Three-terminal leading-out chip type tantalum capacitor and manufacturing method thereof

By designing a three-terminal lead-out structure and optimizing manufacturing method in tantalum capacitors, the use of tantalum pentoxide dielectric film and conductive polymer materials can achieve polarity installation and high-frequency filtering effects, solving the filtering performance and structure of existing tantalum capacitors The shortcomings have improved the high-frequency performance and application fields of capacitors.

CN118983191APending Publication Date: 2024-11-19CHINA ZHENHUA GRP XINYUN ELECTRONICS COMP ANDDEV CO LTD
View PDF 0 Cites 0 Cited by

Patent Information

Application Number
CN202411201337.9
Authority / Receiving Office
CN · China
Patent Type
Applications(China)
Current Assignee / Owner
Filing Date
2024-08-29
Publication Date
2024-11-19

AI Technical Summary

Technical Problem

The existing three-terminal tantalum capacitors have problems in structural design and manufacturing methods that cannot achieve polarity-free installation and high-efficiency filtering effects, especially the ultra-low equivalent series inductance (ESL) and insufficient filtering performance.

Method used

By designing a three-end lead-out chip tantalum capacitor, including a tantalum core, shell, cathode terminal and anode terminal, a tantalum pentoxide dielectric film and conductive polymer material are used to combine silver paste and graphite layer to form a low-equivalent series inductor, to achieve The three ends of the positive electrode and the two negative electrodes are drawn out, and the structure and manufacturing process of the capacitor are optimized through welding and the use of adhesive layers.

Benefits of technology

It realizes polarity-free installation, shortens the current path, improves the filtering frequency band, overcomes the structural defects of traditional tantalum electrolytic capacitors, improves high-frequency performance and application fields, and has the characteristics of novel design, simple use and obvious effects.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure CN118983191A_ABST
    Figure CN118983191A_ABST
Patent Text Reader

Abstract

The invention discloses a three-terminal lead-out chip type tantalum capacitor and a manufacturing method thereof, the capacitor comprises a tantalum core, a shell, a cathode terminal and an anode terminal, the shell wraps the outer layer of the tantalum core, the cathode terminal is connected with the tantalum core, and the anode terminal is connected with the tantalum core through a lead frame. Through the innovation of a tantalum electrolytic capacitor leading-out end connection method, the characteristic that the capacitor has polarity is converted into non-polarity installation, one positive electrode input and two negative electrode outputs form a filter, the filter is converted into low equivalent series inductance through positive and negative electrode path shortening, and the filtering frequency band is improved. The tantalum electrolytic capacitor overcomes the defects of the existing tantalum electrolytic capacitor structure, improves the high-frequency performance of the capacitor, expands the application field, and has the characteristics of novel design, simplicity in use and obvious effect.
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] The invention belongs to the technical field of capacitors, and in particular relates to a three-terminal lead-out chip-type tantalum capacitor and a manufacturing method thereof. Background Art

[0002] In addition to the characteristics of traditional tantalum chip capacitors, the three-terminal lead-out chip tantalum capacitors also have the characteristics of ultra-low ESL. At the same time, if the internal structure can be cleverly designed to form a low-pass filter function, the high-frequency filtering effect can be improved. In addition, during the installation process, the non-polar chip tantalum capacitor has the characteristics of preventing installation short circuits, reverse voltages, ripple voltages, etc.

[0003] The patent document with the announcement number CN104240955A discloses a tantalum electrolytic capacitor, including a positive terminal, a negative terminal, a cathode and an anode tantalum core; the anode tantalum core is in the shape of a rectangular parallelepiped, the cathode covers the outer surface of the anode tantalum core, a positive terminal is arranged on one or two faces of the anode tantalum core, one end of the positive terminal passes through the cathode and is embedded in the anode tantalum core, and the other end is placed on the outside of the cathode, and the contact part between the positive terminal and the cathode is insulated by a tantalum pentoxide dielectric film; the outside of one or two faces of the non-positive lead-out surface of the cathode is connected to the negative terminal. The invention can eliminate the influence of the capacitor's own ESR and ESL on the filtering effect by converting the harmful equivalent series resistance ESR and equivalent series inductance ESL that the capacitor itself cannot block the interference signal into the beneficial ESR and ESL that can block the interference signal in the filter circuit. However, the lead-out of the patent is not a three-terminal lead-out; it does not have a non-polarity function; compared with the patent, the present application has the advantage of lower equivalent series inductance.

[0004] The patent document with announcement number CN218038878U discloses a tantalum electrolytic capacitor with reverse connection protection, including a plastic shell; a capacitor core is encapsulated inside the plastic shell, the outer end of the capacitor core is led out of the plastic shell through a negative foil, and the inside of the capacitor core is led out of the plastic shell through a tantalum wire and a positive foil, and the negative foil is provided with two terminals outside the plastic shell. This patent sets the positive electrode port in the middle of the surface of the tantalum electrolytic capacitor, and sets two negative electrode ports symmetrically on both sides of the positive electrode, so that the capacitor is not restricted by direction during installation and use, and avoids the circuit failure and burning of circuit components caused by the reverse installation of the positive and negative electrodes of the tantalum electrolytic capacitor. However, there are certain deficiencies in the manufacturing method, ultra-low equivalent series inductance (ESL), etc., and the above technical problems cannot be well solved. Summary of the invention

[0005] In order to solve the above technical problems, the present invention provides a three-terminal lead-out chip-type tantalum capacitor and a manufacturing method thereof.

[0006] The present invention is achieved through the following technical solutions.

[0007] The present invention provides a three-terminal lead-out chip tantalum capacitor, comprising a tantalum core, a shell, a cathode terminal and an anode terminal, wherein the shell is coated on the outer layer of the tantalum core, the cathode terminal is connected to the tantalum core, and the anode terminal is connected to the tantalum core through a lead frame.

[0008] Preferably, a fixing part and an adhesive layer A are provided on the shell, the fixing part is connected to one side of the cathode end, the adhesive layer A is connected to the other side of the cathode end, the cathode end is arranged on both sides of the lead frame, the cathode end is connected to the tantalum core through the adhesive layer B, and the cathode end is curved.

[0009] Preferably, the adhesive layer A is connected to one side of the wide end surface of the cathode, the adhesive layer B is made of silver paste, a fixing hole is provided on the fixing member, and the fixing member is connected to the housing through the fixing hole.

[0010] Preferably, the outer wall of the tantalum core is provided with a dielectric film, an outer layer A, an outer layer B and an outer layer C in sequence from the inside to the outside.

[0011] Preferably, the dielectric film is a tantalum pentoxide dielectric film, and the outer layer A material includes one or more of manganese dioxide, a conductive polymer or a non-solid electrolyte material.

[0012] Preferably, the outer layer B is made of graphite, and the outer layer C is made of silver paste.

[0013] Preferably, a groove is provided at one end of the lead frame close to the tantalum core, a tantalum wire is provided in the groove, and the tantalum wire is connected to the tantalum core via a connecting sheet, and the connecting sheet is a polytetrafluoroethylene sheet.

[0014] A method for manufacturing a three-terminal lead-out chip tantalum capacitor comprises the following steps:

[0015] S1: pressing tantalum powder and tantalum wire into a rectangular tantalum block;

[0016] S2: sintering the tantalum block at high temperature to obtain a tantalum core;

[0017] S3: forming a dielectric film on the inner and outer surfaces of the tantalum core;

[0018] S4: generating an outer layer A on the surface of the dielectric film;

[0019] S5: Dipping auxiliary materials on the surface of the tantalum core covered with the outer layer A to complete the extraction of the electrical performance parameters of the capacitor;

[0020] S6: placing the tantalum wire on the lead frame and connecting it by welding, placing the cathode terminal on the surface of the adhesive layer A and leading it out through the curing of the adhesive layer A, thus completing the three-terminal lead-out of one positive electrode and two negative electrodes;

[0021] S7: Encapsulate the outer shell.

[0022] Preferably, in step S2, the tantalum block is subjected to high-temperature sintering according to the specific volume of tantalum powder to obtain a tantalum core, wherein the specific volume of the tantalum powder is ≤23000uF.V / g, and the tantalum core is sintered at a temperature of 1600-2100°C for 15-45min.

[0023] Preferably, in step S4, the outer layer A is formed by immersing the dielectric membrane surface in a manganese nitrate solution and then performing a high-temperature thermal decomposition method, wherein the specific gravity of the manganese nitrate solution is 1.0-1.8, the solution temperature is 35-75° C., the immersion time in the manganese nitrate solution is 3-20 min, and high-temperature thermal decomposition is performed after the immersion is completed, the high-temperature thermal decomposition temperature is 190-310° C., and the time is 3-20 min.

[0024] Preferably, the auxiliary materials in step S5 include graphite and silver paste. After the surface is impregnated with the auxiliary materials, it is dried at room temperature for 10 to 45 minutes, and then cured at 40 to 200° C. The timing starts when the temperature reaches the set value, and the curing time is 20 to 50 minutes.

[0025] Preferably, the welding in step S6 includes resistance welding and laser welding, and the packaging method of the shell in step S7 includes molded plastic packaging, ceramic shell packaging, and metal shell packaging.

[0026] The beneficial effects of the present invention are:

[0027] The present invention, through the innovation of the connection method of the lead-out terminal of the tantalum electrolytic capacitor, transforms the polarity of the capacitor itself into a non-polar installation, forms a filter with one positive input and two negative outputs, and transforms it into a low equivalent series inductance by shortening the positive and negative paths, thereby improving the filtering frequency band. The defects of the existing tantalum electrolytic capacitor structure are overcome, the high-frequency performance of the capacitor is improved, and its application field is expanded, and it has the characteristics of novel design, simple use, and obvious effect. BRIEF DESCRIPTION OF THE DRAWINGS

[0028] Figure 1 It is a front view of the present invention;

[0029] Figure 2 is a top view of the present invention;

[0030] Figure 3 is a side view of the present invention;

[0031] Figure 4 is a bottom view of the present invention;

[0032] Figure 5 It is a schematic diagram of the structure of the tantalum core of the present invention;

[0033] Figure 6 It is the internal equivalent circuit diagram of the present invention;

[0034] In the figure: 1-tantalum core, 2-tantalum wire, 3-housing, 4-lead frame, 41-groove, 5-fixing piece, 6-cathode end, 7-adhesive layer A, 8-anode end, 9-adhesive layer B, 10-fixing hole, 11-connecting piece, 12-dielectric film, 13-outer layer A, 14-outer layer B, 15-outer layer C. DETAILED DESCRIPTION

[0035] The technical solution of the present invention is further described below, but the scope of protection claimed is not limited to the description.

[0036] Example:

[0037] like Figures 1 to 6 As shown, a three-terminal lead-out chip tantalum capacitor includes a tantalum core 1, a shell 3, a cathode terminal 6 and an anode terminal 8, wherein the shell 3 is coated on the outer layer of the tantalum core 1, the cathode terminal 6 is connected to the tantalum core 1, and the anode terminal 8 is connected to the tantalum core 1 through a lead frame 4.

[0038] A fixing part 5 and an adhesive layer A7 are provided on the shell 3, the fixing part 5 is connected to one side of the cathode terminal 6, the adhesive layer A7 is connected to the other side of the cathode terminal 6, the cathode terminal 6 is provided on both sides of the lead frame 4, the cathode terminal 6 is connected to the tantalum core 1 through the adhesive layer B9, and the cathode terminal 6 is curved.

[0039] The adhesive layer A7 is connected to one side of the wide surface of the cathode terminal 6 . The adhesive layer B9 is made of silver paste. A fixing hole 10 is provided on the fixing member 5 . The fixing member 5 is connected to the housing 3 through the fixing hole 10 .

[0040] The outer wall of the tantalum core 1 is provided with a dielectric film 12, an outer layer A13, an outer layer B14 and an outer layer C15 in sequence from the inside to the outside.

[0041] The oxide film 12 is a tantalum pentoxide dielectric film, and the outer layer A13 material includes one or more of manganese dioxide, conductive polymer or non-solid electrolyte material. Conductive polymer means that the cathode material is a conductive polymer; non-solid electrolyte material means that the cathode is not solid and is used as a liquid cathode by immersing in a conductive solution.

[0042] The material of the outer layer B14 is graphite, and the material of the outer layer C15 is silver paste.

[0043] The lead frame 4 is provided with a groove 41 at one end close to the tantalum core 1 , and the tantalum wire 2 is arranged in the groove 41 . The tantalum wire 2 is connected to the tantalum core 1 through a connecting sheet 11 , and the connecting sheet 11 is a polytetrafluoroethylene sheet.

[0044] A method for manufacturing a three-terminal lead-out chip tantalum capacitor comprises the following steps:

[0045] S1: pressing tantalum powder and tantalum wire into a rectangular tantalum block with a certain strength;

[0046] S2: sintering the tantalum block at different temperatures according to the specific volume of the tantalum powder to obtain a tantalum core 1;

[0047] S3: forming a dielectric film 12 on the inner and outer surfaces of the porous tantalum core 1 by electrochemical treatment;

[0048] S4: forming an outer layer A13 by immersing the surface of the dielectric film 12 in manganese nitrate solutions of different specific gravities and then performing high temperature thermal decomposition;

[0049] S5: dipping auxiliary materials on the surface of the tantalum core 1 covered with the outer layer A13 to complete the extraction of the electrical performance parameters of the capacitor;

[0050] S6: placing the tantalum wire 2 on the lead frame 4 and connecting them by welding, placing the cathode terminal 6 on the two bonding layers A7 and leading them out through the curing of the bonding layers A7, thus completing the three-terminal lead-out of one positive electrode and two negative electrodes;

[0051] S7: The housing 3 is packaged.

[0052] In the step S2, the tantalum block is sintered at different temperatures according to the specific volume of the tantalum powder to obtain the tantalum core 1. The tantalum powder has a specific volume of ≤23000uF.V / g and is sintered at a temperature of 1600-2100°C for 15-45min.

[0053] The electrochemical treatment step in step S3 includes:

[0054] A phosphoric acid aqueous solution, a nitric acid aqueous solution and an ethylene glycol solution are used, and the solution temperature is 25 to 90°C. According to different tantalum powder specific volumes, different tantalum block powder weights and other conditions, a current density of 5 to 100 mA / g is applied to boost the voltage. After the boosting is completed, a constant voltage is used to improve the uniformity and consistency of the dielectric film 12, that is, the dielectric oxide film, and the constant voltage time is 30 minutes to 12 hours; after the constant voltage is completed, high-temperature boiling and washing are performed at a temperature of 75 to 100°C for 1 to 8 hours; after the boiling and washing is completed, heat treatment is performed at a temperature of 250 to 420°C for 10 to 60 minutes; finally, fill formation is performed for 30 to 360 minutes to complete the chemical formation of the dielectric film 12.

[0055] In the step S4, the outer layer A13 is generated by immersing the surface of the dielectric membrane 12 in manganese nitrate solutions of different specific gravities and then performing high-temperature thermal decomposition. The specific gravity of the manganese nitrate solution is 1.0-1.8, and it is divided into different specific gravity solution steps. The solution temperature is 35-75° C., and the solution specific gravities are immersed for different times (the number of times is greater than 1). The immersion time in the manganese nitrate solution is 3-20 minutes. After the immersion, high-temperature thermal decomposition is performed. The high-temperature thermal decomposition temperature is 190-310° C. and the time is 3-20 minutes.

[0056] The auxiliary materials in step S5 include graphite and silver paste. After the surface is impregnated with the auxiliary materials, it is dried at room temperature for 10 to 45 minutes, and then placed in a high-temperature oven for curing at 40 to 200° C. The timing starts when the temperature reaches the set value, and the curing time is 20 to 50 minutes;

[0057] The welding in step S6 includes resistance welding and laser welding, and the packaging method of the shell 3 in step S7 includes molded plastic packaging, ceramic shell packaging, and metal shell packaging.

[0058] Combination Figure 1 , Figure 2 , Figure 3 ,and Figure 4 A basic structural schematic diagram of the present invention is given. It can be seen from the accompanying drawings that the present invention is a three-terminal lead-out chip-type solid electrolyte tantalum capacitor. The positive terminal is designed in the middle of the shape, which does not affect the polarity selection of the two ends of the product, so it has the characteristics of a non-polar capacitor.

[0059] Figure 6 The capacitor shown is input from the positive pole, and the two negative poles on the left and right are two capacitors, which form a filter after being connected in series with its internal inductance, and have the performance characteristics of a filter; the structure is a bottom lead structure, the lead path is short, and its equivalent series inductance is small, which can broaden its frequency characteristics. Therefore, the structure of the present invention is completely different from that of the traditional chip-type solid electrolyte tantalum capacitor. The tantalum core anode tantalum wire is welded on the side positive lead frame anode pillow, and the wide cathode surface is bonded and solidified on the cathode bonding surface on both sides with bonding silver paste to complete the non-polar three-terminal lead chip tantalum capacitor.

[0060] Figure 5 The manufacturing of the tantalum core shown in the figure first presses the tantalum powder particles into shape according to the design, and performs vacuum sintering to obtain the anode tantalum core 1, and then forms a dielectric film 12 by electrochemistry, that is, a tantalum pentoxide dielectric oxide film, and then covers the dielectric film 12 with a manganese dioxide outer layer A13 as a cathode, and the surface of the outer layer A13 is impregnated with a graphite outer layer B14 and a silver paste outer layer C15 as auxiliary leads. The tantalum wire of the tantalum core anode is welded to the lead frame 4, and the surface of the wide cathode end 6 is bonded and cured to the bonding layer 7 with bonding silver paste, and is limited by the cathode tantalum core limiting plate and the fixing plate 5 to avoid left and right displacement, and the product is molded and sealed with an epoxy resin shell 3.

Claims

1. A three-terminal lead-out chip tantalum capacitor, Features: The invention comprises a tantalum core (1), a shell (3), a cathode terminal (6) and an anode terminal (8), wherein the shell (3) is coated on the outer layer of the tantalum core (1), the cathode terminal (6) is connected to the tantalum core (1), and the anode terminal (8) is connected to the tantalum core (1) via a lead frame (4).

2. A three-terminal lead-out chip tantalum capacitor as claimed in claim 1, Features: A fixing part (5) and an adhesive layer A (7) are provided on the housing (3); the fixing part (5) is connected to one side of the cathode end (6); the adhesive layer A (7) is connected to the other side of the cathode end (6); the cathode end (6) is provided on both sides of the lead frame (4); the cathode end (6) is connected to the tantalum core (1) via an adhesive layer B (9); and the cathode end (6) is in a curved shape.

3. A three-terminal lead-out chip tantalum capacitor as claimed in claim 2, Features: The adhesive layer A (7) is connected to one side of the wide surface of the cathode terminal (6); the adhesive layer B (9) is made of silver paste; a fixing hole (10) is provided on the fixing member (5); and the fixing member (5) is connected to the housing (3) through the fixing hole (10).

4. A three-terminal lead-out chip tantalum capacitor as claimed in claim 1, Features: The outer wall of the tantalum core (1) is provided with a dielectric film (12), an outer layer A (13), an outer layer B (14) and an outer layer C (15) in sequence from the inside to the outside.

5. A three-terminal lead-out chip tantalum capacitor as claimed in claim 4, Features: The dielectric film (12) is a tantalum pentoxide dielectric film, and the material of the outer layer A (13) includes one or more of manganese dioxide, a conductive polymer or a non-solid electrolyte material; The material of the outer layer B (14) is graphite, and the material of the outer layer C (15) is silver paste.

6. A three-terminal lead-out chip tantalum capacitor as claimed in claim 1, Features: A groove (41) is arranged at one end of the lead frame (4) close to the tantalum core (1), a tantalum wire (2) is arranged in the groove (41), and the tantalum wire (2) is connected to the tantalum core (1) via a connecting sheet (11); the connecting sheet (11) is a polytetrafluoroethylene sheet.

7. A method for manufacturing a three-terminal lead-out chip tantalum capacitor according to any one of claims 1 to 6, It is characterized in that The following steps are involved: S1: pressing tantalum powder and tantalum wire into a rectangular tantalum block; S2: sintering the tantalum block at a high temperature to obtain a tantalum core (1); S3: forming a dielectric film (12) on the inner and outer surfaces of the tantalum core (1); S4: generating an outer layer A (13) on the surface of the dielectric film (12); S5: dipping auxiliary materials on the surface of the tantalum core (1) covered with the outer layer A (13) to complete the extraction of the electrical performance parameters of the capacitor; S6: placing the tantalum wire (2) on the lead frame (4) and connecting them by welding, placing the cathode terminal (6) on the surface of the adhesive layer A (7) and leading out through the curing of the adhesive layer A (7), thereby completing the three-terminal lead-out of one positive electrode and two negative electrodes; S7: Packaging of the housing (3) is performed.

8. A method for manufacturing a three-terminal lead-out chip tantalum capacitor as claimed in claim 7, Features: In the step S2, the tantalum block is subjected to high temperature sintering according to the specific volume of the tantalum powder to obtain a tantalum core (1), wherein the specific volume of the tantalum powder is ≤23000uF.V / g, and the tantalum core (1) is sintered at a temperature of 1600-2100°C for 15-45 minutes.

9. A method for manufacturing a three-terminal lead-out chip tantalum capacitor as claimed in claim 7, Features: In the step S4, the outer layer A (13) is formed by immersing the dielectric film (12) in a manganese nitrate solution and then performing a high-temperature thermal decomposition method. The specific gravity of the manganese nitrate solution is 1.0 to 1.8, the solution temperature is 35 to 75° C., the immersion time is 3 to 20 minutes, and high-temperature thermal decomposition is performed after the immersion. The high-temperature thermal decomposition temperature is 190 to 310° C. and the time is 3 to 20 minutes.

10. A method for manufacturing a three-terminal lead-out chip tantalum capacitor as claimed in claim 7, Features: The auxiliary materials in step S5 include graphite and silver paste. After the surface is impregnated with the auxiliary materials, it is dried at room temperature for 10 to 45 minutes, and then cured at 40 to 200° C. The timing starts when the temperature reaches the set value, and the curing time is 20 to 50 minutes; The welding in step S6 includes resistance welding and laser welding, and the packaging method of the shell (3) in step S7 includes molded plastic packaging, ceramic shell packaging, and metal shell packaging.