Production method of outdoor environment-friendly removable adhesive vehicle body sticker
By using graphene oxide modified nanozirconia and photochromic materials in the production of outdoor environmentally friendly removable glue body patches, the problem of insufficient bubble lines and performance in production is solved, and a high-performance, environmentally friendly and low-cost car film is achieved. Production, and the vehicle film changes color under light to enhance the UV barrier effect.
Patent Information
- Application Number
- CN202310518950.2
- Authority / Receiving Office
- CN · China
- Patent Type
- Applications(China)
- Current Assignee / Owner
- Filing Date
- 2023-05-10
- Publication Date
- 2024-11-12
- Estimated Expiration
- Not applicable · inactive patent
AI Technical Summary
The existing outdoor environmentally friendly removable adhesive body patch production method is prone to bubbles or traces during the production process of TPU composite film, and the calendering effect is poor. At the same time, the traditional solvent-based adhesive is replaced by hot melt adhesives and water-based adhesives, which reduces the interior of the vehicle. VOC emissions, but there is a problem of insufficient performance of environmentally friendly materials.
The graphene oxide modified nanozirconia is used as the key component of environmentally friendly glue. By combining it with the acrylate matrix resin system, the mechanical and mechanical properties of the vehicle film are improved, and the combination of main photochromic materials and auxiliary photochromic materials is achieved. The vehicle film changes color under light and enhances the barrier effect of light intensity and ultraviolet rays.
It improves the mechanical properties of the vehicle membrane and the ultraviolet barrier effect, simplifies the production process, reduces costs, and is environmentally friendly and does not cause pollution to the environment. It has simple construction operation, long service life, low price and wide application range.
Smart Images

Figure HDA0004220171840000011 
Figure HDA0004220171840000021
Abstract
Description
Technical Field
[0001] The invention relates to the technical field of vehicle protective films, and in particular to a method for producing an outdoor environmentally friendly removable adhesive vehicle body sticker. Background Art
[0002] Since its launch, automobile films have gone through three stages: "tea paper", "explosion-proof film" and "sunscreen and heat-insulating film". "Tea paper" is a first-generation product, commonly known as solar film, which is characterized by strong light-shielding and simple installation; its disadvantages are that it is not heat-insulating, easy to fade, and easy to debond. "Explosion-proof film" is a second-generation product. It uses new viscose and thicker film layers to improve the explosion-proof effect, and has certain heat insulation and sunscreen properties. The heat insulation rate is between 20% and 60%, and the ultraviolet light blocking rate is about 80%. "Sunscreen and heat-insulating film" is a third-generation product. Compared with the first two types of automobile films, the ultraviolet blocking rate of this film has been increased to 90% to 100%, and the infrared blocking rate has been increased to about 40% to 95%. The adhesive is more viscous, thereby achieving the effect of reducing the thickness of the film and improving the explosion-proof performance. As the functions of automobile films become stronger and stronger, people begin to focus on the production of environmentally friendly films. Therefore, the present invention provides a production method for outdoor environmentally friendly removable adhesive car body stickers, aiming at the following problems in the prior art: 1. The existing production method of outdoor environmentally friendly removable adhesive body stickers has the problem that bubbles or lines are easily generated when producing TPU composite films, and the calendering effect is not good; 2. The existing production method of outdoor environmentally friendly removable adhesive body stickers, the traditional solvent-based adhesives used for automotive films are gradually replaced by environmentally friendly materials such as hot melt adhesives and water-based adhesives, which greatly reduces the impact of adhesives on VOC emissions in the car. Summary of the invention
[0003] In order to solve the above technical problems, the technical solution adopted by the present invention is: A method for producing an outdoor environmentally friendly removable adhesive vehicle sticker comprises the following steps: S1. Raw material extraction: TPU raw materials are extracted from petroleum, and the petroleum is poured into a reactor. Chemical raw materials are added to the reactor to mix and react with the petroleum, and then the TPU raw materials are filtered out through a filtering device for cooling and cutting into particles. The raw materials for preparing environmentally friendly glue include: butyl acrylate, isooctyl acrylate and acrylic acid, active diluent, tackifying resin, graphene oxide modified nano zirconium oxide and photoinitiator; S2, color treatment: 35% main photochromic material, 62% auxiliary photochromic material and the balance deionized water, the main photochromic material is a silver halide and a condensed ring aromatic compound or a mixture of both, the auxiliary photochromic material is diarylethene; S3, calendering and laminating: The TPU film is calendered and laminated by placing the TPU film on the TPU roller, and then the PET film is prevented on the PET roller. At this time, the active rubber roller and the driven steel roller are calendered to form a car film; S4, film winding: TPU film is wound, and the winding ring is driven by the winding roller to rotate and then wound around the car film. After the winding roller is wound, the linear speed of the winding is controlled to increase.
[0004] The further improvement of the technical solution of the present invention is: S1 TPU film extrusion molding, putting TPU raw material particles into a mixing processing box, adding a permanent antistatic agent, a lubricant, talcum powder, and a matting agent and putting them into a twin-screw extruder in sequence.
[0005] A further improvement of the technical solution of the present invention is that: after a period of time, the TPU material is plasticized and extruded, and the plasticized and extruded TPU material is placed in a rolling device, and a double-roll pressing process is used under the conditions of a die temperature of 185-200°C and a roller temperature of 35-50°C to roll-form the TPU film material to form a TPU film.
[0006] A further improvement of the technical solution of the present invention is that: S1 tackifying resin is selected from several of rosin resin, petroleum resin, coumarone resin, terpene resin, and oil-soluble phenolic formaldehyde, and the tackifying resin is selected from two of rosin resin, petroleum resin, coumarone resin, terpene resin, and oil-soluble phenolic formaldehyde.
[0007] A further improvement of the technical solution of the present invention is that the graphene and concentrated sulfuric acid are mixed uniformly, stirred for 1.5 hours under ice bath conditions, then 10g of potassium permanganate solution is added, stirring is continued for 2.5 hours, 40mL of 35% sulfuric acid is added and allowed to stand for 1.5 hours, the mixed solution is washed until the pH value of the solution is neutral, the mixture obtained by centrifugation and drying is added to 150mL of ethanol aqueous solution containing 3g of silane coupling agent, stirred, centrifuged, washed and dried to obtain graphene oxide modified by silane coupling agent, 15mL of reducing agent ammonia water and ethylenediamine are added, heated to 85°C and refluxed for 5 hours, the product is washed until the pH value is neutral, and graphene oxide modified nano zirconium oxide is obtained after drying.
[0008] The further improvement of the technical solution of the present invention is that: S2 is to mix the silver phosphide and the condensed ring aromatic compound in a ratio of 3:1 to prepare a polyacid deionized water solution, and the prepared diarylethene deionized water solution is added under stirring.
[0009] Due to the adoption of the above technical solution, the present invention has the following technical advances compared with the prior art: The present invention provides a production method of an outdoor environmentally friendly removable adhesive vehicle sticker. Under the joint action of graphene oxide modified nano zirconium oxide, a certain proportion of graphene oxide modified nano zirconium oxide is added to the raw materials of environmentally friendly adhesive for vehicle film, thereby further improving the mechanical and mechanical properties of the system. After oxidation, the number of oxygen-containing functional groups on graphene increases, making the properties more active than graphene. After modification, the silane coupling agent is easier to combine with zirconium oxide powder and play a synergistic role in the acrylic ester matrix resin system. By controlling the selection and proportion of each raw material component, an environmentally friendly adhesive for vehicle film with excellent performance is obtained. In addition, the preparation process of the environmentally friendly adhesive for vehicle film of the present invention is simple and low in cost.
[0010] The invention provides a production method of an outdoor environmentally friendly removable adhesive vehicle sticker. Under the action of color treatment, 35% of the main photochromic material, 62% of the auxiliary photochromic material and the balance of deionized water are added. The main photochromic material is one of silver halide and polycyclic aromatic compound or a mixture of the two, and the auxiliary photochromic material is diarylethene. According to the principle of photochromism, the vehicle film will undergo a color change reaction under light, from colorless to blue, and has a good barrier effect on light intensity and ultraviolet rays. The materials used in this technology are environmentally friendly and reliable, will not cause damage to the ecological environment, and overcome the solid waste pollution caused by the original materials after use. Compared with other methods, this technology has the advantages of no pollution, easy operation, high efficiency, and no corrosion to workpieces. Its greater advantages are simple, easy to operate on site, good fluidity, and easy mechanical construction; simple construction operation, high construction efficiency; long service life of the vehicle film, excellent and reliable performance indicators of the invention; no toxicity of the vehicle film, safe and environmentally friendly; once used, the vehicle film will not affect the performance of the window material, and will not cause secondary pollution to the environment; the invention is low in price and has a wide range of applications. BRIEF DESCRIPTION OF THE DRAWINGS
[0011] Figure 1 A schematic diagram of the raw material extraction structure of a production method of an outdoor environmentally friendly removable adhesive vehicle body sticker of the present invention; Figure 2 It is a structural schematic diagram of the color processing of the present invention. Implementation
[0012] The present invention is further described in detail below in conjunction with embodiments: Example
[0013] like Figure 1-2 As shown, the present invention provides a method for producing an outdoor environmentally friendly removable adhesive vehicle body sticker, comprising the following steps: S1. Raw material extraction: TPU raw materials are extracted from petroleum, and the petroleum is poured into a reactor. Chemical raw materials are added to the reactor to mix and react with the petroleum, and then the TPU raw materials are filtered out through a filtering device for cooling and cutting into particles. The raw materials for preparing environmentally friendly glue include: butyl acrylate, isooctyl acrylate and acrylic acid, active diluent, tackifying resin, graphene oxide modified nano zirconium oxide and photoinitiator; S2, color treatment: 35% main photochromic material, 62% auxiliary photochromic material and the balance deionized water, the main photochromic material is a silver halide and a condensed ring aromatic compound or a mixture of both, the auxiliary photochromic material is diarylethene; S3, calendering and laminating: The TPU film is calendered and laminated by placing the TPU film on the TPU roller, and then the PET film is prevented on the PET roller. At this time, the active rubber roller and the driven steel roller are calendered to form a car film; S4, film winding: TPU film is wound, and the winding ring is driven by the winding roller to rotate and then wound around the car film. After the winding roller is wound, the linear speed of the winding is controlled to increase.
[0014] In this implementation case, according to the principle of photochromism, the car film will change color when exposed to light, from colorless to blue, and has a good barrier effect on light intensity and ultraviolet rays. The materials used in this technology are environmentally friendly and reliable, and will not cause damage to the ecological environment, overcoming the solid waste pollution caused by the original materials after use. Compared with other methods, this technology has the advantages of no pollution, easy operation, high efficiency, and no corrosion to the workpiece. Its greater advantages are simplicity, convenience for on-site operation, good fluidity, and easy mechanical construction; simple construction operation and high construction efficiency; long service life of the car film, and excellent and reliable performance indicators of the invention; no toxic effects of the car film, safe and environmentally friendly; once used, the car film will not affect the performance of the window material and will not cause secondary pollution to the environment; the invention is low-priced and has a wide range of applications. Example
[0015] like Figure 1-2As shown, on the basis of Example 1, the present invention provides a technical solution: preferably, S1TPU film extrusion molding, TPU raw material particles are placed in a mixing and processing box, permanent antistatic agent, lubricant, talcum powder, and matting agent are added and placed in a twin-screw extruder in sequence, and the TPU material is plasticized and extruded after a period of time, and the plasticized and extruded TPU material is placed in a rolling device, and a double-roller pressing process is used under the conditions of a die temperature of 185-200°C and a roller temperature of 35-50°C to roll-form the TPU film material to form a TPU film, S1 tackifying resin is selected from several of rosin resin, petroleum resin, coumarone resin, terpene resin, and oil-soluble phenolic formaldehyde, and the tackifying resin is selected from two of rosin resin, petroleum resin, coumarone resin, terpene resin, and oil-soluble phenolic formaldehyde, and the graphene is mixed evenly with concentrated sulfuric acid, stirred for 1.5h under ice bath conditions, and then 10g of potassium permanganate solution is added, and stirring is continued for 2.5h, and 40mL of 35% sulfuric acid was allowed to stand for 1.5h, and the mixed solution was washed until the pH value of the solution was neutral. The mixture obtained by centrifugation and drying was added to 150mL of ethanol aqueous solution containing 3g of silane coupling agent. After stirring, centrifugal separation, washing and drying, graphene oxide modified by silane coupling agent was obtained. 15mL of reducing agent ammonia water and ethylenediamine were added, and the mixture was heated to 85℃ and refluxed for 5h. The product was washed until the pH value was neutral and dried to obtain graphene oxide modified nano zirconium oxide. S2 was prepared by mixing silver phosphide and condensed ring aromatic compound in a ratio of 3:1 to prepare a polyacid deionized water solution. The prepared diarylethene deionized water solution was added under stirring.
[0016] In this embodiment, a certain proportion of graphene oxide modified nano zirconium oxide is added to the raw materials of the environmentally friendly adhesive for car films, which further improves the mechanical and mechanical properties of the system. After oxidation, the number of oxygen-containing functional groups on graphene increases, making the properties more active than graphene. After modification, the silane coupling agent is easier to combine with zirconium oxide powder and play a synergistic role in the acrylic matrix resin system. By controlling the selection and ratio of each raw material component, an environmentally friendly adhesive for car films with excellent performance is obtained, and the preparation process of the environmentally friendly adhesive for car films of the present invention is simple and low in cost.
[0017] The working principle of the production method of this outdoor environmentally friendly removable adhesive vehicle body sticker is described in detail below.
[0018] like Figure 1-2As shown, TPU raw materials are extracted from petroleum, and the petroleum is poured into a reactor. Chemical raw materials are added to the reactor to mix and react with the petroleum, and then the TPU raw materials are filtered out through a filtering device for cooling and cutting into particles. The raw materials for preparing environmentally friendly glue include: butyl acrylate, isooctyl acrylate and acrylic acid, active diluent, tackifying resin, graphene oxide modified nano zirconium oxide and photoinitiator. The tackifying resin is selected from several of rosin resin, petroleum resin, coumarone resin, terpene resin and oil-soluble phenolic formaldehyde. The tackifying resin is selected from two of rosin resin, petroleum resin, coumarone resin, terpene resin and oil-soluble phenolic formaldehyde. Graphene and concentrated sulfuric acid are evenly mixed, stirred for 1.5 hours under ice bath conditions, and then 10g of potassium permanganate solution is added, and stirring is continued for 2.5 hours. 40mL of The mixture was allowed to stand for 1.5 h with 35% sulfuric acid, and washed until the pH value of the solution was neutral. The mixture obtained by centrifugation and drying was added to 150 mL of ethanol aqueous solution containing 3 g of silane coupling agent. After stirring, centrifugal separation, washing and drying, graphene oxide modified by silane coupling agent was obtained. 15 mL of reducing agent ammonia water and ethylenediamine were added, and the mixture was heated to 85 ° C and refluxed for 5 h. The product was washed until the pH value was neutral and dried to obtain graphene oxide modified nano zirconium oxide. A certain proportion of graphene oxide modified nano zirconium oxide was added to the raw materials of environmentally friendly glue for car film, which further improved the mechanical and mechanical properties of the system. After oxidation, the number of oxygen-containing functional groups on graphene increases, making its properties more active than graphene. After modification, the silane coupling agent is easier to combine with zirconium oxide powder and play a synergistic role in the acrylic ester matrix resin system. By controlling the selection and ratio of each raw material component, an environmentally friendly adhesive for car film with excellent performance is obtained. In addition, the preparation process of the environmentally friendly adhesive for car film of the present invention is simple and the cost is low. The main photochromic material is 35%, the auxiliary photochromic material is 62% and the balance is deionized water. The main photochromic material is one or two of silver halide and polycyclic aromatic compound. The auxiliary photochromic material is diarylethene. Silver phosphide and polycyclic aromatic compounds are mixed in a ratio of 3:1 to prepare a polyacid deionized water solution. The prepared diarylethene deionized water solution is stirred. According to the principle of photochromism, the car film will change color under light, from colorless to blue, and has a good barrier effect on light intensity and ultraviolet rays. The materials used in this technology are environmentally friendly and reliable, and will not cause damage to the ecological environment, overcoming the solid waste pollution caused by the original materials after use. Compared with other methods, this technology has the advantages of no pollution, easy operation, high efficiency, and no corrosion to the workpiece.Its greater advantages are simplicity, convenience for on-site operation, good fluidity, and easy mechanical construction; the construction operation is simple and the construction efficiency is high; the car film has a long service life, and the invention has excellent and reliable performance indicators; the car film has no toxic effects and is safe and environmentally friendly; the car film will not affect the performance of the window material after use, and will not cause secondary pollution to the environment; the invention is low in price and has a wide range of applications. The TPU film is calendered and compounded. The TPU film is placed on the TPU roller, and the PET film is placed on the PET roller. At this time, the car film is formed by calendering the active rubber roller and the driven steel roller. The TPU film is rolled up, and the winding ring is driven by the winding roller to rotate and then wrapped around the car film. After the winding roller is wound, the linear speed of the winding is controlled to increase.
[0019] The above generally describes the present invention in detail, but it is obvious to a person skilled in the art that some modifications or improvements can be made to the present invention. Therefore, modifications or improvements that do not depart from the spirit of the present invention are within the scope of protection of the present invention.
Claims
1. A method for producing an outdoor environmentally friendly removable adhesive vehicle body sticker, The method comprises the following steps, characterized in that: S1. Raw material extraction: TPU raw materials are extracted from petroleum, and the petroleum is poured into a reactor. Chemical raw materials are added to the reactor to mix and react with the petroleum, and then the TPU raw materials are filtered out through a filtering device for cooling and cutting into particles. The raw materials for preparing environmentally friendly glue include: butyl acrylate, isooctyl acrylate and acrylic acid, active diluent, tackifying resin, graphene oxide modified nano zirconium oxide and photoinitiator; S2, color treatment: 35% main photochromic material, 62% auxiliary photochromic material and the balance deionized water, the main photochromic material is a silver halide and a condensed ring aromatic compound or a mixture of both, the auxiliary photochromic material is diarylethene; S3, calendering and laminating: The TPU film is calendered and laminated by placing the TPU film on the TPU roller, and then the PET film is prevented on the PET roller. At this time, the active rubber roller and the driven steel roller are calendered to form a car film; S4, film winding: TPU film is wound, and the winding ring is driven by the winding roller to rotate and then wound around the car film. After the winding roller is wound, the linear speed of the winding is controlled to increase.
2. The method for producing an outdoor environmentally friendly removable adhesive vehicle sticker according to claim 1, characterized in that: S1TPU film extrusion molding, put the TPU raw material particles into the mixing processing box, add permanent antistatic agent, lubricant, talcum powder, matting agent and put them into the twin-screw extruder in turn.
3. The method for producing an outdoor environmentally friendly removable adhesive vehicle sticker according to claim 2, characterized in that: After a period of time, the TPU material is plasticized and extruded, and the plasticized and extruded TPU material is placed in a rolling device. Under the conditions of a die temperature of 185-200°C and a roller temperature of 35-50°C, a double-roller pressing process is used to roll-form the TPU film material to form a TPU film.
4. The method for producing an outdoor environmentally friendly removable adhesive vehicle sticker according to claim 1, characterized in that: S1 tackifying resin is selected from several of rosin resin, petroleum resin, coumarone resin, terpene resin and oil-soluble phenolic formaldehyde, and the tackifying resin is selected from two of rosin resin, petroleum resin, coumarone resin, terpene resin and oil-soluble phenolic formaldehyde.
5. The method for producing an outdoor environmentally friendly removable adhesive vehicle sticker according to claim 4, characterized in that: Graphene and concentrated sulfuric acid were mixed evenly, stirred for 1.5 hours under ice bath conditions, and then 10 g of potassium permanganate solution was added, and stirring was continued for 2.5 hours. 40 mL of 35% sulfuric acid was added and allowed to stand for 1.5 hours. The mixed solution was washed until the pH value of the solution was neutral. The mixture obtained by centrifugation and drying was added to 150 mL of ethanol aqueous solution containing 3 g of silane coupling agent. After stirring, centrifugal separation, washing and drying, graphene oxide modified with silane coupling agent was obtained. 15 mL of reducing agent ammonia water and ethylenediamine were added, and the mixture was heated to 85°C and refluxed for 5 hours. The product was washed until the pH value was neutral, and graphene oxide modified nano zirconium oxide was obtained after drying.
6. The method for producing an outdoor environmentally friendly removable adhesive vehicle sticker according to claim 1, characterized in that: S2: mixing silver phosphide and condensed ring aromatic compound in a ratio of 3:1 to prepare a polyacid deionized water solution, and adding the prepared diarylethene deionized water solution under stirring.