Precise temperature control secondary quenching heat treatment process for large carburizing steel conical bearing
Through precise temperature control secondary quenching heat treatment process and material disassembly tooling, the triangular deformation, bending deformation and air-cooling impact of large carburized steel conical bearings during the heat treatment process is solved, and the optimal hardness and tissue performance of the product are achieved, satisfying the Application requirements for heavy loads and impact loads.
Patent Information
- Application Number
- CN202411200425.7
- Authority / Receiving Office
- CN · China
- Patent Type
- Applications(China)
- Current Assignee / Owner
- Filing Date
- 2024-08-29
- Publication Date
- 2024-11-08
AI Technical Summary
In traditional heat treatment, large carburized steel conical bearings have triangular deformation, bending deformation, size problems and air-cooling affect hardness. The existing tooling cannot meet its placement and quenching needs.
Accurate temperature-controlled secondary quenching heat treatment process, including secondary heating, oil bath quenching, low-temperature tempering and cooling processes. Through material scattering and mold pressing technology, temperature and pressure are controlled to ensure that the product reaches the optimal hardness after heat treatment and Organizational performance.
It effectively reduces the deformation and bending deformation of triangles after heat treatment, solves the problem of insufficient tooling size, and ensures that the hardness and tissue performance of the product after being released from the oven through precise temperature control and mold pressing technology.
Smart Images

Figure CN118910390A_ABST
Abstract
Description
Technical Field
[0001] The present invention relates to heat treatment of bearing products, and in particular to a precise temperature-controlled secondary quenching heat treatment process for large-scale carburized steel tapered bearings, and belongs to the technical field of bearing heat treatment. Background Art
[0002] Traditionally, large carburized steel tapered bearings are processed using G20Cr2Ni4 as raw material. If the waiting time is too long before entering the secondary quenching after the carburizing of the rings is completed, the surface quenching temperature will drop, resulting in problems such as troostite and underheating at the organizational level.
[0003] This large carburized steel tapered bearing belongs to the light and thin series. Taking a specific bearing as an example, the wall thickness of the small end face of the ring is 28.36mm, the maximum wall thickness at the large end face is 56.5mm, and the product height is only 95mm. The technical problems existing in the heat treatment process are as follows: The bearing ring needs to be clamped and positioned in the soft turning process. Since the ring is a thin series, a large amount of machining allowance is reserved for soft turning after forging. After the machining, there will be machining stress after the product turning. The stress release in the subsequent heat treatment process will cause triangular deformation, making subsequent machining difficult. During the carburizing process, the ring is light and thin, so the product cannot be compacted on the pad, which will cause the subsequent buckling and deformation to be difficult to control; In the process of preparing for secondary quenching after carburizing, since the outer diameter of the product is 2430mm and the limit size of the existing tooling for heat treatment is 2400mm, there is a size problem in the swinging process; Since the product is carburized steel, it needs to be quenched in a mold after heating. If the air cooling time is too long during the air cooling of the mold after taking it out of the furnace, it will affect the hardness and structure of the product after quenching. Therefore, it is necessary to develop heat treatment technology that can solve the above technical problems and meet production needs. Summary of the invention
[0004] In view of the above-mentioned technical problems that need to be solved, the purpose of the present invention is to provide a precise temperature-controlled secondary quenching heat treatment process for large-scale carburized steel tapered bearings, which can solve the problem of reducing triangular deformation after heat treatment, reduce bending deformation after heat treatment, solve the problem that the existing heat treatment tooling dimensions cannot meet the requirements for bearing placement, and solve the problem of air cooling of bearing products after they are out of the furnace; it is mainly used in applications that bear heavy loads and impact loads, such as steel, cement, wind power and other components.
[0005] In order to achieve the above-mentioned purpose, the technical scheme adopted by the present invention is: a large-scale carburized steel tapered bearing precision temperature control secondary quenching heat treatment process, the soft turning ring after turning is heat treated, the heat treatment process includes: secondary heating, oil bath quenching, low temperature tempering, air cooling and cooling process; the secondary heating process is an austenitizing process, wherein: the temperature, starting 815 ° C, 30 minutes before the temperature is 820 ° C, 10 minutes before the temperature is 825 ° C, the total heating time is 200 minutes, the carbon potential is 0.85%, and the process nitrogen source and other gas sources are introduced; the oil bath quenching: the temperature is 40-80 ° C, the string is 10 minutes, the stay is 30 minutes, the string stirring frequency is 28-32HZ, and the stay stirring frequency is 20HZ; the low temperature tempering: the temperature is 150-160 ° C, the time is 6-10h; The specifications of the large bearing involved in the process of the present invention are: the outer diameter of the ring is 2430mm; Furthermore, before the secondary heating process, the ferrule needs to be pre-treated by a swinging tool and heated in a pit quenching furnace in the secondary heating process; Furthermore, after the secondary heating, when entering the oil quenching process, the ferrule needs to be pressed by a mold and quenched in the quenching oil tank in the oil quenching process; Furthermore, the nitrogen flow rate of the secondary heating process is 6-10m³ / h, and other gas sources include methanol and propane, wherein methanol: 3.0-3.5L / h, propane: 0-1.4L / h; This solution raises the temperature from 815℃ to 820℃ 30 minutes before the product is taken out of the furnace during the secondary heating process, and raises the temperature from 820℃ to 825℃ 10 minutes before the product is taken out of the furnace. This precise temperature control method is used to solve the problem of air cooling after the ferrule is taken out of the furnace; it ensures that the surface of different layers of the product can still reach the process target temperature after the loss of normal temperature air after being taken out of the heating furnace; Furthermore, in order to solve the problem of reducing the triangular deformation after heat treatment, the soft-turned ring after turning is subjected to stress relief annealing at a temperature of 650°C for 8 hours to release stress after the rough turning process in the soft turning process, and then fine-processed to the soft-turned finished product state; the reason is that the ring belongs to the light and thin series, resulting in a large processing allowance reserved for soft turning after forging, which will cause processing stress after product turning; Furthermore, the technical solution reduces the bending deformation after heat treatment and the means for the existing heat treatment tooling to be insufficient in size and unable to meet the requirements is achieved through the swing tooling of the solution; the swing tooling includes a number of shims evenly arranged on the quenching base and a pad located between the upper end surface of the shim and the lower end surface of the ring; when in use, a number of shims are evenly placed on the upper surface of the existing 2400mm quenching base, so that the lower end surface (bottom surface) of the ring is in a theoretical plane and the pad is placed on the theoretical plane, and then the ring is placed on the pad, so that the product and the pad are compacted, thereby achieving the flatness of the ring during the clamping process, and ensuring the flatness of the ring after heat treatment; Furthermore, the washer is a circular ring with a thickness of 50 mm and a diameter of 100 mm; two pads are provided on each washer; the ring is leveled by the pad, further ensuring that the ring is padded on the pad to ensure flatness.
[0006] Furthermore, in this scheme, the ring needs to be pressed by the mold using a double-hanging interlacing method after being heated and entering the oil bath quenching; the specific means are: one hanger lifts the ring product out of the heating furnace, and another hanger uses a three-claw hook to clamp and place it on the mold, and the other hanger then lifts the upper mold and drops it on the upper end of the product, thereby completing the entire pressing process, and the pressing is completed and then enters the quenching oil tank for quenching; Furthermore, the entire compression molding process is controlled within 3 minutes and 50 seconds to 4 minutes, meeting the performance indicators of the surface hardness and core hardness, as well as the structure, troostite and the like after the product is heat treated.
[0007] Furthermore, in the oil bath quenching process, the string movement is achieved by moving the crane up and down.
[0008] Furthermore, in the oil bath quenching process, the specific stirring method is: stirring in the quenching oil tank, four large stirring motors drive the impellers to perform rapid stirring in the first step, and when staying, four small stirring motors on the sides drive the impellers to cool slowly.
[0009] The beneficial effects of the present invention are: Achieve technological innovation from multiple aspects; solve the problem of reducing triangle deformation after heat treatment by releasing stress through 650℃ 8-hour stress relief annealing after rough turning process in soft turning process; By setting up and applying the swinging tooling, the problem of the product and the pad being unable to be pressed together is solved, and the bending deformation after heat treatment is reduced, thereby ensuring the flatness of the ferrule product after heat treatment; At the same time, the existing heat treatment tooling is combined with the material placement tooling to solve the problem that the original tooling cannot meet the product placement requirements due to its limited size. By using precise temperature control during the heating process, the problem of surface temperature loss during quenching due to long air cooling time can be avoided; Finally, after the heating is completed, the die is subjected to oil quenching to meet the product's surface hardness, core hardness, structure, troostite and other performance indicators after heat treatment. BRIEF DESCRIPTION OF THE DRAWINGS
[0010] Figure 1 This is a flow chart of the process curve for the precise temperature-controlled secondary quenching heat treatment of large carburized steel tapered bearings of the present invention.
[0011] Figure 2 This is a diagram of a bearing product according to the present invention.
[0012] Figure 3 It is the material placing tooling diagram of the present invention.
[0013] Figure 4 This is a die diagram of the compression mold of the present invention (mold pressing state).
[0014] Figure 5 for Figure 4 Side view of.
[0015] In the figure, 1, quenching base, 2, washer, 3, ring, 4, the location of the ring of the mold. DETAILED DESCRIPTION
[0016] In order to make the structure and function of the present invention clearer, the technical solutions in the embodiments of the present invention will be clearly and completely described below in conjunction with the accompanying drawings in the embodiments of the present invention.
[0017] See also Figure 1 , this solution is specifically described with specific process parameters of an embodiment of the present invention; The precision temperature-controlled secondary quenching heat treatment process for large carburized steel tapered bearings is used to heat treat the soft-turned rings after turning. The heat treatment process includes: secondary heating, oil bath quenching, low-temperature tempering, air cooling and cooling processes; the secondary heating process is an austenitizing process, wherein: the temperature is 815°C at the start, the temperature reaches 820°C 30 minutes before leaving the furnace, 825°C 10 minutes before leaving the furnace, the total heating time is 200 minutes, the carbon potential is 0.85%, and the process nitrogen source and other gas sources are introduced; the oil bath quenching: the temperature is 40-80°C, the string is moved for 10 minutes, the dwell time is 30 minutes, the string stirring frequency is 28-32HZ, and the dwell stirring frequency is 20HZ; the low-temperature tempering: the temperature is 150-160°C, and the time is 6-10h; Before the secondary heating process, the ferrule needs to be pre-treated by a swinging tool and heated in a pit-type quenching furnace in the secondary heating process; After secondary heating, the ring needs to be pressed by a die and quenched in the quenching oil tank in the oil quenching process. The nitrogen flow rate of the secondary heating process is 6-10m³ / h, and other gas sources include methanol and propane, wherein methanol: 3.0-3.5L / h, propane: 0-1.4L / h; This solution uses the method of raising the temperature from 815°C to 820°C 30 minutes before the second heating process, and raising the temperature from 820°C to 825°C 10 minutes before the final heating. The purpose of using this precise temperature control method is to solve the problem of air cooling of the ferrule after it is taken out of the furnace; to ensure that after the product is taken out of the heating furnace, the surfaces of different layers can still reach the process target temperature after being lost to normal temperature air; it should be noted that if the precise temperature control process of this solution is not adopted, the surface temperature of the die will drop to a temperature below the process target range due to the time required for the die pressing, resulting in low hardness on the surface and higher hardness as it goes deeper; at the same time, the organization will be underheated, so it can be explained that this solution can achieve a better austenitized structure.
[0018] Based on the technical solution of this application and the technical problems existing in the heat treatment process of this product, the following corresponding innovative improvements have been made: 1. Reduce the problem of triangle deformation after heat treatment The ring needs to be positioned on a fixture during the soft turning process. As the ring is a thin series, a large amount of machining allowance is reserved for soft turning after forging, which will cause machining stress after the product is turned. We use stress relief annealing at 650°C for 8 hours after the rough turning process in the soft turning process to release the stress, and then perform fine machining to the soft turning finished product state.
[0019] 2. Reduce bending deformation after heat treatment This is achieved through the material swinging tooling of the scheme; the material swinging tooling comprises a number of washers evenly arranged on the quenching base and a pad located between the upper end surface of the washers and the lower end surface of the ferrule; when in use, a number of washers are evenly arranged on the upper surface of the existing 2400mm quenching base, so that the lower end surface (bottom surface) of the ferrule is in a theoretical plane and the pad is arranged on the theoretical plane, and then the ferrule is placed on the pad, so that the product and the pad are compacted, thereby achieving the flatness of the ferrule during the clamping process and ensuring the flatness of the ferrule after heat treatment; Among them, the washer is a circular ring with a thickness of 50mm and a diameter of 100mm; two pads are set on each washer; the ring is leveled by the pad, further ensuring that the ring is padded on the pad to ensure flatness.
[0020] 3. Ring secondary quenching tooling material placement In order to solve the problem that the existing heat treatment tooling cannot meet the requirements of this product, shims are placed on the existing 2400mm quenching base to ensure the loading and placement of the product.
[0021] 4. Solve the problem of air cooling after the product comes out of the oven In this scheme, the ring needs to be pressed by the mold using a double-hanging interlacing method after being heated and entering the oil bath quenching; the specific means are: one hanger lifts the ring product out of the heating furnace, and the other hanger uses a three-claw hook to clamp and place it on the mold, and the other hanger then lifts the upper mold and drops it on the upper end of the product, thereby completing the entire pressing process, and the pressing is completed and then enters the quenching oil tank for quenching; The entire compression molding process is controlled within 3 minutes and 50 seconds to 4 minutes, meeting the product's performance indicators such as surface hardness and core hardness after heat treatment as well as structure, troostite, etc.
[0022] The physical test results of the product are as follows: Decarburization depth: 0.07mm Martensite structure: Level 2 Functional area Troostite (3-4mm): None Surface hardness: 59.6HRC 59.5HRC 59.7HRC Core hardness: 40.4HRC 41.3HRC 41.4HRC 58HRC Depth: 6.54mm 550HV1 Depth: 8.45mm Retained austenite: 18.6% Grain size: 8 levels.
[0023] The above examples are only the best embodiments of the present invention. Obviously, the present invention is not limited to the above embodiments, and many variations are possible. All variations that can be directly derived or associated with the contents disclosed by a person skilled in the art should be considered as the protection scope of the present invention.
Claims
1. A precision temperature controlled secondary quenching heat treatment process for large carburized steel tapered bearings, characterized in that: The soft-turned ring after turning is heat treated, and the heat treatment process includes: secondary heating, oil bath quenching, low-temperature tempering, air cooling and cooling process; the secondary heating process is an austenitizing process, wherein: the temperature is 815°C at the start, the temperature reaches 820°C 30 minutes before the furnace, 825°C 10 minutes before the furnace, the total heating time is 200 minutes, the carbon potential is 0.85%, and the process nitrogen source and other gas sources are introduced; the oil bath quenching: the temperature is 40-80°C, the string is switched for 10 minutes, the dwell time is 30 minutes, the string stirring frequency is 28-32HZ, and the dwell stirring frequency is 20HZ; the low-temperature tempering: the temperature is 150-160°C, and the time is 6-10h.
2. According to claim 1, a large carburizing steel tapered bearing precision temperature control secondary quenching heat treatment process is characterized by: Before the secondary heating process, the ferrule needs to be pre-treated by a swinging tool and heated in a pit-type quenching furnace in the secondary heating process.
3. According to claim 1, a large carburizing steel tapered bearing precision temperature control secondary quenching heat treatment process is characterized by: After the secondary heating, the ring needs to be pressed by a mold and quenched in the quenching oil tank in the oil quenching process.
4. According to claim 1, a large carburizing steel tapered bearing precision temperature control secondary quenching heat treatment process is characterized by: The nitrogen flow rate of the secondary heating process is 6-10m³ / h, and other gas sources include methanol and propane, among which methanol: 3.0-3.5L / h, propane: 0-1.4 L / h.
5. According to claim 1, a large carburizing steel tapered bearing precision temperature control secondary quenching heat treatment process is characterized by: The soft-turned ferrule after turning is subjected to stress relief annealing at a temperature of 650° C. for 8 hours to release stress after the rough turning process in the soft-turning process.
6. According to claim 2, a large carburizing steel tapered bearing precision temperature control secondary quenching heat treatment process is characterized by: The material placing tooling comprises a plurality of shims evenly arranged on the quenching base and a pad located between the upper end surface of the shims and the lower end surface of the ferrule; when in use, the existing 2400mm upper surface of the quenching base is used to evenly place a plurality of shims, so that the lower end surface of the ferrule is in a theoretical plane and the pad is placed on the theoretical plane, and then the ferrule is placed on the pad, so that the product and the pad are compacted, thereby achieving the flatness of the ferrule during the clamping process.
7. According to claim 6, a large carburized steel tapered bearing precision temperature control secondary quenching heat treatment process is characterized by: The washer is a circular ring with a thickness of 50 mm and a diameter of 100 mm; two of the cushion blocks are arranged on each washer.
8. According to claim 3, a large carburizing steel tapered bearing precision temperature control secondary quenching heat treatment process is characterized by: After the ring is heated and then enters the oil bath for quenching, it needs to be pressed through the mold using a double-hoist interlaced method; the specific method is: one hoist lifts the ring product out of the heating furnace, and another hoist uses a three-claw hook to clamp it and place it on the mold, and the other hoist then lifts the upper mold and drops it on the upper end of the product, thereby completing the entire pressing process. After the pressing is completed, it enters the quenching oil tank for quenching.
9. The precise temperature-controlled secondary quenching heat treatment process for large carburized steel tapered bearings according to claim 8 is characterized in that: The entire compression molding process is controlled within 3 minutes 50 seconds to 4 minutes.