Cosmetic sheet mask for improved product delivery

Microdenier fiber nonwoven fabric made of fibrillated two-component island fibers solves the problem that cosmetic sheet masks cannot effectively release products in a short period of time, and achieves rapid delivery and high-strength effects. Mass production and distribution.

CN118974337APending Publication Date: 2024-11-15ELC MANAGEMENT LLC
View PDF 9 Cites 0 Cited by

Patent Information

Application Number
CN202380030263.4
Authority / Receiving Office
CN · China
Patent Type
Applications(China)
Current Assignee / Owner
Priority Date
2022-03-01
Filing Date
2023-02-22
Publication Date
2024-11-15

AI Technical Summary

Technical Problem

Existing cosmetic sheet masks cannot effectively release sufficient doses of water-based products in a short period of time, and their strength and durability are insufficient to meet the needs of large-scale production and distribution, resulting in increased costs and waste.

Method used

Using microdenier fiber nonwoven fabrics made of fibrillated two-component island fibers, island fibers with controlled release rates are produced by hydraulic entanglement technology, combining the preferred jet strip spacing and fiber material ratio to form a high A fabric that is strong and capable of quickly releasing liquid products.

Benefits of technology

A local delivery system for rapid delivery of cosmetics or personal care products within 3 minutes to 5 minutes is achieved, while having sufficient strength and durability, suitable for large-scale production and use.

✦ Generated by Eureka AI based on patent content.
Patent Text Reader

Abstract

The nonwoven fabric can be made into a topical delivery system having increased and controlled product release rates while still having the strength and durability required for large scale production and dispensing. Such a release system comprises a fabric made of microdenier fibers, which are produced by fibrillating two-component sea-island fibers. Masks made from these fabrics can achieve sufficient product delivery within 3 minutes to 5 minutes or less.
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] The present invention relates to nonwoven fabrics, and their use as topical delivery systems for cosmetic and personal care products. More particularly, the present invention relates to sheet masks (including patches) made from nonwoven fabrics. Background Art

[0002] Cosmetic and personal care sheet masks are commonly used to deliver products to the face and other areas of the body. Typically, the retention duration recommended for sheet masks is 10 to 30 minutes. This time is needed to allow a significant dose of the product immersed in the mask to be transferred to the skin. Moreover, when the mask is on the skin, the user can experience a comfortable cooling sensation. However, having to wear a sheet mask (e.g., a facial mask) for 10 to 30 minutes may be inconvenient for busy consumers, who will benefit from getting the most from the sheet mask in a much shorter time. In addition, generally, the release rate of the product from a conventional sheet mask does not match the absorption rate of the skin. When the unabsorbed product is exposed to the ambient atmosphere, degradation occurs, such as evaporation loss. As a result, additional products are usually immersed in the mask to ensure that the user will receive enough doses. This increases costs and waste. Due to these and other reasons, there is still a need for a cosmetic sheet mask that can deliver a dose of an aqueous product in significantly less than 10 minutes. The rate at which the aqueous product is released from the sheet fabric depends primarily on the porosity of the fabric. Generally, if fiber density and / or fiber size is reduced, porosity (and release rate) will increase, but the integrity of the fabric made from these smaller fibers is compromised and may not have the desired strength and durability. Thus, one challenge addressed by the present invention is how to prepare a cosmetic sheet mask that has an increased and controllable release rate while still having the strength and durability required for large-scale production and distribution.

[0003] Different fabrics for making beauty sheet masks have different fluid handling properties, such as the amount of fluid preparations that fabrics can keep, the rate of release into the skin and evaporation losses. These properties also depend on the arrangement of the fibers (structures) in a given fabric. For example, cellulose fabrics (such as cotton and rayon) can absorb up to 8 times of their quality, while polyester (PET) fabrics may only keep one or two times of their quality. In cellulose fabrics, fluid resides in the space (holes) between fabric fibers, and resides in the holes of separate fibers. In polyester fabrics, fluid cannot penetrate into separate fibers, but only resides in the space (holes) between fibers.

[0004] Another type of fabric is a nonwoven fabric. A nonwoven fabric is an arrangement of fibers that are bound together by entanglement of the fibers in any of several ways, including mechanical, thermal and chemical ways. Nonwoven materials can be in the form of webs, pads, batts and sheets. The properties of nonwoven materials will depend in part on the raw material selection and the process of web forming, bonding and finishing. US3,338,992 is an example of an early attempt to produce a nonwoven web from continuous synthetic fibers. As used herein, "fiber" is a structure with a high aspect ratio (length / diameter). Although there is no universal consistency, we use the definition of "microfiber" as a material with a diameter of about 0.5μ to 5μ and a linear mass density of less than 1 denier (den) (where denier is defined as the number of grams of fiber per 9000 meters). Compared with microfibers, "nanofibers" are defined as having a diameter of less than about 0.5μ, a relatively high surface area to volume ratio and a high porosity. "Microdenier" fibers we refer to fibers less than 1 denier. "Staple fibers" refer to relatively short fibers of definite length, whereas "filament fibers" are longer, effectively continuous fibers having a very high aspect ratio.

[0005] There are a variety of techniques for producing the fibers that ultimately make up nonwoven fabrics. "Multicomponent fibers" are made from two or more materials (e.g., different synthetic polymers). Fabrics made from multicomponent fibers benefit from having properties from each individual fiber component. Alternatively, after producing multicomponent fibers, it is sometimes useful to separate the component fibers from each other for separate processing. Microdenier fibers are typically produced in this manner. Common separation techniques can be classified as mechanical or solvent-based (e.g., dissolving one type of fiber and leaving another, or swelling the fibers to separate them).

[0006] "Bicomponent fibers" consist of two polymers with different chemical and physical properties. Typically, the two polymers are coextruded from the same spinneret to form a single filament in which the two polymers are delineated along a fine interface. The parameters necessary to successfully process two different raw materials in this manner (e.g., viscosity of the polymer fluids, stretchability, compatibility with the spinning process) are known in the art. Several geometric arrangements of bicomponent fibers are common. Some of these are known in the art as side-by-side, segmented pie-shaped, segmented ribbon-shaped, segmented cross-shaped, pointed trilobal, side-by-side bow-tie, core-sheath, and island-in-the-sea. The present invention employs an island-in-the-sea fabric made by a specific technique.

[0007] Usually, the sea-island fiber comprises many small filaments of a polymer (island) placed in a matrix of another polymer (sea). US6,455,156 discloses a technology for preparing this type of bicomponent fiber. However, in this method, an alkaline solution must be used to dissolve the sea matrix to reach the island fibers (which are not adversely affected by the alkaline solution). The use of an environmentally unfriendly alkaline solution is a shortcoming of the method, and the polymer that can be used for the island component is also limited to those that are not adversely affected by the alkaline solution.

[0008] US7,981,226 and US8,420,556 (incorporated herein by reference in their entirety) disclose a method of making high strength, high surface area nonwoven fabrics from microdenier, island-in-the-sea fibers by fibrillating bicomponent fibers. As a result, the island component is released from the sea matrix. Typically, the sea component is weak enough that it can be fibrillated by hydroentanglement, and the island component and the sea component must have little or no affinity for each other; that is, they must be incompatible. Incompatibility is defined as "the two fiber components form a clear interface between them so that one does not diffuse into the other." However, as explained in '226 and '556, "The key feature of the present invention is that the sea fibers are entangled and intertwined with the island fibers upon fibrillation. Thus, while the island fibers can be made at the micron and nanometer levels, the sea component is also separated between the individual fibers that form the micron and nanometer fibers of the sea component. Thus, the sea fibers and the island fibers produce continuous micron and nanometer fibers from a single bicomponent fiber. Furthermore, they are able to entangle and intertwine within themselves, forming high strength fibers, while the fibers retain their structural integrity."

[0009] As further explained in US7,981,226 and US8,420,556, prior to fibrillation, the outer fibers wrap around the inner fibers, and as a result, the inner fibers solidify before the outer fibers solidify. This promotes very strong island fibers, which can then be separated from the sea fibers by fibrillation or other external energy. In this process, both the inner island fibers and the outer sea fibers remain as continuous fibers, and bonds are subsequently formed between the various fibers. "This promotes the high strength aspect of the present invention, even though the corresponding fibers themselves are at the micron and nanometer level."

[0010] US7,981,226 and US8,420,556 also disclose that it is preferred if the external energy for fibrillation is provided in the form of a hydroentanglement method by water jets. In order for it to work, both the internal island fibers and the external sea fibers must be insoluble in water. For this reason, if hydroentanglement is to be used or if the fiber is to be used for a fabric of a wet application, PVA cannot be used, which is a material commonly used in conventional sea-island fiber structures. Hydroentanglement is usually carried out on a web with bicomponent fibers, and microdenier fibers of about 0.5 microns or less can be produced. The filament fibers produced in this way can be incorporated into a nonwoven fabric that can be formed by spunbonding. Alternatively, staple fibers can be formed into a web and bonded by any of several known methods. The nonwoven fabric produced in this way is said to be used to make tents, parachutes, outdoor fabrics, house wraps, awnings, screening programs, rags, cleaning cloths and textiles. According to '226 and '556, the island fibers and sea fibers may comprise thermoplastic polymers such as nylon 6, nylon 6 / 6, nylon 6,6 / 6, nylon 6 / 10, nylon 6 / 11, nylon 6 / 12, polypropylene, polyethylene, polyester, copolyester, copolyetherester elastomer, polyolefin, polyacrylate, and thermoplastic liquid crystal polymer. In addition, the thermoplastic polymer may comprise a copolyetherester elastomer having long-chain etherester units and short-chain ester units bonded head-to-tail by ester bonds.

[0011] To the best of our knowledge, nonwoven fabrics such as those described below have never been used to produce cosmetic or personal care sheet masks that rapidly release product into the skin.

[0012] Purpose of the Invention

[0013] A primary object of the present invention is a topical delivery system, such as a cosmetic or personal care sheet mask, having an increased and controlled release rate while still having the strength and durability required for large scale production and distribution.

[0014] Another object of the present invention is to provide a topical delivery system, such as a cosmetic or personal care sheet mask, which can achieve adequate product release within 10 minutes or less, such as 3 minutes to 5 minutes or less. Summary of the invention

[0015] We describe nonwoven topical delivery systems for improved product delivery, such as cosmetic or personal care sheet masks. These topical delivery systems comprise fabrics made from microdenier fibers produced by fibrillating bicomponent island-in-the-sea fibers. Fibrillation is performed by hydroentanglement using jet bars, wherein the jet-to-jet spacing is in the range of 600μ to 2400μ. The materials and other relevant parameters of the fibers are selected to provide a durable topical delivery system with a controllable product release rate. DETAILED DESCRIPTION

[0016] We have found that certain fabrics made from microdenier fibers are particularly useful in the area of ​​topical delivery, particularly cosmetic sheet masks, for improved product delivery. We describe a customized island-in-the-sea process to produce fabrics with certain defined parameter values. Particularly advantageous combinations of polymer materials (island component / sea component) for the applications described herein include: polyamide 6 / polylactic acid; polyamide 6 / polyethylene; polypropylene / polylactic acid, but the invention is not limited to these combinations. In a preferred embodiment of the invention, the weight ratio of the island component polymer to the sea component polymer is between about 1:4 and about 1:6. For example, the island component polymer may constitute about 15% to 20% by weight of the bicomponent fiber, while the sea component constitutes 80% to 85% by weight. Our observation is that masks made from such fabrics are superior in topical delivery of fluid products. This is especially true when the hydroentanglement step is performed using a preferred jet-to-jet spacing. The preferred jet-to-jet spacing is in the range of about 600μ to 2400μ, with a water pressure of 10 bar to 1,000 bar. If the jet-to-jet spacing is less than about 600 μ, the resulting fabric is too thin and too dense to effectively release the liquid product, so that a full dose of the product cannot be delivered in less than 10 minutes. On the other hand, if the jet spacing is greater than about 2400 μ, the fibers may separate, causing the fabric to lose mechanical integrity. Using the preferred island-to-sea ratio and the preferred jet-to-jet spacing, we have noted a "sweet spot" where the fabric maintains sufficient mechanical integrity for the applications contemplated herein while still being able to effectively release the liquid product. The basis weight of the fabric produced within this sweet spot is about 30 g / m 2 Up to 100g / m 2 , preferably about 80g / m 2 Up to 100g / m 2 Nonwoven fabrics made in accordance with the present invention also have a unique "quilted" structure that provides a visual distinction from fabrics made by other methods.

[0017] Also important is the fiber packing density (also known as the solid volume fraction). The fiber packing density is the ratio of the volume occupied by the fibers to the volume of the fabric. Preferred fabrics of the present invention have a fiber packing density of about 5% to 30%, meaning that most of the sheet is empty space. However, when all other parameters are as specified herein, the resulting fabric is sufficiently strong and durable for the applications contemplated herein.

[0018] When applied as a cosmetic sheet mask, in order to deliver the liquid composition to the skin surface, the mask is impregnated with the liquid composition. Given the packing density specified above, the weight of the liquid composition that can be impregnated into the mask is generally in the range of 2 to 8 times the weight of the mask. At the same time, the specified packing density enables the product to be quickly transferred to the target surface. Therefore, we are able to produce a cosmetic sheet mask that delivers a dose of product to the target surface in 3 minutes to 5 minutes or less. As mentioned above, for cosmetic sheet masks currently on the market, it is not uncommon to suggest that the retention duration is 10 minutes to 30 minutes. This is the amount of time required to transfer the entire dose of product to the skin surface. On the contrary, we have found that, using the parameters specified herein, a cosmetic sheet mask made of a sea island nonwoven fabric can achieve similar or superior results in 3 minutes to 5 minutes (preferably as little as 3 minutes), while achieving the strength and durability required for large-scale production, distribution and use of the mask.

[0019] Optionally, one or both of the island component and the sea component can be made of sustainable materials. Examples of available sustainable materials include: polyvinyl alcohol, polybutylene succinate, recycled polyethylene, recycled polypropylene, recycled polyester or copolyester. Optionally, one or both of the island component and the sea component can be made of bio-based materials rather than fossil-derived materials. Such materials include, for example, polyethylene derived from sugar cane and polyamide derived from castor oil. Fabrics made from bio-based materials (especially disposable items, such as cosmetic sheet masks) are generally better for the environment and long-term sustainability.

[0020] According to the present invention, the cosmetic sheet mask (including patch) can be prepared by impregnating the sea-island nonwoven fabric with one or more skin care preparations for treating the skin. According to the above-mentioned filling density, the total weight of one or more preparations that can be impregnated into the sheet mask is generally in the range of 2 to 8 times the weight of the mask. The impregnation sheet mask can be completed by any suitable means known in the art. Such a cosmetic sheet mask can be used to treat various skin conditions. The sheet mask can be configured to conform to the predetermined treatment area of ​​the user's skin, such as the face, neck, abdomen or limbs or any part thereof. For example, a complete mask generally extends from the hairline of the forehead to the chin, and extends from the ear to the ear, and is provided with holes for the eyes, nose and mouth. Partial masks can be shaped to be applied to the area under the eyes, or to the side areas of the eyes that produce crow's feet, around the mouth that produces frown lines, or the T-zone of the nose. The exact size and shape of the cosmetic sheet will depend on the intended use and product characteristics. The cosmetic sheet will have sufficient flexibility, and its size and shape are suitable for being consistent with the desired treatment area of ​​the user's skin. When the sheet masks are applied to the skin and conform to the contours of the skin, they can deliver to the skin a predetermined dose of one or more skin care formulations for treating the skin.

[0021] The preparation may include one or more skin benefit agents. Skin benefit agents may be selected from: anti-wrinkle or skin firming agents; anti-aging agents; moisturizers; skin whitening or depigmentation agents; anti-inflammatory agents; anti-acne agents; DNA repair agents; skin lipid barrier repair agents; anti-cellulite agents; wound healing agents; stretch marks / scar removers; swelling agents; hair growth blockers; hair growth stimulators; dark circles reduction or detumescence agents; collagen synthesis or blood circulation enhancers; antioxidants; sebum control agents; and pore minimizing agents. Skin benefit agents may be charged or neutral. Exemplary anti-wrinkle agents include, but are not limited to, acetyl hexapeptide-8, palmitoyl oligopeptides, dipeptide diaminobutyryl, benzylamide diacetate, etc. Exemplary skin firming agents include, but are not limited to, algae extracts, pullulan, sweet almond seed extracts, carbomers, palmitoyl oligopeptides, palmitoyl tetrapeptide-7, Quercus suber extracts, etc. Exemplary anti-aging agents include, but are not limited to, teprenone, trisodium resveratrol triphosphate, Polygonum cuspidatum root extract, whey protein, and the like. Exemplary moisturizers include, but are not limited to, hyaluronic acid, glycerol, urea, trehalose, and the like. Exemplary skin whitening or depigmenting agents include, but are not limited to, ascorbic acid, magnesium ascorbyl phosphate, aminopropyl ascorbyl phosphate, mulberry root extract, Scutellaria baicalensis extract, grape extract, ferulic acid, hinokitiol, and the like. Exemplary anti-inflammatory agents include, but are not limited to, Selaginella extract, fur seal whip extract, Polygonum cuspidatum root extract, and the like. Exemplary anti-acne agents include, but are not limited to, salicylic acid, glycolic acid, lactobionic acid, and the like. Exemplary DNA repair agents include, but are not limited to, C1-C8 alkyl tetrahydroxycyclohexanoate, micrococcal lysate, bifid yeast fermentation lysate, and the like. Exemplary skin lipid barrier repair agents include, but are not limited to, phytosphingosine, linoleic acid, cholesterol, and the like. Exemplary anti-cellulite agents include, but are not limited to, Coleus forskohlii root extract, Magnolia grandiflora bark extract, Nelubo nucifera leaf extract, and the like. Exemplary wound healing agents include, but are not limited to, Mimosa tenuiflora bark extract, soy protein, and the like. Exemplary bulking agents include, but are not limited to, yeast / Acetobacter xylinum black tea ferment, Anemarrhena asphodeloides root extract, sodium hyaluronate, and the like. Exemplary hair growth retardants include, but are not limited to, ursolic acid, phytosphingosine, Boswella serrata extract, and the like. Exemplary hair growth stimulants include, but are not limited to, Serenoa serrulata fruit extract, licorice extract, acetylglucosamine, and the like.Exemplary dark circle reducing or de-puffing agents include, but are not limited to, hesperidin methyl chalcone, dipeptide-2, Passiflora incarnate flower extract, linoleic acid, isolinoleic acid, etc. Exemplary collagen synthesis or blood circulation enhancers include, but are not limited to, arginine, Ascophyllum nodosum extract, Asparagopsis armata extract, caffeine, etc. Exemplary antioxidants include, but are not limited to, nordihydroguaiaretic acid, grape seed extract, green tea leaf extract, etc.

Claims

1. An island-in-the-sea nonwoven fabric made of bicomponent island-in-the-sea fibers, wherein: The bicomponent island fiber comprises: island fibers made of a first polymer material; a sea fiber made from a second polymeric material; and The sea fibers and the island fibers are entangled by water jets, wherein the spacing between the jets is 600μ to 2400μ.

2. The sea-island nonwoven fabric according to claim 1, wherein: The first polymer material is polyamide 6, and the second polymer material is polylactic acid, or The first polymer material is polyamide 6 and the second polymer material is polyethylene, or The first polymer material is polypropylene and the second polymer material is polylactic acid.

3. The sea-island nonwoven fabric according to claim 1, wherein: The first polymeric material, the second polymeric material, or both are selected from the group consisting of polyvinyl alcohol, polybutylene succinate, recycled polyethylene, recycled polypropylene, recycled polyester, copolyester, polyethylene derived from sugar cane, and polyamide derived from castor oil. 4 . The island-in-the-sea nonwoven fabric of claim 1 , wherein a weight ratio of the first polymer material to the second polymer material is between 1:4 and 1:

6. The sea-island nonwoven fabric according to claim 1 , wherein the fiber filling density of the nonwoven fabric is 5% to 30%.

6. The sea-island nonwoven fabric of claim 1, wherein the island fibers and the sea fibers are microdenier fibers, and the basis weight of the fabric is 30 g / m 2 Up to 100g / m 2 .

7. A sheet mask for delivering a liquid composition to a skin surface, the sheet mask comprising an island-in-the-sea nonwoven fabric made of bicomponent island-in-the-sea fibers, wherein: The bicomponent island fiber comprises: island fibers made of a first polymer material; a sea fiber made from a second polymeric material; and Entangling the sea fibers and the island fibers by water jets; The nonwoven fabric is impregnated with the liquid composition. 8 . The sheet mask according to claim 7 , wherein the water jetting is performed with a jet-to-jet interval of 600 μ to 2400 μ.

9. The sheet mask of claim 7, wherein the nonwoven fabric is configured to conform to a predetermined treatment area of ​​a user's skin, such as the face, neck, abdomen, limbs, or any portion thereof. 10 . The sheet mask according to claim 9 , wherein the weight of the liquid composition in the nonwoven fabric is 2 to 8 times the weight of the nonwoven fabric.

11. The sheet mask according to claim 9, which is configured as a complete facial mask.

Citation Information

Patent Citations

  • Process for forming non-woven filamentary structures from fiber-forming synthetic organic polymers

    US3338992A

  • Hollow fibers and manufacturing method of hollow fibers

    US6455156B2

  • High strength, durable micro and nano-fiber fabrics produced by fibrillating bicomponent islands in the sea fibers

    US7981226B2

  • High strength, durable micro and nano-fiber fabrics produced by fibrillating bicomponent islands in the sea fibers

    US8420556B2

  • Non-woven fabric for cosmetics

    CN111719241A