Electric automobile cooling liquid and preparation method thereof
Through the electric vehicle coolant raw materials and preparation methods with specific ratios, the problem of low conductivity and long-term stability of electric vehicle coolant is solved, and the effect of low conductivity and excellent long-term stability is achieved, reducing electrical safety hazards and maintenance costs simplify the production process.
Patent Information
- Application Number
- CN202410959563.7
- Authority / Receiving Office
- CN · China
- Patent Type
- Applications(China)
- Current Assignee / Owner
- Filing Date
- 2024-07-17
- Publication Date
- 2024-11-08
AI Technical Summary
Existing electric vehicle coolant has shortcomings in low conductivity and long-term stability, which may lead to electrical safety hazards and reduced cooling efficiency, and high maintenance costs.
Using raw materials such as ethylene glycol, water, sodium borate, octadecyl phosphate, casson, triethanolamine oleate, benzyl triazole, nanocopper, defoaming agent, buffer and boron nitride nanotubes, through specific By combining and preparing methods, electric vehicle coolant with low conductivity and excellent long-term stability is prepared, which enhances corrosion, corrosion and heat conductivity, and ensures uniform mixing of raw materials through ultrasonic dispersion.
It achieves a comprehensive effect of low conductivity and excellent long-term stability, reduces electrical safety hazards, improves cooling efficiency, simplifies production processes, shortens production cycles, and reduces energy consumption and maintenance costs.
Smart Images

Figure BDA0004949888800000071 
Figure BDA0004949888800000081
Abstract
Description
Technical Field
[0001] The present application relates to the technical field of electric vehicle coolant, and in particular to an electric vehicle coolant and a preparation method thereof. Background Art
[0002] With the increasing attention paid to environmental protection and energy sustainability around the world, new energy technologies are advancing rapidly, and the electric vehicle market has ushered in unprecedented growth. The core of electric vehicles lies in efficient battery systems and electric drive systems. These systems generate a lot of heat under high power output. If the heat cannot be effectively dissipated, it will directly affect the performance, driving safety and even the overall life of the vehicle. Therefore, effective thermal management has become one of the key factors to ensure the performance, safety and life of electric vehicles. As an important part of the thermal management system, electric vehicle coolant is particularly important.
[0003] Electric vehicle coolant is compounded with antifreeze, corrosion inhibitor and other raw materials. It is used in the thermal management system of pure electric vehicles. It is a functional liquid with cooling, anti-corrosion, anti-freezing and heat preservation functions. Compared with the coolant used in traditional fuel vehicles, electric vehicle coolant not only needs to have basic functions such as heat dissipation, anti-freezing and anti-corrosion, but also needs to ensure stable operation under extreme temperatures, and requires low conductivity to ensure electrical safety.
[0004] If some existing electric vehicle coolants fail to sufficiently reduce conductivity, and because the thermal management system of electric vehicles is closely adjacent to the high-voltage electrical system, short circuits may occur when the coolant leaks, leading to serious safety hazards such as circuit system failures, high voltage current generation, and even spontaneous combustion or battery explosion. Some other coolants have reduced stability after long-term use, leading to accelerated corrosion of metal parts and increased deposits inside the cooling system, which not only reduces cooling efficiency but also increases maintenance costs.
[0005] Therefore, there is an urgent need to develop an electric vehicle coolant with low conductivity and excellent long-term stability. Summary of the invention
[0006] In order to solve at least one of the above technical problems, an electric vehicle coolant with low conductivity and excellent long-term stability is developed. The present application provides an electric vehicle coolant and a preparation method thereof.
[0007] On the one hand, the present application provides an electric vehicle coolant, whose raw material composition, measured by weight, includes: 40-60 parts of ethylene glycol, 40-60 parts of water, 0.5-2 parts of sodium borate, 0.5-2 parts of octadecyl phosphate, 0.01-0.1 parts of kason, 0.2-0.8 parts of triethanolamine oleate, 0.5-2 parts of benzotriazole, 0.01-0.1 parts of nano copper, 0.01-0.5 parts of defoaming agent, 0.1-1 parts of buffer, and 0.1-1 parts of boron nitride nanotubes.
[0008] By adopting the above technical solution, the present application adopts specific raw materials and proportions to produce an electric vehicle coolant with low conductivity and excellent long-term stability. The present application adds ethylene glycol as an antifreeze agent, which can significantly reduce the freezing point of water and provide antifreeze protection; it also helps to increase the boiling point of the coolant, prevent boiling at high temperatures, and ensure that the system can still work effectively at extreme temperatures.
[0009] The addition of sodium borate in this application can prevent corrosion of metal parts in the cooling system, and can also form a protective film to reduce electrochemical corrosion. Octadecyl phosphate works together with sodium borate to enhance the anti-corrosion effect, while also having certain lubricating properties and reducing wear. Kasson can prevent deposits or corrosion from forming inside the cooling system and improve the long-term stability of the coolant. Triethanolamine oleate can help disperse and stabilize the particles in the coolant, reduce foam generation, and improve the efficiency of the cooling system. Benzotriazole can effectively prevent corrosion of copper parts, and together with other corrosion inhibitors, form a comprehensive anti-corrosion protection. Nano copper can enhance the thermal conductivity of the coolant, maintain low conductivity, and may also have certain antibacterial properties.
[0010] The present application also adds boron nitride nanotubes, which can significantly improve the thermal conductivity efficiency of the coolant, enhance the heat dissipation effect, help reduce the electrical conductivity of the coolant, and help disperse and stabilize other additives, thereby improving the long-term stability of the coolant.
[0011] Optionally, the raw material composition includes, by weight: 45-55 parts of ethylene glycol, 45-55 parts of water, 1-1.5 parts of sodium borate, 1-1.5 parts of octadecyl phosphate, 0.03-0.08 parts of kason, 0.4-0.6 parts of triethanolamine oleate, 1-1.5 parts of benzotriazole, 0.03-0.08 parts of nano copper, 0.1-0.4 parts of defoaming agent, 0.3-0.8 parts of buffer, and 0.3-0.8 parts of boron nitride nanotubes.
[0012] Optionally, the raw material composition includes, by weight: 50 parts of ethylene glycol, 50 parts of water, 1.2 parts of sodium borate, 1.2 parts of octadecyl phosphate, 0.05 parts of kason, 0.5 parts of triethanolamine oleate, 1.2 parts of benzotriazole, 0.05 parts of nano copper, 0.25 parts of defoaming agent, 0.5 parts of buffer, and 0.5 parts of boron nitride nanotubes.
[0013] Optionally, the weight ratio of triethanolamine oleate to benzotriazole is 1:2-3.
[0014] By adopting the above technical solution, the specific ratio of triethanolamine oleate and benzotriazole in the present application can form a more balanced protective layer on a wider range of metal surfaces, ensuring the long-term safety of all metal components in the cooling system.
[0015] Optionally, the defoaming agent is selected from at least one of polydimethylsiloxane, octanol and dodecanol.
[0016] By adopting the above technical solution, the defoaming agent can quickly eliminate foam and reduce the cooling efficiency loss caused by foam.
[0017] Optionally, the buffer is selected from at least one of potassium dihydrogen phosphate, disodium hydrogen phosphate and sodium citrate.
[0018] By adopting the above technical solution, the buffer can maintain the pH value of the coolant stable, prevent metal corrosion or additive failure caused by pH fluctuations, and improve the long-term stability of the coolant.
[0019] Optionally, the boron nitride nanotubes are single-walled boron nitride nanotubes with an average diameter of 1 to 2 nm.
[0020] By adopting the above technical solutions, single-walled boron nitride nanotubes have a high specific surface area and a pure crystal structure, which can effectively improve the thermal conductivity of the coolant. It helps to quickly remove the heat generated by the battery and motor and maintain the system at the optimal operating temperature. Single-walled boron nitride nanotubes also have low electrical conductivity, and a specific average diameter gives them good dispersibility, ensuring the long-term stability of the coolant and reducing the maintenance cost of the cooling system.
[0021] In a second aspect, the present application provides a method for preparing the above-mentioned electric vehicle coolant, comprising the following steps: S1, mixing the ethylene glycol with water, and sequentially adding sodium borate, octadecyl phosphate, benzotriazole, nano copper, and boron nitride nanotubes, stirring and mixing to obtain a mixed solution; S2. Adding kason, triethanolamine oleate, defoamer and buffer into the mixed solution, stirring and mixing, and ultrasonically dispersing to obtain the electric vehicle coolant.
[0022] By adopting the above technical solution, the preparation method adopted in this application has a simple process flow, convenient operation, shortened production cycle, improved production efficiency, reduced energy consumption and environmental protection. Step-by-step mixing ensures effective mixing and dispersion of all raw materials, thereby achieving a comprehensive effect of low conductivity and excellent long-term stability.
[0023] Optionally, in step S1, the stirring time is 1.5 to 2 hours.
[0024] Optionally, in step S2, the stirring time is 1 to 1.5 hours, and the ultrasonic time is 1.5 to 2 hours.
[0025] By adopting the above technical solution, the stirring time and ultrasonic time of the present application are helpful for uniform dispersion of the raw materials, thereby improving the long-term stability of the electric vehicle coolant.
[0026] In summary, the present invention includes at least one of the following beneficial technical effects: 1. This application adopts specific raw materials and proportions to produce an electric vehicle coolant with low conductivity and excellent long-term stability.
[0027] 2. The application adds boron nitride nanotubes, which helps to reduce the conductivity of the coolant and also helps to disperse and stabilize other additives, thereby improving the long-term stability of the coolant.
[0028] 3. The preparation method adopted in this application has a simple process flow, is easy to operate, shortens the production cycle, improves production efficiency, reduces energy consumption and is environmentally friendly.
[0029] 4. The step-by-step mixing of this application ensures the effective mixing and dispersion of all raw materials, thereby achieving the comprehensive effect of low conductivity and excellent long-term stability. DETAILED DESCRIPTION
[0030] The present application is further described in detail below with reference to the embodiments.
[0031] The present application designs an electric vehicle coolant, and its raw material composition includes, by weight: 40-60 parts of ethylene glycol, 40-60 parts of water, 0.5-2 parts of sodium borate, 0.5-2 parts of octadecyl phosphate, 0.01-0.1 parts of kason, 0.2-0.8 parts of triethanolamine oleate, 0.5-2 parts of benzotriazole, 0.01-0.1 parts of nano copper, 0.01-0.5 parts of defoaming agent, 0.1-1 parts of buffer, and 0.1-1 parts of boron nitride nanotubes.
[0032] The electric vehicle coolant of the present application is prepared by the following method, comprising the following steps: S1, mixing the ethylene glycol with water, and sequentially adding sodium borate, octadecyl phosphate, benzotriazole, nano copper, and boron nitride nanotubes, stirring and mixing to obtain a mixed solution; S2. Adding kason, triethanolamine oleate, defoamer and buffer into the mixed solution, stirring and mixing, and ultrasonically dispersing to obtain the electric vehicle coolant.
[0033] The applicant has designed the technical solution of the present application to address the problems that the conductivity of existing electric vehicle coolants is not low enough, which may pose electrical safety hazards, lack long-term stability, and reduce cooling efficiency.
[0034] The raw materials used in this application are as follows: Ethylene glycol: CAS: 107-21-1.
[0035] Sodium borate: CAS: 13840-56-7.
[0036] Octadecyl phosphate: CAS: 39471-52-8.
[0037] CAS: CAS: 2682-20-4.
[0038] Triethanolamine oleate: CAS: 88107-10-2.
[0039] Benzotriazole: CAS: 95-14-7.
[0040] Nano copper: Zhejiang Yamei Nano Technology Co., Ltd., purity: 99.9%.
[0041] Polydimethylsiloxane: CAS: 9016-00-6.
[0042] Octanol: CAS: 111-87-5.
[0043] Potassium dihydrogen phosphate: CAS: 7778-77-0.
[0044] Sodium citrate: CAS: 68-04-2. Specific embodiments
[0045] Examples 1 to 5 Example 1 The present embodiment provides an electric vehicle coolant, and its raw material composition includes, by weight: 60 parts of ethylene glycol, 40 parts of water, 2 parts of sodium borate, 0.5 parts of octadecyl phosphate, 0.01 parts of kason, 0.8 parts of triethanolamine oleate, 2 parts of benzotriazole, 0.01 parts of nano copper, 0.01 parts of defoaming agent, 1 part of buffer, and 0.1 parts of boron nitride nanotubes; The defoaming agent is polydimethylsiloxane; the buffer is potassium dihydrogen phosphate; and the boron nitride nanotubes are single-walled boron nitride nanotubes with an average diameter of 2 nm.
[0046] The preparation method comprises the following steps: S1. Mix ethylene glycol and water, and add sodium borate, octadecyl phosphate, benzotriazole, nano copper, and boron nitride nanotubes in sequence, and stir for 1.5 hours to obtain a mixed solution; S2. Add kason, triethanolamine oleate, defoamer and buffer into the mixed solution, stir and mix for 1 hour, and ultrasonically disperse for 1.5 hours to obtain electric vehicle coolant.
[0047] Example 2 The present embodiment provides an electric vehicle coolant, and its raw material composition includes, by weight: 45 parts of ethylene glycol, 55 parts of water, 1 part of sodium borate, 1.5 parts of octadecyl phosphate, 0.03 parts of kason, 0.4 parts of triethanolamine oleate, 1 part of benzotriazole, 0.03 parts of nano copper, 0.4 parts of defoaming agent, 0.3 parts of buffer, and 0.8 parts of boron nitride nanotubes; The defoaming agent is polydimethylsiloxane; the buffer is potassium dihydrogen phosphate; and the boron nitride nanotubes are single-walled boron nitride nanotubes with an average diameter of 2 nm.
[0048] The preparation method comprises the following steps: S1. Mix ethylene glycol and water, and add sodium borate, octadecyl phosphate, benzotriazole, nano copper, and boron nitride nanotubes in sequence, and stir for 1.5 hours to obtain a mixed solution; S2. Add kason, triethanolamine oleate, defoamer and buffer into the mixed solution, stir and mix for 1 hour, and ultrasonically disperse for 1.5 hours to obtain electric vehicle coolant.
[0049] Example 3 The present embodiment provides an electric vehicle coolant, and its raw material composition includes, by weight: 50 parts of ethylene glycol, 50 parts of water, 1.2 parts of sodium borate, 1.2 parts of octadecyl phosphate, 0.05 parts of kason, 0.5 parts of triethanolamine oleate, 1.2 parts of benzotriazole, 0.05 parts of nano copper, 0.25 parts of defoaming agent, 0.5 parts of buffer, and 0.5 parts of boron nitride nanotubes; The defoaming agent is polydimethylsiloxane; the buffer is potassium dihydrogen phosphate; and the boron nitride nanotubes are single-walled boron nitride nanotubes with an average diameter of 2 nm.
[0050] The preparation method comprises the following steps: S1. Mix ethylene glycol and water, and add sodium borate, octadecyl phosphate, benzotriazole, nano copper, and boron nitride nanotubes in sequence, and stir for 1.5 hours to obtain a mixed solution; S2. Add kason, triethanolamine oleate, defoamer and buffer into the mixed solution, stir and mix for 1 hour, and ultrasonically disperse for 1.5 hours to obtain electric vehicle coolant.
[0051] Example 4 The present embodiment provides an electric vehicle coolant, and its raw material composition includes, by weight: 55 parts of ethylene glycol, 45 parts of water, 1.5 parts of sodium borate, 1 part of octadecyl phosphate, 0.08 parts of kason, 0.6 parts of triethanolamine oleate, 1.5 parts of benzotriazole, 0.08 parts of nano copper, 0.1 parts of defoaming agent, 0.8 parts of buffer, and 0.3 parts of boron nitride nanotubes; The defoaming agent is polydimethylsiloxane; the buffer is potassium dihydrogen phosphate; and the boron nitride nanotubes are single-walled boron nitride nanotubes with an average diameter of 2 nm.
[0052] The preparation method comprises the following steps: S1. Mix ethylene glycol and water, and add sodium borate, octadecyl phosphate, benzotriazole, nano copper, and boron nitride nanotubes in sequence, and stir for 1.5 hours to obtain a mixed solution; S2. Add kason, triethanolamine oleate, defoamer and buffer into the mixed solution, stir and mix for 1 hour, and ultrasonically disperse for 1.5 hours to obtain electric vehicle coolant.
[0053] Example 5 The present embodiment provides an electric vehicle coolant, and its raw material composition includes, by weight: 40 parts of ethylene glycol, 60 parts of water, 0.5 parts of sodium borate, 2 parts of octadecyl phosphate, 0.1 parts of kason, 0.2 parts of triethanolamine oleate, 0.5 parts of benzotriazole, 0.1 parts of nano copper, 0.5 parts of defoaming agent, 0.1 parts of buffer, and 1 part of boron nitride nanotubes; The defoaming agent is polydimethylsiloxane; the buffer is potassium dihydrogen phosphate; and the boron nitride nanotubes are single-walled boron nitride nanotubes with an average diameter of 2 nm.
[0054] The preparation method comprises the following steps: S1. Mix ethylene glycol and water, and add sodium borate, octadecyl phosphate, benzotriazole, nano copper, and boron nitride nanotubes in sequence, and stir for 1.5 hours to obtain a mixed solution; S2. Add kason, triethanolamine oleate, defoamer and buffer into the mixed solution, stir and mix for 1 hour, and ultrasonically disperse for 1.5 hours to obtain electric vehicle coolant.
[0055] Comparative Examples 1 to 4 Comparative Example 1 The difference between Comparative Example 1 and Example 3 is that no boron nitride nanotubes are added in Comparative Example 1.
[0056] Comparative Example 2 The difference between Comparative Example 2 and Example 3 is that, in Comparative Example 2, triethanolamine oleate and benzotriazole are not added.
[0057] Comparative Example 3 The difference between Comparative Example 3 and Example 3 is that no triethanolamine oleate is added in Comparative Example 3.
[0058] Comparative Example 4 The difference between Comparative Example 4 and Example 3 is that no benzotriazole is added in Comparative Example 4.
[0059] Experimental testing Test items and test methods According to GB 29743.2 "Motor Vehicle Coolant Part 2: Electric Vehicle Coolant", the conductivity of the electric vehicle coolant prepared in this application is tested, and a cyclic bench corrosion test is carried out. The test conditions are 80°C and the cycle is 1064h. The mass change of the brass test piece and the conductivity change rate of the electric vehicle coolant after the test are detected; Conductivity change rate = (conductivity after the test - conductivity before the test) × 100% / conductivity before the test.
[0060] The electric vehicle coolants prepared in Examples 1 to 5 and Comparative Examples 1 to 4 were subjected to conductivity testing, as well as the brass mass change and conductivity change rate of the electric vehicle coolant after the cyclic bench corrosion test. The test results are shown in Table 1.
[0061] Table 1 From the test results in Table 1, it can be seen that the electric vehicle coolant prepared in Examples 1 to 5 has low conductivity. After the cyclic bench corrosion test, the mass change of brass is small and the conductivity change rate is small, indicating that the long-term stability of the electric vehicle coolant is excellent.
[0062] In Comparative Example 1, no boron nitride nanotubes were added, and the conductivity of the obtained electric vehicle coolant increased, and the long-term stability was significantly deteriorated.
[0063] In Comparative Example 2, no triethanolamine oleate and benzotriazole were added. After the cyclic bench corrosion test, the quality of brass and the conductivity change rate of the prepared electric vehicle coolant changed greatly, and the long-term stability was significantly reduced.
[0064] Comparative Example 3 did not add triethanolamine oleate, and Comparative Example 4 did not add benzotriazole. The long-term stability of the obtained electric vehicle coolant was not as good as that of Example 3.
[0065] Embodiments 6 to 10 Example 6 The difference between Example 6 and Example 3 is that in Example 6, the weight ratio of triethanolamine oleate to benzotriazole is 1:2, and the total weight of triethanolamine oleate and benzotriazole is 1.7 parts.
[0066] Example 7 The difference between Example 7 and Example 3 is that in Example 7, the weight ratio of triethanolamine oleate to benzotriazole is 1:3, and the total weight of triethanolamine oleate and benzotriazole is 1.7 parts.
[0067] Example 8 The difference between Example 8 and Example 3 is that in Example 8, the defoaming agent is octanol.
[0068] Example 9 The difference between Example 9 and Example 3 is that in Example 9, the buffer is sodium citrate.
[0069] Example 10 The difference between Example 10 and Example 3 is that the preparation method of Example 10 is as follows: S1, ethylene glycol is mixed with water, sodium borate, octadecyl phosphate, benzotriazole, nano copper, and boron nitride nanotubes are added in sequence, and the mixture is stirred for 2 hours to obtain a mixed solution; S2. Add kason, triethanolamine oleate, defoamer and buffer into the mixed solution, stir and mix for 1.5 hours, and ultrasonically disperse for 2 hours to obtain electric vehicle coolant.
[0070] The electric vehicle coolant prepared in Examples 6 to 10 was subjected to conductivity testing, and the brass mass change and conductivity change rate of the electric vehicle coolant after the cyclic bench corrosion test were tested. The test results are shown in Table 2.
[0071] Table 2 From the test results in Table 2, it can be seen that the difference between Example 6 and Example 7 and Example 3 is that the weight ratios of triethanolamine oleate and benzotriazole are different, and the long-term stability of the electric vehicle coolant prepared in Example 3 is the best.
[0072] Different defoaming agents and buffers are used in Examples 8 and 9, respectively. The conductivity and long-term stability of the obtained electric vehicle coolant are similar to those of Example 3.
[0073] In the preparation method of Example 10, the stirring speed and the ultrasonic speed are different from those of Example 3. The electric vehicle coolant prepared in Example 10 has lower conductivity and better long-term stability. It is speculated that the longer stirring time and ultrasonic time make the raw materials in the electric vehicle coolant more evenly dispersed.
[0074] The above are all preferred embodiments of the present application, and the protection scope of the present application is not limited thereto. Therefore, any equivalent changes made according to the structure, shape, and principle of the present application should be included in the protection scope of the present application.
Claims
1. An electric vehicle coolant, It is characterized in that The raw material composition includes, by weight: 40-60 parts of ethylene glycol, 40-60 parts of water, 0.5-2 parts of sodium borate, 0.5-2 parts of octadecyl phosphate, 0.01-0.1 parts of kason, 0.2-0.8 parts of triethanolamine oleate, 0.5-2 parts of benzotriazole, 0.01-0.1 parts of nano copper, 0.01-0.5 parts of defoaming agent, 0.1-1 parts of buffer, and 0.1-1 parts of boron nitride nanotubes.
2. The electric vehicle coolant according to claim 1, It is characterized in that The raw material composition includes, by weight: 45-55 parts of ethylene glycol, 45-55 parts of water, 1-1.5 parts of sodium borate, 1-1.5 parts of octadecyl phosphate, 0.03-0.08 parts of kason, 0.4-0.6 parts of triethanolamine oleate, 1-1.5 parts of benzotriazole, 0.03-0.08 parts of nano copper, 0.1-0.4 parts of defoaming agent, 0.3-0.8 parts of buffer, and 0.3-0.8 parts of boron nitride nanotubes.
3. The electric vehicle coolant according to claim 1, It is characterized in that The raw material composition includes, by weight: 50 parts of ethylene glycol, 50 parts of water, 1.2 parts of sodium borate, 1.2 parts of octadecyl phosphate, 0.05 parts of kason, 0.5 parts of triethanolamine oleate, 1.2 parts of benzotriazole, 0.05 parts of nano copper, 0.25 parts of defoaming agent, 0.5 parts of buffer, and 0.5 parts of boron nitride nanotubes.
4. The electric vehicle coolant according to claim 1, It is characterized in that The weight ratio of the triethanolamine oleate to benzotriazole is 1:2-3.
5. The electric vehicle coolant according to claim 1, It is characterized in that The defoaming agent is selected from at least one of polydimethylsiloxane, octanol and dodecanol.
6. The electric vehicle coolant according to claim 1, It is characterized in that The buffer is selected from at least one of potassium dihydrogen phosphate, disodium hydrogen phosphate and sodium citrate.
7. The electric vehicle coolant according to claim 1, It is characterized in that The boron nitride nanotubes are single-walled boron nitride nanotubes with an average diameter of 1-2 nm.
8. A method for preparing the electric vehicle coolant according to any one of claims 1 to 7, It is characterized in that The following steps are involved: S1, mixing the ethylene glycol with water, and sequentially adding sodium borate, octadecyl phosphate, benzotriazole, nano copper, and boron nitride nanotubes, stirring and mixing to obtain a mixed solution; S2. Adding kason, triethanolamine oleate, defoamer and buffer into the mixed solution, stirring and mixing, and ultrasonically dispersing to obtain the electric vehicle coolant.
9. The method for preparing the electric vehicle coolant according to claim 8, It is characterized in that In step S1, the stirring time is 1.5 to 2 hours.
10. The method for preparing the electric vehicle coolant according to claim 8, It is characterized in that In step S2, the stirring time is 1 to 1.5 hours, and the ultrasonic time is 1.5 to 2 hours.