Preparation method of perylene-based composite material and application of perylene-based composite material in electrochemical luminescence detection of glucose
By modifying the electrode with perylene-based composite TAPB COF, the problem of insufficient sensitivity and stability of the electrochemiluminescence detection method is solved, and electrochemiluminescence detection with high sensitivity and stability is achieved, with good application prospects.
Patent Information
- Application Number
- CN202411047049.2
- Authority / Receiving Office
- CN · China
- Patent Type
- Applications(China)
- Current Assignee / Owner
- Filing Date
- 2024-08-01
- Publication Date
- 2024-11-19
- Estimated Expiration
- 2044-08-01
AI Technical Summary
The existing electrochemiluminescence detection methods are insufficient in sensitivity and stability, making it difficult to achieve efficient and reliable glucose detection.
The electrode is modified by perylene-3,4,9,10-tetracarboxylic dianhydride and 1,3,5-tris(4-aminophenyl)benzene under specific conditions to form The catalyst was mixed with Nafion solution and coated on a glass carbon electrode for electrochemiluminescence detection of glucose.
High sensitivity and stability were achieved, the linear calibration curve correlation coefficient for detecting glucose was 0.993, the detection limit was 1.87×10-5μM, and the relative standard deviation was 3.4%. The system had good ECL stability and reproducibility.
Smart Images

Figure CN118978697A_ABST
Abstract
Description
Technical Field
[0001] The patent of this invention belongs to the field of electroluminescence, and relates to a method for preparing a perylene-based composite material and its application in electrochemiluminescence detection of glucose. Background Art
[0002] Glucose (Glu) is an important nutrient for human metabolism. Many chronic diseases such as cardiovascular disease, hyperglycemia, obesity, and diabetes are closely related to Glu. Therefore, it is necessary to establish a highly sensitive method for detecting Glu in the human body. At present, the methods for determining Glu include fluorescence analysis, colorimetry, flow injection analysis, electrochemiluminescence (ECL), etc. Among them, ECL is one of the most widely used blood glucose detection technologies due to its advantages such as fast response speed, high reliability, and high sensitivity, and has broad application prospects. Electrochemiluminescence combines the advantages of electrochemistry and spectroscopy, and generates light signals in an electrochemical manner through the redox reaction of the luminophore. This technology has been widely used in single-molecule electrochemical reaction imaging, medical diagnosis, environmental monitoring and evaluation, immunoassay, and drug analysis. Luminol has the advantages of non-toxicity and high luminescence efficiency, and is one of the most classic and common ECL luminescent materials. Excited 3-aminophthalate is the main emission of luminol ECL, which can be produced by using a variety of reactants, including superoxide radicals, hypobromite, or hydrogen peroxide. To date, most conventional luminol-H2O2 ECL systems use H2O2 as a classic co-reactant to generate reactive oxygen species (ROS), which react with electrochemically oxidized luminol anions and exhibit significant anodic emission. The present invention uses a novel TAPB polymer as an effective co-reactant luminol electroluminescence to establish a new method for detecting Glu. Summary of the invention
[0003] The purpose of the present invention is to provide a method for preparing a perylene-based composite material TAPB COF modified electrode with readily available raw materials, simple preparation method, high catalytic efficiency and good selectivity, and its application in electrochemiluminescence detection of Glu.
[0004] The technical scheme adopted by the present invention is: a perylene-based composite material, and the preparation method comprises the following steps: mixing perylene-3,4,9,10-tetracarboxylic dianhydride PTCDA and imidazole in DMF, stirring, adding 1,3,5-tri(4-aminophenyl)benzene TAPB dissolved in DMF dropwise, reacting after the dropwise addition is completed, cooling to room temperature and adding methanol, collecting precipitates by filtering, washing with DMF and methanol, drying the powder, removing residual imidazole, and obtaining a deep red powder.
[0005] The above-mentioned perylene-based composite material is stirred at 180°C.
[0006] The above-mentioned perylene-based composite material is reacted at 190° C. for 72 hours.
[0007] The above-mentioned perylene-based composite material has a molar ratio of perylene-3,4,9,10-tetracarboxylic dianhydride to 1,3,5-tri(4-aminophenyl)benzene=3:2.
[0008] In the above-mentioned perylene-based composite material, the residual imidazole is removed by refluxing methanol at 80°C.
[0009] A perylene-based composite material modified electrode is prepared by dissolving the perylene-based composite material in ethanol, ultrasonically oscillating, then mixing with a Nafion ethanol solution, ultrasonically dispersing the mixture uniformly, and evenly coating 5.0 μL of the mixed solution on a treated glassy carbon electrode, and drying the surface to obtain a perylene-based composite material modified electrode.
[0010] The above-mentioned perylene-based composite material modified electrode has a volume ratio of ethanol solution of perylene-based composite material: ethanol solution of Nafion = 1:1, the concentration of the ethanol solution of perylene-based composite material is 1g / L, and the concentration of the ethanol solution of Nafion is 1%.
[0011] The above-mentioned perylene-based composite material modified electrode is used in the electrochemiluminescence detection of glucose.
[0012] The above application method is as follows: the above-mentioned perylene-based composite material modified electrode is used as the working electrode, the counter electrode is a platinum sheet electrode, the reference electrode uses an Ag / AgCl reference electrode, the electrolyte uses 100mM phosphate buffer, pH=9 PBS, and a constant O2 flow is introduced for 0.5h before the test. Electrochemical and ECL tests are performed at a scanning speed of 50mV / s in the voltage range of -1.0 to 0.3V and a 700V photomultiplier tube.
[0013] The beneficial effects of the present invention are:
[0014] 1. The present invention modifies the synthesized catalyst material on the glassy carbon electrode for catalytic reaction. The raw materials are simple and easy to obtain, and the synthesis operation is easy. Before ECL measurement, a constant O2 flow is passed through the electrolyte solution for 0.5h to achieve an oxygen-saturated atmosphere, thereby improving the efficiency of the electrocatalytic reaction.
[0015] 2. The catalyst material synthesized in the present invention is used for electrochemiluminescence detection of glucose. By fitting the variation of ECL intensity with Glu concentration, the linear calibration curve with a correlation coefficient of 0.993 and a detection limit of 1.87×10 -5 μM (S / N=3).
[0016] 3. The ECL luminescence intensity of the catalyst material synthesized by the present invention is very stable when continuously scanning 10 cycles of potential in the potential range of -1.2V to 0V in a PBS solution (pH=9) containing 100mM luminol. The relative standard deviation (RSD) is calculated to be 3.4%, indicating that the system has good ECL stability and reproducibility. The COF catalyst obtained by the present invention has good application prospects in the field of electrochemiluminescence detection of glucose. BRIEF DESCRIPTION OF THE DRAWINGS
[0017] Figure 1 This is the FT-IR image of the perylene-based composite material TAPB COF modified electrode prepared in Example 1.
[0018] Figure 2 1 is the XRD pattern of TAPB COF powder in the perylene-based composite material TAPB COF modified electrode prepared in Example 1.
[0019] Figure 3 It is the N2 adsorption-desorption test graph of the perylene-based composite material TAPB COF modified electrode in Example 1 and their corresponding pore size distribution graphs.
[0020] Figure 4 This is a comparison chart of the ECL intensity of the perylene-based composite material TAPB COF modified electrode in Example 2 in O2, air and N2 gas.
[0021] Figure 5 This is the stability curve of the luminol electrochemiluminescence system of the perylene-based composite material TAPB COF in Example 2 after 10 scans.
[0022] Figure 6 This is a comparison chart of the ECL intensity of the perylene-based composite material TAPB COF / GCE in Example 2 in Glu solutions of different concentrations.
[0023] Figure 7 is the ΔI and lgC in Example 2 Glu The linear-log plot of (ΔI=I0-I, where I0 and I are the ECL intensities in the absence and presence of Glu, respectively). DETAILED DESCRIPTION
[0024] Example 1 Preparation of perylene-based composite material TAPB COF modified electrode
[0025] (I) The preparation method is as follows:
[0026] 1) Pretreatment of glassy carbon electrode: Use 3μm Al2O3 powder to grind and polish the bare glassy carbon electrode to a mirror surface, then rinse the electrode from the side with distilled water, put it in a bottle with distilled water for 3 minutes, take it out and rinse it with distilled water. Blow dry the surface with nitrogen, and then use CV to scan at a scan rate of 0.03V / s in 15mL 1mmol / L potassium ferrocyanide solution. When the peak potential difference (ΔEp) between the oxidation peak and the reduction peak is 70-80mV, it is qualified, indicating that the cleanliness of the electrode is good. Rinse with water again, blow dry with nitrogen and set aside; if it is unqualified, polish it again and use CV characterization until the qualified potential difference is reached.
[0027] 2) Preparation of perylene-based composite material TAPB COF: 0.6 mmol perylene-3,4,9,10-tetracarboxylic dianhydride (PTCDA) was mixed with 20 g imidazole in DMF (17 mL) and stirred at 180°C. 0.4 mmol 1,3,5-tri(4-aminophenyl)benzene (TAPB) dissolved in 3 mL DMF was added dropwise for about 20 min. The above solution was reacted at 190°C for 72 h. The mixture was then cooled to room temperature and methanol was added. The precipitate was collected by filtration and washed with DMF and methanol. The dried powder was refluxed with methanol at 80°C to remove the residual imidazole to obtain a dark red powder.
[0028] 3) Preparation of working electrode: Dissolve 5.0 mg of TAPB COF powder obtained in step 2) in 5.0 mL of ethanol, ultrasonically vibrate for 1 h, and then mix with 1% Nafion ethanol solution at a volume ratio of 1:1, and then ultrasonicate for 15 min to evenly disperse the solution. Apply 5.0 μL of the mixed solution evenly on the treated glassy carbon electrode and wait for its surface to dry before use.
[0029] (II) Test results
[0030] Figure 1 FIG. 1 is the FTIR spectrum of the TAPB COF catalyst powder prepared in Example 1. The structure of TA-PBCOF was further analyzed and confirmed by infrared spectroscopy. Figure 1 Visible 1698cm -1 、1654cm -1 The asymmetric stretching vibration peak of the carbonyl group in the imide and the 1350 cm -1 The stretching vibration peak of CNC at 3338 cm appears in the infrared absorption curve of TAPB. -1 The -NH2 stretching vibration peak at α disappeared, indicating that TA-PB COF was successfully prepared. Figure 2The XRD spectrum of the TAPB COF catalyst powder prepared in Example 1 is compared with the spectrum of the raw material. In the newly synthesized TA-PB COF catalyst powder, the raw material peak disappears, and a (0 0 1) crystal plane appears at 20-30°, proving the generation of a new substance.
[0031] Example 2 Application of perylene-based composite material TAPB COF modified electrode in electrochemiluminescence detection of Glu
[0032] Test method: The prepared TAPB COF-modified glassy carbon electrode was used as the working electrode, the counter electrode was a platinum electrode, the reference electrode was an Ag / AgCl reference electrode, and the electrolyte was 100mM phosphate buffer (PBS with pH=9). A constant O2 flow was introduced for 0.5h before the test. Electrochemical and ECL tests were performed at a scanning speed of 50mV / s in the voltage range of -1.0 to 0.3V and under the condition of a 700V photomultiplier tube, to explore the effect of different concentrations of Glu on the electrochemiluminescence (ECL) intensity.
[0033] The specific surface area of TAPB COF was investigated by nitrogen adsorption test at 77K, such as Figure 3 As shown, TAPB COF exhibits type IV isotherm characteristics, and the BET surface area of TAPT COF is calculated to be 55.04 m 2 ·g -1 ,As can be seen from the inset, the pore size is about 20nm, indicating that the porosity of the material is increased, which is beneficial to the adsorption behavior.
[0034] Example 3 Electrochemiluminescence detection of TAPB COF modified electrode under different atmospheres
[0035] The ECL intensity of TAPB COF modified glassy carbon electrode in O2, air and N2 atmospheres is shown in Figure 2. Figure 4 As shown in the figure, under the condition of O2 saturation, the ECL intensity reached the strongest. This result proves that O2 is the key species of the electrocatalytic reaction, and its participation in the ORR reaction provides the necessary ROS for the oxidation of luminol, thereby maximizing the ECL signal.
[0036] Stability test such as Figure 5 As shown: First, a PBS solution (pH = 9) containing 100 mM luminol was added to the electrolytic cell, and then the ECL intensity was continuously scanned for 10 cycles in the potential range of -1.2 V to 0 V. The results showed that the ECL intensity was very stable. After calculation, the relative standard deviation (RSD) = 3.4%, indicating that the system has good ECL stability and reproducibility.
[0037] Example 4: Perylene-based composite material TAPB COF modified electrode for electrochemiluminescence detection of Glu
[0038] Depend on Figure 6 , Figure 7 It can be seen that with the change of Glu concentration, the ECL intensity on TA-PB COF / GCE changes, which can be expressed by the equation ΔI = 1045.4logC Glu +4615 describes (ΔI=I0-I, where I0 and I are the ECL intensities in the absence and presence of Glu, respectively). The ECL intensity decreases monotonically with increasing Glu concentration, and the correlation coefficient (R 2 ) was 0.993, which showed that there was a very strong linear correlation between ECL intensity and Glu concentration. In addition, the detection limit of Glu was 1.87×10 -5 μM, which is the lowest concentration measured at a signal-to-noise ratio (S / N) of 3.
[0039] When in use, evenly apply the mixed solution of TAPB COF powder, ethanol and Nafion on the treated glassy carbon electrode, and wait for its surface to dry before use. When performing quantitative analysis of Glu, optimizing experimental parameters is a key step to ensure accuracy and sensitivity. The optimization of experimental parameters includes but is not limited to electrode modification, temperature, pH value and electrolyte selection. After these parameters are optimized, the quantitative analysis capability can be evaluated by testing a series of DA solutions of different concentrations.
[0040] In summary, the perylene-based composite material TAPB COF modified electrode of the present invention has good sensitivity, selectivity, stability and reproducibility, and has excellent electrochemiluminescence performance, and has a relatively ideal development prospect in the field of electrochemiluminescence detection of glucose.
Claims
1. A perylene-based composite material, characterized in that: The preparation method comprises the following steps: mixing perylene-3,4,9,10-tetracarboxylic dianhydride PTCDA and imidazole in DMF, stirring, adding 1,3,5-tri(4-aminophenyl)benzene TAPB dissolved in DMF dropwise, reacting after the dropwise addition is completed, cooling to room temperature and adding methanol, collecting the precipitate by filtering, washing with DMF and methanol, drying the powder, removing the residual imidazole, and obtaining a dark red powder.
2. A perylene-based composite material according to claim 1, characterized in that: The stirring is carried out at 180°C.
3. A perylene-based composite material according to claim 1, characterized in that: The reaction was carried out at 190°C for 72 hours.
4. The perylene-based composite material according to claim 1, characterized in that: The molar ratio of perylene-3,4,9,10-tetracarboxylic dianhydride to 1,3,5-tri(4-aminophenyl)benzene is 3:
2.
5. The perylene-based composite material according to claim 1, characterized in that: The removal of residual imidazole is performed by refluxing methanol at 80°C to remove the residual imidazole.
6. A perylene-based composite material modified electrode, characterized in that: The preparation method is as follows: dissolve the perylene-based composite material described in any one of claims 1 to 5 in ethanol, ultrasonically oscillate, then mix with Nafion ethanol solution, ultrasonically disperse evenly, and evenly apply 5.0 μL of the mixed solution on the treated glassy carbon electrode, and after the surface is dried, obtain the perylene-based composite material modified electrode.
7. The perylene-based composite material modified electrode according to claim 6, characterized in that: In terms of volume ratio, the ethanol solution of the perylene-based composite material: the ethanol solution of Nafion = 1:1, the concentration of the ethanol solution of the perylene-based composite material is 1 g / L, and the concentration of the ethanol solution of Nafion is 1%.
8. Use of the perylene-based composite material modified electrode according to claim 6 in electrochemiluminescence detection of glucose.
9. The use according to claim 8, characterized in that: The method is as follows: the perylene-based composite material modified electrode described in claim 6 is used as the working electrode, the counter electrode is a platinum sheet electrode, the reference electrode is an Ag / AgCl reference electrode, the electrolyte is a 100mM phosphate buffer solution, PBS with a pH of 9, a constant O2 flow is introduced for 0.5h before the test, and electrochemical and ECL tests are performed at a scanning speed of 50mV / s in a voltage range of -1.0 to 0.3V and a 700V photomultiplier tube.
Citation Information
Patent Citations
Tubular covalent organic framework polyimide and preparation method and battery application thereof
CN109627441A
D-A type perylene conjugated polymer lithium ion battery positive electrode material with high rate performance and preparation method thereof
CN113501956A
Preparation method and application of polyimide COF material based on perylene tetracarboxylic dianhydride
CN116217931A
Cited By
Porous crystal polymer as well as preparation method and application thereof
CN119842067A