Industrial paraffin-based firework and cracker bottom sealing and sealing general material and process
By using the back cover sealing material prepared by quartz sand and high-temperature paraffin, the problems of low versatility and long curing time caused by the difference between the back cover and the sealing material in the production of fireworks and firecrackers are solved, and an efficient, safe and environmentally friendly production process is achieved, ensuring the product Quality and productivity.
Patent Information
- Application Number
- CN202411146295.3
- Authority / Receiving Office
- CN · China
- Patent Type
- Applications(China)
- Current Assignee / Owner
- Filing Date
- 2024-08-20
- Publication Date
- 2024-11-15
AI Technical Summary
The difference between the bottom seal and the sealing materials in the existing fireworks and firecrackers leads to low versatility of the machine, cumbersome production links, long curing time of the sealing materials, and problems such as moisture absorption, moisture recovery, and clumping, which reduces product quality and production efficiency.
Using a general material for back sealing and sealing based on industrial paraffin, a combination of quartz sand and high-temperature paraffin is used to prepare materials with high melting point, non-flammability and good bonding, shorten the curing time, and prepare by mixing liquid paraffin and quartz sand. Ensure the stability and adaptability of the material.
It improves the production efficiency of fireworks and firecrackers, ensures product quality, does not regain and absorbs moisture, avoids lead damage, simplifies the production process, reduces costs, and improves processability and safety.
Smart Images

Figure CN118956345A_ABST
Abstract
Description
Technical Field
[0001] The invention relates to the technical field of fireworks and firecrackers production and processing, and in particular to a general material and process for sealing the bottom and mouth of fireworks and firecrackers based on industrial paraffin. Background Art
[0002] Fireworks are often used in festivals and performances. The production process generally includes tube making, bottom sealing, charge loading, lead loading, sealing, packaging, etc. At present, the bottom sealing process generally uses a machine to press and dry the viscous yellow mud, while the sealing process mostly uses manual or machine mixing of dry powder that can react with water or glue to solidify and inject it into the tube mouth, and then air-dry until the sealing material solidifies.
[0003] The difference between the above-mentioned bottom seal and sealing materials reduces the versatility of the machine, limits the production capacity of the machine, and the production process is relatively cumbersome. In addition, the above-mentioned sealing materials require a long curing time, usually more than 10 hours, which prolongs the production cycle and reduces production efficiency. There are also defects such as moisture absorption, moisture resorption, and agglomeration, which lead to loose seals and damaged leads, reducing the quality of fireworks and firecrackers. After sealing, due to the need for airing, a certain transfer site is occupied, which increases the production cost; the bottom seal and sealing materials will generate a lot of smoke and dust during the preparation process, which will cause certain harm to operators and the environment.
[0004] In order to solve the above problems that occur in the production process of fireworks and firecrackers, a general bottom sealing material and process for fireworks and firecrackers that does not affect performance, has a short curing time, and is easy to produce and store is needed. Summary of the invention
[0005] In order to solve the above-mentioned technical problems, the present invention provides a general material and process for the bottom sealing of fireworks and firecrackers. The quartz sand used in the present invention is widely available and inexpensive, which can ensure the sufficient supply of materials. Its high melting point and non-flammability ensure the safety of the filling material for the bottom sealing of fireworks and firecrackers. The industrial paraffin used is easy to store and transport. Its low melting point and good plasticity and curing properties improve the adaptability to the tube mouths of fireworks and firecrackers of different shapes and materials, shorten the curing time, and its characteristics of no moisture regain and moisture absorption will not cause damage to the fuse, thus ensuring product quality. The strong wettability of liquid industrial paraffin to dry objects ensures its bonding stability with quartz sand particles, so that the bottom sealing material has a certain strength. In order to achieve the above-mentioned purpose, the present invention adopts the following technical scheme:
[0006] A general material for sealing the bottom and mouth of fireworks and firecrackers based on industrial paraffin is made from the following raw materials in parts by weight: 60 to 80 parts of quartz sand and 20 to 40 parts of industrial paraffin.
[0007] Furthermore, the universal material for sealing the bottom and mouth of fireworks and firecrackers based on industrial paraffin is made of the following raw materials in parts by weight: 65 to 75 parts of quartz sand and 25 to 35 parts of industrial paraffin.
[0008] Furthermore, the universal material for sealing the bottom and mouth of fireworks and firecrackers based on industrial paraffin is made of the following raw materials in parts by weight: 70 parts of quartz sand and 30 parts of industrial paraffin.
[0009] Furthermore, the quartz sand has a particle size of 0.5-32, and the specific required particle size depends on the inner diameter of the barrel. The particle size is proportional to the inner diameter of the barrel. It does not need to remove impurities, but needs to be dried.
[0010] Furthermore, the industrial paraffin is high-temperature paraffin with a melting point above 60°C and no purity requirement.
[0011] Furthermore, a preparation method of a general material for sealing the bottom and mouth of fireworks and firecrackers based on industrial paraffin comprises the following steps: (1) Dry the quartz sand particles with a particle size of 0.5-32 and preheat them to 50-70°C for use; (2) Place the solid industrial paraffin in a heating tank and heat it evenly to above 70°C using a heating element to completely melt the solid paraffin into a liquid state; (3) Add the quartz sand particles of step (1) into the heating tank containing liquid paraffin in step (2), and evenly mix the paraffin and the quartz sand particles at a temperature of 60-75° C. and stir for 5-10 minutes to obtain the bottom and mouth sealing universal material.
[0012] The present invention also discloses a fireworks and firecrackers bottom sealing and mouth sealing process based on industrial paraffin wax, and the bottom sealing and mouth sealing operation of fireworks and firecrackers is completed, comprising the following steps: (1) pouring a section of the general fireworks and firecrackers bottom and mouth sealing material based on industrial paraffin at one end of the barrel and curing it for 1 to 2 hours to complete the bottom sealing process; (2) loading pyrotechnic powder into the end of the bottom and top sealing universal material near the solidified bottom and top sealing universal material in the above step (1), thereby completing the charging process; (3) Add the pyrotechnic powder in step (2) and insert the fuse at the end away from the bottom cover in step (1). The fuse should be able to extend into the pyrotechnic powder for a certain length, thus completing the insertion and fuse process; (4) Evenly lay a layer of paper or fine sand with a particle size of 0.5-1.5 or other powdery or granular solid with stable properties as a barrier layer at the junction of the fuse and the pyrotechnic powder in the above step (3) to prevent the pyrotechnic powder from directly contacting the liquid paraffin in the universal material for the bottom and mouth sealing in step (5); (5) Pour a predetermined amount of general bottom and top sealing material into one end of the barrier layer laid in step (4) and cure it for 2 to 3 hours to complete the sealing process.
[0013] Since the present invention adopts the above technical solution, it has the following beneficial effects: (1) The universal material for sealing the bottom and mouth of fireworks and firecrackers of the present invention has simple components, light weight, short curing time, high adaptability to the material and shape of the barrel, and greatly improves the production efficiency of fireworks and firecrackers; (2) It does not absorb moisture, is not easy to loosen, and will not damage the lead wire, thus ensuring product quality; (3) It is easy to prepare, convenient to store, safe and environmentally friendly, low cost, strong processability, harmless to the health of production personnel during the operation process, not easy to splash and injure people after being ignited, no pollution to the environment, and has a certain degree of recyclability. BRIEF DESCRIPTION OF THE DRAWINGS
[0014] In order to more clearly illustrate the technical solutions in the embodiments of the present application, the drawings required for use in the description of the embodiments will be briefly introduced below. Obviously, the drawings described below are only some embodiments of the present application. For ordinary technicians in this field, other drawings can be obtained based on these drawings without creative work.
[0015] In order to more clearly illustrate the technical solutions in the embodiments of the present application, the drawings required for use in the description of the embodiments will be briefly introduced below. Obviously, the drawings described below are only some embodiments of the present application. For ordinary technicians in this field, other drawings can be obtained based on these drawings without creative work.
[0016] FIG1 is a schematic diagram of the cross-sectional structure of fireworks and firecrackers according to the fireworks and firecrackers bottom sealing and opening sealing process based on industrial paraffin wax of the present invention;
[0017] FIG2 is a schematic flow diagram of a fireworks and firecracker bottom sealing process based on industrial paraffin according to the present invention;
[0018] Description of reference numerals: 1. barrel; 2. bottom sealing material; 3. pyrotechnic powder; 4. barrier layer; 5. fuse DETAILED DESCRIPTION
[0019] In order to make the purpose, technical solution and advantages of the embodiments of the present application clearer, the technical solution in the embodiments of the present application will be clearly and completely described below in conjunction with the drawings in the embodiments of the present application. Obviously, the described embodiments are part of the embodiments of the present application, not all of the embodiments. Based on the embodiments in the present application, all other embodiments obtained by ordinary technicians in this field without making creative work are within the scope of protection of this application.
[0020] In the description of the present invention, it is necessary to understand that the orientations or positional relationships indicated by terms such as “upper”, “lower”, “front”, “back”, “left”, “right”, “top”, “bottom”, “inside”, “outside”, and “one end” are based on the orientations or positional relationships shown in the accompanying drawings and are only for the convenience of describing the present invention and simplifying the description. They do not indicate or imply that the device or material referred to must have a specific orientation, be constructed and operated in a specific orientation, and therefore should not be understood as a limitation on the present invention.
[0021] Example 1
[0022] This example provides a universal material for the bottom and mouth sealing of fireworks and firecrackers based on industrial paraffin, which is made of the following raw materials in parts by weight: 80 parts of quartz sand and 20 parts of industrial paraffin.
[0023] Furthermore, the quartz sand has a particle size of 1, does not need to be cleaned of impurities, and needs to be dried.
[0024] Furthermore, the industrial paraffin is high-temperature paraffin with a melting point above 60°C and no purity requirement.
[0025] The preparation of a universal material for back and mouth sealing of fireworks and firecrackers based on industrial paraffin comprises the following steps: (1) Dry the quartz sand particles and preheat them to above 50-70°C for use; (2) Place the solid industrial paraffin in a heating tank and heat it evenly to above 70°C using a heating element to completely melt the solid paraffin into a liquid state; (3) Add the quartz sand particles of step (1) into the heating tank containing liquid paraffin in step (2), and evenly mix the paraffin and the quartz sand particles at a temperature of 60-75° C. and stir for 5-10 minutes to obtain the bottom and mouth sealing universal material.
[0026] The fireworks and firecrackers bottom sealing process based on industrial paraffin completes the fireworks and firecrackers bottom sealing operation, including the following steps: (1) pouring a section of the general fireworks and firecrackers bottom and mouth sealing material based on industrial paraffin at one end of the barrel and curing it for 1 to 2 hours to complete the bottom sealing process; (2) loading pyrotechnic powder into the end of the bottom and top sealing universal material near the solidified bottom and top sealing universal material in the above step (1), thereby completing the charging process; (3) Add the pyrotechnic powder in step (2) and insert the fuse at the end away from the bottom cover in step (1). The fuse should be able to extend into the pyrotechnic powder for a certain length, thus completing the insertion and fuse process; (4) evenly laying a barrier layer at the junction of the fuse and the pyrotechnic powder in the above step (3) to prevent the pyrotechnic powder from directly contacting the liquid paraffin in the universal material for the bottom and mouth sealing in step (5); (5) Pour a predetermined amount of general bottom and top sealing material into one end of the barrier layer laid in step (4) and cure it for 2 to 3 hours to complete the sealing process.
[0027] Furthermore, the material used for the barrier layer is a paper sheet or fine sand with a particle size of 0.5 to 1.5 or a powdery or granular solid substance with stable properties.
[0028] Furthermore, the material used for the barrel is any material such as paper, plastic or fiber that can withstand a temperature above 70°C, and there is no specific restriction on the shape of the barrel.
[0029] Example 2
[0030] This example provides a universal material for the bottom and mouth sealing of fireworks and firecrackers based on industrial paraffin, which is made of the following raw materials in parts by weight: 70 parts of quartz sand and 30 parts of industrial paraffin.
[0031] Furthermore, the quartz sand has a particle size of 2, does not need to be cleaned of impurities, and needs to be dried.
[0032] Furthermore, the industrial paraffin is high-temperature paraffin with a melting point above 60°C and no purity requirement.
[0033] The preparation method is the same as Example 1.
[0034] The bottom sealing and mouth sealing process steps are the same as those in Example 1.
[0035] Example 3.
[0036] This example provides a universal material for the bottom and mouth sealing of fireworks and firecrackers based on industrial paraffin, which is made of the following raw materials in parts by weight: 60 parts of quartz sand and 40 parts of industrial paraffin.
[0037] Furthermore, the quartz sand has a particle size of 4, does not need to be cleaned of impurities, and needs to be dried.
[0038] Furthermore, the industrial paraffin is high-temperature paraffin with a melting point above 60°C and no purity requirement.
[0039] The preparation method is the same as Example 1.
[0040] The bottom sealing and mouth sealing process steps are the same as those in Example 1.
Claims
1. A general material for sealing the bottom and mouth of fireworks and firecrackers based on industrial paraffin, characterized in that: The invention is prepared from the following raw materials in parts by weight: 60-80 parts of quartz sand and 20-40 parts of industrial paraffin wax.
2. The general material for back and mouth sealing of fireworks and firecrackers based on industrial paraffin according to claim 1, characterized in that: The invention is prepared from the following raw materials in parts by weight: 65-75 parts of quartz sand and 25-35 parts of industrial paraffin wax.
3. The general material for back and mouth sealing of fireworks and firecrackers based on industrial paraffin according to claim 1, characterized in that: The invention is made from the following raw materials in parts by weight: 70 parts of quartz sand and 30 parts of industrial paraffin.
4. The general material for back and mouth sealing of fireworks and firecrackers based on industrial paraffin according to any one of claims 1 to 3, characterized in that: The quartz sand has a particle size of 0.5-32, does not need to remove impurities, and needs to be dried. The particle size is proportional to the inner diameter of the barrel.
5. The general material for back and mouth sealing of fireworks and firecrackers based on industrial paraffin according to any one of claims 1 to 3, characterized in that: The industrial paraffin wax is high-temperature paraffin wax with a melting point above 60°C and no purity requirement is imposed.
6. Preparation of a universal material for back and mouth sealing of fireworks and firecrackers based on industrial paraffin, characterized in that: The following steps are involved: (1) Dry the quartz sand particles with a particle size of 0.5-32 and preheat them to 50-70°C for use; (2) Place the solid industrial paraffin in a heating tank and heat it evenly to above 70°C using a heating element to completely melt the solid paraffin into a liquid state; (3) Add the quartz sand particles of step (1) into the heating tank containing liquid paraffin in step (2), uniformly mix the paraffin and the quartz sand particles at a temperature of 60-75° C. and stir for 5-10 minutes, and keep the temperature for 5-10 minutes to obtain the bottom and mouth sealing universal material.
7. The method for preparing a fireworks and firecrackers bottom sealing material based on industrial paraffin according to claim 6, characterized in that: In step (1), the quartz sand particles need to be preheated before mixing with the paraffin wax, and the preheating temperature is 50-70°C.
8. A fireworks and firecrackers bottom sealing process based on industrial paraffin, characterized in that: The process comprises the following steps: (1) pouring a section of the general material for back-sealing and sealing fireworks and firecrackers based on industrial paraffin at one end of the barrel, and curing it for 1 to 2 hours to complete the back-sealing process; (2) loading pyrotechnic powder into the end of the general material for back-sealing and sealing near the cured end in the above step (1), and completing the charging process; (3) loading pyrotechnic powder into the end of the above step (2) and away from the back-sealing in the step (1), and inserting a fuse, requiring that the fuse can extend into the pyrotechnic powder for a certain length, and completing the insertion process; (4) evenly laying a barrier layer at the junction of the fuse and the pyrotechnic powder in the above step (3) to prevent the pyrotechnic powder from directly contacting the liquid paraffin in the general material for back-sealing and sealing in the step (5); (5) pouring a predetermined amount of general material for back-sealing and sealing into the end on which the barrier layer is laid in the step (4), and curing it for 2 to 3 hours to complete the sealing process.
9. The process steps of sealing the bottom and mouth of fireworks and firecrackers based on industrial paraffin according to claim 8, characterized in that: In step (4), the barrier layer material is a paper sheet or fine sand with a particle size of 0.5-1.5 or other powdery or granular solid with stable properties. The thickness of the barrier layer is above 4 mm, without specific limitation.
10. The process steps of sealing the bottom and mouth of fireworks and firecrackers based on industrial paraffin according to claim 8, characterized in that: In step (1), the shape of the barrel is not particularly limited.