Battery cell winding process, battery cell and battery

By bonding the diaphragm and the pole sheet in the battery cell winding process and winding it whole, the problems of troubles in the prior art and poor battery cell quality are solved, and the production efficiency and battery cell quality are improved.

CN118919806APending Publication Date: 2024-11-08HUNAN DUDU INTELLIGENT TECH CO LTD
View PDF 0 Cites 0 Cited by

Patent Information

Application Number
CN202410960567.7
Authority / Receiving Office
CN · China
Patent Type
Applications(China)
Current Assignee / Owner
Filing Date
2024-07-17
Publication Date
2024-11-08

AI Technical Summary

Technical Problem

The existing battery cell winding process is troublesome, time-consuming and labor-intensive, low production efficiency, and prone to relative deviation of the pole sheet and the diaphragm, resulting in poor battery cell quality.

Method used

After the diaphragm and the pole sheet are bonded, the winding layer is formed, and the overall winding is carried out to reduce the relative deviation between the pole sheet and the diaphragm, and improve operational convenience and production efficiency.

Benefits of technology

It achieves more convenient operation, time and effort, improves the quality and production efficiency of the battery cell, and reduces the relative deviation between the pole sheet and the diaphragm.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure CN118919806A_ABST
    Figure CN118919806A_ABST
Patent Text Reader

Abstract

The invention discloses a battery cell winding process, a battery cell and a battery, and relates to the technical field of battery processing, the battery cell winding process comprises the following steps: diaphragm preparation: providing a first diaphragm and a second diaphragm; winding layer manufacturing: two pole pieces are pasted on the two surfaces of the first diaphragm respectively, a second diaphragm is pasted on the surface, away from the first diaphragm, of one pole piece to form a winding layer, and the two pole pieces are the positive pole piece and the negative pole piece respectively; one end of the winding layer is fixed to a winding device, and the winding layer is wound through the winding device. According to the battery cell winding process, the battery cell and the battery, the operation is more convenient, more time and labor are saved, the production efficiency is higher, in the winding process, the relative deviation of the pole piece and the diaphragm can be reduced, and the quality of the wound battery cell is better.
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] The present invention relates to the technical field of battery processing, and in particular to a battery core winding process, a battery core and a battery. Background Art

[0002] In the prior art, the winding process of the battery cell is generally to fix the starting ends of two diaphragms on a winding device, and place a pole piece between the two diaphragms, and place another pole piece on the side of one diaphragm away from the other diaphragm, one of the pole pieces is the positive pole piece, and the other pole piece is the negative pole piece, and then wind it through the winding device.

[0003] The existing winding process requires that the starting ends of both diaphragms be fixed to the winding device and two pole pieces be placed, which is cumbersome to operate, time-consuming and labor-intensive, and has low production efficiency. In addition, during the winding process, the pole piece and the diaphragm are prone to relative displacement, resulting in poor quality of the wound battery cell. Summary of the invention

[0004] The present invention aims to solve at least one of the technical problems existing in the prior art. To this end, the present invention proposes a battery cell winding process, which is not only more convenient to operate, more time-saving and labor-saving, and has higher production efficiency, but also can reduce the relative offset between the pole piece and the diaphragm during the winding process, and the battery cell formed by winding has better quality.

[0005] The present invention also provides a battery cell made by the battery cell winding process.

[0006] The present invention also provides a battery having the battery core.

[0007] The battery cell winding process according to the first aspect of the present invention includes the following steps:

[0008] Diaphragm preparation: providing a first diaphragm and a second diaphragm;

[0009] Preparation of winding layer: two pole pieces are respectively attached to two surfaces of the first diaphragm, and the second diaphragm is attached to the surface of one of the pole pieces away from the first diaphragm to form a winding layer, wherein the two pole pieces are respectively a positive pole piece and a negative pole piece;

[0010] Winding forming: fixing one end of the winding layer to a winding device, and winding the winding layer by the winding device.

[0011] The battery cell winding process according to the embodiment of the present invention has at least the following beneficial effects:

[0012] In the embodiment of the present invention, before winding, two diaphragms and two pole pieces are bonded together to form a winding layer, and then one end of the winding layer is fixed to a winding device, and the winding layer is wound as a whole by the winding device. Compared with the prior art, which requires fixing the starting ends of both diaphragms to the winding device and placing two pole pieces, the present invention only requires winding the entire winding layer, which is more convenient to operate, more time-saving and labor-saving, and has higher production efficiency. Moreover, since the diaphragm and the pole piece have been bonded together before winding, the relative displacement of the pole piece and the diaphragm can be reduced during the winding process, and the quality of the battery cell formed by winding is better.

[0013] According to some embodiments of the present invention, the membrane preparation comprises:

[0014] Adhesive is applied to both surfaces of the membrane coil, and then the membrane coil is cut into the first membrane and the second membrane.

[0015] According to some embodiments of the present invention, the membrane preparation further comprises:

[0016] Before the pole piece is attached to the first diaphragm or before the first diaphragm is attached to the first diaphragm, the first diaphragm and the second diaphragm are dried at a temperature of 40° C. to 65° C. for a drying time of 10 minutes to 30 minutes.

[0017] According to some embodiments of the present invention, the diaphragm coil is made of a polyolefin porous membrane; and / or the adhesive is a polyarylene polyacrylic acid glue.

[0018] According to some embodiments of the present invention, the winding layer manufacturing includes:

[0019] After the winding layer is formed, the winding layer is dried at a temperature of 30° C. to 50° C. for a time of 15 minutes to 20 minutes.

[0020] According to some embodiments of the present invention, the battery core winding process further includes cutting the winding layer:

[0021] Before winding the winding layer, cutting the winding layer so that the winding layer forms a plurality of winding units arranged along the width direction of the winding layer;

[0022] Then, the winding unit is wound by the winding device to form a winding core.

[0023] According to some embodiments of the present invention, the battery core winding process further includes cutting the winding layer:

[0024] After the winding layer is wound, the wound layer is cut to form a plurality of winding cores arranged along the width direction of the winding layer.

[0025] According to some embodiments of the present invention, the battery core winding process further includes core compacting:

[0026] The core is compacted by a warm pressing plate, the temperature of the warm pressing plate is 40° C. to 50° C., and the compaction time is 15 seconds to 20 seconds.

[0027] The battery cell according to the second embodiment of the present invention is manufactured by the battery cell winding process described in the first embodiment.

[0028] The battery cell according to the embodiment of the present invention has at least the following beneficial effects:

[0029] By adopting the battery cell winding process of the first aspect of the embodiment of the present invention, not only is the operation more convenient, more time-saving and labor-saving, and the production efficiency higher, but also the relative displacement between the pole piece and the diaphragm can be reduced during the winding process, and the quality of the battery cell formed by winding is better.

[0030] A battery according to an embodiment of the third aspect of the present invention comprises the battery cell described in the embodiment of the second aspect.

[0031] The battery according to the embodiment of the present invention has at least the following beneficial effects:

[0032] By adopting the battery cell winding process of the first aspect of the embodiment of the present invention, not only is the operation more convenient, more time-saving and labor-saving, and the production efficiency higher, but also the relative displacement between the pole piece and the diaphragm can be reduced during the winding process, and the quality of the battery cell formed by winding is better.

[0033] Additional aspects and advantages of the present invention will be given in part in the following description, and some advantages will become obvious from the following description, or will be learned through practice of the present invention. BRIEF DESCRIPTION OF THE DRAWINGS

[0034] The present invention will be further described below with reference to the accompanying drawings and embodiments, wherein:

[0035] Figure 1 It is a schematic diagram of the winding process of the existing battery cell winding process;

[0036] Figure 2 It is a schematic diagram of forming a winding layer according to an embodiment of the present invention;

[0037] Figure 3 Schematic diagram of the winding process of an embodiment of the present invention.

[0038] Figure Number:

[0039] A first diaphragm 100;

[0040] A second diaphragm 200;

[0041] Positive electrode sheet 300;

[0042] Negative electrode sheet 400;

[0043] Winding layer 500;

[0044] Winding device 600. DETAILED DESCRIPTION

[0045] Embodiments of the present invention are described in detail below, examples of which are shown in the accompanying drawings, wherein the same or similar reference numerals throughout represent the same or similar elements or elements having the same or similar functions. The embodiments described below with reference to the accompanying drawings are exemplary and are only used to explain the present invention, and cannot be understood as limiting the present invention.

[0046] In the description of the present invention, it should be understood that descriptions involving orientation, such as orientation or positional relationship indicated as up, down, etc., are based on the orientation or positional relationship shown in the drawings, and are only for the convenience of describing the present invention and simplifying the description, rather than indicating or implying that the device or element referred to must have a specific orientation, be constructed and operated in a specific orientation, and therefore should not be understood as a limitation on the present invention.

[0047] In the description of the present invention, "a plurality" refers to two or more than two. If there is a description of "first" or "second", it is only used for the purpose of distinguishing technical features, and cannot be understood as indicating or implying relative importance or implicitly indicating the number of the indicated technical features or implicitly indicating the order of the indicated technical features.

[0048] In the description of the present invention, unless otherwise clearly defined, terms such as setting, installing, connecting, etc. should be understood in a broad sense, and technicians in the relevant technical field can reasonably determine the specific meanings of the above terms in the present invention based on the specific content of the technical solution.

[0049] refer to Figure 1 As shown, in the prior art, the winding process of the battery cell generally involves fixing the starting ends of two diaphragms, that is, the first diaphragm 100 and the second diaphragm 200, to a winding device 600, and placing a pole piece between the two diaphragms, and placing another pole piece on the side of one diaphragm away from the other diaphragm, wherein one pole piece is a positive pole piece 300 and the other pole piece is a negative pole piece 400, and then winding is performed through the winding device 600. Since the starting ends of the two diaphragms need to be fixed to the winding device 600 and two pole pieces need to be placed, the operation is cumbersome, time-consuming and labor-intensive, and the production efficiency is low. In addition, during the winding process, the pole piece and the diaphragm are prone to relative displacement, resulting in poor quality of the battery cell formed by winding.

[0050] Reference below Figure 2 and Figure 3 A cell winding process, a cell and a battery according to an embodiment of the present invention are described.

[0051] According to the battery cell winding process of the first embodiment of the present invention, Figure 2 and Figure 3 As shown, the following steps are included:

[0052] Diaphragm preparation: providing a first diaphragm 100 and a second diaphragm 200;

[0053] The winding layer 500 is made by pasting two pole pieces on two surfaces of the first separator 100, and pasting the second separator 200 on the surface of one pole piece away from the first separator 100, so as to form the winding layer 500, wherein the two pole pieces are the positive pole piece 300 and the negative pole piece 400;

[0054] Winding molding: one end of the winding layer 500 is fixed to the winding device 600, and the winding layer 500 is wound by the winding device 600.

[0055] In the embodiment of the present invention, before winding, two diaphragms and two pole pieces are bonded together to form a winding layer 500, and then one end of the winding layer 500 is fixed to the winding device 600, and the winding layer 500 is wound as a whole by the winding device 600. Compared with the prior art, which requires fixing the starting ends of the two diaphragms to the winding device 600 and placing two pole pieces, the present invention only requires winding the winding layer 500 as a whole, which is more convenient to operate, more time-saving and labor-saving, and has higher production efficiency. Moreover, since the diaphragm and the pole piece have been bonded together before winding, the relative displacement of the pole piece and the diaphragm can be reduced during the winding process, and the quality of the battery cell formed by winding is better.

[0056] It should be noted that in the step of making the winding layer 500, the second diaphragm 200 is pasted on the surface of one of the pole pieces away from the first diaphragm 100, and the diaphragm is not pasted on the surface of the other pole piece away from the first diaphragm 100, so as to facilitate the pasting of the other pole piece and the surface of the second diaphragm 200 away from the first diaphragm 100 during the winding process. The winding device 600 is a common device in the battery winding process, and its structure and working principle are not repeated here.

[0057] In addition, the pasting can be performed along the center of the width direction and the center of the length direction of the diaphragm, so that the bonding is more firm and the structural strength is higher, which can further reduce the relative displacement between the pole piece and the diaphragm, and the quality of the battery cell formed by winding is better. In addition, along the length direction of the diaphragm, the diaphragm is 5m to 10mm longer than the pole piece. Such a setting makes it convenient to fix the diaphragm on the winding needle of the winding device 600. In addition, after the winding layer 500 is formed, it can be pressed and compacted by a flat press so that the positive electrode sheet 300 and the negative electrode sheet 400 are firmly and firmly pasted to the diaphragm without gaps, thereby making the quality of the battery cell formed by winding better.

[0058] In some embodiments of the present invention, the membrane preparation includes: applying adhesive on both surfaces of the membrane coil, and then cutting the membrane coil into a first membrane 100 and a second membrane 200 .

[0059] Specifically, the large roll of diaphragm coil purchased from the diaphragm production factory is coated with adhesive, and the adhesive needs to be coated on both the front and back sides of the diaphragm coil, and then the entire diaphragm coil coated with adhesive is cut to form the first diaphragm 100 and the second diaphragm 200. In this embodiment, the method of coating the adhesive first and then cutting will not cause waste of adhesive, and can avoid the problem of adhesive overflow or uneven adhesive coating in the later production process.

[0060] In some embodiments of the present invention, the diaphragm preparation further includes: drying the first diaphragm 100 and the second diaphragm 200 before pasting the pole piece to the first diaphragm 100 or the first diaphragm 100, the drying temperature is 40°C to 65°C, and the drying time is 10 minutes to 30 minutes. For example, the drying temperature can be 40°C, 45°C, 50°C, 55°C, 60°C, 65°C or other suitable temperatures, and the drying time can be 10 minutes, 15 minutes, 20 minutes, 25 minutes, 30 minutes or other suitable times.

[0061] In this embodiment, the drying temperature is 40°C to 65°C, and the drying time is 10 minutes to 30 minutes. In this way, the drying of the adhesive of the first diaphragm 100 and the second diaphragm 200 is semi-drying, which can avoid the adhesive having too much moisture, resulting in a loose adhesion between the electrode and the first diaphragm 100 or the first diaphragm 100, and can also avoid the adhesive being too dry, resulting in the loss of adhesion. It is ensured that the adhesive of the first diaphragm 100 and the second diaphragm 200 after drying still has a certain humidity and adhesion, so that the bonding effect between the electrode and the first diaphragm 100 or the first diaphragm 100 is better.

[0062] In some embodiments of the present invention, the separator coil is made of a polyolefin porous membrane, which can effectively separate the positive electrode sheet 300 and the negative electrode sheet 400 to prevent the two electrodes from contacting and short-circuiting, and also allow the electrolyte ions to pass smoothly, thereby improving the quality of the battery cell. It should be noted that the separator coil can also be made of other suitable materials, which will not be described in detail here.

[0063] In some embodiments of the present invention, the adhesive is polyacrylic acid glue, which is the Chinese name of Polyacrylic acid, and is abbreviated as PAA in English. Polyacrylic acid glue has the characteristics of excellent acid and alkali resistance, excellent water resistance, and good viscosity, and is a more preferred material for preparing the adhesive. It should be noted that the adhesive can also be prepared from other suitable materials, which will not be repeated here.

[0064] In some embodiments of the present invention, the winding layer 500 is made including: after forming the winding layer 500, the winding layer 500 is dried, the drying temperature is 30°C to 50°C, and the drying time is 15 minutes to 20 minutes. For example, the bonding area between the pole piece and the first diaphragm 100 or the second diaphragm 200 can be dried, the drying temperature can be 30°C, 35°C, 40°C, 45°C, 50°C or other suitable temperatures, and the drying time can be 15 minutes, 16 minutes, 17 minutes, 18 minutes, 19 minutes, 20 minutes or other suitable times.

[0065] In this embodiment, a second drying is performed to enable the electrode and the first diaphragm 100 or the second diaphragm 200 to be quickly bonded together. The drying temperature is 30°C to 50°C, and the drying time is 15 minutes to 20 minutes. In this way, after the adhesive of the first diaphragm 100 and the second diaphragm 200 is dried for the first time, the second drying is still semi-drying, which can prevent the adhesive from being too dry and causing the adhesiveness to disappear. It is ensured that the adhesive on the first diaphragm 100 and the second diaphragm 200 after drying still has a certain humidity and adhesion. No other adhesive materials are required, so that the electrode and the first diaphragm 100 and the second diaphragm 200 can be more closely fitted during the winding process, and are not easily deformed after fitting. In addition, the first diaphragm 100 and the second diaphragm 200 can have a certain flexibility and tension to avoid the first diaphragm 100 and the second diaphragm 200 from breaking, thereby improving product quality and bringing market competitiveness to the product.

[0066] In some embodiments of the present invention, the battery cell winding process also includes cutting the winding layer 500: before winding the winding layer 500, the winding layer 500 is cut to form a plurality of winding units arranged along the width direction of the winding layer 500, so that the winding is more convenient, and then the winding unit is wound by the winding device 600 to form a core.

[0067] It should be noted that, in some other embodiments of the present invention, after the winding layer 500 is wound, the rolled winding layer 500 may be cut to form a plurality of winding cores arranged along the width direction of the winding layer 500 .

[0068] It is understandable that when the winding layer 500 is cut, it is necessary to ensure that each cut separator has a positive electrode sheet 300 and a negative electrode sheet 400, and the error of the width and length of each cut separator is within 2 mm.

[0069] In some embodiments of the present invention, the battery cell winding process also includes core compaction: the core is compacted by a warm pressing plate, the temperature of the warm pressing plate is 40°C to 50°C, and the compaction time is 15 seconds to 20 seconds. For example, the warm pressing plate can be connected to a driving mechanism such as a cylinder or an oil cylinder. After the core is wound, the core can be placed between two warm pressing plates with a certain temperature, and then the driving mechanism such as the cylinder or the oil cylinder can be started to control the two warm pressing plates to approach each other. The two voltage stabilizing plates can press and compact the core, so that the electrode and the first diaphragm 100 and the second diaphragm 200 fit more tightly. The temperature of the warm pressing plate is 40°C to 50°C, for example, it can be 40°C, 45°C, 50°C or other suitable temperatures. In this way, the adhesive can be further dried to make the bonding effect between the electrode and the first diaphragm 100 and the second diaphragm 200 better. The compaction time is 15 seconds to 20 seconds, for example, it can be 15 seconds, 16 seconds, 17 seconds, 18 seconds, 19 seconds or 20 seconds, etc., so that the drying and compaction effects can be guaranteed.

[0070] The battery cell according to the second embodiment of the present invention is manufactured by the battery cell winding process of the first embodiment described above.

[0071] By adopting the battery cell winding process of the first aspect of the embodiment of the present invention, not only is the operation more convenient, more time-saving and labor-saving, and the production efficiency higher, but also the relative displacement between the pole piece and the diaphragm can be reduced during the winding process, and the quality of the battery cell formed by winding is better.

[0072] It should be noted that since the battery cell can be manufactured using all the technical solutions of the battery cell winding process of the first embodiment above, it at least has all the beneficial effects brought by the technical solutions of the first embodiment above, and these additional beneficial effects will not be repeated here.

[0073] It is understandable that other structures and operations of the battery cell according to the embodiment of the present invention are known to those skilled in the art and will not be described in detail here.

[0074] A battery according to an embodiment of the third aspect of the present invention comprises a battery cell according to an embodiment of the second aspect.

[0075] By adopting the battery cell of the second embodiment of the present invention, and the battery cell is made by the battery cell winding process of the first embodiment, not only is the operation more convenient, more time-saving and labor-saving, and the production efficiency higher, but also during the winding process, the relative displacement of the pole piece and the diaphragm can be reduced, and the quality of the battery cell formed by winding is better.

[0076] It should be noted that since the battery cell can be manufactured using all the technical solutions of the battery cell winding process of the first embodiment above, it at least has all the beneficial effects brought by the technical solutions of the first embodiment above, and these additional beneficial effects will not be repeated here.

[0077] It is to be understood that other structures and operations of the battery according to the embodiment of the present invention are known to those skilled in the art and will not be described in detail here.

[0078] The embodiments of the present invention are described in detail above with reference to the accompanying drawings, but the present invention is not limited to the above embodiments, and various changes can be made within the knowledge scope of ordinary technicians in the relevant technical field without departing from the purpose of the present invention.

Claims

1. A battery cell winding process, It is characterized in that The steps include: Diaphragm preparation: providing a first diaphragm and a second diaphragm; Preparation of winding layer: two pole pieces are respectively attached to two surfaces of the first diaphragm, and the second diaphragm is attached to the surface of one of the pole pieces away from the first diaphragm to form a winding layer, wherein the two pole pieces are respectively a positive pole piece and a negative pole piece; Winding forming: fixing one end of the winding layer to a winding device, and winding the winding layer by the winding device.

2. The battery cell winding process according to claim 1, It is characterized in that The diaphragm preparation includes: Adhesive is applied to both surfaces of the membrane coil, and then the membrane coil is cut into the first membrane and the second membrane.

3. The battery cell winding process according to claim 2, It is characterized in that The diaphragm preparation further comprises: Before the pole piece is attached to the first diaphragm or before the first diaphragm is attached to the first diaphragm, the first diaphragm and the second diaphragm are dried at a temperature of 40° C. to 65° C. for a drying time of 10 minutes to 30 minutes.

4. The battery cell winding process according to claim 2, It is characterized in that The separator coil is a polyolefin porous membrane; and / or, The bonding glue is polyacrylic acid glue.

5. The battery cell winding process according to claim 1, It is characterized in that The winding layer production includes: After the winding layer is formed, the winding layer is dried at a temperature of 30° C. to 50° C. for a time of 15 minutes to 20 minutes.

6. The battery cell winding process according to claim 1, It is characterized in that Also includes winding layer cutting: Before winding the winding layer, cutting the winding layer so that the winding layer forms a plurality of winding units arranged along the width direction of the winding layer; Then, the winding unit is wound by the winding device to form a winding core.

7. The battery cell winding process according to claim 1, It is characterized in that Also includes winding layer cutting: After the winding layer is wound, the wound layer is cut to form a plurality of winding cores arranged along the width direction of the winding layer.

8. The battery core winding process according to claim 6 or 7, It is characterized in that Also includes core compaction: The core is compacted by a warm pressing plate, the temperature of the warm pressing plate is 40° C. to 50° C., and the compaction time is 15 seconds to 20 seconds.

9. A battery cell, It is characterized in that The battery is manufactured by the battery core winding process according to any one of claims 1 to 8.

10. A battery, It is characterized in that Comprising the battery cell as claimed in claim 9.