Nonmetal anti-explosion additive as well as preparation method and application thereof

By preparing non-metallic antiknock additives containing o-nitrobenzene, diethyldisulfide, polydimethylsiloxane, and methanol, the problems of poor stability and insignificant octane number improvement in existing technologies have been solved, thereby achieving high octane number and improved antioxidant performance of gasoline.

CN118931613APending Publication Date: 2024-11-12YANGPU AOLI PETROCHEM
View PDF 0 Cites 0 Cited by

Patent Information

Application Number
CN202410780493.9
Authority / Receiving Office
CN · China
Patent Type
Applications(China)
Current Assignee / Owner
Filing Date
2024-06-18
Publication Date
2024-11-12

AI Technical Summary

Technical Problem

Existing non-metallic antiknock agents have poor stability and high cost. When added to gasoline, they accelerate oxidation, do not significantly improve the octane rating, and increase the gum content.

Method used

Non-metallic antiknock additives are prepared by using o-nitrobenzene, diethyl disulfide, polydimethylsiloxane and methanol as raw materials, through ultrasonic treatment and radiation treatment. These additives are used in gasoline to interrupt free radical reactions and improve octane number and antioxidant properties.

Benefits of technology

It significantly increases the octane rating of gasoline, reduces gum content, improves cleanliness and stability, reduces knocking rate, and enhances gasoline quality.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure SMS_1
    Figure SMS_1
  • Figure SMS_2
    Figure SMS_2
  • Figure SMS_3
    Figure SMS_3
Patent Text Reader

Abstract

The invention provides a non-metal anti-explosion additive and a preparation method and application thereof, and the non-metal anti-explosion additive comprises the following raw materials in parts by weight: 10-30 parts of o-nitrobenzene, 20-40 parts of diethyl disulfide, 5-15 parts of polydimethylsiloxane and 30-50 parts of methanol. The four raw materials of the non-metal antiknock agent o-nitrobenzene, diethyl disulfide, polydimethylsiloxane and methanol are compounded and react with free radicals in gasoline, the number of the free radicals is reduced, a chain reaction is interrupted, and the octane number of the gasoline is improved synergistically, so that the antiknock performance of the gasoline is improved, the generation of sediments is inhibited, the colloid content is reduced, and the gasoline quality is improved. The cleanliness of the gasoline is improved, the stability and oxidation resistance of the gasoline are improved, and the quality of the gasoline is improved. Meanwhile, the non-metal antiknock agent reduces the surface tension of the gasoline fuel, reduces spontaneous combustion of the gasoline fuel and reduces the occurrence rate of knocking.
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] The invention relates to the field of gasoline additives, and in particular to a non-metallic anti-knock additive and a preparation method and application thereof. Background Art

[0002] The knock in gasoline engines is largely related to the properties of the fuel. If gasoline is easily oxidized, the peroxide formed is not easy to decompose, and the autoignition point is low, it is easy to cause knock. Knock is the phenomenon of premature self-ignition of the mixture before the normal flame arrives. The occurrence of knock depends on the working conditions of the engine and the chemical composition of the fuel. In order to avoid knock, the compression ratio of the gasoline engine can be reduced, but this will reduce the thermal efficiency of the gasoline engine, increase fuel consumption and automobile exhaust pollutant emissions, which is not feasible from the perspective of economy and environmental protection, and also violates the development law of modern science and technology and automobiles. Therefore, it is only required to improve the anti-knock performance of gasoline to adapt to gasoline engines with higher compression ratios. Therefore, gasoline anti-knock is one of the most important indicators of gasoline quality, usually measured by octane number. Refineries are facing the problem of how to increase the octane number of gasoline to meet the demand for unleaded and high-octane gasoline. Since knock in gasoline engines is a chain reaction, additives can be added to gasoline to interrupt the reaction chain to increase the octane number of gasoline. This is one of the most economical and effective methods at present.

[0003] In recent years, the development and research of gasoline antiknock agents has been moving towards non-metallic antiknock agents. Non-metallic antiknock agents mainly include some ethers, alcohols, esters, etc. Common non-metallic antiknock agents can be classified into four categories: ethers, alcohols, esters and methylene cyclopentadiene, including: aniline and its derivatives (N-alkylaniline, dimethylaniline), olefin polymers and various oxygen-containing organic compounds such as methanol, ethanol, isopropyl ketone, tert-butyl ketone, methyl tert-butyl ether (MTBE), ethyl tert-butyl ether (ETBE), tert-amyl methyl ether (TAME), isobutyl acetate, etc.

[0004] The current non-metallic antiknock agents have the problems of poor stability, high cost, accelerated oxidation of gasoline, increased gum content, and low octane number improvement rate when added to gasoline. Summary of the invention

[0005] In view of this, the present invention proposes a non-metallic anti-explosion additive and a preparation method and application thereof to solve the above problems.

[0006] The technical solution of the present invention is achieved in this way:

[0007] A non-metallic anti-explosion additive comprises the following raw materials in parts by weight: 10-30 parts of o-nitrobenzene, 20-40 parts of diethyl disulfide, 5-15 parts of polydimethylsiloxane, and 30-50 parts of methanol.

[0008] Furthermore, according to weight parts, it includes: 20 parts of o-nitrobenzene, 30 parts of diethyl disulfide, 10 parts of polydimethylsiloxane, and 40 parts of methanol.

[0009] A method for preparing a non-metallic anti-knock additive comprises the following specific steps: weighing parts by weight of o-nitrobenzene, diethyl disulfide and methanol, mixing them, ultrasonically treating them, adding polydimethylsiloxane, continuing ultrasonic stirring, and simultaneously performing radiation treatment to obtain a target anti-knock additive.

[0010] Furthermore, the ultrasonic treatment is carried out at 10-40kHz and 400-500W for 20-30min.

[0011] Furthermore, the ultrasonic stirring is continued for 30-60 minutes.

[0012] Furthermore, the radiation treatment is performed at 40-50 kGy, 5-10 kGy / h for 4-8 min.

[0013] The invention discloses an application of a non-metallic anti-knock additive in gasoline.

[0014] Furthermore, the content of the non-metallic antiknock additive in the gasoline is 1.0%-3.0%.

[0015] Compared with the prior art, the present invention has the following beneficial effects:

[0016] 1. The non-metallic antiknock agent of the present invention is compounded with four raw materials, namely, o-nitrobenzene, diethyl disulfide, polydimethylsiloxane and methanol, which react with free radicals in gasoline, reduce the number of free radicals, interrupt the chain reaction, and synergistically improve the octane number of gasoline, thereby improving the antiknock performance of gasoline, inhibiting the formation of sediments, reducing the colloid content, improving the cleanliness of gasoline, improving the stability and antioxidant performance of gasoline, and improving the quality of gasoline. At the same time, the non-metallic antiknock agent of the present invention reduces the surface tension of gasoline fuel, reduces the spontaneous combustion of gasoline fuel, and reduces the incidence of knock.

[0017] 2. The preparation process of the non-metallic anti-explosion agent of the present invention adopts ultrasonic treatment and radiation-assisted treatment, which can significantly improve the preparation efficiency, improve the performance of the non-metallic anti-explosion agent, and improve the stability and safety of the product. DETAILED DESCRIPTION

[0018] In order to better understand the technical content of the present invention, specific embodiments are provided below to further illustrate the present invention.

[0019] Unless otherwise specified, the experimental methods used in the embodiments of the present invention are all conventional methods.

[0020] Unless otherwise specified, the materials, reagents, etc. used in the embodiments of the present invention can be obtained from commercial sources.

[0021] Example 1

[0022] A non-metallic anti-knock additive, comprising the following raw materials in parts by weight:

[0023] 20 parts of o-nitrobenzene, 30 parts of diethyl disulfide, 10 parts of polydimethylsiloxane, 40 parts of methanol.

[0024] The preparation method of the above non-metallic anti-knock additive comprises the following specific steps:

[0025] Weigh the above-mentioned parts by weight of o-nitrobenzene, diethyl disulfide and methanol, mix them, and ultrasonicate them for 25 minutes at 25kHz and 450W. After adding polydimethylsiloxane, continue ultrasonic stirring for 45 minutes and irradiate them for 6 minutes at 45kGy and 8kGy / h to obtain the target anti-knock additive.

[0026] Example 2

[0027] A non-metallic anti-knock additive, comprising the following raw materials in parts by weight:

[0028] 10 parts of o-nitrobenzene, 20 parts of diethyl disulfide, 5 parts of polydimethylsiloxane, 30 parts of methanol.

[0029] The preparation method of the above non-metallic anti-knock additive comprises the following specific steps:

[0030] Weigh the above-mentioned parts by weight of o-nitrobenzene, diethyl disulfide and methanol, mix them, and ultrasonicate them at 10 kHz and 400 W for 20 minutes. After adding polydimethylsiloxane, continue ultrasonic stirring for 30 minutes and irradiate them at 40 kGy and 5 kGy / h for 4 minutes to obtain the target anti-knock additive.

[0031] Example 3

[0032] A non-metallic anti-knock additive, comprising the following raw materials in parts by weight:

[0033] 30 parts of o-nitrobenzene, 40 parts of diethyl disulfide, 15 parts of polydimethylsiloxane, 50 parts of methanol.

[0034] The preparation method of the above non-metallic anti-knock additive comprises the following specific steps:

[0035] Weigh the above-mentioned parts by weight of o-nitrobenzene, diethyl disulfide and methanol, mix them, and ultrasonicate them for 30 minutes at 40kHz and 500W. After adding polydimethylsiloxane, continue ultrasonic stirring for 60 minutes and irradiate them for 8 minutes at 50kGy and 10kGy / h to obtain the target anti-knock additive.

[0036] Comparative Example 1

[0037] Compared with Example 1, the antiknock additive of this comparative example is different in that this comparative example only includes o-nitrobenzene, diethyl disulfide and polydimethylsiloxane, and the amount of the missing methanol is allocated to other components according to the proportion of each component in Example 1, and the rest is consistent with Example 1.

[0038] A non-metallic anti-knock additive, comprising the following raw materials in parts by weight:

[0039] 33.3 parts of o-nitrobenzene, 50 parts of diethyl disulfide, 16.7 parts of polydimethylsiloxane.

[0040] The preparation method of the above non-metallic anti-knock additive comprises the following specific steps:

[0041] Weigh the above-mentioned o-nitrobenzene and diethyl disulfide in parts by weight, mix them, and ultrasonicate them at 25kHz and 450W for 25 minutes. After adding polydimethylsiloxane, continue ultrasonic stirring for 45 minutes and irradiate them at 45kGy and 8kGy / h for 6 minutes to obtain the target anti-knock additive.

[0042] Comparative Example 2

[0043] Compared with Example 1, the anti-knock additive of this comparative example is different in that this comparative example only includes diethyl disulfide, polydimethylsiloxane and methanol, and the amount of missing o-nitrobenzene is allocated to other components according to the proportion of each component in Example 1, and the rest is consistent with Example 1.

[0044] A non-metallic anti-knock additive, comprising the following raw materials in parts by weight:

[0045] 37.5 parts of diethyl disulfide, 12.5 parts of polydimethylsiloxane, 50 parts of methanol.

[0046] The preparation method of the above non-metallic anti-knock additive comprises the following specific steps:

[0047] The above-mentioned parts by weight of diethyl disulfide and methanol were weighed, mixed, and ultrasonicated for 25 minutes at 25kHz and 450W. After adding polydimethylsiloxane, ultrasonic stirring was continued for 45 minutes, and irradiated for 6 minutes at 45kGy and 8kGy / h to obtain the target anti-knock additive.

[0048] Comparative Example 3

[0049] Compared with Example 1, the anti-knock additive of this comparative example is different in that this comparative example only includes o-nitrobenzene, polydimethylsiloxane and methanol, and the amount of the missing diethyl disulfide is distributed to other components according to the proportion of each component in Example 1, and the rest is consistent with Example 1.

[0050] A non-metallic anti-knock additive, comprising the following raw materials in parts by weight:

[0051] 28.6 parts of o-nitrobenzene, 14.3 parts of polydimethylsiloxane, 57.1 parts of methanol.

[0052] The preparation method of the above non-metallic anti-knock additive comprises the following specific steps:

[0053] Weigh the above-mentioned o-nitrobenzene and methanol in parts by weight, mix them, and ultrasonically stir them for 25 minutes at 25kHz and 450W. After adding polydimethylsiloxane, continue ultrasonic stirring for 45 minutes and irradiate them for 6 minutes at 45kGy and 8kGy / h to obtain the target anti-knock additive.

[0054] Comparative Example 4

[0055] Compared with Example 1, the anti-knock additive of this comparative example is different in that this comparative example only includes o-nitrobenzene, diethyl disulfide and methanol, and the amount of the missing polydimethylsiloxane is distributed to other components according to the proportion of each component in Example 1, and the rest is consistent with Example 1.

[0056] A non-metallic anti-knock additive, comprising the following raw materials in parts by weight:

[0057] 22.2 parts of o-nitrobenzene, 33.3 parts of diethyl disulfide, 44.5 parts of methanol.

[0058] The preparation method of the above non-metallic anti-knock additive comprises the following specific steps:

[0059] The above-mentioned o-nitrobenzene, diethyl disulfide and methanol were weighed and mixed, and ultrasonicated for 70 minutes at 25kHz and 450W, and irradiated for 6 minutes at 45kGy and 8kGy / h to obtain the target anti-knock additive.

[0060] Comparative Example 5

[0061] Compared with Example 1, the anti-knock additive of this comparative example is different in that it lacks ultrasound and radiation treatment, and the rest is consistent with Example 1.

[0062] A method for preparing a non-metallic anti-knock additive, the specific steps comprising:

[0063] Weigh the above-mentioned o-nitrobenzene, diethyl disulfide and methanol in parts by weight, mix and stir for 25 minutes, add polydimethylsiloxane, and continue stirring for 45 minutes to obtain the target anti-knock additive.

[0064] Test Example 1

[0065] The non-metallic antiknock additives prepared in Examples 1-3 and Comparative Examples 1-5 were added to 88# catalytic cracking gasoline to measure the octane number improvement of gasoline. The test results are shown in Table 1.

[0066] Table 1

[0067]

[0068]

[0069] As can be seen from Table 1, the non-metallic antiknock agent prepared in Examples 1-3 of the present invention is added to gasoline (mass ratio 1%-3%), and the octane number can be increased by 5.7-7.8 units. Compared with Comparative Examples 1-3, the composition and ratio of the raw material components of Example 1 form a synergistic effect, and the prepared antiknock agent has a good performance of improving the octane number, and the octane number is improved more as the amount of non-metallic antiknock agent added is larger.

[0070] Test Example 2

[0071] The non-metallic antiknock additive prepared in Example 1 and a commercially available non-metallic antiknock agent (purchased from Binzhou Runxi Bioengineering Co., Ltd.) were added to 88# catalytic cracking gasoline, and the actual colloid and induction period in the gasoline were compared. The results are shown in Table 2.

[0072] Table 2

[0073]

[0074] It can be seen from Table 2 that, compared with commercially available non-metallic antiknock agents, the non-metallic antiknock additive of Example 1 of the present invention can prolong the induction period of gasoline and reduce the actual colloid content, thereby ensuring the quality of gasoline products.

[0075] The above description is only a preferred embodiment of the present invention and is not intended to limit the present invention. Any modifications, equivalent substitutions, improvements, etc. made within the spirit and principles of the present invention should be included in the protection scope of the present invention.

Claims

1. A non-metallic anti-knock additive, characterized in that: The raw materials include the following in parts by weight: 10-30 parts of o-nitrobenzene, 20-40 parts of diethyl disulfide, 5-15 parts of polydimethylsiloxane, and 30-50 parts of methanol.

2. A non-metallic anti-knock additive as claimed in claim 1, characterized in that: Calculated by weight, it includes: 20 parts of o-nitrobenzene, 30 parts of diethyl disulfide, 10 parts of polydimethylsiloxane, and 40 parts of methanol.

3. The method for preparing a non-metallic anti-knock additive according to claim 1, characterized in that: The specific steps include: weighing parts by weight of o-nitrobenzene, diethyl disulfide and methanol, mixing them, ultrasonically treating them, adding polydimethylsiloxane, continuing ultrasonic stirring, and simultaneously performing radiation treatment to obtain the target anti-knock additive.

4. The method for preparing a non-metallic anti-explosion additive as claimed in claim 3, wherein the ultrasonic treatment is performed at 10-40 kHz and 400-500 W for 20-30 min.

5. The method for preparing a non-metallic anti-knock additive according to claim 3, characterized in that: The ultrasonic stirring is continued for 30-60 minutes.

6. The method for preparing a non-metallic anti-knock additive according to claim 3, characterized in that: The radiation treatment is performed at 40-50 kGy and 5-10 kGy / h for 4-8 min.

7. Use of the non-metallic antiknock additive according to claim 1 or 2 in gasoline.

8. The use according to claim 7, characterized in that The content of the non-metallic anti-knock additive in the gasoline is 1.0%-3.0%.