Split high-K metal gate super-junction silicon carbide trench MOSFET and preparation method thereof
By introducing split high K metal gate structure and deep groove high K dielectric region in silicon carbide longitudinal power devices, the parasitic capacitance and resistance contradiction in traditional devices is solved, the performance and stability of the device are improved, and suitable for high voltage and low power consumption. application.
Patent Information
- Application Number
- CN202411433922.1
- Authority / Receiving Office
- CN · China
- Patent Type
- Applications(China)
- Current Assignee / Owner
- Filing Date
- 2024-10-15
- Publication Date
- 2024-11-12
AI Technical Summary
Traditional trench superjunction silicon carbide longitudinal power devices have the problem of excessive parasitic capacitance and the contradiction between breakdown voltage and specific on-resistance, which limits their development in the field of high voltage and low power consumption.
Using split high K metal gate structure, the drift region and P-type well region of the deep groove high K dielectric region and split gate metal are used to modulate the conductive channels of the device, reduce the leakage gate capacitance and gate charge, and balance the breakdown voltage. and specific on-resistance.
The breakdown voltage, gate oxygen stability and drift region doping concentration of the device are improved, the on-resistance and power consumption are reduced, and the dynamic performance is improved.
Smart Images

Figure CN118943199A_ABST
Abstract
Description
Technical Field
[0001] The present invention relates to the technical field of semiconductor power devices, in particular to a split high-K metal gate super junction silicon carbide trench MOSFET and a preparation method thereof. Background Art
[0002] Silicon carbide (SiC) materials have become a typical representative of the third generation of power semiconductor materials with its wide band gap, high breakdown field, high thermal conductivity, high carrier saturation rate and other advantages. In particular, SiC power semiconductor devices have the advantages of high frequency, high temperature conductivity, low on-resistance, etc., and are widely used in new energy vehicles, aerospace, satellite communications and other fields. Silicon carbide power semiconductor devices are currently mainly divided into lateral silicon carbide power semiconductor devices and vertical silicon carbide power semiconductor devices. Vertical power semiconductor devices are more suitable for high voltage and low power consumption fields due to their higher breakdown voltage and lower specific on-resistance. In order to solve the problem of excessive parasitic capacitance of vertical silicon carbide power devices and balance the contradictory relationship between breakdown voltage and specific on-resistance, trench structure, split gate technology, super junction technology, and high-K gate oxide dielectric technology are widely used.
[0003] Drain-gate capacitance C of conventional trench superjunction SiC vertical power device gd and gate charge Q gd The larger the gate length, the slower the switching speed, which results in higher power consumption in high-frequency and high-power applications, greatly increasing the cost of the device. In addition, for traditional trench-type superjunction silicon carbide vertical power devices, increasing the breakdown voltage requires extending the length of the device drift region or reducing the drift region doping concentration, which will increase the device's specific on-resistance and reduce the conduction capability.
[0004] In summary, the problem of excessive parasitic capacitance and the contradictory relationship between breakdown voltage and specific on-resistance are the two major problems restricting the development of trench super-junction silicon carbide vertical power devices in the field of high voltage and low power consumption. Summary of the invention
[0005] The technical problem to be solved by the present invention is to provide a split high-K metal gate super junction silicon carbide trench MOSFET and a preparation method thereof in view of the deficiencies of the above-mentioned prior art. The split high-K metal gate super junction silicon carbide trench MOSFET and the preparation method thereof modulate the drift region of the device by introducing a deep trench high-K dielectric region; at the same time, a split high-K metal gate structure is formed by combining the split gate metal and the gate metal, which can modulate the conductive channel generated by the P-type well region when it is inverted, thereby improving the device performance without significantly increasing the process complexity, balancing the contradictory relationship between the breakdown voltage and the specific on-resistance, and reducing the drain-gate capacitance C of the device. gd and gate charge Q gd , and get better performance.
[0006] In order to solve the above technical problems, the technical solution adopted by the present invention is: A split high-K metal gate super junction silicon carbide trench MOSFET comprises a semiconductor drain region, a super junction structure, a P-type well region, a semiconductor source region and a split high-K metal gate structure.
[0007] A drain metal electrode is deposited at the bottom of the semiconductor drain region.
[0008] The superjunction structure is epitaxially grown on top of the semiconductor drain region, and includes a semiconductor N-type drift region and a semiconductor P-type drift region coaxially arranged from the inside to the outside.
[0009] The P-type well region is arranged on the top of the super junction structure.
[0010] The semiconductor source region is arranged on the top of the P-type well region, and a source-end metal electrode is deposited on the top of the semiconductor source region.
[0011] The semiconductor source region includes a semiconductor N-type source region and a semiconductor P-type source region which are coaxially arranged in sequence from the inside to the outside.
[0012] The split high-K metal gate structure includes a deep trench high-K dielectric region, a split gate metal and a gate metal.
[0013] The deep trench high-K dielectric region is coaxially embedded in the middle of the semiconductor N-type source region, the P-type well region and the semiconductor N-type drift region; the top surface of the deep trench high-K dielectric region is flush with the top surface of the semiconductor N-type source region; the thickness of the deep trench high-K dielectric region is T HK The thickness of the deep trench high-K dielectric region is smaller than the width of the semiconductor N-type drift region.
[0014] The split gate metal and the gate metal are coaxially arranged in the middle of the deep trench high-K dielectric region from top to bottom; the top surface of the gate metal is flush with the top surface of the deep trench high-K dielectric region; there is a spacing T between the split gate metal and the gate metal gap There is a set spacing greater than zero between the bottom surface of the split gate metal and the bottom surface of the deep trench high-K dielectric region.
[0015] The dielectric constant ε of the high-K dielectric in the deep trench high-K dielectric region is greater than 3.9. By selecting the dielectric constant ε, the MOSFET has a maximum quality factor without being lower than a set breakdown voltage.
[0016] The high-K dielectric in the deep trench high-K dielectric region is hafnium dioxide.
[0017] Assume that the single side width of the deep trench high-K dielectric region outside the split gate metal is W sg ; By constructing the quality factor and different W sg The relationship curve of the maximum quality factor corresponding to W sg As the best W sg .
[0018] Assume the thickness of the split gate metal is T sg ; By constructing the quality factor and different T sg The relationship curve of the maximum quality factor is T sg As the best T sg .
[0019] By constructing the quality factor and different spacing T gap The relationship curve of the maximum quality factor is T gap As the optimal spacing T gap .
[0020] By constructing the quality factor with different T HK The relationship curve of the maximum quality factor is T HK As the optimal deep trench high-K dielectric region thickness T HK .
[0021] The thickness of the semiconductor source region does not exceed the thickness of the P-type well region; the width of the split gate metal is less than or equal to the width of the gate metal.
[0022] A method for preparing a split high-K metal gate super junction silicon carbide trench MOSFET comprises the following steps.
[0023] Step 1, making a super junction structure: epitaxially grow a layer of N-type doped silicon carbide on the semiconductor drain region to form a semiconductor N-type drift region; use plasma dry etching to symmetrically and vertically etch semiconductor P-type drift region trenches on the left and right sides of the semiconductor N-type drift region; the bottom of the semiconductor P-type drift region trench contacts the semiconductor drain region; epitaxially grow P-type doped silicon carbide in the semiconductor P-type drift region trench and push the junction to form a semiconductor P-type drift region; the semiconductor P-type drift region and the semiconductor N-type drift region are at the same height, and the semiconductor P-type drift region and the semiconductor N-type drift region together constitute a super junction structure.
[0024] Step 2, making a P-type well region and a semiconductor source region: using ion implantation and annealing, a P-type well region and a semiconductor source region are sequentially made on top of the super junction structure made in step 1; wherein the semiconductor N-type source region in the semiconductor source region is located directly above the semiconductor N-type drift region; and the semiconductor P-type source region in the semiconductor source region is located directly above the semiconductor P-type drift region.
[0025] Step 3, forming a deep trench high-K dielectric region: using plasma dry etching, a groove is etched vertically downward at the top center of the semiconductor source region; the groove passes through the semiconductor source region and the P-type well region in sequence, and extends to the semiconductor N-type drift region; using magnetron sputtering method, a high-K dielectric of a set thickness is deposited on the bottom and side of the trench, thereby forming a deep trench high-K dielectric region.
[0026] Step 4: Deposit split gate metal: Use magnetron sputtering to deposit a layer with a thickness of T sg The split gate metal is coaxially deposited in the deep trench high-K dielectric region produced in step 3.
[0027] Step 5: Forming a high-K gate dielectric region: First, the deep trench high-K dielectric region located at the top of the split gate metal is etched vertically downward from the top to the top of the split gate metal through a mask; then, a magnetron sputtering method is used to deposit a thickness of T on the top of the split gate metal. gap The high-K dielectric is connected to the deep trench high-K dielectric regions on both sides to form a high-K gate dielectric region.
[0028] Step 6, depositing metal electrodes: the metal electrodes include gate metal, source metal electrode and drain metal electrode; wherein the gate metal is deposited in the high-K gate dielectric region produced in step 5 by magnetron sputtering; the source metal electrode is deposited on the top of the semiconductor source region by magnetron sputtering, respectively contacting the semiconductor P-type source region and the semiconductor N-type source region; the drain metal electrode is deposited on the bottom of the semiconductor drain region by magnetron sputtering.
[0029] In step 1, the doping concentration of the semiconductor N-type drift region and the semiconductor P-type drift region is not less than 1×10 16 cm -3 In step 2, the doping concentration of the P-type well region is not less than 1×10 17 cm -3 The doping concentration of the semiconductor N-type source region and the semiconductor P-type source region is not less than 1×10 19 cm -3 .
[0030] The present invention has the following beneficial effects: The split high-K metal gate structure of the present invention can simultaneously modulate the conductive channel generated by the device drift region and the P-type well region during inversion, thereby reducing the device's specific on-resistance and threshold voltage, and improving the device's breakdown voltage, gate oxide stability, drift region doping concentration, and quality factor.
[0031] In the present invention, a high-K gate dielectric is used to replace a traditional oxide gate dielectric, thereby reducing the threshold voltage and the electric line density between the gate metal and the split gate metal; the MIS structure composed of the gate metal, the high-K dielectric and the silicon carbide material can increase the density of the electron accumulation layer and reduce the conductive channel resistance generated by the P-type well region during inversion.
[0032] The deep trench high-K dielectric region in the present invention can modulate the electric field distribution of the device drift region and increase the breakdown voltage, and there is an electric field mutation at the bottom of the region and the contact surface of the drift region, and the formed electric field peak further increases the breakdown voltage. In addition, the auxiliary depletion effect of the high-K dielectric can increase the doping concentration of the device drift region, thereby reducing the resistance of the drift region.
[0033] The present invention adopts a split gate structure, wherein the split gate is floated in a deep trench high-K dielectric region, which can reduce the drain-gate capacitance and improve the dynamic performance of the device. BRIEF DESCRIPTION OF THE DRAWINGS
[0034] Figure 1 The present invention is a schematic structural diagram of a split high-K metal gate super junction silicon carbide trench MOSFET.
[0035] Figure 2 The figure is a schematic diagram of partial dimension marking of a split high-K metal gate super junction silicon carbide trench MOSFET of the present invention.
[0036] Figure 3 FIG. 4 is a relationship diagram between the quality factor and the doping concentration of the drift region under different dielectric constants ε of the present invention.
[0037] Figure 4 The present invention is different in W sg The relationship between the breakdown voltage, on-resistance and quality factor under different W sg The relationship between the breakdown voltage and the on-resistance under different W sg The quality factor variation diagram below.
[0038] Figure 5 The present invention has different split gate thickness T sg The relationship between the breakdown voltage, on-resistance and quality factor under different split gate thickness T sg The relationship between the breakdown voltage and the on-resistance under different split gate thickness T sg The quality factor variation diagram below.
[0039] Figure 6 The present invention is different in T gap The relationship between the breakdown voltage, on-resistance and quality factor under different T gap The relationship between the breakdown voltage and the on-resistance under different T gap The quality factor variation diagram below.
[0040] Figure 7 The present invention is different in T HK The relationship between the breakdown voltage, on-resistance and quality factor under different T HK The relationship between the breakdown voltage and the on-resistance under different T HK The quality factor variation diagram below.
[0041] Figure 8This is a schematic diagram of the structure after the semiconductor superjunction drift region is completed in step 1 of the present invention.
[0042] Fig. 9 This is a schematic diagram of the structure after the P-type well region and the semiconductor active region are manufactured in step 2 of the present invention.
[0043] Fig.10 This is a schematic diagram of the structure after the deep trench high-K dielectric area is completed in step 3 of the present invention.
[0044] Fig.11 This is a schematic diagram of the structure after the split-gate metal region is manufactured in step 4 of the present invention.
[0045] Fig.12 This is a schematic diagram of the structure after the high-K gate dielectric region is manufactured in step 5 of the present invention.
[0046] Fig.13 It is a comparison diagram of the relationship between the quality factor and the drift region doping concentration of the new structure of the present invention, the conventional split-gate super junction structure and the conventional super junction structure.
[0047] Fig.14 It is a comparison diagram of the longitudinal electric field distribution of the new structure of the present invention, the conventional split-gate super junction structure and the conventional super junction structure.
[0048] Fig.15 The gate charge Q of the new structure of the present invention, the conventional split-gate superjunction structure and the conventional superjunction structure is gd .
[0049] Fig.16 The drain-gate capacitance C of the new structure of the present invention, the conventional split-gate superjunction structure and the conventional superjunction structure is gd .
[0050] These include: 1. semiconductor drain region; 2. semiconductor N-type drift region; 3. semiconductor P-type drift region; 4. P-type well region; 5. semiconductor N-type source region; 6. semiconductor P-type source region; 7. deep trench high-K dielectric region; 8. split gate metal; 9. gate metal; 10. source metal electrode; 11. drain metal electrode. DETAILED DESCRIPTION
[0051] The present invention will be further described in detail below in conjunction with the accompanying drawings and specific preferred embodiments.
[0052] The present invention takes a silicon carbide vertical trench MOSFET in a super junction drift region as an example and is described in detail. As an alternative, a split high-K metal gate super junction silicon carbide trench MOSFET of the present invention can also be applied to various types of silicon carbide power devices such as a silicon carbide vertical trench MOSFET in an N-type drift region, a silicon carbide vertical trench MOSFET in a P-type drift region, and a silicon carbide lateral trench MOSFET in a super junction drift region.
[0053] like Figure 1 and Figure 2 As shown, a split high-K metal gate super junction silicon carbide trench MOSFET includes a semiconductor drain region 1, a super junction structure, a P-type well region 4, a semiconductor source region and a split high-K metal gate structure.
[0054] A drain metal electrode 11 is deposited at the bottom of the semiconductor drain region.
[0055] The super junction structure is epitaxially grown on the top of the semiconductor drain region, and includes a semiconductor N-type drift region 2 and a semiconductor P-type drift region 3 which are coaxially arranged from the inside to the outside.
[0056] The P-type well region is arranged on the top of the super junction structure.
[0057] The semiconductor source region is arranged on the top of the P-type well region, and a source-end metal electrode 10 is deposited on the top of the semiconductor source region.
[0058] The semiconductor source region includes a semiconductor N-type source region 5 and a semiconductor P-type source region 6 which are coaxially arranged from the inside to the outside and have equal thickness. The semiconductor N-type source region is located directly above the semiconductor N-type drift region, and the semiconductor P-type source region is located directly above the semiconductor P-type drift region. Further, the thickness of the semiconductor source region is preferably not greater than the thickness of the P-type well region.
[0059] Furthermore, the source-end metal electrode is in contact with the semiconductor N-type source region and the semiconductor P-type source region respectively, and is not in contact with the subsequent high-K dielectric and gate metal.
[0060] The split high-K metal gate structure includes a deep trench high-K dielectric region 7 , a split gate metal 8 and a gate metal 9 .
[0061] The deep trench high-K dielectric region is coaxially embedded in the middle of the semiconductor N-type source region, the P-type well region and the semiconductor N-type drift region; the top surface of the deep trench high-K dielectric region is flush with the top surface of the semiconductor N-type source region; the thickness of the deep trench high-K dielectric region is T HK The thickness of the deep trench high-K dielectric region is smaller than the width of the semiconductor N-type drift region.
[0062] The split gate metal and the gate metal are coaxially arranged in the middle of the deep trench high-K dielectric region from top to bottom; the top surface of the gate metal is flush with the top surface of the deep trench high-K dielectric region; there is a spacing T between the split gate metal and the gate metal gap There is a set spacing greater than zero between the bottom surface of the split gate metal and the bottom surface of the deep trench high-K dielectric region.
[0063] The thickness or depth of the gate metal is greater than the bottom of the P-type well region, forming a vertical high-K metal gate structure from top to bottom.
[0064] Furthermore, the width of the split gate metal is preferably less than or equal to the width of the gate metal.
[0065] Furthermore, the materials of the above-mentioned semiconductor drain region, semiconductor N-type drift region, semiconductor P-type drift region, P-type well region, semiconductor N-type source region and semiconductor P-type source region are preferably silicon carbide, and the silicon carbide material is 3C-SiC, 4H-SiC or 6H-SiC, etc., and 4H-SiC is further preferred.
[0066] In this embodiment, taking the thickness of the super junction structure (that is, the thickness of the semiconductor drift region) as 16 microns as an example, the single side width W of the deep trench high-K dielectric region is selected from the high-K dielectric material. sg , Split-gate metal thickness T sg , spacing T gap , and the thickness of the deep trench high-K dielectric region T HK The best value selection is explained in detail.
[0067] 1. Selection of high-K dielectric materials The dielectric constant ε of the high-K dielectric in the deep trench high-K dielectric region is greater than 3.9. When other structural parameters remain the same, by selecting the dielectric constant ε, the MOSFET has a maximum quality factor without being lower than a set breakdown voltage.
[0068] Figure 3 The figure of merit (FOM) and the drift region doping concentration (N) of the present invention under different dielectric constants ε are shown. SJ ). When the dielectric constant ε is 15, 25, 30, and 80, the high-K dielectrics are yttrium trioxide (Y2O3), hafnium dioxide (HfO2), lanthanum oxide (La2O3), and titanium dioxide (TiO2), respectively, and the other structural parameters of the device remain the same. Figure 3 In the figure, the horizontal axis is the doping concentration in the drift region, and the vertical axis is the quality factor. The corresponding parameters of the four maximum quality factor points A, B, C and D are: When ε is 15, the highest quality factor is point A, and its corresponding parameters are: quality factor is 3.38×10 9W / cm 2 , the drift region doping concentration is 4.4×10 16 cm -3 , on-resistance is 1.25mΩ·cm 2 , the breakdown voltage is 2059V.
[0069] When ε is 25, the highest quality factor is point B, and its corresponding parameters are: quality factor is 4.36×10 9 W / cm 2 , the drift region doping concentration is 5.4×10 16 cm -3 , on-resistance is 0.90mΩ·cm 2 , the breakdown voltage is 1986V.
[0070] When ε is 30, the highest quality factor is point C, and its corresponding parameters are: quality factor is 6.02×10 9 W / cm 2 , the drift region doping concentration is 6.4×10 16 cm -3 , the on-resistance is 0.61mΩ·cm 2 , the breakdown voltage is 1922V.
[0071] When ε is 80, the highest quality factor is point D, and its corresponding parameters are: quality factor is 8.72×10 9 W / cm 2 , the drift region doping concentration is 7×10 16 cm -3 , on-resistance is 0.39mΩ·cm 2 , the breakdown voltage is 1850V.
[0072] from Figure 3 It can be seen that the increase in the dielectric constant of the high-K dielectric can significantly improve the quality factor of the present invention. In addition, due to the stronger drift region assisted depletion effect, the higher the dielectric constant, the higher the doping concentration corresponding to the maximum quality factor. Figure 3 As shown, the new structure using titanium dioxide has a doping concentration of 7×10 16 cm -3 8.72×10 9 W / cm 2 The maximum quality factor of hafnium dioxide is 5.4×10 16 cm -3 The obtained 4.36×10 9 W / cm 2Compared with the highest quality factor of the HKMG structure, it is improved by 100%. However, due to the high drift region doping concentration of the new structure using titanium dioxide when the maximum quality factor is reached, the drift region cannot be completely depleted, resulting in a breakdown voltage of only 1850 V. Compared with the corresponding breakdown voltage of 1986 V with the maximum quality factor achieved when using hafnium dioxide, it is reduced by 6.8%. In addition, hafnium dioxide is a commonly used material in HKMG structure, and its manufacturing process is mature. Therefore, considering these factors, the present invention uses hafnium dioxide as the best choice material for high-K dielectrics.
[0073] 2. Single-side width W of deep trench high-K dielectric area sg choose Building quality factor with different W sg The relationship curve of the maximum quality factor corresponding to W sg As the best W sg When building, other structural parameters need to be kept consistent, and the following are similar.
[0074] Figure 4 The present invention is shown in FIG. sg The breakdown voltage (BV), specific on-resistance (R on,sp ) and the change in quality factor (Figure of merit, FOM). Figure 4 The horizontal axis is W sg The vertical axes are breakdown voltage (BV), specific on-resistance (R on,sp ) and quality factor (Figure of merit, FOM). Figure 4 As shown in Figure (a), the breakdown voltage increases with W sg The breakdown voltage increases at first because as W sg As W increases, more electric field lines gather at the high-K metal gate, thereby increasing the electric field near the gate, and thus the breakdown voltage increases. The subsequent decrease in breakdown voltage is due to the increase in metal-insulator-semiconductor (MIS) capacitance with W sg The increase of decreases, making it impossible for the drift region to be completely depleted, thus reducing the breakdown voltage. Figure 4 The on-resistance is increased because the channel resistance increases with W sg increases with the increase of .
[0075] from Figure 4 As can be seen in Figure (b), the maximum quality factor point is point E, at which point, corresponding to W sg The maximum quality factor is 1.14×10 9 W / cm 2The corresponding breakdown voltage and on-resistance are 1524V and 2.03mΩ·cm respectively. 2 That is, the single side width W of the deep trench high-K dielectric region sg The best value is chosen to be 0.3µm.
[0076] 3. Split-gate metal thickness T sg choose Building quality factor with different T sg The relationship curve of the maximum quality factor is T sg As the best T sg .
[0077] Figure 5 The present invention shows that the split gate thickness T sg The breakdown voltage (BV), specific on-resistance (R on,sp ) and the change of quality factor (Figure of merit, FOM). Figure 5 In Figure (a), the horizontal axis is the split gate thickness T sg The vertical axes are breakdown voltage (BV) and specific on-resistance (R on,sp ), from which it can be seen that the breakdown voltage increases with the split gate thickness T sg The specific on-resistance also decreases with the increase of the split gate thickness T sg decreases with the increase of . Figure 5 In Figure (b), the horizontal axis is the split gate thickness T sg , the ordinate is the figure of merit (FOM), from which we can see that the maximum quality factor point is point F, at which point the split gate thickness T sg The maximum quality factor is 1.14×10 9 W / cm 2 The corresponding breakdown voltage and on-resistance are 1524V and 2.03mΩ·cm respectively. 2 That is, the split gate metal thickness T sg The best value is chosen to be 1µm.
[0078] 4. Spacing T between split gate metal and gate metal gap choose Construction quality factor with different spacing T gap The relationship curve of the maximum quality factor is T gap As the optimal spacing T gap .
[0079] Figure 6 The present invention shows that the gap The breakdown voltage (BV), specific on-resistance (Ron,sp ) and the change in quality factor (Figure of merit, FOM). Figure 6 In Figure (a), the horizontal axis is T gap The vertical axes are breakdown voltage (BV) and specific on-resistance (R on,sp ); It can be seen that the breakdown voltage and the specific on-resistance increase with the thickness T between the split gate and the gate. gap 's growth and changes continuously. Figure 6 In Figure (b), the horizontal axis is T gap , the ordinate is the figure of merit (FOM), and the maximum quality factor appears at point G. At this point, T gap The maximum quality factor is 1.75×10 9 W / cm 2 The corresponding breakdown voltage and on-resistance are 1714V and 1.67mΩ·cm respectively. 2 That is, the distance between the split gate metal and the gate metal is T gap The best value chosen is 1.4µm.
[0080] 5. Thickness T of Deep Trench High K Dielectric Region HK choose Building quality factor with different T HK The relationship curve of the maximum quality factor is T HK As the optimal deep trench high-K dielectric region thickness T HK .
[0081] Figure 7 The present invention shows that the HK The breakdown voltage (BV), specific on-resistance (R on,sp ) and the change of quality factor (Figure of merit, FOM). Figure 7 In Figure (a), the horizontal axis is T HK The vertical axes are breakdown voltage (BV) and specific on-resistance (R on,sp ); It can be seen that as T HK As T increases, the breakdown voltage initially increases. HK After reaching 13µm, the breakdown voltage gradually decreases. This is because as T HK As T increases, the modulation effect of the high-K dielectric on the drift region becomes stronger, resulting in denser electric field lines in the drift region, thereby increasing the breakdown voltage. HK As T increases, the electric field near the drain decreases, and the height of the electric field peak also decreases accordingly. The modulation effect of the high-K dielectric on the drift region gradually weakens, resulting in a slow decrease in the breakdown voltage. In addition, it can be seen from the figure that the specific on-resistance increases with THK This is because as T HK With the increase of , its auxiliary depletion effect on the drift region becomes more and more obvious, and the increasing concentration of the drift region leads to a decrease in the specific on-resistance.
[0082] exist Figure 7 In Figure (b), the horizontal axis is T HK , the ordinate is the quality factor (Figure of merit, FOM), from which we can see that the maximum quality factor appears at point H, at which point, T HK The maximum quality factor is 4.36×10 9 W / cm 2 The corresponding breakdown voltage and on-resistance are 1986V and 0.90mΩ·cm respectively. 2 That is, the thickness of the deep trench high-K dielectric region is T HK The best value chosen is 13µm.
[0083] A method for preparing a split high-K metal gate super junction silicon carbide trench MOSFET comprises the following steps.
[0084] Step 1: Make a superjunction structure A layer of N-type doped silicon carbide is epitaxially grown on the N-type heavily doped semiconductor drain region 1 to form a doping concentration of not less than 1×10 16 cm -3 The semiconductor N-type drift region 2 is formed; using a photoresist as a mask, a plasma dry etching is performed to symmetrically and vertically etch a semiconductor P-type drift region trench on the left and right sides of the top of the semiconductor drift region; the semiconductor P-type drift region trench penetrates the semiconductor drift region and contacts the semiconductor drain region; epitaxially grows P-type doped silicon carbide in the semiconductor P-type drift region trench; and the epitaxially grown P-type doped silicon carbide is pushed to form a doping concentration of not less than 1×10 16 cm -3 The semiconductor P-type drift region 3, the semiconductor P-type drift region and the semiconductor N-type drift region together form a super junction structure. After completion, the structure is as follows Figure 8 shown.
[0085] In this embodiment, the semiconductor P-type drift region and the semiconductor N-type drift region have the same height, and the width is preferably 1 to 1.5 microns.
[0086] Step 2: Make P-type well region and semiconductor source region A. Fabrication of P-type well region: Aluminum ions are implanted into the top of the semiconductor drift region by high-energy ion implantation to form a P-type well region 4. Rapid thermal annealing is used to activate and promote diffusion to form a fixed impurity distribution. The doping concentration of the P-type well region is not less than 1×10 17 cm -3The depth of the P-type well region is preferably 2 to 3 microns.
[0087] B. Fabrication of semiconductor N-type source region: Use the same method to implant high-dose nitrogen ions on the P-type well region to form a highly doped semiconductor N-type source region 5. The doping concentration of the semiconductor N-type source region is not less than 1×10 19 cm -3 The depth of the semiconductor N-type source region is preferably 1 to 2 micrometers. The semiconductor N-type source region is located directly above the semiconductor N-type drift region.
[0088] C. Fabrication of semiconductor P-type source region: Aluminum ions are implanted into the left and right sides of the top of the semiconductor source region located directly above the semiconductor P-type drift region using the same method to form a semiconductor P-type source region 6. Rapid thermal annealing is used to activate and promote diffusion to form a fixed impurity distribution. The doping concentration of the semiconductor P-type source region is not less than 1×10 19 cm -3 The depth of the semiconductor P-type source region is preferably 1 to 2 microns, and the width is preferably 0.9 to 1.1 microns. The completed structure is as follows Fig. 9 shown.
[0089] Step 3: Forming a deep trench high-K dielectric region Using photoresist as a mask, plasma dry etching is used to etch a groove vertically downward at the top center of the semiconductor source region; the groove sequentially penetrates the semiconductor source region and the P-type well region, and extends to the semiconductor N-type drift region; wherein the etching depth of the groove in the semiconductor drift region is greater than half of the thickness of the semiconductor drift region, but less than the thickness of the semiconductor drift region, preferably 13 to 15 microns, and the bottom of the groove does not contact the semiconductor drain region; the width of the groove is greater than the gate metal and the split gate metal, and magnetron sputtering deposition is used to deposit a set thickness of high-K dielectric on the bottom and side of the groove, thereby forming a deep trench high-K dielectric region 7, and the completed structure is as shown Fig.10 shown.
[0090] Step 4, depositing split gate metal: a split gate metal 8 with a thickness of 1 micron is coaxially deposited in the deep trench high-K dielectric region made in step 3 by magnetron sputtering. The completed structure is as follows: Fig.11 shown.
[0091] In this embodiment, the split gate metal is preferably made of metal Ni, Ti or Al, etc., and is deposited by magnetron sputtering and then rapidly thermally annealed to form a metal alloy to achieve good ohmic contact. The thickness of the split gate metal is preferably 0.8 to 1.2 microns, and the width is preferably 0.6 to 0.8 microns.
[0092] Step 5: Forming a high-K gate dielectric region: Plasma dry etching is used to etch the deep trench high-K dielectric region at the top of the split gate metal vertically downward from the top to the top of the split gate metal through a mask, while removing the metal deposited on the sidewalls; magnetron sputtering is used to deposit a thickness of T on the bottom and side of the trench. gap The high-K dielectric is then formed to form a high-K gate dielectric region. The completed structure is as follows Fig.12 shown.
[0093] In this embodiment, the high-K gate dielectric region is preferably 4 to 4.5 microns in depth and 0.8 to 1 micron in width.
[0094] Step 6, depositing metal electrodes: the metal electrodes include gate metal 9, source metal electrode 10 and drain metal electrode 11; wherein the gate metal is deposited in the high-K gate dielectric region produced in step 5 by magnetron sputtering; the source metal electrode is deposited on the top of the semiconductor source region by magnetron sputtering, respectively contacting the semiconductor P-type source region and the semiconductor N-type source region; the drain metal electrode is deposited on the bottom of the semiconductor drain region by magnetron sputtering.
[0095] The gate metal, source metal electrode and drain metal electrode are preferably made of metal Ni, Ti or Al, etc., and are deposited by magnetron sputtering and then rapidly thermally annealed to form a metal alloy to achieve good ohmic contact.
[0096] Fig.13 Figure of merit (FOM) and drift region doping concentration (N) of a split high-K metal gate superjunction silicon carbide trench MOSFET (also called a new structure), a split gate superjunction silicon carbide trench MOSFET without a high-K dielectric (a conventional split gate structure), and a conventional superjunction silicon carbide trench MOSFET (also called a conventional structure) provided by the present invention. SJ ). The high-K dielectric of the split high-K metal gate super-junction silicon carbide trench MOSFET is hafnium dioxide, and the other structural parameters of the three devices are consistent.
[0097] exist Fig.13 In FIG. 5 , the maximum quality factor points of the conventional structure, the conventional split-gate structure and the new structure are points J, K and L respectively.
[0098] In the conventional structure, the parameters corresponding to point J are: the quality factor is 1.64×10 9 W / cm 2 , the on-resistance is 2.21mΩ·cm 2 , the breakdown voltage is 1906V.
[0099] In the conventional split-gate structure, the parameters corresponding to point K are: the quality factor is 2.02×10 9 W / cm2 , the on-resistance is 1.84mΩ·cm 2 , the breakdown voltage is 1934V.
[0100] In the new structure, the parameters corresponding to point L are: the quality factor is 4.36×10 9 W / cm 2 , on-resistance is 0.90mΩ·cm 2 , the breakdown voltage is 1986V.
[0101] Depend on Fig.13 It can be seen that all three devices have maximum FOM values. Due to the comprehensive modulation effect of the high-K dielectric deep trench region, the FOM value of the split high-K metal gate super-junction silicon carbide trench MOSFET proposed in the present invention reaches 4.36×10 9 W / cm 2 Compared with the conventional split-gate superjunction silicon carbide trench MOSFET and the conventional superjunction silicon carbide trench MOSFET, the FOM values are increased by 115.8% and 165.8% respectively. Taking the highest point of the FOM value as the best optimization point, the breakdown voltage (BV) of the invention at the highest FOM value reaches 1986V, and the on-resistance (R on,sp ) reaches 0.90mΩ, and the breakdown voltage is increased by 2.6% and 4.2% respectively compared with the other two structures, the on-resistance is reduced by 51.1% and 59.3% respectively, and the drift region doping concentration is increased by more than three times.
[0102] Fig.14 A comparison diagram of the longitudinal electric field distribution of a split high-K metal gate super-junction silicon carbide trench MOSFET (also called a new structure) provided by the present invention, a split gate super-junction silicon carbide trench MOSFET without a high-K dielectric (conventional split gate structure), and a conventional super-junction silicon carbide trench MOSFET is shown. Fig.14 In the figure, the ordinate is the electric field strength and the abscissa is the longitudinal position of the device. Fig.14 It can be seen that for conventional structures, the electric field strength at the corner of the gate trench is close to 10MV / cm, which is very prone to premature breakdown. For the new structure provided by the present invention, the electric field strength at the corner of the gate trench is reduced to below 3MV / cm, and the gate oxide stability is greatly improved. In addition, the high-K dielectric deep trench region introduces a new electric field peak in the drift region, which improves the voltage resistance performance of the device.
[0103] Fig.15 A comparison diagram of the gate charges of a split high-K metal gate super-junction silicon carbide trench MOSFET (also called a new structure) provided by the present invention, a split gate super-junction silicon carbide trench MOSFET without a high-K dielectric (conventional split gate structure), and a conventional super-junction silicon carbide trench MOSFET is shown. Fig.15The vertical axis is the gate-source voltage, and the horizontal axis is the gate charge. Fig.15 It can be seen that, for the new structure provided by the present invention, the gate charge is smaller than that of the conventional split-gate structure and the conventional super junction structure, which greatly reduces the switching loss of the device and improves the dynamic performance of the device.
[0104] Fig.16 A comparison diagram of the drain-gate capacitance of a split high-K metal gate super-junction silicon carbide trench MOSFET (also called a new structure) provided by the present invention, a split-gate super-junction silicon carbide trench MOSFET without a high-K dielectric (conventional split-gate structure), and a conventional super-junction silicon carbide trench MOSFET is shown. Fig.16 The vertical axis is the drain-gate capacitance, and the horizontal axis is the drain-source voltage. Fig.16 It can be seen that for the new structure provided by the present invention, its drain-gate capacitance is smaller than that of the conventional split-gate structure and the conventional superjunction structure, which greatly reduces the switching loss of the device and improves the dynamic performance of the device.
[0105] The preferred embodiments of the present invention are described in detail above; however, the present invention is not limited to the specific details in the above embodiments. Within the technical concept of the present invention, various equivalent transformations can be made to the technical solutions of the present invention, and these equivalent transformations all belong to the protection scope of the present invention.
Claims
1. A split high-K metal gate super junction silicon carbide trench MOSFET, characterized in that: It includes a semiconductor drain region, a super junction structure, a P-type well region, a semiconductor source region and a split high-K metal gate structure; A drain metal electrode is deposited at the bottom of the semiconductor drain region; The superjunction structure is epitaxially grown on the top of the semiconductor drain region, including a semiconductor N-type drift region and a semiconductor P-type drift region coaxially arranged from the inside to the outside; The P-type well region is arranged on the top of the super junction structure; The semiconductor source region is arranged on the top of the P-type well region, and a source-end metal electrode is deposited on the top of the semiconductor source region; The semiconductor source region includes a semiconductor N-type source region and a semiconductor P-type source region which are coaxially arranged in sequence from the inside to the outside; The split high-K metal gate structure includes a deep trench high-K dielectric region, a split gate metal and a gate metal; The deep trench high-K dielectric region is coaxially embedded in the middle of the semiconductor N-type source region, the P-type well region and the semiconductor N-type drift region; the top surface of the deep trench high-K dielectric region is flush with the top surface of the semiconductor N-type source region; the thickness of the deep trench high-K dielectric region is T HK Greater than half of the thickness of the semiconductor N-type drift region, but less than the thickness of the super junction structure; the width of the deep trench high-K dielectric region is less than the width of the semiconductor N-type drift region; The split gate metal and the gate metal are coaxially arranged in the middle of the deep trench high-K dielectric region from top to bottom; the top surface of the gate metal is flush with the top surface of the deep trench high-K dielectric region; there is a spacing T between the split gate metal and the gate metal gap There is a set spacing greater than zero between the bottom surface of the split gate metal and the bottom surface of the deep trench high-K dielectric region.
2. The split high-K metal gate super junction silicon carbide trench MOSFET according to claim 1, characterized in that: The dielectric constant ε of the high-K dielectric in the deep trench high-K dielectric region is greater than 3.
9. By selecting the dielectric constant ε, the MOSFET has a maximum quality factor without being lower than a set breakdown voltage.
3. The split high-K metal gate super junction silicon carbide trench MOSFET according to claim 2, characterized in that: The high-K dielectric in the deep trench high-K dielectric region is hafnium dioxide.
4. The split high-K metal gate super junction silicon carbide trench MOSFET according to claim 1, characterized in that: The single side width of the deep trench high-K dielectric region outside the split gate metal is W sg ; By constructing the quality factor and different W sg The relationship curve of the maximum quality factor corresponding to W sg As the best W sg .
5. The split high-K metal gate super junction silicon carbide trench MOSFET according to claim 1, characterized in that: Assume the thickness of the split gate metal is T sg ; By constructing the quality factor and different T sg The relationship curve of the maximum quality factor is T sg As the best T sg .
6. The split high-K metal gate super junction silicon carbide trench MOSFET according to claim 1, characterized in that: By constructing the quality factor and different spacing T gap The relationship curve of the maximum quality factor is T gap As the optimal spacing T gap .
7. The split high-K metal gate super junction silicon carbide trench MOSFET according to claim 1, characterized in that: By constructing the quality factor with different T HK The relationship curve of the maximum quality factor is T HK As the optimal deep trench high-K dielectric region thickness T HK .
8. The split high-K metal gate super junction silicon carbide trench MOSFET according to claim 1, characterized in that: The thickness of the semiconductor source region does not exceed the thickness of the P-type well region; the width of the split gate metal is less than or equal to the width of the gate metal.
9. A method for preparing a split high-K metal gate super junction silicon carbide trench MOSFET according to any one of claims 1 to 8, characterized in that: The steps include: Step 1, making a super junction structure: epitaxially growing a layer of N-type doped silicon carbide on the semiconductor drain region to form a semiconductor N-type drift region; using plasma dry etching, symmetrically and vertically etching semiconductor P-type drift region grooves on the left and right sides of the semiconductor N-type drift region; The bottom of the semiconductor P-type drift region trench is in contact with the semiconductor drain region; P-type doped silicon carbide is epitaxially grown in the semiconductor P-type drift region trench and a junction is formed to form a semiconductor P-type drift region; The semiconductor P-type drift region and the semiconductor N-type drift region are of the same height, and the semiconductor P-type drift region and the semiconductor N-type drift region together form a super junction structure; Step 2, making a P-type well region and a semiconductor source region: using ion implantation and annealing, a P-type well region and a semiconductor source region are sequentially made on the top of the super junction structure made in step 1; wherein the semiconductor N-type source region in the semiconductor source region is located directly above the semiconductor N-type drift region; and the semiconductor P-type source region in the semiconductor source region is located directly above the semiconductor P-type drift region; Step 3, forming a deep trench high-K dielectric region: using plasma dry etching, a trench is etched vertically downward at the center of the top of the semiconductor source region; the trench sequentially penetrates the semiconductor source region and the P-type well region, and extends to the semiconductor N-type drift region; using a magnetron sputtering method, a high-K dielectric of a set thickness is deposited on the bottom and side of the trench, thereby forming a deep trench high-K dielectric region; Step 4: Deposit split gate metal: Use magnetron sputtering to deposit a layer with a thickness of T sg The split gate metal is coaxially deposited in the deep trench high-K dielectric region made in step 3; Step 5: Forming a high-K gate dielectric region: First, the deep trench high-K dielectric region located at the top of the split gate metal is etched vertically downward from the top to the top of the split gate metal through a mask; then, a magnetron sputtering method is used to deposit a thickness of T on the top of the split gate metal. gap The high-K dielectric is connected to the deep trench high-K dielectric regions on both sides, thereby forming a high-K gate dielectric region; Step 6, depositing metal electrodes: the metal electrodes include gate metal, source metal electrode and drain metal electrode; wherein the gate metal is deposited in the high-K gate dielectric region produced in step 5 by magnetron sputtering; the source metal electrode is deposited on the top of the semiconductor source region by magnetron sputtering, respectively contacting the semiconductor P-type source region and the semiconductor N-type source region; the drain metal electrode is deposited on the bottom of the semiconductor drain region by magnetron sputtering.
10. The method for preparing a split high-K metal gate super junction silicon carbide trench MOSFET according to claim 9, characterized in that: In step 1, the doping concentration of the semiconductor N-type drift region and the semiconductor P-type drift region is not less than 1×10 16 cm -3 In step 2, the doping concentration of the P-type well region is not less than 1×10 17 cm -3 The doping concentration of the semiconductor N-type source region and the semiconductor P-type source region is not less than 1×10 19 cm -3 .
Citation Information
Patent Citations
Integrated high-K dielectric three-groove type silicon carbide longitudinal power device and preparation method thereof
CN117766566A
Super-junction SGT structure with High K medium and manufacturing method of super-junction SGT structure
CN117790312A
Trench gate mosfet device
US20130153999A1
Novel SGT superjunction mosfet structure
US20190206988A1