thereof. Background Art
[0002] Nylon 66 has good comprehensive properties. Compared with other engineering plastics, nylon 66 has the advantages of good mechanical properties, wear resistance, and oil resistance. In recent years, with the rapid development of domestic and foreign automobile, electronic and electrical, communication and other industries, the application proportion of nylon 66 has continued to increase. Among them, the application proportion in the vehicle transportation industry has reached 63%, and the application proportion in the electronic and electrical and office supplies industry has reached 22%. The wide application of nylon 66 materials has put forward higher requirements on its performance, and the modification research on its defects such as poor heat resistance and low elastic modulus has been continuously developed. The modification of nylon 66 can be divided into: one is chemical modification, that is, the molecular structure of nylon 66 is changed by copolymerization, grafting, cross-linking and other methods; the other is physical modification, that is, the modified nylon 66 is prepared by filling and reinforcing with inorganic fillers, blending with other resins, and adding various additives to improve and improve its comprehensive performance. In recent years, the main modification methods of nylon 66 can be divided into copolymerization modification, blending modification and filling modification. However, the modification methods currently used, such as modifying nylon 66 with nanomaterials to prepare nanocomposites, can improve its heat resistance and mechanical properties, but nanomaterials are easy to agglomerate and it is difficult to increase the flexibility of the material. Therefore, further research on it to improve its heat resistance and improve its elastic modulus is of utmost importance. Summary of the invention
[0003] Technical problem to be solved: The purpose of the present invention is to provide a high-temperature resistant nylon material and a preparation method thereof. The modified magnesium aluminate fiber membrane is used as a membrane structure to enhance the heat resistance of nylon 66, so that it can better disperse and withstand thermal stress when subjected to high temperature, and at the same time, its mechanical properties can be enhanced; the magnesium aluminate fiber membrane is coated with phenolic resin, and a carbon film is formed after sintering, and as the sintering temperature increases, the carbon film forms a porous structure, and the pore size changes with temperature. The porous carbon membrane can reduce heat transfer due to the presence of air in the pores, thereby improving the high temperature resistance of the material. At the same time, the porous structure can also reduce the thermal stress of nylon 66 under rapid temperature changes, because the pores can serve as a buffer for thermal expansion and reduce stress concentration inside the material.
[0004] Technical solution: A high temperature resistant nylon material, comprising the following components, measured by weight: 100 parts of nylon 66, 10 to 30 parts of modified magnesium aluminate fiber membrane, 0.5 to 1 part of ethylene bisstearamide, and 0.3 to 0.8 parts of antioxidant. The preparation method of the above-mentioned high temperature resistant nylon material is as follows: S1: Take nylon 66 and dry it; S2: adding ethylene bisstearamide and antioxidant, mixing evenly to obtain a premix; S3: Use a co-rotating twin-screw extruder and a side feeding process to add the modified magnesium aluminate fiber membrane from the side feeding port alone, and add the premix from the main feeding port for extrusion granulation. Furthermore, in S3, the extrusion temperature is 245-280° C., the screw speed is 300-450 rpm, and vacuum is applied. Furthermore, the preparation method of the modified magnesium aluminate fiber membrane is: S31: Mix 70-80 parts of dichloromethane and 2-3 parts of anhydrous ethanol uniformly; S32: slowly add 0.5-1 parts of anhydrous magnesium chloride and 2-4 parts of anhydrous aluminum chloride, and stir for 30-40 minutes; S33: heating to 100° C. to form a precursor; S34: 5 to 6 parts of polyvinyl pyrrolidone, 1 to 2 parts of phenolic resin and 80 to 100 parts of ethanol are mixed, stirred evenly, added to the precursor, and then 20 to 30 parts of anhydrous ethanol and 10 to 15 parts of N, N-dimethylformamide are added, and magnetic stirring is performed for 2 hours to obtain an electrospinning solution; S35: performing electrospinning by an electrospinning device to obtain a precursor fiber membrane coated with a phenolic resin; S36: drying, taking out and calcining, heating up to 900-1000°C at a rate of 4°C / min and calcining for 1h; S37: Take out, crush and sieve to obtain modified magnesium aluminate fiber membrane. Furthermore, the electrospinning conditions in S35 are as follows: the inner diameter of the nozzle is 0.8-1.2 mm, the flow rate of the electrospinning liquid is 1-1.5 mL / h, the spinning voltage is 15 kV, the spinning temperature is 20-22° C., and the receiving distance is 12 cm. Furthermore, the mesh size of the sieving in S37 is 100 meshes. Furthermore, the antioxidant is antioxidant 1010, antioxidant 1098, antioxidant H161, antioxidant H10, antioxidant 168, and antioxidant 626. Beneficial effects: 1. The present invention adopts a modified magnesium aluminate fiber membrane as a membrane structure, which can enhance the heat resistance of nylon 66, better disperse and withstand thermal stress when subjected to high temperature, and can also enhance its mechanical properties. 2. The present invention uses phenolic resin to coat the magnesium aluminate fiber membrane, and forms a carbon film after sintering. As the sintering temperature increases, the carbon film forms a porous structure, and the pore size changes with temperature. The porous carbon film can reduce heat transfer due to the presence of air in the pores, thereby improving the high temperature resistance of the material. At the same time, the porous structure can also reduce the thermal stress of nylon 66 under rapid temperature changes, because the pores can serve as a buffer for thermal expansion and reduce stress concentration inside the material. 3. The magnesium aluminate fiber membrane of the present invention can also improve the flexibility of nylon 66 and provide additional mechanical support, while avoiding the problems of uneven distribution and easy agglomeration of conventional granular materials. The porous structure of the surface carbon film can improve the tensile strength and bending strength of nylon 66. DETAILED DESCRIPTION Example 1 A preparation method of a high temperature resistant nylon material, the preparation method is as follows: S1: Mix 75 parts of dichloromethane and 3 parts of anhydrous ethanol; S2: Slowly add 0.8 parts of anhydrous magnesium chloride and 3 parts of anhydrous aluminum chloride, and stir for 35 minutes; S3: heating to 100°C to form a precursor; S4: 6 parts of polyvinyl pyrrolidone, 1 part of phenolic resin and 100 parts of ethanol were mixed, stirred evenly, added to the precursor, and then 30 parts of anhydrous ethanol and 15 parts of N, N-dimethylformamide were added, and magnetic stirring was performed for 2 hours to obtain an electrospinning solution; S5: electrospinning is performed by an electrospinning device, and the electrospinning conditions are: the inner diameter of the nozzle is 1.0 mm, the flow rate of the electrospinning liquid is 1.3 mL / h, the spinning voltage is 15 kV, the spinning temperature is 21 ° C, and the receiving distance is 12 cm, to obtain a precursor fiber membrane coated with phenolic resin; S6: After drying, take out and calcine, the heating rate is 4°C / min, and the temperature is raised to 950°C and calcined for 1h; S7: taking out, crushing and passing through a 100-mesh sieve to obtain a modified magnesium aluminate fiber membrane; S8: Take 100 parts of nylon 66 and dry; S9: Add 1 part of ethylene bisstearamide and 0.6 parts of antioxidant 1010, mix well, and obtain a premix; S10: Using a co-rotating twin-screw extruder and a side feeding process, 25 parts of modified magnesium aluminate fiber membrane were added from the side feeding port alone, and the premix was added from the main feeding port. The extrusion was performed into granules at an extrusion temperature of 270°C, a screw speed of 400 rpm, and vacuum was applied. Example 2 A preparation method of a high temperature resistant nylon material, the preparation method is as follows: S1: Mix 75 parts of dichloromethane and 3 parts of anhydrous ethanol; S2: Slowly add 0.8 parts of anhydrous magnesium chloride and 3 parts of anhydrous aluminum chloride, and stir for 35 minutes; S3: heating to 100°C to form a precursor; S4: 6 parts of polyvinyl pyrrolidone, 1.5 parts of phenolic resin and 100 parts of ethanol were mixed, stirred evenly, added to the precursor, and then 30 parts of anhydrous ethanol and 15 parts of N,N-dimethylformamide were added, and magnetic stirring was performed for 2 hours to obtain an electrospinning solution; S5: electrospinning is performed by an electrospinning device, and the electrospinning conditions are: the inner diameter of the nozzle is 1.0 mm, the flow rate of the electrospinning liquid is 1.3 mL / h, the spinning voltage is 15 kV, the spinning temperature is 21 ° C, and the receiving distance is 12 cm, to obtain a precursor fiber membrane coated with phenolic resin; S6: After drying, take out and calcine, the heating rate is 4°C / min, and the temperature is raised to 950°C and calcined for 1h; S7: taking out, crushing and passing through a 100-mesh sieve to obtain a modified magnesium aluminate fiber membrane; S8: Take 100 parts of nylon 66 and dry; S9: Add 1 part of ethylene bisstearamide and 0.6 parts of antioxidant 1010, mix well, and obtain a premix; S10: Using a co-rotating twin-screw extruder and a side feeding process, 25 parts of modified magnesium aluminate fiber membrane were added from the side feeding port alone, and the premix was added from the main feeding port. The extrusion was performed into granules at an extrusion temperature of 270°C, a screw speed of 400 rpm, and vacuum was applied. Example 3 A method for preparing a high temperature resistant nylon material, the preparation method is as follows: S1: Mix 75 parts of dichloromethane and 3 parts of anhydrous ethanol; S2: Slowly add 0.8 parts of anhydrous magnesium chloride and 3 parts of anhydrous aluminum chloride, and stir for 35 minutes; S3: heating to 100°C to form a precursor; S4: 6 parts of polyvinyl pyrrolidone, 2 parts of phenolic resin and 100 parts of ethanol were mixed, stirred evenly, added to the precursor, and then 30 parts of anhydrous ethanol and 15 parts of N, N-dimethylformamide were added, and magnetic stirring was performed for 2 hours to obtain an electrospinning solution; S5: electrospinning is performed by an electrospinning device, and the electrospinning conditions are: the inner diameter of the nozzle is 1.0 mm, the flow rate of the electrospinning liquid is 1.3 mL / h, the spinning voltage is 15 kV, the spinning temperature is 21 ° C, and the receiving distance is 12 cm, to obtain a precursor fiber membrane coated with phenolic resin; S6: After drying, take out and calcine, the heating rate is 4°C / min, and the temperature is raised to 950°C and calcined for 1h; S7: taking out, crushing and passing through a 100-mesh sieve to obtain a modified magnesium aluminate fiber membrane; S8: Take 100 parts of nylon 66 and dry; S9: Add 1 part of ethylene bisstearamide and 0.6 parts of antioxidant 1010, mix well, and obtain a premix; S10: Using a co-rotating twin-screw extruder and a side feeding process, 25 parts of modified magnesium aluminate fiber membrane were added from the side feeding port alone, and the premix was added from the main feeding port. The extrusion was performed into granules at an extrusion temperature of 270°C, a screw speed of 400 rpm, and vacuum was applied. Example 4 A preparation method of a high temperature resistant nylon material, the preparation method is as follows: S1: Mix 75 parts of dichloromethane and 3 parts of anhydrous ethanol; S2: Slowly add 0.8 parts of anhydrous magnesium chloride and 3 parts of anhydrous aluminum chloride, and stir for 35 minutes; S3: heating to 100°C to form a precursor; S4: 6 parts of polyvinyl pyrrolidone, 1.5 parts of phenolic resin and 100 parts of ethanol were mixed, stirred evenly, added to the precursor, and then 30 parts of anhydrous ethanol and 15 parts of N,N-dimethylformamide were added, and magnetic stirring was performed for 2 hours to obtain an electrospinning solution; S5: electrospinning is performed by an electrospinning device, and the electrospinning conditions are: the inner diameter of the nozzle is 1.0 mm, the flow rate of the electrospinning liquid is 1.3 mL / h, the spinning voltage is 15 kV, the spinning temperature is 21 ° C, and the receiving distance is 12 cm, to obtain a precursor fiber membrane coated with phenolic resin; S6: After drying, take out and calcine, the heating rate is 4°C / min, and the temperature is raised to 950°C and calcined for 1h; S7: taking out, crushing and passing through a 100-mesh sieve to obtain a modified magnesium aluminate fiber membrane; S8: Take 100 parts of nylon 66 and dry; S9: Add 1 part of ethylene bisstearamide and 0.6 parts of antioxidant 1010, mix well, and obtain a premix; S10: Using a co-rotating twin-screw extruder and a side feeding process, 10 parts of modified magnesium aluminate fiber membrane were added separately from the side feeding port, and the premix was added from the main feeding port. The extrusion was performed into pellets at an extrusion temperature of 270°C, a screw speed of 400 rpm, and vacuum was applied. Example 5 A preparation method of a high temperature resistant nylon material, the preparation method is as follows: S1: Mix 75 parts of dichloromethane and 3 parts of anhydrous ethanol; S2: Slowly add 0.8 parts of anhydrous magnesium chloride and 3 parts of anhydrous aluminum chloride, and stir for 35 minutes; S3: heating to 100°C to form a precursor; S4: 6 parts of polyvinyl pyrrolidone, 1.5 parts of phenolic resin and 100 parts of ethanol were mixed, stirred evenly, added to the precursor, and then 30 parts of anhydrous ethanol and 15 parts of N,N-dimethylformamide were added, and magnetic stirring was performed for 2 hours to obtain an electrospinning solution; S5: electrospinning is performed by an electrospinning device, and the electrospinning conditions are: the inner diameter of the nozzle is 1.0 mm, the flow rate of the electrospinning liquid is 1.3 mL / h, the spinning voltage is 15 kV, the spinning temperature is 21 ° C, and the receiving distance is 12 cm, to obtain a precursor fiber membrane coated with phenolic resin; S6: After drying, take out and calcine, the heating rate is 4°C / min, and the temperature is raised to 950°C and calcined for 1h; S7: taking out, crushing and passing through a 100-mesh sieve to obtain a modified magnesium aluminate fiber membrane; S8: Take 100 parts of nylon 66 and dry; S9: Add 1 part of ethylene bisstearamide and 0.6 parts of antioxidant 1010, mix well, and obtain a premix; S10: Using a co-rotating twin-screw extruder and a side feeding process, 15 parts of modified magnesium aluminate fiber membrane were added from the side feeding port alone, and the premix was added from the main feeding port. The extrusion was performed into pellets at an extrusion temperature of 270°C, a screw speed of 400 rpm, and vacuum was applied. Example 6 A preparation method of a high temperature resistant nylon material, the preparation method is as follows: S1: Mix 75 parts of dichloromethane and 3 parts of anhydrous ethanol; S2: Slowly add 0.8 parts of anhydrous magnesium chloride and 3 parts of anhydrous aluminum chloride, and stir for 35 minutes; S3: heating to 100°C to form a precursor; S4: 6 parts of polyvinyl pyrrolidone, 1.5 parts of phenolic resin and 100 parts of ethanol were mixed, stirred evenly, added to the precursor, and then 30 parts of anhydrous ethanol and 15 parts of N,N-dimethylformamide were added, and magnetic stirring was performed for 2 hours to obtain an electrospinning solution; S5: electrospinning is performed by an electrospinning device, and the electrospinning conditions are: the inner diameter of the nozzle is 1.0 mm, the flow rate of the electrospinning liquid is 1.3 mL / h, the spinning voltage is 15 kV, the spinning temperature is 21 ° C, and the receiving distance is 12 cm, to obtain a precursor fiber membrane coated with phenolic resin; S6: After drying, take out and calcine, the heating rate is 4°C / min, and the temperature is raised to 950°C and calcined for 1h; S7: taking out, crushing and passing through a 100-mesh sieve to obtain a modified magnesium aluminate fiber membrane; S8: Take 100 parts of nylon 66 and dry; S9: Add 1 part of ethylene bisstearamide and 0.6 parts of antioxidant 1010, mix well, and obtain a premix; S10: Using a co-rotating twin-screw extruder and a side feeding process, 20 parts of modified magnesium aluminate fiber membrane were added from the side feeding port alone, and the premix was added from the main feeding port. The extrusion was performed into pellets at an extrusion temperature of 270°C, a screw speed of 400 rpm, and vacuum was applied. Example 7 A method for preparing a high temperature resistant nylon material, the preparation method is as follows: S1: Mix 75 parts of dichloromethane and 3 parts of anhydrous ethanol; S2: Slowly add 0.8 parts of anhydrous magnesium chloride and 3 parts of anhydrous aluminum chloride, and stir for 35 minutes; S3: heating to 100°C to form a precursor; S4: 6 parts of polyvinyl pyrrolidone, 1.5 parts of phenolic resin and 100 parts of ethanol were mixed, stirred evenly, added to the precursor, and then 30 parts of anhydrous ethanol and 15 parts of N,N-dimethylformamide were added, and magnetic stirring was performed for 2 hours to obtain an electrospinning solution; S5: electrospinning is performed by an electrospinning device, and the electrospinning conditions are: the inner diameter of the nozzle is 1.0 mm, the flow rate of the electrospinning liquid is 1.3 mL / h, the spinning voltage is 15 kV, the spinning temperature is 21 ° C, and the receiving distance is 12 cm, to obtain a precursor fiber membrane coated with phenolic resin; S6: After drying, take out and calcine, the heating rate is 4°C / min, and the temperature is raised to 950°C and calcined for 1h; S7: taking out, crushing and passing through a 100-mesh sieve to obtain a modified magnesium aluminate fiber membrane; S8: Take 100 parts of nylon 66 and dry; S9: Add 1 part of ethylene bisstearamide and 0.6 parts of antioxidant 1010, mix well, and obtain a premix; S10: Using a co-rotating twin-screw extruder and a side feeding process, 30 parts of modified magnesium aluminate fiber membrane were added from the side feeding port alone, and the premix was added from the main feeding port. The extrusion was performed into pellets at an extrusion temperature of 270°C, a screw speed of 400 rpm, and vacuum was applied. Example 8 A method for preparing a high temperature resistant nylon material, the preparation method is as follows: S1: Mix 75 parts of dichloromethane and 3 parts of anhydrous ethanol; S2: Slowly add 0.8 parts of anhydrous magnesium chloride and 3 parts of anhydrous aluminum chloride, and stir for 35 minutes; S3: heating to 100°C to form a precursor; S4: 6 parts of polyvinyl pyrrolidone, 1.5 parts of phenolic resin and 100 parts of ethanol were mixed, stirred evenly, added to the precursor, and then 30 parts of anhydrous ethanol and 15 parts of N,N-dimethylformamide were added, and magnetic stirring was performed for 2 hours to obtain an electrospinning solution; S5: electrospinning is performed by an electrospinning device, and the electrospinning conditions are: the inner diameter of the nozzle is 1.0 mm, the flow rate of the electrospinning liquid is 1.3 mL / h, the spinning voltage is 15 kV, the spinning temperature is 21 ° C, and the receiving distance is 12 cm, to obtain a precursor fiber membrane coated with phenolic resin; S6: drying, taking out and calcining, heating rate is 4℃ / min, heating to 900℃ and calcining for 1h; S7: taking out, crushing and passing through a 100-mesh sieve to obtain a modified magnesium aluminate fiber membrane; S8: Take 100 parts of nylon 66 and dry; S9: Add 1 part of ethylene bisstearamide and 0.6 parts of antioxidant 1010, mix well, and obtain a premix; S10: Using a co-rotating twin-screw extruder and a side feeding process, 25 parts of modified magnesium aluminate fiber membrane were added from the side feeding port alone, and the premix was added from the main feeding port. The extrusion was performed into granules at an extrusion temperature of 270°C, a screw speed of 400 rpm, and vacuum was applied. Example 9 A preparation method of a high temperature resistant nylon material, the preparation method is as follows: S1: Mix 75 parts of dichloromethane and 3 parts of anhydrous ethanol; S2: Slowly add 0.8 parts of anhydrous magnesium chloride and 3 parts of anhydrous aluminum chloride, and stir for 35 minutes; S3: heating to 100°C to form a precursor; S4: 6 parts of polyvinyl pyrrolidone, 1.5 parts of phenolic resin and 100 parts of ethanol were mixed, stirred evenly, added to the precursor, and then 30 parts of anhydrous ethanol and 15 parts of N,N-dimethylformamide were added, and magnetic stirring was performed for 2 hours to obtain an electrospinning solution; S5: electrospinning is performed by an electrospinning device, and the electrospinning conditions are: the inner diameter of the nozzle is 1.0 mm, the flow rate of the electrospinning liquid is 1.3 mL / h, the spinning voltage is 15 kV, the spinning temperature is 21 ° C, and the receiving distance is 12 cm, to obtain a precursor fiber membrane coated with phenolic resin; S6: drying, taking out and calcining, heating rate is 4℃ / min, heating to 1000℃ and calcining for 1h; S7: taking out, crushing and passing through a 100-mesh sieve to obtain a modified magnesium aluminate fiber membrane; S8: Take 100 parts of nylon 66 and dry; S9: Add 1 part of ethylene bisstearamide and 0.6 parts of antioxidant 1010, mix well, and obtain a premix; S10: Using a co-rotating twin-screw extruder and a side feeding process, 25 parts of modified magnesium aluminate fiber membrane were added from the side feeding port alone, and the premix was added from the main feeding port. The extrusion was performed into granules at a temperature of 270°C, a screw speed of 400 rpm, and vacuum was applied. Comparative Example 1 The difference between this embodiment and embodiment 2 is that the magnesium aluminate fiber membrane is not modified. Specifically: A preparation method of a high temperature resistant nylon material, the preparation method is as follows: S1: Mix 75 parts of dichloromethane and 3 parts of anhydrous ethanol; S2: Slowly add 0.8 parts of anhydrous magnesium chloride and 3 parts of anhydrous aluminum chloride, and stir for 35 minutes; S3: heating to 100°C to form a precursor; S4: 6 parts of polyvinyl pyrrolidone and 100 parts of ethanol were mixed, stirred evenly, added to the precursor, and then 30 parts of anhydrous ethanol and 15 parts of N, N-dimethylformamide were added, and magnetic stirring was performed for 2 hours to obtain an electrospinning solution; S5: electrospinning is performed by an electrospinning device, and the electrospinning conditions are: the inner diameter of the nozzle is 1.0 mm, the flow rate of the electrospinning liquid is 1.3 mL / h, the spinning voltage is 15 kV, the spinning temperature is 21 ° C, and the receiving distance is 12 cm to obtain a precursor fiber membrane; S6: drying, taking out, and calcining, the heating rate is 4 ° C / min, and the temperature is raised to 950 ° C and calcined for 1 hour; S7: taking out, crushing through a 100-mesh sieve, and obtaining a magnesium aluminate fiber membrane; S8: Take 100 parts of nylon 66 and dry; S9: Add 1 part of ethylene bisstearamide and 0.6 parts of antioxidant 1010, mix well, and obtain a premix; S10: Using a co-rotating twin-screw extruder and a side feeding process, 25 parts of magnesium aluminate fiber membrane were added from the side feeding port alone, and the premix was added from the main feeding port. The extrusion was performed into pellets at an extrusion temperature of 270°C, a screw speed of 400 rpm, and vacuum was applied. Comparative Example 2 The difference between this embodiment and embodiment 5 is that the calcination temperature is 1100° C., as follows: A preparation method of a high temperature resistant nylon material, the preparation method is as follows: S1: Mix 75 parts of dichloromethane and 3 parts of anhydrous ethanol; S2: Slowly add 0.8 parts of anhydrous magnesium chloride and 3 parts of anhydrous aluminum chloride, and stir for 35 minutes; S3: heating to 100°C to form a precursor; S4: 6 parts of polyvinyl pyrrolidone, 1.5 parts of phenolic resin and 100 parts of ethanol were mixed, stirred evenly, added to the precursor, and then 30 parts of anhydrous ethanol and 15 parts of N,N-dimethylformamide were added, and magnetic stirring was performed for 2 hours to obtain an electrospinning solution; S5: electrospinning is performed by an electrospinning device, and the electrospinning conditions are: the inner diameter of the nozzle is 1.0 mm, the flow rate of the electrospinning liquid is 1.3 mL / h, the spinning voltage is 15 kV, the spinning temperature is 21 ° C, and the receiving distance is 12 cm, to obtain a precursor fiber membrane coated with phenolic resin; S6: After drying, take out and calcine, the heating rate is 4°C / min, and the temperature is raised to 1100°C and calcined for 1h; S7: taking out, crushing and passing through a 100-mesh sieve to obtain a modified magnesium aluminate fiber membrane; S8: Take 100 parts of nylon 66 and dry; S9: Add 1 part of ethylene bisstearamide and 0.6 parts of antioxidant 1010, mix well, and obtain a premix; S10: Using a co-rotating twin-screw extruder and a side feeding process, 25 parts of modified magnesium aluminate fiber membrane were added from the side feeding port alone, and the premix was added from the main feeding port. The extrusion was performed into granules at an extrusion temperature of 270°C, a screw speed of 400 rpm, and vacuum was applied. Comparative Example 3 The difference between this embodiment and embodiment 2 is that the addition amount of the modified magnesium aluminate fiber membrane is 40 parts, specifically: A method for preparing a high temperature resistant nylon material, the preparation method is as follows: S1: Mix 75 parts of dichloromethane and 3 parts of anhydrous ethanol; S2: Slowly add 0.8 parts of anhydrous magnesium chloride and 3 parts of anhydrous aluminum chloride, and stir for 35 minutes; S3: heating to 100°C to form a precursor; S4: 6 parts of polyvinyl pyrrolidone, 1.5 parts of phenolic resin and 100 parts of ethanol were mixed, stirred evenly, added to the precursor, and then 30 parts of anhydrous ethanol and 15 parts of N,N-dimethylformamide were added, and magnetic stirring was performed for 2 hours to obtain an electrospinning solution; S5: electrospinning is performed by an electrospinning device, and the electrospinning conditions are: the inner diameter of the nozzle is 1.0 mm, the flow rate of the electrospinning liquid is 1.3 mL / h, the spinning voltage is 15 kV, the spinning temperature is 21 ° C, and the receiving distance is 12 cm, to obtain a precursor fiber membrane coated with phenolic resin; S6: After drying, take out and calcine, the heating rate is 4°C / min, and the temperature is raised to 950°C and calcined for 1h; S7: taking out, crushing and passing through a 100-mesh sieve to obtain a modified magnesium aluminate fiber membrane; S8: Take 100 parts of nylon 66 and dry; S9: Add 1 part of ethylene bisstearamide and 0.6 parts of antioxidant 1010, mix well, and obtain a premix; S10: Using a co-rotating twin-screw extruder and a side feeding process, 40 parts of modified magnesium aluminate fiber membrane are added from the side feeding port alone, and the premix is added from the main feeding port, and extrusion granulation is performed. The extrusion temperature is 270°C, the screw speed is 400rpm, and vacuum is applied. Referring to national standards, various properties of the high temperature resistant nylon materials prepared in various embodiments are tested, and the test results are shown in Table 1 below: Table 1 Thermal degradation temperature(℃) Tensile strength(MPa) Bending strength(MPa) Elastic modulus(GPa) Example 1 678.9 73.4 271.4 2.69 Example 2 683.4 74.1 273.5 2.71 Example 3 683.7 73.9 212.8 2.70 Example 4 610.6 70.1 251.3 2.53 Example 5 634.7 71.5 255.9 2.59 Example 6 659.5 72.8 264.7 2.65 Example 7 685.8 73.0 269.9 2.68 Example 8 674.8 73.8 270.6 2.68 Example 9 677.6 73.4 269.4 2.70 Comparative Example 1 666.4 73.9 271.9 2.68 Comparative Example 2 669.7 72.9 268.1 2.67 Comparative Example 3 685.9 64.3 231.5 2.23 The above embodiments are intended to provide a clear and complete description of the technical solution, and are partial implementations of the present invention, rather than all implementations. However, the implementations of the present invention are not limited to the above embodiments, and any other changes, modifications, substitutions, combinations or simplifications that do not deviate from the spirit and principle of the present invention shall be equivalent replacement methods and are included in the protection scope of the present invention.
Claims
1. A high temperature resistant nylon material, characterized by: The invention comprises the following components in parts by weight: 100 parts of nylon 66, 10 to 30 parts of modified magnesium aluminate fiber membrane, 0.5 to 1 part of ethylene bisstearamide and 0.3 to 0.8 part of antioxidant.
2. The method for preparing a high temperature resistant nylon material according to claim 1, characterized in that: The preparation method is as follows: S1: Take nylon 66 and dry it; S2: adding ethylene bisstearamide and antioxidant, mixing evenly to obtain a premix; S3: Use a co-rotating twin-screw extruder and a side feeding process to add the modified magnesium aluminate fiber membrane from the side feeding port alone, and add the premix from the main feeding port for extrusion granulation.
3. The method for preparing a high temperature resistant nylon material according to claim 2, characterized in that: In the S3, the extrusion temperature is 245-280° C., the screw speed is 300-450 rpm, and vacuum is applied.
4. The method for preparing a high temperature resistant nylon material according to claim 2, characterized in that: The preparation method of the modified magnesium aluminate fiber membrane is: S31: Mix 70-80 parts of dichloromethane and 2-3 parts of anhydrous ethanol uniformly; S32: slowly add 0.5-1 parts of anhydrous magnesium chloride and 2-4 parts of anhydrous aluminum chloride, and stir for 30-40 minutes; S33: heating to 100° C. to form a precursor; S34: 5 to 6 parts of polyvinyl pyrrolidone, 1 to 2 parts of phenolic resin and 80 to 100 parts of ethanol are mixed, stirred evenly, added to the precursor, and then 20 to 30 parts of anhydrous ethanol and 10 to 15 parts of N, N-dimethylformamide are added, and magnetic stirring is performed for 2 hours to obtain an electrospinning solution; S35: performing electrospinning by an electrospinning device to obtain a precursor fiber membrane coated with a phenolic resin; S36: drying, taking out and calcining, heating up to 900-1000°C at a rate of 4°C / min and calcining for 1h; S37: Take out, crush and sieve to obtain modified magnesium aluminate fiber membrane.
5. The method for preparing a high temperature resistant nylon material according to claim 4, characterized in that: The electrospinning conditions in S35 are as follows: the inner diameter of the nozzle is 0.8-1.2 mm, the flow rate of the electrospinning liquid is 1-1.5 mL / h, the spinning voltage is 15 kV, the spinning temperature is 20-22° C., and the receiving distance is 12 cm.
6. The high temperature resistant nylon material according to claim 2, characterized in that: The mesh number of the sieving in S37 is 100 meshes.
7. The high temperature resistant nylon material according to claim 1, characterized in that: The antioxidants are antioxidant 1010, antioxidant 1098, antioxidant H161, antioxidant H10, antioxidant 168, and antioxidant 626.