Coated asphalt reactor

By using a stirring device and defoamer in the coated asphalt reactor, the thorough oxidation of ethylene tar and air is achieved, the problem of insufficient reactor design in the prior art is solved, and high-performance coated asphalt is produced, which improves the Added value and economic benefits of refining products.

CN118925627APending Publication Date: 2024-11-12SINOPEC ENGINEERING INCORPORATION +1
View PDF 0 Cites 1 Cited by

Patent Information

Application Number
CN202310533353.7
Authority / Receiving Office
CN · China
Patent Type
Applications(China)
Current Assignee / Owner
Filing Date
2023-05-11
Publication Date
2024-11-12

AI Technical Summary

Technical Problem

The prior art is difficult to produce high-performance coated asphalt, especially in the oxidation reaction of ethylene tar with air, and the reactor design is not sufficient to achieve complete oxidation.

Method used

A coated asphalt reactor is designed, including a reaction chamber, agitator and a defoamer. The ethylene tar and air are fully stirred by agitating the blades, and the foam is eliminated by using the defoamer to ensure that the reaction raw materials are completely mixed and thoroughly oxidized, and finally the production is High-performance coated asphalt.

Benefits of technology

Through sufficient stirring and defoaming, the complete mixing and thorough oxidation of ethylene tar and air are achieved, and high-performance coated asphalt is produced, which improves the added value and economic benefits of refined products.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure CN118925627A_ABST
    Figure CN118925627A_ABST
Patent Text Reader

Abstract

The invention relates to a coated asphalt reactor, which comprises a reaction chamber, a stirring device and a defoaming device, a feed pipe for introducing an ethylene tar raw material is arranged above the reaction chamber, an air injector for introducing air is arranged below the reaction chamber, an exhaust port is arranged on the top wall of the reaction chamber, and a discharge port is arranged on the bottom wall of the reaction chamber; the stirring device comprises a stirring blade; the stirring blade is arranged in the reaction chamber and is positioned below the air injector; and the bubble remover is arranged in the reaction chamber and is positioned between the air injector and the feeding pipe. According to the invention, the stirring blades are used for full stirring and pushing, and the foam eliminator is used for eliminating foams, so that the ethylene tar raw material and air are completely mixed, thorough oxidation is realized, and finally, high-performance coated asphalt is produced.
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] The present disclosure relates to the technical field of petrochemical industry, and in particular, to a coated asphalt reactor. Background Art

[0002] As a highly aromatized specialty product, coated asphalt is mainly used for mixing with carbon materials to prepare various graphite carbon products. According to different application scenarios, it can be divided into binders, impregnants, and coating agents. It is widely used in the production of graphite electrodes, carbon blocks for metallurgical furnaces and aluminum electrolytic cells, prebaked anodes and anode pastes for electrolytic aluminum, and electrode pastes required for smelting ferroalloys and calcium carbide. At present, the commonly used methods for preparing coated asphalt include chemical catalysis, vacuum flash evaporation, air oxidation, etc. The high-performance asphalt for negative electrode materials produced by air oxidation reaction of ethylene tar can not only meet the development of negative electrode materials for lithium-ion batteries, but also enrich the types of Sinopec's refining products and increase the added value of refining products, with good economic and social benefits.

[0003] However, the reactor is particularly important for the air oxidation reaction of coated asphalt. Therefore, providing a reactor that can produce high-performance coated asphalt is an urgent problem to be solved.

[0004] Invention Nene

[0005] The purpose of the present disclosure is to provide a coated asphalt reactor that can achieve full reaction of ethylene tar feedstock with air and achieve thorough oxidation to produce high-performance coated asphalt products.

[0006] In order to achieve the above object, the present disclosure provides a coated asphalt reactor, comprising:

[0007] A reaction chamber, wherein a feed pipe for introducing ethylene tar raw materials is arranged above the reaction chamber, an air injector for introducing air is arranged below the reaction chamber, an exhaust port is arranged on the top wall of the reaction chamber, and a discharge port is arranged on the bottom wall;

[0008] A stirring device, the stirring device comprising a stirring blade, the stirring blade is arranged inside the reaction chamber and below the air injector;

[0009] A debubbler is arranged inside the reaction chamber and between the air injector and the feed pipe.

[0010] Optionally, the debubble device includes a debubble body, which is provided with a plurality of debubble holes distributed at intervals along the circumferential direction and the radial direction and has a central debubble zone and an edge debubble zone, wherein the openings of the debubble holes in the central debubble zone gradually narrow from top to bottom, and the openings of the debubble holes in the edge debubble zone gradually narrow from bottom to top.

[0011] Optionally, the maximum pore diameter of the defoaming holes gradually increases from the center to the edge.

[0012] Optionally, the area ratio of the central debubble zone to the edge debubble zone is between 1:1 and 2:3.

[0013] Optionally, a plurality of debubblers are arranged in the reaction chamber at intervals along the up-down direction, and the area of ​​the central debubbling zone of the plurality of debubblers gradually decreases from top to bottom.

[0014] Optionally, the stirring device includes a stirring controller, a stirring shaft and a plurality of stirring blades, the stirring shaft is connected between the stirring controller and the plurality of stirring blades, the plurality of stirring blades are evenly distributed along the circumference of the stirring shaft, and the stirring surface of each stirring blade is constructed as a curved surface that gradually inclines downward along the rotation direction.

[0015] Optionally, the discharge end of the feed pipe is arranged inside the reaction chamber and faces downward, the feed end of the feed pipe is arranged outside the reaction chamber and is provided with a cut-off valve, and the feed pipe is connected to the ethylene tar raw material pipe and the purge superheated steam pipe respectively through the cut-off valve.

[0016] Optionally, the air injector comprises an injection pipe having a plurality of injection holes arranged at intervals along its length direction, and one side of the injection pipe is closed and the other side is connected to the air pipe.

[0017] Optionally, the injection hole is configured as a semi-through hole opening downward.

[0018] Optionally, one side of the injection pipe is connected to a stripping superheated steam pipe.

[0019] The beneficial effects of this technical solution are: first, the stirring blades are used to fully stir the ethylene tar raw material and air so that they can be fully mixed and reacted, and then the reaction raw materials are pushed further through the defoamer to eliminate the foam, so as to promote the complete mixing of the ethylene tar raw material and the air, achieve thorough oxidation, and finally produce high-performance coated asphalt.

[0020] Other features and advantages of the present disclosure will be described in detail in the following detailed description. BRIEF DESCRIPTION OF THE DRAWINGS

[0021] The accompanying drawings are used to provide a further understanding of the present disclosure and constitute a part of the specification. Together with the following specific embodiments, they are used to explain the present disclosure but do not constitute a limitation of the present disclosure. In the accompanying drawings:

[0022] Figure 1 is a schematic diagram of a coated asphalt reactor provided by an embodiment of the present disclosure;

[0023] Figure 2 It is a schematic diagram of the operating state of the reaction raw materials;

[0024] Figure 3 is a schematic structural diagram of a debubbler provided in an embodiment of the present disclosure;

[0025] Figure 4 is a cross-sectional view of the defoaming holes in the central defoaming zone provided by an embodiment of the present disclosure;

[0026] Figure 5 is a cross-sectional view of the defoaming holes in the edge defoaming zone provided by an embodiment of the present disclosure;

[0027] Figure 6 is a bottom view schematic diagram of an air injector provided in an embodiment of the present disclosure;

[0028] Figure 7 yes Figure 6 Schematic diagram of CC cross-section;

[0029] Figure 8 is a schematic diagram of the assembly of the stirring blade and the stirring shaft of the embodiment of the present disclosure;

[0030] Fig. 9 yes Figure 8 AA schematic diagram.

[0031] Description of Reference Numerals

[0032] 1 Reaction chamber 11 side wall 12 top wall

[0033] 2 Feed pipe 21 Discharge end 22 Cut-off valve

[0034] 13 bottom wall 3 air injector 31 injection pipe

[0035] 32 injection hole 4 stirring device 41 stirring controller

[0036] 42 stirring shaft 43 stirring blade 5 debubbler

[0037] 51 defoaming body 52 defoaming hole 511 central defoaming area

[0038] 512 Edge debubbling area 6 Purge superheated steam pipe 7 Stripping superheated steam pipe

[0039] 8 Inspection manhole 9 Inspection hook 10 Fixed platform

[0040] d Reaction tail gas f Coated asphalt 501 primary debubbler

[0041] 502 secondary debubbler 20 ethylene tar raw material pipe 30 air pipe

[0042] 431 Mixed Noodles DETAILED DESCRIPTION

[0043] The specific implementation of the present disclosure is described in detail below in conjunction with the accompanying drawings. It should be understood that the specific implementation described herein is only used to illustrate and explain the present disclosure, and is not used to limit the present disclosure.

[0044] In the present disclosure, unless otherwise stated, directional words such as "upper" and "lower" refer to Figure 1 The up-down direction of the drawing, that is, the direction away from the "stirring device" is up. The above definition is only used to explain and illustrate the present disclosure and should not be understood as a limitation of the present disclosure.

[0045] According to the specific implementation of the present disclosure, Figures 1 to 9 As shown, a coated asphalt reactor is provided, including a reaction chamber 1, a stirring device 4 and a debubbler 5, wherein a feed pipe 2 for introducing ethylene tar raw material is arranged above the reaction chamber 1, an air injector 3 for introducing air is arranged below the reaction chamber 1, and an exhaust port is arranged on the top wall 12 of the reaction chamber 1, and a discharge port is arranged on the bottom wall 13; the stirring device 4 includes a stirring blade 43, which is arranged inside the reaction chamber 1 and located below the air injector 3; the debubbler 5 is arranged inside the reaction chamber 1 and located between the air injector 3 and the feed pipe 2.

[0046] refer to Figure 1 As shown, the reaction chamber 1 serves as the place for air oxidation reaction. In the actual reaction process, the ethylene tar raw material is first introduced through the upper feed pipe 2, and the air is introduced through the lower air injector 3. During the introduction process, the stirring blade 43 continuously rotates and stirs to push the reaction raw material to rotate and flow upward, and the ethylene tar raw material and the air can be fully mixed and reacted. Then, in the process of the reaction raw material flowing upward, the defoamer 5 can effectively eliminate the large amount of foam generated in the mixed liquid (because ethylene tar is relatively viscous, a large amount of foam will be generated after the injection of air), further ensuring the complete mixing of the ethylene tar raw material and the air to achieve thorough oxidation. After the oxidation reaction is completed, the reaction exhaust gas d and the coated asphalt f are finally discharged through the exhaust port and the discharge port respectively.

[0047] Through the above technical scheme, the ethylene tar raw material and the air are first fully stirred by the stirring blades so that they can be fully mixed and reacted. Then, the reaction raw materials are further pushed through the defoamer 5 to eliminate the foam, so as to promote the complete mixing of the ethylene tar raw material and the air, achieve thorough oxidation, and finally produce high-performance coated asphalt.

[0048] Among them, reference Figure 2As shown by the arrow, driven by the stirring blade 43, the flow direction of the reaction raw materials in the reaction chamber 1 is: rotating upward from the center, the airflow is adjusted after passing through the debubbler 5 and continues to flow upward until it approaches the side walls 11 on both sides of the reaction chamber 1 and flows downward respectively, thus circulating up and down.

[0049] Based on this, in the specific implementation of the present disclosure, refer to Figures 3 to 5 As shown, the debubble device 5 includes a debubble body 51, which is provided with a plurality of debubble holes 52 spaced along the circumferential direction and the radial direction and has a central debubble area 511 and an edge debubble area 512, wherein the openings of the debubble holes 52 in the central debubble area 511 gradually decrease from top to bottom (refer to Figure 4 ), the opening of the defoaming hole 52 of the edge defoaming zone 512 gradually decreases from bottom to top (refer to Figure 5 ).

[0050] That is, the hole wall of the debubble hole 52 in the embodiment of the present disclosure is constructed as an inclined wall, so as to form a sharp-angle cut bubble mode, and cut the flowing large bubble into a plurality of small bubbles, so as to achieve a complete mixing reaction with the ethylene tar raw material. Specifically, according to the flow direction of the reaction raw material, the debubble body 51 is divided into two debubble areas, respectively referring to Figure 4 and Figure 5 (The arrow in the figure indicates the flow direction of the mixed liquid containing bubbles), so that the large bubbles can be divided into a plurality of small bubbles when passing through the debubble hole 52. Optionally, the inclination angle of the hole wall of the debubble hole 52 can be 50 degrees.

[0051] It should be noted that the debubbling hole 52 can be constructed in any manner, and can be in an irregular shape such as a triangle, a circle or a water drop shape, as long as the hole wall can be inclined to form an acute angle cut bubble. And the shape of the debubbler 5 can be matched with the reaction chamber 1. In the specific embodiment of the present disclosure, the reaction chamber 1 is roughly cylindrical, and the debubbling body 51 adopts a circular structure.

[0052] Since the stirring blades 43 provide greater power to the central area, the flow rate of the reaction raw materials in the central area is higher than the flow rate of the edge area (i.e., the area close to the side wall 11 of the reaction chamber) due to natural gravity. Therefore, combined with the flow direction of the reaction raw materials, in the specific embodiment of the present disclosure, reference is made to Figure 3 As shown, the maximum aperture of the degassing hole 52 gradually increases from the center to the edge, so that the reaction raw materials can pass quickly during the circulation process. Optionally, the apertures of multiple degassing holes 52 distributed along the same circumferential direction can be consistent, as long as the radial aperture can be gradually increased.

[0053] Due to the different installation positions and numbers of the debubblers 5, the area ratio of the central debubbling zone 511 and the edge debubbling zone 512 of each debubbler 5 will be different. Therefore, in the specific embodiment of the present disclosure, the area ratio of the central debubbling zone 511 and the edge debubbling zone 512 is between 1:1-2:3.

[0054] Specifically, in a specific embodiment of the present disclosure, a plurality of debubblers 5 are arranged in the reaction chamber 1 at intervals along the vertical direction, and the area of ​​the central debubbling zone 511 of the plurality of debubblers 5 gradually decreases from top to bottom. Figure 1 As shown, two debubblers 5 are arranged in the reaction chamber 1 to form a two-stage debubbler, that is, the two debubblers 5 can be divided into a primary debubbler 501 and a secondary debubbler 502 according to the different distances from the stirring blades 43. Among them, the primary debubbler 501 is arranged close to the stirring blades 43, and the thrust is relatively concentrated, so the area of ​​the central debubbler zone 511 can be smaller, while the secondary debubbler 502 is relatively far from the stirring blades 43, and the thrust is relatively dispersed, so the area of ​​the central debubbler zone 511 is relatively enlarged, and optionally, the area of ​​the central debubbler zone 511 and the edge debubbler zone 512 of the primary debubbler 501 can be 2:3, and the area of ​​the central debubbler zone 511 and the edge debubbler zone 512 of the secondary debubbler 502 can be 1:1.

[0055] Of course, in other embodiments, one or more stages of debubblers can be provided according to the size of the reaction chamber 1, and different area ratios can be set for each stage of debubbler according to different installation positions, as long as effective debubbling can be achieved.

[0056] In the specific embodiments of the present disclosure, reference is made to Figure 1 As shown, a fixing table 10 is provided inside the reaction chamber 1 corresponding to each debubbler 5, and a maintenance hook 9 is provided on the top wall 12 of the reaction chamber 1. When the debubbler 5 is clogged by coking, it is necessary to manually enter the reaction chamber for maintenance, and the maintenance hook 9 can be used to flush and clean the debubbler.

[0057] Further, in a specific embodiment of the present disclosure, the stirring device 4 includes a stirring controller 41, a stirring shaft 42 and a plurality of stirring blades 43, wherein the stirring shaft 42 is connected between the stirring controller 41 and the plurality of stirring blades 43, and the plurality of stirring blades 43 are evenly distributed along the circumference of the stirring shaft 42, and the stirring surface 431 of each stirring blade 43 is configured as a gradually downwardly inclined arc surface along the rotation direction. Specifically, referring to Fig. 9As shown (the direction of the arrow is the direction of rotation), the stirring surface 431 is constructed as a cambered surface along the direction of rotation, that is, the angle between the tangent of the stirring surface 431 and the horizontal line is gradually reduced along the direction of rotation. Optionally, the above-mentioned angle can be transitioned from 15° to 45°, so as to reduce the resistance from the reaction raw materials when the stirring blade rotates, so that more reaction raw materials can move on the stirring surface 431 of the stirring blade 43, and then with the rotation, the reaction raw materials can be further promoted to flow upward in a spiral, increasing the mixing strength of air and ethylene tar. Of course, in other embodiments, the stirring surface 431 can also be an inclined surface extending downwardly along the direction of rotation or an inflection surface with a corner (i.e., having two inclined surfaces, the angle of the inclined surface close to the bottom is smaller), etc., as long as the reaction raw materials can be promoted to flow upward.

[0058] In addition, in order to facilitate installation and maintenance, in the specific embodiments of the present disclosure, reference is made to Figure 1 As shown, there is a certain gap between the stirring blade 43 and the side wall 11. Optionally, the reaction chamber 1 is constructed as a cylinder, and the ratio of the size of a single stirring blade 43 projected onto the bottom wall 13 to the size of the radius of the reaction chamber 1 can be 6:7.

[0059] Optionally, refer to Figure 1 As shown, the stirring shaft 42 can be arranged below the stirring blade 41. In other embodiments, in order to prevent the stirring shaft 42 from coking, the stirring shaft 42 can also be arranged above the stirring blade 43 until the top wall 12 of the reactor 1, and the stirring controller 41 is placed on the upper part of the top wall 12. This disclosure does not limit this.

[0060] In the specific embodiments of the present disclosure, reference is made to Figure 1 As shown, the discharge end 21 of the feed pipe 2 is arranged inside the reaction chamber 1 and faces downward, the feed end of the feed pipe 2 is arranged outside the reaction chamber 1 and is provided with a shut-off valve 22, and the feed pipe 2 is connected to the ethylene tar raw material pipe 20 and the purge superheated steam pipe 6 respectively through the shut-off valve 22.

[0061] In this way, after the feeding is completed, the shut-off valve 22 can be closed, the valve cavity can be purged with superheated steam, and at the same time, the ethylene tar raw material in the pipeline after the valve can be completely purged into the interior of the reaction chamber 1, so as to effectively prevent the coking of the ethylene tar raw material remaining in the valve body and the feed pipe 2, thereby avoiding clogging of the pipeline; at the same time, when the reactor reaction is completed and the coated asphalt f is discharged, superheated steam can be used to warm the pipes and purge the coated asphalt remaining in the reaction chamber 1, thereby cleaning the interior of the reaction chamber.

[0062] refer to Figure 6As shown, in a specific embodiment of the present disclosure, the air injector 3 includes an injection pipe 31 , which has a plurality of injection holes 32 spaced apart along its length, and one side of the injection pipe 31 is closed and the other side is connected to the air pipe 30 .

[0063] Furthermore, in order to prevent the ethylene tar raw material from entering the air injector 3 after the air injection is stopped, in the specific embodiment of the present disclosure, the injection hole 32 is constructed as a semi-through hole opening downward, so that the ethylene tar raw material can be effectively prevented from entering the injection hole 32 and blocking the air injector 3. Figure 7 (arrows indicate the direction of airflow), in a specific embodiment of the present disclosure, the aperture of the semi-through hole gradually decreases from bottom to top to facilitate the rapid circulation of air.

[0064] In addition, in the specific embodiments of the present disclosure, reference is made to Figure 1 As shown, one side of the injection pipe 31 is connected to the stripping superheated steam pipe 7. Optionally, the stripping superheated steam pipe 7 is connected to the air injector 3 in parallel with the air pipe 30. The control system can automatically control the switching of the air pipe 30 and the stripping superheated steam pipe 7 according to the reaction progress of the coated asphalt reactor. Specifically, after the oxidation reaction is completed, the control system is responsible for cutting off the air pipe 30 and opening the stripping superheated steam pipe 7. The liquid oil remaining after the oxidation reaction is quickly gasified by the superheated steam so that it can be discharged with the reaction tail gas, further cleaning the coated asphalt reactor provided by the present disclosure.

[0065] In order to further avoid coking of the reaction raw materials, as an implementation method, an inserted thermocouple temperature measurement system can also be set inside the reaction chamber 1 to detect the temperature distribution inside the reaction chamber during operation to prevent the problem of raw material coking caused by local high temperature.

[0066] At the same time, considering that in the long-term reaction process, problems such as coking and clogging of the debubbler 5 or blade failure of the stirring blade 43 may occur, reference Figure 1 As shown, optionally, inspection manholes 8 are respectively provided above and below the side wall 11 of the reaction chamber 1, so that after a failure occurs, maintenance can be carried out by opening the inspection manholes 8 after safe cleaning.

[0067] The preferred embodiments of the present disclosure are described in detail above in conjunction with the accompanying drawings; however, the present disclosure is not limited to the specific details in the above embodiments. Within the technical concept of the present disclosure, a variety of simple modifications can be made to the technical solution of the present disclosure, and these simple modifications all fall within the protection scope of the present disclosure.

[0068] It should also be noted that the various specific technical features described in the above specific embodiments can be combined in any suitable manner without contradiction. In order to avoid unnecessary repetition, the present disclosure will not further describe various possible combinations.

[0069] In addition, various embodiments of the present disclosure may be arbitrarily combined, and as long as they do not violate the concept of the present disclosure, they should also be regarded as the contents disclosed by the present disclosure.

Claims

1. A coated asphalt reactor, characterized in that: include: A reaction chamber (1), wherein a feed pipe (2) for introducing ethylene tar raw material is arranged above the reaction chamber (1), an air injector (3) for introducing air is arranged below the reaction chamber (1), and an exhaust port is arranged on the top wall (12) of the reaction chamber (1), and a discharge port is arranged on the bottom wall (13); A stirring device (4), the stirring device (4) comprising a stirring blade (43), the stirring blade (43) being arranged inside the reaction chamber (1) and below the air injector (3); A debubbler (5) is arranged inside the reaction chamber (1) and located between the air injector (3) and the feed pipe (2).

2. The coated asphalt reactor according to claim 1, characterized in that: The debubble device (5) comprises a debubble body (51), the debubble body (51) being provided with a plurality of debubble holes (52) spaced apart along the circumferential direction and the radial direction and having a central debubble zone (511) and an edge debubble zone (512), wherein the openings of the debubble holes (52) in the central debubble zone (511) gradually decrease from top to bottom, and the openings of the debubble holes (52) in the edge debubble zone (512) gradually decrease from bottom to top.

3. The coated asphalt reactor according to claim 2, characterized in that: The maximum pore diameter of the degassing holes (52) gradually increases from the center toward the edge.

4. The coated asphalt reactor according to claim 2, characterized in that: The area ratio of the central debubble zone (511) to the edge debubble zone (512) is between 1:1 and 2:

3.

5. The coated asphalt reactor according to any one of claims 2 to 4, characterized in that: A plurality of debubblers (5) are arranged in the reaction chamber (1) at intervals along the up-down direction, and the area of ​​the central debubbling zone (511) of the plurality of debubblers (5) gradually decreases from top to bottom.

6. The coated asphalt reactor according to any one of claims 1 to 4, characterized in that: The stirring device (4) comprises a stirring controller (41), a stirring shaft (42) and a plurality of stirring blades (43); the stirring shaft (42) is connected between the stirring controller (41) and the plurality of stirring blades (43); the plurality of stirring blades (43) are evenly distributed along the circumference of the stirring shaft (42); and a stirring surface (431) of each stirring blade (43) is constructed as a curved surface that gradually tilts downward along the direction of rotation.

7. The coated asphalt reactor according to claim 1, characterized in that: The discharge end (21) of the feed pipe (2) is arranged inside the reaction chamber (1) and faces downward, the feed end of the feed pipe (2) is arranged outside the reaction chamber (1) and is provided with a shut-off valve (22), and the feed pipe (2) is connected to the ethylene tar feed pipe (20) and the purge superheated steam pipe (6) respectively through the shut-off valve (22).

8. The coated asphalt reactor according to claim 1, characterized in that: The air injector (3) comprises an injection pipe (31), wherein the injection pipe (31) is provided with a plurality of injection holes (32) arranged at intervals along its length direction, and one side of the injection pipe (31) is closed, and the other side is connected to the air pipe (30).

9. The coated asphalt reactor according to claim 8, characterized in that: The injection hole (32) is configured as a semi-through hole opening downward.

10. The coated asphalt reactor according to claim 8, characterized in that: One side of the injection pipe (31) is in communication with the stripping superheated steam pipe (7).

Citation Information

Cited By

  • Stirring method for coated asphalt reactor

    CN121775792A