Method and system for purifying N-methylmorpholine-N-oxide and obtained N-methylmorpholine-N-oxide

The crude N-methylmorpholine-N-oxide product was purified by cooling and crystallization, which solved the problems of high energy consumption, serious pollution and low purity in the prior art, and achieved high efficiency and low cost N-methyl Morpholine-N-oxide purification meets Tensil production standards and reduces environmental pollution.

CN118955433APending Publication Date: 2024-11-15HEBEI HUAMAO WEIYE TECH CO LTD
View PDF 0 Cites 0 Cited by

Patent Information

Application Number
CN202410921676.8
Authority / Receiving Office
CN · China
Patent Type
Applications(China)
Current Assignee / Owner
Filing Date
2021-05-18
Publication Date
2024-11-15

AI Technical Summary

Technical Problem

The existing N-methylmorpholine-N-oxide purification process has high energy consumption, polluted the environment, low yield and low purity, and the industrial purification process has serious environmental protection problems and high purification costs.

Method used

The crude N-methylmorpholine-N-oxide product was purified by cooling and crystallization. By controlling the temperature and seed addition amount, it was possible to efficiently remove impurities, avoid the use of ion exchange resin, and reduce energy consumption and pollution.

Benefits of technology

Achieve high efficiency, low cost, green purification of N-methylmorpholine-N-oxide, with a recovery rate of more than 97%, the product conductivity is less than 10μs/cm, and the impurity content is extremely low. It meets the production quality standards of Tennis, and solves the problem. The problem of high salt and high COD wastewater and waste resin polluting the environment.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure CN118955433A_ABST
    Figure CN118955433A_ABST
Patent Text Reader

Abstract

The invention discloses a method and a system for purifying N-methylmorpholine-N-oxide and the obtained N-methylmorpholine-N-oxide. The N-methylmorpholine-N-oxide is derived from an N-methylmorpholine-N-oxide crude product prepared by reaction of N-methylmorpholine and hydrogen peroxide, the mass concentration of N-methylmorpholine-N-oxide in the crude product of N-methylmorpholine-N-oxide is 50%-60%, and the purification method comprises the following steps: cooling and crystallizing the crude product of N-methylmorpholine-N-oxide at-20 DEG C to 78 DEG C to obtain N-methylmorpholine-N-oxide crystals. The NMMO purification method is low in cost, the obtained NMMO product is high in purity, and almost no three wastes are generated. Different from an existing NMMO purification process, the purification method does not need ion exchange resin, so that the environmental protection problems of a large amount of high-salt and high-COD wastewater, waste ion exchange resin and the like caused by regeneration of the ion exchange resin are thoroughly solved.
Need to check novelty before this filing date? Find Prior Art

Description

[0001] The present application is a divisional application filed by the applicant based on the parent application (application number: 202110521394.5, invention name: purification method, system, detection method and obtained N-methylmorpholine-N-oxide). Technical Field

[0002] The present invention relates to a method for purifying N-methylmorpholine-N-oxide, a purification system for N-methylmorpholine-N-oxide and the obtained N-methylmorpholine-N-oxide. Background Art

[0003] N-methylmorpholine-N-oxide (methylmorpholine oxide, NMMO) is an excellent solvent with extremely strong solubility for cellulose. Among the solvents that can dissolve cellulose at present, only NMMO can be truly industrialized and has a promising future. NMMO can dissolve cellulose very well and can obtain a cellulose solution with good fiber and film forming properties. The Tencel (Lyocell) fiber spun from this solution has excellent fiber properties. In addition, the NMMO solvent is easy to recycle during the production process of Lyocell fiber, with a recovery rate of more than 99.5%. Lyocell fiber has great advantages in environmental protection, energy consumption, fiber performance and other aspects, and has a very broad development prospect.

[0004] Industrial NMMO is prepared by the reaction of hydrogen peroxide (H2O2) and N-methylmorpholine. The crude NMMO product obtained by the reaction usually has a darker color. According to the practice of industrial preparation of NMMO by the applicant (Huamao Weiye Green Technology Co., Ltd.), the NMMO yield of the reaction is above 99%, and the total impurity mass content in the crude NMMO reaction product is less than 1%. The impurities contain a certain amount of unreacted N-methylmorpholine, morpholine, hydrogen peroxide and some impurities generated by side reactions such as the strong carcinogen N-nitrosomorpholine, organic peroxides and some unknown impurities. It also contains a certain amount of metal cations such as copper and iron ions and anions such as phosphate and nitrate. The conductivity of the crude NMMO product is generally above 500μs / cm.

[0005] The quality standards of NMMO aqueous solution products with a mass concentration of 50% that can be used for Tencel production are: conductivity less than 10μs / cm, copper ion content less than 2ppm, iron ion content less than 2ppm, unreacted hydrogen peroxide content less than 50ppm, N-methylmorpholine content less than 100ppm, morpholine content less than 200ppm, N-nitrosomorpholine content less than 50ppb, and the product appearance color is a colorless and transparent solution. For Tencel production, the lower the content of the above impurities in the NMMO 50% aqueous solution product, the better, but further reducing the content of these impurities requires more complicated and harsh purification steps and purification process conditions than the current NMMO purification process, and the purification cost will increase significantly.

[0006] In addition, NMMO is an amine oxide, which will undergo a Cope elimination reaction at a certain temperature to generate a corresponding olefin compound with a double bond at the end. Since a large amount of hydrogen peroxide is present in the preparation process of NMMO, hydrogen peroxide will react with olefins to generate corresponding organic peroxides such as organic hydrogen peroxide, peroxide ether and organic peroxyacid, so the crude NMMO product inevitably contains a certain amount of organic peroxide impurities.

[0007] The breakage of cellulose molecular chains in Tencel production is mainly initiated by N-methylmorpholine free radicals produced by the free radical decomposition reaction of NMMO (Adorjan I., Potthast A., Rosenau T., Sixta H. and Kosma P. 2005. Discoloration of cellulose solutions in N-methylmorpholine-N-oxide (Lyocell). Part 1: Studies on model compounds and pulps. Cellulose 12: 51-57) (Rosenau T., Potthast A., Adorjan I., Hofinger A., ​​Sixta H., Firgo H. and Kosma P. 2002. Cellulose solutions in N-methylmorpholime-N-oxide (NMMO) -Degradation processes and stabilizers. Cellulose 9: 283-291). Peroxide includes inorganic peroxides such as hydrogen peroxide and organic peroxides, which are excellent free radical initiators. They can decompose and produce free radicals at a certain temperature, thereby inducing the occurrence of NMMO free radical decomposition reaction, causing cellulose molecular chain fracture, and reducing the strength of Tencel fiber. The final product of NMMO free radical decomposition reaction is morpholine and formaldehyde, and the two may continue to react to generate methylene morpholine carbon ions. If the concentration of methylene morpholine carbon ions in the spinning solution formed by cellulose and NMMO is too high, a large amount of NMMO autocatalytic decomposition reactions with intense exothermicity can be induced, resulting in uncontrolled explosion (US 5556452), so peroxide is very harmful to Tencel production. At present, more and more Tencel manufacturers have realized that organic peroxides in NMMO products may cause harm to Tencel production, and the organic peroxide impurity content except hydrogen peroxide in NMMO has begun to be regulated. Although no further relevant standards have been issued at present, it is required that the peroxide content in NMMO is as low as possible.

[0008] During the production process, NMMO comes into contact with metal equipment, reactors, pipes and containers, resulting in NMMO containing some metal ions such as copper and iron ions. In addition, hydrogen peroxide also contains some metal and non-metal ions. Copper and iron ions will catalyze the decomposition reaction of NMMO, resulting in the loss of NMMO. In the production of Tencel, the copper and iron ions in the NMMO cellulose solution will also complex with cellulose, resulting in cellulose degradation (Wu Cuiling, Li Xinping, Qin Shengli and Wang Jianyong, "Research on a New Organic Cellulose Solvent - NMMO", Journal of Lanzhou University of Technology, 2005, 31(2), 73-76). In addition, copper and iron ions will also complex with propyl gallate added in the production of Tencel to produce a darker color, affecting the chromaticity of the final Tencel fiber. At the same time, copper and iron ions will catalyze the oxidation of cellulose by peroxide in NMMO, accelerate the decomposition of cellulose, and catalyze the Maillard reaction to produce color. It will even catalyze the self-catalytic free radical decomposition reaction of NMMO, releasing a large amount of heat, which may cause an explosion in severe cases (such as CN 104801354B and US5556452). Therefore, excessive copper and iron ions are very harmful to the production of NMMO, so the copper and iron ion content in Tencel-grade NMMO products is required to be as low as possible.

[0009] At present, the industrial purification process of NMMO is a multi-step purification process, in which an ion exchange resin method is used to remove anions and cations and some organic impurities including pigments in the crude NMMO product (CN 104801354 B), and other purification processes (such as X-ray irradiation and special adsorption resins, etc.) are used to remove N-nitrosomorpholine and other organic impurities. In order to obtain higher quality NMMO products, special catalytic reduction treatment is also required to further remove peroxides (including hydrogen peroxide, organic hydrogen peroxide, peroxy ether and organic peroxyacid, etc.). If only ion exchange resin is used to purify NMMO, non-ionic organic impurities including peroxides contained therein cannot be completely removed.

[0010] Failed ion exchange resins need to be regenerated before they can be reused. Cation exchange resins are usually regenerated by continuous flushing with 4-5% hydrochloric acid solution at 4-6 times the volume of the resin, while anion exchange resins are regenerated by continuous flushing with 4-5% NaOH solution at 4-6 times the volume of the resin. After acid-base neutralization, these regenerated waste liquids contain not only about 5% NaCl and other small amounts of metal and non-metal ion salts, but also other organic impurities adsorbed by the resin and a small amount of NMMO adsorbed, so the COD content is usually 5000ppm-20000ppm. Generally, the production of 1 ton of 50% NMMO aqueous solution products will produce 1-2 tons of high-COD and high-salt wastewater. Due to the high salt content, the wastewater cannot be treated by catalytic oxidation, because sodium ions and chloride ions will cause poisoning of the catalyst Pt, and it cannot be directly incinerated by an organic waste liquid incinerator (TO), because high salt will not only seriously corrode the incinerator material, but also a large amount of waste salt remaining in the incinerator will seriously affect the operation of the incinerator. Therefore, usually only multi-effect evaporation (MVR) can be used to concentrate semi-solid waste salt to separate the salt from the COD-containing wastewater. However, this treatment method not only has high energy consumption, but also contains a high COD in the waste salt, which can only be handed over to a qualified environmental protection company as hazardous waste treatment, and the cost is very high. The COD content in the water obtained by MVR evaporation is usually also very high, and must be treated by catalytic oxidation or direct incineration. In addition, ion exchange resins and special adsorption resins for adsorbing organic impurities are not only expensive, but also generally have a lifespan of only 1-2 years. In addition, scrapped resins are listed as hazardous wastes according to the national hazardous waste classification list and must be handled by qualified environmental protection companies, which is also very expensive. At the same time, since ion exchange resins and special resins for adsorbing organic impurities will adsorb NMMO, the yield of NMMO will be reduced. Therefore, the current industrial purification process for preparing Tencel-grade NMMO not only has serious "three wastes" environmental protection problems, but also has very high energy consumption and purification costs.

[0011] "Research on a New Organic Cellulose Solvent - NMMO" (Wu Cuiling, Li Xinping, Qin Shengli and Wang Jianyong, Journal of Lanzhou University of Technology, 2005, 31(2), 73-76) disclosed that NMMO can combine with water molecules to form three crystals with different water contents. One NMMO molecule can combine with one water molecule to form a monohydrate crystal (NMMO·H2O) with the appearance of white crystals, melting point: 76-78°C, NMMO concentration in the crystal is 84.5%, and density is 1.28 g / cm 3 ; 2 NMMO molecules can also form 2.5 hydrate crystals with 5 water molecules (2NMMO·5H2O), which are white crystals with a melting point of 36-39°C, a NMMO concentration of 72.2%, and a density of 1.33 g / cm 3; One NMMO molecule can also form pentahydrate crystals with five water molecules (NMMO·5H2O), with a melting point of -20°C and a NMMO concentration of 56.5% in the crystals. NMMO·H2O and NMMO·2.5H2O can be obtained by dehydrating NMMO aqueous solution. The main research was on the solubility of NMMO hydrate crystals in cellulose. By taking advantage of the low melting point and good cellulose dissolving properties of NMMO·H2O, NMMO·H2O was used to dissolve cellulose. Summary of the invention

[0012] The main purpose of the present invention is to provide a purification method and system for N-methylmorpholine-N-oxide and the obtained N-methylmorpholine-N-oxide, so as to overcome the defects of the prior art N-methylmorpholine-N-oxide purification process, such as high energy consumption, environmental pollution, low yield, and low purity of the obtained N-methylmorpholine-N-oxide.

[0013] In order to achieve the above-mentioned object, the present invention provides a method for purifying N-methylmorpholine-N-oxide, wherein the N-methylmorpholine-N-oxide is derived from a crude N-methylmorpholine-N-oxide product prepared by reacting N-methylmorpholine with hydrogen peroxide, wherein the mass concentration of N-methylmorpholine-N-oxide in the crude N-methylmorpholine-N-oxide product is 50% to 60%. The purification method comprises: cooling and crystallizing the crude N-methylmorpholine-N-oxide product at a temperature between -20°C and 78°C to obtain N-methylmorpholine-N-oxide crystals.

[0014] In one embodiment, the purification method of N-methylmorpholine-N-oxide of the present invention further comprises concentrating the crude N-methylmorpholine-N-oxide product to make the mass concentration of N-methylmorpholine-N-oxide in the crude N-methylmorpholine-N-oxide product be 56.5% to 84.5%, and then cooling and crystallizing.

[0015] In one embodiment of the method for purifying N-methylmorpholine-N-oxide of the present invention, seed crystals are added during the cooling crystallization process, and the amount of the seed crystals added is 0.1% to 1.0% of the weight of the crude N-methylmorpholine-N-oxide product.

[0016] In one embodiment of the method for purifying N-methylmorpholine-N-oxide of the present invention, when the mass concentration of N-methylmorpholine-N-oxide in the crude N-methylmorpholine-N-oxide product is 56.5% to 72.2% after concentration treatment, the temperature of the cooling crystallization is -20 to 39°C; when the mass concentration of N-methylmorpholine-N-oxide in the crude N-methylmorpholine-N-oxide product is greater than 72.2% and less than or equal to 84.5% after concentration treatment, the temperature of the cooling crystallization is greater than 39°C and less than or equal to 78°C.

[0017] In one embodiment of the method for purifying N-methylmorpholine-N-oxide of the present invention, after concentration treatment, the mass concentration of N-methylmorpholine-N-oxide in the crude N-methylmorpholine-N-oxide product is 66% to 71%, and the temperature of the cooling crystallization is 25° C. to 35° C.

[0018] In one embodiment of the method for purifying N-methylmorpholine-N-oxide of the present invention, during the cooling crystallization process, the cooling rate from the beginning of the appearance of crystals to 30°C is 1 to 2°C / hour; between -20°C and 30°C, the cooling rate is 3 to 4°C / hour.

[0019] In one embodiment of the method for purifying N-methylmorpholine-N-oxide of the present invention, the cooling crystallization comprises at least primary cooling crystallization and secondary cooling crystallization, the primary cooling crystallization obtains N-methylmorpholine-N-oxide crystals and a crystallization mother liquor, and the crystallization mother liquor is concentrated and then subjected to secondary cooling crystallization.

[0020] In order to achieve the above object, the present invention also provides N-methylmorpholine-N-oxide obtained by the purification method of the above N-methylmorpholine-N-oxide, the recovery rate of N-methylmorpholine-N-oxide is more than 97%, the liquid chromatography detection result of N-methylmorpholine-N-oxide is that the organic impurity content is 0, the obtained N-methylmorpholine-N-oxide is prepared into an aqueous solution with a mass concentration of 50%, the conductivity of the aqueous solution is 0-10μs / cm, and the hydrogen peroxide content is 0.

[0021] In order to achieve the above object, the present invention further provides a method for purifying N-methylmorpholine-N-oxide, wherein the purification method does not use ion exchange resin.

[0022] In order to achieve the above object, the present invention further provides a purification system for N-methylmorpholine-N-oxide, which is used for purifying N-methylmorpholine-N-oxide in a crude N-methylmorpholine-N-oxide product prepared by reacting N-methylmorpholine with hydrogen peroxide. The purification system comprises:

[0023] A crystallization device, used for crystallization treatment of crude N-methylmorpholine-N-oxide product;

[0024] A control device is connected to the crystallization device to control the crystallization conditions in the crystallization device.

[0025] In one embodiment, the purification system of N-methylmorpholine-N-oxide of the present invention further comprises a concentrating device connected to the crystallization device and the control device, so that the crude N-methylmorpholine-N-oxide product is concentrated in the concentrating device and then input into the crystallization device; the control device controls the concentrating conditions of the concentrating device.

[0026] In order to achieve the above object, the present invention further provides a method for detecting N-methylmorpholine-N-oxide, wherein the N-methylmorpholine-N-oxide is obtained by cooling and crystallizing a crude N-methylmorpholine-N-oxide product prepared by reacting N-methylmorpholine with hydrogen peroxide, and the detection method comprises the determination of the residual rate of crystalline impurities of the N-methylmorpholine-N-oxide, and the determination of the residual rate of crystalline impurities of the N-methylmorpholine-N-oxide comprises the following steps:

[0027] Step 1, performing liquid chromatography determination on the crude N-methylmorpholine-N-oxide product at a wavelength of 200 nm to 220 nm, or 200 nm to 210 nm, performing area integration on all impurity peaks in the obtained liquid chromatogram to obtain the sum of the area integrations of all impurity peaks, which is recorded as the sum of the area integrations of the first impurity peaks;

[0028] Step 2, performing liquid chromatography determination on the N-methylmorpholine-N-oxide, the determination conditions are the same as those in step 1, performing area integration on all impurity peaks in the obtained liquid chromatogram to obtain the sum of the area integrations of all impurity peaks, which is recorded as the sum of the area integrations of the second impurity peaks;

[0029] The first crystal impurity residual rate = the integrated sum of the second impurity peak areas / the integrated sum of the first impurity peak areas.

[0030] In one embodiment of the method for detecting N-methylmorpholine-N-oxide of the present invention, the determination of the residual rate of crystalline impurities of N-methylmorpholine-N-oxide further comprises the following steps:

[0031] Step 3, performing liquid chromatography determination on the crude N-methylmorpholine-N-oxide product at a wavelength of 230 nm-240 nm, performing area integration on all impurity peaks in the obtained liquid chromatogram to obtain the sum of the area integrations of all impurity peaks, which is recorded as the sum of the area integrations of the third impurity peaks;

[0032] Step 4, performing liquid chromatography determination on the N-methylmorpholine-N-oxide, the determination conditions are the same as those in step 3, performing area integration on all impurity peaks in the obtained liquid chromatogram to obtain the sum of the area integrations of all impurity peaks, which is recorded as the sum of the area integrations of the fourth impurity peaks;

[0033] The second crystal impurity residual rate = the fourth impurity peak area integral sum / the third impurity peak area integral sum.

[0034] The method for detecting N-methylmorpholine-N-oxide of the present invention, in one embodiment, further comprises determining the content of N-methylmorpholine and morpholine; the method for determining the content of N-methylmorpholine and morpholine is as follows: performing liquid chromatography determination on N-methylmorpholine-N-oxide, with a determination wavelength of 200nm-210nm and a determination time of greater than or equal to 30 minutes.

[0035] The detection method of N-methylmorpholine-N-oxide of the present invention, in one embodiment, further comprises determining the content of N-nitrosomorpholine; the method for determining the content of N-nitrosomorpholine is: performing liquid chromatography determination on N-methylmorpholine-N-oxide, the determination wavelength is 230nm-240nm, and the determination time is greater than or equal to 30 minutes.

[0036] In one embodiment, the detection method of N-methylmorpholine-N-oxide of the present invention further comprises: determining at least one of hydrogen peroxide content, electrical conductivity, iron ion content, and copper ion content; the determination of the hydrogen peroxide content is carried out in accordance with GB 5009.226-2016; and the determination of the iron ion content or the copper ion content is carried out by an inductively coupled plasma emission spectrometer.

[0037] Beneficial effects of the present invention:

[0038] The invention provides a method for purifying NMMO with high efficiency, low cost and greenness, which mainly comprises crystallizing a crude product, wherein the crystallization operation temperature can be close to room temperature (25-35° C.), and the energy consumption is low; the NMMO recovery rate is above 97%, and the purified NMMO is prepared into an NMMO aqueous solution with a mass concentration of 50%, wherein the conductivity is less than 10 μs / cm, and even reaches about 1 μs / cm, and the copper and iron ion contents are both less than 1 ppb, and HPLC cannot detect the presence of organic impurities such as N-nitrosomorpholine, for example, the HPLC detection result shows that the total impurity content does not exceed 2 ppm (that is, the NMMO purity is greater than 99.999%), and the hydrogen peroxide content is also lower than the detectable lower limit of national standard GB 5009226-2016, and the product quality reaches or exceeds the NMMO product quality standard required for Tencel production; and the NMMO purification method of the invention does not use ion exchange resin, and thoroughly solves the problem of high-salt and high-COD wastewater and waste ion exchange resin polluting the environment faced by the current purification process using ion exchange resin. BRIEF DESCRIPTION OF THE DRAWINGS

[0039] Figure 1 The figure is a schematic diagram of a purification system of N-methylmorpholine-N-oxide according to one embodiment of the present invention.

[0040] Wherein, the reference numerals are:

[0041] 1. Primary concentration device

[0042] 10N-methylmorpholine-N-oxide crude product

[0043] 11 Condensate

[0044] 12First-level concentrated liquid

[0045] 2. Primary crystallization device

[0046] 3. Primary crystallization separation device

[0047] 31 Primary Crystallization

[0048] 32 Primary crystallization mother liquor

[0049] 4 Secondary Concentration Unit

[0050] 41 Secondary Concentrate

[0051] 42 Condensate

[0052] 5. Secondary crystallization device

[0053] 6. Secondary crystallization separation device

[0054] 61 Secondary crystallization

[0055] 62 Secondary crystallization mother liquor

[0056] 7 Dissolution device

[0057] 71 Water

[0058] 72 Crystal dissolving liquid

[0059] 8 Recrystallization device

[0060] 9 Recrystallization separation device

[0061] 91 Recrystallized crystals

[0062] 92 Recrystallization mother liquor DETAILED DESCRIPTION

[0063] The following is a detailed description of the embodiments of the present invention. This embodiment is implemented on the premise of the technical solution of the present invention, and a detailed implementation process is given, but the protection scope of the present invention is not limited to the following embodiments. The experimental methods in the following embodiments that do not specify specific conditions are usually based on conventional conditions. If not otherwise specified, the content in the present invention refers to the mass content, and % refers to mass %.

[0064] The invention discloses a method for purifying N-methylmorpholine-N-oxide, which is mainly used for purifying N-methylmorpholine-N-oxide in a crude N-methylmorpholine-N-oxide product prepared by reacting N-methylmorpholine with hydrogen peroxide. The purification method does not include an ion exchange resin treatment step, and thus can overcome the problems of environmental pollution and high energy consumption caused by purification using ion exchange resins. The purification method has the characteristics of high efficiency, low energy consumption, low cost, green environmental protection, high yield, and high purity of N-methylmorpholine-N-oxide.

[0065] In one embodiment, the present invention provides a method for purifying N-methylmorpholine-N-oxide, wherein the N-methylmorpholine-N-oxide is derived from a crude N-methylmorpholine-N-oxide product prepared by reacting N-methylmorpholine with hydrogen peroxide, wherein the mass concentration of N-methylmorpholine-N-oxide in the crude N-methylmorpholine-N-oxide product is 50% to 60%, and the purification method comprises: cooling and crystallizing the crude N-methylmorpholine-N-oxide product at a temperature between -20°C and 78°C to obtain N-methylmorpholine-N-oxide crystals.

[0066] The crystallization purification method is to cool down the temperature and utilize the different solubility of each component in the mixture in the solvent so that the concentration of the substance to be crystallized and purified in the mother liquor exceeds its saturated solubility to form a supersaturated solution. The substance to be crystallized and purified forms crystals in the supersaturated solution, while the impurity components with relatively low content remain in the mother liquor, thereby achieving the effect of separation and purification. The main factors affecting the purity of the crystal are the adsorption of the mother liquor on the surface of the crystal and the inclusion of the mother liquor in the crystal. The present invention rinses the crystal with a pure N-methylmorpholine-N-oxide saturated solution to remove the mother liquor adsorbed on the surface of the crystal, and improves the inclusion of the mother liquor in the crystal by further improving the crystallization process conditions or by a recrystallization method.

[0067] In industry, since there are problems in transporting pure N-methylmorpholine-N-oxide, and downstream manufacturers using N-methylmorpholine-N-oxide usually use aqueous solution of N-methylmorpholine-N-oxide as raw material, N-methylmorpholine-N-oxide usually prepared in the art is in the form of aqueous solution.

[0068] The present invention utilizes the characteristics of N-methylmorpholine-N-oxide hydrate crystals, and controls the cooling crystallization conditions to combine N-methylmorpholine-N-oxide and water in a specific ratio to form crystals, thereby achieving the purpose of separation from impurities in the aqueous solution. In other words, the present invention obtains N-methylmorpholine-N-oxide hydrate solids through crystallization, thereby achieving the purpose of purifying N-methylmorpholine-N-oxide, and then the N-methylmorpholine-N-oxide hydrate solids are prepared into aqueous solutions of required concentrations to supply to downstream manufacturers.

[0069] In industry, the crude NMMO product prepared by the reaction of N-methylmorpholine and hydrogen peroxide is generally brownish yellow in color, and the mass concentration of NMMO in the crude reaction product is between 50% and 60% depending on the concentration of hydrogen peroxide used. The present invention does not particularly limit the reaction process of N-methylmorpholine and hydrogen peroxide, and conventional reaction conditions in the art may be used.

[0070] In one embodiment, the present invention first concentrates the crude N-methylmorpholine-N-oxide product to obtain a concentrated solution with a mass content of N-methylmorpholine-N-oxide between 56.5% and 84.5%, and then cools and crystallizes the concentrated solution, thereby improving the crystallization efficiency. In another embodiment, the concentration treatment method is evaporation, such as vacuum evaporation, reduced pressure evaporation, normal pressure evaporation, etc.

[0071] In one embodiment, the present invention concentrates the crude N-methylmorpholine-N-oxide product, and when the mass content of N-methylmorpholine-N-oxide in the obtained concentrated solution is 56.5%-72.2%, the concentrated solution is cooled and crystallized between -20-39°C, and the NMMO crystals obtained are 2NMMO·5H2O (i.e., NMMO·2.5H2O); when the mass content of N-methylmorpholine-N-oxide in the obtained concentrated solution is 72.2%-84.5% (excluding 72.2%), the concentrated solution is cooled and crystallized between 39-78°C (excluding 39°C), and the NMMO crystals obtained are NMMO·H2O. In other words, different NMMO concentrations in the concentrated solution determine different crystallization temperatures, thereby obtaining different NMMO crystals.

[0072] In one embodiment, the present invention takes into account the industrial purification cost and operational convenience, concentrates the crude N-methylmorpholine-N-oxide product to a NMMO mass concentration of 66%-71%, and the concentrated solution is cooled and crystallized at a room temperature range of 25-35° C. (the final crystallization temperature is 25° C. or above). Under the optimal crystallization conditions, a high-purity 2NMMO·5H2O crystal and a crystallization yield of more than 50% can be obtained through primary crystallization.

[0073] In one embodiment, seed crystals may be added during the crystallization process, and the amount of seed crystals added is 0.1% to 1.0% of the weight of the crude N-methylmorpholine-N-oxide product, or the amount of seed crystals added is 0.1% to 1.0% of the weight of the above-mentioned concentrated solution. In another embodiment, the amount of seed crystals added is 0.1% to 0.3% of the weight of the crude N-methylmorpholine-N-oxide product, or the amount of seed crystals added is 0.1% to 0.3% of the weight of the above-mentioned concentrated solution. In the cooling crystallization, adding seed crystals to induce crystallization can very effectively reduce the supersaturation of NMMO in the solution and obtain NMMO crystals with higher purity.

[0074] In one embodiment, the seeds added in the present invention are crushed small particles of high purity with uniform particle size as much as possible, and the particle size is, for example, 0.01-0.1 mm, and the amount of seeds added is 0.1-1.0% of the weight of the crude NMMO product. Large seed particles and too little addition will lead to reduced purity of NMMO crystals, and the final NMMO crystal particle size distribution is uneven; too many seeds will result in small crystal particles. In addition, the seeds should not be added too early, otherwise the solution temperature is too high, and the concentration of NMMO hydrate in the solution is lower than its corresponding solubility, resulting in the dissolution of crystals, and the meaning of adding seeds is lost; and the seeds are added too late, the solution temperature is too low, and the supersaturation of the solution is too high at this time, which will reduce the actual effect of adding seeds. The timing of adding seeds is generally determined by the NMMO content in the crude NMMO product or concentrate and the initial cooling temperature. In one embodiment, the seeds are added when the solution is cooled to between 30-37°C.

[0075] In one embodiment, the seed crystals of the present invention are soaked in a high-purity NMMO saturated aqueous solution for at least 1 hour before being added to the crystallization system, which can improve the crystallization effect and ensure that the crystals precipitated in the crystallization system are uniform in size.

[0076] In one embodiment, during the temperature reduction crystallization process of the present invention, from the beginning of crystallization in the crystallization system to the temperature of the crystallization system dropping to 30°C, the cooling rate is controlled at 1-2°C / hour, and after the temperature of the crystallization system is lower than 30°C (such as at -20-30°C), the cooling rate can be controlled at 3-4°C / hour. In this way, the crystal purity can be guaranteed. This is because, in the temperature reduction crystallization, the cooling rate directly determines the crystallization rate. When the crystallization system is in a higher temperature range, the solubility curve of NMMO hydrate changes greatly. Therefore, after crystallization, in the initial stage of crystallization, the cooling rate of the solution system should not be too fast, and the crystal growth rate should be limited, otherwise it will cause the solution supersaturation to be too high, affecting the crystal purity.

[0077] In one embodiment, after the cooling crystallization system reaches the crystallization termination temperature, the crystallization solution is quickly filtered through a Buchner funnel by vacuum filtration, the crystallization mother liquor is released from the filter bottle, and the crystals are washed with a crude NMMO product and a high-purity NMMO aqueous solution with a concentration of 59.5% to obtain NMMO crystals, which are weighed and analyzed for content.

[0078] The present invention can obtain NMMO crystals with very high purity by primary crystallization. The NMMO crystals obtained by the primary crystallization are added with water to prepare a 50% NMMO aqueous solution with a mass concentration of colorless and transparent and a conductivity of 4-10 μs / cm.

[0079] In order to obtain NMMO with higher purity, the cooling crystallization of the present invention includes at least two crystallizations, for example, including primary crystallization and secondary crystallization. That is, after the primary crystallization, the crystals are added with water to prepare a certain concentration of NMMO aqueous solution, and then secondary crystallization (recrystallization) is performed. In one embodiment, the cooling crystallization of the present invention also includes tertiary crystallization, quadruple crystallization, etc.

[0080] The crystals obtained by the secondary crystallization of the present invention are subjected to liquid chromatography analysis and detection, and no organic impurities such as N-nitrosomorpholine, N-methylmorpholine, morpholine, peroxide, etc. can be detected. Water is added to prepare an NMMO aqueous solution with a mass content of 50%, and the conductivity thereof is 3-6 μs / cm, and can even reach about 1 μs / cm.

[0081] In another embodiment, the crystals obtained by secondary crystallization are added with water to prepare an aqueous solution with a NMMO mass concentration of 50%, and the conductivity of the NMMO solution (NMMO mass concentration of 50%) is about 1μs / cm; using Thermo Fisher ICP-OES detection, almost no copper ions and iron ions are detected (thereby indicating that the content of copper ions and iron ions is less than 0.001ppm); according to the national standard GB 5009.226-2016, the presence of hydrogen peroxide cannot be detected. Therefore, the aqueous solution with a NMMO mass concentration of 50% prepared from the crystals obtained after the above treatment can fully meet the quality requirements of Tencel production for NMMO, and is much higher than the quality requirements of Tencel production for NMMO.

[0082] In one embodiment, in order to improve the yield of NMMO, the present invention includes at least secondary crystallization, that is, the crude product of N-methylmorpholine-N-oxide is subjected to primary crystallization to obtain crystals and crystallization mother liquor, and the crystallization mother liquor produced by the primary crystallization is evaporated by vacuum heating to a NMMO mass concentration of 69-71% or 69-70.5%, and then cooled and crystallized (secondary crystallization). The crystallization conditions are consistent with the above-mentioned primary crystallization, and the crystallization rate is about 80-85%. The obtained crystals can be cyclically dissolved in the crude NMMO product and recovered as a raw material liquid for primary crystallization to further improve the purity of the crystals. In order to further improve the yield of NMMO, the crystallization mother liquor obtained by the secondary crystallization can be further concentrated and crystallized. At this time, the amount of crystallization mother liquor obtained by the secondary crystallization is very small, generally less than 3% of the mass of the initial crude NMMO product.

[0083] In a specific embodiment, the purification method of N-methylmorpholine-N-oxide of the present invention comprises: concentrating the NMMO crude product generated by the reaction of N-methylmorpholine and hydrogen peroxide to a NMMO mass content of 56.5-84.5% by reducing pressure and heating evaporation and concentration, obtaining high-purity NMMO hydrate crystals by cooling and crystallizing, and obtaining Tencel-grade NMMO products without ion exchange resin. Wherein, the cooling and crystallizing operating temperature is -20-78°C. Considering the cost and operational suitability of industrial purification, the NMMO mass concentration in the crude product is preferably controlled at 66-71%, so that cooling and crystallizing can be performed at 25-35°C, and a high-purity crystal product and a crystallization yield of more than 50% can be obtained.

[0084] In a specific embodiment, the cooling crystallization method of the present invention is: a crude NMMO product with a NMMO mass concentration of 66.5-70% at a temperature of about 40°C is cooled to a temperature where the seed crystals will not dissolve after being added, and then a small amount of seed crystals are added. The seed crystals are preferably small-particle NMMO·2.5H2O broken crystals that are first immersed in a saturated solution of high-purity NMMO. These small-particle broken crystals are immersed in the saturated solution of NMMO for at least 1 hour. The amount of seed crystals added is 0-1% of the mass of the crude NMMO product, preferably 0.1-0.3%. After adding the seed crystals, the crude NMMO product is slowly cooled by cooling treatment. Between the crystallization temperature and 30°C, the cooling rate is controlled at 1-2°C / hour. When the temperature drops below 30°C, the cooling rate can be appropriately accelerated to 3-4°C / hour. The crystallization termination temperature is 25°C, and crystals with larger particles and uniform particle size distribution are obtained. The crystal solution was quickly filtered, and the mother liquor was collected and weighed after filtration. The crystal was first rinsed with NMMO crude product, and the amount of crude product rinsing liquid was about 30% of the mass of the obtained crystal, and then continued to be rinsed with a high-purity NMMO aqueous solution with a mass concentration of 59.5%, and the amount of rinsing liquid was about 30% of the mass of the crystal to obtain a primary crystallization crystal, and the primary crystallization crystal was collected, weighed and analyzed for crystal purity. The primary crystallization crystal was added with water to prepare an aqueous solution with a mass concentration of 50% NMMO, and the content of various impurities, hydrogen peroxide content, conductivity and metal ion content in the solution were detected.

[0085] Then a secondary crystallization is carried out. The process conditions of the secondary crystallization are similar to those of the primary crystallization. The primary crystals are dissolved in water at 40°C to prepare an aqueous solution with a NMMO mass concentration of 66-70%. The secondary crystallization is carried out under the same crystallization process conditions. The secondary crystals are collected, weighed and analyzed for crystal purity.

[0086] In a specific embodiment, the purification method of NMMO of the present invention is: the crude NMMO product prepared by the reaction of N-methylmorpholine and hydrogen peroxide is concentrated to a NMMO mass concentration of 56.5-84.5% by vacuum heating, and high-purity NMMO hydrate crystals are obtained by cooling and crystallizing, and the crystals are added with water to prepare an aqueous solution with a NMMO mass concentration of 50%, and the conductivity is even about 1μs / cm, the copper and iron ions are less than 0.001ppm, and the high-purity NMMO aqueous solution product with a mass concentration of 50%. The remaining crystallization mother liquor is subjected to secondary or more crystallizations, and the NMMO therein can be recovered to the maximum extent. The secondary crystallization of the crystallization mother liquor can recover more than 97% of the NMMO in the crude NMMO product, and more levels of crystallization will further improve the recovery rate of NMMO.

[0087] Therefore, the present invention provides a method for purifying and preparing NMMO that meets the quality requirements of Lyocell production from the crude product of oxidized methylmorpholine (NMMO) reaction by a crystallization method. Different from the existing NMMO purification method, the present invention does not use ion exchange resin to remove metal ions and non-metal ions and some organic impurities including pigments, and there is no large amount of high-salt and high-COD wastewater generated during the regeneration of ion exchange resins and waste ion exchange resin hazardous wastes and other substances that pollute the environment; the NMMO aqueous solution product produced by the method of the present invention can not only meet or even exceed the current quality requirements of the Lyocell industry for NMMO products, but also has a simple purification process, low purification cost, and high NMMO yield. The present invention is an efficient, simple, low-cost, green purification method for NMMO.

[0088] In one embodiment, the present invention further provides a purification system for N-methylmorpholine-N-oxide, which is used for purifying N-methylmorpholine-N-oxide in a crude N-methylmorpholine-N-oxide product prepared by reacting N-methylmorpholine with hydrogen peroxide. The purification system can be used for the purification of N-methylmorpholine-N-oxide in industrial production, that is, large-scale automated control can be achieved. The purification system comprises:

[0089] A crystallization device, used for crystallization treatment of crude N-methylmorpholine-N-oxide product;

[0090] A control device is connected to the crystallization device to control the crystallization conditions in the crystallization device.

[0091] In another embodiment, the purification system further comprises a concentrating device connected to the crystallization device and the control device, so that the crude N-methylmorpholine-N-oxide product is concentrated in the concentrating device and then input into the crystallization device; the control device controls the concentrating conditions of the concentrating device.

[0092] In one embodiment, the purification system of N-methylmorpholine-N-oxide of the present invention is as follows Figure 1 As shown, the primary concentration device 1 is connected to the primary crystallization device 2, and the crude N-methylmorpholine-N-oxide product 10 is introduced into the primary concentration device 1 for concentration treatment. The primary concentration device 1 is, for example, an evaporation device. The condensate 11 flows out from the top of the primary concentration device 1, and the obtained primary concentrated liquid 12 is introduced into the primary crystallization device 2 for crystallization treatment. The crystallization conditions have been described in detail above and will not be repeated here.

[0093] The primary crystallization device 2 is connected to the primary crystallization separation device 3. The mixture obtained after crystallization in the primary crystallization device 2 is passed into the primary crystallization separation device 3 for solid-liquid separation to obtain primary crystals 31 and primary crystallization mother liquor 32.

[0094] In another embodiment, the primary crystallization separation device 3 is connected to the secondary concentration device 4, so that the primary crystallization mother liquor 32 is passed into the secondary concentration device 4 for concentration treatment to obtain a secondary concentrated liquid 41 and a condensate 42; the secondary concentration device 4 is connected to the secondary crystallization device 5, and the secondary concentrated liquid 41 is passed into the secondary crystallization device 5 for secondary crystallization treatment. In this way, the yield of NMMO can be improved.

[0095] The secondary crystallization device 5 is connected to the secondary crystallization separation device 6, and the mixture obtained after crystallization in the secondary crystallization device 5 is passed into the secondary crystallization separation device 6 for solid-liquid separation to obtain secondary crystallization crystals 61 and secondary crystallization mother liquor 62. In one embodiment, the secondary crystallization separation device 6 is also connected to the secondary concentration device 4, so that the secondary crystallization mother liquor 62 can be circulated back to the secondary concentration device 4 for concentration treatment, and then participate in the crystallization process again to further improve the yield of NMMO. In view of the small amount of NMMO contained in the secondary crystallization mother liquor 62, the secondary crystallization mother liquor 62 can also be directly discharged for treatment.

[0096] In one embodiment, the purification system of N-methylmorpholine-N-oxide of the present invention also includes a dissolution device 7, which is connected to the primary crystallization separation device 3 and the secondary crystallization separation device 6 respectively, so as to transport the primary crystallization crystals 31 and the secondary crystallization crystals 61 to the dissolution device 7, mix with the input water 71, and obtain a crystal dissolving liquid 72.

[0097] The dissolving device 7 is connected to the recrystallization device 8, and the recrystallization device 8 is also connected to the recrystallization separation device 9. The crystal dissolving liquid 72 is transported to the recrystallization device 8 for recrystallization treatment, so that the purity of NMMO can be further improved. The mixture obtained after crystallization in the recrystallization device 8 is transported to the recrystallization separation device 9 to obtain recrystallized crystals 91 and recrystallization mother liquor 92. The recrystallized crystals 91 are subjected to liquid chromatography analysis and detection, and the results show that various organic impurities such as N-nitrosomorpholine, N-methylmorpholine, morpholine, peroxide, etc. present in the NMMO crude product can no longer be detected. The recrystallized crystals 91 are added with water to prepare a 50% NMMO aqueous solution by mass, and its conductivity is 3-6μs / cm.

[0098] In one embodiment, the recrystallization separation device 9 is also connected to the primary crystallization separation device 3 and the secondary crystallization separation device 6 respectively, so as to use the recrystallization mother liquor 92 for washing the primary crystallization crystals 31 and the secondary crystallization crystals 61, reduce the mother liquor adsorbed on the surface of the primary crystallization crystals 31 and the secondary crystallization crystals 61, and further remove impurities contained in the primary crystallization crystals 31 and the secondary crystallization crystals 61.

[0099] In one embodiment, the purification system of N-methylmorpholine-N-oxide of the present invention is used for industrial production, and the purification system also includes a control device (not shown), which is electrically connected to one or more of the primary concentration device 1, the primary crystallization device 2, the primary crystallization separation device 3, the secondary concentration device 4, the secondary crystallization device 5, the secondary crystallization separation device 6, the melting device 7, the recrystallization device 8, and the recrystallization separation device 9 to control the process parameters of the crystallization process.

[0100] In one embodiment, the present invention provides a method for detecting N-methylmorpholine-N-oxide, wherein the N-methylmorpholine-N-oxide is obtained by crystallizing a crude N-methylmorpholine-N-oxide product prepared by reacting N-methylmorpholine with hydrogen peroxide, and the detection method comprises determining the residual rate of crystalline impurities of the N-methylmorpholine-N-oxide, and the determination of the residual rate of crystalline impurities of the N-methylmorpholine-N-oxide comprises the following steps:

[0101] Step 1, performing liquid chromatography determination on the crude N-methylmorpholine-N-oxide product, with a measurement wavelength of 200 nm-220 nm, for example, 200 nm-210 nm, performing area integration on all impurity peaks in the obtained liquid chromatogram to obtain the sum of the area integrations of all impurity peaks, which is recorded as the sum of the area integrations of the first impurity peaks;

[0102] Step 2, performing liquid chromatography determination on the N-methylmorpholine-N-oxide, the determination conditions are the same as those in step 1, performing area integration on all impurity peaks in the obtained liquid chromatogram to obtain the sum of the area integrations of all impurity peaks, which is recorded as the sum of the area integrations of the second impurity peaks;

[0103] The first crystal impurity residual rate = the integrated sum of the second impurity peak areas / the integrated sum of the first impurity peak areas.

[0104] In one embodiment, the determination of the residual rate of crystalline impurities of N-methylmorpholine-N-oxide further comprises the following steps:

[0105] Step 3, performing liquid chromatography determination on the crude N-methylmorpholine-N-oxide product at a wavelength of 230 nm-240 nm, performing area integration on all impurity peaks in the obtained liquid chromatogram to obtain the sum of the area integrations of all impurity peaks, which is recorded as the sum of the area integrations of the third impurity peaks;

[0106] Step 4, performing liquid chromatography determination on the N-methylmorpholine-N-oxide, the determination conditions are the same as those in step 3, performing area integration on all impurity peaks in the obtained liquid chromatogram to obtain the sum of the area integrations of all impurity peaks, which is recorded as the sum of the area integrations of the fourth impurity peaks;

[0107] The second crystal impurity residual rate = the fourth impurity peak area integral sum / the third impurity peak area integral sum.

[0108] In this way, the present invention can detect the impurity residual rate of the obtained crystal from different aspects by measuring the first crystal impurity residual rate and the second crystal impurity residual rate.

[0109] In one embodiment, the detection method of N-methylmorpholine-N-oxide of the present invention further comprises the determination of N-methylmorpholine and morpholine content, the determination of N-nitrosomorpholine content, the determination of at least one of hydrogen peroxide content, electrical conductivity, iron ion content, and copper ion content.

[0110] Wherein, the method for determining the content of N-methylmorpholine and morpholine is: liquid chromatography is performed on N-methylmorpholine-N-oxide, the measurement wavelength is 200nm-210nm, and the measurement time is greater than or equal to 30 minutes. The method for determining the content of N-nitrosomorpholine is: liquid chromatography is performed on N-methylmorpholine-N-oxide, the measurement wavelength is 230nm-240nm, and the measurement time is greater than or equal to 30 minutes. In this way, the content of N-methylmorpholine and morpholine can be obtained according to the obtained liquid chromatography spectrum. The determination of hydrogen peroxide content is carried out in accordance with GB 5009.226-2016; the determination of iron ion content or copper ion content is carried out by inductively coupled plasma emission spectrometry. The conductivity determination can be carried out according to conventional methods in the art, and the present invention is not particularly limited.

[0111] In a specific embodiment, the method for detecting N-methylmorpholine and morpholine content is: liquid chromatography, chromatographic column: AichromBond-1, C18, 5μm 4.6x150mm; mobile phase: 0.2% phosphate buffer; mobile phase flow rate: 1ml / min; column temperature: 35°C; UV detection wavelength: 200nm; injection volume: 20μl, detection time: 30 minutes.

[0112] N-nitrosomorpholine content detection method: liquid chromatography, chromatographic column: AichromBond-1, C18, 5μm4.6x150mm; mobile phase: 0.2% phosphate buffer; mobile phase flow rate: 1ml / min; column temperature: 35℃; UV detection wavelength: 235nm; injection volume: 20μl, detection time: 30 minutes.

[0113] The present invention utilizes the residual impurity rate to indicate the purity of the obtained NMMO crystals. In a specific embodiment, the residual impurity rate detection method is as follows: water is added to the NMMO crude product and the crystals respectively to prepare an aqueous solution with a NMMO mass concentration of 50%, and the prepared NMMO aqueous solution is measured by liquid chromatography, and the UV detection wavelengths are 200nm, 220nm and 235nm respectively (measured at three wavelengths).

[0114] The present invention uses the above detection method to measure the crude NMMO product prepared by the reaction of N-methylmorpholine and hydrogen peroxide used in the following examples, and the results are as follows:

[0115] N-methylmorpholine content: 1130ppm;

[0116] Morpholine content: 133ppm;

[0117] Hydrogen peroxide content: 634ppm;

[0118] N-nitrosomorpholine: 655ppb,

[0119] Conductivity: 732μs / cm;

[0120] Iron ion content: 11.8ppm;

[0121] Copper ion content: 4.2ppm;

[0122] In addition, liquid chromatography analysis showed that the crude NMMO product also contained other organic impurities including a large amount of organic peroxides.

[0123] The technical solution of the present invention is further described below through specific embodiments.

[0124] Example 1

[0125] This example mainly analyzes the influence of different crystallization rates of NMMO on the crystal purity of NMMO.

[0126] The crude NMMO product was evaporated by heating under vacuum and concentrated to NMMO mass concentrations of 63.5%, 65.2%, 66.5%, 67.9% and 69.2%, respectively, and then cooled and crystallized, and the NMMO crude product concentrates of various concentrations began to cool at 37°C, and the temperatures of the solutions with NMMO mass concentrations of 63.5%, 65.2%, 66.5%, 67.9% and 69.2% were respectively reduced to 31.2°C, 32.1°C, 33.2°C, 34.2°C and 35.1°C, and seed crystals pre-soaked in NMMO saturated solution were added in an amount of the crude NMMO product. The amount of 0.15% is added, and after the seed crystal is added, the cooling rate is controlled at 1-2°C / hour until the solution temperature drops to 30°C, and then the cooling rate is accelerated to 3-4°C / hour, the solution temperature drops to 25°C, the crystallization is stopped, and the mother liquor is quickly filtered to separate the mother liquor from the crystals. The mother liquor is collected, and the crystals are first rinsed with a crude product with an NMMO mass concentration of 58.2%, and the rinse volume is about 30% of the crystal mass, and then rinsed with a high-purity NMMO mass concentration of 59% aqueous solution, and the rinse volume is about 30% of the crystal mass. The crystals are collected, weighed to calculate the crystallization rate, and the crystal purity (impurity residual rate) is analyzed and detected.

[0127] Water was added to the crude NMMO product and the obtained crystals to prepare an aqueous solution with a NMMO mass concentration of 50%, and then analyzed and tested. The test results are shown in Table 1.

[0128] Table 1. Effect of different crystallization rates on crystal purity

[0129]

[0130] As shown in Table 1, crystallization can effectively remove various impurities in the crude NMMO product, and the impurity content and conductivity of the obtained crystals are greatly reduced. When the crystallization rate is less than or equal to 65%, the purity of the NMMO crystals remains basically unchanged as the crystallization rate increases, but when the crystallization rate is greater than 65%, the crystal purity decreases slightly as the crystallization rate increases.

[0131] Example 2

[0132] This example mainly analyzes the effect of different crystallization rates on the purity of NMMO crystals. The crude NMMO product is evaporated by vacuum heating and concentrated to a NMMO mass concentration of 67.9%. When the temperature of the crude NMMO product drops to 34.2°C, NMMO seeds pre-soaked in a saturated NMMO solution are added. The amount of seeds added is 0.15% of the mass of the crude NMMO product. The crude NMMO product is divided into 4 parts and crystallized at the following different cooling rates. The crystallization solution is cooled to 25°C, filtered while hot, and the crystals are treated as in Example 1.

[0133] Cooling rate:

[0134] Cooling rate 1: 34.2℃ to 30℃, the cooling rate is controlled at 1℃ / hour, 30-25℃, the cooling rate is controlled at 4℃ / hour.

[0135] Cooling rate 2: 34.2℃ to 30℃, the cooling rate is controlled at 2℃ / hour, 30-25℃, the cooling rate is controlled at 4℃ / hour.

[0136] Cooling rate 3: 34.2℃ to 30℃, the cooling rate is controlled at 2℃ / hour, 30-25℃, the cooling rate is controlled at 2℃ / hour.

[0137] Cooling rate 4: 34.2℃ to 30℃, the cooling rate is controlled at 4℃ / hour, 30-25℃, the cooling rate is controlled at 4℃ / hour.

[0138] The NMMO crystals were added with water to prepare an NMMO aqueous solution with a mass concentration of 50%, and then analyzed and tested. The test results are shown in Table 2.

[0139] Table 2. Effect of different cooling rates on the purity of NMMO crystals

[0140]

[0141] As shown in Table 2, in the initial crystallization stage (from the crystallization temperature to 30°C), the cooling rate should not be too fast, and it is better to control it at 1-2 / hour, otherwise the crystal purity will decrease significantly; in the later stage of cooling crystallization, the cooling rate can be appropriately accelerated. The main reason for the analysis is that the solubility of NMMO crystals changes greatly with temperature in the high temperature zone, so too fast cooling will lead to too high supersaturation of the solution, so that the crystal contains more mother liquor, reducing the crystal purity; in the later stage of crystallization, the crystallization temperature is low, and the trend of NMMO crystal solubility changing with temperature slows down, so the cooling rate can be appropriately accelerated.

[0142] Example 3

[0143] This example mainly analyzes the effect of the amount of seed added on the crystal particle size and crystal purity. The crude NMMO product was evaporated by vacuum heating and concentrated to a NMMO mass concentration of 67.9%. The concentrated crude NMMO product was divided into 6 parts. When the temperature of the crude NMMO product dropped to 34.2°C, NMMO seeds pre-soaked in a saturated NMMO solution were added respectively. The amount of seed added was: 0 (no seed), 0.05%, 0.1%, 0.2%, 0.3% and 0.6% (percentage of the mass of the crude NMMO product), and then crystallized and treated in the manner of Example 1.

[0144] The NMMO crystals were added with water to prepare an aqueous solution with a NMMO mass concentration of 50%, and then tested and analyzed. The analysis results are shown in Table 3.

[0145] Table 3. Effect of different seed addition amounts on crystal purity and particle size

[0146]

[0147]

[0148] As shown in Table 3, not adding seed crystals has a great influence on the crystallization process. When the temperature drops to 25°C, there is still no obvious crystal formation. When the amount of seed crystals added is too little (0.05%), the grain size distribution is uneven, indicating that the amount of seed crystals added is small, the solution system is highly supersaturated, and small crystal nuclei are spontaneously precipitated, and the purity of the obtained crystals is also slightly low. When the amount of seed crystals added is increased, the distribution of crystal particles becomes uniform, the purity of the crystals is improved, and the larger the amount of seed crystals added, the smaller the particles. When too many seed crystals are added (0.6%), the resulting crystal particles are too small, and the particle surface may be contaminated with more mother liquor impurities, resulting in a decrease in crystal purity. At the same time, the crystal particle size is too small, which will also affect the crystal filtration speed. The optimal crystal addition amount is 0.1-0.3% of the mass of the NMMO crude product.

[0149] Example 4.

[0150] This example mainly analyzes the influence of two crystallizations on the purity of NMMO crystals.

[0151] The crude NMMO reaction product was evaporated by heating in vacuum and concentrated to a NMMO mass concentration of 69.2%. At 35.1°C, seed crystals pre-soaked in a saturated NMMO solution were added in an amount of 0.15% of the mass of the crude NMMO product. After the seed crystals were added, the cooling rate was controlled at 1-2°C / hour until the temperature dropped to 30°C, and then the cooling rate was accelerated to 4°C / hour, the temperature dropped to 25°C, the crystallization was stopped, and the mother liquor was quickly filtered while hot to separate the mother liquor from the crystals. The mother liquor was collected as a raw material for the crystallization experiment in Example 5. The crystals were first rinsed with a crude NMMO product having a mass concentration of 60%, and the rinsing amount was approximately 30% of the mass of the crystals, and then rinsed with a high-purity NMMO aqueous solution having a mass concentration of 59.5%, and the rinsing amount was approximately 30% of the mass of the crystals. The crystals (primary crystallization) were weighed to calculate the crystallization rate, and the crystal purity (impurity residual rate) was analyzed and detected.

[0152] The crystals obtained by the above primary crystallization were added with water to prepare a NMMO aqueous solution with a mass concentration of 68.1%, and secondary crystallization was carried out according to the above crystallization process. Seed crystals were added at 34.3°C, and the obtained crystals were washed with a high-purity NMMO aqueous solution with a mass concentration of 59.5% in an amount of 30% of the crystal mass. The crystals (secondary crystallization) were collected, weighed, and the crystallization rate was calculated, and the crystal purity (impurity residual rate) was analyzed and detected.

[0153] Water was added to the NMMO crystals obtained from the primary and secondary crystallizations to prepare aqueous solutions with a NMMO mass concentration of 50%, which were then analyzed and tested. The test results are shown in Table 4.

[0154] Table 4. Effect of two crystallization treatments on crystal purity

[0155]

[0156] Note: The above “cannot be detected”, “not detected” or “no obvious impurity peak” means that the content of the above-mentioned substance to be detected is lower than the minimum detectable value of the instrument.

[0157] As shown in Table 4, secondary crystallization can further purify NMMO, and the contents of various organic impurities are further significantly reduced. The conductivity of a 50% aqueous solution prepared by adding water to NMMO crystals is reduced to 0.9 μs / cm, the copper and iron ions are both less than 1 ppb, and the pH value is 11.4.

[0158] Since the impurity content in the crude NMMO product used for crystallization is less than 1%, the results in Table 4 show that the crystals obtained by the two crystallizations are tested by HPLC, and the impurity content therein is 0.02% of the impurity content in the crude NMMO product (UV detection wavelength: 200nm, 220nm and 235nm), so the total impurity content in the crystals obtained by the two crystallizations does not exceed 2ppm.

[0159] Example 5.

[0160] This example mainly analyzes the mother liquor remaining from the first crystallization and the results of recovering NMMO through multi-stage crystallization. The mother liquor separated from the first crystallization of Example 4 was concentrated by evaporation under reduced pressure and heating to a NMMO mass concentration of 70.1%, and crystallization was carried out according to the crystallization process conditions in Example 4 (adding seed crystals when the mother liquor temperature was 35.2°C), and the obtained crystals were added with water to prepare an aqueous solution with a NMMO mass concentration of 50%, and then analyzed and tested. The test results are shown in Table 5.

[0161] Table 5. Results of re-crystallization of the mother liquor of the first crystallization

[0162]

[0163] As shown in Table 5, the mother liquor of the first crystallization is concentrated again and then crystallized. When the crystallization rate reaches 84%, the purity of the obtained crystals is still very high. The secondary crystallization is equivalent to recovering 96% of the mass of NMMO in the crude NMMO product as NMMO crystals. If it is desired to further improve the NNMO crystallization yield, the mother liquor of the second crystallization can be concentrated and crystallized again, or the total crystallization rate of the second crystallization can be further improved. The crystals obtained by the multi-stage crystallization of the mother liquor can be returned and dissolved in the crude NMMO product as the raw material for the first crystallization.

[0164] In summary, the present invention provides a method for preparing a high-purity NMMO aqueous solution by efficient, low-cost and green purification, including cooling crystallization treatment, the crystallization operation temperature is close to room temperature (25-35° C.), the NMMO reaction crude product is purified by the purification method of the present invention, and the NMMO recovery rate is above 96%; the conductivity of the obtained NMMO aqueous solution with a mass concentration of 50% is about 1 μs / cm, the copper and iron ion contents are both less than 1 ppb, and the HPLC test results show that the total content of organic impurities does not exceed 2 ppm (that is, the NMMO purity is greater than 99.999%), HPLC can hardly detect the presence of N-nitrosomorpholine, and the hydrogen peroxide content is also lower than the detectable lower limit of the national standard GB 5009226-2016, and the product quality reaches or exceeds the NMMO product quality standard required for Tencel production. At the same time, the NMMO purification method of the present invention does not use ion exchange resin, so it completely solves the environmental protection problems such as high-salt and high-COD wastewater and waste ion exchange resin faced by the current purification process using ion exchange resin.

[0165] The NMMO purification method provided by the present invention is also applicable to other fields involving the use and need for purification of NMMO, such as the coagulation bath NMMO purification process in lyocell production, the semiconductor chip NMMO etchant waste liquid, and the NMMO electronic cleaning liquid waste liquid recovery and purification process.

[0166] Of course, the present invention may have many other embodiments. Without departing from the spirit and essence of the present invention, technicians familiar with the field may make various corresponding changes and deformations based on the present invention, but these corresponding changes and deformations should all fall within the scope of protection of the claims of the present invention.

Claims

1. A method for purifying N-methylmorpholine-N-oxide, for a mixture containing N-methylmorpholine-N-oxide, the method comprising: The mixture is cooled and crystallized at a temperature between -20°C and 78°C to obtain N-methylmorpholine-N-oxide crystals.

2. The method for purifying N-methylmorpholine-N-oxide according to claim 1, characterized in that: The mixture is a crude N-methylmorpholine-N-oxide product prepared by reacting N-methylmorpholine with hydrogen peroxide. The mass concentration of N-methylmorpholine-N-oxide in the crude N-methylmorpholine-N-oxide product is 50% to 60%.

3. The method for purifying N-methylmorpholine-N-oxide according to claim 2, characterized in that: The purification method also includes concentrating the crude N-methylmorpholine-N-oxide product to make the mass concentration of N-methylmorpholine-N-oxide in the crude N-methylmorpholine-N-oxide product be 56.5% to 84.5%, and then cooling and crystallizing.

4. The method for purifying N-methylmorpholine-N-oxide according to claim 2, characterized in that: During the cooling crystallization process, seed crystals are added, and the amount of the seed crystals added is 0.1% to 1.0% of the weight of the crude N-methylmorpholine-N-oxide product.

5. The method for purifying N-methylmorpholine-N-oxide according to claim 3, characterized in that: After concentration treatment, when the mass concentration of N-methylmorpholine-N-oxide in the crude N-methylmorpholine-N-oxide product is 56.5% to 72.2%, the temperature of the cooling crystallization is -20 to 39°C; after concentration treatment, when the mass concentration of N-methylmorpholine-N-oxide in the crude N-methylmorpholine-N-oxide product is greater than 72.2% and less than or equal to 84.5%, the temperature of the cooling crystallization is greater than 39°C and less than or equal to 78°C.

6. The method for purifying N-methylmorpholine-N-oxide according to claim 5, characterized in that: After concentration, the mass concentration of N-methylmorpholine-N-oxide in the crude N-methylmorpholine-N-oxide product is 66% to 71%, and the temperature of the cooling crystallization is 25° C. to 35° C.

7. The method for purifying N-methylmorpholine-N-oxide according to claim 1, characterized in that: During the cooling crystallization process, from the beginning of the appearance of crystals to 30°C, the cooling rate is 1-2°C / hour; between -20°C and 30°C, the cooling rate is 3-4°C / hour.

8. The method for purifying N-methylmorpholine-N-oxide according to claim 1, characterized in that: The cooling crystallization includes at least primary cooling crystallization and secondary cooling crystallization. The primary cooling crystallization obtains N-methylmorpholine-N-oxide crystals and a crystallization mother liquor. The crystallization mother liquor is concentrated and then subjected to secondary cooling crystallization.

9. N-methylmorpholine-N-oxide obtained by the method for purifying N-methylmorpholine-N-oxide according to any one of claims 1 to 8, characterized in that: The liquid chromatography detection result of the obtained N-methylmorpholine-N-oxide shows that the organic impurity content is 0; the obtained N-methylmorpholine-N-oxide is prepared into an aqueous solution with a mass concentration of 50%, the conductivity of the aqueous solution is 0-10 μs / cm, and the hydrogen peroxide content is 0.

10. Use of the N-methylmorpholine-N-oxide according to claim 9 in cellulose.

11. A method for preparing N-methylmorpholine-N-oxide, comprising the following steps: Step 1, reacting N-methylmorpholine with hydrogen peroxide to obtain a crude product of N-methylmorpholine-N-oxide; Step 2: crystallize the crude N-methylmorpholine-N-oxide product by cooling at -20°C to 78°C to obtain N-methylmorpholine-N-oxide crystals.

12. A purification system for N-methylmorpholine-N-oxide, characterized in that: The purification system is used for purifying N-methylmorpholine-N-oxide in a mixture containing N-methylmorpholine-N-oxide, and the purification system comprises: A crystallization device, used for crystallization of the mixture; A control device is connected to the crystallization device to control the crystallization conditions in the crystallization device.

13. The purification system of N-methylmorpholine-N-oxide according to claim 12, characterized in that: The purification system further comprises a concentrating device connected to the crystallizing device and the control device, so that the mixture is concentrated in the concentrating device and then input into the crystallizing device; The control device controls the concentration conditions of the concentration device.

14. The purification system of N-methylmorpholine-N-oxide according to claim 12, characterized in that: The mixture is a crude N-methylmorpholine-N-oxide product prepared by reacting N-methylmorpholine with hydrogen peroxide; the purification system is used for purifying N-methylmorpholine-N-oxide in industrial production.