Control method for improving number and quality of direct steel grade continuous casting and continuous casting furnaces
By optimizing the plug rod and water outlet materials, and improving the number and quality of continuous casting furnaces for straight steel, the problems of unstable oxygen content and unstable flow control of molten steel are solved, and more efficient continuous casting production and higher quality steel billets are achieved Production.
Patent Information
- Application Number
- CN202410986126.4
- Authority / Receiving Office
- CN · China
- Patent Type
- Applications(China)
- Current Assignee / Owner
- Filing Date
- 2024-07-23
- Publication Date
- 2024-11-19
- Estimated Expiration
- 2044-07-23
AI Technical Summary
In the process of continuous casting and pouring of straight steel seeds, the oxygen content of the steel is unstable, resulting in large erosion of the plug rod and unstable flow control, with few continuous pouring furnaces, and it is difficult to effectively control the temperature and composition, which affects product quality and competition. force.
By optimizing the plug rod head and water outlet materials, using corrosion-resistant reinforced plug rods and corrosion-resistant extended external immersion water outlets, the material's oxidation resistance and corrosion resistance are improved, the inner diameter of the intermixed water outlet is reduced, and the flow control ability is enhanced.
It effectively increases the number of continuous casting furnaces, reduces the amount of waste billets, improves the purity of the steel water and the quality of the billets, extends the pouring time, and reduces the possibility of fluctuations in the liquid level of the steel water and fluctuations in the rolling slag.
Smart Images

Figure CN118976891A_ABST
Abstract
Description
Technical Field
[0001] The invention relates to a control method for improving the number and quality of continuous casting furnaces, and in particular to a control method for improving the number and quality of continuous casting furnaces for straight-up steel grades, and belongs to the field of steel production. Background Art
[0002] As competition in the steel industry becomes increasingly fierce, reducing processes and increasing cost-efficiency have become key issues that all steel mills need to address.
[0003] The continuous casting machine with large section such as 250*350 adopts the refining process to produce Q195 steel strip, Q195-1, Q235B-2, ball flat A and other steel grades. The molten steel treatment cycle is long, and the refining power consumption and refractory cost are high. The continuous casting machine with small section of 150*150 adopts the refining and light treatment process to produce HRB400-9, HRB500E-2 and other nuclear power rebar varieties. The overall cost is high, which affects the competitiveness of the products.
[0004] However, low-carbon steel grades such as Q195 steel strip are produced using the direct-casting process, and the oxygen content in the molten steel is unstable: when the oxygen content is high, the stopper rod is severely eroded during the pouring process, the flow control is unstable, and the number of continuous casting furnaces is small; when the oxygen content is low, aluminum inclusions cannot float up effectively, the molten steel level fluctuates greatly during the pouring process, and many castings are scrapped.
[0005] HRB400-9 and other nuclear power rebars have high C, Si and Mn contents, large amounts of alloy additions and narrow Ceq requirements. The direct-acting process cannot achieve stable control of temperature and composition, and an urgent problem needs to be solved on site.
[0006] At present, patent CN108570532B discloses a method for improving the quality of straight-up steel grades and the flow control time of stopper rods. The method controls the reasonable oxygen level of molten steel by optimizing the deoxidation system of converter steel-making, and does not require refining to obtain an oxygen level below 40ppm. At the same time, the flow control time of stopper rods is extended to reduce scrap billets due to liquid level fluctuations during the pouring process, and reduce the occurrence of flow stoppage accidents caused by loss of control of stopper rods. It does not involve improvements in the size of stopper rods and nozzle materials to solve the problem of improving the number and quality of continuous casting furnaces for straight-up steel grades.
[0007] Therefore, developing a control method for increasing the number and quality of continuous casting furnaces for straight-up steel grades that can overcome the above defects has become a technical problem that needs to be urgently solved by technical personnel in this field. Summary of the invention
[0008] The technical problem to be solved by the present invention is to overcome the shortcomings of the prior art and provide a control method for improving the number and quality of continuous casting furnaces for straight-up steel grades. The corrosion resistance is enhanced by optimizing the plug rod head and nozzle materials. The control method effectively increases the number of continuous casting furnaces and reduces the amount of waste billets.
[0009] In order to solve the above technical problems, the present invention provides a control method for improving the number and quality of continuous casting furnaces for straight-up steel grades, which specifically includes the following steps: (1) The continuous casting tundish pouring adopts a corrosion-resistant reinforced stopper rod, and the rod head material of the corrosion-resistant reinforced stopper rod includes the following components by mass percentage: FC: 8-12%, MgO: 10-14%, the balance is Al2O3, the sum of the above components is 100%; (2) Reduce the inner diameter of the tundish water inlet for continuous casting and control it to φ25mm; (3) An anti-corrosion extended external immersed nozzle is used, the length of the nozzle is controlled at 740±3 mm, the slag line wall thickness is 30 mm, and the slag line material includes the following components by mass percentage: ZrO2: 75-83%, FC: 10-16%, Al2O3: 6-15%, and the sum of the above components is 100%.
[0010] The technical solution further defined in the present invention is: Furthermore, in the aforementioned control method for improving the number and quality of continuous casting furnaces for straight-up steel grades, the bulk density of the rod head is 2.65 g / cm 3 , porosity 16%, compressive strength 30.2MPa, flexural strength 8.5MPa.
[0011] In the aforementioned control method for improving the number and quality of continuous casting furnaces for straight-up steel grades, the rod head material of the corrosion-resistant reinforced stopper rod includes the following components by mass percentage: FC: 11.8%, MgO: 12.1%, the balance is Al2O3: 76.1%.
[0012] In the aforementioned control method for improving the number and quality of continuous casting furnaces for straight-up steel grades, the slag line material includes the following components by mass percentage: ZrO2: 78%, FC: 14%, Al2O3: 8%, and the sum of the above components is 100%.
[0013] The beneficial effects of the present invention are: The present invention improves the inner diameter of the tundish water inlet from φ30mm to φ25mm, thereby improving the flow control capability.
[0014] The present invention improves the rod head material of the stopper rod, improves the oxidation resistance and corrosion resistance, reduces the processing allowance when processing the stopper rod, and the processing allowance is 8-12mm (the ultimate goal is 0mm), and the processing accuracy can reach 1mm (the ultimate goal is 0mm, that is, no processing), reduces the secondary damage during the processing of the stopper rod, ensures the integrity of the rod head mud particles, and improves the oxidation resistance and corrosion resistance; the tundish water nozzle improves the flow control ability, and the external immersion water nozzle improves the corrosion resistance and life. The overall effect can effectively increase the number of continuous casting furnaces and reduce the amount of waste billets. The present invention optimizes the material of the rod head and the water nozzle to enhance the corrosion resistance. The corrosion resistance of the refractory material is enhanced, the pouring time will be extended, and the number of continuous casting furnaces is also increased; the erosion of the refractory material by the molten steel is reduced, and the refractory dispersion brought into the molten steel is also reduced, thereby improving the quality level of the molten steel purity, etc.; the inner diameter of the tundish water nozzle is reduced to enhance the flow control ability, reduce the fluctuation of the molten steel liquid level, thereby reducing the amount of waste billets caused by excessive liquid level fluctuations, and at the same time, the possibility of fluctuation slag is reduced, thereby improving the internal quality of the billet. BRIEF DESCRIPTION OF THE DRAWINGS
[0015] Figure 1 is a flow chart of an embodiment of the present invention; Figure 2 Schematic diagram of the structure of the corrosion-resistant reinforced stopper rod used in the embodiment of the present invention; Figure 3 It is a schematic structural diagram of the corrosion-resistant extended external immersed water inlet used in an embodiment of the present invention. DETAILED DESCRIPTION Example 1
[0016] This embodiment provides a control method for improving the number and quality of continuous casting furnaces for straight-up steel grades, the process is as follows Figure 1 As shown, the specific steps include: (1) The continuous casting tundish pouring adopts corrosion-resistant reinforced stopper rods such as Figure 2 The specific components and properties of the rod head of the stopper rod are shown in Table 1; Table 1 Parameters of the plug rod head It can be seen from Table 1 that the rod head made of this material can effectively improve the compressive strength and flexural strength of the rod head material and improve the corrosion resistance to molten steel; compared with the prior art, the content of MgO is reduced and the content of Al2O3 is increased. At high temperatures, Al2O3 has higher compressive strength and flexural strength. For example, the compressive strength of the micro-expansion castable with an Al2O3 content of 68% at 1400°C reaches 60MPa, and the flexural strength reaches 9Mpa. In contrast, the compressive strength and flexural strength of MgO are lower. For example, the melting point of pure magnesium oxide is 2800°C, but its compressive strength and flexural strength are much lower than those of Al2O3, which indicates that its structural stability at high temperatures is poor. These data show that under the same temperature conditions, Al2O3 exhibits higher compressive strength and flexural strength, which is due to its higher chemical stability and crystal structure strength.
[0017] (2) Reduce the inner diameter of the tundish water inlet from φ30 mm to φ25 mm; (3) Use erosion-resistant extended external submerged nozzles such as Figure 3 As shown, the length of the nozzle is controlled at 740±3 mm, the slag line wall thickness is 30 mm, and the slag line material includes the following components by mass percentage: ZrO2: 78%, FC: 14%, Al2O3: 8%.
[0018] The total design length is extended from 710mm to 740±3mm, the slag line wall thickness is increased by 5mm, the ZrO2 content of the slag line in the external submerged nozzle is increased by 3-5%, the material has enhanced corrosion resistance, double slag line operation is adopted during production, the number of continuous casting furnaces is increased, and the amount of waste billets in the water change nozzle is reduced.
[0019] The number of continuous casting furnaces and the amount of waste billets after adopting the above method are shown in Table 2; Table 2 Data on the number of continuous casting furnaces and the amount of waste billets before and after improvement It can be seen from Table 2 that the number of continuous casting furnaces for large-section straight-up steel grades such as 250*300 Q195 steel strips increased from 12 furnaces / group to 17 furnaces / group; the number of continuous casting furnaces for small-section straight-up steel grades such as 150*150 increased from 21 furnaces / group to 25 furnaces / group; the amount of scrap billets for large-section straight-up steel grades such as 250*300 Q195 was reduced to 6.57 tons / group, a decrease of 11.56 tons / group compared with before the improvement; the amount of scrap billets for small-section straight-up steel grades such as 150*150 was reduced to 2.98 tons / group, a decrease of 9.98 tons / group compared with before the improvement.
[0020] In addition to the above embodiments, the present invention may also have other implementation modes. Any technical solution formed by equivalent replacement or equivalent transformation falls within the protection scope required by the present invention.
Claims
1. A control method for improving the number and quality of continuous casting furnaces for straight-up steel grades, characterized in that: The specific steps include: (1) The continuous casting tundish pouring adopts a corrosion-resistant reinforced stopper rod, and the rod head material of the corrosion-resistant reinforced stopper rod includes the following components by mass percentage: FC: 8-12%, MgO: 10-14%, the balance is Al2O3, the sum of the above components is 100%; (2) Reduce the inner diameter of the tundish water inlet for continuous casting and control it to φ25mm; (3) Use an anti-corrosion extended external submerged nozzle, the length of which is controlled at 740±3mm, and the slag line wall thickness is 30mm; The slag line material comprises the following components by mass percentage: ZrO2: 75-83%, FC: 10-16%, Al2O3: 6-15%, and the sum of the above components is 100%.
2. The control method for improving the number and quality of continuous casting furnaces for straight-up steel grades according to claim 1 is characterized in that: The rod head material of the corrosion-resistant reinforced stopper rod comprises the following components by mass percentage: FC: 11.8%, MgO: 12.1%, the balance is Al2O3: 76.1%.
3. The control method for improving the number and quality of continuous casting furnaces for straight-up steel grades according to claim 1 is characterized in that: The volume density of the rod head is 2.65 g / cm 3 , porosity 16%, compressive strength 30.2MPa, flexural strength 8.5MPa.
4. The control method for improving the number and quality of continuous casting furnaces for straight-up steel grades according to claim 1 is characterized in that: The slag line material includes the following components by mass percentage: ZrO2: 78%, FC: 14%, Al2O3: 8%, and the sum of the above components is 100%.
Citation Information
Patent Citations
Stopper, tundish and method for removing inclusions in liquid metal
CN112024865A
Stopper rod for continuous casting of high-oxygen steel
CN113526965A
Alumina-magnesia graphite type refractory
CN1291177A
Cited By
Method for reducing erosion of stopper rod in pure iron continuous casting production
CN119910172A
Production method of HYT2 conductive steel
CN121223023A