Surface regeneration treatment method and treatment device for plate

Through the method of laser curtain heating, cooling fluid flow impact combined with water drilling impact, the problem of sheet plating removal is solved, efficient sheet regeneration treatment is achieved, and production efficiency is improved.

CN118932451APending Publication Date: 2024-11-12湖北仕上电子科技有限公司
View PDF 0 Cites 0 Cited by

Patent Information

Application Number
CN202411124511.4
Authority / Receiving Office
CN · China
Patent Type
Applications(China)
Current Assignee / Owner
Filing Date
2024-08-16
Publication Date
2024-11-12

AI Technical Summary

Technical Problem

The prior art is difficult to quickly and efficiently remove and regenerate sheet plating, especially when the plating layer is firm and thin, which affects the material regeneration processing efficiency.

Method used

The surface of the sheet is heated and scanned with a coolant stream, and the heated sheet is impacted by a water knife impact, and thermal expansion, contraction and cleaning of the coating are achieved, and then anodized.

Benefits of technology

It greatly improves the efficiency of sheet regeneration treatment, reduces the adhesion of the coating, and improves cleaning efficiency and production efficiency.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure CN118932451A_ABST
    Figure CN118932451A_ABST
Patent Text Reader

Abstract

The invention provides a surface regeneration treatment method and device for a plate. The surface regeneration treatment method for the plate comprises the following steps that the cleaned and dried plate is fixed to a workbench; the surface of the plate is heated and scanned through a laser curtain, the heated plate is impacted through cooling liquid flow along with the scanning track of the laser curtain, and the plate is cleaned; and the cleaned plate is subjected to anodic oxidation treatment, and a regenerated plate is obtained. According to the surface regeneration treatment method for the plate, the surface of the plate to be treated is rapidly heated to the high temperature in a laser heating mode, then rapid cooling and impact are conducted through the cooling liquid, a coating on the surface of the plate cracks under rapid thermal expansion and cold contraction, the adhesive force of the coating on a plate base material is greatly reduced, and the surface regeneration treatment effect is improved. And the cleaning efficiency of the original coating is improved, so that the production efficiency of plate regeneration is greatly improved on the whole.
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] The invention relates to the technical field of material surface treatment, and in particular to a surface regeneration treatment method and a treatment device for a sheet material. Background Art

[0002] In the production operation of equipment renovation, it is often necessary to peel off the coating on the surface of the equipment. This work is often done by water jet scraping, which can easily peel off the coating and recover precious metals at the same time. Compared with grinding with a grinding wheel, the working surface of the water jet is wider and more delicate. However, the coating on the surface of some materials is very firmly connected and the coating is thin. Even with water jet scraping, it is impossible to peel off the coating smoothly, which seriously affects the recycling efficiency of the entire material.

[0003] In fact, component refurbishment can play an important role in the circuit board industry and the solar panel industry. Compared with making a new plate, refurbishing the plate in the component can greatly reduce the production cost and use cost. However, the refurbishment of the plate may face the aforementioned technical problems. How to quickly and efficiently strip the coating and effectively regenerate it is an issue that needs in-depth consideration. Summary of the invention

[0004] Based on this, it is necessary to provide a surface regeneration treatment method and treatment device for sheet material to address at least one of the above-mentioned problems.

[0005] In a first aspect, the present application provides a surface regeneration treatment method for a sheet material, comprising the following steps:

[0006] Fix the cleaned and dried sheet on the workbench;

[0007] Scanning the surface of the sheet material with a laser curtain for heating, and following the scanning track of the laser curtain, impacting the heated sheet material with a cooling liquid flow to clean the sheet material;

[0008] The cleaned sheet material is subjected to anodizing treatment to obtain a regenerated sheet material.

[0009] In certain implementations of the first aspect, in the step of scanning the surface of the sheet material with a laser curtain for heating, the heating temperature of the laser curtain on the surface of the sheet material is 1200-1800°C.

[0010] In combination with the first aspect and the above-mentioned implementations, in certain implementations of the first aspect, in the step of scanning the surface of the sheet material with a laser curtain for heating, the heating layer depth of the laser curtain is 0.03 to 0.2 mm.

[0011] In combination with the first aspect and the above implementations, in some implementations of the first aspect, the step of impacting the heated sheet material with a coolant flow further includes:

[0012] The cooling liquid flows on the sheet material in a linear track to scan the sheet material after being heated by the laser curtain;

[0013] The sheet material after being scanned by the coolant flow is impacted by a water jet.

[0014] In combination with the first aspect and the above-mentioned implementations, in some implementations of the first aspect, the cooling liquid flow is a water flow.

[0015] In combination with the first aspect and the above-mentioned implementations, in certain implementations of the first aspect, the step of cleaning the sheet material includes water washing, alkali washing, acid washing and passivation of the sheet material.

[0016] In a second aspect, the present application provides a surface regeneration treatment device for a sheet material, which is used to perform the surface regeneration treatment method for a sheet material as described in any one of the first aspects of the present application, and comprises a machine head and a workbench, wherein the machine head is arranged above the workbench and can move along the length direction of the workbench;

[0017] The machine head comprises a laser and a water jet, and the laser curtain emitted by the laser is spaced 5 to 10 cm from the water jet.

[0018] In certain implementations of the second aspect, the nose further includes a water jet generator, which is disposed on a side of the water jet away from the laser.

[0019] In combination with the second aspect and the above-mentioned implementations, in some implementations of the second aspect, the water jet is a water jet generator.

[0020] In combination with the second aspect and the above-mentioned implementations, in certain implementations of the second aspect, the water flow of the water jet generator is at an angle of 75° to 85° to the working surface of the workbench.

[0021] The technical solution provided in the embodiments of the present invention brings the following beneficial technical effects:

[0022] The surface regeneration treatment method of the sheet material provided by the present invention uses laser heating to rapidly heat the surface of the sheet material to be treated to a high temperature, and then rapidly cools and impacts it with a coolant, so that the coating on the surface of the sheet material cracks under rapid thermal expansion and contraction, greatly reducing the adhesion of the coating on the sheet material substrate, and improving the cleaning efficiency of the original coating, thereby greatly improving the overall production efficiency of sheet material regeneration.

[0023] Additional aspects and advantages of the present application will be given in subsequent parts and will be understood in detail from the subsequent description or learned through specific implementations of the present invention. BRIEF DESCRIPTION OF THE DRAWINGS

[0024] Figure 1 It is a schematic flow chart of a surface regeneration treatment method of a sheet material in one embodiment of the present invention;

[0025] Figure 2 A schematic diagram of a sheet material surface operation trajectory in one embodiment of the present invention;

[0026] Figure 3 It is a schematic diagram of a process of impacting a heated sheet material with a coolant flow in one embodiment of the present invention;

[0027] Figure 4 It is a schematic structural diagram of a surface regeneration treatment device for a sheet material in one embodiment of the present invention;

[0028] Figure 5 It is a schematic structural diagram of a surface regeneration treatment device for a sheet material in another embodiment of the present invention.

[0029] Description of reference numerals:

[0030] 1000-machine head, 2000-workbench, 10-sheet material;

[0031] 1100-Laser, 1200-Water jet, 1300-Water jet generator. DETAILED DESCRIPTION

[0032] In order to facilitate the understanding of the present invention, the present invention will be described more fully below with reference to the relevant drawings. Possible embodiments of the present invention are shown in the drawings. However, the present invention can be implemented in many different forms and is not limited to the embodiments described herein by the drawings. The embodiments described with reference to the drawings are exemplary and are used to make the understanding of the disclosure of the present invention more thorough and comprehensive, and cannot be interpreted as limiting the present invention. In addition, if the detailed description of the known technology is non-essential technology for the features of the present invention shown, these technical details may be omitted.

[0033] It will be understood by those skilled in the relevant art that, unless otherwise defined, all terms (including technical and scientific terms) used herein have the same meaning as those generally understood by those skilled in the art in the art to which the present invention belongs. It should also be understood that terms such as those defined in common dictionaries should be understood to have meanings consistent with those in the prior art, and will not be interpreted with idealized or overly formal meanings unless specifically defined as herein.

[0034] It will be understood by those skilled in the art that, unless otherwise stated, the singular forms "a", "an", "said" and "the" used herein may also include plural forms. It should be further understood that the term "comprising" used in the specification of the present application refers to the presence of the features, integers, steps, operations, elements and / or components, but does not exclude the presence or addition of one or more other features, integers, steps, operations, elements, components and / or groups thereof. It should be understood that the term "and / or" used herein includes all or any unit and all combinations of one or more associated listed items.

[0035] The technical solution of the present invention and how the technical solution solves the above-mentioned technical problems are described in detail below with specific embodiments.

[0036] In a first aspect, the present application provides a surface regeneration treatment method for a sheet material, such as Figure 1 As shown, the following steps are included:

[0037] S100: Fix the cleaned and dried sheet on the workbench. The sheet with the coating to be cleaned is first subjected to conventional pretreatment, and after simple cleaning to remove the dust or surface dirt that may exist on the sheet, it is fixed on the workbench. The workbench and the cleaning equipment can move relative to each other, either the workbench is fixed and the cleaning equipment is movable, or the workbench is movable and the cleaning equipment is fixed.

[0038] S200: Scan the surface of the sheet material with a laser curtain for heating, and follow the scanning track of the laser curtain to impact the heated sheet material with a cooling liquid flow to clean the sheet material. Figure 2 As shown, the laser curtain irradiates the sheet material to form a narrow rectangle, which moves at a certain speed along the length direction of the sheet material, covering the entire sheet material from beginning to end. If the width of the laser curtain is not enough to cover the width of the sheet material, the position can be repositioned to repeat the heating scan. It should be noted that "following the scanning trajectory of the laser curtain" in S200 means that the cooling liquid flow is immediately subjected to cooling liquid flow impact treatment after the laser heats the surface of the sheet material, ensuring that the sheet material undergoes rapid changes of rapid heating and rapid cooling, so that the surface coating of the sheet material expands rapidly due to high heat, and then contracts rapidly due to cooling, thereby destroying the integrity of the coating and its adhesion to the sheet material substrate, and the surface coating is cleaned off in combination with the flushing of the cooling liquid flow. Specifically, the cooling liquid flow is usually water flow.

[0039] S300: Anodizing the cleaned sheet material to obtain a regenerated sheet material. After the sheet material is cleaned, a regeneration operation of the sheet material is performed and a new surface coating is re-applied.

[0040] The surface regeneration treatment method of the sheet material provided by the present invention uses laser heating to rapidly heat the surface of the sheet material to be treated to a high temperature, and then rapidly cools and impacts it with a coolant, so that the coating on the surface of the sheet material cracks under rapid thermal expansion and contraction, greatly reducing the adhesion of the coating on the sheet material substrate, and improving the cleaning efficiency of the original coating, thereby greatly improving the overall production efficiency of sheet material regeneration.

[0041] In a first implementation of the first aspect of the embodiment, in the step of scanning the surface of the sheet material with a laser curtain for heating, the heating temperature of the laser curtain on the surface of the sheet material is 1200-1800° C. The specific temperature is determined according to the specific type of the sheet material substrate and the basic characteristics of the coating.

[0042] In combination with the first aspect embodiment and the above-mentioned implementation method, in the second implementation method of the first aspect embodiment, in the step of scanning the surface of the sheet material with a laser curtain for heating, the heating layer depth of the laser curtain is 0.03 to 0.2 mm. Similarly, the position of the heating focus of the laser curtain needs to be determined according to the approximate thickness of the coating. The movement rate of the laser curtain relative to the sheet material is 3 to 8 mm / s. A slow movement speed can cope with the situation where the coating is relatively strong and thick, and a fast movement speed can cope with the situation where the coating thickness is relatively small.

[0043] In combination with the first aspect embodiment and the above implementation, in a third implementation of the first aspect embodiment, the step of impacting the heated sheet with a cooling liquid flow in S200 is as follows: Figure 3 As shown, it also includes:

[0044] S210: The coolant flow scans the sheet material after being heated by the laser curtain in a linear trajectory.

[0045] S220: Using a water jet to impact the sheet material after being scanned by the cooling liquid flow.

[0046] In this implementation, the coolant flow only plays a cooling role and does not participate in the work of flushing the coating on the surface of the sheet. The work of flushing the surface coating that is cracked and loosened after extremely hot and rapid cooling is handed over to a special water jet, which can achieve a more thorough and efficient surface coating cleaning effect.

[0047] Specifically, in combination with the embodiment of the first aspect and the above-mentioned implementation method, in the specific implementation method of the embodiment of the first aspect, the step of cleaning the sheet material includes water washing, alkali washing, pickling and passivation of the sheet material. The step of cleaning the sheet material not only includes stripping the surface coating by a coolant flow or a special water jet, but also includes performing corresponding conventional cleaning operations on the sheet material after stripping the surface coating to prepare for subsequent anodizing. The subsequent anodizing can be carried out according to conventional and appropriate processes, and this application will not go into further detail.

[0048] Based on the same technical concept, an embodiment of the second aspect of the present application provides a surface regeneration treatment device for a sheet material, which is used to perform the surface regeneration treatment method for a sheet material as described in any one of the first aspects of the present application, such as Figure 4 As shown, it includes a head 1000 and a workbench 2000, wherein the head 1000 is arranged above the workbench 2000 and can move along the length direction of the workbench 2000;

[0049] The machine head 1000 includes a laser 1100 and a water jet 1200 , and the laser curtain emitted by the laser 1100 and the water stream of the water jet 1200 are spaced 5 to 10 cm apart.

[0050] The laser 1100 and the water jet 1200 can both be mature products in the prior art. The laser 1100 can be a heating machine that can emit a ribbon beam as much as possible, thereby generating a light curtain, forming a light band heating area with a certain length and width on the surface of the sheet 10. The machine head 1000 is movable, which can drive the laser 1100 and the water jet 1200 to move together. The front laser 1100 emits laser to heat the surface of the sheet 10, and the rear water jet 1200 follows up and sprays coolant to cool the surface of the sheet 10 that is still in a high temperature state, thereby causing the surface coating of the sheet 10 to be drastically cooled and cracked under the high temperature state, which is convenient for cleaning.

[0051] Optionally, in a first implementation of the second aspect of the embodiment, as Figure 5 As shown, the machine head 1000 further includes a water jet generator 1300, which is arranged beside the water jet generator 1200 away from the laser 1100. The work of flushing the surface coating that is cracked and loosened after extremely hot and rapid cooling is handed over to a special water jet, which can obtain a more thorough and efficient surface coating cleaning effect. In order, the water jet generator 1300 is arranged at the first position of the machine head 1000, the water jet generator 1200 is arranged at the second position next to it, and the laser 1100 is arranged at the third position next to the water jet generator 1200.

[0052] Specifically, in the second implementation of the second aspect of the embodiment, the water jet 1200 is a water jet generator 1300. The water jet 1200 and the water jet are combined into one, and water itself is a good coolant.

[0053] Optionally, in combination with the second aspect embodiment and the above implementation, in some implementations of the second aspect embodiment, such as Figure 5As shown, the water flow of the water jet generator 1300 is 75° to 85° with the working surface of the workbench 2000. The water jet of the water jet generator 1300 is not perpendicular to the sheet 10 to avoid vertical impact on the sheet 10 and splashing water, which affects the heating of the sheet 10 surface by the laser 1100 on the side. Instead, the water jet of the water jet generator 1300 is tilted with the workbench 2000 so that the water flow of the water jet generator 1300 is away from the laser heating area after impacting the sheet 10.

[0054] Those skilled in the art will appreciate that the various operations, methods, steps, measures, and schemes in the processes discussed in this application may be alternated, altered, combined, or deleted. Further, other steps, measures, and schemes in the various operations, methods, and processes discussed in this application may also be alternated, altered, rearranged, decomposed, combined, or deleted. Further, the steps, measures, and schemes in the prior art that are similar to those disclosed in this application may also be alternated, altered, rearranged, decomposed, combined, or deleted.

[0055] The terms "first" and "second" are used for descriptive purposes only and should not be understood as indicating or implying relative importance or implicitly indicating the number of the indicated technical features. Thus, a feature defined as "first" or "second" may explicitly or implicitly include one or more of the features. In the description of this application, unless otherwise specified, "plurality" means two or more.

[0056] In the description of this application, it should be noted that, unless otherwise clearly specified and limited, the terms "installed", "connected", and "connected" should be understood in a broad sense, for example, it can be a fixed connection, a detachable connection, or an integral connection; it can be a direct connection, or an indirect connection through an intermediate medium, or it can be the internal communication of two components. For ordinary technicians in this field, the specific meanings of the above terms in this application can be understood according to specific circumstances.

[0057] In the description of this specification, specific features, structures, materials or characteristics may be combined in an appropriate manner in any one or more embodiments or examples.

[0058] It should be understood that, although the steps in the flowchart of the accompanying drawings are displayed in sequence as indicated by the arrows, these steps are not necessarily executed in sequence in the order indicated by the arrows. Unless otherwise specified herein, there is no strict order restriction on the execution of these steps, and they can be executed in other orders. Moreover, at least a part of the steps in the flowchart of the accompanying drawings may include multiple sub-steps or multiple stages, and these sub-steps or stages are not necessarily executed at the same time, but can be executed at different times, and their execution order is not necessarily sequential, but can be executed in turn or alternately with other steps or at least a part of the sub-steps or stages of other steps.

[0059] The above description is only a partial implementation method of the present application. It should be pointed out that for ordinary technicians in this technical field, several improvements and modifications can be made without departing from the principles of the present application. These improvements and modifications should also be regarded as the scope of protection of the present application.

Claims

1. A surface regeneration method for sheet material, characterized in that: The steps include: Fix the cleaned and dried sheet on the workbench; Scanning the surface of the sheet material with a laser curtain for heating, and following the scanning track of the laser curtain, impacting the heated sheet material with a cooling liquid flow to clean the sheet material; The cleaned sheet material is subjected to anodizing treatment to obtain a regenerated sheet material.

2. The surface regeneration treatment method of sheet material according to claim 1, characterized in that: In the step of scanning the surface of the sheet material with a laser curtain for heating, the heating temperature of the laser curtain on the surface of the sheet material is 1200-1800°C.

3. The surface regeneration treatment method of sheet material according to claim 1, characterized in that: In the step of scanning the surface of the sheet material with a laser curtain for heating, the heating layer depth of the laser curtain is 0.03-0.2 mm.

4. The surface regeneration treatment method of sheet material according to claim 1, characterized in that: The step of impacting the heated sheet material with a cooling liquid flow also includes: The cooling liquid flows on the sheet material in a linear track to scan the sheet material after being heated by the laser curtain; The sheet material after being scanned by the coolant flow is impacted by a water jet.

5. The surface regeneration treatment method of sheet material according to claim 1, characterized in that: The cooling liquid flow is water flow.

6. The surface regeneration treatment method of sheet material according to claim 1, characterized in that: The step of cleaning the sheet material comprises water washing, alkali washing, acid washing and passivation of the sheet material.

7. A surface regeneration treatment device for a sheet material, used for performing the surface regeneration treatment method for a sheet material according to any one of claims 1 to 6, characterized in that: It comprises a machine head and a workbench, wherein the machine head is arranged above the workbench and can move along the length direction of the workbench; The machine head comprises a laser and a water jet, and the laser curtain emitted by the laser is spaced 5 to 10 cm from the water jet.

8. The surface regeneration treatment device for sheet material according to claim 7, characterized in that: The machine head further comprises a water jet generator, which is arranged beside the water jet away from the laser.

9. The surface regeneration treatment device of the sheet material according to claim 7, characterized in that: The water jet is a water jet generator.

10. The surface regeneration treatment device for sheet material according to claim 8 or 9, characterized in that: The water flow of the water jet generator is 75° to 85° with the working surface of the workbench.