High-transparency super-hydrophobic coating based on inorganic adhesive and preparation method of high-transparency super-hydrophobic coating
Through the combination of inorganic adhesive and nano SiO2 and fluorinating reagent modification treatment, the problem of traditional superhydrophobic coatings being easily aged under high temperature and ultraviolet light is solved, and a highly transparent and durable superhydrophobic coating is achieved, which is suitable for multiple Glass products.
Patent Information
- Application Number
- CN202411161211.3
- Authority / Receiving Office
- CN · China
- Patent Type
- Applications(China)
- Current Assignee / Owner
- Filing Date
- 2024-08-22
- Publication Date
- 2024-11-12
AI Technical Summary
Existing superhydrophobic coatings tend to age under high temperatures and ultraviolet radiation, and the use of traditional organic adhesives has affected material transparency and mechanical stability.
The inorganic adhesive was synthesized with H3PO4 and Al(OH)3 and mixed with nano SiO2, and the coating was formed by spraying, and the surface superhydrophobic modification was performed using fluorinated reagent to enhance the adhesive strength and stability.
It realizes a superhydrophobic coating that is highly transparent, high temperature resistant, ultraviolet resistant and corrosion-resistant, which significantly improves the stability and durability of the coating. It is suitable for architectural glass, photovoltaic solar panels and automotive windshields and other scenarios.
Smart Images

Figure CN118931235A_ABST
Abstract
Description
Technical Field
[0001] The invention belongs to the technical field of super hydrophobic materials, and in particular relates to a highly transparent super hydrophobic coating based on an inorganic adhesive and a preparation method thereof. Background Art
[0002] Products such as architectural glass, photovoltaic solar panels and automobile windshields are easily invaded by pollutants such as dust due to long-term exposure to the external environment. Traditional cleaning methods such as scrubbing and rinsing are not only inefficient, but also consume a lot of manpower and material resources. To solve this problem, a super-hydrophobic coating can be prepared on its surface. Super-hydrophobic coating refers to a special coating with a water contact angle of more than 150° and a rolling angle of less than 5°. Its surface properties are similar to those of lotus leaves, which can effectively resist the attachment of water droplets and carry away surface dust with the water flow.
[0003] At present, it is still challenging to achieve a stable and transparent superhydrophobic surface. This is mainly due to the fact that the construction of a superhydrophobic surface relies on a micro-nano composite structure. Although this structure gives the surface superhydrophobic properties, it also causes significant light scattering, thereby reducing the transparency of the material. Specifically, in order to achieve superhydrophobicity, the substrate surface needs to be roughened. However, increasing the surface roughness may have a significant effect on transparency and mechanical stability. When the surface roughness is too large, especially when it reaches a level sufficient to induce Mie scattering, a significant light scattering surface may be formed, thereby reducing the transparency of the material.
[0004] To overcome this problem, current transparent super-hydrophobic coatings mostly use nanoparticle stacking structures, which have little effect on the scattering of light, but face the limitation of insufficient stability. To enhance the bonding force between the coating and the substrate, adhesives are usually used for reinforcement. As described in patents such as CN118222145A and CN118374200A, the resin adhesives widely used at present, although having good bonding properties, have the disadvantages of being not resistant to high temperature, ultraviolet radiation and being easy to age due to the nature of their organic materials. Summary of the invention
[0005] The purpose of the present invention is to provide a highly transparent super hydrophobic coating based on an inorganic adhesive and a preparation method thereof, so as to solve the technical problems of the existing adhesives mentioned in the above background technology that are not resistant to high temperature, ultraviolet radiation and are easy to age.
[0006] To achieve the above object, the present invention provides the following technical solutions:
[0007] A method for preparing a highly transparent super-hydrophobic coating based on an inorganic adhesive, specifically comprising the following steps:
[0008] S01. Synthesize inorganic adhesive using H3PO4 and Al(OH)3;
[0009] S02. The inorganic binder is mixed with the nano-SiO2 dispersion to form a mixed solution;
[0010] S03. On the cleaned substrate, forming a coating using the mixed solution;
[0011] S04. The coating is heated and cured;
[0012] S05. Using a fluorinated agent to modify the surface of the cured coating to be super-hydrophobic.
[0013] Furthermore, in step S01, the H3PO4 solution is diluted with deionized water to a concentration of 60%, the molar ratio of H3PO4 to Al(OH)3 is 3:1, and it is fully stirred at a constant temperature of 100°C.
[0014] Furthermore, in step S02, the ratio of each substance in the mixed solution is: nano-SiO2: ethanol: inorganic binder: deionized water = 1g: 30ml: 2g: 10ml, and after being mixed evenly, ultrasonic treatment is performed for 15 minutes. The particle size of SiO2 used is less than 100nm.
[0015] Furthermore, in step S03, spraying is preferably used to form the coating, and the coating thickness is controlled by adjusting the spraying time. Other more diverse coating formation methods may be used, including but not limited to scraping and spin coating.
[0016] Furthermore, in step S05, the coating is modified by vapor deposition. The substrate after curing the coating is placed in a vacuum drying oven together with 2 μl of fluorination reagent, and kept warm at 60° C. in a vacuum environment.
[0017] Further, in step S05, the fluorination agent is selected from: perfluorodecyltrichlorosilane, perfluorohexyltrichlorosilane, perfluorooctyltrichlorosilane, perfluorododecyltrichlorosilane, perfluorohexyltrimethoxysilane, perfluorooctyltrimethoxysilane, perfluorodecyltrimethoxysilane, perfluorohexyltriethoxysilane, perfluorooctyltriethoxysilane, and perfluorodecyltriethoxysilane.
[0018] Another object of the present invention is to provide a highly transparent super-hydrophobic coating prepared by the above method.
[0019] Another object of the present invention is to provide a highly transparent super-hydrophobic structure based on an inorganic adhesive, comprising: a substrate; a super-hydrophobic coating located on the substrate, wherein the super-hydrophobic coating is made of an inorganic adhesive and nano-SiO2 and coated on the substrate, and the inorganic adhesive is synthesized by H3PO4 and Al(OH)3.
[0020] The present invention has the following beneficial effects:
[0021] The present invention proposes an innovative method, that is, inorganic adhesives are mixed with nanoparticles, aiming to enhance the bonding strength between nanoparticles, thereby improving the overall stability of super-hydrophobic coatings. Compared with traditionally widely used organic binders, the pure inorganic particle combination method adopted by the present invention shows a series of significant advantages, including but not limited to excellent anti-aging performance, excellent high temperature tolerance and strong corrosion resistance. These characteristics make the present invention have a wider prospect and potential in the application of related fields.
[0022] At the same time, inorganic adhesives (AP adhesives) are easy to prepare, and the raw materials are easily available and cost-effective. In the process of constructing the nanoparticle stacking structure, inorganic adhesives (AP adhesives) are used to form AP / SiO2 nanostructures to enhance the bonding between particles and between particles and the substrate, ensuring the stability and durability of the structure. The coating is prepared using pneumatic spraying technology, which is easy to operate and produces a highly uniform coating. The coating thickness can be controlled by adjusting the spraying time. BRIEF DESCRIPTION OF THE DRAWINGS
[0023] In order to more clearly illustrate the technical solutions of the embodiments of the present invention, the accompanying drawings required for describing the embodiments will be briefly introduced below. Obviously, the accompanying drawings described below are only some embodiments of the present invention. For ordinary technicians in this field, other accompanying drawings can be obtained based on these accompanying drawings without paying creative work.
[0024] Figure 1 This is a schematic diagram of the process for preparing the transparent coating of the present invention;
[0025] Figure 2 For the comparison of light transmittance test results;
[0026] Figure 3 This is a picture of the hydrophobic angle of the coating formed by a 5-second spraying time;
[0027] Figure 4 Comparison of salt spray cycle test results. DETAILED DESCRIPTION
[0028] The following will be combined with the accompanying drawings to clearly and completely describe the technical solutions in the embodiments of the present invention. Obviously, the described embodiments are only part of the embodiments of the present invention, not all of the embodiments. Based on the embodiments of the present invention, all other embodiments obtained by ordinary technicians in this field without creative work are within the scope of protection of the present invention.
[0029] See also Figure 1-4 As shown, a method for preparing a highly transparent super-hydrophobic coating based on an inorganic adhesive specifically comprises the following steps:
[0030] S01. Synthesis of inorganic binder;
[0031] A certain amount of H3PO4 solution was slowly added to deionized water for dilution until its concentration reached 60%, and then Al(OH)3 was added to the diluted phosphoric acid solution, with the molar ratio of H3PO4 to Al(OH)3 being 3:1. The reaction system was placed under constant temperature conditions, set at 100°C, and stirred for 3 hours to promote the full reaction between H3PO4 and Al(OH)3, ensuring that the synthesis process of the inorganic adhesive achieved the best results.
[0032] The synthesis conditions of the adhesive are 100° C. and 3 h, which can be shortened or prolonged appropriately according to specific needs, so that the adhesive can reach different sol states of transparent or translucent.
[0033] S02. Preparation of AP / SiO2 mixed solution;
[0034] Dissolve 1g of nano-SiO2 in 30ml of anhydrous ethanol and disperse evenly to form a nano-SiO2 dispersion; weigh 2g of the inorganic adhesive obtained in step S01 and dissolve it in 10ml of deionized water; mix the two evenly and then ultrasonicate for 15 minutes to form an AP / SiO2 mixed solution. The nano-SiO2 used has a particle size of less than 100nm.
[0035] S03. Coating formation;
[0036] Before the operation, it is necessary to ensure that the substrate glass sheet has been thoroughly cleaned and meets the cleaning standards. Subsequently, a pneumatic spray gun is used for spraying. During the spraying process, the distance between the spray gun and the substrate is controlled to be maintained at about 20 cm to ensure the consistency and uniformity of the spraying effect. By adjusting the length of the spraying time, the thickness of the coating can be effectively controlled to meet different hydrophobicity and transparency requirements.
[0037] Spraying as a means of coating formation can be replaced by other more diverse coating formation methods, including but not limited to scraping and spin coating.
[0038] S04. Heating and curing;
[0039] The substrate after spray coating was placed on a heating table and cured at 120°C for 120 min and at 240°C for 60 min.
[0040] S05. Surface superhydrophobic modification.
[0041] The coating was modified by vapor deposition method, and the substrate after curing of the coating was placed in a vacuum drying oven together with 2 μl of fluorination reagent, evacuated to a vacuum environment of -0.1 MPa, the temperature was set to 60°C, and kept warm for 2 hours.
[0042] The fluorination agent in this step is selected from the following: perfluorodecyltrichlorosilane, perfluorohexyltrichlorosilane, perfluorooctyltrichlorosilane, perfluorododecyltrichlorosilane, perfluorohexyltrimethoxysilane, perfluorooctyltrimethoxysilane, perfluorodecyltrimethoxysilane, perfluorohexyltriethoxysilane, perfluorooctyltriethoxysilane, and perfluorodecyltriethoxysilane.
[0043] In order to test the optimal spraying time, during the implementation of step S03, spraying times of 5 seconds, 10 seconds and 20 seconds were set respectively, and then a detailed test of transparency was carried out. Figure 2 The transmittance test results of the coatings with different spraying times are given (with transparent glass as the base sample). According to the graphical information, the following conclusion can be drawn: As the spraying time increases, the transparency of the coating shows a downward trend. Specifically, when the spraying time is 5 seconds, the transparency of the coating is relatively excellent.
[0044] Through the super-hydrophobicity test, the hydrophobic angle of the coating formed by the present invention in a spraying time of 5 seconds is 151.7°, which has super-hydrophobic properties.
[0045] In addition, in order to deeply study and accurately evaluate the super-hydrophobic properties and stability of the coating of the present invention, a salt spray cycle experiment was carried out. The salt spray cycle experiment is a widely used method that can effectively simulate the corrosion conditions in the real environment and test the stability of the super-hydrophobic performance of the sample under the action of salt spray corrosion. During the experiment, the sample is placed in a specially designed experimental device that can simulate the generation and circulation of salt spray, so that the surface of the sample is constantly exposed to the spray containing salt. By observing and recording the changes in the super-hydrophobic properties of the sample before and after the experiment, the stability and durability of the sample under the influence of corrosion can be more accurately understood. The test results are as follows Figure 4 As shown. The red data line in the figure represents the sample without adding adhesive, and the blue data line represents the sample with adding adhesive. When the spraying time is 5s and 10s, it can be clearly seen that the water contact angle of the sample with added AP adhesive is more stable than that of the sample without adding AP adhesive after two cycles of salt spray; the sample without adding AP adhesive has no superhydrophobicity. When the spraying time is longer, the sample with added AP adhesive is also more stable than the sample without adding AP adhesive.
[0046] The coating of the present invention is specially designed to meet the self-cleaning needs of highly transparent surfaces. It has a wide range of applicability and can be covered on various windshields, glass protection plates, building glass, camera lens glass or screens. This coating uses inorganic aluminum phosphate as the core adhesive to build a stable and lasting bonding system between silica particles and between them and the substrate. Through a simple spraying process, the formation of a super-hydrophobic surface can be easily achieved, showing excellent stability. The surface has significant characteristics and has multiple functions such as waterproof, anti-fog, anti-fouling and anti-corrosion, ensuring that it can perform well in various complex environments.
[0047] The preferred embodiments of the present invention disclosed above are only used to help explain the present invention. The preferred embodiments do not describe all the details in detail, nor do they limit the invention to the specific implementation methods described. Obviously, many modifications and changes can be made according to the content of this specification. This specification selects and specifically describes these embodiments in order to better explain the principles and practical applications of the present invention, so that those skilled in the art can understand and use the present invention well.
Claims
1. A method for preparing a highly transparent super-hydrophobic coating based on an inorganic adhesive, characterized in that: The specific steps include: S01. Synthesize inorganic adhesive using H3PO4 and Al(OH)3; S02. The inorganic binder is mixed with the nano-SiO2 dispersion to form a mixed solution; S03. On the cleaned substrate, forming a coating using the mixed solution; S04. The coating is heated and cured; S05. Using a fluorinated agent to modify the surface of the cured coating to be super-hydrophobic.
2. A method for preparing a highly transparent super hydrophobic coating based on an inorganic adhesive according to claim 1, characterized in that: In step S01, the H3PO4 solution is diluted with deionized water to a concentration of 60%, the molar ratio of H3PO4 to Al(OH)3 is 3:1, and the solution is fully stirred under constant temperature.
3. A method for preparing a highly transparent super hydrophobic coating based on an inorganic adhesive according to claim 2, characterized in that: In step S02, the ratio of each substance in the mixed solution is: nano-SiO2: ethanol: inorganic adhesive: deionized water = 1g: 30ml: 2g: 10ml, and the mixture is evenly mixed and then ultrasonicated.
4. The method for preparing a highly transparent super hydrophobic coating based on an inorganic adhesive according to claim 3, characterized in that: In step S03, spraying is preferably used to form the coating, and the coating thickness is controlled by adjusting the length of the spraying time.
5. A method for preparing a highly transparent super hydrophobic coating based on an inorganic adhesive according to any one of claims 1 to 4, characterized in that: In step S05, the coating is modified by using a vapor deposition method.
6. A method for preparing a highly transparent super hydrophobic coating based on an inorganic adhesive according to any one of claims 1 to 4, characterized in that: In step S05, the fluorination agent is selected from: perfluorodecyltrichlorosilane, perfluorohexyltrichlorosilane, perfluorooctyltrichlorosilane, perfluorododecyltrichlorosilane, perfluorohexyltrimethoxysilane, perfluorooctyltrimethoxysilane, perfluorodecyltrimethoxysilane, perfluorohexyltriethoxysilane, perfluorooctyltriethoxysilane, and perfluorodecyltriethoxysilane.
7. A highly transparent super hydrophobic coating prepared by the preparation method according to any one of claims 1 to 6.
8. A highly transparent super-hydrophobic structure based on an inorganic adhesive, characterized in that: include: substrate; The super hydrophobic coating is located on the substrate, and the super hydrophobic coating is made of an inorganic adhesive and nano-SiO2 and coated on the substrate, and the inorganic adhesive is synthesized by H3PO4 and Al(OH)3.
Citation Information
Patent Citations
Preparation method of wear-resistant super-amphiphobic coating based on titanium dioxide / silica composite nanoparticles
CN110540765A
Inorganic binder reinforced fluoride-free self-repairing super-hydrophobic spray and preparation and use methods thereof
CN113881253A
Preparation method of anti-wax oil coating
CN118374191A
Robust superhydrophobic material and coating
GB201702279D0
Omni-transparent and superhydrophobic coatings assembled from chain-like nanoparticles
WO2017196789A1