Optical anti-counterfeiting element, optical anti-counterfeiting product and manufacturing method

By setting up a plating layer on the microstructure formation layer of the optical anti-counterfeiting element and setting a non-macro hollow area at the mutation position, the structural deformation and plating defects caused by changes in microstructure parameters are solved, and continuous changes in optical characteristics and improvement of anti-counterfeiting performance are achieved. .

CN118991282APending Publication Date: 2024-11-22ZHONGCHAO SPECIAL SECURITY TECH +1

Patent Information

Application Number
CN202310551025.X
Authority / Receiving Office
CN · China
Patent Type
Applications(China)
Current Assignee / Owner
Filing Date
2023-05-16
Publication Date
2024-11-22

AI Technical Summary

Technical Problem

During the production process of existing optical anti-counterfeiting components, changes in microstructure parameters lead to structural deformation and plating defects, causing actual optical characteristics to deviate from the expected design, affecting anti-counterfeiting performance.

Method used

Plating is provided on the microstructure formation layer of the optical anti-counterfeiting element, and a non-macro hollow area is set at the mutation position. The characteristic width of the hollow area is within the range of 0.1μm to 100μm, and the area does not exceed 0.5% of the total area to ensure that the plating is micro-plating The height of the structure is continuously changed, avoiding plating defects and optical characteristics.

Benefits of technology

It effectively avoids the coating defects and optical characteristic deviations caused by microstructure mutations, ensures the anti-counterfeiting performance of optical anti-counterfeiting components, and ensures that the actual optical effect is close to the design effect.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure CN118991282A_ABST
    Figure CN118991282A_ABST
Patent Text Reader

Abstract

The invention provides an optical anti-counterfeiting element, an optical anti-counterfeiting product and a manufacturing method. The optical security element includes: a base material; the microstructure forming layer is arranged on the surface of one side of the base material, the microstructure forming layer is provided with a microstructure, and the longitudinal section of the microstructure is in a preset shape; the plating layer is arranged on the microstructure forming layer, a plating microstructure is formed after the microstructure is plated with the plating layer, and the height of the plating microstructure changes continuously; wherein when the microstructure has a sudden change position, the plating layer has a hollow area, and when the height of the microstructure continuously changes, the plating layer has no hollow area. According to the optical anti-counterfeiting element, the problem that the actually generated optical effect of the optical anti-counterfeiting element in the prior art is greatly deviated from the expected optical effect is solved.
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] The present invention relates to the technical field of optical anti-counterfeiting equipment, and in particular to an optical anti-counterfeiting element, an optical anti-counterfeiting product and a manufacturing method thereof. Background Art

[0002] Optical anti-counterfeiting products generally use optical microstructures and coatings to modulate incident light to form a variety of optical features such as color, dynamics, and three-dimensionality. These features are different from generally fixed, planar printed patterns. When the optical anti-counterfeiting element is tilted or rotated, the corresponding pattern will produce color changes, dynamics, or give people a special feeling of floating / sunken on the plane, thereby protecting the product.

[0003] Optical microstructures are generally micro-nano structures, which can be refractive elements, such as microlenses; reflective elements, such as reflective surfaces; diffractive elements, such as holographic gratings; or smaller surface plasmon structures that enable light and electrons to interact, such as sub-wavelength gratings. Regardless of the optical principle, the characteristics of these microstructures are generally that they are within the plane of the optical anti-counterfeiting element, and through micro-nano processing, various shapes of surface morphologies with ups and downs are obtained.

[0004] As for another key element, the coating, vacuum physical vapor deposition or chemical vapor deposition is generally used to form an optical film on the surface of the structure. Generally, a single layer of metal material / dielectric material, or a stack of metal and dielectric materials, or a stack of metal / dielectric materials, can be used to obtain specific optical characteristics.

[0005] Under existing process conditions, microstructures are generally obtained by laser interference, laser direct etching or electron beam direct etching, and then mass-produced by molding, UV casting and other methods to transfer the microstructure to other substrates. However, there are two situations that will cause the optical characteristics of the actual product to deviate from the original design. When the microstructure parameters change, the microstructure height suddenly changes, resulting in structural deformation. For example, for two adjacent reflective surfaces facing the same direction, the position of the highest point of the first reflective surface in the plane of the optical element is theoretically the same as the position of the lowest point of the second reflective surface in the plane of the optical anti-counterfeiting element. However, in the actual production process, neither the accuracy of the preparation method (laser, electron beam) nor the resolution of the material (photoresist) can form such a steep mutation, but a gradient from the highest point to the lowest point is formed within a certain size range, such as 0.5-1μm. Such a gradient forms another microstructure, and the other microstructure was not considered at the beginning of the design, so it will interfere with the design effect and cause the optical characteristics to deviate. In addition, shrinkage deformation caused by microstructure replication. The replication process cannot replicate the original microstructure 100%, and deviations will occur to a certain extent, especially at locations where the microstructure is highly mutated.

[0006] The coating on these microstructure change areas will also continue to maintain the above defects due to the same type of coverage, or even amplify the deviation caused by the above defects. Therefore, it is necessary to weaken or avoid these problems in actual production so that the actual optical characteristics are as consistent as possible with the expected design. Summary of the invention

[0007] The main purpose of the present invention is to provide an optical anti-counterfeiting element, an optical anti-counterfeiting product and a manufacturing method to solve the problem in the prior art that the actual optical effect produced by the optical anti-counterfeiting element deviates greatly from the expected optical effect.

[0008] In order to achieve the above-mentioned purpose, according to one aspect of the present invention, there is provided an optical anti-counterfeiting element, comprising: a substrate; a microstructure forming layer, the microstructure forming layer is arranged on one side surface of the substrate, the microstructure forming layer has a microstructure, and the longitudinal section of the microstructure is a preset shape; a coating, the coating is arranged on the microstructure forming layer, and the microstructure is plated to form a plated microstructure, and the height of the plated microstructure changes continuously; wherein, when the microstructure has a mutation position, the coating has a hollow area, and when the height of the microstructure changes continuously, the coating has no hollow area.

[0009] Furthermore, the hollow area is arranged at the position where the microstructure mutates so that the height of the plated microstructure changes continuously, wherein the hollow area is in the form of non-macro hollow images and texts. Non-macro hollow images and texts refer to hollow images and texts that cannot be directly observed by the human eye and can only be observed with a microscope, and the non-macro hollow images and texts do not affect the anti-counterfeiting effect of the coating.

[0010] Furthermore, a characteristic width of the hollow region is greater than or equal to 0.1 μm and less than or equal to 100 μm.

[0011] Furthermore, the ratio of the area of ​​the hollow region to the total area of ​​the optical anti-counterfeiting element is less than or equal to 0.5.

[0012] Furthermore, when there are multiple hollow areas, at least two of the multiple hollow areas are connected to each other.

[0013] Furthermore, when there are multiple hollow areas, at least two of the multiple hollow areas are not connected to each other.

[0014] Furthermore, the preset shape includes at least one of a sinusoidal shape, a wedge shape, a symmetrical rectangular tooth, an asymmetrical rectangular tooth, a semicircle, a rectangle, and a trapezoid.

[0015] Furthermore, a characteristic size of the microstructure in a plane parallel to the substrate is greater than or equal to 0.1 μm and less than or equal to 500 μm.

[0016] Furthermore, a characteristic size of the microstructure in a plane parallel to the substrate is greater than or equal to 0.2 μm and less than or equal to 100 μm.

[0017] Further, the coating provides a preset reflection characteristic or a preset transmission characteristic.

[0018] Furthermore, the coating is a single-layer reflective layer or a single-layer dielectric layer.

[0019] Further, the coating is a stacked layer formed by stacking a plurality of dielectric layers; or the coating is a stacked layer formed by alternately stacking reflective layers and dielectric layers.

[0020] Furthermore, the optical anti-counterfeiting element also includes a protective layer, which is arranged on the coating layer and is a transparent layer.

[0021] Further, the difference in refractive index between the protective layer and the microstructure forming layer is less than 0.5.

[0022] According to another aspect of the present invention, there is provided an optical anti-counterfeiting product, comprising the above-mentioned optical anti-counterfeiting element.

[0023] According to another aspect of the present invention, a method for manufacturing an optical anti-counterfeiting element is provided. The method for manufacturing an optical anti-counterfeiting element is used to manufacture the above-mentioned optical anti-counterfeiting element. The method for manufacturing an optical anti-counterfeiting element includes: forming a microstructure forming layer having a microstructure on a substrate; forming a coating having a hollow area on the microstructure forming layer; and forming a protective layer on the coating.

[0024] Applying the technical solution of the present invention, the optical anti-counterfeiting element includes a substrate, a microstructure forming layer and a coating. The microstructure forming layer is arranged on one side surface of the substrate, the microstructure forming layer has a microstructure, and the longitudinal section of the microstructure is a preset shape; the coating is arranged on the microstructure forming layer, and the microstructure is plated with the coating to form a plated microstructure, and the height of the plated microstructure changes continuously; wherein, when the microstructure has a mutation position, the coating has a hollow area, and when the height of the microstructure changes continuously, the coating has no hollow area.

[0025] By arranging a coating on the microstructure forming layer, so that the height of the formed coated microstructure changes continuously, defects caused by mutations in the coating are avoided, mutations in the optical characteristics are avoided, and the anti-counterfeiting performance of the optical anti-counterfeiting element is guaranteed. In the present application, there are two situations. One situation is that the microstructure has a mutation position. In this case, there is a hollow area on the coating. The setting of the hollow area is conducive to the continuous change of the height of the coated microstructure, thereby avoiding the mutation affecting the optical characteristics of the optical anti-counterfeiting element. In another situation, the height of the microstructure changes continuously without a mutation position. In this case, the coating has no hollow area, which avoids the risk of changes in the optical properties of the coating due to mutations in the microstructure, and further avoids changes in the anti-counterfeiting characteristics of the optical anti-counterfeiting element. BRIEF DESCRIPTION OF THE DRAWINGS

[0026] The drawings constituting a part of the present application are used to provide a further understanding of the present invention. The exemplary embodiments of the present invention and their descriptions are used to explain the present invention and do not constitute an improper limitation of the present invention. In the drawings:

[0027] Figure 1 A view showing an angle of an optical anti-counterfeiting product in the prior art;

[0028] Figure 2 Shows Figure 1 A schematic diagram of the structure of the microstructure forming layer of the optical anti-counterfeiting element;

[0029] Figure 3 Shows Figure 1 Schematic diagram of the positional relationship between the microstructure forming layer and the coating layer of the optical anti-counterfeiting element;

[0030] Figure 4 Shows Figure 1 The optical effect diagram of the optical anti-counterfeiting product at the first observation angle;

[0031] Figure 5 Shows Figure 1 The optical effect diagram of the optical anti-counterfeiting product under the second observation angle;

[0032] Figure 6 Shows Figure 1The optical effect diagram of the optical anti-counterfeiting product under the third observation angle;

[0033] Figure 7 Shows Figure 1 A position diagram of a light spot generated by the optical anti-counterfeiting element at a first observation angle;

[0034] Figure 8 Shows Figure 1 A position diagram of a light spot generated by the optical anti-counterfeiting element at a second observation angle;

[0035] Fig. 9 Shows Figure 1 A diagram showing the position of a light spot generated by the optical anti-counterfeiting element at a third observation angle;

[0036] Fig.10 A view showing an angle of the optical anti-counterfeiting element according to the first embodiment of the present invention;

[0037] Fig.11 A structural comparison diagram of the optical anti-counterfeiting element before and after hollowing out according to the first embodiment of the present invention is shown;

[0038] Fig.12 Shows Fig.10 A position diagram of a light spot generated by the optical anti-counterfeiting element at a first observation angle;

[0039] Fig.13 Shows Fig.10 A position diagram of a light spot generated by the optical anti-counterfeiting element at a second observation angle;

[0040] Fig.14 Shows Fig.10 Schematic diagram of the optical anti-counterfeiting element generating no light spot at a third observation angle;

[0041] Fig.15 Shows Fig.10 The optical effect diagram of the optical anti-counterfeiting product at the first observation angle;

[0042] Fig.16 Shows Fig.10 The optical effect diagram of the optical anti-counterfeiting product under the second observation angle;

[0043] Fig.17 Shows Fig.10 The optical effect diagram of the optical anti-counterfeiting product under the third observation angle;

[0044] Fig.18 A view showing an angle of the optical anti-counterfeiting element of the second embodiment of the present invention;

[0045] Fig.19 Shows Fig.18 A cross-sectional view at an angle;

[0046] Fig. 20 A view showing an angle of the optical anti-counterfeiting element of the third embodiment of the present invention;

[0047] Fig.21 Shows Fig. 20 A cross-sectional view of an optical anti-counterfeiting element;

[0048] Fig. 22 A flowchart of manufacturing an optical anti-counterfeiting element according to an optional embodiment of the present invention is shown.

[0049] The above drawings include the following reference numerals:

[0050] 10. Microstructure forming layer; 20. Microstructure; 21. First microstructure; 211. First design area; 212. First defect area; 22. Second microstructure; 221. Second design area; 222. Second defect area; 23. Third microstructure; 231. Third design area; 232. Third defect area; 30. Coating; 31. First section coating; 311. First section effective area; 312. First section invalid area; 32. Second section coating; 321. The second effective area; 322, the second invalid area; 33, the third coating; 331, the third effective area; 332, the third invalid area; 34, the hollow area; 40, the carrier; 50, the optical anti-counterfeiting product; 60, the light spot; 70, the reflected light; 80, the first observation angle; 90, the second observation angle; 100, the third observation angle; 120, the protective layer; 130, the optical anti-counterfeiting element; 140, the incident light; 150, the auxiliary protective layer. DETAILED DESCRIPTION

[0051] It should be noted that, in the absence of conflict, the embodiments and features in the embodiments of the present application can be combined with each other. The present invention will be described in detail below with reference to the accompanying drawings and in combination with the embodiments.

[0052] It should be noted that, unless otherwise specified, all technical and scientific terms used in this application have the same meanings as commonly understood by ordinary technicians in the technical field to which this application belongs.

[0053] In the present invention, unless otherwise specified, the directional words used, such as "up, down, top, bottom", usually refer to the directions shown in the drawings, or to the components themselves in the vertical, perpendicular or gravity directions; similarly, for ease of understanding and description, "inside and outside" refer to the inside and outside relative to the outline of each component itself, but the above-mentioned directional words are not used to limit the present invention.

[0054] In order to solve the problem in the prior art that the actual optical effect produced by the optical anti-counterfeiting element has a large deviation from the expected optical effect, the present invention provides an optical anti-counterfeiting element, an optical anti-counterfeiting product and a manufacturing method.

[0055] like Figures 10 to 22 As shown, the optical anti-counterfeiting element 130 includes a substrate, a microstructure forming layer 10 and a coating 30. The microstructure forming layer 10 is arranged on one side surface of the substrate. The microstructure forming layer 10 has a microstructure 20, and the longitudinal section of the microstructure 20 is a preset shape; the coating 30 is arranged on the microstructure forming layer 10, and the microstructure 20 is plated with the coating 30 to form a plated microstructure, and the height of the plated microstructure changes continuously; wherein, when the microstructure 20 has a mutation position, the coating 30 has a hollow area 34, and when the height of the microstructure 20 changes continuously, the coating 30 has no hollow area 34.

[0056] By arranging the coating 30 on the microstructure forming layer 10, the height of the formed plated microstructure changes continuously, thereby avoiding defects caused by mutations in the coating 30, avoiding mutations in the optical characteristics, and ensuring the anti-counterfeiting performance of the optical anti-counterfeiting element 130. In the present application, there are two situations. One situation is that the microstructure 20 has a mutation position. In this case, the coating 30 has a hollow area 34. The setting of the hollow area 34 is conducive to the continuous change of the height of the plated microstructure, thereby avoiding mutations affecting the optical characteristics of the optical anti-counterfeiting element 130. In another situation, the height of the microstructure 20 changes continuously without a mutation position. In this case, the coating 30 has no hollow area 34, thus avoiding the risk of changes in the optical properties of the coating 30 caused by mutations in the microstructure 20, and further avoiding changes in the anti-counterfeiting characteristics of the optical anti-counterfeiting element 130.

[0057] In this embodiment, the hollow area 34 is set at the position where the microstructure 20 mutates, so that the height of the plated microstructure changes continuously, wherein the hollow area 34 is in the form of non-macroscopic hollow images, which refer to hollow images that cannot be directly observed by the human eye and can only be observed using a microscope, and the non-macroscopic hollow images do not affect the anti-counterfeiting effect of the coating 30. The setting of the hollow area 34 makes it so that the microstructure forming layer 10 at this position will not interact with the coating 30 to produce a preset optical effect, effectively avoiding the generation of unnecessary optical features. The hollow area 34 does not affect the anti-counterfeiting effect of the coating 30. The role of the hollow area 34 is to remove the defects of the coating 30 caused by the position where the microstructure 20 mutates, effectively improving the optical performance of the anti-counterfeiting element, and the hollow area 34 cannot be directly observed by the human eye, but can only be seen using a microscope, and can be used as a marker to increase the anti-counterfeiting performance of the anti-counterfeiting element.

[0058] In an optional embodiment, the characteristic width of the hollow area 34 is greater than or equal to 0.1 μm and less than or equal to 100 μm. If the characteristic width of the hollow area 34 is less than 0.1 μm, it is difficult for the hollow area 34 to completely remove the defects caused by the position where the microstructure 20 mutates, thereby affecting the anti-counterfeiting effect. If the characteristic width of the hollow area 34 is greater than 100 μm, the hollow area 34 is easily discovered by the observer, resulting in a deviation between the actual optical effect and the designed optical effect. Limiting the characteristic width of the hollow area 34 to a range of 0.1 μm to 100 μm ensures that the defects caused by the position where the microstructure 20 mutates are completely removed while preventing the hollow area 34 from being discovered by the observer, thereby ensuring the anti-counterfeiting effect of the optical anti-counterfeiting element 130.

[0059] The hollow area 34 in the present application is mainly used to remove the sudden defects of the microstructure 20 caused by the manufacturing accuracy and replication accuracy, so as to make the actual optical effect as close as possible to the designed optical effect. Therefore, the hollow area 34 cannot be too large, otherwise the hollow area 34 will be discovered by the observer, resulting in a deviation between the actual optical effect and the designed optical effect.

[0060] It should be noted that the range of the characteristic width of the hollow area 34 can be calculated according to the Rayleigh criterion.

[0061] In an optional embodiment, the ratio of the area of ​​the hollow region 34 to the total area of ​​the optical anti-counterfeiting element 130 is less than or equal to 0.5. Limiting the ratio of the area of ​​the hollow region 34 to the total area of ​​the optical anti-counterfeiting element 130 to a range of less than or equal to 0.5 is conducive to retaining the original effectively designed microstructure 20 and reducing the deviation between the actual optical effect of the optical anti-counterfeiting element 130 and the designed optical effect.

[0062] It should be noted that, in the present application, the hollow area 34 does not add any additional useful information, so it is necessary to retain as much of the original effectively designed microstructure 20 as possible.

[0063] When the parameters of the microstructure 20 change, the height of the microstructure 20 at that position may suddenly change. For example, facing the same two adjacent reflective surfaces, the position of the highest point of the first reflective surface on the plane where the optical anti-counterfeiting element 130 is located is theoretically the same as the position of the lowest point of the second reflective surface on the plane where the optical anti-counterfeiting element 130 is located, but the height suddenly changes from a maximum value to a minimum value.

[0064] When the parameters of the microstructure 20 change, it may also be caused by microstructures 20 with different parameters. For example, two microstructures with orientations different by 90° may also have a sudden change in the microstructure 20 at the junction.

[0065] In the actual manufacturing process, the preparation accuracy, material resolution and replication transfer process will produce deviations in these mutation areas, which will interfere with the design effect. Therefore, it is necessary to remove the coating 30 above these deviation areas.

[0066] When the height of the microstructure 20 changes continuously, the microstructure 20 is not abrupt, and will not cause obvious interference to the original design during production and replication, so hollowing out is not required.

[0067] Optionally, when there are multiple hollow areas 34 , at least two of the multiple hollow areas 34 are connected to each other.

[0068] Optionally, when there are multiple hollow areas 34 , at least two of the multiple hollow areas 34 are not connected to each other.

[0069] Since the hollow areas 34 are determined according to the parameter changes of the microstructure 20, the hollow areas 34 may be interconnected or not completely connected. Of course, they may also be completely disconnected. The design can be based on the actual needs of the microstructure 20, and no specific restrictions are made here.

[0070] Optionally, the preset shape includes at least one of a sine shape, a wedge shape, a symmetrical rectangular tooth, an asymmetrical rectangular tooth, a semicircle, a rectangle, and a trapezoid. There is basically no restriction on the type of the microstructure 20, and no specific restriction is made here. The preset shape of the microstructure 20 is the shape of the microstructure 20 commonly used in the optical anti-counterfeiting element 130.

[0071] Optionally, the characteristic size of the microstructure 20 in a plane parallel to the substrate is greater than or equal to 0.1 μm and less than or equal to 500 μm. The plane where the optical anti-counterfeiting element 130 is located is defined as the xy plane, and the type and shape of the microstructure 20 are determined in the xy plane. The characteristic size of the microstructure 20 in a plane parallel to the substrate is the characteristic size of the microstructure 20 in the xy plane.

[0072] Preferably, the characteristic size of the microstructure 20 in a plane parallel to the substrate is greater than or equal to 0.2 μm and less than or equal to 100 μm.

[0073] It should be noted that the direction perpendicular to the xy plane is the z-axis direction, and the height of the microstructure 20 changes in the z-axis direction.

[0074] Optionally, the coating layer 30 provides a preset reflection characteristic or a preset transmission characteristic. In order to enhance the optical effect of the optical anti-counterfeiting element 130 , a coating layer 30 with a reflection enhancement or transmission enhancement characteristic is deposited on the microstructure forming layer 10 .

[0075] Optionally, the coating 30 may be a single reflective layer or a single dielectric layer, or a stacked layer formed by stacking multiple dielectric layers; of course, the coating 30 may also be a stacked layer formed by alternately stacking reflective layers and dielectric layers.

[0076] Preferably, the coating 30 is formed by alternating high-refractive index dielectric layers and low-refractive index dielectric layers. This structure can selectively reflect and transmit light of a specific wavelength, forming a first color when observed from the front, and a complementary color of the color when observed through light. When the light is incident at an angle, the optical path of the light when propagating in the coating 30 is different from the optical path when it is incident vertically, forming a second color, thereby forming a color change effect. At the same time, when this structure of alternating high-refractive index dielectric layers and low-refractive index dielectric layers is combined with a one-dimensional sub-wavelength grating, a third color different from the laminated structure can be formed. The period of the one-dimensional sub-wavelength grating is 350nm and the depth is 110nm.

[0077] It can also be formed by stacking a high refractive index dielectric layer, a reflective layer, or a high refractive index dielectric layer, or a Fabry-Perot cavity of a reflective layer-dielectric layer-reflective layer. The Fabry-Perot cavity is a wavelength selection structure with higher reflection efficiency, which is a film structure of "absorption layer / dielectric layer / reflective coating layer". The absorption layer is a metal material with a relatively thin thickness. When light passes through this layer, about half of the light is reflected and the other half is transmitted, so the absorption layer can be called a "semi-reflective and semi-transparent film", including but not limited to chromium, nickel, copper, cobalt, titanium, vanadium, tungsten, tin, silicon, germanium and combinations thereof, and its thickness can be 2nm to 30nm.

[0078] In the "Fabry-Perot resonant cavity" structure, the absorption layer acts as a beam splitter, reflecting the general light (called the first light beam) and transmitting half of the light. After the transmitted light passes through the dielectric layer, it is reflected by the reflective coating and then emitted through the absorption layer (called the second light beam). The first light beam and the second light beam interact with each other to produce interference, forming a selective enhancement of a specific wavelength, so the color can be observed. When the light changes its incident direction, the optical path of the light beam in the dielectric layer changes. If the dielectric material is a high refractive index material, the color remains unchanged or the change is not obvious. If the dielectric material is a low refractive index material, the color changes significantly, and it has the so-called light-changing effect. For example, the "Fabry-Perot resonant cavity" structure can be metal chromium / silicon dioxide / metal aluminum or metal aluminum / aluminum dioxide / metal aluminum. When the observation angle is changed, the color of the Fabry-Perot interferometer can change.

[0079] Half of the dielectric layer is a metal compound. The dielectric layer material can be a low-refractive-index dielectric material with a refractive index less than 1.8, including but not limited to silicon dioxide, magnesium fluoride, cryolite, aluminum oxide and combinations thereof, with a thickness of 100 to 1000 nm; the dielectric material can also be a high-refractive-index material with a refractive index greater than 1.8, including but not limited to any material or combination of ZnS, TiN, TiO2, TiO, Ti2O3, Ti3O5, Ta2O5, Nb2O5, CeO2, Bi2O3, Cr2O3, and Fe2O3. The coating material is generally a metal material with high reflectivity, or it can be a non-metallic material, including but not limited to any material or combination of aluminum, silver, tin, nickel, chromium, platinum, copper, gold, and silicon, with a thickness greater than or equal to 10 nm.

[0080] In the present application, the reflective layer can be a pure metal material or alloy with high reflectivity, and can be a full-spectrum reflective material, such as aluminum, silver, tin, nickel, chromium, platinum and other materials; it can also be a reflective material with a specific color and a corresponding alloy material, such as copper, gold and other materials, which can produce a fixed color while providing a high reflectivity. The function of the reflective layer is mainly to increase the diffraction rate and reflectivity, and the reflective layer itself does not have the effect of color change.

[0081] When the metal reflective material is combined with the reflective grating, the reflection efficiency is improved to form a bright reflection effect. The reflective grating can be a wedge-type blazed grating with a period of 13μm and a depth of 2μm.

[0082] The reflective layer may also be a metal compound, which may be a metal oxide, such as titanium dioxide, zirconium dioxide, etc.; it may also be a metal sulfide, such as zinc sulfide; or it may be other metal compounds.

[0083] The material of the coating layer 30 may also be an optical medium material, such as silicon dioxide.

[0084] The refractive index of the high refractive index medium layer is n≥1.8, including but not limited to any material or combination of ZnS, TiN, TiO2, TiO, Ti2O3, Ti3O5, Ta2O5, Nb2O5, CeO2, Bi2O3, Cr2O3, and Fe2O3.

[0085] The refractive index of the low-refractive-index medium layer is n<1.8, including but not limited to any material or combination of SiO2, MgF2, Na3AlO6, and Al2O3.

[0086] Optionally, the optical anti-counterfeiting element 130 also includes a protective layer, which is disposed on the coating 30 and is a transparent layer. The difference in refractive index between the protective layer and the microstructure forming layer 10 is less than 0.5. In order to achieve better protection performance and durability, a transparent protective layer is covered on the coating 30. The protective layer includes but is not limited to acrylic materials. At the same time, the closer the difference in refractive index between the above-mentioned protective layer and the refractive index of the microstructure forming layer 10 is to 0, the better. In this way, after applying the protective glue, the optical properties of the protective layer in the hollow area 34 and the microstructure forming layer 10 can be considered to be close or even consistent, and the interface between the protective layer and the microstructure forming layer 10 will no longer exist at the optical level, which is equivalent to completely filling the gap in the original hollow area.

[0087] Optionally, the optical anti-counterfeiting element 130 can also be used as a label, logo, wide strip, transparent window, film, etc., and can be attached to various items through various bonding mechanisms, such as transferred to high-security products and high-value-added products such as banknotes and credit cards.

[0088] The optical anti-counterfeiting product 50 includes the above-mentioned optical anti-counterfeiting element 130. The optical anti-counterfeiting product 50 having the above-mentioned optical anti-counterfeiting element 130 has the advantage of good anti-counterfeiting effect. The optical anti-counterfeiting product 50 includes but is not limited to various high-security products and high-value-added products such as banknotes, credit cards, passports, securities, and various packaging papers, packaging boxes, etc.

[0089] According to another aspect of the present invention, a method for manufacturing an optical anti-counterfeiting element 130 is provided. The method for manufacturing the optical anti-counterfeiting element 130 is used to manufacture the above-mentioned optical anti-counterfeiting element 130. The method for manufacturing the optical anti-counterfeiting element 130 includes: forming a microstructure forming layer 10 having a microstructure 20 on a substrate; forming a coating layer 30 having a hollow area 34 on the microstructure forming layer 10; and forming a protective layer 120 on the coating layer 30.

[0090] like Fig.21 As shown, the manufacturing method of the optical anti-counterfeiting element 130 is used to manufacture the above-mentioned optical anti-counterfeiting element 130, and the manufacturing method of the optical anti-counterfeiting element 130 includes: obtaining a microstructure forming layer 10 with a microstructure 20 by molding or UV casting; depositing a coating 30 on the microstructure forming layer 10 by physical vapor deposition; printing a protective glue on the coating 30 by printing to form an auxiliary protective layer 150, and exposing the mutation position of the microstructure 20; placing the above-mentioned structure in a corresponding corrosion solution for immersion, and removing the coating 30 in the exposed area; covering the protective layer 120 on the above-mentioned structure by wet coating to form the optical anti-counterfeiting element 130.

[0091] The protective layer 120 has a refractive index that is the same as or close to that of the microstructure forming layer 10 , forming an optically unified microstructure forming-protective layer.

[0092] Embodiment 1

[0093] In order to facilitate the understanding of the technical solution of the present application, the reasons why the optical anti-counterfeiting elements in the prior art produce non-predetermined optical effects are explained.

[0094] Figures 1 to 9 They are all optical anti-counterfeiting elements 130 in the prior art. The optical anti-counterfeiting element 130 can be attached to a carrier 40 to form an optical anti-counterfeiting product 50. The carrier 40 can be a banknote, paper, passport, securities, etc., and the material can be paper, polypropylene, polycarbonate, etc.

[0095] Figure 2 and Figure 3 for Figure 1 The schematic cross-sectional view of the optical anti-counterfeiting element 130 in the yz plane is shown.

[0096] In order to more clearly identify each location, it will be divided into Figure 2 and Figure 3 Show. Figure 2 In the figure, the microstructure forming layer 10 has reflective surfaces with different inclination angles, and in the cross-sectional view it is a wedge-shaped structure. Take the typical first microstructure 21, second microstructure 22 and third microstructure 23 for illustration. The first microstructure 21 has two parts, namely a first design area 211 with a gentler gradient and a first defect area 212 with a steeper gradient. Similarly, the second microstructure 22 has two parts, namely a second design area 221 with a gentler gradient and a second defect area 222 with a steeper gradient; the third microstructure 23 has two parts, namely a third design area 231 with a gentler gradient and a third defect area 232 with a steeper gradient. When designing the microstructure, the shape of the microstructure is perfect. The first microstructure 21 has only the first design area 211, the second microstructure 22 has the second design area 221, and the third microstructure 23 has the third design area 231. However, due to the limitations of the manufacturing process, material resolution and subsequent replication process of the microstructure 20, the side walls of the microstructure 20 generally will not form a completely vertical situation, and the following will appear. Figure 2 The situation of the first defect area 212, the second defect area 222 and the third defect area 232.

[0097] like Figure 3As shown, a coating layer 30 is covered on the microstructure forming layer 10. The coating layer 30 can be metal aluminum with a thickness of 100 nm, which is deposited on the microstructure forming layer 10 by thermal evaporation. Since the optical film obtained by physical vapor deposition (PVD) such as thermal evaporation can be more evenly covered on the surface of the microstructure 20, which is different from the coating obtained by wet coating, the shape of the coating layer 30 basically maintains the shape of the original microstructure 20, that is, the same type of coverage. Therefore, the first section of the coating layer 31 also has a first section of the effective area 311 and a first section of the invalid area 312; the second section of the coating layer 32 also has a second section of the effective area 321 and a second section of the invalid area 322; the third section of the coating layer 33 also has a third section of the effective area 331 and a third section of the invalid area 332.

[0098] Figures 4 to 6 for Figure 1 The optical anti-counterfeiting element 130 has appearances at different observation angles.

[0099] Figure 4 The position of the light spot 60 on the optical security element 130 is shown at the first observation angle 80. Figure 4 The middle light spot 60 is located below the optical anti-counterfeiting element 130 .

[0100] Figure 5 The position of the light spot 60 on the optical security element 130 is shown at the second observation angle 90. Figure 5 The middle light spot 60 is located above the optical anti-counterfeiting element 130 .

[0101] Figure 6 The position of the light spot 60 on the optical security element 130 is shown at the third observation angle 100. Figure 6 The intensity of the middle light spot 60 is relatively weak. This light spot 60 will also move with the change of the viewing direction, forming a second dynamic feature, which is not designed and may interfere with the dynamic feature required by the first design.

[0102] When the light spot 60 changes from the first observation angle 80 to the second observation angle 90, Figure 4 The position shown gradually moves to Figure 5 At the position shown, the movement of the light spot 60 brings a dynamic effect. When the third observation angle 100 is further increased, a light spot 60 with a weaker intensity appears, and this light spot 60 also moves with the change of the observation direction, forming a second dynamic feature, which is not designed and may interfere with the dynamic feature required by the first design.

[0103] Figures 7 to 9 The sources of the interfering light spots are given.

[0104] Figure 7FIG. 8 shows the reflection position of the coating 30 at the first observation angle 80. At the first observation angle 80, according to the reflection law, the third effective area 331 of the third coating 33 reflects the incident light 140 to form reflected light 70 ( Figure 4 The light spot 60 shown in the figure can be observed by the observer, while the first section coating 31 and the second section coating 32 cannot enter the observer's eyes and cannot be observed.

[0105] Figure 8 FIG. 3 shows the reflection position of the coating 30 at the second observation angle 90. At the second observation angle 90, according to the law of reflection, the reflected light 70 reflected by the first effective area 311 of the first coating 31 is seen by the observer ( Figure 5 60).

[0106] Fig. 9 FIG. 1 shows the reflection position of the coating 30 at the third observation angle 100. At the third observation angle 100, the reflected light 70 reflected by the second invalid area 322 of the second coating 32 is seen by the observer ( Figure 6 The light spot 60 shown in the figure, that is, the interference light spot), is relatively dark because the area of ​​the invalid area is smaller than that of the effective area. However, the light spot is not required by the design, and thus interference is formed.

[0107] When the coating 30 is a "reflective layer / medium layer / reflective layer, wherein the reflective layer is a metal material" coating, a specific color can be formed. This interference will not only cause the light spot to recur, but also cause the interference of color deviation.

[0108] pass Figures 1 to 9 The principle of the appearance of interference light spots has been understood, and the principle of removing interference light spots in the present application is introduced below.

[0109] In order to solve the above problems, it is necessary to remove the coating 30 in the interference area. In order to solve the above problems, it is necessary to remove the coating 30 in the interference area. Since the shape of the microstructure 20 is not easy to change, an effective way is to hollow out and remove the specific area (ie, the invalid area) after the coating 30 is formed, so as to effectively remove the interference.

[0110] Fig.10 This is the case of an optical anti-counterfeiting element 130 of an optional embodiment of the present application, wherein the gray gradient of the square represents the coating 30 on the microstructure 20 with a gradient height, the darker the lower the height, and the whiter the higher the height. The white area around each gray gradient square represents the hollow area 34.

[0111] Fig.11 The state diagram of the optical anti-counterfeiting element 130 before and after hollowing out, from Fig.11It can be seen that after the continuous coating 30 on the microstructure forming layer 10 of the optical anti-counterfeiting element 130 is hollowed out, the coating 30 in the invalid area is completely removed, and the effective area is retained to form the coating 30 with the hollowed-out area 34.

[0112] Figure 12 to Figure 14 The reflected light observed at the first observation angle 80 , the second observation angle 90 , and the third observation angle 100 of the optical security element 130 having the hollow area 34 are respectively shown.

[0113] Figure 12 to Figure 14 for Fig.11 Observation of the coating with cutout areas 34 is shown.

[0114] Fig.12 The reflection position of the coating 30 at a first observation angle 80 is shown. Fig.13 The reflection position of the coating 30 at a second observation angle 90 is shown. Fig.14 The reflection position of the coating 30 at a third observation angle 100 is shown.

[0115] Fig.12 FIG. 8 shows the reflection position of the coating 30 at the first observation angle 80. At the first observation angle 80, according to the reflection law, the third effective area 331 of the third coating 33 reflects the incident light 140 to form reflected light 70 ( Figure 4 The light spot 60 shown in the figure can be observed by the observer, while the first section coating 31 and the second section coating 32 cannot enter the observer's eyes and cannot be observed.

[0116] Fig.13 FIG. 3 shows the reflection position of the coating 30 at the second observation angle 90. At the second observation angle 90, according to the law of reflection, the reflected light 70 reflected by the first effective area 311 of the first coating 31 is seen by the observer ( Figure 5 60).

[0117] Fig.14 The reflection position of the coating 30 at the third observation angle 100 is shown. At the third observation angle 100, the coating 30 of the second invalid area 322 of the second coating 32 is hollowed out, so there is no interference from reflected light, and thus the interference light spot is removed to ensure that the optical anti-counterfeiting element 130 achieves the preset optical effect.

[0118] from Figure 12 to Figure 14 It can be seen that the coating 30 in the effective area can form a light spot. Since the coating 30 in the invalid area is hollowed out and removed, there is no reflected light interference in the invalid area. Therefore, the interfering light spot is removed to ensure that the optical anti-counterfeiting element 130 achieves the preset optical effect.

[0119] The valid area includes a first valid area 311 , a second valid area 321 and a third valid area 331 ; the invalid area includes a first invalid area 312 , a second invalid area 322 and a third invalid area 332 .

[0120] Figures 15 to 17 for Fig.10 The optical anti-counterfeiting element 130 has appearances at different observation angles.

[0121] Fig.15 The position of the light spot 60 on the optical security element 130 is shown at the first observation angle 80. Fig.15 The middle light spot 60 is located below the optical anti-counterfeiting element 130 .

[0122] Fig.16 The position of the light spot 60 on the optical security element 130 at the second observation angle 90 is shown. Fig.16 The middle light spot 60 is located above the optical anti-counterfeiting element 130 .

[0123] Fig.17 The optical effect produced by observing the optical security element 130 at a third observation angle 100 is shown. At the third observation angle 100, no light spot is seen.

[0124] When the light spot 60 changes from the first observation angle 80 to the second observation angle 90, Fig.15 The position shown gradually moves to Fig.16 In the position shown, the movement of the light spot 60 brings a dynamic effect. When the third observation angle 100 is further increased, no light spot appears, and the optical anti-counterfeiting element 130 in the present application has only a dynamic effect.

[0125] Embodiment 2

[0126] The difference from the first embodiment is that the area of ​​the hollow area 34 is different.

[0127] like Fig.18 and Fig.19 As shown, since the height of some microstructures 20 does not change suddenly or the parameters of some reflective surfaces of the microstructures 20 are the same, not all intersections of the reflective surfaces need to be hollowed out. Fig.18 The two areas (a) and (b) in the figure contain two reflective surfaces, but since the reflective surfaces are arranged side by side, there is no change between the two reflective surfaces, so there is no need to hollow them out. Fig.18 In the region (c), although the two reflective surfaces have different parameters and different orientations, since the height of the microstructure 20 at the junction of the two reflective surfaces changes continuously and there is no height mutation, there is no need to hollow it out.

[0128] Fig.19 for Fig.18 In the longitudinal cross-sectional view, a coating 30 is deposited on the surface of the microstructure forming layer 10, a hollow area 34 is provided at the mutation position of the microstructure 20, and the height of the microstructure 20 in other areas changes continuously, and no hollowing is required, and the coating 30 is continuously distributed.

[0129] Embodiment 3

[0130] The difference from the first embodiment is that the present embodiment has a protective layer 120 .

[0131] exist Fig. 20 and 21 In the specific embodiment shown, a protective layer 120 is disposed on the plating layer 30 .

[0132] In this embodiment, the protective glue is generally evenly coated on the surface of the coating layer 30 by wet coating to form the protective layer 120. When the refractive index of the microstructure forming layer 10 and the protective layer 120 is the same or close, it can be considered that the optical properties of the two materials are the same, and the reflection and refraction efficiency of the contact surface between the two can be ignored. They can be regarded as one material. Fig.21 In the illustrated case, the plating layer 30 in a separated state is buried between the microstructure forming layer 10 and the protective layer 120 .

[0133] Obviously, the above-described embodiments are only a part of the embodiments of the present invention, rather than all the embodiments. Based on the embodiments of the present invention, all other embodiments obtained by ordinary technicians in this field without creative work should fall within the scope of protection of the present invention.

[0134] It should be noted that the terms used herein are only for describing specific embodiments and are not intended to limit the exemplary embodiments according to the present application. As used herein, unless the context clearly indicates otherwise, the singular form is also intended to include the plural form. In addition, it should be understood that when the terms "comprise" and / or "include" are used in this specification, it indicates the presence of features, steps, operations, devices, components and / or combinations thereof.

[0135] It should be noted that the terms "first", "second", etc. in the specification and claims of the present application and the above-mentioned drawings are used to distinguish similar objects, and are not necessarily used to describe a specific order or sequence. It should be understood that the numbers used in this way can be interchanged where appropriate, so that the embodiments of the present application described herein can be implemented in an order other than those illustrated or described herein.

[0136] The above description is only a preferred embodiment of the present invention and is not intended to limit the present invention. For those skilled in the art, the present invention may have various modifications and variations. Any modification, equivalent replacement, improvement, etc. made within the spirit and principle of the present invention shall be included in the protection scope of the present invention.

Claims

1. An optical anti-counterfeiting element, characterized in that: include: Base material; A microstructure forming layer (10), the microstructure forming layer (10) being disposed on a surface of one side of the substrate, the microstructure forming layer (10) having a microstructure (20), the longitudinal section of the microstructure (20) being a preset shape; A coating (30), wherein the coating (30) is disposed on the microstructure forming layer (10), and the microstructure (20) is coated with the coating (30) to form a coated microstructure, wherein the height of the coated microstructure changes continuously; Wherein, when the microstructure (20) has a mutation position, the coating (30) has a hollow region (34), and when the height of the microstructure (20) changes continuously, the coating (30) has no hollow region (34).

2. The optical anti-counterfeiting element according to claim 1, characterized in that: The hollow area (34) is arranged at a position where the microstructure (20) undergoes a sudden change, so that the height of the plated microstructure changes continuously, wherein the hollow area (34) is in the form of a non-macroscopic hollow pattern, which refers to a hollow pattern that cannot be directly observed by the human eye and can only be observed using a microscope, and the non-macroscopic hollow pattern does not affect the anti-counterfeiting effect of the plated layer (30).

3. The optical anti-counterfeiting element according to claim 2, characterized in that: The characteristic width of the hollow area (34) is greater than or equal to 0.1 μm and less than or equal to 100 μm.

4. The optical anti-counterfeiting element according to claim 2, characterized in that: The ratio of the area of ​​the hollow region (34) to the total area of ​​the optical anti-counterfeiting element is less than or equal to 0.

5.

5. The optical anti-counterfeiting element according to claim 2, characterized in that: When there are a plurality of hollow regions (34), at least two of the plurality of hollow regions (34) are interconnected.

6. The optical anti-counterfeiting element according to claim 2, characterized in that: When there are a plurality of hollow regions (34), at least two of the plurality of hollow regions (34) are not connected to each other.

7. The optical anti-counterfeiting element according to any one of claims 1 to 6, characterized in that: The preset shape includes at least one of a sine shape, a wedge shape, a symmetrical rectangular tooth, an asymmetrical rectangular tooth, a semicircular rectangle, and a trapezoid.

8. The optical anti-counterfeiting element according to any one of claims 1 to 6, characterized in that: The characteristic size of the microstructure (20) in a plane parallel to the substrate is greater than or equal to 0.1 μm and less than or equal to 500 μm.

9. The optical anti-counterfeiting element according to claim 8, characterized in that: The characteristic size of the microstructure (20) in a plane parallel to the substrate is greater than or equal to 0.2 μm and less than or equal to 100 μm.

10. The optical anti-counterfeiting element according to any one of claims 1 to 6, characterized in that: The coating (30) provides a preset reflection characteristic or a preset transmission characteristic.

11. The optical anti-counterfeiting element according to any one of claims 1 to 6, characterized in that: The coating (30) is a single-layer reflective layer or a single-layer dielectric layer.

12. The optical anti-counterfeiting element according to any one of claims 1 to 6, characterized in that: The coating (30) is a laminate formed by stacking multiple dielectric layers; or The coating (30) is a laminate formed by alternately stacking reflective layers and dielectric layers.

13. The optical anti-counterfeiting element according to any one of claims 1 to 6, characterized in that: The optical anti-counterfeiting element further comprises a protective layer (120), wherein the protective layer is arranged on the coating layer (30), and the protective layer (120) is a transparent layer.

14. The optical anti-counterfeiting element according to claim 13, characterized in that: The difference in refractive index between the protective layer and the microstructure forming layer (10) is less than 0.

5.

15. An optical anti-counterfeiting product, characterized in that: An optical anti-counterfeiting element comprising any one of claims 1 to 14.

16. A method for manufacturing an optical anti-counterfeiting element, characterized in that: The method for manufacturing the optical anti-counterfeiting element is used to manufacture the optical anti-counterfeiting element according to any one of claims 1 to 14, and the method for manufacturing the optical anti-counterfeiting element comprises: forming a microstructure forming layer (10) having a microstructure (20) on a substrate; forming a plating layer (30) having a hollow region (34) on the microstructure forming layer (10); A protective layer (120) is formed on the plating layer (30).

Citation Information

Patent Citations

  • See-through security element with microstructures

    CN101528474A

  • Optical anti-counterfeiting element and preparation method thereof and optical anti-counterfeiting product

    CN110450560A

  • Anti-counterfeiting image element and anti-counterfeiting product

    CN115891480A

  • Security element having pressure-sensitive appearance

    EP2349736A2

Cited By

  • Optical Anti-counterfeiting element, optical Anti-counterfeiting product, and manufacturing method

    EP4530088A1

  • Optical Anti-counterfeiting element, optical Anti-counterfeiting product, and manufacturing method

    WO2024234684A1