Process and system for treating tail gas in film coating process in production of photovoltaic cells

By using silane combustion towers and N2O-NH3 high-efficiency reactors in the production of coating process of photovoltaic cell cells, combined with metal M-loaded silica particle catalyst, the treatment problems of SiH4, N2O and NH3 in the exhaust gas were successfully solved, and pollutants were realized Effective removal and greenhouse gas emission reduction avoid secondary pollution.

CN118925494APending Publication Date: 2024-11-12苏州仕净环保科技有限公司
View PDF 0 Cites 1 Cited by

Patent Information

Application Number
CN202411208137.6
Authority / Receiving Office
CN · China
Patent Type
Applications(China)
Current Assignee / Owner
Filing Date
2024-08-30
Publication Date
2024-11-12

AI Technical Summary

Technical Problem

Existing photovoltaic cell production coating process exhaust gas treatment technology cannot effectively treat SiH4, N2O and NH3 gases, resulting in the greenhouse gas N2O not being treated, causing environmental pollution and health hazards.

Method used

Using a process and system, including a silane combustion tower, dust collector and N2O-NH3 high-efficiency reactor, the metal M-loaded silica particle catalyst catalyzed the reaction of N2O and NH3 at low temperature to generate N2 and H2O, and realize SiH4 and N2O in the exhaust gas Simultaneous processing with NH3.

Benefits of technology

The stable emission of pollutants is achieved, the emission of greenhouse gas N2O is reduced, and the secondary pollution is avoided. The catalyst cost is low, the catalytic temperature is low, and the reaction efficiency is high.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure CN118925494A_ABST
    Figure CN118925494A_ABST
Patent Text Reader

Abstract

The invention discloses a photovoltaic cell production coating process tail gas treatment process and system, and the process comprises the following steps: S1, introducing coating process tail gas generated in the photovoltaic cell production process into a silane combustion tower, and mixing and combusting the coating process tail gas with introduced air and nitrogen; s2, tail gas discharged by combustion of silane passes through a dust remover and then enters an N2O-NH3 efficient reactor, N2O and NH3 in the tail gas react at the first temperature under the action of a catalyst to generate N2 and H2O, and the tail gas generated by the efficient reactor is finally discharged through an exhaust funnel; the catalyst is metal M-loaded silicon dioxide particles, and the metal M is any one of nickel, copper and iron. The efficient treatment process provided by the invention not only realizes stable up-to-standard emission of SiH4, NH3 and N2O, but also does not generate secondary pollution (such as secondary pollution caused by ammonia-containing wastewater generated after ammonia gas is sprayed and washed in a traditional treatment process), and simultaneously realizes emission reduction of greenhouse gas N2O in the tail gas.
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] The present invention relates to the technical field of waste gas treatment, and in particular to a process and system for treating tail gas in a photovoltaic cell production coating process. Background Art

[0002] The TOPcon process is the mainstream technology for the production of photovoltaic cells. In the TOPcon process, the SiNx coating process is used to prepare an anti-reflection layer with excellent passivation effect on the surface of the cell, so as to reduce the reflectivity of the incident light on the front surface of the cell and reduce the carrier recombination rate on the front surface of the cell, thereby increasing the open circuit voltage and short circuit current of the cell, and further increasing the photoelectric conversion efficiency of the cell. The entire coating process is carried out in the PECVD equipment, and SiH4, N2O, and NH3 gases are introduced. The three gases react in a plasma state and deposit on the surface of the silicon wafer to form Si3N4 and Si2N2O3 films with high hardness, high dielectric strength, and good moisture resistance, which can play a protective role on the surface of the cell. The residual SiH4, N2O, and NH3 gases in the SiNx coating process are discharged in the form of coating tail gas.

[0003] Silane waste gas in the coating tail gas is toxic, flammable and explosive. N2O is a very strong greenhouse gas, 310 times stronger than CO2 in terms of greenhouse effect, and has a very significant impact on the ozone layer. Ammonia is a colorless, irritating and smelly gas. When it is discharged into the air, it will not only pollute the environment, but also harm human health. Therefore, the tail gas from the photovoltaic cell production coating process must be treated before it can be discharged.

[0004] At present, the treatment measures for the tail gas of the photovoltaic cell production coating process are mainly concentrated on silane combustion and ammonia spray absorption, and there is no treatment measure for N2O. The discharged tail gas of the photovoltaic cell production coating process also contains a large amount of greenhouse gas N2O. The present invention develops a photovoltaic cell production coating process tail gas treatment solution to achieve simultaneous treatment of the three gases SiH4, N2O and NH3 in the coating tail gas to meet the exhaust gas discharge index requirements. Summary of the invention

[0005] The technical problem to be solved by the present invention is to provide a process and system for treating tail gas in the coating process of photovoltaic cell production in view of the deficiencies in the above-mentioned prior art.

[0006] In order to solve the above technical problems, the technical solution adopted by the present invention is as follows: In a first aspect of the present invention, a process for treating tail gas in a photovoltaic cell production coating process is provided, comprising the following steps:

[0007] S1. The coating process tail gas generated in the production process of photovoltaic cells is introduced into a silane combustion tower, mixed with the introduced air and nitrogen, and burned;

[0008] The tail gas discharged from the combustion of S2 and silane enters the N2O-NH3 high-efficiency reactor after passing through the dust collector. The N2O and NH3 in the tail gas react to generate N2 and H2O under the action of the catalyst at the first temperature. The tail gas generated by the high-efficiency reactor is finally discharged through the exhaust pipe;

[0009] Wherein, the catalyst is metal M loaded silica particles, and the metal M is any one of nickel, copper and iron.

[0010] Preferably, the catalyst is prepared by the following method:

[0011] 1) Preparation of activated silicon dioxide:

[0012] Take 20-30 mesh silicon dioxide and soak it in hydrochloric acid solution, stir it at 70-90°C for 6-24h, filter it, wash it with deionized water until it is neutral, dry it at 90-120°C for 4-16h, and cool it to room temperature to obtain activated silicon dioxide;

[0013] 2) Preparation of metal M-loaded silica particles:

[0014] The nitrate of metal M is dissolved in an ethanol aqueous solution, and then activated silica is added, the mass ratio of the nitrate of metal M to the activated silica is 2:1-5:1, the mixture is stirred at room temperature for 1.5-6 hours, and then heated to 90-110° C. and stirred for 2-8 hours, cooled to room temperature, filtered and collected precipitates, evaporated under reduced pressure, washed with deionized water until neutral, vacuum dried at 70-90° C. for 5-20 hours, and then calcined at 300-500° C. in a nitrogen atmosphere for 2-8 hours, and finally cooled to room temperature and ground to 20-30 meshes to obtain metal M-loaded silica particles, i.e., the catalyst.

[0015] Preferably, the catalyst is nickel-supported silica particles, which are prepared by the following method:

[0016] 1) Preparation of activated silicon dioxide:

[0017] Take 100g of 20-30 mesh silica and soak it in 1000mL of 8mol / L hydrochloric acid solution, stir it at 80℃ for 12h, filter it, wash it with deionized water until it is neutral, dry it at 105℃ for 8h, and cool it to room temperature to obtain activated silica;

[0018] 2) Preparation of nickel-loaded silica particles:

[0019] Ni(NO3)2·6H2O is dissolved in an ethanol aqueous solution composed of deionized water and ethanol in a volume ratio of 1:1, and then activated silica is added, with a mass ratio of Ni(NO3)2·6H2O:activated silica being 3:1, and stirred at room temperature for 3 hours, and then heated to 100°C and stirred for 4 hours, cooled to room temperature, filtered and collected precipitates for reduced pressure volatilization, washed with deionized water until neutral, vacuum dried at 80°C for 10 hours, and then calcined in a tubular furnace at 400°C for 4 hours in a nitrogen atmosphere, and finally cooled to room temperature and ground to 20-30 meshes to obtain metal nickel-loaded silica particles, i.e., the catalyst.

[0020] Preferably, the catalyst is metallic copper-supported silica particles, which are prepared by the following method:

[0021] 1) Preparation of activated silicon dioxide:

[0022] Take 100g of 20-30 mesh silica and soak it in 1000mL of 8mol / L hydrochloric acid solution, stir it at 80℃ for 12h, filter it, wash it with deionized water until it is neutral, dry it at 105℃ for 8h, and cool it to room temperature to obtain activated silica;

[0023] 2) Preparation of metallic copper-loaded silica particles:

[0024] Cu(NO3)2·3H2O is dissolved in an ethanol aqueous solution composed of deionized water and ethanol in a volume ratio of 1:1, and then activated silica is added, the mass ratio of Cu(NO3)2·3H2O:activated silica is 2:1, stirred at room temperature for 3 hours, then heated to 100°C and stirred for 4 hours, cooled to room temperature, filtered and collected precipitates for reduced pressure volatilization, washed with deionized water until neutral, vacuum dried at 80°C for 10 hours, and then calcined in a tubular furnace at 400°C for 4 hours in a nitrogen atmosphere, finally cooled to room temperature, ground to 20-30 mesh, to obtain metal nickel-loaded silica particles, i.e., the catalyst.

[0025] Preferably, the catalyst is metallic iron-supported silica particles, which are prepared by the following method:

[0026] 1) Preparation of activated silicon dioxide:

[0027] Take 100g of 20-30 mesh silica and soak it in 1000mL of 8mol / L hydrochloric acid solution, stir it at 80℃ for 12h, filter it, wash it with deionized water until it is neutral, dry it at 105℃ for 8h, and cool it to room temperature to obtain activated silica;

[0028] 2) Preparation of metallic iron-loaded silica particles:

[0029] Fe(NO3)3·9H2O is dissolved in an ethanol aqueous solution composed of deionized water and ethanol in a volume ratio of 1:1, and then activated silica is added, the mass ratio of Fe(NO3)3·9H2O:activated silica is 5:1, stirred at room temperature for 3 hours, then heated to 100°C and stirred for 4 hours, cooled to room temperature, filtered and collected precipitates for reduced pressure volatilization, washed with deionized water until neutral, vacuum dried at 80°C for 10 hours, and then calcined in a tubular furnace at 400°C for 4 hours in a nitrogen atmosphere, finally cooled to room temperature, ground to 20-30 mesh, and obtained metallic iron-loaded silica particles, i.e., the catalyst.

[0030] Preferably, in step S1, the volume ratio of air to nitrogen is 10-12:3-4.

[0031] Preferably, in step S2, the first temperature is 200-350°C.

[0032] Preferably, the N2O-NH3 high-efficiency reactor includes a cylindrical shell with a cavity inside, an air inlet pipe arranged on the upper part of the shell and connected to the cavity, an exhaust pipe located in the middle of the cavity, a filter connected to the bottom of the exhaust pipe, a catalyst filled between the cylindrical shell and the exhaust pipe, and a thermal insulation layer covering the outer surface of the cylindrical shell. The upper end of the exhaust pipe extends upward from the cylindrical shell, and the gas entering from the air inlet pipe passes through the catalyst in the cylindrical shell and then enters the exhaust pipe through the filter, and is finally discharged from the upper end of the exhaust pipe.

[0033] Preferably, the photovoltaic cell production coating process tail gas treatment process comprises the following steps:

[0034] S1. The coating process tail gas generated in the production process of photovoltaic cells is introduced into the silane combustion tower, mixed with the introduced air and nitrogen, and the ratio of air to nitrogen is controlled to be 10-12:3-4. The mixed gas of silane in the combustion tube generates a plasma flame through arc discharge and self-ignites. The temperature of the tail gas after combustion is 500-600℃;

[0035] The tail gas discharged from the combustion of S2 and silane enters the N2O-NH3 high-efficiency reactor after passing through the dust collector. The N2O and NH3 in the tail gas react at 200-300°C under the action of the catalyst to generate N2 and H2O. The tail gas generated by the high-efficiency reactor is finally discharged through the exhaust pipe;

[0036] Part of the silica powder produced in the silane combustion tower settles and gathers at the bottom of the tower, and the other part enters the dust collector with the exhaust gas and is collected.

[0037] In a second aspect of the present invention, a photovoltaic cell production coating process tail gas treatment system is provided, which uses the above-mentioned process to treat the coating process tail gas generated in the photovoltaic cell production process, and the system includes a silane combustion tower, a dust collector, a N2O-NH3 high-efficiency reactor, a fan and an exhaust pipe connected in sequence;

[0038] Under the action of the fan, the coating process exhaust gas generated in the production process of photovoltaic cells enters the silane combustion tower, mixes with the air and nitrogen introduced into the tower and burns. The exhausted exhaust gas is dedusted by the dust collector and then enters the N2O-NH3 high-efficiency reactor. Under the action of the catalyst filled in the N2O-NH3 high-efficiency reactor, it reacts to generate N2 and H2O. The exhaust gas generated by the high-efficiency reactor is finally discharged through the exhaust pipe.

[0039] The beneficial effects of the present invention are:

[0040] The present invention provides a novel and efficient treatment process and system for tail gas from a film coating process generated during the production of photovoltaic cells. The present invention is superior to the conventional silane combustion + ammonia washing process. The efficient treatment process of the present invention not only achieves stable and standard emission of pollutants (SiH4, NH3, N2O), but also does not generate secondary pollution (such as in conventional treatment processes, ammonia will generate ammonia-containing wastewater after spray washing, causing secondary pollution), and simultaneously achieves emission reduction of greenhouse gas N2O in tail gas.

[0041] The present invention ingeniously utilizes two characteristic pollutants N2O and NH3 in the tail gas of the photovoltaic cell production coating process, gives full play to the redox characteristics of the two pollutants, does not need to provide an additional heat source, utilizes the heat of the tail gas after silane combustion, and can react and remove N2O and NH3 in a high-efficiency reactor filled with a homemade catalyst, thereby achieving the simultaneous removal of NH3 and N2O without the generation of secondary pollutants.

[0042] The catalyst provided by the present invention can catalyze the reaction of NH3 and N2O to generate N2 and H2O. On the one hand, the catalyst adsorbs N2O and NH3 in the tail gas onto the catalyst surface, and on the other hand, it exerts oxidation and reduction effects through the change of the valence of metal ions, thereby promoting the redox reaction of N2O and NH3 at low temperature. At the same time, the catalyst also serves as a transfer carrier of O atoms, transferring O from N2O to NH3, thereby making the reaction easier and faster, and the catalyst has low cost and low catalytic temperature. BRIEF DESCRIPTION OF THE DRAWINGS

[0043] Figure 1 A flow chart of the tail gas treatment process of the photovoltaic cell production coating process of the present invention;

[0044] Figure 2 It is a schematic structural diagram of the N2O-NH3 high-efficiency reactor of the present invention;

[0045] Figure 3 The pore size distribution diagram of the nickel-supported catalyst and the iron-supported catalyst prepared in the examples;

[0046] Figure 4 The pore size distribution diagram of the nickel-supported catalyst and the copper-supported catalyst prepared in the examples;

[0047] Figure 5 The monitoring result of NH3 emission concentration in the tail gas at the exhaust pipe outlet in the embodiment;

[0048] Figure 6 The monitoring result of N2O emission concentration in the tail gas at the exhaust pipe outlet in the embodiment;

[0049] Figure 7 The monitoring results of the exhaust gas pollutant emission concentration at the exhaust pipe outlet when the copper-supported catalyst is filled in the embodiment.

[0050] Description of reference numerals:

[0051] 1—columnar shell; 2—intake pipe; 3—exhaust pipe; 4—filter; 5—catalyst; 6—insulation layer. DETAILED DESCRIPTION

[0052] The present invention is further described in detail below in conjunction with embodiments so that those skilled in the art can implement the invention with reference to the description.

[0053] It should be understood that terms such as “having”, “including” and “comprising” used herein do not exclude the existence or addition of one or more other elements or combinations thereof.

[0054] The test methods used in the following examples are conventional methods unless otherwise specified. The materials and reagents used in the following examples are all commercially available unless otherwise specified. In the following examples, if no specific conditions are specified, the experiments were carried out under conventional conditions or conditions recommended by the manufacturer. The reagents or instruments used, if the manufacturer is not specified, are all conventional products that can be purchased commercially.

[0055] Reference Figure 1 and Figure 2 The present invention provides a photovoltaic cell production coating process tail gas treatment system and process, the system comprises a silane combustion tower, a dust collector (preferably a bag dust collector), a N2O-NH3 high-efficiency reactor, a fan and an exhaust pipe connected in sequence; the process comprises the following steps:

[0056] S1. The coating process tail gas generated in the production process of photovoltaic cells enters the silane combustion tower through the air duct under the traction of the fan. At the same time, the air and nitrogen are mixed stably and continuously to ensure the gentle combustion of silane within a safe and controllable range (for example, the ratio of air to nitrogen is controlled to be 10-12:3-4). The mixed gas of silane in the combustion tube generates a plasma flame through arc discharge and self-ignites. The temperature of the tail gas after combustion is 500-600℃;

[0057] After silane is burned, SiO2 is generated. Most of the silica powder settles to the bottom of the tower under the action of gravity, and the remaining silica powder enters the downstream bag filter through the air duct under the traction of the fan. The whole system is in a slightly negative pressure state. The combustion reaction equation is:

[0058] SiH4+2O2=SiO2+2H2O

[0059] S2. The tail gas (temperature about 200-350℃) treated by the bag filter enters the N2O-NH3 high-efficiency reactor under the traction of the fan. At this temperature, the N2O and NH3 in the tail gas react to generate N2 and H2O through the action of the catalyst. The GHSV is set to 15000-20000h -1 No additional heat source is required, and the tail gas produced by the high-efficiency reactor is finally discharged through the exhaust pipe; the reaction equation is as follows:

[0060] 3N2O+2NH3=4N2+3H2O

[0061] The catalyst is metal M-loaded silica particles, and the metal M is any one of nickel, copper, and iron. The catalyst is prepared by the following method:

[0062] 1) Preparation of activated silicon dioxide:

[0063] Take 20-30 mesh silicon dioxide and soak it in hydrochloric acid solution, stir it at 70-90°C for 6-24h, filter it, wash it with deionized water until it is neutral, dry it at 90-120°C for 4-16h, and cool it to room temperature to obtain activated silicon dioxide;

[0064] 2) Preparation of metal M-loaded silica particles:

[0065] The nitrate of metal M is dissolved in an ethanol aqueous solution, and then activated silica is added, the mass ratio of the nitrate of metal M: activated silica is 2:1-5:1, stirred at room temperature for 1.5-6 hours, then heated to 90-110°C and stirred for 2-8 hours, cooled to room temperature, filtered and collected precipitates for reduced pressure volatilization, washed with deionized water to neutrality, vacuum dried at 70-90°C for 5-20 hours, then calcined at 300-500°C in a nitrogen atmosphere for 2-8 hours, finally cooled to room temperature, ground to 20-30 meshes, and obtained metal M-loaded silica particles, i.e., catalyst.

[0066] The mechanism of action of the catalyst is as follows:

[0067] N2O is adsorbed onto the catalyst surface and forms a complex with the catalyst. The NO bond breaks to release N2, and O forms aO with the catalyst. - NH3 is also adsorbed on the catalyst and reacts with aO - The reaction generates N2 and H2O; the catalyst is the intermediate active substance in the reaction of N2O and NH3. On the one hand, its function is to adsorb N2O and NH3 in the exhaust gas to the catalyst surface, and on the other hand, it plays an oxidizing and reducing role through the change of the valence of metal ions, promoting the redox reaction of N2O and NH3 at low temperature. At the same time, the catalyst also acts as a transfer carrier of O atoms, transferring O from N2O to NH3, thus making the reaction easier and faster.

[0068] At present, catalytic decomposition is usually used for the treatment of N2O, and the catalysts used are mostly precious metal catalysts, such as Pt, Pd, Ag, Au, Ru, etc., but these precious metal catalysts have the disadvantages of being expensive and having a high catalytic temperature (>350°C). The catalyst prepared by the present invention can overcome the above problems. The present invention cleverly utilizes two characteristic pollutants N2O and NH3 in the tail gas of the photovoltaic cell production coating process, and with the help of the self-made catalyst, gives full play to the redox characteristics of the two, can achieve the removal of the two pollutants, and has low cost and low catalytic temperature (200-350°C).

[0069] In a preferred embodiment, the catalyst is metal nickel-supported silica particles, which are prepared by the following method:

[0070] 1) Preparation of activated silicon dioxide:

[0071] Take 100g of 20-30 mesh silica and soak it in 1000mL of 8mol / L hydrochloric acid solution, stir it at 80℃ for 12h, filter it, wash it with deionized water until it is neutral, dry it at 105℃ for 8h, and cool it to room temperature to obtain activated silica;

[0072] 2) Preparation of nickel-loaded silica particles:

[0073] Ni(NO3)2·6H2O is dissolved in an ethanol aqueous solution composed of deionized water and ethanol in a volume ratio of 1:1, and then activated silica is added, with a mass ratio of Ni(NO3)2·6H2O:activated silica being 3:1, and stirred at room temperature for 3 hours, and then heated to 100°C and stirred for 4 hours, cooled to room temperature, filtered and collected precipitates for reduced pressure volatilization, washed with deionized water until neutral, vacuum dried at 80°C for 10 hours, and then calcined in a tubular furnace at 400°C for 4 hours in a nitrogen atmosphere, and finally cooled to room temperature and ground to 20-30 meshes to obtain metal nickel-loaded silica particles, i.e., the catalyst.

[0074] In a preferred embodiment, the catalyst is metallic copper-supported silica particles, which are prepared by the following method:

[0075] 1) Preparation of activated silicon dioxide:

[0076] Take 100g of 20-30 mesh silica and soak it in 1000mL of 8mol / L hydrochloric acid solution, stir it at 80℃ for 12h, filter it, wash it with deionized water until it is neutral, dry it at 105℃ for 8h, and cool it to room temperature to obtain activated silica;

[0077] 2) Preparation of metallic copper-loaded silica particles:

[0078] Cu(NO3)2·3H2O is dissolved in an ethanol aqueous solution composed of deionized water and ethanol in a volume ratio of 1:1, and then activated silica is added, the mass ratio of Cu(NO3)2·3H2O:activated silica is 2:1, stirred at room temperature for 3 hours, then heated to 100°C and stirred for 4 hours, cooled to room temperature, filtered and collected precipitates for reduced pressure volatilization, washed with deionized water until neutral, vacuum dried at 80°C for 10 hours, and then calcined in a tubular furnace at 400°C for 4 hours in a nitrogen atmosphere, finally cooled to room temperature, ground to 20-30 mesh, to obtain metallic copper-loaded silica particles, i.e., the catalyst.

[0079] In a preferred embodiment, the catalyst is metallic iron-supported silica particles, which are prepared by the following method:

[0080] 1) Preparation of activated silicon dioxide:

[0081] Take 100g of 20-30 mesh silica and soak it in 1000mL of 8mol / L hydrochloric acid solution, stir it at 80℃ for 12h, filter it, wash it with deionized water until it is neutral, dry it at 105℃ for 8h, and cool it to room temperature to obtain activated silica;

[0082] 2) Preparation of metallic iron-loaded silica particles:

[0083] Fe(NO3)3·9H2O is dissolved in an ethanol aqueous solution composed of deionized water and ethanol in a volume ratio of 1:1, and then activated silica is added, the mass ratio of Fe(NO3)3·9H2O:activated silica is 5:1, stirred at room temperature for 3 hours, then heated to 100°C and stirred for 4 hours, cooled to room temperature, filtered and collected precipitates for reduced pressure volatilization, washed with deionized water until neutral, vacuum dried at 80°C for 10 hours, and then calcined in a tubular furnace at 400°C for 4 hours in a nitrogen atmosphere, finally cooled to room temperature, ground to 20-30 mesh, to obtain metal nickel-loaded silica particles, i.e., the catalyst.

[0084] In a preferred embodiment, the N2O-NH3 high-efficiency reactor includes a cylindrical shell 1 with a cavity inside, an intake pipe 2 arranged on the upper part of the shell and connected to the cavity, an exhaust pipe 3 located in the middle of the cavity, a wire filter 4 connected to the bottom of the exhaust pipe 3, a catalyst 5 filled between the cylindrical shell 1 and the exhaust pipe 3, and a thermal insulation layer 6 coated on the outer surface of the cylindrical shell 1. The upper end of the exhaust pipe 3 extends upward from the cylindrical shell 1. The gas entering from the intake pipe 2 passes through the catalyst in the cylindrical shell 1 and then enters the exhaust pipe 3 through the filter 4, and is finally discharged from the upper end of the exhaust pipe 3.

[0085] The above is the overall concept of the present invention, and detailed embodiments and comparative examples are provided below on the basis of the overall concept of the present invention to further illustrate the present invention.

[0086] In the following examples, each catalyst was prepared by the following method:

[0087] 1) Preparation of activated silicon dioxide:

[0088] Take 100g of silica with a particle size range of 20-30 mesh (Qingdao Jiyida Silica Reagent Co., Ltd., specific surface area 382.6m2 / g, pore diameter 7.1nm, pore volume 0.725cm3 / g) and soak it in 1000mL of 8mol / L hydrochloric acid solution, stir at 80℃ for 12h, filter, wash with deionized water until neutral, dry in an oven at 105℃ for 8h, cool to room temperature, and obtain activated silica, which is stored in a desiccator for later use;

[0089] 2) Preparation of metal M-loaded silica particles:

[0090] Three catalysts were prepared using Ni(NO3)2·6H2O, Cu(NO3)2·3H2O, and Fe(NO3)3·9H2O respectively: metal nickel-loaded silica particles, metal copper-loaded silica particles, and metal iron-loaded silica particles, which were respectively denoted as nickel-loaded catalyst, copper-loaded catalyst, and iron-loaded catalyst. The specific preparation methods are as follows:

[0091] Dissolve Ni(NO3)2·6H2O, Cu(NO3)2·3H2O, and Fe(NO3)3·9H2O in a sufficient amount of ethanol aqueous solution composed of deionized water and ethanol in a volume ratio of 1:1, and then add activated silica. The mass ratios of the raw materials in the three catalysts are:

[0092] The mass ratio of Ni(NO3)2·6H2O:activated silica is 3:1, the mass ratio of Cu(NO3)2·3H2O:activated silica is 2:1, and the mass ratio of Fe(NO3)3·9H2O:activated silica is 5:1;

[0093] After adding, the mixture was stirred at room temperature for 3 hours, then heated to 100°C and stirred for 4 hours, cooled to room temperature, filtered and collected, and the precipitate was evaporated under reduced pressure, washed with deionized water until neutral, vacuum dried at 80°C for 10 hours, and then calcined at 400°C in a tubular furnace under a nitrogen atmosphere for 4 hours, and finally cooled to room temperature and ground into 20-30 meshes to obtain three catalysts: a nickel-supported catalyst, a copper-supported catalyst, and an iron-supported catalyst.

[0094] Reference Figure 3 and Figure 4 , is the pore size distribution diagram of the three catalysts prepared above, and the following Table 1 is the performance data of the three catalysts:

[0095] Table 1

[0096]

[0097] Example 1

[0098] A photovoltaic cell production coating process tail gas treatment system and process, the system comprises a silane combustion tower, a dust collector, a N2O-NH3 high-efficiency reactor, a fan and an exhaust pipe connected in sequence;

[0099] The N2O-NH3 high-efficiency reactor includes a cylindrical shell 1 with a cavity inside, an intake pipe 2 arranged on the upper part of the shell and connected to the cavity, an exhaust pipe 3 located in the middle of the cavity, a filter screen 4 connected to the bottom of the exhaust pipe 3, a catalyst 5 filled between the cylindrical shell 1 and the exhaust pipe 3, and a thermal insulation layer 6 coated on the outer surface of the cylindrical shell 1. The upper end of the exhaust pipe 3 extends upward from the cylindrical shell 1. The gas entering from the intake pipe 2 passes through the catalyst in the cylindrical shell 1 and then enters the exhaust pipe 3 through the filter screen 4, and is finally discharged from the upper end of the exhaust pipe 3.

[0100] The process package of this system is as follows:

[0101] S1. Exhaust gas from the film coating process generated during the production of photovoltaic cells (its main parameters are as follows, which are a fluctuating range: air volume 100~120m 3 / h, SiH4 concentration 1000~1100mg / m 3 、NH3 concentration 230~350mg / m 3 、N2O concentration 700~800mg / m 3 ) is drawn by the fan through the air duct into the silane combustion chamber of the silane combustion tower, and the air and nitrogen introduced stably and continuously are mixed to ensure the gentle combustion of silane within a safe and controllable range (control the compressed air volume 12m 3 / h, nitrogen volume 4m 3 / h) to ensure gentle combustion of silane within a safe and controllable range; the mixed gas of silane in the combustion tube generates a plasma flame through arc discharge and self-ignites, and the exhaust gas temperature after combustion fluctuates within the range of 500-600℃;

[0102] After silane burns, SiO2 is generated. Most of the silica powder settles to the bottom of the tower and gathers under the action of gravity. The remaining silica powder enters the downstream bag dust collector through the air duct under the traction of the fan. The whole system is in a slightly negative pressure state.

[0103] S2, the tail gas treated by the bag filter (temperature fluctuates in the range of 220-350℃) enters the N2O-NH3 high-efficiency reactor under the traction of the fan, and the air velocity GHSV is set to 18000h -1 The exhaust gas enters the columnar shell 1 of the N2O-NH3 high-efficiency reactor from the upper part through the intake pipe 2, enters the exhaust pipe 3 through the lower steel wire filter 4 after passing through the catalyst, and is finally discharged from the upper end of the exhaust pipe 3; at this temperature, N2O and NH3 in the exhaust gas react to generate N2 and H2O through the action of the catalyst, and no additional heat source is required. The exhaust gas generated by the high-efficiency reactor is finally discharged through a 25m exhaust chimney; the particle concentration, NH3 concentration, and N2O concentration at the exhaust chimney outlet are regularly monitored.

[0104] In this example, three catalysts were respectively filled into the same N2O-NH3 high-efficiency reactor for testing and comparison. The reactor was operated continuously for 20 days, and the NH3 emission concentration data in the exhaust gas at the exhaust pipe outlet were monitored as follows: Figure 5 As shown in Figure 2, N2O emission concentration data is as follows: Figure 6 As shown:

[0105] The copper-loaded catalyst was continuously run for 20 days, and the exhaust gas pollutant emission concentration data at the exhaust pipe outlet was monitored. Figure 7 shown.

[0106] According to monitoring data, all three catalysts have shown excellent exhaust catalytic treatment effects, with SiH4 treatment efficiency in the coating process exhaust gas > 99%, NH3 treatment efficiency > 95%, and N2O treatment efficiency > 97%. The particulate matter and N2O emissions in the exhaust gas discharged through the exhaust pipe meet the requirements of the "Battery Industry Pollutant Emission Standard" (GB30484-2013), and NH3 emissions meet the emission standard limit requirements of the "Odor Pollutant Emission Standard" (GB14554-93). Among them, the effect is relatively best when the copper-loaded catalyst is filled.

[0107] Comparative Example

[0108] The traditional process is used to treat the tail gas from the coating process generated during the production of photovoltaic cells. The process steps are as follows:

[0109] S1, the coating process tail gas generated in the production process of photovoltaic cells (the source is the same as that of Example 1, and its main parameters are as follows, which is a fluctuation range: air volume 100-120m 3 / h, SiH4 concentration 1000~1100mg / m 3 、NH3 concentration 230~350mg / m 3 、N2O concentration 700~800mg / m 3 ) is drawn by the fan through the air duct into the silane combustion chamber of the silane combustion tower, and the air and nitrogen introduced stably and continuously are mixed to ensure the gentle combustion of silane within a safe and controllable range (control the compressed air volume 12m 3 / h, nitrogen volume 4m 3 / h) to ensure gentle combustion of silane within a safe and controllable range; the mixed gas of silane in the combustion tube generates a plasma flame through arc discharge and self-ignites, and the exhaust gas temperature after combustion fluctuates within the range of 500-600℃;

[0110] After silane burns, SiO2 is generated. Most of the silica powder settles to the bottom of the tower and gathers under the action of gravity. The remaining silica powder enters the downstream bag dust collector through the air duct under the traction of the fan. The whole system is in a slightly negative pressure state.

[0111] S2. The tail gas treated by the bag filter (temperature fluctuates within the range of 220-350℃) enters the high-efficiency spray tower under the traction of the fan. The tail gas enters from the lower end of the spray tower, is absorbed by the absorbent (water) sprayed under the upper end of the spray tower, and is discharged from the upper end of the spray tower. After the NH3 in the tail gas is absorbed by the absorbent, it is discharged from the bottom of the spray tower in the form of ammonia nitrogen wastewater. Subsequently, a wastewater treatment system needs to be added to treat the ammonia nitrogen wastewater or ammonium sulfate wastewater before discharge.

[0112] After treatment by this process, the particulate matter in the exhaust gas discharged through the exhaust pipe meets the requirements of the "Battery Industry Pollutant Emission Standard" (GB30484-2013), and the NH3 emission meets the emission standard limit requirements of the "Odor Pollutant Emission Standard" (GB14554-93). However, this process has no obvious treatment effect on N2O, and long-term N2O emissions will inevitably aggravate the greenhouse effect.

[0113] Although the embodiments of the present invention have been disclosed as above, they are not limited to the applications listed in the specification and the implementation modes. They can be fully applied to various fields suitable for the present invention. For those familiar with the art, additional modifications can be easily implemented. Therefore, without departing from the general concept defined by the claims and the scope of equivalents, the present invention is not limited to specific details.

Claims

1. A process for treating tail gas from a photovoltaic cell production coating process, characterized in that: The following steps are involved: S1. The coating process tail gas generated in the production process of photovoltaic cells is introduced into a silane combustion tower, mixed with the introduced air and nitrogen, and burned; The tail gas discharged from the combustion of S2 and silane enters the N2O-NH3 high-efficiency reactor after passing through the dust collector. The N2O and NH3 in the tail gas react to generate N2 and H2O under the action of the catalyst at the first temperature. The tail gas generated by the high-efficiency reactor is finally discharged through the exhaust pipe; Wherein, the catalyst is metal M loaded silica particles, and the metal M is any one of nickel, copper and iron.

2. The photovoltaic cell production coating process tail gas treatment process according to claim 1, characterized in that: The catalyst is prepared by the following method: 1) Preparation of activated silicon dioxide: Take 20-30 mesh silicon dioxide and soak it in hydrochloric acid solution, stir it at 70-90°C for 6-24h, filter it, wash it with deionized water until it is neutral, dry it at 90-120°C for 4-16h, and cool it to room temperature to obtain activated silicon dioxide; 2) Preparation of metal M-loaded silica particles: The nitrate of metal M is dissolved in an ethanol aqueous solution, and then activated silica is added, the mass ratio of the nitrate of metal M to the activated silica is 2:1-5:1, the mixture is stirred at room temperature for 1.5-6 hours, and then heated to 90-110° C. and stirred for 2-8 hours, cooled to room temperature, filtered and collected precipitates, evaporated under reduced pressure, washed with deionized water until neutral, vacuum dried at 70-90° C. for 5-20 hours, and then calcined at 300-500° C. in a nitrogen atmosphere for 2-8 hours, and finally cooled to room temperature and ground to 20-30 meshes to obtain metal M-loaded silica particles, i.e., the catalyst.

3. The process for treating tail gas from the film coating process of photovoltaic cell production according to claim 2, characterized in that: The catalyst is nickel-supported silica particles, which are prepared by the following method: 1) Preparation of activated silicon dioxide: Take 100g of 20-30 mesh silica and soak it in 1000mL of 8mol / L hydrochloric acid solution, stir it at 80℃ for 12h, filter it, wash it with deionized water until it is neutral, dry it at 105℃ for 8h, and cool it to room temperature to obtain activated silica; 2) Preparation of nickel-loaded silica particles: Ni(NO3)2·6H2O is dissolved in an ethanol aqueous solution composed of deionized water and ethanol in a volume ratio of 1:1, and then activated silica is added, with a mass ratio of Ni(NO3)2·6H2O:activated silica being 3:1, and stirred at room temperature for 3 hours, and then heated to 100°C and stirred for 4 hours, cooled to room temperature, filtered and collected precipitates for reduced pressure volatilization, washed with deionized water until neutral, vacuum dried at 80°C for 10 hours, and then calcined in a tubular furnace at 400°C for 4 hours in a nitrogen atmosphere, and finally cooled to room temperature and ground to 20-30 meshes to obtain metal nickel-loaded silica particles, i.e., the catalyst.

4. The process for treating tail gas from the film coating process of photovoltaic cell production according to claim 2, characterized in that: The catalyst is metallic copper-supported silica particles, which are prepared by the following method: 1) Preparation of activated silicon dioxide: Take 100g of 20-30 mesh silica and soak it in 1000mL of 8mol / L hydrochloric acid solution, stir it at 80℃ for 12h, filter it, wash it with deionized water until it is neutral, dry it at 105℃ for 8h, and cool it to room temperature to obtain activated silica; 2) Preparation of metallic copper-loaded silica particles: Cu(NO3)2·3H2O is dissolved in an ethanol aqueous solution composed of deionized water and ethanol in a volume ratio of 1:1, and then activated silica is added, the mass ratio of Cu(NO3)2·3H2O:activated silica is 2:1, stirred at room temperature for 3 hours, then heated to 100°C and stirred for 4 hours, cooled to room temperature, filtered and collected precipitates for reduced pressure volatilization, washed with deionized water until neutral, vacuum dried at 80°C for 10 hours, and then calcined in a tubular furnace at 400°C for 4 hours in a nitrogen atmosphere, finally cooled to room temperature, ground to 20-30 mesh, to obtain metallic copper-loaded silica particles, i.e., the catalyst.

5. The process for treating tail gas from the film coating process of photovoltaic cell production according to claim 2, characterized in that: The catalyst is metallic iron-supported silica particles, which are prepared by the following method: 1) Preparation of activated silicon dioxide: Take 100g of 20-30 mesh silica and soak it in 1000mL of 8mol / L hydrochloric acid solution, stir it at 80℃ for 12h, filter it, wash it with deionized water until it is neutral, dry it at 105℃ for 8h, and cool it to room temperature to obtain activated silica; 2) Preparation of metallic iron-loaded silica particles: Fe(NO3)3·9H2O is dissolved in an ethanol aqueous solution composed of deionized water and ethanol in a volume ratio of 1:1, and then activated silica is added, the mass ratio of Fe(NO3)3·9H2O:activated silica is 5:1, stirred at room temperature for 3 hours, then heated to 100°C and stirred for 4 hours, cooled to room temperature, filtered and collected precipitates for reduced pressure volatilization, washed with deionized water until neutral, vacuum dried at 80°C for 10 hours, and then calcined in a tubular furnace at 400°C for 4 hours in a nitrogen atmosphere, finally cooled to room temperature, ground to 20-30 mesh, to obtain metal nickel-loaded silica particles, i.e., the catalyst.

6. The process for treating tail gas from the film coating process of photovoltaic cell production according to claim 2, characterized in that: In step S1, the volume ratio of air to nitrogen is 10-12:3-4.

7. The process for treating tail gas from the film coating process of photovoltaic cell production according to claim 6, characterized in that: In step S2, the first temperature is 200-350°C.

8. The process for treating tail gas from the film coating process of photovoltaic cell production according to claim 7, characterized in that: The N2O-NH3 high-efficiency reactor includes a cylindrical shell with a cavity inside, an intake pipe arranged on the upper part of the shell and connected to the cavity, an exhaust pipe located in the middle of the cavity, a filter connected to the bottom of the exhaust pipe, a catalyst filled between the cylindrical shell and the exhaust pipe, and a heat-insulating layer covering the outer surface of the cylindrical shell. The upper end of the exhaust pipe extends upward from the cylindrical shell, and the gas entering from the intake pipe passes through the catalyst in the cylindrical shell and then enters the exhaust pipe through the filter, and is finally discharged from the upper end of the exhaust pipe.

9. The process for treating tail gas from the film coating process of photovoltaic cell production according to claim 8, characterized in that: The following steps are involved: S1. The coating process tail gas generated in the production process of photovoltaic cells is introduced into the silane combustion tower, mixed with the introduced air and nitrogen, and the ratio of air to nitrogen is controlled to be 10-12:3-4. The mixed gas of silane in the combustion tube generates a plasma flame through arc discharge and self-ignites. The temperature of the tail gas after combustion is 500-600℃; The tail gas discharged from the combustion of S2 and silane enters the N2O-NH3 high-efficiency reactor after passing through the dust collector. The N2O and NH3 in the tail gas react at 200-300°C under the action of the catalyst to generate N2 and H2O. The tail gas generated by the high-efficiency reactor is finally discharged through the exhaust pipe; Part of the silica powder produced in the silane combustion tower settles and gathers at the bottom of the tower, and the other part enters the dust collector with the exhaust gas and is collected.

10. A photovoltaic cell production coating process tail gas treatment system, characterized in that: The process described in any one of claims 1 to 9 is used to treat the coating process tail gas generated in the production process of photovoltaic cells. The system includes a silane combustion tower, a dust collector, a N2O-NH3 high-efficiency reactor, a fan and an exhaust pipe connected in sequence; Under the action of the fan, the coating process exhaust gas generated in the production process of photovoltaic cells enters the silane combustion tower, mixes with the air and nitrogen introduced into the tower and burns. The exhausted exhaust gas is dedusted by the dust collector and then enters the N2O-NH3 high-efficiency reactor. Under the action of the catalyst filled in the N2O-NH3 high-efficiency reactor, it reacts to generate N2 and H2O. The exhaust gas generated by the high-efficiency reactor is finally discharged through the exhaust pipe.

Citation Information

Cited By

  • Waste gas recovery system in silicon solar energy industry

    CN224524396U