Glass ceramic efficient hot bending equipment and production process
By directly heating glass raw materials with mobile workbenches and multiple heating plates in microcrystalline glass thermal bending equipment, the problems of high production costs and poor product quality in the existing technology are solved, and efficient and accurate temperature control is achieved, improving the quality of the product. Production efficiency and product quality.
Patent Information
- Application Number
- CN202411165667.7
- Authority / Receiving Office
- CN · China
- Patent Type
- Applications(China)
- Current Assignee / Owner
- Filing Date
- 2024-08-23
- Publication Date
- 2024-11-15
AI Technical Summary
The existing microcrystalline glass thermal bending equipment has problems such as high production costs, poor product quality, inaccurate temperature control and uneven temperature, resulting in low production efficiency and poor product quality.
It adopts a microcrystalline glass high-efficiency thermal bending equipment and production process, including a mobile workbench and multiple heating plates. By directly heating glass raw materials and precisely controlling the temperature, it reduces mold quantity and energy consumption, and improves production efficiency and product quality.
It improves the production efficiency and product quality of microcrystalline glass, reduces the number of molds and equipment energy consumption, and achieves cost reduction and efficiency improvement.
Smart Images

Figure CN118954918A_ABST
Abstract
Description
Technical Field
[0001] The present invention relates to the field of glass-ceramic hot bending, and in particular to a glass-ceramic high-efficiency hot bending device and a production process. Background Art
[0002] Optical glass is being used more and more widely, but existing materials have limited strength and are easily broken under external forces. Therefore, material manufacturers have developed microcrystalline glass with higher strength. However, with the increase in material strength, the molecular properties of the material have also changed. In the temperature range of 750℃~1200℃, the glass will continue to grow crystals, causing the originally transparent glass to gradually turn blue, and eventually turn white to an opaque state. In order to complete the hot bending production temperature, it must be increased to the softening temperature of the microcrystalline glass, which is about 800℃. At this time, the softening temperature and the crystallization temperature range of the glass coincide. At the same time, the longer the glass stays in the high temperature zone, the higher the temperature, and the more intense the crystal growth of the microcrystalline glass. Therefore, the traditional hot bending process cannot produce qualified microcrystalline hot bending products.
[0003] In the prior art, it is necessary to put the raw glass-ceramic material before heat bending into a mold, put the mold into a high-temperature device, move the mold slowly inside the device, and gradually heat it up to a softening temperature of about 800°C, then gradually apply pressure, and after the mold is fully closed, the mold continues to move, then slowly cools down and flows out of the furnace from the outlet. This equipment usually adopts a multi-station type, with about 20 stations, which means that more than 20 sets of molds need to be put into use at the same time. Assuming the production cycle is two minutes, the number of high-temperature zones is ten stations, which means that each piece of glass needs to stay in the high-temperature zone for at least 20 minutes. Too long a stay time will directly cause the glass crystal growth to intensify and result in poor production quality. The prior art has the following disadvantages: 1. High production cost. In order to ensure production efficiency, a multi-station solution is generally adopted, but a multi-process solution means higher energy consumption of the equipment and more mold investment.
[0004] 2. Poor production quality and no production. Limited by the production principle, it is impossible to directly heat the material. Instead, the glass is heated indirectly by heating the mold and transferring the heat to the glass material through the mold. Since the mold is made of graphite and has a certain thickness, it takes longer to heat up. It takes about five times longer for the mold to heat up to the set softening temperature than to directly raise the glass to the set softening temperature. Therefore, it means that the glass will stay in the high temperature zone for a longer time. Staying in the high temperature zone for a long time will directly cause quality abnormalities such as blue glass crystal growth.
[0005] 3. Inaccurate temperature control. Microcrystalline materials are very sensitive to temperature. When the temperature exceeds 750°C, the glass will begin to grow crystals. The higher the temperature, the faster the growth rate. Since the traditional method is to heat the graphite mold with a heater and transfer the heat to the glass through the graphite mold, and since the heat will be lost during the transfer process, there is no way to accurately control the actual temperature of the microcrystalline glass. For example, we need 800°C, but the temperature transferred to the microcrystalline glass through the mold may only be 780°C. In this case, we need to compensate for the temperature and set the temperature to 820°C to ensure that the temperature of the glass can reach 800°C, but this will lead to an increase in ambient temperature and inaccurate glass temperature, which will directly affect production quality.
[0006] 4. Uneven temperature. Affected by the bending structure of the product, the surface structure of the mold is also uneven and the thickness is uneven, which leads to uneven temperature transmitted from the heater to the glass through the mold. When it is at the critical temperature of hot bending, it will cause the glass to break due to insufficient local temperature or turn blue due to excessive local temperature, which will directly affect the production quality. Summary of the invention
[0007] The present invention aims to solve at least one of the technical problems existing in the prior art. To this end, the present invention proposes a high-efficiency hot bending device for microcrystalline glass, which can greatly improve the production efficiency and production yield of microcrystalline glass, reduce the number of molds and equipment energy consumption, thereby achieving the effect of reducing costs and increasing efficiency.
[0008] The present invention also provides a high-efficiency hot-bending production process for glass-ceramics.
[0009] The first aspect of the present invention provides a glass-ceramic high-efficiency hot bending device and production process, comprising: The first station is the loading and unloading station; The second station is a preheating station and a slow cooling station, comprising a first lifting mechanism and a first upper heating plate located at the top, wherein the first lifting mechanism is used to drive the first upper heating plate to rise and fall; The third station is a molding station, comprising a second lifting mechanism located above, a second upper heating plate and an upper mold, wherein the upper mold is fixed to the bottom surface of the second upper heating plate, and the second lifting mechanism is used to drive the second upper heating plate and the upper mold to rise and fall; The movable workbench can be moved to the first station, the second station and the third station. The movable workbench is provided with a lower water cooling plate, a lower heating plate and a lower mold from bottom to top, and the lower mold is fixed on the top surface of the lower heating plate.
[0010] According to some embodiments of the present invention, the lower cold water plate is connected to a lifting component, and the lifting component is used to drive the lower cold water plate to rise or fall, and the lower cold water plate can contact the lower heating plate.
[0011] According to some embodiments of the present invention, a heat insulation plate is provided between the first lifting mechanism and the first upper heating plate, and between the second lifting mechanism and the second upper heating plate.
[0012] According to some embodiments of the present invention, an upper water cooling plate is further provided on the heat insulation plate, and the upper water cooling plate is connected to the first lifting mechanism or the second lifting mechanism.
[0013] According to some embodiments of the present invention, the first lifting mechanism and the second lifting mechanism are hydraulic lifting mechanisms.
[0014] According to some embodiments of the present invention, the second lifting mechanism includes a power system, a servo motor and a pressure sensor, and the power system is controlled by the servo motor and the pressure sensor.
[0015] In a second aspect of the present invention, a glass-ceramic efficient hot bending production process is also provided, using the above-mentioned glass-ceramic efficient hot bending equipment, comprising the following steps: S100, loading process: the movable workbench is located at the first station, and the glass-ceramic raw material is placed in the lower mold on the movable workbench, and the temperature of the lower mold is 300-400° C.; S200, preheating process: the movable workbench moves to the second station, the temperature of the first upper heating plate is 800-820°C, the first upper heating plate moves down and contacts the lower mold to directly bake the glass-ceramics raw material, the lower mold is heated to 650-700°C to heat the glass-ceramics raw material, so that the glass-ceramics raw material is heated to the softening temperature of 800°C; S300, molding process: the movable workbench moves to the third station, the upper mold temperature is 750-800°C, the upper mold descends rapidly to apply pressure to the glass-ceramic raw material to form and hold the pressure, and after holding the pressure for a first period of time, the upper mold rises to separate from the lower mold; S400, slow cooling process: the movable workbench moves to the second station, the first upper heating plate descends to be close to the lower mold to maintain continuous baking and heat preservation of the formed microcrystalline glass, after baking and heat preservation for a second time, the first upper heating plate rises, and at the same time, the lower water cooling plate rises and contacts the lower heating plate to cool down, and the lower mold and the formed microcrystalline glass are gradually cooled to 300-400°C; S500, unloading process: the movable workbench moves to the first station for unloading.
[0016] According to some embodiments of the present invention, in the preheating step S200, the time duration for heating the glass-ceramics raw material is 55-65 seconds.
[0017] According to some embodiments of the present invention, in the S300 molding process, after holding the pressure for a first period of time, the first upper heating plate slowly rises.
[0018] According to some embodiments of the present invention, in the S400 slow cooling process, after baking and keeping warm for a second time period, the second upper heating plate slowly rises.
[0019] A glass-ceramic efficient hot bending device and production process according to an embodiment of the present invention has at least the following beneficial effects: 1. Improve production efficiency. First, in the preheating process, the temperature of the first upper heating plate is 800-820℃ to directly bake the glass-ceramic raw material, which is faster than the method of indirectly heating the lens through the glass-ceramic raw material. Secondly, in the slow cooling process, the lower water cooling plate is used to cool the lower heating plate and the lower mold to reduce the cooling time. Finally, in the unloading process, the temperature at which the glass-ceramic completes stress release is 400 degrees, and the glass-ceramic can be taken out at 300-400℃. There is no need to wait until the lower mold and the glass-ceramic product cool to room temperature, so the cooling time is shorter.
[0020] 2. Improve production yield. In the preheating process, the first upper heating plate directly bakes the raw material of the microcrystalline glass. Compared with the traditional mold heating which requires temperature compensation, the direct heating and temperature control by the heating plate are more accurate. Compared with the uneven thickness of the mold itself which causes uneven glass temperature, the direct heating by the heating plate is more uniform. Therefore, it can prevent the microcrystalline glass from growing due to excessive temperature and breakage due to uneven temperature, which is beneficial to improving the product quality of the microcrystalline glass.
[0021] 3. It can reduce the number of molds. Due to the improvement of production efficiency, two sets of molds can achieve the output of the original 20 sets of molds. At the same time, it also reduces the investment in mold supporting heating equipment.
[0022] 4. It can reduce the energy consumption of equipment. First, in the preheating process, the first upper heating plate directly bakes the glass-ceramic raw material, which heats up faster and consumes less energy than the indirect heating method through the mold. Secondly, in the molding process, the temperature of the upper mold and the lower mold do not need to reach 800°C. It is only necessary to ensure that the glass-ceramic raw material is heated to 800°C in the preheating process, so less heat is required to be provided to the mold. Finally, it is not cooled to room temperature in the slow cooling process, so less heat is lost in the cooling process, and less heating energy is required to heat the mold in subsequent production. Overall, the energy waste caused by frequent heating and cooling of the mold is reduced, because the core of hot bending molding is to heat up the glass, not the mold.
[0023] In summary, the high-efficiency hot bending equipment and production process of microcrystalline glass can greatly improve the production efficiency and production yield of microcrystalline glass, reduce the number of molds and equipment energy consumption, thereby achieving the effect of reducing costs and increasing efficiency.
[0024] Additional aspects and advantages of the present invention will be given in part in the following description and in part will be obvious from the following description, or will be learned through practice of the present invention. BRIEF DESCRIPTION OF THE DRAWINGS
[0025] In order to more clearly illustrate the embodiments of the present invention or the technical solutions of the prior art, the drawings required for use in the embodiments or the description of the prior art will be briefly introduced below. Obviously, the drawings described below are only some embodiments of the present invention. For ordinary technicians in this field, other drawings can be obtained based on these drawings without paying creative work.
[0026] Figure 1 is a schematic diagram of an embodiment of the first aspect of the present invention; Figure 2 This is a flow chart of an embodiment of the second aspect of the present invention.
[0027] Figure numerals: first station 1, second station 2, first lifting mechanism 21, first upper heating plate 22, third station 3, second lifting mechanism 31, second upper heating plate 32, upper mold 33, movable workbench 4, lower water-cooling plate 41, lower heating plate 42, lower mold 43, insulation plate 5, upper water-cooling plate 6, loading process S100, preheating process S200, molding process S300, slow cooling process S400, unloading process S500. DETAILED DESCRIPTION
[0028] Embodiments of the present invention are described in detail below, examples of which are shown in the accompanying drawings, wherein the same or similar reference numerals throughout represent the same or similar elements or elements having the same or similar functions. The embodiments described below with reference to the accompanying drawings are exemplary and are only used to explain the present invention, and cannot be understood as limiting the present invention.
[0029] In the description of the present invention, it is necessary to understand that descriptions involving orientation, such as up, down, front, back, left, right, etc., indicating orientations or positional relationships, are based on the orientations or positional relationships shown in the drawings, and are only for the convenience of describing the present invention and simplifying the description, and do not indicate or imply that the device or element referred to must have a specific orientation, be constructed and operated in a specific orientation, and therefore cannot be understood as a limitation on the present invention.
[0030] In the description of the present invention, "several" means one or more, "more" means more than two, "greater than", "less than", "exceed", etc. are understood to exclude the number itself, and "above", "below", "within", etc. are understood to include the number itself. If there is a description of first and second, this is only for the purpose of distinguishing the technical features, and cannot be understood as indicating or implying relative importance or implicitly indicating the number of the indicated technical features or implicitly indicating the order of the indicated technical features.
[0031] In the description of the present invention, it should be noted that, unless otherwise clearly specified and limited, the terms "installation, connection and connection" should be understood in a broad sense, for example, it can be a fixed connection, a detachable connection, or an integral connection; it can be a mechanical connection or an electrical connection; it can be a direct connection, or it can be an indirect connection through an intermediate medium, or it can be the internal communication of two components. For ordinary technicians in this field, the specific meanings of the above terms in the present invention can be understood according to specific circumstances.
[0032] Reference below Figure 1-Figure 2 A glass-ceramic efficient hot bending device and production process is described in detail with a specific embodiment. It is worth noting that the following description is only an exemplary description and not a specific limitation of the invention.
[0033] like Figure 1 As shown, a high-efficiency hot bending device for microcrystalline glass according to the first aspect of the present invention includes a first workstation 1, a second workstation 2, a third workstation 3 and a movable workbench 4.
[0034] Among them, the first station 1 is a loading and unloading station; the second station 2 is a preheating station and a slow cooling station, including a first lifting mechanism 21 and a first upper heating plate 22 located at the top, and the first lifting mechanism 21 is used to drive the first upper heating plate 22 to rise and fall; the third station 3 is a molding station, including a second lifting mechanism 31, a second upper heating plate 32 and an upper mold 33 located at the top, and the upper mold 33 is fixed on the bottom surface of the second upper heating plate 32, and the second lifting mechanism 31 is used to drive the second upper heating plate 32 and the upper mold 33 to rise and fall; the mobile workbench 4 can move to the first station 1, the second station 2 and the third station 3, and the mobile workbench 4 is sequentially provided with a lower water-cooling plate 41, a lower heating plate 42 and a lower mold 43 from bottom to top, and the lower mold 43 is fixed on the top surface of the lower heating plate 42. Specifically, the upper mold 33 is a convex mold, and the lower mold 43 is a concave mold, and the lower mold 43 is provided with an installation cavity for placing microcrystalline glass raw materials.
[0035] In some specific embodiments of the present invention, the lower water cooling plate 41 is connected to a lifting component (the lifting component is not shown in the figure), and the lifting component is used to drive the lower water cooling plate to rise or fall, and the lower water cooling plate 41 can contact the lower heating plate 42. In this way, the lower water cooling plate 41 can rise and contact the lower heating plate 42 to cool down when the lower heating plate 42 needs to be cooled, and fall and separate when the lower heating plate 42 does not need to be cooled, thereby reducing heat loss and playing a role in energy saving.
[0036] It should be noted that a heat insulation plate 5 is provided between the first lifting mechanism 21 and the first upper heating plate 22, and between the second lifting mechanism 31 and the second upper heating plate 32. The heat insulation plate 5 can prevent heat from being transferred to the first lifting mechanism 21 and the second lifting mechanism 31, while reducing the heat loss of the first upper heating plate 22 and the second upper heating plate 32, thereby saving energy. In addition, an upper water cooling plate 6 is provided on the heat insulation plate 5, and the upper cold water plate 6 is connected to the first lifting mechanism 21 or the second lifting mechanism 31. The upper water cooling plate 6 is provided on the heat insulation plate 5 to cool down the heat insulation plate 5 when the temperature is overheated, thereby preventing high temperature deformation.
[0037] It is understandable that the first lifting mechanism 21 and the second lifting mechanism 31 are hydraulic lifting mechanisms. The hydraulic lifting mechanism is stable in operation and can accurately drive the upper heating plate and the upper mold 33 to move to a suitable height for operation. Specifically, the second lifting mechanism 31 includes a power system, a servo motor and a pressure sensor (the power system, the servo motor and the pressure sensor are not shown separately in the figure), and the power system is controlled by the servo motor and the pressure sensor. The servo motor can accurately control the lifting height of the second upper heating plate 32 and the upper mold 33 driven by the second lifting mechanism, and the pressure sensor can monitor the clamping pressure of the upper mold 33 in real time, so as to ensure that the pressure is maintained at a certain pressure.
[0038] like Figure 2 As shown, a glass-ceramic efficient hot bending production process according to the second aspect of the present invention uses the above-mentioned glass-ceramic efficient hot bending equipment, and specifically comprises the following steps: Loading process S100: At the beginning, the movable workbench 4 is located at the first station 1, and the operator first places the microcrystalline glass raw material in the lower mold 43 on the movable workbench 4. At this time, the temperature of the lower mold 43 is 300-400°C.
[0039] Preheating process S200: The mobile workbench 4 moves to the second workstation 2, and the first lifting mechanism 21 drives the first upper heating plate 22 to descend and contact the surface of the lower mold 43 of the mobile workbench 4. The temperature of the first upper heating plate 22 is 800-820°C to directly bake the microcrystalline glass raw material. At the same time, the lower mold 43 is heated to 650-700°C to heat the microcrystalline glass raw material. At this time, under the joint action of the first upper heating plate 22 and the lower heating plate 42, the microcrystalline glass raw material is quickly heated and heated to the softening temperature of 800°C at about 60°C.
[0040] Forming process S300: The mobile workbench 4 quickly moves to the third station 3 with the lower mold 43 and the microcrystalline glass raw material that has been heated to the softening temperature. The second upper heating plate 32 heats the upper mold 33 to 700-750℃ in advance. The upper mold 33 that has completed the heating preparation above the third station 3 quickly descends to apply pressure to the microcrystalline glass raw material for molding. The power system of the second lifting mechanism 31 is controlled by a servo motor and is equipped with a pressure sensor. When the pressure reaches the set pressure value, the current pressure is maintained for pressure holding. Since the temperature of the upper mold 33 is lower than the softening temperature of the microcrystalline glass, when the upper mold 33 presses down to cause the microcrystalline glass to be molded and completely closed, the molded microcrystalline glass contacts the lower film and quickly cools down to shape, completing the molding. After the first period of pressure holding, the upper mold 33 slowly rises according to the set process requirements, gradually separates from the lower mold 43 and the molded microcrystalline glass, so as to prevent the microcrystalline glass from breaking or causing stress concentration due to excessive cooling.
[0041] Slow cooling process S400: After the upper mold 33 and the lower mold 43 are completely separated, the movable workbench 4 quickly drives the lower mold 43 to move to the second workstation 2, and the first upper heating plate 22 quickly descends to maintain continuous baking and insulation of the formed microcrystalline glass. After baking and insulation for the second period of time, it slowly moves away from the lower mold 43 according to the process requirements. At the same time, the lower water-cooling plate 41 rises and contacts the lower heating plate 42 to cool the lower heating plate 42. Under the action of the slow departure of the first upper heating plate 22 and the cooling of the lower water-cooling plate 41, the lower mold 43 and the formed microcrystalline glass slowly cool down to the annealing temperature of 300-400℃.
[0042] Unloading process S500: After the temperature is lowered, the movable workbench 4 moves to the first station 1 for unloading, and then reloads to enter the next round of production cycle.
[0043] The high-efficiency hot bending equipment and production process of microcrystalline glass can greatly improve the production efficiency and production yield of microcrystalline glass, reduce the number of molds and equipment energy consumption, thereby achieving the effect of reducing costs and increasing efficiency. The specific performance is as follows: 1. Improve production efficiency. First, in the preheating process, the temperature of the first upper heating plate 22 is 800-820°C to directly bake the microcrystalline glass raw material, which is faster than the method of indirectly heating the lens through the microcrystalline glass raw material. Secondly, in the slow cooling process, the lower water cooling plate 41 is used to cool the lower heating plate 42 and the lower mold 43 to reduce the cooling time. Finally, in the unloading process, the temperature at which the microcrystalline glass completes stress release is 400 degrees, and the glass microcrystalline can be taken out at 300-400°C. There is no need to wait until the lower mold 43 and the microcrystalline glass product cool to room temperature, so the cooling time is shorter.
[0044] 2. Improve production yield. In the preheating process, the first upper heating plate 22 directly bakes the glass-ceramic raw material. Compared with the traditional mold heating which requires temperature compensation, the direct heating and temperature control by the heating plate are more accurate. Compared with the uneven thickness of the mold itself which causes uneven glass temperature, the direct heating by the heating plate is more uniform. Therefore, it can prevent the glass-ceramic from growing due to excessive temperature and breakage due to uneven temperature, which is beneficial to improving the product quality of the glass-ceramic.
[0045] 3. It can reduce the number of molds. Due to the improvement of production efficiency, two sets of molds can achieve the output of the original 20 sets of molds. At the same time, it also reduces the investment in mold supporting heating equipment.
[0046] 4. It can reduce the energy consumption of equipment. First, in the preheating process, the first upper heating plate 22 directly bakes the microcrystalline glass raw material, which heats up faster and consumes less energy than the indirect heating method through the mold. Secondly, in the molding process, the temperature of the upper mold 33 and the lower mold 43 do not need to reach 800°C. It is only necessary to ensure that the microcrystalline glass raw material is heated to 800°C in the preheating process, so less heat is required to be provided to the mold. Finally, it is not cooled to room temperature in the slow cooling process, so less heat is dissipated during the cooling process, and less heating energy is required to heat the mold in subsequent production. Overall, the energy waste caused by frequent heating and cooling of the mold is reduced, because the core of hot bending molding is to heat up the glass, not the mold.
[0047] In the description of this specification, the description with reference to the terms "one embodiment, some embodiments, illustrative embodiments, examples, specific examples or some examples" etc. means that the specific features, structures, materials or characteristics described in conjunction with the embodiment or example are included in at least one embodiment or example of the present invention. In this specification, the schematic representation of the above terms does not necessarily refer to the same embodiment or example. Moreover, the specific features, structures, materials or characteristics described may be combined in any one or more embodiments or examples in a suitable manner.
[0048] The embodiments of the present invention are described in detail above with reference to the accompanying drawings, but the present invention is not limited to the above embodiments, and various changes can be made within the knowledge scope of ordinary technicians in the relevant technical field without departing from the purpose of the present invention.
Claims
1. A highly efficient glass-ceramic hot bending device, characterized in that: include: The first station is the loading and unloading station; The second station is a preheating station and a slow cooling station, comprising a first lifting mechanism and a first upper heating plate located at the top, wherein the first lifting mechanism is used to drive the first upper heating plate to rise and fall; The third station is a molding station, comprising a second lifting mechanism located above, a second upper heating plate and an upper mold, wherein the upper mold is fixed to the bottom surface of the second upper heating plate, and the second lifting mechanism is used to drive the second upper heating plate and the upper mold to rise and fall; The movable workbench can be moved to the first station, the second station and the third station. The movable workbench is provided with a lower water cooling plate, a lower heating plate and a lower mold from bottom to top, and the lower mold is fixed on the top surface of the lower heating plate.
2. The glass-ceramic high-efficiency hot bending equipment according to claim 1, characterized in that: The lower cold water plate is connected with a lifting component, and the lifting component is used to drive the lower cold water plate to rise or fall, and the lower cold water plate can contact the lower heating plate.
3. The glass-ceramic high-efficiency hot bending equipment according to claim 1, characterized in that: A heat insulation plate is provided between the first lifting mechanism and the first upper heating plate, and between the second lifting mechanism and the second upper heating plate.
4. The glass-ceramic high-efficiency hot bending device according to claim 3, characterized in that: The heat insulation plate is also provided with an upper water cooling plate, and the upper cooling water plate is connected to the first lifting mechanism or the second lifting mechanism.
5. The glass-ceramic high-efficiency hot bending equipment according to claim 1, characterized in that: The first lifting mechanism and the second lifting mechanism are hydraulic lifting mechanisms.
6. The glass-ceramic efficient hot bending equipment according to claim 1, characterized in that: The second lifting mechanism includes a power system, a servo motor and a pressure sensor, and the power system is controlled by the servo motor and the pressure sensor.
7. A high-efficiency hot bending production process for glass-ceramics, characterized in that: The use of a glass-ceramic efficient hot bending device according to any one of claims 1 to 6 comprises the following steps: S100, loading process: the movable workbench is located at the first station, and the glass-ceramic raw material is placed in the lower mold on the movable workbench, and the temperature of the lower mold is 300-400° C.; S200, preheating process: the movable workbench moves to the second station, the temperature of the first upper heating plate is 800-820°C, the first upper heating plate moves down and contacts the lower mold to directly bake the glass-ceramics raw material, and at the same time the lower mold is heated to 650-700°C to heat the glass-ceramics raw material, so that the glass-ceramics raw material is heated to the softening temperature of 800°C; S300, molding process: the movable workbench moves to the third station, the upper mold temperature is 750-800°C, the upper mold descends rapidly to apply pressure to the glass-ceramic raw material to form and hold the pressure, and after holding the pressure for a first period of time, the upper mold rises to separate from the lower mold; S400, slow cooling process: the movable workbench moves to the second station, the first upper heating plate descends to be close to the lower mold to maintain continuous baking and heat preservation of the formed microcrystalline glass, after baking and heat preservation for a second time, the first upper heating plate rises, and at the same time, the lower water cooling plate rises and contacts the lower heating plate to cool down, and the lower mold and the formed microcrystalline glass are gradually cooled to 300-400°C; S500, unloading process: the movable workbench moves to the first station for unloading.
8. The high-efficiency hot bending production process of glass-ceramics according to claim 7, characterized in that: In the S200 preheating process, the glass-ceramics raw material is heated for 55-65 seconds.
9. The high-efficiency hot bending production process of glass-ceramics according to claim 7, characterized in that: In the S300 molding process, after holding the pressure for a first period of time, the second upper heating plate slowly rises.
10. The high-efficiency hot bending production process of glass-ceramics according to claim 7, characterized in that: In the S400 slow cooling process, after baking and keeping warm for the second time period, the first upper heating plate slowly rises.
Citation Information
Patent Citations
Glass ceramic hot bending, forming and crystallizing tunnel furnace and method for producing glass ceramic products
CN106977084A
Hot bending machine and hot bending forming method
CN109970327A
Glass ceramic, glass ceramic product and manufacturing method thereof
CN115028365A
AG effect glass ceramic preparation mold, glass ceramic and preparation method thereof
CN115432946A
3D glass hot -bend forming machine