Pressing process for front and back lamination reinforcement of FPC (Flexible Printed Circuit) and application

Through integrated chemical equipment and vacuum air bag compression technology, the problem of deep indentation of FPC and reinforcement positions is solved, the damage and deformation of FPC is reduced, the product quality and pass rate are improved, and it is suitable for mass production.

CN118921836APending Publication Date: 2024-11-08SHENZHEN XINYU TENGYUE ELECTRONICS
View PDF 0 Cites 0 Cited by

Patent Information

Application Number
CN202410972678.X
Authority / Receiving Office
CN · China
Patent Type
Applications(China)
Current Assignee / Owner
Filing Date
2024-07-19
Publication Date
2024-11-08

AI Technical Summary

Technical Problem

In the prior art, the indentation of FPC and reinforcement positions is deep, resulting in pressure damage and disconnection of the product, affecting product quality.

Method used

Using integrated workpiece, the FPC reinforcement workpiece is connected through adhesive tape, PIN nail positioning and release membrane are set, and the vacuum air bag is used for compression processing, the pressing temperature and pressure are controlled, and the reinforcement height of the bonding position is reduced and the reinforcement height is reduced. Compression indentation.

Benefits of technology

It effectively reduces FPC damage, avoids severe deformation and laminate damage, improves product qualification rate, and is suitable for mass production.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure CN118921836A_ABST
    Figure CN118921836A_ABST
Patent Text Reader

Abstract

The invention relates to the technical field of processing of flexible circuit boards, in particular to a laminating process for front and back lamination reinforcement of an FPC (Flexible Printed Circuit) and application. The invention provides a pressing process for FPC front and back lamination reinforcement, and the process comprises the steps: carrying out the connection processing of two FPC reinforcement tools, and obtaining an integrated tool, and the material thickness of the integrated tool is smaller than the reinforcement thickness; placing the FPC of which the two sides are provided with reinforcements on one side of the integrated tool through the positioning of the PINs, pressing the other side of the integrated tool to the bonded and reinforced FPC, and assembling to obtain a to-be-pressed assembly; and pressing the to-be-pressed assembly to obtain a product containing FPC front and back lamination reinforcement. According to the pressing process, it is guaranteed that in the pressing treatment process of the product, the joint of the product and the attaching reinforcing position has a proper space, pressing indentations are reduced, and the problem of FPC damage is solved.
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] The present application belongs to the field of flexible circuit board processing technology, and in particular, relates to a lamination process and application of FPC front and back lamination reinforcement. Background Art

[0002] Flexible Printed Circuit (FPC), also known as soft circuit board, flexible circuit board, is favored for its excellent characteristics such as light weight, thin thickness, free bending and folding, and its application range is also very wide. In the application process of different fields and different products, FPC has different product structures based on different needs.

[0003] Among them, in the commonly used products, the front and back of each product need to be attached to a 1.2mm thick steel sheet. The conventional pressing method can be found through the slicing method, such as Figure 1 As shown, the deformation at the junction of the FPC and the reinforcement is relatively large. At the same time, the FPC is damaged at the stress-bearing position of the reinforcement, affecting the use of the product.

[0004] Therefore, there is an urgent need to solve the problem of FPC damage by using a pressing tool with a tool that can bear part of the reinforcement thickness to improve product quality. Summary of the invention

[0005] The purpose of the present application is to provide a lamination process and application for the front and back lamination reinforcement of FPC, aiming to solve the problem in the prior art that ordinary lamination tooling is prone to deep indentations at the positions of FPC and reinforcement during the product preparation process, resulting in pressure damage and wire breakage of the product.

[0006] In order to achieve the above application purpose, the technical solution adopted in this application is as follows:

[0007] In a first aspect, the present application provides a lamination process for reinforcing the front and back of an FPC, comprising the following steps:

[0008] Connecting two FPC reinforcement fixtures to obtain an integrated fixture, wherein the material thickness of the integrated fixture is thinner than the thickness of the reinforcement;

[0009] The FPC with double-sided reinforcement is placed on one side of the integrated tooling by positioning with PIN pins, and then the other side of the integrated tooling is pressed against the laminated and reinforced FPC to assemble the component to be pressed;

[0010] The components to be pressed are pressed to obtain a product with FPC front and back lamination reinforcement.

[0011] Furthermore, a surface of the FPC reinforcement tooling is provided with an empty groove corresponding to the position where the FPC surface patch is to be reinforced.

[0012] Furthermore, the material thickness of the integrated tooling is 0.2 to 0.3 mm thinner than the thickness of the reinforcement.

[0013] Furthermore, the step of connecting two FPC reinforcement fixtures to obtain an integrated fixture includes: providing an adhesive tape, and using the adhesive tape to connect the two FPC reinforcement fixtures to obtain an integrated fixture.

[0014] Furthermore, the adhesive tape is selected from a material that can withstand high temperatures above 200°C.

[0015] Further, the step of assembling the component to be pressed includes:

[0016] A first release film is provided on one side of the FPC with double-sided reinforcement,

[0017] A second release film is arranged on the other side of the FPC with reinforcement on both sides to obtain a component to be pressed.

[0018] Furthermore, the thickness of the first release film and the second release film is 0.025-0.05 mm.

[0019] Furthermore, the step of pressing the component to be pressed comprises:

[0020] Red silica gel is arranged on one side of the component to be pressed.

[0021] The component to be pressed is placed on a press base, wherein the red silica gel is placed above the press base;

[0022] A vacuum air bag is placed on the other side of the component to be pressed;

[0023] The pressing process is carried out by means of a vacuum air bag.

[0024] Furthermore, the temperature of the pressing treatment is 180-190° C., the time is 150-300 seconds, and the pressure is 20-22 kgf / cm.

[0025] In a second aspect, an embodiment of the present application provides an FPC product with front and back lamination reinforcement, and the FPC product with front and back lamination reinforcement is prepared by the above-mentioned FPC front and back lamination reinforcement lamination process.

[0026] The first aspect of the present application provides a lamination process for front and back lamination reinforcement of FPC. The lamination process mainly provides an integrated tooling and controls the material of the integrated tooling to be thinner than the thickness of the reinforcement, thereby greatly reducing the reinforcement height of the lamination position and ensuring that there is a suitable space at the junction of the product and the lamination reinforcement position during the lamination process of the product, thereby reducing the lamination indentation and improving the problem of FPC damage.

[0027] The second aspect of the present application provides an FPC product with front and back lamination and reinforcement. The provided FPC product with front and back lamination and reinforcement is prepared by the above-mentioned FPC front and back lamination and reinforcement pressing process. The preparation process can greatly improve the problem of FPC damage. The obtained FPC product with front and back lamination and reinforcement does not have serious deformation, the laminated layers of the pressed FPC are not damaged, the product qualification rate is improved, and it is conducive to mass production. BRIEF DESCRIPTION OF THE DRAWINGS

[0028] In order to more clearly illustrate the technical solutions in the embodiments of the present application, the drawings required for use in the embodiments or the description of the prior art will be briefly introduced below. Obviously, the drawings described below are only some embodiments of the present application. For ordinary technicians in this field, other drawings can be obtained based on these drawings without paying any creative work.

[0029] Figure 1 It is a schematic diagram of cutting a product prepared by a conventional pressing method in the prior art of this application.

[0030] Figure 2 It is an analysis diagram of the lamination process for front and back lamination reinforcement of FPC provided in the embodiment of the present application.

[0031] Figure 3 This is a physical picture of the lamination process for front and back bonding and reinforcement of FPC provided in the embodiment of the present application.

[0032] Figure 4 This is a physical picture of the lamination process for front and back bonding and reinforcement of FPC provided in the embodiment of the present application. DETAILED DESCRIPTION

[0033] In order to make the technical problems, technical solutions and beneficial effects to be solved by the present application more clearly understood, the present application is further described in detail below in conjunction with the embodiments. It should be understood that the specific embodiments described herein are only used to explain the present application and are not used to limit the present application.

[0034] In this application, the term "and / or" describes the association relationship of associated objects, indicating that there may be three relationships. For example, A and / or B can mean: A exists alone, A and B exist at the same time, and B exists alone. A and B can be singular or plural. The character " / " generally indicates that the associated objects are in an "or" relationship.

[0035] In this application, "at least one" means one or more, and "plurality" means two or more. "At least one of the following" or similar expressions refers to any combination of these items, including any combination of single items or plural items. For example, "at least one of a, b, or c", or "at least one of a, b, and c" can all mean: a, b, c, ab (i.e., a and b), ac, bc, or abc, where a, b, c can be single or multiple, respectively.

[0036] It should be understood that in the various embodiments of the present application, the size of the serial numbers of the above-mentioned processes does not mean the order of execution, some or all of the steps can be executed in parallel or sequentially, and the execution order of each process should be determined by its function and internal logic, and should not constitute any limitation on the implementation process of the embodiments of the present application.

[0037] The terms used in the embodiments of the present application are only for the purpose of describing specific embodiments, and are not intended to limit the present application. The singular forms "a", "an" and "the" used in the embodiments of the present application and the appended claims are also intended to include plural forms, unless the context clearly indicates other meanings.

[0038] The weight of the relevant components mentioned in the embodiment description of the present application can not only refer to the specific content of each component, but also represent the proportional relationship between the weights of the components. Therefore, as long as the content of the relevant components is proportionally enlarged or reduced according to the embodiment description of the present application, it is within the scope disclosed in the embodiment description of the present application. Specifically, the mass described in the embodiment description of the present application can be a mass unit known in the chemical industry such as μg, mg, g, kg, etc.

[0039] The terms "first" and "second" are used only for descriptive purposes to distinguish objects such as substances from each other, and should not be understood as indicating or implying relative importance or implicitly indicating the number of indicated technical features. For example, without departing from the scope of the embodiments of the present application, the first XX may also be referred to as the second XX, and similarly, the second XX may also be referred to as the first XX. Thus, features defined as "first" and "second" may explicitly or implicitly include one or more of the features.

[0040] The first aspect of the embodiment of the present application provides a lamination process for reinforcing the front and back of an FPC, comprising the following steps:

[0041] S01. The two FPC reinforcement fixtures are connected to obtain an integrated fixture, wherein the material thickness of the integrated fixture is thinner than the thickness of the reinforcement;

[0042] S02. The double-sided reinforced FPC is placed on one side of the integrated tooling by positioning the PIN pins, and then the other side of the integrated tooling is pressed against the laminated reinforced FPC to assemble the assembly to be pressed;

[0043] S03. The components to be pressed are pressed to obtain a product with FPC front and back lamination reinforcement.

[0044] The first aspect of the embodiment of the present application provides a lamination process for front and back lamination reinforcement of FPC. The lamination process mainly provides an integrated tooling and controls the material of the integrated tooling to be thinner than the thickness of the reinforcement, thereby greatly reducing the reinforcement height of the lamination position, ensuring that during the lamination process of the product, there is a suitable space at the junction of the product and the lamination reinforcement position, reducing the lamination indentation and improving the problem of FPC damage.

[0045] In step S01, Figure 2 As shown, two FPC reinforcement fixtures are connected to obtain an integrated fixture, wherein the material thickness of the integrated fixture is thinner than the thickness of the reinforcement.

[0046] In some embodiments, a surface of the FPC reinforcement tooling is provided with an empty groove corresponding to the position where the FPC surface is to be reinforced.

[0047] In some embodiments, the material thickness of the integrated tooling is 0.2-0.3 mm thinner than the thickness of the reinforcement. In some specific embodiments, the material thickness of the FPC reinforcement tooling is 1.0 mm.

[0048] In some embodiments, the step of connecting two FPC reinforcement fixtures to obtain an integrated fixture includes: providing an adhesive tape, and using the adhesive tape to connect the two FPC reinforcement fixtures to obtain an integrated fixture.

[0049] In some embodiments, the adhesive tape is selected from a material that can withstand high temperatures above 200°C.

[0050] In some specific embodiments, the adhesive tape has a width of 20 mm and a thickness of 0.02-0.04 mm.

[0051] In step S02, Figure 3-4 As shown, the FPC with double-sided reinforcement is placed on one side of the integrated tooling through the positioning of PIN nails, and then the other side of the integrated tooling is pressed against the bonded and reinforced FPC to assemble the component to be pressed.

[0052] In some embodiments, the step of assembling the component to be pressed includes:

[0053] S021. A first release film is provided on one side of the double-sided reinforced FPC,

[0054] S022. Arrange a second release film on the other side of the FPC with double-sided reinforcement to obtain an assembly to be pressed.

[0055] In some embodiments, the thickness of the first release film and the second release film is 0.025-0.05 mm.

[0056] In some embodiments, the first release film and the second release film use PET modified film as raw materials. The provided PET modified film is mainly processed by using high temperature resistant additives on PET film to ensure that the obtained material has good high temperature resistance.

[0057] In step S03, the components to be pressed are pressed to obtain a product with front and back FPC laminated and reinforced.

[0058] In some embodiments, the step of pressing the component to be pressed includes:

[0059] S031. Red silica gel is provided on one side of the component to be pressed,

[0060] S032. The component to be pressed is placed on the press base, wherein the red silica gel is placed above the press base;

[0061] S033. Place a vacuum air bag on the other side of the assembly to be pressed;

[0062] S034. Perform pressing process through vacuum air bag.

[0063] In some embodiments, the pressing process is performed at a temperature of 180 to 190° C., for a time of 150 to 300 seconds, and at a pressure of 20 to 22 kgf / cm.

[0064] A second aspect of an embodiment of the present application provides an FPC product with front and back lamination reinforcement, wherein the FPC product with front and back lamination reinforcement is prepared by the above-mentioned FPC front and back lamination reinforcement lamination process.

[0065] The second aspect of the embodiment of the present application provides an FPC product with front and back lamination and reinforcement. The provided FPC product with front and back lamination and reinforcement is prepared by the above-mentioned FPC front and back lamination and reinforcement pressing process. The preparation process can greatly improve the problem of FPC damage. The obtained FPC product with front and back lamination and reinforcement does not have serious deformation, the laminated layers of the pressed FPC are not damaged, the product qualification rate is improved, and it is conducive to mass production.

[0066] The following describes the invention in conjunction with specific embodiments.

[0067] Example 1

[0068] A lamination process for reinforcing the front and back of FPC

[0069] The steps include:

[0070] The two FPC reinforcement fixtures are connected by adhesive tape to obtain an integrated fixture, wherein the material thickness of the integrated fixture is 0.2 mm thinner than the thickness of the reinforcement, and the material thickness of the FPC reinforcement fixture is 1.0 mm; the surface of the FPC reinforcement fixture is provided with an empty groove corresponding to the position of the FPC surface reinforcement; and the adhesive tape is selected from a material resistant to high temperatures above 200°C, and the size of the adhesive tape is 20 mm in width and 0.02 mm in thickness;

[0071] The FPC with double-sided reinforcement is placed on one side of the integrated tooling by positioning with PIN pins, and then the other side of the integrated tooling is pressed toward the laminated and reinforced FPC, a first release film is set on one side of the FPC with double-sided reinforcement, and a second release film is set on the other side of the FPC with double-sided reinforcement, and the assembly to be pressed is assembled; wherein the thickness of the first release film and the second release film is 0.025 mm;

[0072] Red silica gel is arranged on one side of the component to be pressed, and the component to be pressed is placed on a press base, wherein the red silica gel is placed above the press base; a vacuum air bag is placed on the other side of the component to be pressed; and a pressing process is performed by the vacuum air bag; wherein the pressing process is performed at a temperature of 180°C, a time of 150 seconds, and a pressure of 20kgf / cm;

[0073] The obtained product contains FPC front and back lamination reinforcement.

[0074] Product analysis: Through cross-sectional analysis, the junction between the FPC and the reinforcement will not be deformed, and the laminated FPC will not be damaged.

[0075] Example 2

[0076] A lamination process for reinforcing the front and back of FPC

[0077] The steps include:

[0078] The two FPC reinforcement fixtures are connected by adhesive tape to obtain an integrated fixture, wherein the material thickness of the integrated fixture is 0.25 mm thinner than the thickness of the reinforcement, and the material thickness of the FPC reinforcement fixture is 1.0 mm; the surface of the FPC reinforcement fixture is provided with an empty groove corresponding to the position of the FPC surface reinforcement; and the adhesive tape is selected from a material resistant to high temperatures above 200°C, and the size of the adhesive tape is 20 mm in width and 0.03 mm in thickness;

[0079] The FPC with double-sided reinforcement is placed on one side of the integrated tooling through the positioning of PIN pins, and then the other side of the integrated tooling is pressed toward the laminated and reinforced FPC, a first release film is set on one side of the FPC with double-sided reinforcement, and a second release film is set on the other side of the FPC with double-sided reinforcement, and the assembly to be pressed is assembled; wherein the thickness of the first release film and the second release film is 0.03 mm;

[0080] Red silica gel is arranged on one side of the component to be pressed, and the component to be pressed is placed on a press base, wherein the red silica gel is placed above the press base; a vacuum air bag is placed on the other side of the component to be pressed; and a pressing process is performed by the vacuum air bag; wherein the pressing process is performed at a temperature of 185°C, a time of 200 seconds, and a pressure of 21kgf / cm;

[0081] The obtained product contains FPC front and back lamination reinforcement.

[0082] Product analysis: Through cross-sectional analysis, the junction between the FPC and the reinforcement will not be deformed, and the laminated FPC will not be damaged.

[0083] Example 3

[0084] A lamination process for reinforcing the front and back of FPC

[0085] The steps include:

[0086] The two FPC reinforcement fixtures are connected by adhesive tape to obtain an integrated fixture, wherein the material thickness of the integrated fixture is 0.3 mm thinner than the thickness of the reinforcement, and the material thickness of the FPC reinforcement fixture is 1.0 mm; the surface of the FPC reinforcement fixture is provided with an empty groove corresponding to the position of the FPC surface reinforcement; and the adhesive tape is selected from a material resistant to high temperatures above 200°C, and the size of the adhesive tape is 20 mm in width and 0.04 mm in thickness;

[0087] The FPC with double-sided reinforcement is placed on one side of the integrated tooling through the positioning of PIN pins, and then the other side of the integrated tooling is pressed against the laminated and reinforced FPC, a first release film is set on one side of the FPC with double-sided reinforcement, and a second release film is set on the other side of the FPC with double-sided reinforcement, and the assembly to be pressed is assembled; wherein the thickness of the first release film and the second release film is 0.05 mm;

[0088] Red silica gel is arranged on one side of the component to be pressed, and the component to be pressed is placed on a press base, wherein the red silica gel is placed above the press base; a vacuum air bag is placed on the other side of the component to be pressed; and a pressing process is performed by the vacuum air bag; wherein the pressing process is performed at a temperature of 190°C, a time of 300 seconds, and a pressure of 22kgf / cm;

[0089] The obtained product contains FPC front and back lamination reinforcement.

[0090] Product analysis: Through cross-sectional analysis, the junction between the FPC and the reinforcement will not be deformed, and the laminated FPC will not be damaged.

[0091] In summary, the present application provides a lamination process for FPC front and back bonding reinforcement. The lamination process mainly provides an integrated tooling and controls the material of the integrated tooling to be thinner than the thickness of the reinforcement, thereby greatly reducing the reinforcement height of the lamination position and ensuring that there is a suitable space at the junction of the product and the bonding reinforcement position during the lamination process of the product, thereby reducing the lamination indentation and improving the problem of FPC damage.

[0092] The above description is only a preferred embodiment of the present application and is not intended to limit the present application. Any modifications, equivalent substitutions and improvements made within the spirit and principles of the present application should be included in the protection scope of the present application.

Claims

1. A lamination process for reinforcing the front and back of FPC, characterized in that: The steps include: Connecting two FPC reinforcement fixtures to obtain an integrated fixture, wherein the material thickness of the integrated fixture is thinner than the thickness of the reinforcement; The FPC with double-sided reinforcement is placed on one side of the integrated tooling by positioning with PIN pins, and then the other side of the integrated tooling is pressed against the laminated and reinforced FPC to assemble the component to be pressed; The components to be pressed are pressed to obtain a product with FPC front and back lamination reinforcement.

2. The lamination process for reinforcing the front and back of FPC according to claim 1, characterized in that: The surface of the FPC reinforcement tooling is provided with an empty groove corresponding to the position where the FPC surface is reinforced.

3. The lamination process for reinforcing the front and back of FPC according to claim 1, characterized in that: The material thickness of the integrated tooling is 0.2 to 0.3 mm thinner than the thickness of the reinforcement.

4. The lamination process for reinforcing the front and back of FPC according to claim 1, characterized in that: The step of connecting two FPC reinforcement fixtures to obtain an integrated fixture includes: providing an adhesive tape, and using the adhesive tape to connect the two FPC reinforcement fixtures to obtain an integrated fixture.

5. The lamination process for reinforcing the front and back of FPC according to claim 4, characterized in that: The adhesive tape is selected from materials that can withstand high temperatures above 200°C.

6. The lamination process for reinforcing the front and back of FPC according to claim 1, characterized in that: The steps of assembling the component to be pressed include: A first release film is provided on one side of the FPC with double-sided reinforcement, A second release film is arranged on the other side of the FPC with reinforcement on both sides to obtain a component to be pressed.

7. The lamination process for reinforcing the front and back of FPC according to claim 6, characterized in that: The thickness of the first release film and the second release film is 0.025-0.05 mm.

8. The lamination process for reinforcing the front and back of FPC according to claim 1, characterized in that: The step of pressing the component to be pressed comprises: Red silica gel is arranged on one side of the component to be pressed. The component to be pressed is placed on a press base, wherein the red silica gel is placed above the press base; A vacuum air bag is placed on the other side of the component to be pressed; The pressing process is carried out by means of a vacuum air bag.

9. The lamination process for reinforcing the front and back of FPC according to claim 1, characterized in that: The pressing treatment is performed at a temperature of 180 to 190° C., for a time of 150 to 300 seconds, and at a pressure of 20 to 22 kgf / cm.

10. A front and back laminated reinforced FPC product, characterized in that: The front and back lamination reinforced FPC product is prepared by the front and back lamination reinforced FPC lamination process described in any one of claims 1 to 9.