Solid waste landfill bottom anti-seepage system leakage point repairing method and repairing material thereof

Through the combination of directional drilling inclined wells and loaded sodium percarbonate biomass repair materials, the problem of leakage of HDPE membrane at the bottom of the solid waste landfill site is solved, and the leakage point is quickly and reliable, reducing engineering volume and odor, and Improves the acid and alkali resistance and self-healing ability of the repair materials.

CN118933102AInactive Publication Date: 2024-11-12ZHEJIANG JINKE CHEM
View PDF 6 Cites 0 Cited by

Patent Information

Application Number
CN202411427450.9
Authority / Receiving Office
CN · China
Patent Type
Applications(China)
Current Assignee / Owner
Filing Date
2024-10-14
Publication Date
2024-11-12
Estimated Expiration
Not applicable · inactive patent

AI Technical Summary

Technical Problem

During transportation, laying and operation, the HDPE film at the bottom of the solid waste landfill site leaks due to uneven foundation sinking and chemically corrosive substances. The existing repair methods are large in quantity, high in cost, long time and produce odors.

Method used

Positioning leakage points by directed drilling inclined wells, using waste biomass repair materials based on loaded sodium percarbonate and thermoplastic protective film for repair, combining high-precision three-dimensional resistance inversion imaging method and fast condensation one-step method solid waste-based low-carbon geology The polymer was secondary blocked.

Benefits of technology

It realizes convenient, fast and reliable repair of leak points, reduces construction complexity and odor, and has good acid and alkali resistance and self-healing ability to avoid re-leakage.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure CN118933102A_ABST
    Figure CN118933102A_ABST
Patent Text Reader

Abstract

The invention provides a method for repairing a leakage point of an anti-seepage system at the bottom of a solid waste filling field. The method comprises the following working steps: S1) accurately positioning a leakage point part in the solid waste filling field; s2) directionally drilling an inclined shaft from the outer side of the slope of the solid waste landfill to the direction of the potential leakage point part, wherein the inclined shaft extends into the solid waste landfill to cover the leakage point part; 3) extracting and collecting leachate, sludge and residues accumulated in the inclined shaft, and performing subsequent harmless treatment; and S4, a waste biomass leakage point repairing material based on loaded sodium percarbonate is injected into the inclined shaft, oxidation repairing is conducted on soil and underground water around the leakage point, and then a thermoplastic protection film is sprayed on the repairing material. The technical problems that in the prior art, the repairing work amount of the bottom leakage points of the solid waste landfill is large, cost is high, consumed time is long, and peculiar smell is large can be solved.
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] The invention relates to the technical field of environmental geotechnical engineering, and in particular to a method for repairing leakage points of a bottom anti-seepage system of a solid waste landfill and a repair material thereof. Background Art

[0002] Most of the solid waste landfills in my country (such as domestic waste landfills, fly ash and other hazardous waste landfills, etc.) use HDPE membrane as the bottom anti-seepage layer of the site. The HDPE membrane will be damaged during transportation and laying; more importantly, during the operation of the landfill and after the closure of the landfill, the foundation will sink unevenly and the HDPE membrane will deform due to the influence of the overlying landfill load, resulting in mechanical damage; and the continuous action of chemical corrosive substances and pollutants in the waste will also cause chemical fatigue of the anti-seepage membrane. These reasons will eventually cause the HDPE membrane to leak, threatening the environmental safety of the surrounding soil and groundwater. Therefore, timely finding the exact location of the leakage point of the landfill and reliably repairing it is a difficult point in the field of environmental geotechnical engineering at home and abroad.

[0003] At present, leakage problems found during the laying stage of the impermeable membrane and the construction stage of the water-conducting layer and water collection facilities on the membrane are relatively easy to repair using simple methods. However, during the operation and closure stage, since a large amount of hazardous waste has been accumulated on the impermeable layer, its repair requires not only accurate monitoring and positioning of the leakage point, but also corresponding engineering measures. The conventional treatment method is to implement excavation and drainage measures on the landfill, expose the leakage point and then carry out repairs; this method has a large amount of engineering, high cost, long time consumption, and produces a lot of odor. Therefore, it is very important to find a technology that can be applied in situ to achieve convenient, fast and reliable repair and repair of leakage points. Summary of the invention

[0004] The purpose of the invention is to solve the technical problems in the prior art that the repair work of leakage points at the bottom of solid waste landfills is large in amount, high in cost, time-consuming and has a strong odor.

[0005] In order to achieve the above object, the present invention is implemented by the following technical solutions: A method for repairing leakage points in a bottom anti-seepage system of a solid waste landfill comprises the following working steps: S1) Accurately locate the leakage point in the solid waste landfill; S2) Directionally drilling an inclined well from the outside of the solid waste landfill slope toward the potential leak site, the inclined well extending into the solid waste landfill to cover the leak site, and during the drilling process, the inner and outer pipes of the drilling casing perform different tasks respectively, the outer pipe sprays fast-hardening cement slurry for wall protection, and after the inner pipe is drilled to the leak site, the inner pipe end is unfolded in a shower shape and repair slurry is radially sprayed to cover the leak site; S3) extracting and collecting the leachate, sludge and residue accumulated in the inclined well for subsequent harmless disposal; S4) injecting a sodium percarbonate-loaded waste biomass leak repair material into the inclined well to oxidize and repair the soil and groundwater around the leak, and then spraying a thermoplastic protective film on the repair material.

[0006] Furthermore, locating the leakage point in the solid waste landfill includes the following working steps: S1-1) Collect the resistivity and pH value near the leak point; S1-2) Using high-precision three-dimensional resistance inversion imaging, the specific location, shape and size of the leak point are inverted based on the difference in resistivity and pH value.

[0007] Furthermore, in step S2), the drilling tool of the inclined well is a skid-mounted high-precision drilling platform.

[0008] Furthermore, in step S2), the well is drilled to extend 1-2 meters into the solid waste pile of the landfill, the aperture of the inclined well is 60-70 cm, the outer pipe diameter is 30-40 cm, and the inner pipe diameter is 30 cm.

[0009] Furthermore, the spraying process of the protective film in step S4) is as follows: S4-1) The first layer of leak repair protective film is formed by heating and blowing the high polymer material on the drilling tool; S4-2) The drilling rig sprays dry ice or other coolants to quickly cool the leak point; S4-3) The drilling rig sprays a quick-setting one-step solid waste-based low-carbon geopolymer onto the leak point and the wall of the inclined well, thereby achieving secondary sealing of the leak point and supporting the wall.

[0010] Furthermore, the polymer material is a composition of isocyanate and polyol in a molar ratio of 1:0.8-1.3.

[0011] Furthermore, the fast-setting one-step solid waste-based low-carbon geopolymer comprises: 10-15% self-cementing biological bacteria, 20-30% magnesium oxide, 40-50% granulated blast furnace slag, 5-10% calcined waste kaolin, 2-5% commercial solid sodium hydroxide, 3%-8% waste lime and 5%-10% commercial concrete fast-setting agent.

[0012] A leakage repair material for the bottom anti-seepage system of a solid waste landfill, wherein the repair material is a leakage repair material based on waste biomass loaded with sodium percarbonate, and the construction method thereof is as follows: a) Pre-treatment of straw biomass waste and landfill excavation sludge waste, including mixing, natural air drying, debris removal and grinding; b) carbonizing the pretreated granular material in a) at 850° C. for 2 hours in a nitrogen atmosphere of 100 ml / min; c) The carbonized granular material in b) is stirred with a sodium percarbonate aqueous solution at 40° C. and a rotation speed of 100 d / min to obtain a final product.

[0013] Compared with the prior art, the present invention has the following advantages: The method of the present invention locates the leakage point and then directionally drills an inclined well from the outer side of the solid waste landfill slope toward the leakage point, which can greatly reduce the construction complexity and workload, facilitate improving the operation efficiency and convenience, and can also support while drilling, further improving the operation efficiency; and then, by filling the anti-seepage repair material, the leakage point can be repaired in time to complete the repair operation.

[0014] Since the excavated volume and open area are small, the odor is relatively small; a specific plan for anti-seepage repair materials is also proposed, which has good acid and alkali resistance, good workability, high strength, and good resistance to secondary damage; at the same time, self-cementing biological bacteria are conducive to secondary reproduction and self-healing of leakage points, making the material easy to pump, with a certain self-healing ability, continuous repair, and avoid leakage again. BRIEF DESCRIPTION OF THE DRAWINGS

[0015] Figure 1 It is a flow chart of the present invention.

[0016] Figure 2 It is a schematic diagram of the engineering of step S1) of the present invention.

[0017] Figure 3 It is a schematic diagram of the engineering of step S2) of the present invention.

[0018] Figure 4 It is a schematic diagram of the engineering of step S3) of the present invention.

[0019] Figure 5 It is a schematic diagram of the engineering of step S4) of the present invention.

[0020] Figure 6 This is a comparison chart of the effects of different anti-seepage materials. DETAILED DESCRIPTION

[0021] The embodiments of the present invention are described in further detail below in conjunction with the accompanying drawings.

[0022] The technical solutions in the embodiments of the present invention will be described clearly and completely below in conjunction with the accompanying drawings in the embodiments of the present invention. Obviously, the described embodiments are only part of the embodiments of the present invention, not all of the embodiments. Based on the embodiments of the present invention, all other embodiments obtained by ordinary technicians in this field without creative work are within the scope of protection of the present invention.

[0023] It should be noted that all directional indications in the embodiments of the present invention are only used to explain the relative position relationship, movement status, etc. between various components in a certain specific posture. If the specific posture changes, the directional indication will also change accordingly.

[0024] The present invention is described below with reference to specific embodiments in conjunction with the accompanying drawings.

[0025] The embodiment of the present invention provides a method for repairing leakage points in the bottom anti-seepage system of a solid waste landfill, thereby solving the technical problems in the prior art of large engineering workload, long time consumption and strong odor in repairing leakage points at the bottom of a solid waste landfill.

[0026] like Figure 1 As shown, a method for repairing leakage points in the bottom anti-seepage system of a solid waste landfill is as follows: Figure 1 As shown, the working steps are as follows: S1) Accurately locate the leakage point in the solid waste landfill, such as Figure 2 As shown; S1-1) Collect the resistivity and pH value near the leak point; S1-2) Using high-precision three-dimensional resistance inversion imaging, the specific location, shape and size of the leak point are inverted based on the difference in resistivity and pH value.

[0027] Specifically, high-precision three-dimensional resistance inversion imaging technology is used to collect the resistivity and pH value near the leakage point. Relying on the different resistivities and pH values ​​of the anti-seepage membrane and the soil and combining with the self-developed inversion model, the point is identified as an anti-seepage membrane or soil. The difference in the electrochemical properties of the interface is judged by the two parameters of resistivity and pH value, and the location, shape and size of the leakage point are inverted. At the same time, the inversion imaging technology can collect the geographic coordinates of the leakage point, and transmit the coordinates to the skid-mounted high-precision drilling platform, which can assist the drilling system to accurately drill to the vicinity of the point to be repaired.

[0028] S2) Directional drilling of an inclined well from the outside of the solid waste landfill slope toward the potential leak site, the inclined well extending into the solid waste landfill to cover the leak site, and during the drilling process, the inner and outer pipes of the drilling casing perform different tasks respectively, the outer pipe sprays fast-hardening cement slurry for wall protection, and after the inner pipe is drilled to the leak site, the inner pipe end is unfolded in a shower shape and the repair slurry is radially sprayed to cover the leak site, such as Figure 3 As shown; The drilling tool for the inclined well is a skid-mounted high-precision drilling platform; the skid-mounted high-precision drilling platform is a skid-mounted design that can adapt to a variety of terrains and slopes. After the construction site is selected, the instrument can automatically set support points near the platform to ensure that the platform does not overturn during the grouting process. The drilling system is a casing injection mode. After the casing is drilled to the designated coordinate location, the inner and outer pipes perform different tasks respectively, that is, the outer pipe can spray fast-hardening cement slurry to protect the wall to prevent collapse accidents in subsequent construction; after the inner pipe is drilled to the leak point, the end of the inner pipe unfolds into a shower-like spray device, which can transport the repair slurry to the leak point and evenly radially form a cake-shaped slurry to cover the leak point.

[0029] The well is drilled to extend 1 to 2 meters into the solid waste pile of the landfill. The diameter of the inclined well is 60 to 70 cm. Depending on the depth and size of the landfill, the diameter of the outer pipe is 30 to 40 cm and the diameter of the inner pipe is 30 cm.

[0030] S3) extracting and collecting the leachate, sludge and residue accumulated in the inclined well for subsequent harmless disposal, such as Figure 4 As shown; S4) injecting the sodium percarbonate-loaded waste biomass leak repair material into the inclined well to oxidize and repair the soil and groundwater around the leak, and then spraying a thermoplastic protective film on the repair material, such as Figure 5 As shown; Among them, the repair material is a waste biomass leak repair material based on sodium percarbonate, and its construction method is as follows: a) Pre-treatment of straw biomass waste and landfill excavation sludge waste, including mixing, natural air drying, removal of debris and grinding to less than 200 microns; b) carbonizing the pretreated granular material in a) for 2 hours at 850° C. (heating rate of 5° C. / min) in a nitrogen atmosphere of 100 ml / min; c) The carbonized granular material in b) is stirred with a sodium percarbonate aqueous solution at 40° C. and a rotation speed of 100 d / min to obtain a final product.

[0031] Among them, the spraying process of the protective film is as follows: S4-1) The drilling tool is covered with a polymer material by heating and blow molding to form a first layer of leak repair protective film; the polymer material is a composition of isocyanate and polyol in a molar ratio of 1:0.8-1.3, and the polymer material is lightly stirred and mixed by a brush head on the tool head to form it at room temperature; S4-2) The drilling rig sprays dry ice or other coolants to quickly cool the leak point; S4-3) The drilling rig sprays a quick-setting one-step solid waste-based low-carbon geopolymer onto the leak point and the wall of the inclined well, thereby achieving secondary sealing of the leak point, protecting the polymer cover layer and supporting the wall at the same time; the quick-setting one-step solid waste-based low-carbon geopolymer is: 10-15% self-cementing biological bacteria, 20-30% magnesium oxide, 40-50% granulated blast furnace slag, 5-10% calcined waste kaolin, 2-5% commercial solid sodium hydroxide, 3%-8% waste lime and 5%-10% commercial concrete quick-setting agent.

[0032] The fast-setting one-step solid waste-based low-carbon geopolymer provided by the present invention has good acid and alkali resistance, good workability, high strength, and is not conducive to secondary damage. At the same time, the self-cementing biological bacteria are conducive to secondary reproduction and self-healing leakage points, so that the material is easy to pump and has a certain self-healing ability.

[0033] like Figure 6 As shown, the repair effect of the waste biomass leak repair material based on sodium percarbonate loading is compared with the traditional cement-based material, and it can be concluded that the new material proposed by the present invention has a significantly higher repair rate than the traditional cement material. Among them, the control group is the non-repair situation.

[0034] Obviously, those skilled in the art can make various changes and modifications to the present invention without departing from the spirit and scope of the present invention. Thus, if these modifications and variations of the present invention fall within the scope of the claims of the present invention and their equivalents, the present invention is also intended to include these modifications and variations.

Claims

1. A method for repairing leakage points in the bottom anti-seepage system of a solid waste landfill. Features The following steps are included: S1) Accurately locate the leakage point in the solid waste landfill; S2) Directionally drilling an inclined well from the outside of the solid waste landfill slope toward the leakage point, the inclined well extending into the solid waste landfill to cover the leakage point, and during the drilling process, the inner and outer pipes of the drilling casing perform different tasks respectively, the outer pipe sprays fast-hardening cement slurry for wall protection, and after the inner pipe is drilled to the leakage point, the end of the inner pipe unfolds in a shower shape and sprays the repair slurry radially to cover the leakage point; S3) extracting and collecting the leachate, sludge and residue accumulated in the inclined well for subsequent harmless disposal; S4) injecting a sodium percarbonate-loaded waste biomass leak repair material into the inclined well to oxidize and repair the soil and groundwater around the leak, and then spraying a thermoplastic protective film on the repair material.

2. A method for repairing leakage points in a bottom anti-seepage system of a solid waste landfill according to claim 1, Features: Locating the leak point in the solid waste landfill includes the following steps: S1-1) Collect the resistivity and pH value near the leak point; S1-2) Using high-precision three-dimensional resistance inversion imaging, the specific location, shape and size of the leak point are inverted based on the difference in resistivity and pH value.

3. A method for repairing leakage points in a bottom anti-seepage system of a solid waste landfill according to claim 1, Features: In step S2), the drilling tool for the inclined well is a skid-mounted high-precision drilling platform.

4. A method for repairing leakage points in a bottom anti-seepage system of a solid waste landfill according to claim 3, Features: In step S2), the well is drilled to extend 1-2 meters into the solid waste pile of the landfill, the aperture of the inclined well is 60-70 cm, the outer pipe diameter is 30-40 cm, and the inner pipe diameter is 30 cm.

5. A method for repairing leakage points in a bottom anti-seepage system of a solid waste landfill according to claim 1, Features: The spraying process of the protective film in step S4) is as follows: S4-1) The first layer of leak repair protective film is formed by heating and blowing the high polymer material on the drilling tool; S4-2) Use the drilling rig to spray dry ice or other coolants to quickly cool the leaking point; S4-3) The drilling rig sprays a quick-setting one-step solid waste-based low-carbon geopolymer onto the leak point and the wall of the inclined well, thereby achieving secondary sealing of the leak point and supporting the wall.

6. A method for repairing leakage points in a bottom anti-seepage system of a solid waste landfill according to claim 5, Features: The polymer material is a composition of isocyanate and polyol in a molar ratio of 1:0.8-1.

3.

7. A method for repairing leakage points in a bottom anti-seepage system of a solid waste landfill according to claim 5, Features: The fast-setting one-step solid waste-based low-carbon geopolymer comprises: 10-15% of self-cementing biological bacteria, 20-30% of magnesium oxide, 40-50% of granulated blast furnace slag, 5-10% of calcined waste kaolin, 2-5% of commercial solid sodium hydroxide, 3%-8% of waste lime and 5%-10% of commercial concrete fast-setting agent.

8. A material for repairing leaks in the bottom anti-seepage system of a solid waste landfill. Features: The repair material is a waste biomass leak repair material based on sodium percarbonate, and its construction method is as follows: a) Pre-treatment of straw biomass waste and landfill excavation sludge waste, including mixing, natural air drying, debris removal and grinding; b) carbonizing the pretreated granular material in a) at 850° C. for 2 hours in a nitrogen atmosphere of 100 ml / min; c) The carbonized granular material in b) is stirred with a sodium percarbonate aqueous solution at 40° C. and a rotation speed of 100 d / min to obtain a final product.

Citation Information

Patent Citations

  • Steel slag eco-concrete, steel slag eco-concrete product and preparation method thereof

    CN101880147A

  • Drilling injection vibration stirring construction equipment and foundation construction method

    CN106223331A

  • Trenchless wading pipeline inner wall repair material and preparation method thereof

    CN106634510A

  • Method for repairing leakage of HDPE films on landfill side slope