Cold casting system

By using a shunt seat and a stepped cooling ingot die in the cold casting system, combined with a vibration mechanism, the problems of low production efficiency and unstable finished product quality in the cold casting system are solved, and efficient cooling and uniform finished product quality are achieved.

CN118926492APending Publication Date: 2024-11-12XINJIANG TBEA LOULAN NEW MATERIAL TECH CO LTD
View PDF 0 Cites 0 Cited by

Patent Information

Application Number
CN202411033020.9
Authority / Receiving Office
CN · China
Patent Type
Applications(China)
Current Assignee / Owner
Filing Date
2024-07-30
Publication Date
2024-11-12

AI Technical Summary

Technical Problem

The existing cold casting system has low production efficiency, resulting in low output, increasing labor intensity and cost, and long cooling time leads to component segregation of the silicon liquid during cooling and solidification, affecting the stability and uniformity of the finished product quality.

Method used

A cold casting system is designed, including a support table, a shunt seat, a cooling ingot die and a vibration mechanism. The shunt seat is used to divert the casting liquid. The flow guide surface of the cooling ingot die is stepped. The vibration mechanism drives the vibration of the cooling ingot die to reduce the vibration of the Cooling time and breaking the casting liquid.

Benefits of technology

It improves the cooling efficiency of the casting liquid, prevents component segregation, improves the stability and uniformity of the finished product quality, reduces manual crushing process, and improves production efficiency and output.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure CN118926492A_ABST
    Figure CN118926492A_ABST
Patent Text Reader

Abstract

The invention discloses a cold casting system, and relates to the technical field of smelting equipment. The cold casting system comprises a supporting table, a flow dividing base, a cooling ingot mold and a vibration mechanism, the flow dividing base, the cooling ingot mold and the vibration mechanism are installed on the supporting table, and the flow dividing base is used for containing casting liquid and provided with a plurality of flow dividing openings used for guiding the casting liquid. A feeding end and a discharging end are formed at the two ends of the cooling ingot mold respectively, a flow guide face is formed at the top of the cooling ingot mold and is arranged in a step face mode with the height decreasing in sequence in the direction from the feeding end to the discharging end, the feeding end communicates with the multiple flow dividing openings, and the flow guide face is used for guiding casting liquid entering the feeding end to the discharging end. The cooling ingot mold is used for cooling the casting liquid flowing through the flow guide surface, so that the casting liquid forms blocky solids; and the vibration mechanism is used for driving the cooling ingot mold to vibrate to crush and disperse blocky solids. The device has the advantages of being high in production efficiency, improving the product yield, reducing the labor intensity and the cost, being short in cooling time, and improving the stability and the uniformity of the quality of a finished product.
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] The invention relates to the technical field of smelting equipment, and in particular to a cold casting system. Background Art

[0002] In the process of smelting industrial raw materials, such as smelting industrial silicon, the cooling ingot mold in the cold casting system currently used is a cast iron ingot mold. The molten metal silicon enters the cooling ingot mold from the silicon bag along the chute. After cooling, it needs to be manually crushed and packaged for storage. The production efficiency is low, resulting in low output, and increased labor intensity and cost. Moreover, generally a silicon ingot needs to be cooled for more than 24 hours before the subsequent process can be carried out. The cooling time is long, and it takes about 7 times to lift from the completion of casting in the cooling ingot mold to packaging and storage. In addition, due to the long cooling time, the silicon liquid will undergo component segregation during the cooling and solidification process, resulting in uneven distribution of silicon impurity element content, which seriously affects the stability and uniformity of the finished product quality. Summary of the invention

[0003] The main purpose of the present invention is to propose a cold casting system, which aims to solve the technical problems of low production efficiency of existing cold casting systems, resulting in low output, increased labor intensity and cost, and long cooling time, which seriously affects the stability and uniformity of the quality of the finished product.

[0004] To achieve the above object, the present invention provides a cold casting system, which includes a support platform and:

[0005] A diverter seat, the diverter seat is used to hold the casting liquid, and the diverter seat is provided with a plurality of diverter ports for guiding the casting liquid;

[0006] A cooling ingot mold, wherein two ends of the cooling ingot mold respectively form a feed end and a discharge end, and a guide surface is formed on the top of the cooling ingot mold, and the guide surface is arranged in a step-like manner with decreasing heights in a direction from the feed end to the discharge end, and the feed end is connected to a plurality of the diversion ports, and the guide surface is used to guide the casting liquid entering the feed end to the discharge end, and the cooling ingot mold is used to cool the casting liquid flowing through the guide surface, so that the casting liquid forms a block solid;

[0007] A vibration mechanism is used to drive the cooling ingot mold to vibrate so as to break and disperse the block solid.

[0008] In one embodiment, the vibration mechanism is located at the bottom of the cooling ingot mold, and the vibration mechanism includes a vibration module, and the vibration module includes a driving component, a transmission component and a pushing member, the pushing member is vertically arranged, and the driving component is installed on the support platform, the driving component is connected to one end of the transmission component, and the other end of the transmission component is elastically connected to the lower end of the pushing member, and the upper end of the pushing member is connected to the bottom of the cooling ingot mold, and the driving component is used to drive the transmission component to drive the pushing member to reciprocate and rise and fall, so as to drive the cooling ingot mold to vibrate up and down.

[0009] In one embodiment, the transmission assembly includes a connecting block and a guide column, the guide column is vertically arranged, and the driving assembly is connected to the lower end of the guide column through the connecting block. The guide column is provided with an installation cavity, and the pushing member is a pushing rod. The lower end of the pushing rod extends into the installation cavity and slides with the cavity wall of the installation cavity, and the upper end of the pushing rod extends out of the installation cavity from the upper end of the guide column and is connected to the bottom of the cooling ingot mold. An elastic member is provided in the installation cavity, and the upper and lower ends of the elastic member are respectively abutted against the cavity wall of the installation cavity and the lower end of the pushing rod. The driving assembly is used to drive the guide column to reciprocate and rise and fall through the connecting block, so as to drive the pushing rod to reciprocate and rise and fall through the elastic member.

[0010] In one embodiment, it also includes a transmission seat, which includes a sleeve and a top plate arranged on the top of the sleeve, the bottom of the sleeve is open, and a sliding cavity connected to the opening is formed in the sleeve, the upper end of the guide column extends from the opening into the sliding cavity and slides with the inner wall of the sleeve, the upper end of the push rod is located in the sliding cavity and connected to the top plate, and the top plate is connected to the bottom of the cooling ingot mold.

[0011] In one embodiment, the vibration mechanism also includes a first support plate, a second support plate and a buffer module, the buffer module includes an elastic mounting column and a buffer spring, the first support plate is installed on the support platform, the driving assembly is installed on the first support plate, the second support plate is located above the first support plate, and the top of the second support plate is connected to the cooling ingot mold, the bottom of the second support plate is connected to the top plate, the first support plate and the second support plate are connected by the elastic mounting column, the buffer spring is arranged on the outer sleeve of the elastic mounting column, and the upper and lower ends of the buffer spring are respectively abutted against the second support plate and the first support plate.

[0012] In one embodiment, the driving assembly includes a rotating driving member and a cam, the rotating driving member is installed on the support platform, the output shaft of the rotating driving member extends in a horizontal direction and is connected to the cam, the outer edge of the cam is connected to the bottom of the connecting block, and the top of the connecting block is connected to the lower end of the guide column, and the rotating driving member is used to drive the cam to rotate around the output shaft to drive the connecting block and the guide column to reciprocate and rise and fall through the outer edge of the cam.

[0013] In one embodiment, the cold casting system further comprises a material shifting mechanism, the material shifting mechanism is located at the discharge end, the material shifting mechanism comprises a roller shaft and a support seat, the support seat is mounted on the support platform, the roller shaft is horizontally arranged along a direction perpendicular to the feed end to the discharge end, and the roller shaft is rotatably mounted on the support platform and is located above the guide surface, a plurality of paddles are arranged on the periphery of the roller shaft, and the plurality of paddles are driven to rotate by driving the roller shaft to rotate, so that the plurality of paddles shift the block solid to the direction of the discharge end;

[0014] and / or,

[0015] The cold casting system further comprises a tilting mechanism, which is mounted on the support platform and arranged close to the diverter seat, and is used to pour the casting liquid into the diverter seat.

[0016] In one embodiment, the diverter seat includes a seat body and an overflow groove, a guide groove and a diverter groove all installed on the seat body, the seat body is installed on the support platform, the overflow groove and the diverter groove are connected through the guide groove, the overflow groove is used to hold the casting liquid, and a plurality of diverter plates are arranged at intervals at the bottom of the diverter groove to divide the diverter groove into a plurality of diverter paths, and the diverter port is formed at one end of each diverter path away from the guide groove.

[0017] In one embodiment, the end of the overflow groove away from the guide groove forms a feed end, and the end where the diversion port is located is a discharge end. The size of the guide groove is gradually expanded from the feed end toward the discharge end, and the size of the diversion groove is gradually expanded from the feed end toward the discharge end. The bottom of the overflow groove, the bottom of the guide groove and the bottom of the diversion groove form a flow surface, and the flow surface is an arc-shaped surface with a decreasing height from the feed end to the discharge end.

[0018] In one embodiment, there are multiple cooling ingot molds, and the multiple cooling ingot molds are arranged in sequence from the feed end to the discharge end, and the multiple guide surfaces are arranged in steps with decreasing heights in sequence from the feed end to the discharge end;

[0019] In any two adjacent cooling ingot molds, the discharge end of one of the cooling ingot molds is connected to the feed end of the other cooling ingot mold, and the feed end of the cooling ingot mold arranged near the diverter seat is located below the plurality of diverter ports and is connected to the plurality of diverter ports;

[0020] Each of the cooling ingot molds is correspondingly provided with a vibration mechanism, and the vibration mechanism is used to drive the corresponding cooling ingot mold to vibrate.

[0021] In the technical solution of the present invention, a diverter seat, a cooling ingot mold and a vibration mechanism are installed on the support table. The diverter seat is used to hold the casting liquid, and the diverter seat is provided with a plurality of diverter ports for guiding the casting liquid. Diverting the casting liquid can not only speed up the flow speed, but also evenly cast the casting liquid onto the cooling ingot mold, thereby avoiding local overheating of the cooling ingot mold and burn-through damage.

[0022] The two ends of the cooling ingot mold respectively form a feed end and a discharge end, and the top of the cooling ingot mold forms a guide surface, which is arranged in a step-like manner with a gradually decreasing height from the feed end to the discharge end. The casting liquid entering from the feed end is guided from the guide surface to the discharge end. During the flow of the casting liquid, the cooling ingot mold can cool it. The guide surface is arranged in a step-like manner with a gradually decreasing height from the feed end to the discharge end, which is conducive to the rapid flow of the casting liquid, thereby reducing the cooling time of the casting liquid.

[0023] Moreover, the vibration mechanism can drive the cooling ingot mold to vibrate, further speeding up the flow rate of the casting liquid on the guide surface and reducing the cooling time of the casting liquid. In addition, the cooling ingot mold can also cool the casting liquid flowing through the guide surface into block solids, and under the action of vibration, the block solids are broken and dispersed and transferred to the discharge end.

[0024] The cold casting system of the present invention is provided with a diverter seat on a support platform, and a plurality of diverter ports are provided on the diverter seat to divert the casting liquid, and a cooling ingot mold is provided. The guide surface on the cooling ingot mold is a stepped surface, which can accelerate the cooling of the casting liquid, thereby reducing the cooling time of the casting liquid, preventing the casting liquid from component segregation during the solidification process, making it difficult to introduce impurities into the cooling ingot mold, and improving the stability and uniformity of the finished product quality. In addition, the cold casting system can drive the cooling ingot mold to vibrate by providing a vibration mechanism to break and disperse the block solid, without the need for a manual crushing process, and has the advantages of high production efficiency and increased product output, and reduces manual labor intensity and costs. BRIEF DESCRIPTION OF THE DRAWINGS

[0025] In order to more clearly illustrate the embodiments of the present invention or the technical solutions in the prior art, the drawings required for use in the embodiments or the description of the prior art will be briefly introduced below. Obviously, the drawings described below are only some embodiments of the present invention. For ordinary technicians in this field, other drawings can be obtained based on the structures shown in these drawings without paying creative work.

[0026] Figure 1 It is a front cross-sectional schematic diagram of a cold casting system according to an embodiment of the present invention;

[0027] Figure 2 for Figure 1 A magnified view of middle;

[0028] Figure 3 A top partial cross-sectional view of a cold casting system according to an embodiment of the present invention;

[0029] Figure 4 It is a schematic cross-sectional view of a vibration mechanism in a cold casting system according to an embodiment of the present invention;

[0030] Figure 5 A schematic diagram of the installation position of a rotating driving member of a vibration mechanism in a cold casting system according to an embodiment of the present invention;

[0031] Figure 6 It is a structural schematic diagram of a vibration module in a cold casting system according to an embodiment of the present invention;

[0032] Figure 7 It is a front cross-sectional view of a manifold seat in a cold casting system according to an embodiment of the present invention;

[0033] Figure 8 A top cross-sectional view of a manifold seat in a cold casting system according to an embodiment of the present invention;

[0034] Fig. 9 It is a side cross-sectional view of a manifold seat in a cold casting system according to an embodiment of the present invention.

[0035] Description of Figure Numbers:

[0036] 100, cold casting system; 10, support platform; 20, diverter seat; 21, overflow trough; 22, guide trough; 23, diverter trough; 231, diverter plate; 232, diverter port; 24, seat body; 30, cooling ingot mold; 301, feed end; 302, discharge end; 31, cooling hole; 32, guide surface; 40, vibration mechanism; 40a, vibration module; 41, drive assembly; 411, rotary drive member; 412, cam; 42, transmission assembly; 421, connecting block; 422, guide column; 4221, mounting cavity; 423, transmission seat; 4231 , sleeve; 4232, top plate; 4233, sliding cavity; 424, elastic member; 43, push member; 43a, push rod; 44, buffer module; 441, elastic mounting column; 442, buffer spring; 45, first support plate; 46, second support plate; 50, material shifting mechanism; 51, roller; 52, support seat; 53, shifting piece; 60, tipping mechanism; 61, liquid storage barrel; 62, first hydraulic rod; 63, second hydraulic rod; 64, V-shaped support frame; 641, first support rod; 642, second support rod; 65, installation clamp; 70, fire-resistant layer.

[0037] The realization of the purpose, functional features and advantages of the present invention will be further explained in conjunction with embodiments and with reference to the accompanying drawings. DETAILED DESCRIPTION

[0038] The following will be combined with the drawings in the embodiments of the present invention to clearly and completely describe the technical solutions in the embodiments of the present invention. Obviously, the described embodiments are only part of the embodiments of the present invention, not all of the embodiments. Based on the embodiments of the present invention, all other embodiments obtained by ordinary technicians in this field without creative work are within the scope of protection of the present invention.

[0039] It should be noted that if the embodiments of the present invention involve directional indications (such as up, down, left, right, front, back, etc.), the directional indications are only used to explain the relative position relationship, movement status, etc. between the components under a certain specific posture (as shown in the accompanying drawings). If the specific posture changes, the directional indication will also change accordingly.

[0040] In addition, if there are descriptions involving "first", "second", etc. in the embodiments of the present invention, the descriptions of "first", "second", etc. are only used for descriptive purposes and cannot be understood as indicating or suggesting their relative importance or implicitly indicating the number of the indicated technical features. Therefore, the features defined as "first" and "second" may explicitly or implicitly include at least one of the features. In addition, the technical solutions between the various embodiments can be combined with each other, but they must be based on the ability of ordinary technicians in the field to implement them. When the combination of technical solutions is contradictory or cannot be implemented, it should be deemed that such a combination of technical solutions does not exist and is not within the scope of protection required by the present invention.

[0041] In the process of smelting industrial raw materials, such as smelting industrial silicon, the cooling ingot mold in the cold casting system currently used is a cast iron ingot mold. The molten metal silicon enters the cooling ingot mold from the silicon bag along the chute. After cooling, it needs to be manually crushed and packaged for storage. The production efficiency is low, resulting in low output, and increased labor intensity and cost. Moreover, generally a silicon ingot needs to be cooled for more than 24 hours before the subsequent process can be carried out. The cooling time is long, and it takes about 7 times to lift from the completion of casting in the cooling ingot mold to packaging and storage. In addition, due to the long cooling time, the silicon liquid will undergo component segregation during the cooling and solidification process, resulting in uneven distribution of silicon impurity element content, which seriously affects the stability and uniformity of the finished product quality.

[0042] In order to solve the above problems, the present invention provides a cold casting system 100 .

[0043] like Figures 1 to 3 As shown, in one embodiment, the cold casting system 100 includes a support platform 10 and a diverter seat 20, a cooling ingot mold 30 and a vibration mechanism 40 installed on the support platform 10, the diverter seat 20 is used to hold the casting liquid, and the diverter seat 20 is provided with a plurality of diverter ports 232 for guiding the casting liquid; the two ends of the cooling ingot mold 30 respectively form a feed end 301 and a discharge end 302, and the top of the cooling ingot mold 30 forms a guide surface 32, and the guide surface 32 is arranged in a step-like manner with decreasing heights along the direction from the feed end 301 to the discharge end 302, the feed end 301 is connected to the plurality of diverter ports 232, the guide surface 32 is used to guide the casting liquid entering the feed end 301 to the discharge end 302, and the cooling ingot mold 30 is used to cool the casting liquid flowing through the guide surface 32, so that the casting liquid forms a block solid; the vibration mechanism 40 is used to drive the cooling ingot mold 30 to vibrate, so that the block solid is broken and dispersed.

[0044] The cold casting system 100 of the present invention can be used for smelting industrial raw materials, such as smelting industrial silicon, and accordingly, the casting liquid can be silicon liquid. The cold casting system 100 of this embodiment is described by taking the use of smelting industrial silicon as an example.

[0045] In one embodiment of the present invention, referring to Figure 1A diverter seat 20, a cooling ingot mold 30 and a vibration mechanism 40 are installed on the support platform 10. The diverter seat 20 is used to hold the casting liquid, and the diverter seat 20 is provided with a plurality of diverter ports 232 for diverting the casting liquid. Diverting the casting liquid can not only speed up the flow speed, but also evenly transport the casting liquid to the guide surface 32 of the cooling ingot mold 30, thereby avoiding local overheating and burn-through damage of the cooling ingot mold 30.

[0046] like Figure 1 As shown, the left end of the cooling ingot mold 30 is the feed end 301, and the right end is the discharge end 302. A guide surface 32 is formed on the top of the cooling ingot mold 30. The casting liquid entering from the left end is guided from the guide surface 32 to the right end. During the flow of the casting liquid, the cooling ingot mold 30 can cool it. The guide surface 32 is arranged in a stepped surface with a height gradually decreasing from the left end to the right end, which is conducive to the rapid flow of the casting liquid, thereby reducing the cooling time of the casting liquid.

[0047] Moreover, the vibration mechanism 40 can drive the cooling ingot mold 30 to vibrate, further speeding up the flow speed of the casting liquid on the guide surface 32 and reducing the cooling time of the casting liquid. In addition, the cooling ingot mold 30 can also cool the casting liquid flowing through the guide surface 32 into a block solid, and under the action of vibration, the block solid is broken and dispersed and transferred to the right end.

[0048] The cold casting system 100 of the present invention is provided with a diverter seat 20 on the support platform 10, and a plurality of diverter ports 232 are provided on the diverter seat 20 to divert the casting liquid, and a cooling ingot mold 30 is provided. The guide surface 32 on the cooling ingot mold 30 is a stepped surface, which can accelerate the cooling of the casting liquid, thereby reducing the cooling time of the casting liquid, preventing the casting liquid from component segregation during the solidification process, making it difficult to introduce impurities into the cooling ingot mold 30, and improving the stability and uniformity of the finished product quality. In addition, the cold casting system 100 can drive the cooling ingot mold 30 to vibrate by providing a vibration mechanism 40 to break and disperse the block solid, without the need for a manual crushing process, and has the advantages of high production efficiency and increased product output, and reduces manual labor intensity and cost.

[0049] In the existing process of smelting industrial silicon, the cooling ingot mold 30 uses a cast iron ingot mold. Fe, Al, and Ca are the main impurity elements in metallic silicon. Among them, Al and Ca elements can be mostly removed by oxygen blowing refining, but there is currently no means to remove Fe, which is introduced from the raw materials or the production process. The molten metal silicon will corrode the cast iron ingot mold at high temperature, and bring the iron elements in the cast iron ingot mold into the finished product, which will affect the product quality and cause the loss of the cast iron ingot mold. One ton of industrial silicon will corrode about 1kg of the ingot mold. In the cold casting system 100 of this embodiment, the cooling ingot mold 30 uses a copper mold, which is not only low in cost, but also not easy to introduce copper impurities into the casting liquid, and will not corrode the copper mold.

[0050] In one embodiment, the vibration mechanism 40 is located at the bottom of the cooling ingot mold 30, and the vibration mechanism 40 includes a vibration module. The vibration module 40a includes a driving component 41, a transmission component 42 and a push piece 43. The push piece 43 is vertically arranged, and the driving component 41 is installed on the support platform 10. The driving component 41 is connected to one end of the transmission component 42, and the other end of the transmission component 42 is elastically connected to the lower end of the push piece 43. The upper end of the push piece 43 is connected to the bottom of the cooling ingot mold 30. The driving component 41 is used to drive the transmission component 42 to drive the push piece 43 to reciprocate and rise and fall, so as to drive the cooling ingot mold 30 to vibrate up and down.

[0051] like Figures 4 to 5 As shown, the driving assembly 41 of the vibration module 40a can drive the transmission assembly 42 to drive the push piece 43 to move up and down. Specifically, one end of the transmission assembly 42 is elastically connected to the lower end of the push piece 43, and the upper end of the push piece 43 is connected to the cooling ingot mold 30. Therefore, during the up and down movement of the push piece 43, the cooling ingot mold 30 can be driven to vibrate up and down, so as to achieve the process of crushing and dispersing the block solid by the up and down vibration. Moreover, since the cooling ingot mold 30 can vibrate up and down, the flow speed of the casting liquid can be further accelerated, the cooling time can be reduced, and the component segregation of the casting liquid during solidification can be reduced.

[0052] Furthermore, in order to avoid the rigid connection between the transmission component 42 and the push piece 43, which would cause the impact force on the cooling ingot mold 30 to be too high and thus cause unstable vibration of the cooling ingot mold 30, the present embodiment adopts a method of elastically connecting one end of the transmission component 42 with the lower end of the push piece 43 to reduce the impact force on the cooling ingot mold 30 and improve the vibration stability of the cooling ingot mold 30.

[0053] Furthermore, if Figure 4 As shown, there are multiple vibration modules 40a, and the multiple vibration modules 40a are evenly distributed at intervals. By setting up multiple vibration modules 40a, the power source for the up and down vibration of the cooling ingot mold 30 is improved, thereby ensuring the vibration reliability and stability of the cooling ingot mold 30.

[0054] In one embodiment, the transmission assembly 42 includes a connecting block 421 and a guide column 422, the guide column 422 is vertically arranged, the driving assembly 41 is connected to the lower end of the guide column 422 through the connecting block 421, a mounting cavity 4221 is provided in the guide column 422, the pushing member 43 is a pushing rod 43a, the lower end of the pushing rod 43a extends into the mounting cavity 4221 and slides with the cavity wall of the mounting cavity 4221, the upper end of the pushing rod 43a extends out of the mounting cavity 4221 from the upper end of the guide column 422 and is connected to the bottom of the cooling ingot mold 30, an elastic member 424 is provided in the mounting cavity 4221, the upper and lower ends of the elastic member 424 are respectively abutted against the cavity wall of the mounting cavity 4221 and the lower end of the pushing rod 43a, the driving assembly 41 is used to drive the guide column 422 to reciprocate and rise and fall through the connecting block 421, so as to drive the pushing rod 43a to reciprocate and rise and fall through the elastic member 424.

[0055] like Figure 6 As shown, the driving assembly 41 drives the guide column 422 to move up and down through the connecting block 42, and the installation cavity 4221 provided in the guide column 422 is slidably matched with the push rod 43a, so as to guide the push rod 43a through the guide column 422. When the driving assembly 41 drives the guide column 422 to move upward through the connecting block 421, the elastic member 424 can drive the push rod 43a to move upward stably, and when the driving assembly 41 drives the guide column 422 to move downward through the connecting block 421, the elastic member 424 can drive the push rod 43a to move downward stably, thereby ensuring the stability of the push rod 43a during the upward and downward movement.

[0056] Specifically, the elastic member 424 can be a spring sleeved on the push rod 43a. The push rod 43a can guide and limit the spring, which is beneficial for the stable expansion and contraction of the spring. The spring has the advantages of good elasticity, low cost and easy material acquisition.

[0057] In one embodiment, the transmission assembly 42 also includes a transmission seat 423, the transmission seat 423 includes a sleeve 4231 and a top plate 4232 arranged on the top of the sleeve 4231, the bottom of the sleeve 4231 is open, and a sliding cavity 4233 connected to the opening is formed in the sleeve 4231, the upper end of the guide column 422 extends from the opening into the sliding cavity 4233 and slides with the inner wall of the sleeve 4231, the upper end of the push rod 43a is located in the sliding cavity 4233 and is connected to the top plate 4232, and the top plate 4232 is connected to the bottom of the cooling ingot mold 30.

[0058] like Figure 6 As shown, the sliding cavity 4233 provided in the sleeve 4231 is slidably matched with the upper end of the guide column 422, so as to guide the guide column 422 through the sleeve 4231. The top plate 4232 provided on the top of the sleeve 4231 can increase the contact area with the cooling ingot mold 30 and improve the vibration stability of the cooling ingot mold 30.

[0059] In one embodiment, the vibration mechanism 40 also includes a first support plate 45, a second support plate 46 and a buffer module 44, the buffer module 44 includes an elastic mounting column 441 and a buffer spring 442, the first support plate 45 is installed on the support platform 10, the first support plate 45 is installed with a driving assembly 41, the second support plate 46 is located above the first support plate 45, and the top of the second support plate 46 is connected to the cooling ingot mold 30, the bottom of the second support plate 46 is connected to the top plate 4232, the first support plate 45 and the second support plate 46 are connected by an elastic mounting column 441, the elastic mounting column 441 is outerly provided with a buffer spring 442, and the upper and lower ends of the buffer spring 442 are respectively abutted against the second support plate 46 and the first support plate 45.

[0060] like Figure 4 As shown, the top of the second support plate 46 is connected to the cooling ingot mold 30, which provides stable support for the cooling ingot mold 30, increases the contact area with the cooling ingot mold 30, and improves the vibration stability of the cooling ingot mold 30. The elastic mounting column 441 and the buffer spring 442 are arranged between the first support plate 45 and the second support plate 46. The elastic mounting column 441 and the buffer spring 442 can be elastically deformed during the up and down vibration of the vibration mechanism 40, which has a buffering effect, reduces the impact force on the cooling ingot mold 30, and improves the vibration stability of the cooling ingot mold 30.

[0061] Furthermore, the first support plate 45 and the second support plate 46 are both rectangular, and the first support plate 45 and the second support plate 46 are arranged in parallel, and the bottom of the cooling ingot mold 30 is also configured as a plane matching the second support plate 46, which is convenient for assembly and can improve the vibration stability of the cooling ingot mold 30.

[0062] like Figure 1 As shown, the number of buffer modules 44 can be multiple, which can enhance the buffering effect on the cooling ingot mold 30 and further improve the vibration stability of the cooling ingot mold 30. In one embodiment, for example, the number of buffer modules 44 is five, of which four buffer modules 44 are distributed at the four corners of the space surrounded by the first support plate 45 and the second support plate 46, and the remaining buffer module 44 is arranged in the middle of the space, and the layout is reasonable.

[0063] In one embodiment, the driving assembly 41 includes a rotating driving member 411 and a cam 412. The rotating driving member 411 is installed on the support platform 10. The output shaft of the rotating driving member 411 extends in the horizontal direction and is connected to the cam 412. The outer edge of the cam 412 is connected to the bottom of the connecting block 421. The top of the connecting block 421 is connected to the lower end of the guide column 422. The rotating driving member 411 is used to drive the cam 412 to rotate around the output shaft, so as to drive the connecting block 421 and the guide column 422 to reciprocate and rise and fall through the outer edge of the cam 412.

[0064] like Figure 6 As shown, the rotary drive member 411 drives the cam 412 to rotate through the output shaft, and the outer edge of the cam 412 drives the connecting block 421 and the guide column 422 to move up and down. In this embodiment, the driving assembly 41 adopts the method of the rotary drive member 411 driving the cam 412 to realize the up and down movement of the guide column 422, which simplifies the structure of the driving assembly 41 and facilitates manufacturing.

[0065] Furthermore, the rotary drive member 411 may be a servo motor, a stepper motor, an asynchronous motor, or a rotary hydraulic cylinder, which has a simple structure and is easy to install.

[0066] In one embodiment, the cold casting system 100 also includes a material shifting mechanism 50, which is located at the discharge end 302. The material shifting mechanism 50 includes a roller 51 and a support seat 52. The support seat 52 is installed on the support platform 10. The roller 51 is horizontally arranged in a direction perpendicular to the feed end 301 to the discharge end 302, and the roller 51 is rotatably installed on the support platform 10 and is located above the guide surface 32. A plurality of paddles 53 are provided on the outer periphery of the roller 51. The plurality of paddles 53 are driven to rotate by driving the roller 51 to rotate, so that the plurality of paddles 53 shift the block solid to the direction of the discharge end 302.

[0067] like Figure 1 As shown, the material-shifting mechanism 50 is installed at the right end near the cooling ingot mold 30, that is, at the discharge end 302 of the cooling ingot mold 30. By driving the roller 51 in the material-shifting mechanism 50 to rotate, since a plurality of paddles 53 are provided on the roller 51, the plurality of paddles 53 can shift the block solid toward the right end, which is convenient for quickly collecting the block solid and has high working efficiency.

[0068] It should be noted that the driving method of the roller shaft 51 in this embodiment can be flexibly set, and the roller shaft 51 can be driven manually or driven by a motor to rotate, which saves time and effort. When the roller shaft 51 is driven by a motor, the motor can be set on the support seat 52, and the structure is compact.

[0069] like Figure 3 As shown, a plurality of paddle groups are arranged at intervals along the circumferential direction on the roller shaft 51, and each paddle group includes a plurality of paddles 53 arranged at intervals along the axial direction of the roller shaft 51. By providing a plurality of paddle groups, the efficiency of collecting bulk solids can be further improved and time can be saved.

[0070] In one embodiment, a collection frame may be provided below the guide surface 32 at the discharge end 302 of the cooling ingot mold 30 to collect the block solids.

[0071] In one embodiment, the cold casting system 100 further includes a tilting mechanism 60 , which is installed on the support platform 10 and disposed close to the manifold seat 20 . The tilting mechanism 60 is used to pour the casting liquid into the manifold seat 20 .

[0072] like Figure 2 As shown, the tipping mechanism 60 includes a liquid storage barrel 61, a first hydraulic rod 62 and a second hydraulic rod 63, a support frame 64 and a mounting clamp 65. The mounting clamp 65 is fixedly sleeved on the outer peripheral wall of the liquid storage barrel 61. The two ends of the support frame 64 are respectively a first hinged end and a second hinged end. The first hinged end is hinged to one side of the mounting clamp 65 through a first hinge axis, and the second hinged end is hinged to the support platform 10 through a second hinge axis. The first hydraulic rod 62 is installed on the support platform 10. The hydraulic end of the first hydraulic rod 62 is hinged to the support frame 64 at a position between the first hinged end and the second hinged end. One end of the second hydraulic rod 63 is hinged to the support platform 10, and the other end is hinged to the mounting clamp 65.

[0073] The liquid storage barrel 61 can store casting liquid, and a casting port is formed at one end of the liquid storage barrel 61. When casting is required, the first hydraulic rod 62 extends upward to drive the support frame 64 to rotate counterclockwise, so that the liquid storage barrel 61 moves from the initial position to the preset position, and then the second hydraulic cylinder 63 extends to rotate the mounting hoop 65 and the liquid storage barrel 61 around the first hinge axis, so that the liquid storage barrel 61 rotates from the vertical state to the tilting state, so that the casting liquid in the liquid storage barrel 61 is tilted from the casting port to the diverter seat 20, so that the tilting mechanism 60 is set to realize the pouring process of the casting liquid, which saves time and effort and is easy to operate.

[0074] It can be understood that the dumping state is an inclined state or a horizontal state or a state close to the horizontal state, and it is sufficient to dump the casting liquid in the liquid storage barrel 61 from the casting port into the diverter seat 20 .

[0075] Furthermore, the V-shaped support frame 64 specifically includes a first support rod 641 and a second support rod 642, one end of the first support rod 641 and one end of the second support rod 642 are connected, and the connection between one end of the first support rod 641 and one end of the second support rod 642 is hinged to one side of the mounting clamp 65 through a first hinge axis, that is, one end of the first support rod 641 and one end of the second support rod 642 form a first hinge end, and the other end of the first support rod 641 is hinged to the support platform 10 through a second hinge axis, that is, the other end of the first support rod 641 is the second hinge end, and a first hydraulic rod 62 is installed on the support platform 10, and the hydraulic end of the first hydraulic rod 62 is hinged to the first support rod 641 at a position between one end and the other end of the first support rod 641, and the other end of the second support rod 642 can be supported on the support platform 10 as a supporting end, so as to play a supporting role when the liquid storage barrel 61 pours the casting liquid, thereby ensuring the stability of the liquid storage barrel 61 during the pouring process.

[0076] In one embodiment, a refractory layer 70 is provided on the upper surface of the support platform 10 near the tipping mechanism 60 and the diverter seat 20 to prevent damage to the support platform 10 . The material of the refractory layer 70 is not limited.

[0077] In one embodiment, the diverter seat 20 includes a seat body 24 and an overflow groove 21, a guide groove 22 and a diverter groove 23 all installed on the seat body. The seat body 24 is installed on the support platform 10. The overflow groove 21 and the diverter groove 23 are connected through the guide groove 22. The overflow groove 21 is used to hold the casting liquid. A plurality of diverter plates 231 are arranged at intervals at the bottom of the diverter groove 23 to divide the diverter groove 23 into a plurality of diverter paths. A diverter port 232 is formed at one end of each diverter path away from the guide groove 22.

[0078] like Figures 7 to 9 As shown, the overflow trough 21 is used to hold the casting liquid, which can prevent the casting liquid from overflowing the diverter seat 20 during casting. Two diverter plates 231 are arranged at intervals at the bottom of the diverter trough 23 to divide the diverter trough 23 into two diverter paths. Each diverter path forms a diverter port 232 at one end away from the guide trough 22. The diverter port 232 can divert the flow, speed up the flow rate of the casting liquid, reduce the cooling time, and evenly cast the casting liquid onto the cooling ingot mold 30, thereby avoiding local overheating and burn-through damage of the cooling ingot mold 30.

[0079] Furthermore, the material of the diverter seat 20 can be made of alumina. When the casting liquid is silicon liquid, the impurities in the silicon liquid contain Al and Ca impurities, and the freezing point of Al and Ca impurities is higher than that of silicon liquid, so that the Al and Ca impurities can first solidify in the diverter seat 20 to form impurity bodies, and the impurity bodies are easy to deposit on the bottom of the overflow groove 21, the guide groove 22 and the diverter groove 23, so that most of the Al and Ca impurities can be removed in the diverter seat 20, thereby improving product quality, and no subsequent manual finishing process is required, further accelerating production efficiency.

[0080] Furthermore, one end of the diverter plate 231 close to the guide groove 22 is configured to be in an arc shape to facilitate flow diversion and improve the diverter effect.

[0081] In one embodiment, the end of the overflow groove 21 away from the guide groove 22 forms a feed end, and the end where the diverter port 232 is located is a discharge end. The size of the guide groove 22 is gradually expanded from the feed end toward the discharge end, and the size of the diverter groove 23 is gradually expanded from the feed end toward the discharge end. The bottom of the overflow groove 21, the bottom of the guide groove 22 and the bottom of the diverter groove 23 form a flow surface, and the flow surface is an arc-shaped surface with a decreasing height from the feed end to the discharge end.

[0082] like Figure 8As shown, the left end of the overflow trough 21 is the feeding end, and the right end where the diverter port 232 is located is the discharging end. The size of the guide trough 22, specifically the size of the cross section, is gradually expanded from the left end to the direction close to the right end, that is, the size of the guide trough 22 in the front-to-back direction gradually increases to the right, which plays a role in buffering, slowing down and draining the casting liquid in the guide trough 22. The size of the diverter trough 23, specifically the size of the cross section, is gradually expanded from the left end to the direction close to the right end, that is, the size of the diverter trough 23 in the front-to-back direction gradually increases to the right, which plays a role in buffering, slowing down and draining the casting liquid in the diverter trough 23. The bottom of the overflow trough 21, the bottom of the guide trough 22 and the bottom of the diverter trough 23 form a flow surface, and the flow surface is an arc surface with a decreasing height from the left end to the right end, which facilitates the smoothness of the flow of the casting liquid and accelerates the flow speed of the casting liquid.

[0083] In one embodiment, there are multiple cooling ingot molds 30, and the multiple cooling ingot molds 30 are arranged in sequence from the feed end 301 to the discharge end 302, and the multiple guide surfaces 32 are arranged in steps with decreasing heights from the feed end 301 to the discharge end 302; among any two adjacent cooling ingot molds 30, the discharge end 302 of one cooling ingot mold 30 is connected to the feed end 301 of the other cooling ingot mold 30, and the feed end 301 of the cooling ingot mold 30 arranged near the diverter seat 20 is located below the multiple diverter ports 232 and is connected to the multiple diverter ports 232; each cooling ingot mold 30 is correspondingly provided with a vibration mechanism 40, and the vibration mechanism 40 is used to drive the corresponding cooling ingot mold 30 to vibrate.

[0084] like Figure 1 As shown, multiple cooling ingot molds 30 are arranged in sequence from the left end to the right end, and multiple guide surfaces 32 corresponding to each cooling ingot mold 30 are arranged in steps with gradually decreasing heights from the left end to the right end, thereby accelerating the flow rate of the casting liquid and reducing the cooling time.

[0085] Taking the case where there are three cooling ingot molds 30 as an example, the feed end 301 of the cooling ingot mold 30 at the left end is connected to multiple branch ports 232, the discharge end 302 of the cooling ingot mold 30 at the left end is connected to the feed end 301 of the cooling ingot mold 30 at the right end through the middle cooling ingot mold 30, and the discharge end 302 of the cooling ingot mold 30 at the right end is below the roller 51, which facilitates the smoothness and continuity of the flow of the casting liquid.

[0086] Each cooling ingot mold 30 may be provided with a corresponding vibration mechanism 40, which can ensure the stability of the up and down vibration of the cooling ingot mold 30 and facilitate the control of the vibration frequency.

[0087] In other embodiments, a plurality of cooling ingot molds 30 may share one vibration mechanism 40, thereby simplifying the structure and reducing the cost.

[0088] It can be understood that the interiors of the plurality of cooling ingot molds 30 are provided with cooling holes 31 for installing cold water pipelines, and the cooling holes 31 are located below the guide surface 32 and arranged close to the guide surface 32. Specifically, each cooling ingot mold 30 is provided with cooling holes 31 at positions below each step of the guide surface 32, and cooling water circulates in the cold water pipeline to promote rapid solidification of the casting liquid, further reduce the cooling time, and prevent the casting liquid from having uneven distribution of impurity elements due to component segregation, which affects the quality of the product.

[0089] The above are only preferred embodiments of the present invention, and are not intended to limit the patent scope of the present invention. All equivalent structural changes made using the contents of the present invention's specification and drawings, or directly / indirectly applied in other related technical fields, are included in the patent protection scope of the present invention.

Claims

1. A cold casting system, It is characterized in that The cold casting system comprises a support platform and: A diverter seat, the diverter seat is used to hold the casting liquid, and the diverter seat is provided with a plurality of diverter ports for guiding the casting liquid; A cooling ingot mold, wherein two ends of the cooling ingot mold respectively form a feed end and a discharge end, and a guide surface is formed on the top of the cooling ingot mold, and the guide surface is arranged in a step-like manner with decreasing heights in a direction from the feed end to the discharge end, and the feed end is connected to a plurality of the diversion ports, and the guide surface is used to guide the casting liquid entering the feed end to the discharge end, and the cooling ingot mold is used to cool the casting liquid flowing through the guide surface, so that the casting liquid forms a block solid; A vibration mechanism is used to drive the cooling ingot mold to vibrate so as to break and disperse the block solid.

2. The cold casting system according to claim 1, It is characterized in that The vibration mechanism is located at the bottom of the cooling ingot mold, and the vibration mechanism includes a vibration module, and the vibration module includes a driving component, a transmission component and a pushing member. The pushing member is vertically arranged, and the driving component is installed on the support platform. The driving component is connected to one end of the transmission component, and the other end of the transmission component is elastically connected to the lower end of the pushing member, and the upper end of the pushing member is connected to the bottom of the cooling ingot mold. The driving component is used to drive the transmission component to drive the pushing member to reciprocate and rise and fall, so as to drive the cooling ingot mold to vibrate up and down.

3. The cold casting system according to claim 2, It is characterized in that The transmission assembly includes a connecting block and a guide column, the guide column is vertically arranged, the driving assembly is connected to the lower end of the guide column through the connecting block, the guide column is provided with an installation cavity, the pushing member is a pushing rod, the lower end of the pushing rod extends into the installation cavity and slides with the cavity wall of the installation cavity, the upper end of the pushing rod extends out of the installation cavity from the upper end of the guide column and is connected to the bottom of the cooling ingot mold, an elastic member is provided in the installation cavity, the upper and lower ends of the elastic member are respectively abutted against the cavity wall of the installation cavity and the lower end of the pushing rod, the driving assembly is used to drive the guide column to reciprocate and rise and fall through the connecting block, so as to drive the pushing rod to reciprocate and rise and fall through the elastic member.

4. The cold casting system according to claim 3, It is characterized in that The transmission assembly also includes a transmission seat, which includes a sleeve and a top plate arranged on the top of the sleeve. The bottom of the sleeve is open, and a sliding cavity connected to the opening is formed in the sleeve. The upper end of the guide column extends from the opening into the sliding cavity and slides with the inner wall of the sleeve. The upper end of the push rod is located in the sliding cavity and connected to the top plate, and the top plate is connected to the bottom of the cooling ingot mold.

5. The cold casting system according to claim 4, It is characterized in that The vibration mechanism also includes a first support plate, a second support plate and a buffer module, the buffer module includes an elastic mounting column and a buffer spring, the first support plate is mounted on the support platform, the driving assembly is mounted on the first support plate, the second support plate is located above the first support plate, and the top of the second support plate is connected to the cooling ingot mold, the bottom of the second support plate is connected to the top plate, the first support plate and the second support plate are connected by the elastic mounting column, the buffer spring is arranged on the outer sleeve of the elastic mounting column, and the upper and lower ends of the buffer spring are respectively abutted against the second support plate and the first support plate.

6. The cold casting system according to claim 3, It is characterized in that The driving assembly includes a rotating driving member and a cam, the rotating driving member is installed on the support platform, the output shaft of the rotating driving member extends in the horizontal direction and is connected to the cam, the outer edge of the cam is connected to the bottom of the connecting block, and the top of the connecting block is connected to the lower end of the guide column, and the rotating driving member is used to drive the cam to rotate around the output shaft to drive the connecting block and the guide column to reciprocate and rise and fall through the outer edge of the cam.

7. The cold casting system according to any one of claims 1 to 6, It is characterized in that The cold casting system further comprises a material shifting mechanism, which is located at the discharge end. The material shifting mechanism comprises a roller shaft and a support seat, which is mounted on the support platform. The roller shaft is horizontally arranged in a direction perpendicular to the feed end to the discharge end, and the roller shaft is rotatably mounted on the support platform and is located above the guide surface. A plurality of paddles are arranged on the periphery of the roller shaft, and the plurality of paddles are driven to rotate by driving the roller shaft to rotate, so that the plurality of paddles shift the block solid to the direction of the discharge end. and / or, The cold casting system further comprises a tilting mechanism, which is mounted on the support platform and arranged close to the diverter seat, and is used to pour the casting liquid into the diverter seat.

8. The cold casting system according to any one of claims 1 to 6, It is characterized in that The diverter seat includes a seat body and an overflow groove, a guide groove and a diverter groove all installed on the seat body. The seat body is installed on the support platform. The overflow groove and the diverter groove are connected through the guide groove. The overflow groove is used to hold the casting liquid. A plurality of diverter plates are arranged at intervals on the bottom of the diverter groove to divide the diverter groove into a plurality of diverter paths. The diverter port is formed at one end of each diverter path away from the guide groove.

9. The cold casting system according to claim 8, It is characterized in that The end of the overflow groove away from the guide groove forms a feed end, and the end where the diversion port is located is a discharge end. The size of the guide groove is gradually expanded from the feed end toward the discharge end, and the size of the diversion groove is gradually expanded from the feed end toward the discharge end. The bottom of the overflow groove, the bottom of the guide groove and the bottom of the diversion groove form a flow surface, and the flow surface is an arc-shaped surface with a decreasing height from the feed end to the discharge end.

10. The cold casting system according to any one of claims 1 to 6, It is characterized in that There are multiple cooling ingot molds, and the multiple cooling ingot molds are arranged in sequence from the feed end to the discharge end, and the multiple guide surfaces are arranged in steps with decreasing heights in sequence from the feed end to the discharge end; In any two adjacent cooling ingot molds, the discharge end of one of the cooling ingot molds is connected to the feed end of the other cooling ingot mold, and the feed end of the cooling ingot mold arranged near the diverter seat is located below the plurality of diverter ports and is connected to the plurality of diverter ports; Each of the cooling ingot molds is correspondingly provided with a vibration mechanism, and the vibration mechanism is used to drive the corresponding cooling ingot mold to vibrate.