Efficient filtering composite cigarette holder and preparation method thereof
Through the stacking design of polylactic acid electrospinning membrane and zigzag structure, the existing smoke filtering nozzle has solved the problem of smoke filtration efficiency and contact area optimization, and achieved efficient filtering of harmful substances in smoke, improving adsorption effect and air Liquidity.
Patent Information
- Application Number
- CN202411234515.8
- Authority / Receiving Office
- CN · China
- Patent Type
- Applications(China)
- Current Assignee / Owner
- Filing Date
- 2024-09-04
- Publication Date
- 2024-11-15
AI Technical Summary
Existing filter nozzles have limitations in improving filtration efficiency, especially in increasing the contact area between smoke and filter material and optimizing the pore structure, it is difficult to effectively intercept harmful substances in smoke.
The polylactic acid electrospinning membrane, serrated polylactic acid electrospinning membrane and skin core structure polylactic fiber three-layer laminated composite structure is adopted. The contact area between smoke and filter material is increased through the serrated structure and stacking angle design, and the filtration efficiency is improved. .
It significantly improves the smoke filtration efficiency, enhances the adsorption ability to harmful substances, provides better filtration and adsorption effect, and ensures air flow and reduces suction resistance.
Smart Images

Figure CN118947960A_ABST
Abstract
Description
Technical Field
[0001] The invention relates to the technical field of rolled tobacco, and in particular to a high-efficiency filtering composite cigarette holder and a preparation method thereof. Background Art
[0002] The background technology of filter cigarette holders originated in the early 20th century, when tobacco companies invented early filter tips in order to reduce the discomfort of tobacco leaves directly touching the lips. The original filter tips were made of paper, and later developed to use materials such as cotton and asbestos. In the 1950s, with the development of acetate fiber, filter cigarettes began to be widely used. The materials of filter tips have evolved from paper and cotton to acetate fiber, activated carbon, polypropylene tow, inorganic mineral fiber and other materials. In the past 30 years, the emergence of new technologies has changed the shape of filter tips, such as laser perforation technology, which allows a portion of air to be inhaled during inhalation, thereby reducing the concentration of cigarette smoke. In addition to the basic filtering function, some filter tips also add substances such as mint to reduce the irritation of smoke, or use nanomaterials to improve filtering efficiency. The filtration efficiency of the filter depends on its design and materials, and includes mechanisms such as direct interception, inertial compression and diffusion precipitation. Improving the filtration efficiency of filter cigarette holders can be achieved through a variety of technical means. The following are some key methods and innovations: (1) Multi-stage filtration system: By setting up multiple filtration layers, such as activated carbon layers and nano-scale filter material layers, particles of different sizes in smoke can be more effectively intercepted and harmful chemicals can be adsorbed; (2) Optimizing pore structure: Designing porous filter materials, by optimizing porosity and pore size, to effectively intercept large particles in smoke, while ensuring air flow and reducing inhalation resistance; (3) Activated carbon adsorption: Using activated carbon as a filter material, and utilizing its high adsorption performance to adsorb harmful substances in smoke, such as tar and nicotine; (4) Application of nanotechnology: Using nanomaterials as filter media, due to their ultra-high filtration efficiency, they can fully filter out harmful substances in cigarettes; (5) Air circulation interval adjustment: Setting adjustable air circulation intervals between filter elements allows users to adjust inhalation resistance according to their personal smoking habits; (6) Using special filter elements: Some filter cigarette holders use special filter elements, such as filter elements containing herbal essences such as ginseng, which can not only filter tar but also provide certain health benefits. Through these methods, the filtration efficiency of the filter cigarette holder is significantly improved, which helps to reduce the harmful substances inhaled by smokers. Summary of the invention
[0003] Technical problem to be solved: The purpose of the present invention is to provide a high-efficiency filtering composite cigarette holder, which is formed by three-layer composite winding of polylactic acid electrospinning membrane, zigzag polylactic acid electrospinning membrane and skin-core structure polylactic acid fiber. The zigzag structure and the angled design increase the contact area between smoke and filter material, thereby improving the filtering efficiency.
[0004] Technical solution: A high-efficiency filtering composite cigarette holder, which is formed by three-layer lamination and composite winding of a polylactic acid electrospinning membrane, a zigzag polylactic acid electrospinning membrane and a skin-core structured polylactic acid fiber. Preferably, the method for preparing the polylactic acid electrospinning membrane comprises the following steps: S11. Adding polylactic acid to dichloromethane and stirring to dissolve to obtain a 5.5-7wt% electrospinning solution; S12. The electrospinning solution is electrospun to obtain an electrospinning fiber membrane, with a voltage of 16-20 kV, a flow rate of 0.8-1.5 mL / h, and a receiving distance of 15-22 cm. Preferably, the method for preparing the polylactic acid electrospinning membrane comprises the following steps: S21. Adding polylactic acid to dichloromethane and stirring to dissolve to obtain 5.5-7wt% electrospinning solution; S22 electrospins the electrospinning solution to obtain an electrospinning fiber membrane, with a voltage of 16-20 kV, a flow rate of 0.8-1.5 mL / h, and a receiving distance of 15-22 cm. S23. Placing the electrospun fiber membrane in a zigzag-shaped mold for heat setting treatment to obtain a zigzag-shaped polylactic acid fiber membrane. Preferably, the method for preparing the polylactic acid electrospinning membrane further comprises the following steps: adding nanoporous carbon balls to the electrospinning solution prepared in S21, wherein the content of the nanoporous carbon balls in the electrospinning solution is 1.5-3wt%. Preferably, the temperature of the heat setting treatment in step S23 is 100-120° C. and the time is 40-60 seconds. Preferably, the sawtooth structure is formed by connecting a plurality of circular arc sawtooth units in sequence, the diameter of each circular arc sawtooth unit is 0.5-1.2 mm, and the interval between adjacent sawtooth paper pieces is 0.1-0.2 mm. The above-mentioned method for preparing the high-efficiency filtering composite cigarette holder comprises the following steps: S1. Using low melting point polylactic acid as the skin material and high melting point polylactic acid as the core material, the skin material and the core material are dried and melted to obtain a skin spinning solution and a core spinning solution, and spinning is performed to obtain a skin-core structure polylactic acid fiber; S2. The polylactic acid electrospun membrane, the skin-core structure polylactic acid fiber and the zigzag polylactic acid electrospun membrane are stacked in three layers at a certain angle to obtain a laminated composite structure; S3. With the direction parallel to the core-skin structure polylactic acid fiber as the axis, the laminated composite structure is wound to obtain a cigarette holder tow, and then a high-efficiency filtering composite cigarette holder is obtained through thermal bonding. Preferably, in step S1, the mass ratio of the low melting point polylactic acid to the high melting point polylactic acid is 50-70:30-50, the melting point of the low melting point polylactic acid is 115-130°C, and the melting point of the high melting point polylactic acid is 150-170°C. Preferably, in the step S2, the axis of the arc-shaped through groove in the arc-shaped sawtooth unit of the sawtooth polylactic acid electrospinning membrane is at an angle of 30-60° to the core-skin structure polylactic acid fiber. Preferably, in step S2, the mass ratio of the polylactic acid electrospinning membrane, the core-skin structure polylactic acid fiber and the zigzag polylactic acid electrospinning membrane is 4-5:5.5-8:6.5-8.5. Beneficial effects: The high-efficiency filtering composite cigarette holder of the present invention has the following advantages: 1. The cigarette holder of the present invention is formed by three layers of composite winding of polylactic acid electrospinning membrane, zigzag polylactic acid electrospinning membrane and skin-core structure polylactic acid fiber. The zigzag polylactic acid electrospinning membrane is 30-60° with the axis of the cigarette holder, which is similar to the swirl structure. The zigzag structure and the angled design increase the contact area between smoke and filter material, thereby improving the filtration efficiency. 2. The polylactic acid fibers of the sheath-core structure of the present invention are spun and woven using two polylactic acid raw materials with different melting points. During the thermal bonding process, the polylactic acid fibers added to the sheath layer will melt to a certain extent, so that the polylactic acid fibers are bonded to each other, and the polylactic acid fibers and the polylactic acid electrospun fiber bundles are bonded to each other; 3. The diameter of the arc sawtooth unit in the sawtooth structure of the present invention is 0.5-1.2 mm. The mouthpiece in this diameter range has a better filtering and adsorption effect. This is because the arc sawtooth of this diameter can increase the contact area, and the flow rate of the smoke will not be affected by the diameter when the smoke passes through, and the sensory effect is better. BRIEF DESCRIPTION OF THE DRAWINGS Figure 1 It is a schematic diagram of the structure of the high-efficiency filtering composite cigarette holder prepared by the present invention, wherein 1 is a polylactic acid electrospinning membrane, 2 is a skin-core structured polylactic acid fiber, and 3 is a zigzag polylactic acid electrospinning membrane. DETAILED DESCRIPTION The present invention will be further described below in conjunction with embodiments, which are explanations of the present invention and are not limited to the following embodiments: Example 1 A method for preparing a high-efficiency filtering composite cigarette holder, the method comprising the following steps: S1. Using low-melting-point polylactic acid with a melting point of 115°C as the skin material and high-melting-point polylactic acid with a melting point of 150°C as the core material, drying and melting the skin material and the core material to obtain skin spinning solution and core spinning solution, respectively, the mass ratio of low-melting-point polylactic acid to high-melting-point polylactic acid is 50:30, spinning to obtain skin-core structure polylactic acid fiber; S2. The polylactic acid electrospinning membrane, the core-skin structure polylactic acid fiber and the zigzag polylactic acid electrospinning membrane are stacked in three layers at a certain angle, the mass ratio of the polylactic acid electrospinning membrane, the core-skin structure polylactic acid fiber and the zigzag polylactic acid electrospinning membrane is 4:5.5:6.5, and the axis of the arc-shaped through groove in the arc-shaped zigzag unit of the zigzag polylactic acid electrospinning membrane is 30° with the core-skin structure polylactic acid fiber to obtain a laminated composite structure; S3. With the direction parallel to the core-sheath structure of the polylactic acid fiber as the axis, the laminated composite structure is wound to obtain a cigarette holder tow, and then thermally bonded to obtain a high-efficiency filter composite cigarette holder; The preparation method of the polylactic acid electrospinning membrane comprises the following steps: S11. Adding polylactic acid to dichloromethane and stirring to dissolve, to obtain a 5.5 wt% electrospinning solution; S12. The electrospinning solution was electrospun to obtain an electrospinning fiber membrane, the voltage was 16 kV, the flow rate was 0.8 mL / h, the receiving distance was 22 cm, and a polylactic acid electrospinning membrane was prepared; S13. Take a portion of the polylactic acid electrospun membrane, place the electrospun fiber membrane in a zigzag structure mold for heat setting treatment, the heat setting temperature is 100°C, the time is 60s, and a polylactic acid fiber membrane with a zigzag structure is obtained. The zigzag structure is formed by connecting a number of circular arc zigzag units in sequence, the diameter of each circular arc zigzag unit is 1.2mm, and the interval between adjacent zigzag paper pieces is 0.1mm. Example 2 A method for preparing a high-efficiency filtering composite cigarette holder, the method comprising the following steps: S1. Using low-melting-point polylactic acid with a melting point of 130°C as the skin material and high-melting-point polylactic acid with a melting point of 170°C as the core material, drying and melting the skin material and the core material to obtain skin spinning solution and core spinning solution, respectively, the mass ratio of low-melting-point polylactic acid to high-melting-point polylactic acid is 70:50, spinning to obtain skin-core structure polylactic acid fiber; S2. The polylactic acid electrospinning membrane, the core-skin structure polylactic acid fiber and the zigzag polylactic acid electrospinning membrane are stacked in three layers at a certain angle, the mass ratio of the polylactic acid electrospinning membrane, the core-skin structure polylactic acid fiber and the zigzag polylactic acid electrospinning membrane is 5:5.8:8.5, and the axis of the arc-shaped through groove in the arc-shaped zigzag unit of the zigzag polylactic acid electrospinning membrane is 60° with the core-skin structure polylactic acid fiber to obtain a laminated composite structure; S3. With the direction parallel to the core-sheath structure of the polylactic acid fiber as the axis, the laminated composite structure is wound to obtain a cigarette holder tow, and then thermally bonded to obtain a high-efficiency filter composite cigarette holder; The preparation method of the polylactic acid electrospinning membrane comprises the following steps: S11. adding polylactic acid to dichloromethane and stirring to dissolve to obtain a 7 wt % electrospinning solution; S12. The electrospinning solution was electrospun to obtain an electrospinning fiber membrane at a voltage of 20 kV, a flow rate of 1.5 mL / h, and a receiving distance of 22 cm to prepare a polylactic acid electrospinning membrane; S13. Take a portion of the polylactic acid electrospun membrane, place the electrospun fiber membrane in a zigzag structure mold for heat setting treatment, the heat setting temperature is 120°C, the time is 40s, and a polylactic acid fiber membrane with a zigzag structure is obtained. The zigzag structure is formed by connecting a number of circular arc zigzag units in sequence, the diameter of each circular arc zigzag unit is 0.5mm, and the interval between adjacent zigzag paper pieces is 0.2mm. Example 3 A method for preparing a high-efficiency filtering composite cigarette holder, the method comprising the following steps: S1. Using low-melting-point polylactic acid with a melting point of 120°C as the skin material and high-melting-point polylactic acid with a melting point of 160°C as the core material, drying and melting the skin material and the core material to obtain skin spinning solution and core spinning solution respectively, wherein the mass ratio of low-melting-point polylactic acid to high-melting-point polylactic acid is 6:4, and spinning is performed to obtain skin-core structure polylactic acid fibers; S2. The polylactic acid electrospinning membrane, the core-skin structure polylactic acid fiber and the zigzag polylactic acid electrospinning membrane are stacked in three layers at a certain angle, the mass ratio of the polylactic acid electrospinning membrane, the core-skin structure polylactic acid fiber and the zigzag polylactic acid electrospinning membrane is 4.5:7:7, and the axis of the arc-shaped through groove in the arc-shaped zigzag unit of the zigzag polylactic acid electrospinning membrane is 45° to the core-skin structure polylactic acid fiber to obtain a laminated composite structure; S3. With the direction parallel to the core-sheath structure of the polylactic acid fiber as the axis, the laminated composite structure is wound to obtain a cigarette holder tow, and then thermally bonded to obtain a high-efficiency filter composite cigarette holder; The preparation method of the polylactic acid electrospinning membrane comprises the following steps: S11. adding polylactic acid to dichloromethane and stirring to dissolve to obtain a 6 wt % electrospinning solution; S12. The electrospinning solution was electrospun to obtain an electrospinning fiber membrane at a voltage of 18 kV, a flow rate of 1.2 mL / h, and a receiving distance of 18 cm to prepare a polylactic acid electrospinning membrane; S13. Take a portion of the polylactic acid electrospun membrane, place the electrospun fiber membrane in a zigzag structure mold for heat setting treatment, the heat setting temperature is 110°C, the time is 50s, and a polylactic acid fiber membrane with a zigzag structure is obtained. The zigzag structure is formed by connecting a number of circular arc zigzag units in sequence, the diameter of each circular arc zigzag unit is 1mm, and the interval between adjacent zigzag paper pieces is 0.1mm. Example 4 A method for preparing a high-efficiency filtering composite cigarette holder, the method comprising the following steps: S1. Using low-melting-point polylactic acid with a melting point of 120°C as the skin material and high-melting-point polylactic acid with a melting point of 155°C as the core material, drying and melting the skin material and the core material to obtain skin spinning solution and core spinning solution, respectively, wherein the mass ratio of low-melting-point polylactic acid to high-melting-point polylactic acid is 55:35, and spinning is performed to obtain skin-core structure polylactic acid fibers; S2. The polylactic acid electrospinning membrane, the core-skin structure polylactic acid fiber and the zigzag polylactic acid electrospinning membrane are stacked in three layers at a certain angle, the mass ratio of the polylactic acid electrospinning membrane, the core-skin structure polylactic acid fiber and the zigzag polylactic acid electrospinning membrane is 4:6:7, and the axis of the arc-shaped through groove in the arc-shaped zigzag unit of the zigzag polylactic acid electrospinning membrane is 40° to the core-skin structure polylactic acid fiber to obtain a laminated composite structure; S3. With the direction parallel to the core-sheath structure of the polylactic acid fiber as the axis, the laminated composite structure is wound to obtain a cigarette holder tow, and then thermally bonded to obtain a high-efficiency filter composite cigarette holder; The preparation method of the polylactic acid electrospinning membrane comprises the following steps: S11. adding polylactic acid to dichloromethane and stirring to dissolve to obtain a 6 wt % electrospinning solution; S12. The electrospinning solution was electrospun to obtain an electrospinning fiber membrane. The voltage was 20 kV, the flow rate was 1.2 mL / h, and the receiving distance was 22 cm to prepare a polylactic acid electrospinning membrane. The preparation method of the polylactic acid electrospinning membrane comprises the following steps: S21. The polylactic acid was added to dichloromethane and stirred to dissolve to obtain a 5.5wt% electrospinning solution, and nanoporous carbon spheres were added to the electrospinning solution. The content of the nanoporous carbon spheres in the electrospinning solution was 3wt%; S22 electrospins the electrospinning solution to obtain an electrospinning fiber membrane with a voltage of 16 kV, a flow rate of 1.2 mL / h, and a receiving distance of 18 cm. S23. The electrospun fiber membrane is placed in a zigzag structure mold for heat setting treatment. The heat setting temperature is 100°C and the time is 60s to obtain a polylactic acid fiber membrane with a zigzag structure. The zigzag structure is composed of a number of circular arc zigzag units connected in sequence. The diameter of each circular arc zigzag unit is 0.8mm, and the interval between adjacent zigzag paper pieces is 0.2mm. Example 5 A method for preparing a high-efficiency filtering composite cigarette holder, the method comprising the following steps: S1. Using low-melting-point polylactic acid with a melting point of 125°C as the skin material and high-melting-point polylactic acid with a melting point of 165°C as the core material, drying and melting the skin material and the core material to obtain skin spinning solution and core spinning solution, respectively, wherein the mass ratio of low-melting-point polylactic acid to high-melting-point polylactic acid is 65:45, and spinning is performed to obtain skin-core structure polylactic acid fibers; S2. The polylactic acid electrospinning membrane, the core-skin structure polylactic acid fiber and the zigzag polylactic acid electrospinning membrane are stacked in three layers at a certain angle, the mass ratio of the polylactic acid electrospinning membrane, the core-skin structure polylactic acid fiber and the zigzag polylactic acid electrospinning membrane is 5:7:8, and the axis of the arc-shaped through groove in the arc-shaped zigzag unit of the zigzag polylactic acid electrospinning membrane is 50° with the core-skin structure polylactic acid fiber to obtain a laminated composite structure; S3. With the direction parallel to the core-sheath structure of the polylactic acid fiber as the axis, the laminated composite structure is wound to obtain a cigarette holder tow, and then thermally bonded to obtain a high-efficiency filter composite cigarette holder; The preparation method of the polylactic acid electrospinning membrane comprises the following steps: S11. adding polylactic acid to dichloromethane and stirring to dissolve to obtain a 6 wt % electrospinning solution; S12. The electrospinning solution was electrospun to obtain an electrospinning fiber membrane. The voltage was 16 kV, the flow rate was 1 mL / h, and the receiving distance was 18 cm to prepare a polylactic acid electrospinning membrane. The preparation method of the polylactic acid electrospinning membrane comprises the following steps: S21. The polylactic acid was added to dichloromethane and stirred to dissolve to obtain a 7wt% electrospinning solution, and nanoporous carbon spheres were added to the electrospinning solution. The content of the nanoporous carbon spheres in the electrospinning solution was 1.5wt%; S22 electrospins the electrospinning solution to obtain an electrospinning fiber membrane with a voltage of 20 kV, a flow rate of 1 mL / h, and a receiving distance of 22 cm. S23. The electrospun fiber membrane is placed in a zigzag structure mold for heat setting treatment. The heat setting temperature is 120°C and the time is 40s to obtain a polylactic acid fiber membrane with a zigzag structure. The zigzag structure is composed of a number of circular arc zigzag units connected in sequence. The diameter of each circular arc zigzag unit is 1.1mm, and the interval between adjacent zigzag paper pieces is 0.1mm. Example 6 A method for preparing a high-efficiency filtering composite cigarette holder, the method comprising the following steps: S1. Using low-melting-point polylactic acid with a melting point of 120°C as the skin material and high-melting-point polylactic acid with a melting point of 160°C as the core material, drying and melting the skin material and the core material to obtain skin spinning solution and core spinning solution respectively, wherein the mass ratio of low-melting-point polylactic acid to high-melting-point polylactic acid is 6:4, and spinning is performed to obtain skin-core structure polylactic acid fibers; S2. The polylactic acid electrospinning membrane, the core-skin structure polylactic acid fiber and the zigzag polylactic acid electrospinning membrane are stacked in three layers at a certain angle, the mass ratio of the polylactic acid electrospinning membrane, the core-skin structure polylactic acid fiber and the zigzag polylactic acid electrospinning membrane is 4.5:7:7, and the axis of the arc-shaped through groove in the arc-shaped zigzag unit of the zigzag polylactic acid electrospinning membrane is 30° with the core-skin structure polylactic acid fiber to obtain a laminated composite structure; S3. With the direction parallel to the core-sheath structure of the polylactic acid fiber as the axis, the laminated composite structure is wound to obtain a cigarette holder tow, and then thermally bonded to obtain a high-efficiency filter composite cigarette holder; The preparation method of the polylactic acid electrospinning membrane comprises the following steps: S11. adding polylactic acid to dichloromethane and stirring to dissolve to obtain a 6 wt % electrospinning solution; S12. The electrospinning solution was electrospun to obtain an electrospinning fiber membrane at a voltage of 18 kV, a flow rate of 1.2 mL / h, and a receiving distance of 18 cm to prepare a polylactic acid electrospinning membrane; S13. Take a portion of the polylactic acid electrospun membrane, place the electrospun fiber membrane in a zigzag structure mold for heat setting treatment, the heat setting temperature is 110°C, the time is 50s, and a polylactic acid fiber membrane with a zigzag structure is obtained. The zigzag structure is formed by connecting a number of circular arc zigzag units in sequence, the diameter of each circular arc zigzag unit is 1mm, and the interval between adjacent zigzag paper pieces is 0.1mm. Example 7 A method for preparing a high-efficiency filtering composite cigarette holder, the method comprising the following steps: S1. Using low-melting-point polylactic acid with a melting point of 120°C as the skin material and high-melting-point polylactic acid with a melting point of 160°C as the core material, drying and melting the skin material and the core material to obtain skin spinning solution and core spinning solution respectively, wherein the mass ratio of low-melting-point polylactic acid to high-melting-point polylactic acid is 6:4, and spinning is performed to obtain skin-core structure polylactic acid fibers; S2. The polylactic acid electrospinning membrane, the core-skin structure polylactic acid fiber and the zigzag polylactic acid electrospinning membrane are stacked in three layers at a certain angle, the mass ratio of the polylactic acid electrospinning membrane, the core-skin structure polylactic acid fiber and the zigzag polylactic acid electrospinning membrane is 4.5:7:7, and the axis of the arc-shaped through groove in the arc-shaped zigzag unit of the zigzag polylactic acid electrospinning membrane is 60° with the core-skin structure polylactic acid fiber to obtain a laminated composite structure; S3. With the direction parallel to the core-sheath structure of the polylactic acid fiber as the axis, the laminated composite structure is wound to obtain a cigarette holder tow, and then thermally bonded to obtain a high-efficiency filter composite cigarette holder; The preparation method of the polylactic acid electrospinning membrane comprises the following steps: S11. adding polylactic acid to dichloromethane and stirring to dissolve to obtain a 6 wt % electrospinning solution; S12. The electrospinning solution was electrospun to obtain an electrospinning fiber membrane at a voltage of 18 kV, a flow rate of 1.2 mL / h, and a receiving distance of 18 cm to prepare a polylactic acid electrospinning membrane; S13. Take a portion of the polylactic acid electrospun membrane, place the electrospun fiber membrane in a zigzag structure mold for heat setting treatment, the heat setting temperature is 110°C, the time is 50s, and a polylactic acid fiber membrane with a zigzag structure is obtained. The zigzag structure is formed by connecting a number of circular arc zigzag units in sequence, the diameter of each circular arc zigzag unit is 1mm, and the interval between adjacent zigzag paper pieces is 0.1mm. Comparative Example 1 A method for preparing a high-efficiency filtering composite cigarette holder, the method comprising the following steps: S1. Using low-melting-point polylactic acid with a melting point of 120°C as the skin material and high-melting-point polylactic acid with a melting point of 160°C as the core material, drying and melting the skin material and the core material to obtain skin spinning solution and core spinning solution respectively, wherein the mass ratio of low-melting-point polylactic acid to high-melting-point polylactic acid is 6:4, and spinning is performed to obtain skin-core structure polylactic acid fibers; S2. The polylactic acid electrospinning membrane, the core-skin structure polylactic acid fiber and the zigzag polylactic acid electrospinning membrane are stacked in three layers at a certain angle, the mass ratio of the polylactic acid electrospinning membrane, the core-skin structure polylactic acid fiber and the zigzag polylactic acid electrospinning membrane is 4.5:7:7, and the axis of the arc-shaped through groove in the arc-shaped zigzag unit of the zigzag polylactic acid electrospinning membrane is 90° to the core-skin structure polylactic acid fiber to obtain a laminated composite structure; S3. With the direction parallel to the core-sheath structure of the polylactic acid fiber as the axis, the laminated composite structure is wound to obtain a cigarette holder tow, and then thermally bonded to obtain a high-efficiency filter composite cigarette holder; The preparation method of the polylactic acid electrospinning membrane comprises the following steps: S11. adding polylactic acid to dichloromethane and stirring to dissolve to obtain a 6 wt % electrospinning solution; S12. The electrospinning solution was electrospun to obtain an electrospinning fiber membrane at a voltage of 18 kV, a flow rate of 1.2 mL / h, and a receiving distance of 18 cm to prepare a polylactic acid electrospinning membrane; S13. Take a portion of the polylactic acid electrospun membrane, place the electrospun fiber membrane in a zigzag structure mold for heat setting treatment, the heat setting temperature is 110°C, the time is 50s, and a polylactic acid fiber membrane with a zigzag structure is obtained. The zigzag structure is formed by connecting a number of circular arc zigzag units in sequence, the diameter of each circular arc zigzag unit is 1mm, and the interval between adjacent zigzag paper pieces is 0.1mm. Comparative Example 2 A method for preparing a high-efficiency filtering composite cigarette holder, the method comprising the following steps: S1. Using low-melting-point polylactic acid with a melting point of 120°C as the skin material and high-melting-point polylactic acid with a melting point of 160°C as the core material, drying and melting the skin material and the core material to obtain skin spinning solution and core spinning solution respectively, wherein the mass ratio of low-melting-point polylactic acid to high-melting-point polylactic acid is 6:4, and spinning is performed to obtain skin-core structure polylactic acid fibers; S2. The polylactic acid electrospinning membrane, the core-skin structure polylactic acid fiber and the zigzag polylactic acid electrospinning membrane are stacked in three layers at a certain angle, the mass ratio of the polylactic acid electrospinning membrane, the core-skin structure polylactic acid fiber and the zigzag polylactic acid electrospinning membrane is 4.5:7:7, and the axis of the arc-shaped through groove in the arc-shaped zigzag unit of the zigzag polylactic acid electrospinning membrane is parallel to the core-skin structure polylactic acid fiber to obtain a laminated composite structure; S3. With the direction parallel to the core-sheath structure of the polylactic acid fiber as the axis, the laminated composite structure is wound to obtain a cigarette holder tow, and then thermally bonded to obtain a high-efficiency filter composite cigarette holder; The preparation method of the polylactic acid electrospinning membrane comprises the following steps: S11. adding polylactic acid to dichloromethane and stirring to dissolve to obtain a 6 wt % electrospinning solution; S12. The electrospinning solution was electrospun to obtain an electrospinning fiber membrane at a voltage of 18 kV, a flow rate of 1.2 mL / h, and a receiving distance of 18 cm to prepare a polylactic acid electrospinning membrane; S13. Take a portion of the polylactic acid electrospun membrane, place the electrospun fiber membrane in a zigzag structure mold for heat setting treatment, the heat setting temperature is 110°C, the time is 50s, and a polylactic acid fiber membrane with a zigzag structure is obtained. The zigzag structure is formed by connecting a number of circular arc zigzag units in sequence, the diameter of each circular arc zigzag unit is 1mm, and the interval between adjacent zigzag paper pieces is 0.1mm. Comparative Example 3 A method for preparing a high-efficiency filtering composite cigarette holder, the method comprising the following steps: S1. Using low-melting-point polylactic acid with a melting point of 120°C as the skin material and high-melting-point polylactic acid with a melting point of 160°C as the core material, drying and melting the skin material and the core material to obtain skin spinning solution and core spinning solution respectively, wherein the mass ratio of low-melting-point polylactic acid to high-melting-point polylactic acid is 6:4, and spinning is performed to obtain skin-core structure polylactic acid fibers; S2. The polylactic acid electrospun membrane, the skin-core structure polylactic acid fiber and the polylactic acid electrospun membrane are three-layered, the mass ratio of the polylactic acid electrospun membrane, the skin-core structure polylactic acid fiber and the polylactic acid electrospun membrane is 4.5:7:4.5 to obtain a laminated composite structure; S3. With the direction parallel to the core-sheath structure of the polylactic acid fiber as the axis, the laminated composite structure is wound to obtain a cigarette holder tow, and then thermally bonded to obtain a high-efficiency filter composite cigarette holder; The preparation method of the polylactic acid electrospinning membrane comprises the following steps: S11. adding polylactic acid to dichloromethane and stirring to dissolve to obtain a 6 wt % electrospinning solution; S12. The electrospinning solution was electrospun to obtain an electrospinning fiber membrane. The voltage was 18 kV, the flow rate was 1.2 mL / h, and the receiving distance was 18 cm to prepare a polylactic acid electrospinning membrane. Comparative Example 4 A method for preparing a high-efficiency filtering composite cigarette holder, the method comprising the following steps: S1. Using low-melting-point polylactic acid with a melting point of 120°C as the skin material and high-melting-point polylactic acid with a melting point of 160°C as the core material, drying and melting the skin material and the core material to obtain skin spinning solution and core spinning solution respectively, wherein the mass ratio of low-melting-point polylactic acid to high-melting-point polylactic acid is 6:4, and spinning is performed to obtain skin-core structure polylactic acid fibers; S2. The polylactic acid electrospinning membrane, the core-skin structure polylactic acid fiber and the zigzag polylactic acid electrospinning membrane are stacked in three layers at a certain angle, the mass ratio of the polylactic acid electrospinning membrane, the core-skin structure polylactic acid fiber and the zigzag polylactic acid electrospinning membrane is 4.5:7:7, and the axis of the arc-shaped through groove in the arc-shaped zigzag unit of the zigzag polylactic acid electrospinning membrane is 45° to the core-skin structure polylactic acid fiber to obtain a laminated composite structure; S3. With the direction parallel to the core-sheath structure of the polylactic acid fiber as the axis, the laminated composite structure is wound to obtain a cigarette holder tow, and then thermally bonded to obtain a high-efficiency filter composite cigarette holder; The preparation method of the polylactic acid electrospinning membrane comprises the following steps: S11. adding polylactic acid to dichloromethane and stirring to dissolve to obtain a 6 wt % electrospinning solution; S12. The electrospinning solution was electrospun to obtain an electrospinning fiber membrane at a voltage of 18 kV, a flow rate of 1.2 mL / h, and a receiving distance of 18 cm to prepare a polylactic acid electrospinning membrane; S13. Take a portion of the polylactic acid electrospun membrane, place the electrospun fiber membrane in a zigzag structure mold for heat setting treatment, the heat setting temperature is 110°C, the time is 50s, and a polylactic acid fiber membrane with a zigzag structure is obtained. The zigzag structure is formed by connecting a number of circular arc zigzag units in sequence, the diameter of each circular arc zigzag unit is 1.5mm, and the interval between adjacent zigzag paper pieces is 0.1mm. Absorption resistance(kPa) Filter rod ventilation rate (%) Example 1 1.32 39.12 Example 2 1.51 33.12 Example 3 1.40 35.65 Example 4 1.34 39.56 Example 5 1.38 37.24 Example 6 1.31 38.23 Example 7 1.55 31.23 Comparative Example 1 1.85 26.18 Comparative Example 2 1.15 51.23 Comparative Example 3 1.26 36.56 Comparative Example 4 1.24 40.23 Note: GB / T 22838 test is adopted, the cigarette specification is 84mm in length (54mm tobacco material section + 30mm filter rod section, the cigarette circumference is 17.0mm, and the weight of the tobacco material section in the cigarette is 0.40±0.1g. Note: The retention rate of sample tar and total particulate matter is determined according to the method of GB / T19609-2004. Obviously, the above embodiments are merely examples for the purpose of clear explanation, and are not intended to limit the implementation methods. For those skilled in the art, other different forms of changes or modifications can be made based on the above description. It is not necessary and impossible to list all the implementation methods here. The obvious changes or modifications derived therefrom are still within the scope of protection of the invention.
Claims
1. A high-efficiency filtering composite cigarette holder, characterized in that: The high-efficiency filtering composite cigarette holder is formed by three-layer lamination and composite winding of a polylactic acid electrostatic spinning membrane, a zigzag polylactic acid electrostatic spinning membrane and a sheath-core structure polylactic acid fiber.
2. The high efficiency filter composite cigarette holder according to claim 1, characterized in that: The preparation method of the polylactic acid electrospinning membrane comprises the following steps: S11. Adding polylactic acid to dichloromethane and stirring to dissolve to obtain 5.5-7wt% electrospinning solution; S12. The electrospinning solution is electrospun to obtain an electrospinning fiber membrane, with a voltage of 16-20 kV, a flow rate of 0.8-1.5 mL / h, and a receiving distance of 15-22 cm.
3. The high efficiency filter composite cigarette holder according to claim 2, characterized in that: The preparation method of the polylactic acid electrospinning membrane comprises the following steps: S21. Adding polylactic acid to dichloromethane and stirring to dissolve to obtain 5.5-7wt% electrospinning solution; S22 electrospins the electrospinning solution to obtain an electrospinning fiber membrane, with a voltage of 16-20 kV, a flow rate of 0.8-1.5 mL / h, and a receiving distance of 15-22 cm. S23. Placing the electrospun fiber membrane in a zigzag-shaped mold for heat setting treatment to obtain a zigzag-shaped polylactic acid fiber membrane.
4. The high efficiency filter composite cigarette holder according to claim 3, characterized in that: The method for preparing the polylactic acid electrospinning membrane further comprises the following steps: adding nanoporous carbon balls to the electrospinning solution prepared in S21, wherein the content of the nanoporous carbon balls in the electrospinning solution is 1.5-3wt%.
5. The high efficiency filter composite cigarette holder according to claim 3, characterized in that: The temperature of the heat setting treatment in step S23 is 100-120° C. and the time is 40-60 seconds.
6. The high efficiency filter composite cigarette holder according to claim 3, characterized in that: The sawtooth structure is formed by connecting a plurality of circular arc sawtooth units in sequence, the diameter of each circular arc sawtooth unit is 0.5-1.2 mm, and the interval between adjacent sawtooth paper pieces is 0.1-0.2 mm.
7. The method for preparing a high-efficiency filtering composite cigarette holder according to claim 1, characterized in that: The preparation method of the high-efficiency filtering composite cigarette holder comprises the following steps: S1. Using low melting point polylactic acid as the skin material and high melting point polylactic acid as the core material, the skin material and the core material are dried and melted to obtain a skin spinning solution and a core spinning solution, and spinning is performed to obtain a skin-core structure polylactic acid fiber; S2. The polylactic acid electrospun membrane, the skin-core structure polylactic acid fiber and the zigzag polylactic acid electrospun membrane are stacked in three layers at a certain angle to obtain a laminated composite structure; S3. With the direction parallel to the core-skin structure polylactic acid fiber as the axis, the laminated composite structure is wound to obtain a cigarette holder tow, and then a high-efficiency filtering composite cigarette holder is obtained through thermal bonding.
8. The method for preparing a high-efficiency filtering composite cigarette holder according to claim 1, characterized in that: In the step S1, the mass ratio of the low melting point polylactic acid to the high melting point polylactic acid is 50-70:30-50, the melting point of the low melting point polylactic acid is 115-130°C, and the melting point of the high melting point polylactic acid is 150-170°C.
9. The method for preparing a high-efficiency filtering composite cigarette holder according to claim 1, characterized in that: In the step S2, the axis of the arc-shaped through groove in the arc-shaped sawtooth unit of the sawtooth polylactic acid electrospinning membrane is 30-60 degrees with the core-skin structure polylactic acid fiber.
10. The method for preparing a high-efficiency filtering composite cigarette holder according to claim 1, characterized in that: In the step S2, the mass ratio of the polylactic acid electrospinning membrane, the core-skin structure polylactic acid fiber and the zigzag polylactic acid electrospinning membrane is 4-5:5.5-8:6.5-8.5.
Citation Information
Patent Citations
Sheath-core polylactic acid tobacco tow and filter stick and preparation method thereof
CN103074716A
Polylactic acid tow molded filter tip flake and molding equipment and technology
CN110537728A
System mouth stick is rolled up to nanofiber composite bed
CN207574506U
Improvements in and relating to filters for tobacco smoke
GB868058A
Method of forming cigarette filter material
US4283186A