Low-binding-energy solvent for low-temperature lithium ion battery electrolyte and application of low-binding-energy solvent

By introducing strong electronegative groups into solvent molecules, the binding energy of lithium ions and solvents is reduced, the problems of increasing viscosity and conductivity of electrolytes in low-temperature lithium ion batteries are solved, and the low-temperature capacity and cycling performance of lithium ion batteries are improved .

CN118983529AInactive Publication Date: 2024-11-19LANZHOU UNIVERSITY OF TECHNOLOGY
View PDF 6 Cites 0 Cited by

Patent Information

Application Number
CN202411367907.1
Authority / Receiving Office
CN · China
Patent Type
Applications(China)
Current Assignee / Owner
Filing Date
2024-09-29
Publication Date
2024-11-19
Estimated Expiration
Not applicable · inactive patent

AI Technical Summary

Technical Problem

Under low temperature conditions, the electrolyte viscosity of lithium-ion batteries increases and the conductivity decreases, resulting in a decrease in the migration rate and diffusion rate of lithium ions, affecting the electrochemical performance. The binding energy of solvents and lithium ions makes it difficult for lithium ions to desolvate, resulting in the battery Reaction kinetic rate slows down.

Method used

Introducing strong electronegative groups, such as halogen atoms (-F, -Cl) into the solvent molecules, reduce the binding energy of lithium ions and solvents, improve the desolvation process of lithium ions, and improve battery capacity and cycling performance.

Benefits of technology

By reducing the binding energy of lithium ions and solvents, the desolvation of lithium ions is promoted, the capacity and circulation performance of low-temperature lithium ion batteries are improved, and the electrochemical performance is significantly improved.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure CN118983529A_ABST
    Figure CN118983529A_ABST
Patent Text Reader

Abstract

The invention provides a low-binding-energy solvent for a low-temperature lithium ion battery electrolyte, which is prepared by introducing a strong electronegative group to a matrix solvent molecule, and also provides application of the low-binding-energy solvent for preparing the low-temperature lithium ion battery electrolyte. According to the low-binding-energy electrolyte for the low-temperature lithium ion battery, the electron cloud density of oxygen on solvent molecules is reduced by introducing strong electronegativity groups into the solvent molecules, so that the binding energy of the solvent molecules and lithium ions is reduced, the potential barrier in the desolvation process of the lithium ions is reduced, the desolvation process of the lithium ions is promoted, and the lithium ion battery performance is improved. And thus, the capacity and cycle performance of the lithium ion battery at low temperature are improved.
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] The invention belongs to the technical field of electrochemical energy storage, and in particular relates to a low binding energy solvent for low-temperature lithium-ion battery electrolyte and an application thereof. Background Art

[0002] With the rapid development of electric vehicles and grid-scale energy storage, people have increased their demand for the performance of lithium-ion batteries in extreme environments. Especially at low temperatures, the performance of traditional lithium-ion batteries is seriously degraded, and even lithium dendrites are generated, leading to safety accidents.

[0003] The reason is that under low temperature conditions, the solvent molecules and lithium ions (Li + ) enhances the interaction between the solvent and Li, which increases the viscosity of the electrolyte and reduces the conductivity, thereby reducing the migration rate of lithium ions in the bulk electrolyte, the diffusion rate in the electrode, and the charge transfer rate. + The greater the binding energy of Li + The more difficult it is to break free from the constraints of the solvent at the electrode-electrolyte interface, the slower the overall reaction kinetics rate inside the battery, resulting in poor electrochemical performance. In order to solve the above-mentioned problems faced by lithium-ion batteries under low temperature conditions, low-temperature electrolyte systems have been designed from the aspects of selecting low-viscosity solvents, using new salts or increasing the concentration of lithium salts, which can effectively improve the conductivity of the electrolyte. However, the choice of solvent has limitations on the solubility of lithium salts. Therefore, inventing a design method with low binding energy solvents has important practical significance and application value for the development of low-temperature lithium-ion battery electrolytes. Summary of the invention

[0004] The technical problem to be solved by the present invention is to provide a low binding energy solvent for low-temperature lithium-ion battery electrolyte and its application in view of the above-mentioned deficiencies in the prior art. The low binding energy solvent introduces strongly electronegative groups into the matrix solvent molecules, thereby improving the capacity and cycle performance of the lithium-ion battery at low temperatures.

[0005] To solve the above technical problems, the technical solution adopted by the present invention is: a low binding energy solvent for low-temperature lithium-ion battery electrolyte, wherein the low binding energy solvent is obtained by introducing strongly electronegative groups into the matrix solvent molecules.

[0006] Preferably, the matrix solvent molecules are ether solvents or carboxylate solvents;

[0007] The strongly electronegative group is a halogen atom (-F, -Cl).

[0008] Preferably, when the matrix solvent molecule is an ether solvent, the molecular structure of the low binding energy solvent is: or ROZ, wherein R is an alkyl group and Z is the strongly electronegative group;

[0009] When the matrix solvent molecule is a carboxylate solvent, the molecular structure formula of the low binding energy solvent is: or Wherein R is an alkyl group, and Z is the strongly electronegative group.

[0010] Preferably, when the matrix solvent molecule is an ether solvent, the matrix solvent molecule is tetrahydrofuran or ethylene glycol dimethyl ether;

[0011] When the matrix solvent molecule is a carboxylic acid ester solvent, the matrix solvent molecule is ethyl acetate.

[0012] The present invention also provides the above-mentioned low binding energy solvent for low-temperature lithium ion battery electrolyte, and the low binding energy solvent is used to prepare low-temperature lithium ion battery electrolyte.

[0013] Preferably, the concentration of the lithium salt in the low-temperature lithium-ion battery electrolyte is 0.5-1.5 mol / L.

[0014] Preferably, the lithium salt is lithium bis(fluorosulfonyl)imide (LiFSI).

[0015] The positive electrode material of lithium-ion batteries is LiFePO4; the negative electrode material of lithium-ion batteries is graphite.

[0016] Compared with the prior art, the present invention has the following advantages:

[0017] The low binding energy electrolyte used in the low-temperature lithium-ion battery of the present invention is prepared by introducing electron-withdrawing groups into the solvent molecules to reduce the electron cloud density of oxygen on the solvent molecules, thereby reducing the binding energy between the solvent molecules and lithium ions, reducing the barrier of the lithium ion desolvation process, thereby promoting the lithium ion desolvation process, and further improving the capacity and cycle performance of the lithium-ion battery at low temperatures.

[0018] The present invention is further described in detail below with reference to the accompanying drawings and embodiments. BRIEF DESCRIPTION OF THE DRAWINGS

[0019] Figure 1 This is a comparison diagram of the electrostatic potential distribution of solvent molecules in the conventional electrolyte prepared in Comparative Example 1, the high binding energy electrolyte prepared in Comparative Example 2, and the low-temperature and low binding energy electrolyte prepared in Example 1.

[0020] Figure 2 Comparison diagram of the binding energy and ESP distribution of lithium ions and solvent molecules in the conventional electrolyte prepared in Comparative Example 1, the high binding energy electrolyte prepared in Comparative Example 2, and the low-temperature and low binding energy electrolyte prepared in Example 1.

[0021] Figure 3 This is a comparison chart of Raman test results of the conventional electrolyte prepared in Comparative Example 1, the high binding energy electrolyte prepared in Comparative Example 2, and the low-temperature and low binding energy electrolyte prepared in Example 1.

[0022] Figure 4 This is a comparison chart of Fourier transform infrared test results of the conventional electrolyte prepared in comparative example 1, the high binding energy electrolyte prepared in comparative example 2, and the low temperature and low binding energy electrolyte prepared in example 1.

[0023] Figure 5 This is a comparison diagram of the desolvation potential of lithium ions in the conventional electrolyte prepared in Comparative Example 1, the high binding energy electrolyte prepared in Comparative Example 2, and the low-temperature and low binding energy electrolyte prepared in Example 1.

[0024] Figure 6 The figure is a comparison chart of the LiFePO4||Li half-cell cycle performance test under -20°C conditions for the conventional electrolyte prepared in Comparative Example 1, the high binding energy electrolyte prepared in Comparative Example 2, and the low-temperature low binding energy electrolyte prepared in Example 1.

[0025] Figure 7 This is the electrostatic potential diagram of the solvent after different numbers of strongly electronegative groups -F are introduced into ethyl acetate in Example 2.

[0026] Figure 8 After introducing different numbers of electronegative groups into the EA solvent in Example 2, Li + The distance from the solvent changes.

[0027] Fig. 9 is the activation energy of the EA electrolyte with different -F groups introduced in Example 2 in the LiFePO4||Li half-cell.

[0028] Fig.10 In Example 2, the cycling performance of LiFePO4||Li half-cells composed of EA electrolytes with different -F groups introduced at -20°C and a rate of 0.2C was compared.

[0029] Fig.11 The electrostatic potential diagram of ethylene glycol dimethyl ether and ethylene glycol dimethyl ether with -F group introduced in Example 3.

[0030] Fig.12 is Li in Example 3 + Binding energies with two solvents, DME and DME-F.

[0031] Fig.13 The cycling performance of the graphite (Gr)||Li half-cell assembled with two electrolyte systems in Example 3 at -20°C and 0.2C rate. DETAILED DESCRIPTION

[0032] The preparation process of the lithium-ion battery positive electrode material used in the comparative examples and embodiments of the present invention is as follows: 80wt% of LiFePO4 positive electrode material powder or graphite (Gr) negative electrode material powder, 10wt% of conductive agent acetylene black, and 10wt% of binder PVDF are fully mixed, and then N-methylpyrrolidone is added and stirred evenly to obtain positive or negative electrode material electrode slurry; then, the obtained slurry is evenly coated on aluminum foil, dried, rolled, and then cut into circular pole pieces with a diameter of 14mm by a punching machine to obtain lithium-ion battery positive or negative pole pieces.

[0033] LiFSI (lithium bis(fluorosulfonyl)imide) was added to THF to make the final concentration of LiFSI 1 mol·L -1 , that is, 1 mol·L -1 LiFSI THF electrolyte;

[0034] THF and MeTHF were mixed in equal volumes and LiFSI was added to make the final concentration of LiFSI 1 mol·L -1 , that is, 1 mol·L -1 LiFSI THF / MeTHF electrolyte;

[0035] THF and THFCl were mixed in equal volumes and then LiFSI was added to make the final concentration of LiFSI 1 mol·L -1 , that is, 1 mol·L -1 LiFSI THF / THFCl electrolyte;

[0036] Two strong electronegative groups (-F) were introduced into ethyl acetate (EA) to obtain EA-2F; three strong electronegative groups (-F) were introduced into ethyl acetate (EA) to obtain EA-3F; after adding LiFSI with EA-2F as solvent, the final concentration of LiFSI was 1 mol·L -1 , that is, 1 mol·L -1 LiFSI EA-2F electrolyte;

[0037] A mixture of EA-2F and EA-3F in equal volume ratio was used as solvent. After adding LiFSI, the final concentration of LiFSI was 1 mol·L -1 , to obtain 1 mol·L -1 LiFSI EA-2F / EA-3F electrolyte;

[0038] A strong electronegative group (-F) was introduced into ethylene glycol dimethyl ether (DME) to obtain DME-F solvent. After adding LiFSI into DME as solvent, the final concentration of LiFSI was 1 mol·L -1 , to obtain 1 mol L-1 LiFSIDME electrolyte. DME-F was used as solvent and LiFSI was added to make the final concentration of LiFSI 1 mol·L -1 , to obtain 1 mol L -1 LiFSIDME-F electrolyte.

[0039] The above-mentioned electrolytes are the electrolytes used in Comparative Examples 1-2 and Examples 1-3.

[0040] Seal the centrifuge tubes containing the electrolytes configured in the above-mentioned comparative examples and embodiments respectively and shake until LiFSI is completely dissolved, and let stand for use. The configuration of the electrolytes in all the above-mentioned comparative examples and embodiments and the assembly of the corresponding lithium-ion batteries are carried out in a glove box with a high-purity argon environment (H2O content is less than 0.1ppm, O2 content is less than 0.1ppm). The above-mentioned electrolytes are used as the test electrolyte system, LiFePO4 positive electrode or Gr negative electrode is used as the working electrode, and lithium sheet is used as the counter electrode to assemble into a 2025 type button half-cell, and the test is carried out after standing for 12h.

[0041] Comparative Example 1

[0042] Using tetrahydrofuran (THF) as solvent, the calculated amount of LiFSI was prepared with THF to obtain 1 mol·L - 1 LiFSI+THF electrolyte, after LiFSI is completely dissolved in THF, a conventional electrolyte is obtained. It is applied to LiFePO4||Li half-cells to test the electrochemical performance of LiFePO4||Li half-cells and the properties of the electrolyte at -20°C.

[0043] Comparative Example 2

[0044] A strong positively charged group (-CH3) was introduced into tetrahydrofuran (THF), and THF and 2-methyltetrahydrofuran (MeTHF) mixed in equal volume ratio were used as solvents. The calculated corresponding amount of LiFSI was prepared with THF and MeTHF to obtain 1 mol·L - 1 LiFSI THF / MeTHF electrolyte, after LiFSI is completely dissolved in the mixed solvent of THF and MeTHF, an electrolyte with strong positive groups introduced into the solvent is obtained. It is applied to LiFePO4||Li half-cell to test the electrochemical performance of LiFePO4||Li half-cell and the properties of the electrolyte at -20℃.

[0045] Example 1

[0046] A strong electronegative group (-Cl) was introduced into tetrahydrofuran (THF), and an equal volume mixture of THF and tetrahydrofuran chloride (THFCl) was used as solvent. The calculated corresponding amount of LiFSI was prepared with THF and THFCl to obtain 1 mol·L -1 LiFSI THF / THFCl electrolyte, after LiFSI is completely dissolved in the mixed solvent of THF and THFCl, a low-temperature low-binding-energy electrolyte with strong electronegative groups introduced into the low-binding-energy solvent is obtained. It is applied to LiFePO4||Li half-cells to test the electrochemical performance of LiFePO4||Li half-cells at -20°C and the properties of the electrolyte.

[0047] Example 2

[0048] Two strong electronegative groups (-F) were introduced into ethyl acetate (EA) to obtain EA-2F; three strong electronegative groups (-F) were introduced into ethyl acetate (EA) to obtain EA-3F; after adding LiFSI with EA-2F as solvent, the final concentration of LiFSI was 1 mol·L -1 , that is, 1 mol·L -1 LiFSI EA-2F electrolyte;

[0049] A mixture of EA-2F and EA-3F in equal volume ratio was used as solvent. After adding LiFSI, the final concentration of LiFSI was 1 mol·L -1 , to obtain 1 mol·L -1 LiFSI EA-2F / EA-3F electrolyte;

[0050] 1 mol·L -1 LiFSI EA-2F electrolyte and 1 mol·L -1 LiFSI EA-2F / EA-3F electrolytes were used in LiFePO4||Li half-cells, and the electrochemical performance of LiFePO4||Li half-cells and the properties of the electrolytes were tested at -20°C.

[0051] Example 3

[0052] A strong electronegative group (-F) was introduced into ethylene glycol dimethyl ether (DME) to obtain DME-F solvent;

[0053] DME was used as solvent and LiFSI was added to make the final concentration of LiFSI 1 mol·L -1 , to obtain 1 mol L - 1 LiFSIDME electrolyte.

[0054] DME-F was used as solvent and LiFSI was added to make the final concentration of LiFSI 1 mol·L -1 , to obtain 1 mol L - 1 LiFSIDME-F electrolyte.

[0055] 1 mol L -1 LiFSIDME electrolyte and 1 mol L -1 LiFSIDME-F electrolyte was applied to Gr||Li half-cells to test the electrochemical performance of Gr||Li half-cells and the properties of the electrolyte at -20°C.

[0056] Figure 1 The ESP distribution on the surface of different solvent molecules reveals the possible interactions between solvent molecules and Li + The negative region on THF is centered on the O atom, so Li + It tends to combine with oxygen atoms with more negative charges on THF. Affected by the introduction of different electron effect groups on the solvent molecules, the O atoms on THFCl with the introduction of strong electronegative groups show a lower degree of negative area, and the O atoms on MeTHF with the introduction of electron-donating groups show a higher degree of negative area. This shows that compared with THF and solvent molecules with the introduction of strong electronegative groups, the introduction of strong electronegative groups reduces the electron cloud density on oxygen atoms in the solvent.

[0057] Figure 2 Researched Li + The binding energy with different solvent molecules is affected by the change of the electron cloud density distribution on the O atoms in the solvent molecules. + The binding energy with THFCl introduced with strong electronegative groups is only -42.75 kcal mol -1 , while the binding energies with THF and MeTHF are -47.93 kcal mol -1 and -49.43 kcal mol -1 The results show that the electron cloud density on the O atom in MeTHF introduced with the electron-donating group increases, which will lead to the Li + The solvation ability is enhanced; on the contrary, the reduction of the electron cloud density of O on the THFCl solvent molecule with the introduction of a strong electronegative group will weaken the ion-dipole interaction, resulting in the solvent molecule and Li + The binding becomes weaker and changes Li + The solvation structure of Li + desolvation process.

[0058] Figure 3Raman test The electrolyte systems in Comparative Examples 1-2 and Example 1 were compared with pure lithium salt LiFSI to reveal the interaction between solvent, cations and anions. It can be seen from the spectrum of pure lithium salt LiFSI that FSI - The bending peak of SNS appears at 774 cm -1 When LiFSI is dissolved in THF / MeTHF solvent, FSI - The SNS bending peak has a significant red shift (716cm -1 ), which shows that Li + With FSI - Strong dissociation. In the electrolyte system of Comparative Example 1, FSI - The red shift of the SNS bending peak is much smaller. In the electrolyte of Example 1 after the introduction of the strong electronegative group, FSI - The SNS bending peak shifts the least, from 774cm -1 To 738cm -1 These results show that at 1 mol L -1 In LiFSI THF / THFCl, Li + With FSI - The strongest interaction exists, more ion pairs are generated in the electrolyte, and anion-rich CIP and AGG type solvation structures are formed. This is because the introduction of strong electronegative groups on the solvent molecules can reduce the Li + The ion-dipole interaction with the solvent promotes the entry of anions into the Li + of the solvation shell.

[0059] Figure 4 Fourier transform infrared test The electrolyte systems in Comparative Examples 1-2 and Example 1 were compared with the corresponding pure solvents to reveal the interaction between the solvent, cations and anions. The ether functional group COC has a wavelength of 1300-1000 cm -1 There is a strong infrared absorption peak, which depends on the local environment of the ether bond. + The peak will shift during coordination. The peak position of the solvent without coordination is about 1066cm -1 , this peak is the stretching vibration peak of COC. After LiFSI is introduced into the solvent, the peak shifts slightly. The COC peak in Example 1 shifts slightly compared with that in Comparative Example 1, while the peak shifts significantly in Comparative Example 2, indicating that there is a relatively weak interaction between the solvent and LiFSI in Example 1, while the interaction between the solvent and the lithium salt in Comparative Example 2 is relatively strong. The FT-IR results show that the Li in Example 1 in the three electrolyte systems + There is the weakest ion-dipole interaction with solvent molecules.

[0060] Figure 5 The Li + The desolvation potential of the electrolyte system in Example 1 is the smallest, which indicates that the lithium ions in this system are most likely to achieve Li + of desolvation.

[0061] Figure 6 The cycling performance of the LiFePO4||Li half-cells of the three electrolytes in Comparative Examples 1-2 and Example 1 at -20°C and 0.2C rate is shown. The initial discharge capacity of the battery with the electrolyte containing strong electronegative groups is 78.4 mAh g -1 After 100 cycles, the capacity retention rate is 90.43%. The initial discharge capacity of the battery with THF-based electrolyte is 101.7 mAh g -1 After 100 cycles, the capacity retention rate was 91.15%. The battery with the strong electronegative group electrolyte showed the best discharge capacity, which was 109.1 mAh g -1 After 100 cycles, the capacity retention rate is still 93.22%. This shows that the low binding energy electrolyte with electron-withdrawing groups is beneficial to improving the discharge capacity and cycle stability of lithium-ion batteries with LiFePO4 as the positive electrode material at low temperatures.

[0062] Figure 7 The electrostatic potential diagram of the solvent after different numbers of strongly electronegative groups -F were introduced into ethyl acetate (EA) in Example 2 shows that as the number of strongly electronegative groups introduced increases, the electron cloud density on C=O decreases, which will lead to Li + The interaction with the solvent is reduced.

[0063] Figure 8 The results show that the Li + The distance between Li + The distance between Li and the solvent increases. Without the introduction of the strong electronegative group -F, + The distance between the solvent molecules is When a -F group is introduced, the distance increases to When two -F groups are introduced, the distance increases to When three -F groups are introduced, the distance increases to This further proves that with the introduction of strong electronegative groups, Li + The interaction with the solvent is reduced, which is more conducive to Li + From the electrolyte into the electrode material, thereby improving its low-temperature performance.

[0064] Fig. 9 The activation energy of EA electrolytes with different -F groups introduced in LiFePO4||Li half-cells was compared. It can be concluded that in Example 2, the activation energy of the electrolyte prepared by the mixed solvents with two and three -F groups introduced is the smallest, which indicates that lithium ions in this system are more likely to achieve Li + of desolvation.

[0065] Fig.10 The cycling performance of the LiFePO4||Li half-cell composed of EA electrolytes with different -F groups was tested and compared at -20°C and 0.2C rate. The initial discharge capacity of the battery assembled by the electrolyte with two -F groups was 135 mAh g -1 After 100 cycles, the capacity retention rate was 97.6%. The initial discharge capacity of the battery assembled with the electrolyte prepared by introducing two or three -F groups was 143 mAh g -1 After 100 cycles, the capacity retention rate was 99.3%. This shows that the introduction of low binding energy electrolyte with strong electronegative groups is beneficial to improving the discharge capacity and cycle stability of lithium-ion batteries with LiFePO4 as the positive electrode material at low temperatures.

[0066] Fig.11 The electrostatic potential diagram of ethylene glycol dimethyl ether (DME) and ethylene glycol dimethyl ether with -F group (DME-F, i.e. fluoroethylene glycol dimethyl ether) in Example 3 shows that with the introduction of -F group, the electron cloud density on DME (O) decreases, which will lead to Li + The interaction with the solvent is reduced.

[0067] Fig.12 Compared with Li in Example 3 + The binding energies of Li with DME and DME-F are found + The binding energy with DME-F is small. + Compared with the -69.84 kcal mol presented by DME -1 The binding energy of Li + The binding energy with DME-F is only -46.73 kcal mol -1 , which means Li + It is easier to break free from the constraints of DME-F solvent molecules on the electrode surface and enter the electrode material to achieve charge storage.

[0068] Fig.13 The cycling performance of the graphite (Gr)||Li half-cell assembled with the two electrolyte systems in Example 3 at -20°C and 0.2C rate is compared. It can be seen that due to the introduction of the strongly electronegative group -F, 1.0 mol L -1The initial capacity of the battery of LiFSIDME-F system is 196.7 mAh g -1 After 200 cycles, the capacity still shows an upward trend. The initial capacity of the battery of the original 1.0 mol / L LiFSIDME system can reach 216.5 mAh g -1 However, during the cycle, the capacity decayed rapidly, and after 200 cycles, the remaining capacity was only 181.2 mAh g -1 ; It shows that the battery cycle performance is greatly improved after the introduction of fluoroethylene glycol dimethyl ether (DME-F) solvent with weaker binding energy.

[0069] The low binding energy solvent in the present invention is obtained by introducing a strong electronegative group into the matrix solvent molecule, wherein the strong electronegative group is a halogen atom (-F, -Cl).

[0070] When the matrix solvent molecule is an ether solvent, such as tetrahydrofuran and ethylene glycol dimethyl ether, the molecular structure formula of the low binding energy solvent is: or ROZ, wherein R is an alkyl group and Z is the strongly electronegative group;

[0071] When the matrix solvent molecule is a carboxylic acid ester solvent, such as ethyl acetate, the molecular structure formula of the low binding energy solvent is: or Wherein R is an alkyl group, and Z is the strongly electronegative group.

[0072] The above is only a preferred embodiment of the present invention and does not limit the present invention in any way. Any simple modification, change and equivalent change made to the above embodiment according to the technical essence of the invention still falls within the protection scope of the technical solution of the present invention.

Claims

1. A low binding energy solvent for low temperature lithium ion battery electrolyte, characterized in that: The low binding energy solvent is obtained by introducing a strong electronegative group into a matrix solvent molecule.

2. The low binding energy solvent for low temperature lithium ion battery electrolyte according to claim 1, characterized in that: The matrix solvent molecules are ether solvents or carboxylate solvents; The strong electronegative group is a fluorine atom or a chlorine atom.

3. The low binding energy solvent for low temperature lithium ion battery electrolyte according to claim 2, characterized in that: When the matrix solvent molecule is an ether solvent, the molecular structure formula of the low binding energy solvent is: or ROZ, wherein R is an alkyl group and Z is the strongly electronegative group; When the matrix solvent molecule is a carboxylate solvent, the molecular structure formula of the low binding energy solvent is: or Wherein R is an alkyl group, and Z is the strongly electronegative group.

4. The low binding energy solvent for low temperature lithium ion battery electrolyte according to claim 3, characterized in that: When the matrix solvent molecule is an ether solvent, the matrix solvent molecule is tetrahydrofuran or ethylene glycol dimethyl ether; When the matrix solvent molecule is a carboxylic acid ester solvent, the matrix solvent molecule is ethyl acetate.

5. A low binding energy solvent for low temperature lithium ion battery electrolyte according to any one of claims 1 to 4, characterized in that: The low binding energy solvent is used for preparing low-temperature lithium ion battery electrolyte.

6. The use according to claim 5, characterized in that: The lithium salt in the low-temperature lithium-ion battery electrolyte is lithium bis(fluorosulfonyl)imide.

Citation Information

Patent Citations

  • Ether electrolyte and lithium-sulfur secondary battery

    CN110416597A

  • Low-temperature electrolyte taking ethyl fluoroacetate as solvent and application of low-temperature electrolyte

    CN111952671A

  • Fluorine-containing ether electrolyte cosolvent for lithium metal / lithium ion / lithium sulfur battery, electrolyte and lithium secondary battery

    CN112382792A

  • Novel ester electrolyte suitable for rapid charging of lithium metal battery

    CN118281317A

  • Ether-based low-temperature-resistant electrolyte for lithium ion battery as well as preparation method and application of ether-based low-temperature-resistant electrolyte