Pressure control method for thin edge of automotive trim injection molded part

By dividing the thin edges of the injection molded parts of the automobile interior into sub-regions according to the wall thickness, real-time monitoring and analysis of process parameters, calculating the pressure loss evaluation index, and adjusting the pressure calibration coefficient, the problem of inaccurate pressure monitoring during the injection molding process is solved, and the problem of inaccurate pressure monitoring of thin edges is achieved. More finer pressure control and more stable injection molding quality.

CN118990969AActive Publication Date: 2024-11-22JIANGSU QINLONG VEHICLE LAMP
View PDF 5 Cites 0 Cited by

Patent Information

Application Number
CN202411414049.1
Authority / Receiving Office
CN · China
Patent Type
Applications(China)
Current Assignee / Owner
Filing Date
2024-10-11
Publication Date
2024-11-22
Estimated Expiration
2044-10-11

AI Technical Summary

Technical Problem

The existing thin edge pressure control method for injection molding parts in the automotive interior is not accurate enough for the pressure monitoring of thin edges in the injection molding process, and it is impossible to accurately control the pressure at different positions of the thin edges of the plastic parts, resulting in injection molding defects and unstable quality.

Method used

The thin edges of the plastic parts are divided into several sub-regions according to the wall thickness distribution. By installing sensors on the injection molding machine to monitor the process parameters in real time, data feature extraction and analysis are performed, the thin edge comprehensive pressure loss evaluation index is calculated, and the pressure calibration coefficient is adjusted to calibrate the injection molding pressure. , realize fine control of thin edge pressure.

Benefits of technology

The accuracy of thin-edge pressure monitoring in the injection molding process is improved, defects caused by uneven pressure distribution are reduced, more uniform and stable pressure distribution is achieved, production costs and mold trials are reduced, and production efficiency is improved.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure CN118990969A_ABST
    Figure CN118990969A_ABST
Patent Text Reader

Abstract

The invention relates to the field of automobile interiors, and discloses an automobile interior injection molded part thin edge pressure control method, which comprises the steps of area division, data acquisition, data recording and preprocessing, feature extraction, pressure loss analysis, pressure loss calibration and adjustment execution, and is characterized in that a plastic part thin edge is divided into a plurality of sub-areas according to wall thickness distribution; the method comprises the following steps of: monitoring and acquiring a plurality of target sub-areas, preprocessing monitored and acquired technological parameters of the thin edge injection molding process of the plastic part in each target sub-area, performing feature extraction and parallel analysis on the preprocessed parameters, comprehensively analyzing and calculating a comprehensive pressure loss evaluation index and a pressure calibration coefficient of the thin edge, and realizing evaluation and pressure loss calibration of the total pressure loss of the thin edge of the plastic part. The problem that pressure monitoring of the thin edge in the injection molding process is not accurate enough is solved, the influence of wall thickness change on melt flow and pressure distribution is considered, and therefore more refined pressure control is achieved, and quality defects caused by improper pressure control in the mold testing process are reduced.
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] The invention relates to the technical field of automobile interior decoration, and more specifically to a method for controlling the thin edge pressure of an automobile interior decoration injection molding part. Background Art

[0002] With the rapid development of the automobile industry, people have higher and higher requirements for the quality and appearance of automobile interiors. As an important part of automobile interiors, the quality of injection molded parts directly affects the overall quality of the car. However, during the injection molding process, problems such as insufficient pressure and incomplete filling are prone to occur in thin-edge parts, which will not only affect the appearance quality of the injection molded parts, but may also lead to performance degradation. The traditional pressure control method is mainly achieved by adjusting the pressure and speed of the injection molding machine, but this method is not ideal for the pressure control effect of thin-edge parts. With the continuous development of computer technology and sensor technology, a pressure control method for thin edges of automobile interior injection molded parts has emerged. It uses machine vision pressure control and neural network pressure control, monitors the pressure changes during the injection molding process in real time, and automatically adjusts the pressure and speed of the injection molding machine according to the monitoring results, thereby achieving effective control of the thin-edge pressure;

[0003] However, the above process still has the following disadvantages:

[0004] First, the existing pressure control method for the thin edge of automobile interior injection molding parts is not accurate enough in monitoring the pressure of the thin edge during the injection molding process, lacks consideration of the injection defects caused by the uneven pressure distribution of the thin edge of the plastic part, and cannot accurately control the pressure at different positions of the thin edge of the plastic part;

[0005] Secondly, there is a lack of pressure control at different locations according to the distribution of wall thickness changes, and a lack of accurate pressure adjustment from the perspective of uneven pressure distribution. This will lead to quality defects due to improper pressure control during the mold trial and make it impossible to stabilize product quality. Summary of the invention

[0006] In order to overcome the above-mentioned defects of the prior art, the present invention provides a method for controlling the thin edge pressure of an automobile interior injection molded part to solve the problems existing in the above-mentioned background technology.

[0007] The present invention provides the following technical solution: a method for controlling the thin edge pressure of an automobile interior injection molded part, comprising:

[0008] S1: Divide the thin edge of the plastic part into several sub-areas according to the wall thickness distribution and number them as 1, 2, 3...m. Install sensors on the injection molding machine to monitor and collect the injection molding process parameters of the thin edge of the plastic part in each target sub-area in real time, and transmit the collected injection molding process parameters of the thin edge of the plastic part in each target sub-area to S2;

[0009] S2: Record the thin edge injection molding process parameters of each target sub-area plastic part through the built-in recorder of the injection molding machine, then pre-process the thin edge injection molding process parameters of each target sub-area plastic part in parallel, and transmit the pre-processed thin edge injection molding process parameters of each target sub-area plastic part to S3;

[0010] S3: by extracting data features of the process parameters of the thin edge injection molding process of the plastic parts in each target sub-region, the temperature fluctuation value, melt pressure loss and acceleration pressure loss in each target sub-region are obtained respectively, and the extracted temperature fluctuation value, melt pressure loss and acceleration pressure loss in each target sub-region are transmitted to S4;

[0011] S4: analyzing the temperature fluctuation value, melt pressure loss and acceleration pressure loss in each target sub-region extracted in parallel, calculating the injection pressure loss value of the sub-region, and transmitting the injection pressure loss value of the sub-region to S5;

[0012] S5: performing a comprehensive analysis on the injection pressure loss values ​​of the sub-regions analyzed in each target sub-region and calculating a thin edge comprehensive pressure loss evaluation index, which evaluates the overall loss of injection pressure at the thin edge of the plastic part, and transmits the thin edge comprehensive pressure loss evaluation index to S6;

[0013] S6: Calculate the pressure calibration coefficient according to the thin edge comprehensive pressure loss evaluation index, calibrate the thin edge injection pressure loss by the pressure calibration coefficient, control the injection pressure to make the thin edge fill uniformly, and transmit the pressure control adjustment execution instruction to S7;

[0014] S7: Execute the pressure control adjustment execution instruction, adjust the injection molding process parameters, and generate the pressure adjustment stop execution instruction.

[0015] Preferably, the area division method of S1 is:

[0016] According to the distribution of wall thickness variation of the thin edge of the plastic part, it is divided into different gradient areas from thin to thick, and the wall thickness of each area is numbered in sequence from thin to thick;

[0017] The data collection method of S1 is:

[0018] According to the number of areas divided by the thin edge wall thickness distribution of the plastic part, a corresponding number of types of sensors are arranged on the injection molding machine to cover each target sub-area, and measure and collect the process parameters of the thin edge injection molding process of the plastic part in each target sub-area, including temperature, pressure, holding time and speed. The types of sensors include pressure sensors, temperature sensors and speed sensors.

[0019] Preferably, the S2 automatically records the process parameters of the thin-edge injection molding process of plastic parts in each target sub-area in chronological order by setting the data recording time of each area in the built-in recorder, and then stores them in the database according to the divided areas. The specific operation of the parallel preprocessing of the process parameters of the thin-edge injection molding process of plastic parts in each target sub-area is: data cleaning, filtering and removal of abnormal values ​​of the process parameters of the thin-edge injection molding process of plastic parts in multiple target sub-areas at the same time.

[0020] Preferably, S3 extracts the characteristics of the pre-processed thin edge injection molding process parameters of the plastic parts in each target sub-region, obtains the characteristic parameters that affect the injection molding pressure change of the plastic parts, and calculates them;

[0021] The temperature fluctuation value is obtained by periodically recording the actual value of the mold temperature T from the beginning of injection molding. a1 , T a2 , Λ, T an , Actual value of melt temperature T b1 , T b2 , Λ, T bn And the actual value of ambient temperature T c1 , T c2 , Λ, T cn , the calculation formula for calculating the temperature fluctuation value is T ai Indicates recording the actual value of the mold temperature for the i-th time, T bi Indicates recording the actual value of the melt temperature for the i-th time, T ci Indicates recording the actual value of the i-th ambient temperature. Indicates the average value of the mold temperature recorded n times, It indicates the average value of melt temperature recorded n times. Indicates the average value of the ambient temperature recorded n times;

[0022] The melt pressure loss is used to monitor the pressure loss during melt friction during the injection molding process and record the actual value of the melt temperature T for the i-th time. bi , the calculation formula for melt pressure loss is L represents the melt flow channel length, It represents the average flow rate of the melt during injection molding, D represents the flow channel diameter, u0 represents the viscosity of the melt at the reference temperature T0, t0 represents the reference temperature of the melt, α represents the temperature index, and 0.3≤α≤0.6. The specific value is adjusted according to experimental data;

[0023] The acceleration pressure loss is used to monitor the pressure loss caused by the acceleration and deceleration of the melt in the flow channel during the injection molding process. The melt inlet velocity v1 and outlet velocity v2 are recorded respectively. The calculation formula for calculating the acceleration pressure loss is: ρ represents the density of the melt.

[0024] Preferably, S4 simultaneously analyzes the injection pressure loss values ​​of sub-regions in multiple target sub-regions through the temperature fluctuation value ΔT, melt pressure loss ΔP1 and acceleration pressure loss ΔP2 in each target sub-region. The calculation formula of the injection pressure loss value of the sub-region is Δp j =(ΔP1+ΔP2+P′) ΔT , P′ represents the local pressure loss, and the sub-region injection pressure loss value calculated for each target sub-region is transmitted to S5.

[0025] Preferably, the S5 monitors and evaluates the overall injection pressure loss state through the thin edge comprehensive pressure loss evaluation index, and the formula for calculating the thin edge comprehensive pressure loss evaluation index is: Δp1, Δp2, Δp3, Λ, Δp m Indicates the injection pressure loss value of the 1st, 2nd, 3rd, ...mth target sub-region, Δp j represents the injection pressure loss value of the jth sub-area, It represents the average value of the injection pressure loss values ​​of m sub-areas.

[0026] Preferably, S6 compares the thin edge comprehensive pressure loss evaluation index with a preset pressure loss threshold to calculate the pressure calibration coefficient: S represents the comprehensive pressure loss evaluation index of thin edge, s′ represents the preset pressure loss threshold. When the pressure calibration coefficient u is in the range of (0,1), it means that the pressure loss in the current injection molding process is within the controllable range, the quality of the injection molded parts meets the design requirements, and there is no need to control and adjust the pressure. When the pressure calibration coefficient u is in the range of [1, +∞), it means that the pressure loss in the injection molding process exceeds the controllable range. At this time, the pressure loss will have an adverse effect on the quality of the injection molded parts, and the injection molding process needs to be controlled and adjusted, and the pressure control adjustment execution instruction is immediately generated and transmitted to S7.

[0027] Preferably, the S7 is used to receive and execute the pressure control adjustment execution instruction, adjust the injection molding process parameters, and monitor the pressure changes during the adjustment process in real time. When the pressure loss is detected to be within the controllable range, the pressure adjustment stop execution instruction is immediately triggered, and the pressure adjustment stop execution instruction is sent to S6, and the execution behavior is stopped.

[0028] Technical effects and advantages of the present invention:

[0029] The present invention divides the thin edge of a plastic part into several sub-areas according to the wall thickness distribution, and installs sensors on the injection molding machine to monitor and collect the injection molding process parameters of the thin edge of the plastic part in each target sub-area in real time, and records the injection molding process parameters of the thin edge of the plastic part in each target sub-area respectively through the built-in recorder of the injection molding machine, and then pre-processes the injection molding process parameters of the thin edge of the plastic part in each target sub-area in parallel, which is conducive to solving the problem of inaccurate pressure monitoring of the thin edge in the injection molding process, takes into account the influence of the change of wall thickness on the melt flow and pressure distribution, thereby realizing more refined pressure control, reducing the injection molding defects caused by uneven pressure distribution, and extracting and analyzing the characteristics of the thin edge of the plastic part in each target sub-area. After the analysis, the process parameters of the thin edge injection molding process of the target sub-area plastic part are comprehensively analyzed to obtain the thin edge comprehensive pressure loss evaluation index to evaluate the overall loss of injection pressure at the thin edge of the plastic part. Then, the thin edge injection molding pressure loss and pressure control adjustment execution operations are calibrated through the calculated pressure calibration coefficient. By calculating the pressure loss value in each area, the pressure demand of each area can be more accurately predicted and adjusted, the injection pressure can be automatically controlled, and a more uniform and stable pressure distribution adjustment can be achieved, which is conducive to reducing quality defects caused by improper pressure control during the trial mold, reducing the number of trial molds and production costs, thereby improving production efficiency and reducing production costs. BRIEF DESCRIPTION OF THE DRAWINGS

[0030] Figure 1 It is a diagram of the method steps of the present invention.

[0031] Figure 2 It is a system structure block diagram of the present invention. DETAILED DESCRIPTION

[0032] The technical solution of the present invention will be clearly and completely described below in conjunction with the accompanying drawings in the present invention. In addition, the forms of the various structures recorded in the following embodiments are only examples. The thin edge pressure control method of an automobile interior injection molding part involved in the present invention is not limited to the various structures recorded in the following embodiments. All other embodiments obtained by ordinary technicians in this field without making creative work belong to the scope of protection of the present invention.

[0033] The present invention provides a method for controlling the thin edge pressure of an automobile interior injection molded part, comprising:

[0034] S1: Divide the thin edge of the plastic part into several sub-areas according to the wall thickness distribution and number them as 1, 2, 3...m. By installing sensors on the injection molding machine, the injection molding process parameters of the thin edge of the plastic part in each target sub-area are monitored and collected in real time, and the collected injection molding process parameters of the thin edge of the plastic part in each target sub-area are transmitted to S2.

[0035] In this embodiment, the area division method of S1 is:

[0036] According to the distribution of wall thickness variation of the thin edge of the plastic part, it is divided into different gradient areas from thin to thick, and the wall thickness of each area is numbered in sequence from thin to thick;

[0037] The data collection method of S1 is:

[0038] According to the number of areas divided by the thin edge wall thickness distribution of the plastic part, a corresponding number of types of sensors are arranged on the injection molding machine to cover each target sub-area, and measure and collect the process parameters of the thin edge injection molding process of the plastic part in each target sub-area, including temperature, pressure, holding time and speed. The types of sensors include pressure sensors, temperature sensors and speed sensors.

[0039] It should be specified that the specific operation process of S1 area division is: use 3D scanning equipment to obtain the precise wall thickness data of the thin edge of the plastic part, use CAD software to process the wall thickness data, identify the wall thickness change law, and then divide the thin edge of the plastic part into multiple gradient areas from thin to thick according to the wall thickness change law. The wall thickness change in each area should be relatively uniform, and each area is numbered, starting from the area with the thinnest wall thickness, and numbered 1, 2, 3...m in sequence. Sensors are installed at representative positions in each gradient area to cover the injection molding process parameters of the area.

[0040] S2: Record the thin-edge injection molding process parameters of each target sub-area plastic part through the built-in recorder of the injection molding machine, then pre-process the thin-edge injection molding process parameters of each target sub-area plastic part in parallel, and transmit the pre-processed thin-edge injection molding process parameters of each target sub-area plastic part to S3.

[0041] In this embodiment, S2 sets the data recording time of each area in the built-in recorder, automatically records the process parameters of the thin-edge injection molding process of plastic parts in each target sub-area in chronological order, and then stores them in the database according to the divided areas. The specific operation of parallel preprocessing of the process parameters of the thin-edge injection molding process of plastic parts in each target sub-area is: data cleaning, filtering and removal of abnormal values ​​of the process parameters of the thin-edge injection molding process of plastic parts in multiple target sub-areas at the same time.

[0042] Specifically, the S2 can choose a built-in recorder with programmable functions and support multi-channel data acquisition, automatically starting and stopping recording according to a preset schedule.

[0043] S3: By extracting data features of the process parameters of the thin-edge injection molding process of the plastic parts in each target sub-region, the temperature fluctuation value, melt pressure loss and acceleration pressure loss in each target sub-region are obtained respectively, and the extracted temperature fluctuation value, melt pressure loss and acceleration pressure loss in each target sub-region are transmitted to S4.

[0044] In this embodiment, S3 extracts the characteristics of the pre-processed thin edge injection molding process parameters of each target sub-region, obtains the characteristic parameters that affect the injection molding pressure change of the thin edge of the plastic part, and calculates them;

[0045] The temperature fluctuation value is obtained by periodically recording the actual mold temperature T from the beginning of injection molding. a1 , T a2 , Λ, T an , Actual value of melt temperature T b1 , T b2 , Λ, T bn And the actual value of ambient temperature T c1 , T c2 , Λ, T cn , the calculation formula for calculating the temperature fluctuation value is T ai Indicates recording the actual value of the mold temperature for the i-th time, T bi Indicates recording the actual value of the melt temperature for the i-th time, T ci Indicates recording the actual value of the i-th ambient temperature. Indicates the average value of the mold temperature recorded n times, It indicates the average value of melt temperature recorded n times. Indicates the average value of the ambient temperature recorded n times;

[0046] Melt pressure loss is used to monitor the pressure loss during melt friction during the injection molding process and record the actual value of the melt temperature T for the i-th time. bi , the calculation formula for melt pressure loss is L represents the melt flow channel length, It represents the average flow rate of the melt during injection molding, D represents the flow channel diameter, u0 represents the viscosity of the melt at the reference temperature T0, t0 represents the reference temperature of the melt, α represents the temperature index, and 0.3≤α≤0.6. The specific value is adjusted according to experimental data;

[0047] Acceleration pressure loss is used to monitor the pressure loss caused by the acceleration and deceleration of the melt in the flow channel during the injection molding process. The melt inlet velocity v1 and outlet velocity v2 are recorded respectively. The calculation formula for the acceleration pressure loss is: ρ represents the density of the melt.

[0048] S4: The temperature fluctuation values, melt pressure loss and acceleration pressure loss extracted in each target sub-region are analyzed in parallel, and the injection pressure loss value of the sub-region is calculated, and the injection pressure loss value of the sub-region is transmitted to S5.

[0049] In this embodiment, S4 simultaneously analyzes the injection pressure loss values ​​of the sub-regions in multiple target sub-regions through the temperature fluctuation value ΔT, melt pressure loss ΔP1 and acceleration pressure loss ΔP2 in each target sub-region. The calculation formula of the injection pressure loss value of the sub-region is Δp j =(ΔP1+ΔP2+P′) ΔT , P′ represents the local pressure loss, and the sub-region injection pressure loss value calculated for each target sub-region is transmitted to S5.

[0050] It should be specifically stated that the specific analysis process of the local pressure loss P′ in S4 is as follows:

[0051] S41: During the injection molding process, determine the local loss area, including flow channel corners, dead ends, cross-section changes, and geometric shape change areas;

[0052] S42: Record the average melt flow velocity v′ and melt density ρ′ in the local loss area;

[0053] S43: Calculate the local pressure loss as K represents the local loss coefficient, and its specific value is calculated and verified by experimental data.

[0054] S5: The injection pressure loss values ​​of the sub-regions analyzed in each target sub-region are comprehensively analyzed and a thin edge comprehensive pressure loss evaluation index is calculated. The thin edge comprehensive pressure loss evaluation index evaluates the overall loss of injection pressure at the thin edge of the plastic part, and the thin edge comprehensive pressure loss evaluation index is transmitted to S6.

[0055] In this embodiment, S5 monitors and evaluates the overall injection pressure loss state through the thin edge comprehensive pressure loss evaluation index. The formula for calculating the thin edge comprehensive pressure loss evaluation index is: Δp1, Δp2, Δp3, Λ, Δp m Indicates the injection pressure loss value of the 1st, 2nd, 3rd, ...mth target sub-region, Δp j represents the injection pressure loss value of the jth sub-area, It represents the average value of the injection pressure loss values ​​of m sub-areas.

[0056] S6: Calculate the pressure calibration coefficient according to the thin edge comprehensive pressure loss evaluation index, calibrate the thin edge injection pressure loss through the pressure calibration coefficient, control the injection pressure to make the thin edge fill uniformly, and transmit the pressure control adjustment execution instruction to S7.

[0057] In this embodiment, S6 compares the thin edge comprehensive pressure loss evaluation index with the preset pressure loss threshold and calculates the pressure calibration coefficient: S represents the comprehensive pressure loss evaluation index of thin edge, s′ represents the preset pressure loss threshold. When the pressure calibration coefficient u is in the range of (0,1), it means that the pressure loss in the current injection molding process is within the controllable range, the quality of the injection molded parts meets the design requirements, and there is no need to control and adjust the pressure. When the pressure calibration coefficient u is in the range of [1, +∞), it means that the pressure loss in the injection molding process exceeds the controllable range. At this time, the pressure loss will have an adverse effect on the quality of the injection molded parts, and the injection molding process needs to be controlled and adjusted, and the pressure control adjustment execution instruction is immediately generated and transmitted to S7.

[0058] S7: Execute the pressure control adjustment execution instruction, adjust the injection molding process parameters, and generate the pressure adjustment stop execution instruction.

[0059] In this embodiment, S7 is used to receive and execute the pressure control adjustment execution instruction, adjust the injection molding process parameters, and monitor the pressure changes during the adjustment process in real time. When the pressure loss is detected to be within the controllable range, the pressure adjustment stop execution instruction is immediately triggered, and a pressure adjustment stop execution instruction is sent to S6, and the execution behavior is stopped.

[0060] It should be specifically explained that the S7's pressure control adjustment execution process includes: increasing the injection pressure or holding pressure to compensate for pressure loss; adjusting the melt temperature and mold temperature to improve the fluidity and cooling effect of the plastic; and using pressure sensors to monitor the pressure changes and adjustments of the injection molding process in real time, and transmitting the pressure control results to the database for storage, providing managers with a pressure control result query function.

[0061] like Figure 2 The present embodiment shown provides an implementation system corresponding to a method for controlling thin-edge pressure of automotive interior injection molding parts, including an area division module, a data acquisition module, a data recording and preprocessing module, a feature extraction module, a pressure loss analysis module, a comprehensive analysis module, a pressure loss calibration module and an adjustment execution module, wherein the area division module is connected to the data acquisition module, the data acquisition module is connected to the data recording and preprocessing module, the data recording and preprocessing module is connected to the feature extraction module, the feature extraction module is connected to the pressure loss analysis module, the pressure loss analysis module is connected to the comprehensive analysis module, the comprehensive analysis module is connected to the pressure loss calibration module, and the pressure loss calibration module is connected to the adjustment execution module.

[0062] The area division module divides the thin edge of the plastic part into a plurality of sub-areas according to the wall thickness distribution and numbers them as 1, 2, 3...m;

[0063] The data acquisition module monitors and collects the process parameters of the thin edge injection molding process of each target sub-area plastic part in real time by installing sensors on the injection molding machine;

[0064] The data recording and preprocessing module records the thin edge injection molding process parameters of each target sub-region plastic part through the built-in recorder of the injection molding machine, and then performs parallel preprocessing on the thin edge injection molding process parameters of each target sub-region plastic part;

[0065] The feature extraction module extracts data features of the process parameters of the thin edge injection molding process of the plastic parts in each target sub-region, and obtains the temperature fluctuation value, melt pressure loss and acceleration pressure loss in each target sub-region respectively;

[0066] The pressure loss analysis module analyzes the extracted temperature fluctuation values, melt pressure loss and acceleration pressure loss in each target sub-region in parallel, and calculates the injection pressure loss value of the sub-region;

[0067] The comprehensive analysis module comprehensively analyzes the injection pressure loss values ​​of the sub-regions analyzed in each target sub-region and calculates a thin edge comprehensive pressure loss evaluation index, which evaluates the overall loss of injection pressure at the thin edge of the plastic part;

[0068] The pressure loss calibration module calculates a pressure calibration coefficient according to the thin edge comprehensive pressure loss evaluation index, calibrates the thin edge injection molding pressure loss by the pressure calibration coefficient, and controls the injection molding pressure to make the thin edge fill uniformly;

[0069] The adjustment execution module executes the pressure control adjustment execution instruction, adjusts the injection molding process parameters, and generates a pressure adjustment stop execution instruction.

[0070] Finally: The above description is only a preferred embodiment of the present invention and is not intended to limit the present invention. Any modifications, equivalent substitutions, improvements, etc. made within the spirit and principles of the present invention should be included in the protection scope of the present invention.

[0071] The above is only a specific implementation of the present application, but the protection scope of the present application is not limited thereto. Any technician familiar with the technical field can easily think of changes or substitutions within the technical scope disclosed in the present application, which should be included in the protection scope of the present application. Therefore, the protection scope of the present application should be based on the protection scope of the claims.

Claims

1. A method for controlling the thin edge pressure of an automobile interior injection molded part, characterized in that: The following steps are involved: S1: Divide the thin edge of the plastic part into several sub-areas according to the wall thickness distribution and number them as 1, 2, 3...m. Install sensors on the injection molding machine to monitor and collect the injection molding process parameters of the thin edge of the plastic part in each target sub-area in real time, and transmit the collected injection molding process parameters of the thin edge of the plastic part in each target sub-area to S2; S2: Record the thin edge injection molding process parameters of each target sub-area plastic part through the built-in recorder of the injection molding machine, then pre-process the thin edge injection molding process parameters of each target sub-area plastic part in parallel, and transmit the pre-processed thin edge injection molding process parameters of each target sub-area plastic part to S3; S3: by extracting data features of the process parameters of the thin edge injection molding process of the plastic parts in each target sub-region, the temperature fluctuation value, melt pressure loss and acceleration pressure loss in each target sub-region are obtained respectively, and the extracted temperature fluctuation value, melt pressure loss and acceleration pressure loss in each target sub-region are transmitted to S4; S4: analyzing the temperature fluctuation value, melt pressure loss and acceleration pressure loss in each target sub-region extracted in parallel, calculating the injection pressure loss value of the sub-region, and transmitting the injection pressure loss value of the sub-region to S5; S5: performing a comprehensive analysis on the injection pressure loss values ​​of the sub-regions analyzed in each target sub-region and calculating a thin edge comprehensive pressure loss evaluation index, which evaluates the overall loss of injection pressure at the thin edge of the plastic part, and transmits the thin edge comprehensive pressure loss evaluation index to S6; S6: Calculate the pressure calibration coefficient according to the thin edge comprehensive pressure loss evaluation index, calibrate the thin edge injection pressure loss by the pressure calibration coefficient, control the injection pressure to make the thin edge fill uniformly, and transmit the pressure control adjustment execution instruction to S7; S7: Execute the pressure control adjustment execution instruction, adjust the injection molding process parameters, and generate the pressure adjustment stop execution instruction.

2. A method for controlling thin edge pressure of automobile interior injection molded parts according to claim 1, characterized in that: The area division method of S1 is as follows: According to the distribution of wall thickness variation of the thin edge of the plastic part, it is divided into different gradient areas from thin to thick, and the wall thickness of each area is numbered in sequence from thin to thick; The data collection method of S1 is: According to the number of areas divided by the thin edge wall thickness distribution of the plastic part, a corresponding number of types of sensors are arranged on the injection molding machine to cover each target sub-area, and measure and collect the process parameters of the thin edge injection molding process of the plastic part in each target sub-area, including temperature, pressure, holding time and speed. The types of sensors include pressure sensors, temperature sensors and speed sensors.

3. The method for controlling the thin edge pressure of an automobile interior injection molded part according to claim 1, characterized in that: The S2 sets the data recording time of each area in the built-in recorder, automatically records the process parameters of the thin-edge injection molding process of each target sub-area plastic part in chronological order, and then stores them in the database according to the divided areas. The specific operation of the parallel preprocessing of the process parameters of the thin-edge injection molding process of each target sub-area plastic part is: data cleaning, filtering and removal of abnormal values ​​of the process parameters of the thin-edge injection molding process of multiple target sub-areas plastic parts at the same time.

4. The method for controlling the thin edge pressure of an automobile interior injection molded part according to claim 1, characterized in that: S3 extracts the characteristics of the pre-processed thin edge injection molding process parameters of the plastic parts in each target sub-region, obtains the characteristic parameters that affect the injection molding pressure change of the thin edge of the plastic parts, and calculates them; The temperature fluctuation value is obtained by periodically recording the actual value of the mold temperature T from the beginning of injection molding. a1 , T a2 , Λ, T an , Actual value of melt temperature T b1 , T b2 , Λ, T bn And the actual value of ambient temperature T c1 , T c2 , Λ, T cn , the calculation formula for calculating the temperature fluctuation value is T ai Indicates recording the actual value of the mold temperature for the i-th time, T bi Indicates recording the actual value of the melt temperature for the i-th time, T ci Indicates recording the actual value of the i-th ambient temperature. Indicates the average value of the mold temperature recorded n times, Indicates the average value of the melt temperature recorded n times, T c Indicates the average value of the ambient temperature recorded n times; The melt pressure loss is used to monitor the pressure loss during melt friction during the injection molding process and record the actual value of the melt temperature T for the i-th time. bi , the calculation formula for melt pressure loss is L represents the melt flow channel length, It represents the average flow rate of the melt during injection molding, D represents the flow channel diameter, u0 represents the viscosity of the melt at the reference temperature T0, t0 represents the reference temperature of the melt, α represents the temperature index, and 0.3≤α≤0.

6. The specific value is adjusted according to experimental data; The acceleration pressure loss is used to monitor the pressure loss caused by the acceleration and deceleration of the melt in the flow channel during the injection molding process. The melt inlet velocity v1 and outlet velocity v2 are recorded respectively. The calculation formula for calculating the acceleration pressure loss is: ρ represents the density of the melt.

5. The method for controlling thin edge pressure of automobile interior injection molded parts according to claim 1, characterized in that: S4 simultaneously analyzes the injection pressure loss values ​​of the sub-regions in the multiple target sub-regions through the temperature fluctuation value ΔT, melt pressure loss ΔP1 and acceleration pressure loss ΔP2 in each target sub-region. The calculation formula of the injection pressure loss value of the sub-region is Δp j =(ΔP1+ΔP2+P′) ΔT , P′ represents the local pressure loss, and the sub-region injection pressure loss value calculated for each target sub-region is transmitted to S5.

6. The method for controlling thin edge pressure of automobile interior injection molding according to claim 1, characterized in that: The S5 monitors and evaluates the overall injection pressure loss state through the thin edge comprehensive pressure loss evaluation index. The formula for calculating the thin edge comprehensive pressure loss evaluation index is: Δp1, Δp2, Δp3, Λ, Δp m Indicates the injection pressure loss value of the 1st, 2nd, 3rd, ...mth target sub-region, Δp j represents the injection pressure loss value of the jth sub-area, It represents the average value of the injection pressure loss values ​​of m sub-areas.

7. The method for controlling thin edge pressure of automobile interior injection molded parts according to claim 1, characterized in that: The S6 compares the thin edge comprehensive pressure loss evaluation index with the preset pressure loss threshold and calculates the pressure calibration coefficient: S represents the comprehensive pressure loss evaluation index of thin edge, s′ represents the preset pressure loss threshold. When the pressure calibration coefficient u is in the range of (0,1), it means that the pressure loss in the current injection molding process is within the controllable range, the quality of the injection molded parts meets the design requirements, and there is no need to control and adjust the pressure. When the pressure calibration coefficient u is in the range of [1, +∞), it means that the pressure loss in the injection molding process exceeds the controllable range. At this time, the pressure loss will have an adverse effect on the quality of the injection molded parts, and the injection molding process needs to be controlled and adjusted, and the pressure control adjustment execution instruction is immediately generated and transmitted to S7.

8. The method for controlling the thin edge pressure of an automobile interior injection molded part according to claim 1, characterized in that: The S7 is used to receive and execute the pressure control adjustment execution instruction, adjust the injection molding process parameters, and monitor the pressure changes during the adjustment process in real time. When the pressure loss is detected to be within the controllable range, the pressure adjustment stop execution instruction is immediately triggered, and the pressure adjustment stop execution instruction is sent to S6, and the execution behavior is stopped.

Citation Information

Patent Citations

  • Mold temperature and pressure control injection molding process of highlight injection molded piece and control system

    CN103722705A

  • Method and apparatus for overmolding fragile hollow article

    CN107000280A

  • Multi-target optimization method for injection molding process parameters of thin-walled injection molded part

    CN110640982A

  • Injection molding method for thin-walled products

    CN110871555A

  • Manufacture of unevenly thick-walled molded article

    JP1995164496A