Red light adjustable fluorescent material and preparation method and application thereof

By applying high pressure to the red fluorescent material (C7H7N2)2PbCl4-Mn at room temperature, it improves its fluorescence brightness, solves the problem of weak emission in its natural state, realizes adjustable fluorescence peak position, and expands its pressure sensor and anti-counterfeiting Application prospects in the field.

CN118956375APending Publication Date: 2024-11-15WUYI UNIV
View PDF 0 Cites 0 Cited by

Patent Information

Application Number
CN202410967468.1
Authority / Receiving Office
CN · China
Patent Type
Applications(China)
Current Assignee / Owner
Filing Date
2024-07-18
Publication Date
2024-11-15

AI Technical Summary

Technical Problem

The existing red fluorescent material (C7H7N2)2PbCl4-Mn emits weakly in a natural state, making it difficult to improve its fluorescence brightness, limiting its application in pressure sensors and other fields.

Method used

By placing the fluorescent material in the sealed sample cavity of the high-pressure device, applying a pressure of 15 to 16 GPa at room temperature, using diamond anvil and dimethyl silicone oil as pressure transfer medium, red adjustable fluorescent material was prepared after unloading the pressure. , use the ruby ​​fluorescence peak to perform pressure calibration.

Benefits of technology

The brightness of the fluorescent material is significantly improved, and the fluorescence peak is red-shifted from 626nm to 775nm, achieving adjustable fluorescence emission peaks, broadening its application range in pressure sensors and anti-counterfeiting fields.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure CN118956375A_ABST
    Figure CN118956375A_ABST
Patent Text Reader

Abstract

The invention relates to the technical field of luminescent materials, and particularly discloses a red light adjustable fluorescent material as well as a preparation method and application thereof. The fluorescent material is placed in a sealed sample cavity of a high-pressure device, pressure is applied to an anvil at normal temperature, and the red light adjustable fluorescent material is prepared after pressure relief. According to the (C7H7N2) 2PbCl4-Mn fluorescent material disclosed by the invention, the pressure is increased to 15.18 GPa at normal temperature, and the fluorescence peak is subjected to red shift from 626 nm to 775 nm along with the increase of the pressure. The fluorescent emission peak is adjustable in a large range, the application range of the red light adjustable fluorescent material (C7H7N2) 2PbCl4-Mn is widened, and the fluorescent material has a wide application prospect in the fields of pressure sensors, anti-counterfeiting and the like.
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] The present invention relates to the technical field of luminescent materials, and in particular to a red light tunable fluorescent material and a preparation method and application thereof. Background Art

[0002] Fluorescent materials are widely used in lighting, display, biological imaging and other fields. However, the method of preparing high-brightness red fluorescent materials still needs to be improved. In particular, fluorescent materials such as (C7H7N2)2PbCl4-Mn have weak emission in their natural state. If they are prepared into sensors, they need to be prepared by specific methods to improve their fluorescence brightness.

[0003] Pressure sensors are used in many fields, including but not limited to automobiles, aviation, medical treatment, environmental protection, etc. They can be used to detect and monitor pressure changes in various physical processes to ensure the normal operation of equipment and the safety of personnel. By measuring the fluorescence intensity of the material, the pressure applied to the material can be inferred, thus achieving contactless measurement of pressure.

[0004] Therefore, it is necessary to provide a red light tunable fluorescent material and a preparation method and application thereof, so as to improve the brightness of the fluorescent material and open up new possibilities for the development of pressure sensing technology. Summary of the invention

[0005] The present invention aims to solve at least one of the technical problems existing in the above-mentioned prior art. To this end, the present invention proposes a red light tunable fluorescent material and a preparation method and application thereof, thereby improving the brightness of the fluorescent material and opening up new possibilities for the development of pressure sensing technology.

[0006] A first aspect of the present invention provides a method for preparing a red light tunable fluorescent material.

[0007] Specifically, the following steps are included:

[0008] The fluorescent material is placed in a sealed sample chamber of a high-pressure device, pressure is applied to an anvil at room temperature, and a red light tunable fluorescent material is obtained after the pressure is released.

[0009] Preferably, the fluorescent material is (C7H7N2)2PbCl4-Mn.

[0010] Preferably, the anvil is a diamond anvil.

[0011] Preferably, the pressure is 15-16 GPa.

[0012] More preferably, the pressure is 15 to 15.5 GPa.

[0013] More preferably, the pressure is 15.18 GPa.

[0014] Preferably, the pressure of the pressure relief is normal pressure.

[0015] Preferably, the high-pressure device further comprises a gasket.

[0016] Preferably, the material of the gasket is T301 steel sheet. After the gasket is pre-pressed by a diamond anvil, a micro-pore sample cavity with a diameter of 145-155 μm is punched at the center of the pre-pressed pit by an electric spark puncher.

[0017] Further preferably, the diameter is 150 μm.

[0018] Preferably, the high-pressure device also includes a pressure transmission medium.

[0019] Further preferably, the pressure transmission medium is dimethyl silicone oil. Adding dimethyl silicone oil into the sealed sample cavity can ensure that the pressure in the cavity is hydrostatic pressure.

[0020] Preferably, the pressure calibration object of the applied pressure is the ruby ​​fluorescence peak. After the fluorescent material is loaded into the sealed sample cavity, a ruby ​​ball is placed therein, and the pressure in the sealed sample cavity is calibrated using the ruby ​​fluorescence spectrum, with the ruby ​​fluorescence peak being the calibration object of the pressure magnitude.

[0021] Further preferably, the method for detecting the ruby ​​fluorescence spectrum comprises the following steps:

[0022] The laser is irradiated onto the sample in the sample chamber of the DAC press through the optical path in the Nikon Ti-U inverted biological microscope. The fluorescence signal is converted into a fluorescence spectrum by a fiber optic spectrometer (Brand: OceanOptics, Model: QE65000) connected to the microscope.

[0023] A second aspect of the present invention provides a red light tunable fluorescent material.

[0024] Specifically, the red light tunable fluorescent material is prepared by the preparation method provided by the first aspect of the present invention.

[0025] A third aspect of the present invention provides an application of a red light tunable fluorescent material in the field of pressure sensors.

[0026] A fourth aspect of the present invention provides an application of a red light tunable fluorescent material in the field of anti-counterfeiting.

[0027] Compared with the prior art, the beneficial effects of the present invention are as follows:

[0028] The (C7H7N2)2PbCl4-Mn fluorescent material of the present invention increases the pressure to 15.18GPa at room temperature, and the fluorescence peak red-shifts from 626nm to 775nm as the pressure increases. The fluorescence emission peak is adjustable over a wide range, which is conducive to broadening the application scope of the red light adjustable fluorescent material (C7H7N2)2PbCl4-Mn, and has broad application prospects in the fields of pressure sensors and anti-counterfeiting. BRIEF DESCRIPTION OF THE DRAWINGS

[0029] Figure 1 This is the fluorescence spectrum of (C7H7N2)2PbCl4-Mn at normal pressure 1atm under the conditions of Comparative Example 1;

[0030] Figure 2 This is a comparison chart of the fluorescence spectra of (C7H7N2)2PbCl4-Mn at different pressure points under the conditions of Example 1;

[0031] Figure 3 It is a comparison diagram of the fluorescence spectra of (C7H7N2)2PbCl4-Mn under the conditions of Comparative Example 1 and (C7H7N2)2PbCl4-Mn under the conditions of Example 1;

[0032] Figure 4 Fluorescence photographs of various pressure points of (C7H7N2)2PbCl4-Mn under the conditions of Example 1;

[0033] Figure 5 It is the fluorescence peak position diagram after the fluorescence spectrum statistics of (C7H7N2)2PbCl4-Mn under the conditions of Example 1;

[0034] Figure 6 This is a fluorescence intensity diagram after statistics of the fluorescence spectrum of (C7H7N2)2PbCl4-Mn under the conditions of Example 1. DETAILED DESCRIPTION

[0035] In order to make the technical scheme of the present invention more clearly understood by those skilled in the art, the following embodiments are listed for illustration. It should be pointed out that the following embodiments do not limit the protection scope of the present invention.

[0036] Unless otherwise specified, the raw materials, reagents or devices used in the following examples can be obtained from conventional commercial sources or by existing known methods.

[0037] Example 1

[0038] A red light tunable fluorescent material and a preparation method thereof.

[0039] The (C7H7N2)2PbCl4-Mn fluorescent material was placed in a sealed sample chamber of a diamond anvil (DAC) with an anvil face diameter of 400μm. A T301 stainless steel gasket was selected and a 40μm thick pit was pre-pressed. A microporous sample chamber with a diameter of 150μm was obtained in the center of the pit using an electric spark punch. After the fluorescent material was loaded into the sample chamber, dimethyl silicone oil was used as the pressure transmission medium, and then a ruby ​​ball was loaded to determine the actual pressure in the sample chamber. The pressure calibration used the standard ruby ​​fluorescence method. The in-situ high-pressure fluorescence experiment used a 10mW 355nm laser excitation. No pressure-transmitting medium was added in the high-pressure experiment. The diamond anvil pressed the fluorescent material to 15.18GPa, and then the diamond anvil released the pressure to normal pressure 1atm to obtain a high-brightness red fluorescent (C7H7N2)2PbCl4-Mn red light tunable fluorescent material. The fluorescence spectrum of (C7H7N2)2PbCl4-Mn was recorded by a spectrometer, and the fluorescence spectrum was recorded when the pressure was R1 atm.

[0040] Comparative Example 1

[0041] A fluorescent material and a preparation method thereof.

[0042] The (C7H7N2)2PbCl4-Mn fluorescent material was placed in a sealed sample chamber of a diamond anvil (DAC) with an anvil face diameter of 400μm. A T301 stainless steel gasket was selected and a 40μm thick pit was pre-pressed. A microporous sample chamber with a diameter of 150μm was obtained in the center of the pit using an electric spark puncher. After the fluorescent material was loaded into the sample chamber, dimethyl silicone oil was used as a pressure transmission medium, and then a ruby ​​ball was loaded to determine the actual pressure in the sample chamber. The pressure calibration was performed using the standard ruby ​​fluorescence method. The in-situ high-pressure fluorescence experiment used a 10mW 355nm laser excitation. No pressure transmission medium was added to the high-pressure experiment. At room temperature, the diamond anvil maintained a normal pressure of 1atm on the fluorescent material for 60s to obtain the (C7H7N2)2PbCl4-Mn fluorescent material. The fluorescence spectrum of (C7H7N2)2PbCl4-Mn was recorded by a spectrometer, and the fluorescence spectrum when the pressure was 1atm was recorded.

[0043] Test results:

[0044] Figure 1 The fluorescence spectrum of (C7H7N2)2PbCl4-Mn at 1atm under the conditions of Comparative Example 1 is shown in FIG. Figure 1 A weak fluorescence emission peak can be observed. Figure 2This is a comparison chart of the fluorescence spectra of (C7H7N2)2PbCl4-Mn at pressure points of 2.17 GPa to 15.18 GPa under the conditions of Example 1. Under this condition, the peak position of (C7H7N2)2PbCl4-Mn is red-shifted, and the fluorescence peak can be red-shifted from 626 nm to 775 nm as the pressure increases. Figure 3 The fluorescence spectra of (C7H7N2)2PbCl4-Mn under the conditions of Comparative Example 1 and (C7H7N2)2PbCl4-Mn under the conditions of Example 1 are compared. When the pressure is increased to 15.18 GPa and then released to R1 atm, a larger fluorescence emission peak is observed compared to the normal pressure of 1 atm in Comparative Example 1. Figure 4 The 1atm and R1atm fluorescence photos in the paper also further confirmed this. Figure 5 and 6 It can be observed that the peak position of (C7H7N2)2PbCl4-Mn under the conditions of Example 1 has a regular linear change with the increase of pressure, and the peak intensity also has a continuous change. This advantage makes the (C7H7N2)2PbCl4-Mn material under the conditions of Example 1 with adjustable fluorescence have broad application prospects in the fields of pressure sensors, detection, anti-counterfeiting, etc. The enhanced fluorescence emission after pressure relief broadens the application range of the material.

[0045] The preferred specific embodiments of the present invention are described in detail above. It should be understood that a person skilled in the art can make many modifications and changes based on the concept of the present invention without creative work. Therefore, any technical solution obtained by any modification, equivalent replacement, improvement, etc. made by a person skilled in the art based on the concept of the present invention through logical analysis, reasoning or limited experiments on the basis of the prior art shall be within the scope of protection determined by the claims.

Claims

1. A method for preparing a red light tunable fluorescent material, characterized in that: The following steps are involved: The fluorescent material is placed in a sealed sample chamber of a high-pressure device, pressure is applied to an anvil at room temperature, and a red light tunable fluorescent material is obtained after the pressure is released.

2. The preparation method according to claim 1, characterized in that: The fluorescent material is (C7H7N2)2PbCl4-Mn.

3. The preparation method according to claim 1, characterized in that: The anvil is a diamond anvil.

4. The preparation method according to claim 1, characterized in that: The pressure is 15-16 GPa.

5. The preparation method according to claim 1, characterized in that: The pressure of the decompression is normal pressure.

6. The preparation method according to claim 1, characterized in that: The high-voltage device also includes a gasket.

7. The preparation method according to claim 6, characterized in that: The material of the gasket is T301 steel sheet.

8. A red light tunable fluorescent material, characterized in that: The red light tunable fluorescent material is prepared by the preparation method described in any one of claims 1 to 7.

9. Application of the red light tunable fluorescent material according to claim 8 in the field of pressure sensors.

10. Use of the red light tunable fluorescent material according to claim 8 in the field of anti-counterfeiting.