Monocrystalline silicon growth furnace and control method thereof

By setting a second housing cover and a protective gas connection pipe in a single crystal silicon growth furnace, isolating the volatile gas from the heating assembly, and combining the synchronous rotation of the housing and the lifting mechanism, the corrosion and structural complexity of the heating assembly are solved. It extends service life and improves crystallization quality.

CN118979305APending Publication Date: 2024-11-19ZHONGHUAN ADVANCED (XUZHOU) SEMICONDUCTOR MATERIALS CO LTD +1
View PDF 0 Cites 0 Cited by

Patent Information

Application Number
CN202411179472.8
Authority / Receiving Office
CN · China
Patent Type
Applications(China)
Current Assignee / Owner
Filing Date
2022-10-27
Publication Date
2024-11-19

AI Technical Summary

Technical Problem

In existing single crystal silicon growth furnaces, SiO gas and CO gas are in direct contact with the heating assembly, causing corrosion of the heating assembly, shortening its service life, and increasing the risk of contamination during crystal growth.

Method used

A single crystal silicon growth furnace is designed, and the crystal growth chamber is isolated from the heating assembly by providing a second housing cover and a protective gas connection tube to avoid contact with volatile gases. The heating assembly is arranged in the first housing and the second housing. The first drive mechanism realizes synchronous rotation of the housing and the lifting mechanism, simplifying the top structure.

Benefits of technology

It effectively extends the service life of the heating assembly, reduces contamination during crystal growth, improves crystal crystallization quality, and simplifies the complexity of the furnace top structure.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure CN118979305A_ABST
    Figure CN118979305A_ABST
Patent Text Reader

Abstract

The invention discloses a monocrystalline silicon growth furnace and a control method thereof.The monocrystalline silicon growth furnace comprises a first shell, a second shell, a crucible assembly, a heating assembly, a heat preservation assembly, a first driving mechanism, a crystal pulling mechanism and a shielding gas connecting pipe, the first shell is provided with a crystal growth chamber, a crystal pulling chamber and an isolation chamber, and the second shell covers the first shell; a mounting cavity is formed between the first shell and the second shell, the heating assembly is arranged in the mounting cavity, the heat preservation assembly is arranged in the mounting cavity and covers the heating assembly, the first driving mechanism is arranged at the bottom of the first shell to support and drive the first shell to rotate relative to the second shell, and an exhaust hole is formed in the first driving mechanism. The crystal lifting mechanism is fixedly arranged in the isolation chamber and is suitable for synchronously rotating along with the first shell; and the protective gas connecting pipe penetrates through the isolation chamber and is communicated to the crystal pulling chamber. According to the monocrystalline silicon growth furnace provided by the embodiment of the invention, the service life of the heating assembly can be prolonged, and the complexity of the top structure of the monocrystalline silicon growth furnace can be simplified.
Need to check novelty before this filing date? Find Prior Art

Description

[0001] This application is a divisional application of a patent application with an application date of October 27, 2022, application number 202211341782.6, and invention name “Single crystal silicon growth furnace and its control method”. Technical Field

[0002] The present invention relates to the technical field of crystal growth, and in particular to a single crystal silicon growth furnace and a control method thereof. Background Art

[0003] In the related art, in order to heat the silicon material in the crucible assembly, a heating assembly is usually arranged on the side of the crucible assembly. During the crystal growth process, SiO gas will volatilize from the surface of the melt and condense into particles when encountering the cold furnace wall. These particles may fall and pollute the melt. Therefore, during the crystal growth process, a protective gas such as argon needs to be introduced into the furnace from the top of the single crystal silicon growth furnace. Argon can take away SiO gas, and can also take away CO gas generated by the reaction of SiO and graphite elements to prevent CO from being integrated into the melt and polluting the crystal.

[0004] However, SiO gas and CO gas are in direct contact with the heating components. When these gases are discharged outward along with the protective gas, they will corrode the heating components, seriously affecting the service life of the side heating components. Summary of the invention

[0005] The present invention aims to solve at least one of the technical problems existing in the prior art. To this end, the present invention provides a single crystal silicon growth furnace, which can extend the service life of the heating component and simplify the complexity of the top structure of the single crystal silicon growth furnace.

[0006] The present invention also proposes a control method for a single crystal silicon growth furnace, and the control method is used to control the single crystal silicon growth furnace.

[0007] According to a first aspect of the present invention, a single crystal silicon growth furnace comprises: a first shell, wherein the first shell has a crystal growth chamber, a crystal pulling chamber and an isolation chamber, wherein the crystal pulling chamber is connected to the top side of the crystal growth chamber, and the isolation chamber is connected to the top side of the crystal pulling chamber; a second shell, wherein the second shell cover is arranged outside the first shell, and an installation cavity is formed between the second shell and the first shell; a crucible assembly, wherein the crucible assembly is arranged in the crystal growth chamber; a heating assembly, wherein the heating assembly is arranged in the installation cavity and is used to heat the crucible assembly; and a heat preservation assembly, wherein the heat preservation assembly is arranged in the installation cavity and the cover is arranged in the installation cavity. The invention relates to a heating component; a first driving mechanism, which is arranged at the bottom of the first shell to support and drive the first shell to rotate relative to the second shell, and an exhaust hole is formed on the first driving mechanism, and the gas in the crystal growth chamber is suitable for being discharged from the crystal growth chamber through the exhaust hole; a crystal pulling mechanism, which is fixedly arranged in the isolation chamber and is suitable for extending into the crystal pulling chamber for pulling crystals, and the crystal pulling mechanism is suitable for rotating synchronously with the first shell; a protective gas connecting pipe, which is passed through the isolation chamber and connected to the crystal pulling chamber.

[0008] According to the single crystal silicon growth furnace of the embodiment of the present invention, a second shell cover is arranged outside the first shell, a heating component is arranged between the first shell and the second shell, and a protective gas connecting pipe is connected to the first shell, so that the first shell separates the environmental space required for crystal growth from the space where the heating component is located, thereby preventing the volatile gas in the crystal growth chamber and the crystal pulling chamber from contacting the heating component and corroding the heating component, ensuring the normal operation of the heating component, and thus extending the service life of the heating component; and by arranging a first driving mechanism to realize the synchronous rotation of the first shell and the crystal pulling mechanism, thereby realizing the rotation of the crystal, it is convenient to simplify the complexity of the top structure of the single crystal silicon growth furnace.

[0009] In some embodiments, the first shell includes: a main body, the main body includes a first upper shell, a heat-conductive shell and a first lower shell arranged in sequence from top to bottom, the crystal pulling chamber is formed in the first upper shell, the heat-conductive shell, the first lower shell and parts of the first upper shell jointly define the crystal growth chamber, the heat-conductive shell is arranged around the crucible assembly and is located between the crucible assembly and the heating assembly, the heat-conductive shell is a carbon-carbon composite material, the upper end of the heating assembly is not higher than the upper end of the heat-conductive shell, and the lower end of the heating assembly is not lower than the lower end of the heat-conductive shell; an isolation cover, the isolation cover is an integral part with the first upper shell, the isolation cover covers the outer side of the first upper shell, and the bottom wall of the isolation cover is rotatably connected to the top wall of the second shell, and the isolation cover and the first upper shell define the isolation chamber separated from the external space.

[0010] In some embodiments, the single crystal silicon growth furnace also includes: a cooling component, a connecting chamber is provided between the crystal growth chamber and the crystal pulling chamber to connect the crystal growth chamber and the crystal pulling chamber, and the cooling component is integrally formed on the cavity wall of the connecting chamber and extends downward into the crystal growth chamber for cooling the crystal.

[0011] In some embodiments, a first liquid inlet channel and a first liquid outlet channel are defined in the cavity wall of the crystal pulling chamber, a second liquid inlet channel and a second liquid outlet channel are defined in the cavity wall of the connecting chamber, a third liquid inlet channel and a third liquid outlet channel are defined in the cooling assembly, the first liquid inlet channel, the second liquid inlet channel, the third liquid inlet channel, the third liquid outlet channel, the second liquid outlet channel and the first liquid outlet channel are connected in sequence and are respectively used for flowing cooling medium, at least part of the isolation chamber is arranged around the crystal pulling chamber, a water inlet pipe is provided at the inlet of the first liquid inlet channel, a water outlet pipe is provided at the outlet of the first liquid outlet channel, and the water inlet pipe and the water outlet pipe are both penetrated through the isolation chamber.

[0012] In some embodiments, the cross-sectional area of ​​the connecting chamber increases from top to bottom, and the inner diameter of the cooling assembly is larger than the inner diameter of the crystal pulling chamber.

[0013] In some embodiments, the isolation chamber includes a first chamber and a second chamber, the first chamber is arranged around the crystal pulling chamber, and the second chamber is arranged on the upper side of the first chamber and the crystal pulling chamber and is communicated with the first chamber and the crystal pulling chamber respectively.

[0014] In some embodiments, the crystal pulling mechanism includes a winding wheel, a supporting wheel and a pulling rope. The winding wheel is rotatably disposed in the first chamber, the supporting wheel is rotatably disposed in the second chamber, and the pulling rope is wound around the winding wheel and around the supporting wheel to be suitable for passing through the top opening of the crystal pulling chamber.

[0015] In some embodiments, a pivot hole is formed on the top wall of the second shell, the crystal pulling chamber is penetrated through the pivot hole and pivotally matched with the pivot hole, and the second shell is supported on the bottom wall of the first chamber and pivotally matched with the bottom wall of the first chamber.

[0016] In some embodiments, the single crystal silicon growth furnace also includes: a crucible driving mechanism, which is used to drive the crucible assembly to move relative to the heating assembly; a weighing mechanism, which is arranged between the crucible assembly and the crucible driving mechanism and is used to weigh the bearing weight of the crucible assembly, and the weighing mechanism is coaxially arranged with the crucible assembly.

[0017] In some embodiments, the single crystal silicon growth furnace also includes: a guide assembly, which is arranged in the crystal growth chamber and located on the upper side of the crucible assembly, and the guide assembly is rotatably connected to the first shell around the central axis of the guide assembly; a second driving mechanism, which is used to drive the guide assembly to rotate relative to the first shell.

[0018] In some embodiments, the first shell is formed with a first perspective window, the second shell is formed with a second perspective window, the guide assembly is formed with a perspective channel, the perspective channel extends straight toward the direction of the solid-liquid interface in the crucible assembly, and the single crystal silicon growth furnace has a preset state, in which the first perspective window, the second perspective window and the perspective channel are on the same straight line.

[0019] According to the control method of a single crystal silicon growth furnace of an embodiment of the second aspect of the present invention, the control method includes: in the equal-diameter growth stage of the single crystal silicon rod, controlling the first shell to rotate clockwise relative to the second shell by the first driving mechanism; controlling the crucible assembly to rotate counterclockwise relative to the first shell by the crucible driving mechanism, and controlling the crucible assembly to rotate clockwise relative to the second shell; controlling the guide assembly to rotate counterclockwise relative to the crucible assembly by the second driving mechanism, and controlling the guide assembly to rotate clockwise relative to the second shell.

[0020] According to the control method of the single crystal silicon growth furnace of the embodiment of the present invention, by controlling the rotation direction and speed of the first shell, the crucible assembly and the guide assembly, the atmosphere in the furnace and the flow field of the protective gas can be improved, so as to better meet the crystal growth requirements and improve the crystallization quality of the crystal.

[0021] Additional aspects and advantages of the present invention will be given in part in the following description and in part will be obvious from the following description, or will be learned through practice of the present invention. BRIEF DESCRIPTION OF THE DRAWINGS

[0022] The above and / or additional aspects and advantages of the present invention will become apparent and easily understood from the description of the embodiments in conjunction with the following drawings, in which:

[0023] Figure 1 is a schematic structural diagram of a single crystal silicon growth furnace according to an embodiment of the present invention, wherein the crystal is in the initial stage of isodiameter growth;

[0024] Figure 2 yes Figure 1 The schematic diagram of the structure of the single crystal silicon growth furnace shown in , wherein the crystal is in the late stage of isodiameter growth;

[0025] Figure 3 yes Figure 2A side view of a single crystal silicon growth furnace shown in;

[0026] Figure 4 yes Figure 3 A partial enlarged view of a single crystal silicon growth furnace shown in FIG.

[0027] Figure 5 yes Figure 4 An enlarged view of the D section circled in the middle;

[0028] Figure 6 The figure is a flow chart of a control method for a single crystal silicon growth furnace according to an embodiment of the present invention.

[0029] Reference numerals:

[0030] Single crystal silicon growth furnace 100,

[0031] The first housing 1, the exhaust hole 1a, the opening 1b,

[0032] The main body 11, the crystal growth chamber 11a, the communication chamber 11b, the crystal pulling chamber 111a,

[0033] The first upper shell 111, the slide groove 111f, the heat-conducting housing 112, the first lower shell 113,

[0034] The first liquid inlet channel 111b, the first liquid outlet channel 111c, the second liquid inlet channel 111d, the second liquid outlet channel 111e, the isolation cover 12, the isolation chamber 12a, the first chamber A, the second chamber B, the water inlet pipe 121, the water outlet pipe 122,

[0035] Shielding gas connecting pipe 123,

[0036] Cooling assembly 13, third liquid inlet channel 13a, third liquid outlet channel 13b, first perspective window 14,

[0037] The second housing 2, the mounting cavity 2a, the pivot hole 2b, the second upper housing 21, the second perspective window 211, the second lower housing 22, the crucible assembly 3, the quartz crucible 31, the graphite crucible 32,

[0038] Heating component 4, heat preservation component 5, first driving mechanism 6,

[0039] Crystal lifting mechanism 7, retracting wheel 71, supporting wheel 72, lifting rope 73,

[0040] Crucible driving mechanism 8, third driving mechanism 81, lifting mechanism 82,

[0041] Weighing mechanism 9,

[0042] The guide assembly 10, the perspective channel 10a, the slide rail 10b,

[0043] The first matching section 10c, the second matching section 10d, the avoidance groove 10e, and the second driving mechanism C. DETAILED DESCRIPTION

[0044] Embodiments of the present invention are described in detail below, examples of which are shown in the accompanying drawings, wherein the same or similar reference numerals throughout represent the same or similar elements or elements having the same or similar functions. The embodiments described below with reference to the accompanying drawings are exemplary and are only used to explain the present invention, and cannot be understood as limiting the present invention.

[0045] The disclosure below provides many different embodiments or examples to implement different structures of the present invention. In order to simplify the disclosure of the present invention, the parts and settings of specific examples are described below. Of course, they are only examples, and the purpose is not to limit the present invention. In addition, the present invention can repeat reference numbers and / or letters in different examples. This repetition is for the purpose of simplicity and clarity, and does not itself indicate the relationship between the various embodiments and / or settings discussed. In addition, the present invention provides various specific processes and examples of materials, but those of ordinary skill in the art can be aware of the applicability of other processes and / or the use of other materials.

[0046] Hereinafter, a single crystal silicon growth furnace 100 according to an embodiment of the present invention will be described with reference to the accompanying drawings.

[0047] like Figure 1-Figure 3 As shown, the single crystal silicon growth furnace 100 includes: a first shell 1, a second shell 2, a crucible assembly 3, a heating assembly 4 and a protective gas connecting pipe 123, the first shell 1 has a crystal growth chamber 11a, a crystal pulling chamber 111a and an isolation chamber 12a, the crystal pulling chamber 111a is connected to the top side of the crystal growth chamber 11a, the isolation chamber 12a is connected to the top side of the crystal pulling chamber 111a, the second shell 2 is covered outside the first shell 1, and an installation cavity 2a is formed between the second shell 2 and the first shell 1, the crucible assembly 3 is arranged in the crystal growth chamber 11a, and the crucible assembly 3 is used to hold silicon material, the heating assembly 4 is arranged in the installation cavity 2a, and the heating assembly 4 is used to heat the crucible assembly 3. The protective gas connecting pipe 123 is arranged in the isolation chamber 12a, and the protective gas connecting pipe 123 is connected to the crystal pulling chamber 111a, so that the protective gas connecting pipe 123 introduces protective gas (such as argon) into the crystal pulling chamber 111a to ensure a favorable gas environment for crystal growth and stabilize the working pressure inside the single crystal silicon growth furnace 100. At the same time, the protective gas can promptly take away the volatiles (such as silicon oxides or other impurities, etc.) generated in the crystal pulling chamber 111a and the crystal growth chamber 11a to ensure the crystallization rate and crystal quality of the crystal.

[0048] It can be seen that the first shell 1 isolates the crystal growth chamber 11a and the crystal pulling chamber 111a from the installation chamber 2a, and the heating component 4 is arranged in the installation chamber 2a. Under the premise of ensuring that the heating component 4 can heat the crucible component 3, the volatile gas (such as SiO gas and CO gas, etc.) generated during the crystal growth process will not flow into the installation chamber 2a and contact the heating component 4, thereby preventing the above-mentioned volatile gas from corroding the heating component 4, ensuring the normal operation of the heating component 4, and thus extending the service life of the heating component 4. In addition, it can also prevent the impurities generated by the heating component 4 during the heating process from entering the melt, thereby reducing the impact on the quality of crystal growth.

[0049] like Figure 1-Figure 3 As shown, the single crystal silicon growth furnace 100 also includes a heat preservation component 5, which is arranged in the installation cavity 2a, and the heat preservation component 5 cover is arranged outside the heating component 4 to reduce the heat loss of the heating component 4, improve the heating efficiency of the heating component 4 to the crucible component 3, and save the energy consumption of the heating component 4 and save production costs.

[0050] In some examples, the heating component 4 includes a resistive heater, and the insulation component 5 is connected to the peripheral wall of the second shell 2 through a radially outer support arm. The suspended design can reduce the space occupied by the insulation component 5; of course, the settings of the heating component 4 and the insulation component 5 are not limited to this.

[0051] like Figure 1 and Figure 2 As shown, the single crystal silicon growth furnace 100 also includes a first driving mechanism 6 and a crystal pulling mechanism 7. The first driving mechanism 6 drives the first shell 1 to rotate relative to the second shell 2. The crystal pulling mechanism 7 is fixed in the isolation chamber 12a, which can prevent the crystal pulling mechanism 7 from being exposed to the outside and causing interference, thereby affecting the pulling process of the crystal. Part of the crystal pulling mechanism 7 is suitable for extending into the crystal pulling chamber 111a for pulling the crystal. The crystal pulling mechanism 7 is suitable for rotating synchronously with the first shell 1, and the first driving mechanism 6 can also control the rotation of the crystal pulling mechanism 7, thereby driving the crystal to rotate, so that the crystal rotates synchronously with the first shell 1 to meet the rotation requirements of the crystal during the crystal growth process. The crystal pulling mechanism 7 does not need to be configured with a mechanism to control its own rotation, thereby simplifying the complexity of the top structure of the single crystal silicon growth furnace 100.

[0052] It can be seen that the arrangement of the first driving mechanism 6 and the crystal pulling mechanism 7 in the present application meets the crystal pulling rotation requirements while ensuring that the heating component 4 is effectively separated from the volatile gases generated during the crystal growth process.

[0053] Among them, the first driving mechanism 6 is arranged at the bottom of the first shell 1 to support the first shell 1, which is convenient for lowering the center of gravity of the single crystal silicon growth furnace 100, and is beneficial to increasing the stability of the single crystal silicon growth furnace 100. At the same time, since the height of the first driving mechanism 6 is relatively low, it is convenient for maintenance personnel to repair the first driving mechanism 6, and it is convenient to ensure that the first driving mechanism 6 does not occupy the space of the installation cavity 2a, so as to flexibly arrange and install the heating component 4.

[0054] According to the single crystal silicon growth furnace 100 of the embodiment of the present invention, by arranging the second shell 2 to cover the outside of the first shell 1, the heating component 4 is arranged between the first shell 1 and the second shell 2, and the protective gas connecting pipe 123 is connected to the first shell 1, so that the first shell 1 separates the environmental space required for crystal growth (i.e., the internal space of the first shell 1) from the space where the heating component 4 is located (i.e., the installation cavity 2a), thereby preventing the volatile gases (such as SiO gas and CO gas, etc.) in the crystal growth chamber 11a and the crystal pulling chamber 111a from contacting with the heating component 4 and corroding the heating component 4, ensuring the normal operation of the heating component 4, thereby extending the service life of the heating component 4; and by arranging the first driving mechanism 6 to realize the synchronous rotation of the first shell 1 and the crystal pulling mechanism 7, thereby realizing the rotation of the crystal, it is convenient to simplify the complexity of the top structure of the single crystal silicon growth furnace 100.

[0055] like Figure 1 As shown, the first driving mechanism 6 is arranged at the bottom of the first shell 1 to support the first shell 1, and an exhaust hole 1a is formed on the first driving mechanism 6. The protective gas and volatiles or other gases in the crystal growth chamber 11a can be discharged through the exhaust hole 1a to ensure the stability of the internal working pressure of the single crystal silicon growth furnace 100.

[0056] Of course, the present application is not limited thereto. In another example of the present application, the first driving mechanism 6 is disposed in the first shell 1 , and an exhaust hole 1 a is formed on the bottom wall of the first shell 1 .

[0057] Optionally, in Figure 1 In the example, the crucible assembly 3 includes a quartz crucible 31 and a graphite crucible 32. A tray is provided at the bottom of the graphite crucible 32. The tray has a slot formed therein. The slot is limitedly matched with the graphite crucible 32 so that the tray limits and supports the graphite crucible 32.

[0058] In some embodiments, Figure 1-Figure 3As shown, the first shell 1 includes a main body 11, and the main body 11 includes a first upper shell 111, a heat-conducting shell 112, and a first lower shell 113 arranged in sequence from top to bottom. The crystal pulling chamber 111a is formed in the first upper shell 111, and a portion of the first upper shell 111, the heat-conducting shell 112, and the first lower shell 113 jointly define the crystal growth chamber 11a. It can be understood that a portion of the first upper shell 111 forms the crystal pulling chamber 111a, and another portion of the first upper shell 111 participates in forming the crystal growth chamber 11a. The heat-conducting shell 112 is arranged around the crucible assembly 3, and the heat-conducting shell 112 is located between the crucible assembly 3 and the heating assembly 4. The heat-conducting shell 112 has good heat conductivity. The heat-conducting shell 112 can effectively transfer the heat of the heating assembly 4 to the crucible assembly 3 to ensure the heat received by the crucible assembly 3 and the material in the crucible assembly 3; for example, the thermal conductivity of the heat-conducting shell 112 is greater than the thermal conductivity of the first upper shell 111 and the first lower shell 113, so as to realize flexible material selection of various parts of the main body 11 and meet the requirements of various parts of the main body 11 for thermal conductivity, strength and thermal insulation performance.

[0059] Among them, the upper end of the heating component 4 is not higher than the upper end of the heat-conducting shell 112, and the lower end of the heating component 4 is not lower than the lower end of the heat-conducting shell 112, then the height of the heating component 4 in the up and down direction is less than or equal to the axial height of the heat-conducting shell 112, which is convenient for ensuring that more heat dissipated by the heating component 4 is transferred toward the crucible assembly 3 through the heat-conducting shell 112, thereby ensuring that at least most of the heat dissipated by the heating component 4 toward the first shell 1 is transferred to the crucible assembly 3 through the heat-conducting shell 112 to heat the silicon material.

[0060] exist Figure 1-Figure 3 In the example, the heat-conducting housing 112 is a carbon-carbon composite material, and the carbon-carbon composite material has a low density (<2.0 g / cm 3 ), high strength, high specific modulus, high thermal conductivity, low expansion coefficient, good thermal shock resistance, high dimensional stability, etc., thereby ensuring that the heat-conducting housing 112 can take into account both structural strength and thermal conductivity. Of course, the material of the heat-conducting housing 112 is not limited thereto.

[0061] Optionally, the first upper shell 111 is detachably connected to the heat-conductive shell 112, and the heat-conductive shell 112 is detachably connected to the first lower shell 113, so as to facilitate disassembly, assembly, repair or replacement between the first upper shell 111 and the heat-conductive shell 112, and between the first lower shell 113 and the heat-conductive shell 112. When one or two of the first upper shell 111, the heat-conductive shell 112 and the first lower shell 113 are damaged, it is only necessary to replace a part of the main body 11, thereby saving equipment maintenance costs.

[0062] For example, the first upper shell 111 is threadedly connected to the heat-conducting shell 112, and the first lower shell 113 is threadedly connected to the heat-conducting shell 112. This makes it easy to ensure the sealing of the main body 11 while achieving the detachability between the first upper shell 111 and the heat-conducting shell 112 and the detachability between the first lower shell 113 and the heat-conducting shell 112.

[0063] In addition, it should be noted that the first upper shell 111 is detachably connected to the heat-conducting shell 112. When the rod is subsequently taken out (that is, when the crystal growth is completed and needs to be taken out from the single crystal growth furnace 100), the first upper shell 111 can be removed from the heat-conducting shell 112. For example, when the first upper shell 111 and the heat-conducting shell 112 are threadedly matched, the first upper shell 111 and the crystal can be separated from the single crystal silicon growth furnace 100 by rotating the first upper shell 111; then, the crystal is pushed out of the crystal pulling chamber 111a through the reverse rotation of the crystal pulling mechanism 7, thereby completing the rod taking process.

[0064] Optionally, when the first driving mechanism 6 is disposed at the bottom of the first shell 1 to support the first shell 1 , the first driving mechanism 6 may be connected to the first lower shell 113 to drive the entire first shell 1 to rotate.

[0065] like Figure 1 As shown, the first housing 1 further includes an isolation cover 12, and the isolation cover 12 is an integral part with the first upper shell 111. Thus, the integral structure can not only ensure the structural and performance stability of the isolation cover 12 and the first upper shell 111, but also facilitate molding and simple manufacturing, and eliminate unnecessary assembly parts and connection processes, thereby ensuring the connection reliability between the isolation cover 12 and the first upper shell 111. Furthermore, the overall strength and stability of the integral structure are higher, and the service life is longer.

[0066] The isolation cover 12 covers the outer side of the first upper shell 111, and the bottom wall of the isolation cover 12 is rotatably connected to the top wall of the second shell 2, ensuring the smooth and stable rotation of the first shell 1 relative to the second shell 2, thereby ensuring the stability of the crystal rotation. In one example of the present application, the outer diameter of the isolation cover 12 is the same as the outer diameter of the heat-conducting shell 112. As a result, the isolation cover 12 and the main body 11 are more coordinated in appearance and size, avoiding the problem of "big head and small body" or "small head and big body" rotation mismatch, which is conducive to improving the stability of the rotation of the first shell 1 relative to the second shell 2.

[0067] The isolation cover 12 and the first upper shell 111 define an isolation chamber 12a separated from the external space to ensure the isolation of the isolation chamber 12a from the external space, and part of the crystal pulling mechanism 7 (such as the crystal pulling rope) is suitable for extending into the crystal pulling chamber 111a for pulling the crystal, and the crystal pulling chamber 111a is formed with a through opening 1b for the crystal pulling mechanism 7 to pass through. Since the isolation chamber 12a has good sealing performance, the sealing requirements for the crystal pulling chamber 111a and the crystal pulling mechanism 7 at the through opening 1b can be appropriately reduced, so as to reduce the layout requirements of the crystal pulling mechanism 7 while ensuring the sealing performance of the crystal growth chamber 11a and the crystal pulling chamber 111a.

[0068] It can be seen that the isolation chamber 12a is located outside the installation cavity 2a, so as to ensure that the isolation chamber 12a provides sufficient installation space for the crystal pulling mechanism 7, and does not cause the space of the installation cavity 2a to be too large, which is convenient for reducing the heat dissipation space provided by the installation cavity 2a for the heating component 4, which is beneficial to improving the heating efficiency of the heating component 4 for the crucible component 3; at least part of the first upper shell 111 extends out of the installation cavity 2a, so that at least part of the crystal pulling chamber 111a is located outside the installation cavity 2a, which is beneficial to reducing the heat transferred from the installation cavity 2a to the crystal pulling chamber 111a, so that the temperature of the crystal pulling chamber 111a is lower than the temperature of the crystal growth chamber 11a, thereby ensuring the cooling efficiency of the crystal in the crystal pulling chamber 111a.

[0069] For example, in Figure 1-Figure 3 In the example, a rotating assembly is provided between the bottom wall of the isolation cover 12 and the top wall of the second shell 2, so that the isolation cover 12 is rotatably connected to the second shell 2 through the rotating assembly, and the rotating assembly is configured as follows: the second shell 2 supports the isolation cover 12 through the rotating assembly, so that the rotating assembly is used to bear the vertical force, which is beneficial to improve the stability of the first shell 1; at this time, the rotating assembly can be located outside the installation cavity 2a, and there is no need to open an installation port on the second shell 2 to install the rotating assembly, which simplifies the processing of the second shell 2, and the heat in the installation cavity 2a will not be dissipated through the position of the rotating assembly, which is convenient for further reducing the energy consumption of the heating assembly 4. Optionally, the rotating assembly is a bearing (such as a thrust ball bearing, or a tapered roller bearing, etc.) or a pulley assembly, etc.

[0070] Of course, the configuration of the rotating assembly is not limited thereto; the rotating assembly may also be configured such that the rotating assembly only bears horizontal radial forces.

[0071] In some embodiments, Figure 1As shown, the single crystal silicon growth furnace 100 also includes a cooling component 13, and a connecting chamber 11b is provided between the crystal growth chamber 11a and the crystal pulling chamber 111a to connect the crystal growth chamber 11a and the crystal pulling chamber 111a, so as to facilitate the transition between the crystal growth chamber 11a and the crystal pulling chamber 111a; the cooling component 13 is located above the crucible component 3, and the cooling component 13 is integrally formed on the cavity wall of the connecting chamber 11b, and the cooling component 13 extends downward into the crystal growth chamber 11a for cooling the crystal, thereby facilitating the molding of the cooling component 13, saving the installation process of the cooling component 13, improving the crystal production efficiency, and at the same time facilitating the cooling component 13 to provide sufficient avoidance space for the pulling of the crystal, for example, when the cooling component 13 is a cylindrical structure, it is convenient to ensure that the crystal can pass through the radial inner side of the cooling component 13.

[0072] In one example of the present application, the inner diameter of the crystal growth chamber 11a is R1, and the inner diameter of the crystal pulling chamber 111a is R2, and they satisfy: 0.2≤R2 / R1≤0.3. By setting the ratio of the inner diameter of the crystal pulling chamber 111a to the inner diameter of the crystal growth chamber 11a to be between 0.2-0.3, the flow rate of the protective gas flowing through the crystal pulling chamber 111a can be increased, so that the crystal rod can be cooled quickly. Moreover, the sudden drop in the temperature of the crystal rod can be avoided, which is conducive to ensuring the quality of the crystal rod.

[0073] It should be noted that the cooling component 13 and the cavity wall of the connecting chamber 11b can be processed and formed at one time, for example, the cooling component 13 and the cavity wall of the connecting chamber 11b can be integrally cast. Of course, the present application is not limited thereto, and the cooling component 13 can also be processed on the basis of the cavity wall of the connecting chamber 11b. In this case, the cooling component 13 and the cavity wall of the connecting chamber 11b can be formed after two processing steps. It can be understood that no matter what the specific processing sequence of the cooling component 13 and the cavity wall of the connecting chamber 11b is, as long as the cooling component 13 and the cavity wall of the connecting chamber 11b are an integrated structure after the overall processing of the first shell 1 is completed.

[0074] In some embodiments, Figure 1As shown, a first liquid inlet channel 111b and a first liquid outlet channel 111c are defined in the wall of the crystal pulling chamber 111a, a second liquid inlet channel 111d and a second liquid outlet channel 111e are defined in the wall of the communicating chamber 11b, a third liquid inlet channel 13a and a third liquid outlet channel 13b are defined in the cooling assembly 13, the first liquid inlet channel 111b, the second liquid inlet channel 111d, the third liquid inlet channel 13a, the third liquid outlet channel 13b, the second liquid outlet channel 111e and the first liquid outlet channel 111c are connected in sequence, and the first liquid inlet channel 111b, the second liquid inlet channel 111d, the third liquid inlet channel 13a, the third liquid outlet channel 13b, the second liquid outlet channel 111e and the first liquid outlet channel 111c are respectively used for flowing cooling medium, then the first liquid inlet channel 111b, the second liquid inlet channel 111d, the third liquid inlet channel 13a, the third liquid outlet channel 13b, the second liquid outlet channel 111e and the first liquid outlet channel 111c are arranged in series, and the cavity wall of the crystal pulling chamber 111a and the cavity wall of the connecting chamber 11b can also be used to cool the crystal, which effectively expands the cooling range of the cooling medium and extends the flow path of the cooling medium, thereby improving the cooling efficiency of the crystal; moreover, since the cooling component 13 and the cavity wall of the connecting chamber 11b are integrally formed, it is convenient to ensure the reliable connection between the channel in the cooling component 13 and the channel in the cavity wall of the connecting chamber 11b.

[0075] In an example of the present application, the inner diameter of the crystal growth chamber 11a is R1, the inner diameter of the crystal pulling chamber 111a is R2, the inner diameter of the cooling assembly 13 is R3, and the following conditions are satisfied: 0.35≤R3 / R1≤0.45, 1.2≤R3 / R2≤1.7.

[0076] It is understandable that the structures of the above-mentioned channels for flowing cooling medium can be specifically set according to actual needs, for example, the channels can extend in a spiral in the up-down direction. Taking the first liquid inlet channel 111b and the first liquid outlet channel 111c as an example, the first liquid inlet channel 111b and the first liquid outlet channel 111c both extend in a spiral in the circumferential direction of the crystal pulling chamber 111a.

[0077] Among them, Figure 3 As shown, at least part of the isolation chamber 12a is arranged around the crystal pulling chamber 111a, a water inlet pipe 121 is provided at the inlet of the first liquid inlet channel 111b, and a water outlet pipe 122 is provided at the outlet of the first liquid outlet channel 111c. The water inlet pipe 121 and the water outlet pipe 122 are both penetrated through the isolation chamber 12a, and the heat exchange medium flows into the first liquid inlet channel 111b from the water inlet pipe 121, and flows through the second liquid inlet channel 111d, the third liquid inlet channel 13a, the third liquid outlet channel 13b and the second liquid outlet channel 111e in sequence, and then flows from the first liquid outlet channel 111c to the water outlet pipe 122, so that the heat exchange medium flows through the crystal pulling chamber 111a, the connecting chamber 11b, the cooling assembly 13, the connecting chamber 11b in sequence, and is finally discharged from the crystal pulling chamber 111a.

[0078] It can be seen that the isolation cover 12 has a certain supporting and protecting effect on the water inlet pipe 121 and the water outlet pipe 122, so that the connection position of the water inlet pipe 121 and the first liquid inlet channel 111b, and the connection position of the water outlet pipe 122 and the first liquid outlet channel 111c are both located in the isolation chamber 12a, avoiding the water inlet pipe 121 and the water outlet pipe 122 from bending and being damaged at the connection position of the water inlet pipe 121 and the first liquid inlet channel 111b, and at the connection position of the water outlet pipe 122 and the first liquid outlet channel 111c due to external force collision, etc., so as to ensure the reliable connection between the water inlet pipe 121 and the first liquid inlet channel 111b, and the reliable connection between the water outlet pipe 122 and the first liquid outlet channel 111c.

[0079] In some embodiments, Figure 1 As shown, the cross-sectional area of ​​the connecting chamber 11b increases from top to bottom, the crystal pulling chamber 111a is connected to the upper side of the connecting chamber 11b, and the crystal growth chamber 11a is connected to the lower side of the connecting chamber 11b. The inner diameter of the crystal pulling chamber 111a is smaller than the inner diameter of the crystal growth chamber 11a, which is convenient for realizing a stable transition between the crystal pulling chamber 111a and the crystal growth chamber 11a, avoiding the occurrence of a sudden change in the cross-sectional position in the internal space of the first shell 1, thereby facilitating the flow stability of the airflow in the process of flowing from the crystal pulling chamber 111a to the crystal growth chamber 11a, so as to effectively ensure the atmosphere in the furnace; the inner diameter of the cooling component 13 is larger than the inner diameter of the crystal pulling chamber 111a, and when the crystal pulling mechanism 7 pulls the crystal, it ensures that there is a suitable radial distance between the crystal and the cooling component 13, avoiding the crystal from contacting the cooling component 13 when rotating, and at the same time ensuring the cooling effect on the crystal.

[0080] Optionally, in Figure 1 In the example, the cavity wall of the connecting chamber 11b is formed into a conical cylindrical structure for easy processing.

[0081] In some embodiments, Figure 1-Figure 3 As shown, the isolation chamber 12a includes a first chamber A and a second chamber B. The first chamber A is arranged around the crystal pulling chamber 111a, and the second chamber B is arranged on the upper side of the first chamber A and the crystal pulling chamber 111a, and the second chamber B is connected with the first chamber A and the crystal pulling chamber 111a respectively, so that the isolation chamber 12a provides sufficient layout space for the crystal pulling mechanism 7. At the same time, the first chamber A is arranged around the crystal pulling chamber 111a. On the premise of realizing the crystal pulling mechanism 7, it is beneficial to reduce the space occupied by the second chamber B, so as to avoid the isolation chamber 12a and the crystal pulling chamber 111a from being "top-heavy".

[0082] In some embodiments, Figure 1As shown, the crystal pulling mechanism 7 includes a reel 71, a support wheel 72 and a pulling rope 73. The reel 71 is rotatably disposed in the first chamber A, and the support wheel 72 is rotatably disposed in the second chamber B. The pulling rope 73 is wound around the reel 71 and around the support wheel 72 to be suitable for passing through the top opening 1b of the crystal pulling chamber 111a, thereby ensuring that the crystal pulling mechanism 7 rotates synchronously with the first shell 1. At the same time, it is convenient to realize the dispersed arrangement of the reel 71 and the support wheel 72 while ensuring the smooth lifting and lowering of the crystal pulling rope 73. There is no need to centrally arrange the entire crystal pulling mechanism 7 on the upper side of the crystal pulling chamber 111a, which is beneficial to improving the force on the wall of the crystal pulling chamber 111a.

[0083] It can be seen that the reel wheel 71 can be a driving wheel to control the speed of the crystal moving up and down, and the support wheel 72 can change the arrangement direction of the crystal pulling rope 73 extending from the reel wheel 71 to achieve the movement of the crystal by the crystal pulling rope 73 moving up and down.

[0084] like Figure 1-Figure 3 As shown, the central axis of the through opening 1b can coincide with the rotation axis of the first shell 1, so as to ensure that the rotation axis of the crystal pulling rope 73 coincides with the rotation axis of the first shell 1, reduce the shaking of the crystal pulling rope 73, ensure the smooth movement of the crystal and the stability of the crystal rotation, avoid crystal distortion, etc., and improve the quality of the crystal.

[0085] In some embodiments, Figure 1 As shown, a pivot hole 2b is formed on the top wall of the second shell 2, the crystal pulling chamber 111a is penetrated through the pivot hole 2b, and the crystal pulling chamber 111a is pivotally matched with the pivot hole 2b, the second shell 2 is supported on the bottom wall of the first chamber A, and the second shell 2 is pivotally matched with the bottom wall of the first chamber A, then the second shell 2 is matched with the crystal pulling chamber 111a and the first chamber A respectively, while realizing the smooth rotation of the first shell 1 relative to the second shell 2, the rotation stability of the first shell 1 can be improved.

[0086] For example, in Figure 1-Figure 3 In the example, the second housing 2 includes a second upper housing 21 and a second lower housing 22 fixedly connected up and down, and the second upper housing 21 and the second lower housing 22 are detachably connected, which facilitates the disassembly and assembly of the second housing 2, and when the second upper housing 21 and the second lower housing 22 are damaged, only part of the second housing 2 needs to be replaced, saving equipment maintenance costs. For example, the second upper housing 21 and the second lower housing 22 are threadedly connected.

[0087] It should be noted that the first upper shell 111 is detachably connected to the heat-conducting shell 112, and the second upper shell 21 is detachably connected to the second lower shell 22. When the rod is taken out later (that is, when the crystal growth is completed and needs to be taken out from the single crystal growth furnace 100), the second upper shell 21 can be removed from the second lower shell 22, and the first upper shell 111 can be removed from the heat-conducting shell 112 at the same time. For example, the second upper shell 21 and the second lower shell 22 are threadedly matched, and the first upper shell 111 and the heat-conducting shell 112 are threadedly matched. By rotating the second upper shell 21 and the first upper shell 111, the second upper shell 21, the first upper shell 111 and the crystal can be separated from the single crystal silicon growth furnace 100; then, through the reverse rotation of the crystal pulling mechanism 7, the crystal is pushed out of the crystal pulling chamber 111a, thereby completing the rod taking process.

[0088] In some embodiments, Figure 1 As shown, the single crystal silicon growth furnace 100 also includes a crucible driving mechanism 8 and a weighing mechanism 9. The crucible driving mechanism 8 can be coaxially arranged with the first driving mechanism 6. The crucible driving mechanism 8 is used to drive the crucible assembly 3 to move relative to the heating assembly 4. The weighing mechanism 9 is arranged between the crucible assembly 3 and the crucible driving mechanism 8. For example, the weighing mechanism 9 is arranged between the bottom wall of the crucible assembly 3 and the top wall of the crucible driving mechanism 8. The weighing mechanism 9 is used to weigh the bearing weight of the crucible assembly 3. The weighing mechanism 9 can obtain the consumption of silicon material in the crucible assembly 3 to accurately determine whether the crystal pulling is completed.

[0089] It can be seen that the crucible driving mechanism 8 drives the crucible assembly 3 to move through the weighing mechanism 9. The weighing mechanism 9 can detect the remaining silicon material in the crucible assembly 3 in real time during the crystal pulling process, and determine whether the crystal pulling is completed based on the detection data, so that the single crystal silicon growth furnace 100 can stop the crystal pulling work in time to reduce the waste of silicon material and save production costs.

[0090] The weighing mechanism 9 is coaxially arranged with the crucible assembly 3 to improve the detection accuracy of the weighing mechanism 9, reduce measurement and calculation deviations, and improve the accuracy of determining whether the crystal pulling is completed.

[0091] In some embodiments, Figure 1-Figure 3 As shown, the crucible driving mechanism 8 is arranged in the crystal growth chamber 11a, and the crucible driving mechanism 8 includes a third driving mechanism 81 and a lifting mechanism 82. The third driving mechanism 81 is used to drive the crucible assembly 3 to rotate relative to the heating assembly 4, and the lifting mechanism 82 is used to drive the crucible assembly 3 to move up and down, so as to realize the up and down movement and rotation of the crucible assembly 3 to meet the crystal pulling requirements. In one example of the present application, the crucible assembly 3 is driven up and down by the lifting mechanism 82, so that the distance between the liquid surface of the molten soup and the bottom wall of the guide assembly 10 remains unchanged, so that the growth environment at the triple point position remains unchanged, thereby ensuring the growth quality of the crystal rod.

[0092] The third driving mechanism 81 indirectly drives the crucible assembly 3 to rotate through the lifting mechanism 82 , so that the lifting mechanism 82 , the weighing mechanism 9 and the crucible assembly 3 rotate synchronously; or, the lifting mechanism 82 indirectly drives the crucible assembly 3 to move through the third driving mechanism 81 .

[0093] Optionally, the lifting mechanism 82 is a driving cylinder, such as a pneumatic cylinder.

[0094] In some embodiments, Figure 1-Figure 3 As shown, the first driving mechanism 6 is arranged at the bottom of the first shell 1 to support the first shell 1, and the third driving mechanism 81 is arranged at the lower side of the lifting mechanism 82. The third driving mechanism 81 and the first driving mechanism 6 are at the same height position, and the third driving mechanism 81 and the first driving mechanism 6 are spaced apart to avoid interference between the third driving mechanism 81 and the first driving mechanism 6.

[0095] In some embodiments, Figure 1 As shown, the single crystal silicon growth furnace 100 also includes a guide component 10 and a second driving mechanism C. The guide component 10 is arranged in the crystal growth chamber 11a, and the guide component 10 is located on the upper side of the crucible component 3. The guide component 10 is rotatably connected to the first shell 1 around the central axis of the guide component 10, so that the guide component 10 can rotate relative to the first shell 1 around its central axis. The second driving mechanism C is used to drive the guide component 10 to rotate relative to the first shell 1, so that the protective gas blown out of the protective gas connecting pipe 123 passes through the crystal pulling chamber 111a and is distributed more evenly under the action of the rotation of the guide component 10, so that the rotation of the guide component 10 can weaken the rotation of the protective gas caused by the rotation of the first shell 1, thereby improving the uniformity of the purged protective gas and ensuring the atmosphere in the furnace.

[0096] For example, in Figure 1 and Figure 5 In the example, an annular slide groove 111f is formed on the inner circumferential wall of the first shell 1, and a slide rail 10b is provided on the outer circumferential wall of the guide assembly 10. The slide rail 10b slides and fits in the slide groove 111f to realize the pivotal connection between the guide assembly 10 and the first shell 1. The slide rail 10b has gear teeth. The second driving mechanism C includes a driving motor, which is arranged on the first shell 1. The driving motor meshes with the gear teeth of the slide rail 10b through gears to realize power transmission.

[0097] Optionally, in Figure 5In the example, a bearing is provided between the slide rail 10b and the peripheral wall of the slide groove 111f to reduce the sliding resistance of the slide rail 10b; the slide rail 10b includes a first mating section 10c and a second mating section 10d, the first mating section 10c is arranged around the second mating section 10d, and in the axial direction of the first shell 1, the length of the first mating section 10c is greater than the length of the second mating section 10d, so that an avoidance groove 10e is formed between the first mating section 10c, the second mating section 10d and the wall surface of the slide groove 111f, then the second mating section 10d is formed with an avoidance groove 10e on at least one of the two sides in the axial direction of the first shell 1, and the avoidance groove 10e is used to install a bearing, for example, the second mating section 10d is provided with bearings on both sides in the axial direction of the first shell 1.

[0098] In some embodiments, Figure 1 As shown, the first shell 1 is formed with a first perspective window 14, the second shell 2 is formed with a second perspective window 211, and the guide assembly 10 is formed with a perspective channel 10a, which extends straightly toward the direction of the solid-liquid interface in the crucible assembly 3; the single crystal silicon growth furnace 100 has a preset state, in which the first perspective window 14, the second perspective window 211 and the perspective channel 10a are on the same straight line, so that the operator can observe the intersection area of ​​the melt and the crystal (i.e., the halo area of ​​the crystal) through the first perspective window 14, the second perspective window 211 and the perspective channel 10a, which is convenient for the operator to judge the crystal growth situation, etc.

[0099] For example, the first perspective window 14 extends along the circumference of the first shell 1, the first perspective window 14 rotates with the first shell 1, the second perspective window 211 extends along the circumference of the second shell 2, and the perspective channel 10a rotates with the guide component 10. When the field of view corresponding to the first perspective window 14, the field of view corresponding to the second perspective window 211 and the field of view corresponding to the perspective channel 10a intersect, the single crystal silicon growth furnace 100 is in a preset state, and the operator can observe the intersection area of ​​liquid silicon and crystal through the first perspective window 14, the second perspective window 211 and the perspective channel 10a.

[0100] Optionally, in Figure 1-Figure 3 In the example, the first shell 1 and the second shell 2 are coaxially arranged. On the cross section of the first shell 1, with the central axis of the first shell 1 as the center of the circle, the center angle corresponding to the first perspective window 14 does not exceed 60°, for example, the center angle corresponding to the first perspective window 14 is 10°, or 20°, or 30°, or 45°, or 60°, etc.; on the cross section of the second shell 2, with the central axis of the second shell 2 as the center of the circle, the center angle corresponding to the second perspective window 211 does not exceed 60°, for example, the center angle corresponding to the second perspective window 211 is 10°, or 15°, or 30°, or 50°, or 60°, etc. In an example of the present application, the center angle of the second perspective window 211 is equal to the center angle of the first perspective window 14.

[0101] Optionally, in the longitudinal section of the first shell 1, the width of the first perspective window 14 gradually increases radially from the inside to the outside, in the longitudinal section of the second shell 2, the width of the second perspective window 211 gradually increases radially from the inside to the outside, and in the longitudinal section of the guide assembly 10, the width of the perspective channel 10a gradually increases radially from the inside to the outside, so that the observation channel formed by the first perspective window 14, the second perspective window 211 and the perspective channel 10a has a larger observation operation space outside the second shell 2.

[0102] According to the control method of the single crystal silicon growth furnace 100 of the second embodiment of the present invention, the single crystal silicon growth furnace 100 includes a first shell 1, a second shell 2, a crucible assembly 3, a heating assembly 4, an insulation assembly 5, a first driving mechanism 6, a crystal pulling mechanism 7, a protective gas connecting pipe 123 and a guide assembly 10.

[0103] like Figure 6 As shown, the control method of the single crystal silicon growth furnace 100 includes: in the equal diameter growth stage of the single crystal silicon rod, controlling the first shell 1 to rotate clockwise relative to the second shell 2 by the first driving mechanism 6; controlling the crucible assembly 3 to rotate counterclockwise relative to the first shell 1 by the crucible driving mechanism 8, and controlling the crucible assembly 3 to rotate clockwise relative to the second shell 2 by the crucible driving mechanism 8; controlling the guide assembly 10 to rotate counterclockwise relative to the crucible assembly 3 by the second driving mechanism C, and controlling the guide assembly 10 to rotate clockwise relative to the second shell 2.

[0104] It should be noted that, in the present application, "clockwise rotation" and "counterclockwise rotation" are relative concepts, and the corresponding rotation directions are opposite.

[0105] It can be seen that in the control method of the present application, relative to the second shell 2, the rotation direction of the first shell 1, the rotation direction of the crucible assembly 3 and the rotation direction of the flow guide assembly 10 are the same (all clockwise), the rotation speed of the flow guide assembly 10 is less than the rotation speed of the crucible assembly 3, and the rotation speed of the crucible assembly 3 is less than the rotation speed of the first shell 1; wherein, the second shell 2 always remains stationary during the crystal growth process. Thus, by the counterclockwise rotation of the flow guide assembly 10 relative to the first shell 1, in order to offset the rotation of the protective gas to a certain extent driven by the first shell 1, the rotation speed of the protective gas flow swept into the molten soup in the crucible assembly 3 is relatively small or does not rotate, so as to better guide the protective gas flow to the solid-liquid interface to protect the crystal growth.

[0106] According to the control method of the single crystal silicon growth furnace 100 of the embodiment of the present invention, by controlling the rotation direction and speed of the first shell 1, the crucible assembly 3 and the guide assembly 10, the atmosphere in the furnace and the flow field of the protective gas can be improved, so as to better meet the crystal growth requirements and improve the crystallization quality of the crystal.

[0107] In some embodiments, the crucible driving mechanism 8 is constructed as follows: the crucible driving mechanism 8 is directly arranged on the first driving mechanism 6, and the first driving mechanism 6 drives the crucible assembly 3 to rotate synchronously through the crucible driving mechanism 8, and the crucible driving mechanism 8 is used to drive the crucible assembly 3 to rotate relative to the first shell 1; that is, when the crucible driving mechanism 8 is in operation, the crucible assembly 3 rotates relative to the first shell 1 driven by the crucible driving mechanism 8, so that the crucible assembly 3 and the first shell 1 rotate asynchronously, and when the crucible driving mechanism 8 is not in operation, the crucible assembly 3 is driven by the first driving mechanism 6, and the driving force is transmitted to the crucible assembly 3 through the first shell 1 and the crucible driving mechanism 8, so that the crucible assembly 3 and the first shell 1 rotate synchronously.

[0108] Of course, the present application is not limited thereto. In some other embodiments, the crucible drive mechanism 8 is configured as follows: the crucible drive mechanism 8 is arranged radially inward of the first drive mechanism 6, and a bearing is arranged between the crucible drive mechanism 8 and the first drive mechanism 6, the first drive mechanism 6 is used to drive the first shell 1 to rotate, and the first drive mechanism 6 cannot drive the crucible assembly 3 to rotate through the crucible drive mechanism 8, and the crucible drive mechanism 8 is used to drive the crucible assembly 3 to rotate relative to the first shell 1; that is, whether the crucible drive mechanism 8 is running or not, the driving force of the first drive mechanism 6 cannot be transmitted to the crucible assembly 3 through the crucible drive mechanism 8. For example, the crucible drive mechanism 8 is spaced apart from the first drive mechanism 6, and the crucible drive mechanism 8 is pivotally matched with the first shell 1 or the first drive mechanism 6, so that the driving force of the first drive mechanism 6 cannot be transmitted to the crucible drive mechanism 8.

[0109] It can be seen that the crucible driving mechanism 8 of the present application can be flexibly configured according to actual needs.

[0110] In the description of the present invention, it should be understood that the terms "center", "length", "upper", "lower", "top", "bottom", "inner", "outer", "axial", "circumferential" and the like indicate positions or positional relationships based on the positions or positional relationships shown in the accompanying drawings, and are only for the convenience of describing the present invention and simplifying the description, rather than indicating or implying that the device or element referred to must have a specific orientation, be constructed and operated in a specific orientation, and therefore cannot be understood as a limitation on the present invention. In addition, features defined as "first" and "second" may explicitly or implicitly include one or more of the features. In the description of the present invention, unless otherwise specified, "multiple" means two or more.

[0111] In the description of the present invention, it should be noted that, unless otherwise clearly specified and limited, the terms "installed", "connected", and "connected" should be understood in a broad sense, for example, it can be a fixed connection, a detachable connection, or an integral connection; it can be a mechanical connection or an electrical connection; it can be a direct connection, or it can be indirectly connected through an intermediate medium, or it can be the internal communication of two components. For ordinary technicians in this field, the specific meanings of the above terms in the present invention can be understood according to specific circumstances.

[0112] In the description of this specification, the description with reference to the terms "one embodiment", "some embodiments", "illustrative embodiments", "examples", "specific examples", or "some examples" means that the specific features, structures, materials or characteristics described in conjunction with the embodiment or example are included in at least one embodiment or example of the present invention. In this specification, the schematic representation of the above terms does not necessarily refer to the same embodiment or example. Moreover, the specific features, structures, materials or characteristics described may be combined in any one or more embodiments or examples in a suitable manner.

[0113] Although the embodiments of the present invention have been shown and described, it will be appreciated by those skilled in the art that various changes, modifications, substitutions and variations may be made to the embodiments without departing from the principles and spirit of the present invention, and that the scope of the present invention is defined by the claims and their equivalents.

Claims

1. A single crystal silicon growth furnace, characterized in that: include: A first shell, wherein the first shell has a crystal growth chamber, a crystal pulling chamber, and an isolation chamber, wherein the crystal pulling chamber is connected to the top side of the crystal growth chamber, and the isolation chamber is connected to the top side of the crystal pulling chamber; A second shell, the second shell is covered outside the first shell and forms a mounting cavity with the first shell; A crucible assembly, wherein the crucible assembly is disposed in the crystal growth chamber; A heating component, which is disposed in the mounting cavity and is used to heat the crucible component; A heat preservation component, the heat preservation component is arranged in the installation cavity and the cover is arranged outside the heating component; a first driving mechanism, the first driving mechanism being arranged at the bottom of the first shell to support and drive the first shell to rotate relative to the second shell, the first driving mechanism being formed with an exhaust hole, and the gas in the crystal growth chamber being suitable for being discharged from the crystal growth chamber through the exhaust hole; A crystal pulling mechanism, the crystal pulling mechanism is fixedly arranged in the isolation chamber and is suitable for extending into the crystal pulling chamber for pulling the crystal, and the crystal pulling mechanism is suitable for synchronously rotating with the first shell; A protective gas connecting pipe is provided in the isolation chamber and is connected to the crystal pulling chamber.

2. The single crystal silicon growth furnace according to claim 1, characterized in that: The first housing comprises: A main body, the main body comprising a first upper shell, a heat-conducting shell and a first lower shell which are sequentially arranged from top to bottom, the crystal pulling chamber is formed in the first upper shell, the heat-conducting shell, the first lower shell and parts of the first upper shell together define the crystal growth chamber, the heat-conducting shell is arranged around the crucible assembly and is located between the crucible assembly and the heating assembly, the heat-conducting shell is a carbon-carbon composite material, the upper end of the heating assembly is not higher than the upper end of the heat-conducting shell, and the lower end of the heating assembly is not lower than the lower end of the heat-conducting shell; The isolation cover is an integral part of the first upper shell, the isolation cover covers the outer side of the first upper shell, and the bottom wall of the isolation cover is rotatably connected to the top wall of the second shell, and the isolation cover and the first upper shell define the isolation chamber separated from the external space.

3. The single crystal silicon growth furnace according to claim 1, characterized in that: Also includes: A cooling component is provided between the crystal growth chamber and the crystal pulling chamber to connect the crystal growth chamber and the crystal pulling chamber. The cooling component is integrally formed on the cavity wall of the connecting chamber and extends downward into the crystal growth chamber to cool the crystal.

4. The single crystal silicon growth furnace according to claim 3, characterized in that: A first liquid inlet channel and a first liquid outlet channel are defined in the cavity wall of the crystal pulling chamber, a second liquid inlet channel and a second liquid outlet channel are defined in the cavity wall of the connecting chamber, a third liquid inlet channel and a third liquid outlet channel are defined in the cooling assembly, the first liquid inlet channel, the second liquid inlet channel, the third liquid inlet channel, the third liquid outlet channel, the second liquid outlet channel and the first liquid outlet channel are sequentially connected and are used for flowing cooling medium respectively. At least part of the isolation chamber is arranged around the crystal pulling chamber, a water inlet pipe is provided at the inlet of the first liquid inlet channel, a water outlet pipe is provided at the outlet of the first liquid outlet channel, and the water inlet pipe and the water outlet pipe are both arranged through the isolation chamber.

5. The single crystal silicon growth furnace according to claim 3, characterized in that: The cross-sectional area of ​​the connecting chamber increases from top to bottom, and the inner diameter of the cooling component is larger than the inner diameter of the crystal pulling chamber.

6. The single crystal silicon growth furnace according to claim 1, characterized in that: The isolation chamber includes a first chamber and a second chamber, the first chamber is arranged around the crystal pulling chamber, and the second chamber is arranged on the upper sides of the first chamber and the crystal pulling chamber and is communicated with the first chamber and the crystal pulling chamber respectively.

7. The single crystal silicon growth furnace according to claim 6, characterized in that: The crystal pulling mechanism includes a winding wheel, a supporting wheel and a pulling rope. The winding wheel is rotatably disposed in the first chamber, the supporting wheel is rotatably disposed in the second chamber, and the pulling rope is wound around the winding wheel and around the supporting wheel to be suitable for passing through the top opening of the crystal pulling chamber.

8. The single crystal silicon growth furnace according to claim 6, characterized in that: A pivot hole is formed on the top wall of the second shell, the crystal pulling chamber is penetrated through the pivot hole and pivotally matched with the pivot hole, and the second shell is supported on the bottom wall of the first chamber and pivotally matched with the bottom wall of the first chamber.

9. The single crystal silicon growth furnace according to claim 1, characterized in that: Also includes: A crucible driving mechanism, the crucible driving mechanism is used to drive the crucible assembly to move relative to the heating assembly; A weighing mechanism is disposed between the crucible assembly and the crucible driving mechanism and is used to weigh the bearing weight of the crucible assembly. The weighing mechanism is coaxially disposed with the crucible assembly.

10. The single crystal silicon growth furnace according to any one of claims 1 to 9, characterized in that: Also includes: A flow guide assembly, the flow guide assembly is disposed in the crystal growth chamber and is located on the upper side of the crucible assembly, the flow guide assembly is rotatably connected to the first shell around the central axis of the flow guide assembly; A second driving mechanism, wherein the second driving mechanism is used to drive the flow guide assembly to rotate relative to the first shell.

11. The single crystal silicon growth furnace according to claim 10, characterized in that: The first shell is formed with a first perspective window, the second shell is formed with a second perspective window, the flow guide assembly is formed with a perspective channel, and the perspective channel extends linearly toward the direction of the solid-liquid interface in the crucible assembly. The single crystal silicon growth furnace has a preset state, in which the first perspective window, the second perspective window and the perspective channel are on the same straight line.

12. A control method for a single crystal silicon growth furnace according to claim 10 or 11, characterized in that: The control method comprises: in the isodiameter growth stage of the single crystal silicon rod, Controlling the first housing to rotate clockwise relative to the second housing by the first driving mechanism; Controlling the crucible assembly to rotate counterclockwise relative to the first shell and controlling the crucible assembly to rotate clockwise relative to the second shell by a crucible driving mechanism; The second driving mechanism controls the flow guide assembly to rotate counterclockwise relative to the crucible assembly, and controls the flow guide assembly to rotate clockwise relative to the second shell.