Flat solid oxide fuel cell functional layer sealing detection method
Through the combination of gas pressure-regulating assembly and pressure loading assembly, rapid and accurate leakage detection of the electrolyte layer of solid oxide fuel cell is achieved, solving the existing problems of low detection efficiency and insufficient applicability, and improving production efficiency and cost-effectiveness .
Patent Information
- Application Number
- CN202411224530.4
- Authority / Receiving Office
- CN · China
- Patent Type
- Applications(China)
- Current Assignee / Owner
- Filing Date
- 2024-09-03
- Publication Date
- 2024-11-08
- Estimated Expiration
- Not applicable · inactive patent
AI Technical Summary
The existing seal detection method of solid oxide fuel cell functional layer cannot determine the leakage rate of the electrolyte layer, the detection process is low, batch detection cannot be detected, and cannot match the subject to be inspected of multiple specifications.
The detection method including gas pressure stabilization assembly and pressure loading assembly is adopted. The gas pressure stabilization assembly is used to buffer and regulate the pressure of the gas, and combined with cylinder pressurization, the positive pressure detection of the battery is realized, the leakage amount is judged, and the detection efficiency and accuracy are improved. And use replaceable fixtures to apply batteries of different specifications.
It realizes fast and accurate electrolyte layer airtightness testing, improves production efficiency, reduces labor costs, supports batch inspection and the application of multi-spec batteries.
Smart Images

Figure CN118913555A_ABST
Abstract
Description
Technical Field
[0001] The present invention relates to the technical field of solid oxide fuel cells and material processing, and more specifically to a method for detecting the sealing of a functional layer of a flat solid oxide fuel cell. Background Art
[0002] Solid oxide fuel cell (SOFC) is a highly efficient, pollution-free, all-solid-state power generation device that can adapt to a variety of fuel gases and does not require an additional reformer. The battery structure mainly includes a support, an anode layer, an electrolyte layer, a barrier layer, a cathode layer, etc. Among them, the electrolyte layer must form a dense isolation layer to block the fuel gas and air. The sealing of the electrolyte is particularly important, so the electrolyte layer needs to be tested for sealing.
[0003] The following are the methods for detecting the electrolyte layer: 1. Observe by scanning with an electron microscope. This method can observe the density of the electrolyte layer more intuitively and accurately, but it cannot determine the leakage rate of the electrolyte layer;
[0004] 2. Use negative pressure airtightness tester to test the airtightness of the battery. This method pumps negative pressure on the battery functional layer and then maintains the pressure to observe its leakage rate. This method has high requirements on the flatness of the battery. If the flatness is poor, it is necessary to manually press the upper part of the battery to make the equipment workbench adsorb the battery to complete the subsequent negative pressure detection and observation, thus affecting the efficiency of the entire detection process.
[0005] 3. The current testing methods are not capable of carrying out mass testing and the testing time is too long.
[0006] 4. The existing detection methods have single functions and cannot match many kinds of inspection objects.
[0007] In view of this, we propose a method for detecting the sealing of the functional layer of a planar solid oxide fuel cell. Summary of the invention
[0008] The purpose of the present invention is to provide a method for detecting the sealing of a functional layer of a flat solid oxide fuel cell, so as to solve the technical problems that the current method for detecting the sealing of a functional layer of a solid oxide fuel cell cannot determine the leakage rate of the electrolyte layer, the detection process is inefficient, batch detection is impossible, the detection time is long, and multiple specifications of objects cannot be matched.
[0009] In order to solve the above technical problems, the present invention provides the following technical solutions: A method for detecting the sealing of a functional layer of a flat solid oxide fuel cell, comprising a gas pressure stabilizing assembly and a pressure loading assembly, wherein the gas pressure stabilizing assembly comprises a first pressure reducing valve, a solenoid valve, a first proportional valve, a gas tank and a first supporting frame, wherein the first pressure reducing valve, the solenoid valve, the first proportional valve and the gas tank are arranged on the first supporting frame;
[0010] The pressure loading assembly includes a three-position five-way solenoid valve, a second proportional valve, a cylinder, a work platform fixture, a pressurizing fixture, a second pressure reducing valve, a second support frame and a mounting frame. The three-position five-way solenoid valve, the second proportional valve, the work platform fixture and the second pressure reducing valve are arranged on the second support frame, a mounting frame is arranged on the top of the work platform fixture, the cylinder is arranged at the center of the top of the mounting frame, and the pressurizing fixture is arranged at the piston end of the cylinder;
[0011] The output end of the gas tank is connected to the working platform fixture through a conduit.
[0012] The battery cell of the present invention is subjected to positive pressure testing. The battery is placed on the lower working platform fixture, and the battery cell is pressurized and sealed by controlling the upper pressurization fixture. When all contact surfaces are completely sealed, the product is inflated to make its internal pressure higher than the external atmospheric pressure. The pressure change is observed by an airtightness detector to determine the size of the leakage, and then the leakage of the product is inferred. Therefore, the battery electrolyte layer can be effectively and quickly tested for airtightness. The gas voltage stabilizing component can buffer and stabilize the gas to ensure the accuracy of the airtightness test. The positive pressure combined with the cylinder pressurization can make the battery test efficiently complete the test, improve the production efficiency, reduce the labor cost, thereby reducing the production cost, and facilitate batch testing. The working platform fixture of the present invention is easy to replace and can be used for airtightness testing of batteries of different specifications.
[0013] Preferably, a high-precision pressure gauge is arranged on the top of the gas tank.
[0014] Preferably, a locking piece is arranged on the pressurizing fixture.
[0015] Preferably, a universal joint is arranged at the piston end of the cylinder, and the universal joint is connected to the pressurizing fixture, and a pressure sensor is arranged on the universal joint.
[0016] Preferably, the mounting frame includes a guide rod and a mounting plate, the guide rod is arranged at the four corners of the top of the working platform clamp, the mounting plate is arranged at the top of the guide rod, and the guide rod passes through the pressurizing clamp.
[0017] Preferably, the input end of the first pressure reducing valve is connected to an external source, the output end of the first pressure reducing valve is connected to the input end of the first proportional valve through a conduit, the output end of the first proportional valve is connected to the input end of the solenoid valve through a conduit, and the output end of the solenoid valve is connected to the input end of the gas tank through a conduit.
[0018] Preferably, the input end of the second pressure reducing valve is connected to an external source, the output end of the second pressure reducing valve is connected to the input end of a three-position five-way solenoid valve through a conduit, the output end of the three-position five-way solenoid valve is connected to the input end of a second proportional valve through a conduit, and the input end of the second proportional valve is respectively connected to the air inlet and air outlet of the cylinder through a conduit.
[0019] A method for using a method for detecting the sealing of a functional layer of a planar solid oxide fuel cell comprises the following steps:
[0020] S1, coming out from the gas source, the gas is reduced in pressure by the first pressure reducing valve, and then passes through the first proportional valve to control the pressure, and then passes through the solenoid valve to reach the gas tank, and the gas tank stabilizes and buffers the incoming gas, and finally enters the work platform fixture through the pipeline;
[0021] S2, the gas source is decompressed by the second pressure reducing valve, and reaches the second proportional valve after the gas path is controlled by the three-position five-way solenoid valve. Under the regulation of the second proportional valve, pressure is applied to the cylinder, and the battery cell is pressurized and fixed at this time;
[0022] S3. Perform positive pressure testing on the battery cell. Place the battery on the lower working platform fixture, and pressurize and seal the battery cell by controlling the upper pressurization fixture. When all contact surfaces are completely sealed, the product is inflated with gas after being stabilized and buffered by the gas tank to make its internal pressure higher than the external atmospheric pressure. The amount of leakage is determined by observing the pressure changes, and the leakage amount of the product can be inferred.
[0023] Compared with the prior art, the present invention has the following beneficial effects:
[0024] 1. The present invention performs positive pressure testing on battery cells, places the battery on the lower working platform fixture, and controls the upper part of the pressurized fixture to pressurize and seal the battery cells. When all contact surfaces are completely sealed, the product is inflated to make its internal pressure higher than the external atmospheric pressure. The pressure change is observed by an airtightness detector to determine the size of the leakage, and then the leakage of the product is inferred. Therefore, the airtightness test of the battery electrolyte layer can be effectively and quickly performed. Therefore, the present invention has the advantage of quickly detecting the size of the leakage of the battery electrolyte layer.
[0025] 2. The gas pressure stabilizing component in the present invention can buffer and stabilize the gas pressure, thereby ensuring the accuracy of air tightness detection.
[0026] 3. The present invention can efficiently complete the battery inspection through positive pressure combined with cylinder pressurization, improve production efficiency, reduce labor costs, thereby reducing production costs, and facilitate batch inspection.
[0027] 4. The fixture of the present invention is easy to replace and can be used for airtight testing of batteries of different specifications. BRIEF DESCRIPTION OF THE DRAWINGS
[0028] Figure 1 It is a schematic diagram of the workflow of the present invention;
[0029] Figure 2 It is an overall schematic diagram of the present invention;
[0030] Figure 3 It is a schematic diagram of the structure of the gas pressure stabilizing assembly of the present invention;
[0031] Figure 4 It is a schematic diagram of the structure of the pressure loading component of the present invention.
[0032] Description of the numbers in the figure:
[0033] 1. Gas pressure stabilizing assembly; 101. First pressure reducing valve; 102. Solenoid valve; 103. First proportional valve; 104. Gas tank; 105. High-precision pressure gauge; 106. First support stand; 2. Pressure loading assembly; 201. Three-position five-way solenoid valve; 202. Second proportional valve; 203. Cylinder; 204. Work platform fixture; 205. Pressurizing fixture; 206. Locking piece; 207. Universal joint; 208. Pressure sensor; 209. Second pressure reducing valve; 2010. Second support stand; 2011. Mounting frame; 2012. Guide rod; 2013. Mounting plate. DETAILED DESCRIPTION
[0034] like Figure 1 , Figure 2 , Figure 3 and Figure 4 As shown, the present invention relates to a method for detecting the sealing of a functional layer of a flat solid oxide fuel cell, comprising a gas pressure stabilizing component 1 and a pressure loading component 2, wherein the gas pressure stabilizing component 1 comprises a first pressure reducing valve 101, a solenoid valve 102, a first proportional valve 103, a gas tank 104 and a first supporting frame 106, wherein the first pressure reducing valve 101, the solenoid valve 102, the first proportional valve 103 and the gas tank 104 are arranged on the first supporting frame 106; the input end of the first pressure reducing valve 101 is connected to an external source, and the first pressure reducing valve 101 is connected to an external source. The output end is connected to the input end of the first proportional valve 103 through a conduit, the output end of the first proportional valve 103 is connected to the input end of the solenoid valve 102 through a conduit, the output end of the solenoid valve 102 is connected to the input end of the gas tank 104 through a conduit, and the gas comes out from the gas source end, the gas is reduced in pressure by the first pressure reducing valve 101, and then passes through the first proportional valve 103 for pressure control, and then passes through the solenoid valve 102 to reach the gas tank 104, and the gas introduced is stabilized and buffered by the gas tank 104, and finally enters the working platform fixture 204 through the pipeline;
[0035] The pressure loading assembly 2 includes a three-position five-way solenoid valve 201, a second proportional valve 202, a cylinder 203, a work platform fixture 204, a pressurizing fixture 205, a second pressure reducing valve 209, a second support frame 2010 and a mounting frame 2011. The three-position five-way solenoid valve 201, the second proportional valve 202, the work platform fixture 204 and the second pressure reducing valve 209 are arranged on the second support frame 2010, the mounting frame 2011 is arranged on the top of the work platform fixture 204, the cylinder 203 is arranged at the top center of the mounting frame 2011, and the pressurizing fixture 205 is arranged at the piston end of the cylinder 203; the input end of the second pressure reducing valve 209 is connected to an external source, and the second pressure reducing valve 209 is connected to the external source. The output end of the pressure reducing valve 209 is connected to the input end of the three-position five-way solenoid valve 201 through a conduit, and the output end of the three-position five-way solenoid valve 201 is connected to the input end of the second proportional valve 202 through a conduit, and the input end of the second proportional valve 202 is respectively connected to the air inlet and the air outlet of the cylinder 203 through a conduit. The air source is reduced in pressure by the second pressure reducing valve 209, and reaches the second proportional valve 202 after the air path is controlled by the three-position five-way solenoid valve 201. Under the regulation of the second proportional valve 202, pressure is applied to the cylinder 203, and the cylinder 203 applies pressure to the pressurizing fixture 205. At this time, the pressurizing fixture 205 cooperates with the working platform fixture 204 to pressurize and fix the battery sheet;
[0036] The output end of the gas tank 104 is connected to the work platform fixture 204 through a conduit.
[0037] Perform positive pressure testing on the battery cell, place the battery on the lower working platform fixture 204, and control the upper part of the pressurizing fixture 205 to pressurize and seal the battery cell. When all contact surfaces are completely sealed, the gas after pressure stabilization and buffering by the gas tank 104 is used to inflate the product, so that its internal pressure is higher than the external atmospheric pressure. The size of the leakage is judged by observing the pressure change, and then the leakage of the product is inferred. Therefore, the battery electrolyte layer can be effectively and quickly tested for air tightness, because the gas tank 104 can buffer and stabilize the gas, which can ensure the accuracy of the air tightness test, and the positive pressure combined with the pressurization of the cylinder 203 can make the battery test efficiently, improve the production efficiency, reduce labor costs, thereby reducing production costs, and facilitate batch testing. The working platform fixture 204 is easy to replace and can be used for air tightness testing of batteries of different specifications.
[0038] Specifically, a high-precision pressure gauge 105 is arranged on the top of the gas tank 104. The high-precision pressure gauge 105 is convenient for observing the pressure change, so as to judge the leakage amount.
[0039] Furthermore, a locking piece 206 is arranged on the pressurizing fixture 205 . After the pressurizing fixture 205 cooperates with the working platform fixture 204 to pressurize and seal the battery cell, the pressurizing fixture 205 and the working platform fixture 204 are locked by the locking piece 206 .
[0040] Furthermore, a universal joint 207 is arranged at the piston end of the cylinder 203, and the universal joint 207 is connected to the pressurizing clamp 205. A pressure sensor 208 is arranged on the universal joint 207. The cylinder 203 is connected to the pressurizing clamp 205 through the universal joint 207. The pressure sensor 208 is used to detect the size of the pressure applied by the pressurizing clamp 205 to the battery cell.
[0041] It is worth mentioning that the mounting frame 2011 includes a guide rod 2012 and a mounting plate 2013. The guide rod 2012 is arranged at the four corners of the top of the working platform clamp 204, and the mounting plate 2013 is arranged on the top of the guide rod 2012. The guide rod 2012 passes through the pressurizing clamp 205. The guide rod 2012 facilitates the stable up and down displacement of the pressurizing clamp 205, and the mounting plate 2013 is used for the installation of the cylinder 203.
[0042] Working principle: This embodiment provides a method for detecting the sealing of a functional layer of a flat solid oxide fuel cell. When in use, first, the gas comes out from the gas source end, is reduced in pressure by the first pressure reducing valve 101, and then is controlled by the first proportional valve 103, and then reaches the gas tank 104 through the solenoid valve 102. The gas tank 104 stabilizes and buffers the gas entering, and finally enters the working platform fixture 204 through the pipeline;
[0043] Secondly, the gas source is decompressed by the second pressure reducing valve 209, and reaches the second proportional valve 202 after the gas path is controlled by the three-position five-way solenoid valve 201. Under the regulation of the second proportional valve 202, pressure is applied to the cylinder 203, and the cylinder 203 applies pressure to the pressurizing fixture 205. At this time, the pressurizing fixture 205 cooperates with the working platform fixture 204 to pressurize and fix the battery cell;
[0044] Finally, the battery cell is tested for positive pressure. The battery is placed on the lower working platform fixture 204. The battery cell is pressurized and sealed by controlling the upper part of the pressurizing fixture 205. The pressurizing fixture 205 is then locked with the working platform fixture 204 by the locking piece 206. When all contact surfaces are completely sealed, the product is inflated with the gas after pressure stabilization and buffering by the gas tank 104, so that its internal pressure is higher than the external atmospheric pressure. The pressure change is observed by the high-precision pressure gauge 105 to determine the size of the leakage, and then the leakage of the product is inferred. Therefore, the battery electrolyte layer can be effectively and quickly tested for air tightness, because the gas tank 104 can buffer and stabilize the gas, which can ensure the accuracy of the air tightness test, and the positive pressure combined with the cylinder 203 pressurization can make the battery test efficiently, thereby improving production efficiency, reducing labor costs, thereby reducing production costs, and facilitating batch testing. The working platform fixture 204 is easy to replace and can be used for air tightness testing of batteries of different specifications.
[0045] The embodiments of the present invention disclose preferred embodiments, but are not limited thereto. A person skilled in the art can easily understand the spirit of the present invention based on the above embodiments and make different extensions and changes. However, as long as they do not deviate from the spirit of the present invention, they are all within the protection scope of the present invention.
Claims
1. A method for detecting the sealing of a functional layer of a planar solid oxide fuel cell, characterized in that: The invention comprises a gas pressure stabilizing assembly (1) and a pressure loading assembly (2); the gas pressure stabilizing assembly (1) comprises a first pressure reducing valve (101), a solenoid valve (102), a first proportional valve (103), a gas tank (104) and a first supporting frame (106); the first pressure reducing valve (101), the solenoid valve (102), the first proportional valve (103) and the gas tank (104) are arranged on the first supporting frame (106); The pressure loading assembly (2) comprises a three-position five-way solenoid valve (201), a second proportional valve (202), a cylinder (203), a working platform fixture (204), a pressurizing fixture (205), a second pressure reducing valve (209), a second supporting frame (2010) and a mounting frame (2011); the three-position five-way solenoid valve (201), the second proportional valve (202), the working platform fixture (204) and the second pressure reducing valve (209) are arranged on the second supporting frame (2010); a mounting frame (2011) is arranged on the top of the working platform fixture (204); the cylinder (203) is arranged at the top center of the mounting frame (2011); and the pressurizing fixture (205) is arranged at the piston end of the cylinder (203); The output end of the gas tank (104) is connected to the working platform fixture (204) via a conduit.
2. A method for detecting sealing of a functional layer of a planar solid oxide fuel cell according to claim 1, characterized in that: A high-precision pressure gauge (105) is arranged on the top of the gas tank (104).
3. A method for detecting sealing of a functional layer of a planar solid oxide fuel cell according to claim 1, characterized in that: A locking piece (206) is arranged on the pressurizing clamp (205).
4. A method for detecting sealing of a functional layer of a planar solid oxide fuel cell according to claim 1, characterized in that: A universal joint (207) is arranged at the piston end of the cylinder (203), and the universal joint (207) is connected to the pressurizing fixture (205), and a pressure sensor (208) is arranged on the universal joint (207).
5. A method for detecting sealing of a functional layer of a planar solid oxide fuel cell according to claim 1, characterized in that: The mounting frame (2011) comprises a guide rod (2012) and a mounting plate (2013); the guide rod (2012) is arranged at the four corners of the top of the working platform clamp (204); the mounting plate (2013) is arranged at the top of the guide rod (2012); and the guide rod (2012) passes through the pressure clamp (205).
6. A method for detecting sealing of a functional layer of a planar solid oxide fuel cell according to claim 1, characterized in that: The input end of the first pressure reducing valve (101) is connected to an external source, the output end of the first pressure reducing valve (101) is connected to the input end of a first proportional valve (103) through a conduit, the output end of the first proportional valve (103) is connected to the input end of an electromagnetic valve (102) through a conduit, and the output end of the electromagnetic valve (102) is connected to the input end of a gas tank (104) through a conduit.
7. A method for detecting sealing of a functional layer of a planar solid oxide fuel cell according to claim 1, characterized in that: The input end of the second pressure reducing valve (209) is connected to an external source, the output end of the second pressure reducing valve (209) is connected to the input end of the three-position five-way solenoid valve (201) through a conduit, the output end of the three-position five-way solenoid valve (201) is connected to the input end of the second proportional valve (202) through a conduit, and the input end of the second proportional valve (202) is respectively connected to the air inlet and the air outlet of the cylinder (203) through a conduit.
8. A method for using a method for detecting sealing of a functional layer of a planar solid oxide fuel cell according to any one of claims 1 to 7, characterized in that: The following steps are involved: S1, the gas comes out from the gas source, is decompressed by the first pressure reducing valve (101), passes through the first proportional valve (103) for pressure control, and then passes through the solenoid valve (102) to reach the gas tank (104), and the gas tank (104) stabilizes and buffers the gas entering, and finally enters the working platform fixture (204) through the pipeline; S2, the gas source is decompressed by the second pressure reducing valve (209), and reaches the second proportional valve (202) after the gas path is controlled by the three-position five-way solenoid valve (201). Under the regulation of the second proportional valve (202), pressure is applied to the cylinder (203), and the battery cell is pressurized and fixed at this time; S3, perform positive pressure testing on the battery cell, place the battery cell on the lower working platform fixture (204), and control the upper part of the pressurizing fixture (205) to pressurize and seal the battery cell. When all contact surfaces are completely sealed, the gas after pressure stabilization and buffering by the gas tank (104) is used to inflate the product so that its internal pressure is higher than the external atmospheric pressure. The amount of leakage is determined by observing the pressure change, and then the leakage amount of the product is inferred.
Citation Information
Patent Citations
Real-time gas tightness detection equipment for fuel cell stack
CN108120568A
Air tightness detection method of solid oxide fuel cell
CN111829737A
Device and method for detecting air tightness of hydrogen fuel cell stack
CN116625599A
New energy battery sealing performance detection equipment and detection method thereof
CN117213763A
Airtight test equipment for alkaline electrolytic cell