Thiourea, preparation method and application thereof
By controlling the acid insoluble content in lime nitrogen and optimizing the preparation process of thiourea, the silicon content in thiourea is reduced, the problem of filter capsule blockage during thiourea synthesis is solved, and the production efficiency and product quality of polythioalk and optical lenses are improved.
Patent Information
- Application Number
- CN202411043624.1
- Authority / Receiving Office
- CN · China
- Patent Type
- Applications(China)
- Current Assignee / Owner
- Filing Date
- 2024-07-31
- Publication Date
- 2024-11-15
AI Technical Summary
During the preparation of polythiol and optical lenses, thiourea is prone to clogging of the filter capsule during synthesis, resulting in low production efficiency and unstable product quality. The main reason is that the acid insoluble substances in lime nitrogen contain silicone oxygen compounds in alkaline environments Convert to silicates or silicates to form flocs or particles to block the filter capsule.
By controlling the content of acid insoluble matter in lime nitrogen, ensuring that the silicon content in thiourea is less than 30ppm, the preparation of thiourea is carried out by two reaction steps. The pH value of the first step is set to above 7, and the reaction temperature of the second step is 70°C to 90°C to reduce the formation of silicon oxygen compounds, extend the use time of the filter capsule and improve production efficiency.
It effectively avoids filter capsule blockage, improves the production efficiency of polythiol and optical lenses, shortens the pouring time, and reduces it from more than 100 minutes to less than 50 minutes, significantly improving product quality.
Smart Images

Figure BDA0004972962460000081
Abstract
Description
Technical Field
[0001] The invention relates to the technical field of chemical synthesis, and in particular to thiourea, a preparation method thereof and application thereof. Background Art
[0002] Thiourea, also known as thiourea, is an important chemical raw material and organic chemical intermediate. It is used to produce drugs such as sulfaimidazole, methylthiouracil, methionine, etc. It is the raw material for synthesizing ascaridole and contraceptives. It can also be used to synthesize anti-thyroid drugs, anti-tuberculosis drugs, intravenous anesthetics, etc.; Thiourea can also be used as a high-purity analytical reagent for the determination of osmium, bismuth, rhodium, selenium, lead, tellurium, nitrites, etc. It is also used as a chromatographic analysis reagent, a complex indicator for the determination of bismuth, a masking agent, etc.
[0003] In the field of optical materials, thiourea is usually used as a vulcanizing agent, such as the synthesis of polythiol series products used as optical materials, which have the advantages of economy, environmental protection, high conversion rate and stable product quality. However, with the development of production technologies such as polythiol and optical lenses towards intelligence, refinement and automation, there are problems of unstable production and low production efficiency in the preparation process of polythiol and synthesis or optical lenses. For example, the filter capsule is prone to blockage during the synthesis of polythiourea, resulting in reduced filtration efficiency, slowed flow rate and even pipe burst after blockage, which seriously affects production efficiency. Summary of the invention
[0004] In view of this, the present invention provides a thiourea, a preparation method thereof and an application thereof. The thiourea provided in the present application has a low silicon content and will not block the filter capsule when used to synthesize polythiol, thereby improving production efficiency.
[0005] Patent CN112358613B discloses a kind of preparation method of polythiol, it first mixes epihalohydrin raw material and composite solvent to suspension, then suspension is mixed with flocculant and impurity therein is carried out flocculation process, then obtain polyol with mercaptoethanol, basic compound mixed reaction, then mix with thiourea, acid to carry out salt-forming reaction, finally hydrolyze under alkaline conditions, obtain optical resin polythiol.This method adopts flocculant to remove impurity in epihalohydrin raw material, improves the color and aspect of the finished product, makes the polythiol chromaticity obtained lower.But the applicant finds in the production practice process, although this method has removed the impurity in epihalohydrin raw material, the phenomenon of filter capsule blocking still occurs in the polythiol production process. The applicant has found through research that the cause of the filter capsule blockage during the production of polythiol comes from the acid-insoluble matter in the lime nitrogen, the raw material for producing thiourea. The acid-insoluble matter contains silicon oxide compounds, which do not exist directly as impurities. Instead, in the alkaline environment of thiourea synthesis, the silicon oxide compounds are converted into compounds or complexes such as silicates or silicate esters, and gradually form floccules or particles, which remain in the thiourea product and block the filter capsule during the subsequent synthesis of polythiol. Based on this, the applicant has found that by controlling the content of acid-insoluble matter in lime nitrogen, the content of silicon in thiourea can be controlled, thereby extending the service life of the filter capsule, eliminating the need for frequent replacement of the filter capsule, and improving production efficiency.
[0006] The present application provides a thiourea, wherein the silicon content in the thiourea is less than 30 ppm.
[0007] In some specific implementations, the silicon content in the thiourea is less than 25 ppm.
[0008] The present application also provides a method for preparing thiourea described in the above technical solution, comprising the following steps:
[0009] Lime nitrogen and hydrogen sulfide undergo addition reaction to obtain thiourea; wherein the content of acid insoluble matter in the lime nitrogen is less than 5%.
[0010] In some specific implementations, the following steps are specifically included:
[0011] a) adding hydrogen sulfide into thiourea mother liquor and then adding lime nitrogen to carry out the first reaction;
[0012] b) adding lime nitrogen to the reaction solution obtained by the first reaction, and performing a second reaction to obtain thiourea.
[0013] In some specific implementations, the pH values of the first reaction and the second reaction are independently above 7.
[0014] In some specific implementations, in step a), the mass ratio of hydrogen sulfide to lime nitrogen is 800-1200:500-800;
[0015] The ratio of the amount of lime nitrogen in step b) to the amount of lime nitrogen in step a) is 500-800:2000-4000.
[0016] In some specific implementations, lime nitrogen is added in batches in step a);
[0017] In the step b), lime nitrogen is added once;
[0018] The temperature of the second reaction is 70° C. to 90° C., and the time is 2 h to 5 h.
[0019] The present application also provides a method for preparing polythiol, comprising the following steps:
[0020] Lime nitrogen and hydrogen sulfide undergo addition reaction to obtain thiourea; wherein the content of acid insoluble matter in the lime nitrogen is less than 5%;
[0021] The thiourea reacts with a polyol to obtain a polythiol.
[0022] The present application also provides polythiol prepared by the preparation method described in the above technical solution.
[0023] The present application also provides a method for preparing an optical material, comprising the following steps:
[0024] Lime nitrogen and hydrogen sulfide undergo addition reaction to obtain thiourea; wherein the content of acid insoluble matter in the lime nitrogen is less than 5%;
[0025] The thiourea reacts with the polyol to obtain polythiol;
[0026] The polythiol and isocyanate undergo polymerization reaction to obtain an optical material.
[0027] The present application uses lime nitrogen with an acid-insoluble content of less than 5% as a raw material, and reacts with hydrogen sulfide to produce a silicon content of less than 30ppm in the thiourea. When the thiourea with a low silicon content is used as a raw material to prepare polythiols and then to prepare optical lenses, the content of flocculants or impurity particles in the slurry is relatively low, and the slurry can avoid blocking the filter capsule during the casting process of the lens, thereby improving production efficiency and product quality. Experimental results show that when the thiourea provided by the present application is used to produce polythiols and then to produce optical lenses, the time for 40kg of material and 4 people to cast at the same time can be shortened from more than 100 minutes to less than 50 minutes, greatly improving production efficiency. DETAILED DESCRIPTION
[0028] It should be understood that the expression "one or more of..." includes each of the items recited after the expression individually and in various different combinations of two or more of the recited items, unless otherwise understood from the context and usage. The expression "and / or" in combination with three or more recited items should be understood to have the same meaning, unless otherwise understood from the context.
[0029] The use of the terms "comprising", "having" or "containing", including their grammatical synonyms, should generally be understood as open and non-restrictive, for example not excluding other unrecited elements or steps, unless otherwise specifically stated or otherwise understood from the context.
[0030] It should be understood that the order of steps or the order in which certain actions are performed is not important as long as the present invention remains operable. In addition, two or more steps or actions may be performed simultaneously.
[0031] The use of any and all examples or exemplary language, such as "for example" or "including", herein is intended only to better illustrate the invention and does not limit the scope of the invention unless otherwise claimed. No language in this specification should be construed as indicating that any non-claimed element is essential to the practice of the invention.
[0032] In addition, the numerical ranges and parameters used to define the present invention are approximate values, and the relevant values in the specific embodiments have been presented as accurately as possible. However, any numerical value inherently inevitably contains standard deviations due to individual test methods. Therefore, unless otherwise expressly stated, it should be understood that all ranges, quantities, values and percentages used in this disclosure are modified by "about". Here, "about" generally means that the actual value is within plus or minus 10%, 5%, 1% or 0.5% of a specific value or range.
[0033] The present application provides a thiourea, wherein the silicon content in the thiourea is less than 30 ppm, preferably less than 25 ppm, more preferably less than 22 ppm, and more preferably less than 20 ppm. In some specific implementations, the silicon content in the thiourea is detected using an X-ray fluorescence spectrometer (XRF).
[0034] The present application also provides a method for preparing thiourea described in the above technical solution, comprising the following steps:
[0035] Lime nitrogen and hydrogen sulfide undergo addition reaction to obtain thiourea; wherein the content of acid insoluble matter in the lime nitrogen is less than 5%.
[0036] The present application uses hydrogen sulfide and lime nitrogen as raw materials to carry out addition reaction to prepare thiourea. Lime nitrogen is also called calcium cyanamide. Except for the content of acid-insoluble matter, the present application has no special restrictions on it and it can be purchased from the market. The content of acid-insoluble matter in the lime nitrogen is less than 5%, preferably less than 4%, more preferably less than 3.5%, and more preferably less than 2%. In some specific implementations, the content of acid-insoluble matter in the lime nitrogen is determined by referring to the method described in GB / T 23742-2009 "Determination of hydrochloric acid insoluble ash in feed".
[0037] In some specific implementations, the method for preparing thiourea specifically comprises the following steps:
[0038] a) adding hydrogen sulfide into thiourea mother liquor and then adding lime nitrogen to carry out the first reaction;
[0039] b) adding lime nitrogen to the reaction solution obtained by the first reaction, and performing a second reaction to obtain thiourea.
[0040] The present application uses thiourea mother liquor as the reaction medium, and the thiourea content in the thiourea mother liquor is preferably 5% to 20%, and more preferably 10 to 15%. Hydrogen sulfide gas is introduced into the thiourea mother liquor, and then lime nitrogen is added for the first reaction. In some specific implementations, the flow rate of the hydrogen sulfide gas is 200g / h to 700g / h, and preferably 400g / h to 500g / h; in some specific implementations, when the hydrogen sulfide gas is introduced, the temperature of the reaction medium is preferably 20°C to 40°C, and more preferably 30°C to 40°C. In some specific implementations, in step a), lime nitrogen is added in multiple times, for example, it can be added in three times, and one-third of the amount of lime nitrogen is added each time, and the interval time for each time is preferably 20min to 40min, and preferably 30min. After adding lime nitrogen, the first reaction is carried out while passing hydrogen sulfide gas. The first reaction is an exothermic reaction. When the temperature reaches 40°C to 70°C, preferably 45°C to 60°C, and more preferably 50°C to 55°C, the introduction of hydrogen sulfide is stopped. In some specific implementations, in step a), the mass ratio of hydrogen sulfide to lime nitrogen is 800 to 1200:500 to 800, preferably 900 to 1100:600 to 700. In some specific implementations, the pH value of the first reaction is above 7. In some specific implementations, after the first reaction is completed, the content of calcium hydrosulfide in the obtained reaction solution is preferably 5% to 15%, more preferably 8 to 12%, and most preferably 9.5%.
[0041] After the first reaction is completed, lime nitrogen is added to the obtained reaction solution for a second reaction. In some specific implementations, lime nitrogen is added once in step b). In some specific implementations, the ratio of the amount of lime nitrogen in step b) to the amount of lime nitrogen in step a) is 500-800:2000-4000, preferably 600-700:2500-3500, more preferably 600-700:2800-3200. In some specific implementations, the pH value of the second reaction is above 7. In some specific implementations, the temperature of the second reaction is 70°C-90°C, preferably 75°C-85°C, and the time is 2h-5h, preferably 3h-4h.
[0042] After the second reaction is completed, the slurry after the reaction is filtered, crystallized, centrifuged, and dried to obtain thiourea. The present application has no special restrictions on the filtering, crystallization, centrifugation, and drying processes, and commonly used methods by those skilled in the art can be used.
[0043] The present application also provides a method for preparing polythiol, comprising the following steps:
[0044] Lime nitrogen and hydrogen sulfide undergo addition reaction to obtain thiourea; wherein the content of acid insoluble matter in the lime nitrogen is less than 5%;
[0045] The thiourea reacts with a polyol to obtain a polythiol.
[0046] In the present application, thiourea is obtained according to the method described above, and then reacted with a polyol to prepare a polythiol. The present application has no particular limitation on the preparation method of the polythiol, and the method commonly used by those skilled in the art can be used, for example, referring to the method disclosed in CN112430326A, a polyol, thiourea and an acid solution are mixed to form a salt, and then an alkali solution is added to hydrolyze to obtain a polythiol, and then a polythiol compound is obtained by acid washing, extraction, etc.
[0047] In some specific implementations, the polythiol includes but is not limited to 2,3-dithio(2-mercapto)-1-propanethiol, thiodiglycol mercaptan, dithiomethyldithiane, bis(mercaptomethyl)-3,6,9-trithiaundecane-1,11-dithiol, which can be selected according to the raw material polyol.
[0048] The present application also provides polythiol prepared by the preparation method described in the above technical solution. Since the silicon content in thiourea is low, the silicon content in the prepared polythiol is low.
[0049] The present application also provides a method for preparing an optical material, comprising the following steps:
[0050] Lime nitrogen and hydrogen sulfide undergo addition reaction to obtain thiourea; wherein the content of acid insoluble matter in the lime nitrogen is less than 5%;
[0051] The thiourea reacts with the polyol to obtain polythiol;
[0052] The polythiol and isocyanate undergo polymerization reaction to obtain an optical material.
[0053] After the polythiol is prepared according to the method described above, it is polymerized with isocyanate to obtain an optical material. The present application has no particular restrictions on the preparation method of the optical material, and the method commonly used by those skilled in the art can be used, for example, referring to the method disclosed in CN112430326A, the polythiol compound, isocyanate and catalyst are mixed, and then degassed under negative pressure; then the degassed mixture is heated to perform a polymerization reaction, and the optical material can be obtained.
[0054] The present invention uses lime nitrogen with an acid-insoluble content of less than 5% as a raw material, and reacts with hydrogen sulfide to produce a thiourea with a silicon content of less than 30 ppm. When the thiourea with a low silicon content is used as a raw material to prepare polythiol and then to prepare optical lenses, the content of flocculants or impurity particles in the slurry is relatively small, and the slurry can avoid blocking the filter capsule during the casting process of the lens, thereby improving production efficiency and product quality.
[0055] The thiourea, preparation method and application thereof provided in the present application are further described below in conjunction with examples.
[0056] In the following examples, the acid-insoluble content (%) in lime nitrogen was determined by referring to the method described in GB / T23742-2009 "Determination of hydrochloric acid insoluble ash in feed";
[0057] Evaluation of silicon content in thiourea: X-ray fluorescence spectrometer (XRF) was used for detection;
[0058] The pouring speed evaluation of optical lens production is carried out according to the following method: During lens production, 1 cylinder of material contains 40 kg, 4 people are pouring at the same time, and the total pouring time required is.
[0059] Example 1
[0060] (1) Preparation of thiourea:
[0061] First, 15000g of thiourea mother liquor was added to the reactor, and the thiourea content in the mother liquor was 11.2%. The reactor was heated to 35°C, and hydrogen sulfide was introduced into the reactor, and the hydrogen sulfide flow rate was controlled at 400-500g / h; after the hydrogen sulfide was introduced, 600g of lime nitrogen was added to the reactor in three times, and the acid insoluble content in the lime nitrogen was 0.2%, and each time 200g was separated by 30min; after the addition of lime nitrogen, hydrogen sulfide was continued to be introduced for 1 hour and then stopped, and 950g of hydrogen sulfide was introduced in total. After the reaction exotherm was gradually raised to 55°C, the calcium hydrosulfide content of the solution after the first step reaction was detected to be 9.5%, and then 3080g of lime nitrogen was added to the reactor at one time, and the reaction temperature was controlled to 79-81°C, and the reaction was terminated after 3 hours. The slurry after the reaction was filtered, crystallized, centrifuged, and dried to obtain 2082g of the final thiourea product, with a thiourea content of 99.2% and a yield of 95.3%.
[0062] The thiourea product was tested and found to contain 5 ppm silicon.
[0063] (2) Preparation of polythiol:
[0064] Add 156.6g (2.0mol) of mercaptoethanol to a four-necked flask equipped with a thermometer, a stirrer, and a constant pressure dropping funnel, and add 133.3g (1.0mol) of a 30% aqueous sodium hydroxide solution through the constant pressure dropping funnel. Similarly, add 92.6g (1.0mol) of epichlorohydrin through the constant pressure dropping funnel, and react for 30 minutes after the addition is completed. Then add 405.6g (4.0mol) of hydrochloric acid with a concentration of 36% and 229.8g (3.0mol) of thiourea prepared in step (1), react at 110°C for 100-240min to form thiourea; then cool to 60°C, add 425.0g (4.5mol) of ammonia water with a concentration of 18%, and hydrolyze for 3h, separate the layers to obtain a lower layer of crude product, and the crude product is acid-washed and water-washed, and water is removed by vacuum evaporation, and fine filtration is performed to obtain a polythiol product.
[0065] (3) Preparation of optical lenses:
[0066] Add 52.0 parts by mass of xylene diisocyanate, 0.01 parts by mass of catalyst (dibutyltin dichloride) and 0.08 parts by mass of release agent (polyphosphate) into the batching kettle, stir and dissolve at 15°C; add 48.0 parts by mass of polythiol prepared in step (2) and stir evenly. Use a vacuum pump for degassing, control the pressure at 350Pa, and degassing time for 0.5h to prepare a mixed solution with a viscosity level between 40mPa.s and 50mPa.s. Pass the solution through a capsule filter and pour it into a glass mold. After pouring, lay it flat on a tray. The capsule filter uses a filter capsule with a pore size of 0.45μm produced by cobetter. 1 cylinder of material 40kg, 4 people pour at the same time, and record the total pouring time required.
[0067] Embodiment 2~4, comparative example 1~3:
[0068] The preparation process of Example 1 is followed, except that the content of the lime nitrogen insoluble matter used is different.
[0069] The silicon content in the obtained thiourea product was detected, and the total casting time required was collected. The results are shown in Table 1, which shows the parameters in the examples and comparative examples of the present application.
[0070] Table 1 Parameters in the Examples and Comparative Examples of the present application
[0071]
[0072] As shown in Table 1, by selecting lime nitrogen with an acid-insoluble content of less than 5% to prepare thiourea, the silicon content in thiourea can be as low as 30 ppm, so that when used to prepare polythiourea or optical lenses, it will not clog the filter capsule and will not affect continuous production, thereby improving production efficiency and product quality.
[0073] The above is only a preferred embodiment of the present invention. It should be pointed out that for ordinary technicians in this technical field, several improvements and modifications can be made without departing from the principle of the present invention. These improvements and modifications should also be regarded as the scope of protection of the present invention.
Claims
1. A thiourea, characterized in that The silicon content in the thiourea is less than 30 ppm.
2. Thiourea according to claim 1, characterized in that The silicon content in the thiourea is less than 25 ppm.
3. The method for preparing thiourea according to claim 1 or 2, comprising the following steps: Lime nitrogen and hydrogen sulfide undergo addition reaction to obtain thiourea; wherein the content of acid-insoluble matter in the lime nitrogen is less than 5%.
4. The preparation method according to claim 3, characterized in that: The specific steps include: a) adding hydrogen sulfide into thiourea mother liquor and then adding lime nitrogen to carry out the first reaction; b) adding lime nitrogen to the reaction solution obtained by the first reaction, and performing a second reaction to obtain thiourea.
5. The preparation method according to claim 4, characterized in that: The pH values of the first reaction and the second reaction are independently 7 or more.
6. The preparation method according to claim 5, characterized in that: In the step a), the mass ratio of hydrogen sulfide to lime nitrogen is 800-1200:500-800; The ratio of the amount of lime nitrogen in step b) to the amount of lime nitrogen in step a) is 500-800:2000-4000.
7. The preparation method according to claim 6, characterized in that: In said step a), lime nitrogen is added in portions; In the step b), lime nitrogen is added once; The temperature of the second reaction is 70° C. to 90° C., and the time is 2 h to 5 h.
8. A method for preparing polythiol, comprising the following steps: Lime nitrogen and hydrogen sulfide undergo addition reaction to obtain thiourea; wherein the content of acid insoluble matter in the lime nitrogen is less than 5%; The thiourea reacts with a polyol to obtain a polythiol.
9. The polythiol prepared by the preparation method according to claim 8.
10. A method for preparing an optical material, comprising the following steps: Lime nitrogen and hydrogen sulfide undergo addition reaction to obtain thiourea; wherein the content of acid insoluble matter in the lime nitrogen is less than 5%; The thiourea reacts with the polyol to obtain polythiol; The polythiol and isocyanate undergo polymerization reaction to obtain an optical material.