Transient-stable double-state response metal thickness measuring method with surface covering layer
Through the temporary stable bistate response method based on pulse excitation and combined with the dual probe structure, the online, lossless and accurate problems of metal surface cover thickness detection are solved, and efficient and low-cost metal thickness measurement is achieved, suitable for various thicknesses and environmental conditions.
Patent Information
- Application Number
- CN202411436664.2
- Authority / Receiving Office
- CN · China
- Patent Type
- Applications(China)
- Current Assignee / Owner
- Filing Date
- 2024-10-15
- Publication Date
- 2024-11-15
- Estimated Expiration
- 2044-10-15
AI Technical Summary
When existing metal thickness measurement technology has cover or impurities on the metal surface, it is difficult to achieve online, non-destructive and accurate thickness detection, and traditional methods have problems such as destructiveness, high cost, and radiation risks.
Using a temporary stable bistate response method based on pulse excitation, the magnetic flux response is stimulated by pulse current, and the steady state values and transition characteristic point slopes of positive and negative pulses are used, combined with the dual probe structure, the metal thickness of the cover layer with the surface is realized. Accurate measurement.
This method does not require the sample to be damaged, it is simple to operate, low cost, avoids radiation risks, is suitable for different thicknesses and environmental conditions, improves measurement accuracy and range, and is especially suitable for the detection of thin layer metal thickness.
Smart Images

Figure CN118960541A_ABST
Abstract
Description
Technical Field
[0001] The invention relates to the field of metal geometric dimension measurement, in particular to a metal thickness measurement method with a surface covering layer and a temporary stable dual-state response method mainly used for measuring the thickness of metal with a surface covering layer. Background Art
[0002] Metal thickness measurement is a key industrial inspection technology, which is widely used in the production, processing and quality control of metal materials. The development background of this technology is closely related to the high requirements of industrial production for material performance and safety. With the advancement of materials science and manufacturing technology, higher requirements are placed on the accuracy and efficiency of metal material thickness measurement. The development of metal thickness measurement technology has experienced a transition from traditional mechanical measurement methods to modern non-contact measurement technologies. The application of these technologies not only improves the accuracy and repeatability of measurement, but also expands the scope of measurement application, making metal thickness measurement adaptable to diverse industrial environments and material properties. Therefore, it is particularly critical to realize and develop metal thickness measurement.
[0003] There are many methods for measuring metal thickness, including but not limited to metallographic method, coulometric method, X-ray fluorescence method, ultrasonic thickness measurement method, etc. These methods have their own characteristics and are suitable for different occasions and metal materials of different thicknesses. Metallographic method is a method of measuring the local thickness of the cross section of a metal sample using a metallographic microscope. Its advantages are its high accuracy and reliability, and its disadvantage is that it is a destructive measurement method because it requires slicing and grinding of the sample; Coulometric method is suitable for measuring the thickness of single-layer and multi-layer metal coatings. Its advantages are high accuracy and reliability, and its disadvantages are that the operation process is relatively complicated, and the price of consumables such as potions is high; X-ray fluorescence method is a non-destructive measurement method. Its advantages are fast and non-destructive measurement, and its disadvantages are high cost and radiation risk; ultrasonic thickness measurement is a thickness measurement method based on the principle of ultrasonic pulse reflection. Its advantages are that it can accurately measure various materials in production equipment, and its disadvantages are that it is easily affected by the surrounding environment. It should be noted that when there is a coating or surface covering on the metal surface, the above detection methods are no longer applicable, unless it is achieved under the premise of destroying the surface coating or removing the surface covering. Therefore, it is urgent to solve the problem of online, non-destructive detection of metal thickness when there is a protective layer or shielding layer on the metal surface.
[0004] In general, the development trend of metal thickness measurement technology is towards higher precision, higher efficiency and more intelligence. With the continuous emergence of new technologies, metal thickness measurement technology will provide stronger support for industrial production and promote industrial production to a higher level. Summary of the invention
[0005] In view of the above problems, the present disclosure proposes a method for measuring the thickness of a metal with a surface covering layer based on a pulse excitation transient stable dual-state response.
[0006] In order to solve at least one of the above technical problems, the present disclosure proposes the following technical solutions: A method for measuring the thickness of metal with a surface covering layer with a transient dual-state response, in which a pulse current is used to excite the coil magnetic flux, and positive and negative pulse responses appear. As the metal thickness increases, the rising speed of the positive pulse response and the falling speed of the negative pulse response gradually decrease and stabilize, thereby realizing the measurement of the metal thickness.
[0007] In some embodiments, a metal thickness measurement method with a surface covering layer having a transient stable dual-state response is a metal thickness measurement method based on a steady-state value of a pulse excitation response, a pulse current excitation steady-state response is a metal thickness measurement characterization method, and a steady-state value of a pulse current excitation magnetic flux response is an intuitive reflection of the metal thickness of the object being measured. The steady-state values of different metal thicknesses in the positive pulse steady-state region decrease as the metal thickness increases, and the steady-state values in the negative pulse steady-state region increase as the metal thickness increases.
[0008] In some embodiments, a method for measuring metal thickness based on a steady-state value of an impulse excitation response comprises the following steps: Step 1-1. Determination of the steady-state value in the stable region, The steady-state value in the stable region of the magnetic flux response curve is used as a characteristic quantity to effectively measure the metal thickness. Therefore, under the action of pulse current excitation, before the next pulse comes, the value of the magnetic flux that is stable and unchanged is recorded as the steady-state value; Step 1-2. Steady-state value-metal thickness relationship expression, Use the power function to fit different metal thicknesses and the corresponding steady-state values in the stable region, and finally get the relationship expression: f ( x )=A x +B, where f ( x ) represents the stable magnetic flux value in the stable region, x Represents metal thickness; Step 1-3. Expression analysis, The steady-state value of the positive pulse stable area and the stable value of the negative pulse stable area are quantitatively compared and analyzed with the fitting relationship curve respectively; Step 1-4. Accuracy assessment, The steady-state values of the positive pulse and negative pulse plateau regions of the response signal of metal aluminum of known thickness under the excitation of the pulse signal are substituted into the fitting expression respectively to obtain its response value, which is then compared with the actual metal thickness to obtain the error.
[0009] In some embodiments, a method for measuring metal thickness based on a steady-state value of an impulse excitation response comprises the following steps: Step 1-1. Determination of the steady-state value in the stable region, Under the same excitation parameters and external conditions, the steady-state values of the positive pulse and negative pulse stable regions corresponding to different metal thicknesses are calculated; Step 1-2. Steady-state value-metal thickness relationship expression, Use the power function to fit different metal thicknesses and the corresponding steady-state values in the stable region, and finally get the relationship expression: f ( x )=A x +B, where f ( x ) represents the stable magnetic flux value in the stable region, x Represents the metal thickness. For the positive pulse response curve, A=-1.107×10 -5 , B=0.003058, for the negative pulse response curve, A=1.107×10 -5 , B=-0.003058; Step 1-3. Expression analysis, The steady-state value in the positive pulse stable zone gradually decreases with the increase of thickness, and the steady-state value in the negative pulse stable zone gradually increases with the increase of thickness; Step 1-4. Accuracy assessment, The steady-state values of the positive pulse and negative pulse plateau regions of the response signal of metal aluminum with a thickness of 0.08 mm and 0.44 mm under the excitation of the pulse signal were substituted into the fitting expression, and the values were obtained to be 0.076 mm and 0.4414 mm respectively. Then, compared with the actual metal thickness, the errors were 3.75% and 0.32%.
[0010] In some embodiments, a method for measuring the thickness of a metal with a surface covering layer with a transient and stable two-state response is a method for characterizing the metal thickness based on the slope of transition characteristic points of a pulse response transient process. The pulse current excitation transient response is a unique attribute of the metal thickness measurement characterization method, which is characterized in that: the transient process of the pulse current excitation flux response contains characteristic information of the metal thickness, and the slope of the transition characteristic points extracted based on the positive and negative pulses of the transient process decreases with the increase of the metal thickness. The slope of the transition characteristic points of the flux response transient process is adopted to effectively measure different metal thicknesses.
[0011] In some embodiments, a method for characterizing metal thickness based on the slope of a transition characteristic point of a pulse response transient process comprises the following steps: Step 2-1. Determine the transition feature points. The transient process of pulse excitation response changes with the change of metal thickness. The slope of transition characteristic point is used as the characteristic quantity of metal thickness measurement to ensure more accurate measurement results. Step 2-2. Fitting the relational expression, The exponential function is used to fit the different thicknesses of metals and the corresponding slopes of transition characteristic points. The fitted relationship expression is: f ( x )=Ae Bx +Ce Dx , where f ( x ) is the slope value of the transition feature point, x Represents metal thickness; Step 2-3. Relational expression analysis, The transition characteristic points extracted from the positive pulse transient process and the transition characteristic points extracted from the negative pulse transient process are quantitatively compared and analyzed with the fitting curves respectively; Step 2-4. Measurement accuracy evaluation, Select metal of known thickness, obtain the slope of the transition characteristic point based on the response curve under the excitation of the pulse signal, substitute it into the fitting expression, calculate the corresponding metal thickness, compare it with the actual metal thickness, and obtain the measurement error.
[0012] In some embodiments, a method for characterizing metal thickness based on the slope of a transition characteristic point of a pulse response transient process comprises the following steps: Step 2-1. Determine the transition feature points. Maximum stable value and time through the stable area t =0 intersection point y =-k x +Φ, and then intersect this straight line with the transition area of each metal thickness to obtain the transition characteristic point Q corresponding to the metal of different thickness, and then calculate the tangent slope of this characteristic point respectively. The transition characteristic point of the negative pulse transient process is obtained in the same way; Step 2-2. Fitting the relational expression, The exponential function is used to fit the different thicknesses of metals and the corresponding slopes of transition characteristic points. The fitted relationship expression is: f ( x )=Ae Bx +Ce Dx , where f ( x ) is the slope value of the transition feature point, xRepresents the metal thickness. For the positive pulse response curve, A=1.435, B=-1.922, C=0.7115, D=-0.1446; for the negative pulse response curve, A=-13.48, B=-19.76, C=-1.578, D=-0.4752; Step 2-3. Relational expression analysis, By analyzing the fitting curve, the slope of the transition feature point extracted from the positive pulse transient process is basically consistent with the metal thickness fitting, while the slope of the transition feature point extracted from the negative pulse transient process is not ideal for the metal thickness fitting. Step 2-4. Measurement accuracy evaluation, The metal thickness is selected as 0.12mm. Based on the response curve under the excitation of the pulse signal, the slope of the transition characteristic point is obtained and substituted into the fitting expression. The metal thickness is calculated to be 0.1213mm and 0.1402mm. It is compared with the actual metal thickness to obtain the measurement error. The results show that the error value of the fitting function of the positive pulse metal thickness and the slope of the transition characteristic point is smaller than the fitting function of the negative pulse metal thickness and the slope of the transition characteristic point. Therefore, the slope of the transition characteristic point of the positive pulse transient process is selected to effectively measure the metal thickness.
[0013] In some embodiments, a method for measuring the thickness of a metal with a surface covering layer with a temporary stable dual-state response is a method for measuring the thickness of a metal based on the stable value of a dual-probe pulse response in a stable region. The dual-probe pulse current excitation steady-state response is an effective way to increase the effective range of metal thickness measurement and improve accuracy. The stable value of the dual-probe pulse response also has the ability to measure metals of different thicknesses. The excitation probe is on one side of the metal, and the probe on the other side serves as the receiving end of the response signal. The stable value of the positive pulse of the magnetic flux response signal decreases significantly with the increase of the metal thickness, and the stable value of the negative pulse decreases significantly with the increase of the metal thickness.
[0014] In some embodiments, a metal thickness measurement method based on a stable value of a dual-probe pulse response stable region is characterized by comprising the following steps: Step 3-1. Determination of the stability value of the dual-probe stable area, Based on the stable value of the stable area of the dual-probe magnetic flux response curve as the characteristic quantity characterization, the method of effectively measuring the thickness of different metals, controlling the pulse width, and reducing the pulse transient response time can obtain a relatively stable and unchanged magnetic flux stable value; Step 3-2. Fitting the expression of the relationship between the two probes in the stable region. Use exponential function to fit the metal thickness to the corresponding stable value of the dual probe stable area. f ( x )=Ae Bx +Ce Dx , where f (x ) is the stable value of the receiving probe in the stable area, x is the metal thickness; Step 3-3. Analysis of the expression of the relationship between the two probe stable regions, The stability values of the positive pulse stable area and the negative pulse stable area of the dual probes were quantitatively compared and analyzed with the fitting curves. Step 3-4. Metal thickness measurement accuracy evaluation, The stable values of the positive pulse stable area and the negative pulse stable area obtained by measuring metal aluminum of known thickness are substituted into the fitting function respectively to obtain the corresponding thickness, which is then compared with the actual metal thickness to obtain the measurement error.
[0015] In some embodiments, a metal thickness measurement method based on a stable value of a dual-probe pulse response stable region is characterized by comprising the following steps: Step 3-1. Determination of the stability value of the dual-probe stable area, Based on the stable value of the stable area of the dual-probe magnetic flux response curve as the characteristic quantity, the different metal thicknesses can be effectively measured. The excitation probe is on one side of the metal, and the probe on the other side is used as the receiving end of the response signal. The stable value of the positive pulse and negative pulse stable area corresponding to different metal thicknesses is obtained; Step 3-2. Fitting the expression of the relationship between the two probes in the stable region. Use exponential function to fit the metal thickness to the corresponding stable value of the dual probe stable area. f ( x )=Ae Bx +Ce Dx , where f ( x ) is the stable value of the receiving probe in the stable area, x is the metal thickness, positive pulse response curve, A=0.000186, B=-1.012, C=9.837×10 -5 , D=-0.3627, negative pulse response curve, A=-0.000186, B=-1.012, C=-9.837×10 -5 , D = -0.3627; Step 3-3. Analysis of the expression of the relationship between the two probe stable regions, The stability value of the dual probe positive pulse stable area gradually decreases with the increase of metal thickness, and the stability value of the negative pulse stable area gradually increases with the increase of metal thickness; Step 3-4. Metal thickness measurement accuracy evaluation, The stable values of the positive pulse stable area and the negative pulse stable area obtained when the thickness of metal aluminum is 0.3mm and 3mm are substituted into the fitting function respectively, and the obtained thickness is 0.3001mm and 2.98mm. They are compared with the actual metal thickness to obtain the measurement error. The results show that both the positive pulse and negative pulse stable areas can effectively realize the measurement of metal thickness.
[0016] The above technical solution has the following advantages or beneficial effects: The present invention provides a method for measuring the thickness of metal with a surface covering thin layer based on pulse excitation transient stable dual-state response, which solves the conflicting problem between measurement accuracy and detection complexity in the prior art, which is specifically manifested as follows: 1) Compared with the metallographic method, the advantage of this method is that it is not a destructive measurement method, because the metallographic method requires slicing and grinding of the sample; compared with the coulometric method, this method is simple and reliable, does not require a relatively complicated operation process, and does not require expensive consumables such as potions; compared with the X-ray fluorescence method, the advantage of this method is that it can be measured quickly and non-destructively without high costs and radiation risks; compared with the ultrasonic thickness measurement method, the advantage of this method is that it is not easily affected by the surrounding environment and is suitable for measuring the thickness of thin metal layers.
[0017] 2) The present invention provides a method for measuring metal thickness in different ranges. Different strategies are adopted for metal thickness in different measuring ranges, thereby improving measurement accuracy and saving measurement costs.
[0018] 3) When there is a coating or impurities on the metal surface, the advantages of the metal thickness measurement method with a thin surface coating based on pulse excitation transient two-state response are particularly prominent. During the implementation of other existing metal thickness measurement methods, the coating and impurities on the surface must be removed first, otherwise the measurement accuracy will be greatly reduced.
[0019] The present invention starts from the nature of eddy current changes in metals, deeply understands the intrinsic relationship between pulse response and metal thickness, and explores effective feature characterization methods and parameters for describing the geometric dimensional properties of metals. BRIEF DESCRIPTION OF THE DRAWINGS
[0020] The present invention and its features, configurations and advantages will become more apparent by reading the detailed description of non-limiting embodiments with reference to the following drawings. The same reference numerals indicate the same parts throughout the drawings. The drawings are not drawn to scale, but rather to illustrate the subject matter of the present invention.
[0021] Figure 1 The transient positive pulse response curves of coils with different metal thicknesses in some embodiments of the present invention; Figure 2The transient negative pulse response curves of coils with different metal thicknesses in some embodiments of the present invention; Figure 3 A single probe pulse excitation metal thickness measurement model in some embodiments of the present invention; Figure 4 These are the transient characteristic points of positive pulses with different metal thicknesses in Scheme 1; Figure 5 These are the transient characteristic points of negative pulses with different metal thicknesses in Scheme 1; Figure 6 These are the transient characteristic points of positive pulses with different metal thicknesses in Scheme 2; Figure 7 These are the transient characteristic points of negative pulses with different metal thicknesses in Scheme 2; Figure 8 A dual-probe pulse excitation metal thickness measurement model in some embodiments of the present invention; Fig. 9 Response curves of dual-probe pulse excitations with different metal thicknesses in some embodiments of the present invention. DETAILED DESCRIPTION
[0022] It should be noted that, in the absence of conflict, the embodiments and features in the embodiments of the present application can be combined with each other. It should be noted that the terms used in the present invention are only for describing specific implementation methods and are not intended to limit the exemplary implementation methods according to the present application.
[0023] It should be understood that when the terms “include” and / or “comprise” are used in this specification, they specify the presence of features, steps, operations, devices, components and / or their combinations.
[0024] The terms “first”, “second” and “third” are used for descriptive purposes only and should not be understood as indicating or implying relative importance.
[0025] The technical solutions in the embodiments of the present invention are described below in conjunction with the drawings in the embodiments of the present invention. It is obvious that the described embodiments are only part of the embodiments of the present invention, rather than all the embodiments. Therefore, the following detailed description of the embodiments of the present invention provided in the drawings is not intended to limit the scope of the invention claimed for protection, but merely represents the selected embodiments of the present invention. Based on the embodiments of the present invention, all other embodiments obtained by those skilled in the art without making creative work belong to the protection scope of the present invention.
[0026] The metal is stimulated by a pulse signal. T =0.2s, pulse width D=0.12s, duty cycle is 60%. The response curve has different reactions to different metal thicknesses. For the positive pulse response curve, as the metal thickness increases, the rate of increase of the magnetic flux in the rising stage will gradually decrease until it stabilizes. For the negative pulse response curve, the rate of decrease of the magnetic flux in the falling stage will gradually decrease until it stabilizes. In order to describe the effectiveness of this method, five kinds of metal aluminum with thicknesses of 0.1mm, 0.3mm, 0.6mm, 1mm, and 1.5mm are first selected to measure their respective magnetic flux changes over time under the same conditions and the same time, and then the magnetic flux changes over time are measured respectively. t =0-0.0004s positive pulse response transient phase and time t = stable value at 0.25s, t = 0.08-0.0805s negative pulse response transient stage magnetic flux change and t =0.1999s stable value. The positive pulse response curves of metals with five thicknesses are as follows Figure 1 As shown, the negative pulse response curve is as follows Figure 2 As shown in Figure 2, both the positive pulse response curve and the negative pulse response curve show different dynamic response processes with different metal thicknesses. The differences here include the transient process of the response curve and the stable area of the response curve.
[0027] The following is a detailed introduction to the implementation of three types of feature extraction strategies based on the transient steady-state process of the coil flux response.
[0028] 1. Metal thickness measurement based on steady-state value of pulse excitation response According to the analysis of the stable region of the positive pulse and negative pulse of the pulse response, it can be seen that with the different metal thicknesses, the stable value after the curve tends to be stable is different, and this area is called the stable region. Therefore, selecting the stable value of the stable region as the characteristic quantity characterization of metal thickness measurement can effectively measure different metal thicknesses.
[0029] The specific steps of the metal thickness measurement process based on the steady-state value of pulse excitation response are as follows: ① Set the excitation parameters and select the metal to be measured; ② Use the probe to measure the impedance value of the coil under the excitation of the pulse signal; ③ Use the signal processing circuit to convert the impedance value at both ends of the coil into a magnetic flux value; ④ According to the magnetic flux response curve, obtain the steady-state value in the stable area; ⑤ According to the input-output fitting function, the obtained steady-state value in the stable area is input into the fitting function to solve the measured metal thickness.
[0030] like Figure 3 As shown in the figure, taking aluminum as an example, the steady-state values of the magnetic flux response stable region corresponding to different metal thicknesses are calculated. The corresponding steady-state values of the positive pulse and negative pulse stable regions are different for different metal thicknesses. The specific implementation method is as follows: Step 1-1. Determination of the steady-state value in the stable region The steady-state values of positive pulse and negative pulse for different metal thicknesses are shown in Table 1.
[0031] Table 1 Metal thickness and response steady-state value Metal thickness Positive pulse Negative pulse 0.01 0.00305791312282679 -0.00305791312282679 0.02 0.00305800232222898 -0.00305800232222898 0.03 0.00305798234799440 -0.00305798234799440 0.05 0.00305793716344307 -0.00305793716344307 0.09 0.00305711370137645 -0.00305711370137645 0.1 0.00305701636548352 -0.00305701636548352 0.13 0.00305681890778909 -0.00305681890778909 0.15 0.00305666383410846 -0.00305666383410846 0.18 0.00305644290645303 -0.00305644290645303 0.22 0.00305601482414572 -0.00305601482414572 0.24 0.00305573066579861 -0.00305573066579861 0.29 0.00305414992017087 -0.00305414992017087 0.31 0.00305405645983401 -0.00305405645983401 0.44 0.00305311375496315 -0.00305311375496315 0.46 0.00305314497678254 -0.00305314497678254 0.48 0.00305269847501445 -0.00305269847501445 0.5 0.00305284718017256 -0.00305284718017256 0.56 0.00305183425948331 -0.00305183425948331 0.59 0.00305142325591487 -0.00305142325591487 0.6 0.00305031994965158 -0.00305031994965158 Step 1-2. Steady-state value-metal thickness relationship expression The power function is used to fit 20 metal thicknesses and their corresponding steady-state values in the stable region.
[0032] The relationship between metal thickness and steady-state value is established as follows: (1) In the formula f ( x ) is the stable magnetic flux value in the stable region, x Represents the metal thickness.
[0033] For the positive pulse response curve, A=-1.107×10 -5 , B=0.003058; For the negative pulse response curve, A=1.107×10 -5 , B=-0.003058.
[0034] Step 1-3. Expression analysis Between the metal thickness d = 0 and 0.6 mm, there is an approximate relationship of formula (1). The metal thickness measurement based on the steady-state values of the positive pulse and negative pulse stable region of the pulse excitation response can be applied within this thickness measurement range. Therefore, when using this method to measure metal thickness, there are certain limitations in the range of metal thickness that can be measured. The fitting effect of the steady-state values of the positive pulse and negative pulse stable region and the metal thickness is evaluated, as shown in Table 2.
[0035] Table 2 Fitting effect evaluation It can be seen from Table 2 that the evaluation of the fitting effect of the steady-state value in the stable region of the positive pulse and the steady-state value in the stable region of the negative pulse are the same as the evaluation of the fitting effect of the steady-state value in the stable region of the negative pulse. Therefore, the metal thickness measurement can be performed based on the steady-state values of both positive and negative pulses of the response curve.
[0036] Step 1-4. Accuracy Assessment A metal with a thickness of 0.08 mm was selected for evaluation using the above method. The measured steady-state value of the positive pulse magnetic flux corresponding to the metal was 0.00305715252917557, and the steady-state value of the negative pulse magnetic flux was -0.00305715252917557. Substituting these into the relationship between the metal thickness and the steady-state value (1), the metal thickness was calculated to be 0.076 mm, and the error between this value and the actual value was 3.75%.
[0037] Similarly, a metal with a thickness of 0.44 mm is selected for evaluation using the above method. The measured steady-state value of the positive pulse magnetic flux corresponding to the metal is 0.00305311375496315; the steady-state value of the negative pulse magnetic flux is -0.00305311375496315. Substituting the relationship between the metal thickness and the steady-state value into the expression (1), the metal thickness is calculated to be 0.4414 mm. The error between this value and the actual value is 0.32%.
[0038] In summary, the stable values of the positive pulse and negative pulse stable areas can be selected for metal thickness measurement.
[0039] 2. Metal thickness measurement based on transient characteristic points of pulse response transient process (1) Implementation methods Stable value and time based on the stable region of metal response t =0, make a line y =k x +Φ, this straight line will intersect the transition area again at a point Q, and the slope of the Q point on the response curve is calculated. In order to ensure that the characteristic points can accurately reflect the change in metal thickness, two sets of solutions are designed. The first solution: the maximum stable value in the stable area and the time t =0, make a line y =k x +Φ, and then intersect this straight line with the response curves of each metal thickness to obtain different intersection points Q, and calculate the slope of each intersection point Q and its corresponding response curve. The second solution: use the stable value of the stable area of each metal thickness and time t =0 y =k x +Φ', these straight lines will intersect with their corresponding response curves to obtain their corresponding intersection points Q', and the slopes of these intersection points Q' and their corresponding response curves are calculated. Among them, when the response area is a positive pulse, the k value is -1, and when the response area is a negative pulse, the k value is 1. This is because the stable value of the stable area is related to time. t=0 is approximately a right angle, so taking 45° as the slope can better reflect the changes in the actual response curve. The following takes metal thicknesses of 0.1mm, 0.6mm, and 1.5mm as examples to make schematic diagrams of Scheme 1 and Scheme 2. The positive and negative pulse transition characteristic points of Scheme 1 are as follows: Figure 4 and Figure 5 As shown, the positive and negative pulse transition characteristic points of Scheme 2 are as follows: Figure 6 and Figure 7 The above two solutions can avoid the errors caused by single data fluctuations and possible erroneous evaluations.
[0040] Therefore, the specific steps of the metal thickness measurement process based on the transition characteristic points of the pulse response transient process are as follows: ① Set the excitation parameters and select the metal to be measured; ② Use the probe to measure the impedance value of the coil under the excitation of the pulse signal; ③ Use the signal processing circuit to transform the impedance values at both ends of the coil to obtain the magnetic flux; ④ According to the magnetic flux response curve, obtain the slope of the transition characteristic points of Scheme 1 and Scheme 2; ⑤ According to the input-output fitting function, the obtained characteristic point slope value is input into the fitting function to solve the measured metal thickness.
[0041] (2) Implementation process Step 2-1. Determination of transition feature points Based on the above method, the slope of the transition feature point corresponding to each metal thickness of Scheme 1 and Scheme 2 is obtained, and then the relationship between the metal thickness and the slope of the feature point of Scheme 1 and Scheme 2 is obtained. The results show that the effect of Scheme 1 is better than the effect evaluation data of Scheme 2, so Scheme 1 is selected for further subdivision research. The metal thickness d=0~3mm is selected and 20 numerical points are divided for research. The slope values of the positive pulse and negative pulse transition feature points of 20 metal thicknesses are shown in Table 3.
[0042] Table 3 Metal thickness and slope value of transition characteristic point Metal thickness Positive pulse Negative pulse 0.01 2.1301 -12.1531 0.04 2.0633 -9.0703 0.08 1.9634 -3.3657 0.12 1.8313 -2.1582 0.16 1.6996 -1.9215 0.2 1.6504 -1.8693 0.25 1.6120 -1.6532 0.35 1.4344 -1.432 0.45 1.2964 -1.3749 0.5 1.2751 -1.3507 0.6 1.1189 -1.2629 0.7 1.0747 -1.2576 0.8 1.0133 -1.1241 1.0 0.9198 -0.9971 1.3 0.7607 -0.8263 1.5 0.7502 -0.8194 1.7 0.6843 -0.7676 2 0.6732 -0.487 2.5 0.6418 -0.366 3 0.6326 -0.2702 Step 2-2. Relational expression fitting The power function is used to fit the 20 metal thicknesses and their corresponding characteristic point slope values.
[0043] The relationship between the fitted metal thickness and the slope value of the characteristic point is expressed as follows: (2) In the formula f ( x ) is the slope value of the characteristic point of scheme 1, x Represents the metal thickness.
[0044] For the positive pulse response curve, A=1.435, B=-1.922, C=0.7115, D=-0.1446; For the negative pulse response curve, A=-13.48, B=-19.76, C=-1.578, D=-0.4752.
[0045] Step 2-3. Relational expression analysis From the analysis, it can be seen that the positive pulse fitting curve is better than the negative pulse fitting curve. Therefore, when using this method to measure metal thickness, it will be more accurate to use the positive pulse response transient process to measure metal thickness. The fitting effect evaluation data is shown in Table 4.
[0046] Table 4 Evaluation of the fitting effect of characteristic point slope and metal thickness of Scheme 1 Step 2-4. Measurement accuracy evaluation The above method was used to evaluate the metal with a thickness of 0.12 mm. The measured positive pulse stable magnetic flux was 0.00305693421008982, and the slope was 1.8313. Substituting it into the positive pulse fitting formula (2) of Scheme 1, the metal thickness was calculated to be 0.1213 mm. Therefore, the error between the actual value and the measured value is 1.08%.
[0047] Similarly, a metal with a thickness of 0.12 mm was selected for negative pulse analysis. The measured negative pulse stable magnetic flux was -0.00305693421008982, and the slope was -2.1582. Substituting it into the negative pulse fitting formula (2) of Scheme 1, the metal thickness was calculated to be 0.1402 mm. Therefore, the error between the actual value and the measured value is 16.8%.
[0048] In summary, the error value obtained by measuring the metal thickness using the transition characteristic points of the positive pulse transient process in Scheme 1 is much smaller than the error value obtained by measuring the metal thickness using the transition characteristic points of the negative pulse transient process in Scheme 1. Therefore, selecting the positive pulse response curve can effectively measure the metal thickness.
[0049] 3. Metal thickness measurement based on the stable value of dual probe pulse response (1) Implementation methods Under the action of a single probe, the greater the metal thickness, the more compact the steady-state value of the stable region of the response curve, so this method is only applicable to a small range of metal thickness. In order to solve the above problems, the original measurement is improved by adding another metal probe under the metal conductor as a signal receiving end to form a dual-probe structure, such as Figure 8 shown.
[0050] The specific steps of the metal thickness measurement process based on the stable value of the dual-probe pulse response are as follows: ① Set the excitation parameters and select the metal to be measured; ② The probe on one side passes a pulse signal to excite the metal, and the probe on the other end of the metal receives the impedance value of its coil; ③ Use the signal processing circuit to transform the impedance values at both ends of the coil to obtain the magnetic flux; ④ According to the magnetic flux response curve, obtain the stable value of the stable area under the action of the dual probes, such as Fig. 9 As shown; ⑤ According to the input-output fitting function, the stable value of the stable area under the action of the dual probes is input into the fitting function to solve the measured metal thickness.
[0051] (2) Implementation process Step 3-1. Determination of the stability value of the dual-probe stable region The metal thickness is selected to be between d=0~5mm and is subdivided into 20 values as shown in Table 5.
[0052] Table 5 Stability value and metal thickness in the stable area under the action of dual probes Step 3-2. Fitting the expression of the relationship between the two probes in the stable region The power function is used to fit 20 metal thicknesses and their corresponding stable values.
[0053] The fitting function formula of the stable value in the stable area based on the dual probe response - metal thickness is as follows: (3) In the formula, f ( x ) is the positive pulse stable magnetic flux value, x Represents the metal thickness.
[0054] For the positive pulse response curve, A=0.000186, B=-1.012, C=9.837×10 -5 , D = -0.3627; For the negative pulse response curve, A=-0.000186, B=-1.012, C=-9.837×10 -5 , D=-0.3627.
[0055] Step 3-3. Analysis of the expression of the relationship between the two probe stationary regions Between the metal thickness d = 0 ~ 5mm, there is an approximate relationship of formula (3). Therefore, the stable value of the negative pulse steady area based on the dual-probe pulse excitation response can be used to measure metals with a thickness of less than 5mm. Compared with the single-probe measurement method, not only the measurement range is increased, but also the displayed accuracy is higher and the relationship is clearer. The fitting effect of the positive pulse and negative pulse steady area stable values and metal thickness is evaluated, as shown in Table 6.
[0056] Table 6 Evaluation of the fitting effect of stable value in stable area and metal thickness It can be seen from Table 6 that the evaluation of the fitting effect of the stable value of the positive pulse stable region and the stable value of the negative pulse stable region and the fitting effect of the metal thickness are the same, so both positive pulse and negative pulse measurements can be selected.
[0057] Step 3-4. Metal thickness measurement accuracy evaluation Selecting a metal thickness of 0.3 mm and using the above method for evaluation, the measured positive pulse magnetic flux stability value is 0.00022509804; the negative pulse magnetic flux stability value is -0.00022509804. Substituting into formula (3), the metal thickness is 0.3001 mm. Therefore, the error between the actual value and the measured value is 0.033%.
[0058] Similarly, the metal thickness of 3mm is evaluated using the above method, and the measured positive pulse magnetic flux stability value is 0.00004250299; the negative pulse magnetic flux stability value is -0.00004250299. Substituting into formula (3), the metal thickness is 2.98mm, and the error between the actual value and the measured value is 0.0067%.
[0059] In summary, the stable values of the dual-probe positive pulse and negative pulse stable areas can be selected for metal thickness measurement.
[0060] The above description is only a preferred embodiment of the present invention, and does not limit the patent scope of the present invention. Any equivalent structural transformation made by using the contents of the present invention description and drawings, or directly or indirectly applied in other related technical fields, are also included in the patent protection scope of the present invention.
Claims
1. A method for measuring the thickness of a metal with a surface coating having a transient stable dual-state response, characterized in that: In this method, pulse current is used for excitation, and the coil magnetic flux shows positive and negative pulse responses. As the metal thickness increases, the rising speed of the positive pulse response and the falling speed of the negative pulse response will gradually decrease and stabilize, thereby realizing the measurement of metal thickness.
2. The method for measuring the thickness of metal with surface covering layer with temporary stable dual-state response according to claim 1 is characterized in that: The metal thickness measurement method with surface covering layer of transient and stable dual-state response is a metal thickness measurement method based on the steady-state value of pulse excitation response. The steady-state response of pulse current excitation is a metal thickness measurement characterization method. The steady-state value of pulse current excitation flux response is an intuitive reflection of the metal thickness of the measured object. The steady-state values of different metal thicknesses in the positive pulse stable area decrease with the increase of metal thickness, and the steady-state values in the negative pulse stable area increase with the increase of metal thickness.
3. The method for measuring the thickness of metal with surface covering layer with temporary stable dual-state response according to claim 2 is characterized in that: The metal thickness measurement method based on the steady-state value of pulse excitation response includes the following steps: Step 1-1. Determination of the steady-state value in the stable region, The steady-state value in the stable region of the magnetic flux response curve is used as a characteristic quantity to effectively measure the metal thickness. Therefore, under the action of pulse current excitation, before the next pulse comes, the value of the magnetic flux that is stable and unchanged is recorded as the steady-state value; Step 1-2. Steady-state value-metal thickness relationship expression, Use the power function to fit different metal thicknesses and the corresponding steady-state values in the stable region, and finally get the relationship expression: f ( x )=A x +B, where f ( x ) represents the stable magnetic flux value in the stable region, x Represents metal thickness; Step 1-3. Expression analysis, The steady-state value of the positive pulse stable area and the stable value of the negative pulse stable area are quantitatively compared and analyzed with the fitting relationship curve respectively; Step 1-4. Accuracy assessment, The steady-state values of the positive pulse and negative pulse plateau regions of the response signal of metal aluminum of known thickness under the excitation of the pulse signal are substituted into the fitting expression respectively to obtain its response value, which is then compared with the actual metal thickness to obtain the error.
4. The method for measuring the thickness of metal with surface covering layer with temporary stable dual-state response according to claim 3 is characterized in that: The metal thickness measurement method based on the steady-state value of pulse excitation response includes the following steps: Step 1-1. Determination of the steady-state value in the stable region, Under the same excitation parameters and external conditions, the steady-state values of the positive pulse and negative pulse stable regions corresponding to different metal thicknesses are calculated; Step 1-2. Steady-state value-metal thickness relationship expression, Use the power function to fit different metal thicknesses and the corresponding steady-state values in the stable region, and finally get the relationship expression: f ( x )=A x +B, where f ( x ) represents the stable magnetic flux value in the stable region, x Represents the metal thickness. For the positive pulse response curve, A=-1.107×10 -5 , B=0.003058, for the negative pulse response curve, A=1.107×10 -5 , B=-0.003058; Step 1-3. Expression analysis, The steady-state value in the positive pulse stable zone gradually decreases with the increase of thickness, and the steady-state value in the negative pulse stable zone gradually increases with the increase of thickness; Step 1-4. Accuracy assessment, The steady-state values of the positive pulse and negative pulse plateau regions of the response signal of metal aluminum with a thickness of 0.08 mm and 0.44 mm under the excitation of the pulse signal were substituted into the fitting expression, and the values were obtained to be 0.076 mm and 0.4414 mm respectively. Then, compared with the actual metal thickness, the errors were 3.75% and 0.32%.
5. The method for measuring the thickness of metal with surface covering layer with temporary stable dual-state response according to claim 1 is characterized in that: The metal thickness measurement method with surface covering layer of transient and stable dual-state response is a method of characterizing metal thickness based on the slope of transition characteristic points of pulse response transient process. The transient response of pulse current excitation is a unique attribute of the metal thickness measurement characterization method. The transient process of pulse current excitation flux response contains characteristic information of metal thickness. The slope of transition characteristic points extracted based on positive and negative pulses of the transient process decreases with the increase of metal thickness. The slope of transition characteristic points of flux response transient process is adopted to effectively measure different metal thicknesses.
6. The method for measuring the thickness of metal with surface covering layer with temporary stable dual-state response according to claim 5 is characterized in that: The method for characterizing metal thickness based on the slope of transition characteristic points of the pulse response transient process includes the following steps: Step 2-1. Determine the transition feature points. The transient process of pulse excitation response changes with the change of metal thickness, and the slope of transition characteristic point is used as the characteristic quantity of metal thickness measurement; Step 2-2. Fitting the relational expression, The exponential function is used to fit the different thicknesses of metals and the corresponding slopes of transition characteristic points. The fitted relationship expression is: f ( x )=Ae Bx +Ce Dx , where f ( x ) is the slope value of the transition feature point, x Represents metal thickness; Step 2-3. Relational expression analysis, The transition characteristic points extracted from the positive pulse transient process and the transition characteristic points extracted from the negative pulse transient process are quantitatively compared and analyzed with the fitting curves respectively; Step 2-4. Measurement accuracy evaluation, Select metal of known thickness, obtain the slope of the transition characteristic point based on the response curve under the excitation of the pulse signal, substitute it into the fitting expression, calculate the corresponding metal thickness, compare it with the actual metal thickness, and obtain the measurement error.
7. The method for measuring the thickness of metal with surface covering layer with temporary stable dual-state response according to claim 6 is characterized in that: The method for characterizing metal thickness based on the slope of transition characteristic points of the pulse response transient process includes the following steps: Step 2-1. Determine the transition feature points. Maximum stable value and time through the stable area t =0 intersection point y =-k x +Φ, and then intersect this straight line with the transition area of each metal thickness to obtain the transition characteristic point Q corresponding to the metal of different thickness, and then calculate the tangent slope of this characteristic point respectively. The transition characteristic point of the negative pulse transient process is obtained in the same way; Step 2-2. Fitting the relational expression, The exponential function is used to fit the different thicknesses of metals and the corresponding slopes of transition characteristic points. The fitted relationship expression is: f ( x )=Ae Bx +Ce Dx , where f ( x ) is the slope value of the transition feature point, x Represents the metal thickness. For the positive pulse response curve, A=1.435, B=-1.922, C=0.7115, D=-0.1446; for the negative pulse response curve, A=-13.48, B=-19.76, C=-1.578, D=-0.4752; Step 2-3. Relational expression analysis; Step 2-4. Measurement accuracy evaluation, The metal thickness is selected as 0.12mm. Based on the response curve under the excitation of the pulse signal, the slope of the transition characteristic point is obtained and substituted into the fitting expression. The metal thickness is calculated to be 0.1213mm and 0.1402mm. It is compared with the actual metal thickness to obtain the measurement error. The results show that the error value of the fitting function of the positive pulse metal thickness and the slope of the transition characteristic point is smaller than the fitting function of the negative pulse metal thickness and the slope of the transition characteristic point. Therefore, the slope of the transition characteristic point of the positive pulse transient process is selected to effectively measure the metal thickness.
8. The method for measuring the thickness of metal with surface covering layer with temporary stable dual-state response according to claim 1 is characterized in that: The metal thickness measurement method with surface covering layer with temporary stable dual-state response is a metal thickness measurement method based on the stable value of the stable area of the dual-probe pulse response. The stable value of the dual-probe pulse response also has the ability to measure metals of different thicknesses. The excitation probe is on one side of the metal, and the probe on the other side serves as the receiving end of the response signal. The stable value of the positive pulse of the magnetic flux response signal decreases significantly with the increase of the metal thickness, and the stable value of the negative pulse decreases significantly with the increase of the metal thickness.
9. The method for measuring the thickness of metal with surface covering layer with temporary stable dual-state response according to claim 8, characterized in that: The metal thickness measurement method based on the stable value of the dual-probe pulse response stable region is characterized by comprising the following steps: Step 3-1. Determination of the stability value of the dual-probe stable area, Based on the stable value of the stable area of the dual-probe magnetic flux response curve as the characteristic quantity characterization, the method of effectively measuring the thickness of different metals, controlling the pulse width, and reducing the pulse transient response time can obtain a relatively stable and unchanged magnetic flux stable value; Step 3-2. Fitting the expression of the relationship between the two probes in the stable region. Use exponential function to fit the metal thickness to the corresponding stable value of the dual probe stable area. f ( x )=Ae Bx +Ce Dx , where f ( x ) is the stable value of the receiving probe in the stable area, x is the metal thickness; Step 3-3. Analysis of the expression of the relationship between the two probe stable regions, The stability values of the positive pulse stable area and the negative pulse stable area of the dual probes were quantitatively compared and analyzed with the fitting curves. Step 3-4. Metal thickness measurement accuracy evaluation, The stable values of the positive pulse stable area and the negative pulse stable area obtained by measuring metal aluminum of known thickness are substituted into the fitting function respectively to obtain the corresponding thickness, which is then compared with the actual metal thickness to obtain the measurement error.
10. The method for measuring the thickness of metal with surface covering layer with temporary stable dual-state response according to claim 9, characterized in that: The metal thickness measurement method based on the stable value of the dual-probe pulse response stable region is characterized by comprising the following steps: Step 3-1. Determination of the stability value of the dual-probe stable area, Based on the stable value of the stable area of the dual-probe magnetic flux response curve as the characteristic quantity, the different metal thicknesses can be effectively measured. The excitation probe is on one side of the metal, and the probe on the other side is used as the receiving end of the response signal. The stable value of the positive pulse and negative pulse stable area corresponding to different metal thicknesses is obtained; Step 3-2. Fitting the expression of the relationship between the two probes in the stable region. Use exponential function to fit the metal thickness to the corresponding stable value of the dual probe stable area. f ( x )=Ae Bx +Ce Dx , where f ( x ) is the stable value of the receiving probe in the stable area, x is the metal thickness, positive pulse response curve, A=0.000186, B=-1.012, C=9.837×10 -5 , D=-0.3627, negative pulse response curve, A=-0.000186, B=-1.012, C=-9.837×10 -5 , D = -0.3627; Step 3-3. Analysis of the expression of the relationship between the two probe stable regions, The stability value of the dual probe positive pulse stable area gradually decreases with the increase of metal thickness, and the stability value of the negative pulse stable area gradually increases with the increase of metal thickness; Step 3-4. Metal thickness measurement accuracy evaluation, The stable values of the positive pulse stable area and the negative pulse stable area obtained when the thickness of metal aluminum is 0.3mm and 3mm are substituted into the fitting function respectively, and the obtained thickness is 0.3001mm and 2.98mm. They are compared with the actual metal thickness to obtain the measurement error. The results show that both the positive pulse and negative pulse stable areas can effectively realize the measurement of metal thickness.
Citation Information
Patent Citations
Metal layer pulsed eddy current thickness measurement method
CN105737728A
Pulsed eddy current detection method and device for detecting wall thickness of stainless steel tube
CN113310394A
Thickness measurement using pulsed eddy current system
CN114993155A
Ferromagnetic metal piece thickness detection method
CN115468479A
Metal identification method for rectangular pulse excitation magnetic flux response rising and falling edge characterization