Coating adhesive with high corrosion resistance and processing method thereof

By preparing a highly corrosion-resistant coating adhesive and combining epoxy resin and quartz powder, the problem of easy peeling of the coating adhesive outdoors was solved, thereby improving corrosion resistance and environmental friendliness. It is suitable for corrosion protection and decoration of various substrates.

CN118995002APending Publication Date: 2024-11-22HANGZHOU HUAYI NEW MATERIALS CO LTD
View PDF 4 Cites 0 Cited by

Patent Information

Application Number
CN202411076242.9
Authority / Receiving Office
CN · China
Patent Type
Applications(China)
Current Assignee / Owner
Filing Date
2024-08-07
Publication Date
2024-11-22

AI Technical Summary

Technical Problem

Existing coating adhesives are prone to peeling and breaking when used outdoors, making it difficult to achieve corrosion resistance.

Method used

Epoxy resin was used as the base monomer and quartz powder as the filler. The coating adhesive was prepared by heating and stirring and heating degassing. Organic and inorganic substances were combined, water was used as the solvent, and dispersants and inorganic flame retardants were added to optimize the corrosion resistance of the coating.

Benefits of technology

It improves the corrosion resistance of the coating adhesive while maintaining its environmental friendliness, and is suitable for anti-corrosion protection and decorative treatment of metals, plastics and wood.

✦ Generated by Eureka AI based on patent content.
Patent Text Reader

Abstract

The invention relates to the field of coating adhesives, and discloses a high-corrosion-resistance coating adhesive which is prepared from the following raw materials: 100 parts of a basic monomer, 30 parts of a curing agent, 20 parts of a solvent, 50 parts of filler and 10 parts of an auxiliary agent, the preparation method of the coating adhesive comprises the following steps: S1, pouring the basic monomer, the curing agent, the solvent, the auxiliary agent and the flame retardant into a semi-closed container, heating and stirring, and stopping stirring after stirring reaction for 3 hours; s2, mixing the solution obtained by stirring with a filler, and adding water in a ratio of 1: 1: 1 for dissolving and mixing; and S3, mixing to obtain a semi-finished product coating adhesive, adding a dispersing agent at the moment, and stirring for not less than 1 hour. According to the high-corrosion-resistance coating adhesive and the processing method thereof, through heating combination of the organic matter and the inorganic matter, the overall corrosion resistance of the coating adhesive can be greatly improved, meanwhile, water is adopted as a solvent, the overall corrosion resistance of the coating adhesive is improved, meanwhile, toxicity cannot be improved, and the whole coating adhesive is more environmentally friendly.
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] The invention relates to the field of coating adhesives, in particular to a highly corrosion-resistant coating adhesive and a processing method thereof. Background Art

[0002] Textile coating finishing agent, also known as coating glue, is a polymer compound that is evenly coated on the surface of the fabric. It forms one or more layers of film on the surface of the fabric through adhesion, which can not only improve the appearance and style of the fabric, but also increase the function of the fabric, making the fabric waterproof, water pressure resistant, breathable and moisture permeable, flame retardant and anti-fouling, as well as light shading and reflection and other special functions.

[0003] Since the advent of coating adhesives, their wide application types have grown and expanded. Most of the existing coating adhesives are PA, PU, ​​PVC, silicone and synthetic rubber. These types of coating adhesives are difficult to achieve corrosion resistance. During daily use, they are easy to fall off and break due to the influence of outdoor weather or environment. Therefore, a corrosion-resistant coating adhesive is urgently needed to solve the above problems. Summary of the invention

[0004] 1. Technical issues to be solved

[0005] In view of the deficiencies in the prior art, the present invention provides a highly corrosion-resistant coating adhesive and a processing method thereof, which has the advantages of corrosion resistance and the like and solves the problems in the above-mentioned background technology.

[0006] (II) Technical solution

[0007] In order to achieve the above-mentioned corrosion resistance purpose, the present invention provides the following technical solution: a highly corrosion-resistant coating adhesive, comprising the following preparation raw materials:

[0008] Base monomer - 100 parts, curing agent - 30 parts, solvent - 20 parts, filler - 50 parts, auxiliary agent - 10 parts, flame retardant - 5 parts.

[0009] Preferably, the preparation steps of the coating adhesive are:

[0010] S1: Pour the base monomer, curing agent, solvent, additive and flame retardant into a semi-closed container for heating and stirring, and stop stirring after stirring for 3 hours;

[0011] S2: Mix the solution obtained by stirring with the filler, and add water in a ratio of 1:1:1 to dissolve and mix;

[0012] S3: After mixing, a semi-finished coating adhesive is obtained, and a dispersant is added and stirred for a period of not less than 1 hour;

[0013] S4: After stirring, a finished coating adhesive is obtained, and the finished coating adhesive is filtered and degassed to obtain a finished coating adhesive.

[0014] Preferably, the base monomer is epoxy resin, the curing agent is an organic dibasic acid, the solvent is water, the filler is quartz powder, the auxiliary agent is a plasticizer, and the flame retardant is an inorganic flame retardant. The quartz powder has strong water resistance and acid and alkali resistance, which can improve the water resistance and acid and alkali resistance of the coating and improve the corrosion resistance of the coating.

[0015] Preferably, the heating and stirring temperature in step S1 is controlled between 130° C. and 150° C. Controlling the mixing temperature can make the mixing between the raw materials more complete and strengthen the binding energy between the organic and inorganic substances.

[0016] Preferably, the addition of filler in step S2 should be divided into three times, with each addition being performed at an interval of 20 minutes. Adding filler in batches can effectively mix the filler with the solvent, effectively reducing the stirring time and improving the processing efficiency.

[0017] Preferably, the degassing time in step S3 is not less than 30 minutes, and the degassing method adopts the heating degassing method. High-temperature degassing uses the principle of temperature increase and viscosity decrease to make bubbles float to the liquid surface more easily and burst, and the degassing efficiency is higher.

[0018] (III) Beneficial effects

[0019] Compared with the prior art, the present invention provides a highly corrosion-resistant coating adhesive and a processing method thereof, which has the following beneficial effects:

[0020] The highly corrosion-resistant coating adhesive and its processing method can greatly improve the overall corrosion resistance of the coating adhesive by combining the heating of organic and inorganic substances. At the same time, by using water as a solvent, the overall corrosion resistance of the coating adhesive is improved without increasing toxicity, and the coating adhesive is more environmentally friendly as a whole. Since the coating adhesive manufactured by this preparation method has high corrosion resistance and excellent processing performance, it can be widely used in the anti-corrosion protection and decorative treatment of various metal, plastic, wood and other substrates, and has broad market prospects. DETAILED DESCRIPTION

[0021] The technical solutions in the embodiments of the present invention are described clearly and completely below. Obviously, the described embodiments are only part of the embodiments of the present invention, not all of them. Based on the embodiments of the present invention, all other embodiments obtained by ordinary technicians in this field without creative work are within the scope of protection of the present invention.

[0022] Example 1

[0023] A preferred embodiment of a highly corrosion-resistant coating adhesive and a processing method thereof provided by the present invention is as follows: A highly corrosion-resistant coating adhesive comprises the following preparation raw materials:

[0024] Base monomer - 100 parts, curing agent - 30 parts, solvent - 20 parts, filler - 50 parts, auxiliary agent - 10 parts, flame retardant - 5 parts.

[0025] In this embodiment, the steps for preparing the coating adhesive are as follows:

[0026] S1: Pour the base monomer, curing agent, solvent, additive and flame retardant into a semi-closed container for heating and stirring, and stop stirring after stirring for 3 hours;

[0027] S2: Mix the solution obtained by stirring with the filler, and add water in a ratio of 1:1:1 to dissolve and mix;

[0028] S3: After mixing, a semi-finished coating adhesive is obtained, and a dispersant is added and stirred for a period of not less than 1 hour;

[0029] S4: After stirring, a finished coating adhesive is obtained, and the finished coating adhesive is filtered and degassed to obtain a finished coating adhesive.

[0030] Example 2

[0031] Based on Example 1, a preferred embodiment of a highly corrosion-resistant coating adhesive and a processing method thereof provided by the present invention is as follows: the base monomer is epoxy resin, the curing agent is an organic dibasic acid, the solvent is water, the filler is quartz powder, the auxiliary agent is a plasticizer, and the flame retardant is an inorganic flame retardant.

[0032] In this embodiment, the heating and stirring temperature in step S1 is controlled between 130° C. and 150° C. Controlling the mixing temperature can make the mixing between the raw materials more complete and strengthen the binding energy between the organic and inorganic substances.

[0033] Furthermore, the addition of filler in step S2 should be divided into three times, with each addition being performed at an interval of 20 minutes. Adding filler in batches can effectively mix the filler with the solvent, effectively reducing the stirring time and improving the processing efficiency.

[0034] Furthermore, the degassing time in step S3 is not less than 30 minutes, and the degassing method adopts the heating degassing method. High-temperature degassing uses the principle of temperature increase and viscosity decrease to make bubbles float to the liquid surface more easily and burst, and the degassing efficiency is higher.

[0035] In summary,.

[0036] It should be noted that, in this article, relational terms such as first and second, etc. are only used to distinguish one entity or operation from another entity or operation, and do not necessarily require or imply any such actual relationship or order between these entities or operations. Moreover, the terms "include", "comprise" or any other variants thereof are intended to cover non-exclusive inclusion, so that a process, method, article or device including a series of elements includes not only those elements, but also other elements not explicitly listed, or also includes elements inherent to such process, method, article or device.

[0037] Although embodiments of the present invention have been shown and described, it will be appreciated by those skilled in the art that various changes, modifications, substitutions and variations may be made to the embodiments without departing from the principles and spirit of the present invention, and that the scope of the present invention is defined by the appended claims and their equivalents.

Claims

1. A highly corrosion-resistant coating adhesive, characterized in that: The preparation includes the following raw materials: Base monomer - 100 parts, curing agent - 30 parts, solvent - 20 parts, filler - 50 parts, auxiliary agent - 10 parts, flame retardant - 5 parts.

2. The method for processing a highly corrosion-resistant coating adhesive according to claim 1, characterized in that: The preparation steps of the coating glue are as follows: S1: Pour the base monomer, curing agent, solvent, additive and flame retardant into a semi-closed container for heating and stirring, and stop stirring after stirring for 3 hours; S2: Mix the solution obtained by stirring with the filler, and add water in a ratio of 1:1:1 to dissolve and mix; S3: After mixing, a semi-finished coating adhesive is obtained, and a dispersant is added and stirred for a period of not less than 1 hour; S4: After stirring, a finished coating adhesive is obtained, and the finished coating adhesive is filtered and degassed to obtain a finished coating adhesive.

3. The highly corrosion-resistant coating adhesive and the processing method thereof according to claim 1, characterized in that: The basic monomer is epoxy resin, the curing agent is organic dibasic acid, the solvent is water, the filler is quartz powder, the auxiliary agent is plasticizer, and the flame retardant is inorganic flame retardant.

4. The highly corrosion-resistant coating adhesive and the processing method thereof according to claim 2, characterized in that: The heating and stirring temperature in step S1 is controlled between 130°C and 150°C.

5. The highly corrosion-resistant coating adhesive and the processing method thereof according to claim 2, characterized in that: The filler addition in step S2 should be divided into three times, with each addition performed at an interval of 20 minutes.

6. The highly corrosion-resistant coating adhesive and the processing method thereof according to claim 2, characterized in that: The degassing time in step S3 is not less than 30 minutes, and the degassing method adopts the heating degassing method.

Citation Information

Patent Citations

  • Flame retardant coating adhesive for fabrics and preparation method thereof

    CN107216791A

  • Preparation method of finishing agent giving textile multiple functions and finishing method

    CN108978224A

  • Anti-fracture cotton yarn and preparation method thereof

    CN116791370A

  • Stiffening finishing agent for scratch-resistant textile fabric and preparation method of stiffening finishing agent

    CN117051593A