Process and device for treating wool feeling of surface layer of textile fabric
By optimizing the fabric processing steps and integrated gas and laser wool burning devices, the problems of uneven wool burning effects, high energy consumption and large equipment footprints of traditional textile fabrics are solved, and the production efficiency and fabric quality are improved, and the wool burning effect is achieved. uniformity and consistency.
Patent Information
- Application Number
- CN202411369746.X
- Authority / Receiving Office
- CN · China
- Patent Type
- Applications(China)
- Current Assignee / Owner
- Filing Date
- 2024-09-29
- Publication Date
- 2024-11-22
AI Technical Summary
The traditional textile fabric surface layer treatment process has problems such as uneven hair burning effect, high energy consumption, and large equipment footprint, which affects production efficiency and may cause damage to the fabric.
Optimized steps of fabric pretreatment, pretreatment, wool burning and post-treatment, including hot alkali desorption and softening, dryer drying, laying machine pre-pull, integrated gas and laser wool burning, water cooling, Wash and iron and organize alkaline water, combined with gas and laser integrated fabric wool burning device for treatment.
It significantly improves the efficiency of the wool burning process and the quality of the fabric, achieves the uniformity and consistency of the wool burning effect, reduces equipment cost and operation complexity, and ensures the softness, durability and aesthetics of the fabric.
Smart Images

Figure CN118996764A_ABST
Abstract
Description
Technical Field
[0001] The invention relates to the technical field of fabric singeing, in particular to a process and a device for treating the wooly feel of a textile fabric surface layer. Background Art
[0002] In the traditional process of treating the wooly feel of the surface of textile fabrics, the steps of pre-treatment, pre-treatment, singeing and post-treatment are usually included. These steps are aimed at improving the surface finish and quality of the fabric. However, the traditional method has certain shortcomings, such as uneven singeing effect, high energy consumption, and large equipment footprint. These problems not only affect production efficiency, but may also damage the fabric.
[0003] Although the existing patent solution has solved the problems of traditional wool-feeling technology for the surface layer of textile fabrics to a certain extent, it still has shortcomings such as high equipment cost and complex operation.
[0004] To this end, the present invention provides a process and device for treating the wooly feel of the surface layer of textile fabrics to solve the above technical problems. Summary of the invention
[0005] Purpose of the invention: To solve the problems of uneven singeing effect, high energy consumption, large equipment footprint, etc. in the prior art, which not only affect the production efficiency, but also may cause damage to the fabric.
[0006] To achieve the above object, the present invention provides the following technical solutions: A process for treating a wooly feel on a surface layer of a textile fabric comprises the following steps: S1: Fabric pre-treatment, including: cleaning, drying and finishing; S2: Fabric pretreatment, including: pre-stretching and brushing; S3: Singeing, including: gas singeing, laser singeing, the singeing process uses a gas and laser integrated fabric singeing device for processing; S4: Fabric post-processing, including cooling, washing, drying and finishing.
[0007] Furthermore, in step S1, the cleaning is performed by using hot alkali solution for desizing and softening; the drying process is performed by using a dryer at 120° C. for 15 minutes for complete drying; and the finishing process is performed by using a resin finishing method.
[0008] Furthermore, in step S2, the fabric is pre-stretched in both longitudinal and transverse directions by using a cloth drawing machine; the bristles are brushed by using a machine to drive a short-hair brush to comb up excess hair on the surface of the fabric along a linear direction to facilitate subsequent singeing.
[0009] Furthermore, in step S3, during the singeing process, both the gas and the laser perform singeing treatment on the front and back sides of the fabric, and the singeing rate is 2 m / s.
[0010] Furthermore, in step S4, during the cooling process, the fabric is washed with water at a rate of 0.5 m / s; during the cleaning process, it is washed with alkaline water at 60°C and then rinsed with warm water at 30°C with a pH value of 7; during the drying process, the temperature of the dryer is adjusted to 80°C for drying, and the drying time is controlled within 20 minutes; and after ironing at 120°C, the edges of the fabric can be neatly trimmed.
[0011] A gas and laser integrated fabric singeing device, used for the singeing treatment of the fabric in the aforementioned step S3, comprises a treatment device body, and the treatment device body also includes: Roller assembly, the roller assembly is used to transport the fabric to each singeing treatment station, the roller assembly is provided with at least four groups, and the positions are staggered up and down; A gas singeing component, the gas singeing component comprising: a burner, the burner is tangent to the roller component, and the burner is aligned with the direction of rotation of the roller component; an air inlet pipe, the air inlet pipe is connected to the burner and is used to provide combustible gas, and the temperature and flame size of the gas singeing component can be adjusted; A laser singeing component, comprising: a laser transmitter and a laser receiver, the laser transmitter and the laser receiver are installed at absolutely horizontal positions, the laser emission position is infinitely close to the roller component, and the temperature of the laser singeing component is adjustable.
[0012] Furthermore, the roller assembly comprises: a roller and a rotating shaft, and the rotation directions of the roller assemblies from top to bottom are opposite to each other.
[0013] Compared with the prior art, the present invention has the following beneficial effects: First, the present invention significantly improves the overall efficiency of the singeing process and the quality of fabrics by optimizing the fabric pre-treatment, pretreatment, singeing and post-treatment steps. In step S1, the use of hot alkali solution for desizing and softening can effectively remove the sizing on the fabric and improve the softness of the fabric; and the complete drying treatment of the dryer at 120°C for 15 minutes can ensure that the fabric reaches an ideal humidity state before singeing, avoiding poor singeing effects caused by uneven humidity. The application of the resin finishing method further enhances the durability and comfort of the fabric.
[0014] Secondly, the pre-stretching treatment in step S2 uses a cloth stretching machine to stretch the fabric in both the vertical and horizontal directions, so that the fabric reaches the optimal tension and stability before singeing. The brushing process uses a short-bristled brush driven by the machine to comb up excess hair on the surface of the fabric, providing a good pretreatment effect for the singeing process.
[0015] Furthermore, the present invention adopts a gas and laser integrated fabric singeing device in the singeing step S3, which realizes simultaneous singeing treatment of the front and back sides of the fabric, with a singeing rate of up to 2m / s, which not only greatly improves the production efficiency but also ensures the uniformity and consistency of the singeing effect.
[0016] In the fabric post-treatment step S4, the quality of the fabric is further improved by optimizing the water flow, washing, drying and finishing. For example, the water flow rate is 0.5m / s, which can quickly cool the fabric and avoid damage to the fabric; the washing process uses 60℃ alkaline water and 30℃ warm water with a pH value of 7 to effectively remove the residues produced by singeing and ensure the cleanliness of the fabric; the drying at 80℃ and the ironing at 120℃ ensure the flatness and beauty of the fabric after drying.
[0017] In addition, the gas and laser integrated fabric singeing device provided by the present invention has the advantages of compact structure, simple operation, low maintenance cost, etc. The setting of the roller assembly allows the fabric to run smoothly during the singeing process, and the temperature and flame size of the gas singeing assembly and the laser singeing assembly are adjustable, making the singeing effect more accurate and controllable. BRIEF DESCRIPTION OF THE DRAWINGS
[0018] Figure 1 It is a schematic diagram of the internal structure of the present invention; Figure 2 It is a top view of the structure cross-section of the present invention.
[0019] In the figure: 101, roller; 102, drum; 201, burner; 202, air inlet pipe; 301, laser transmitter; 302, laser receiver. DETAILED DESCRIPTION
[0020] In the following description, a large number of specific details are provided to provide a more thorough understanding of the present invention. However, it is apparent to those skilled in the art that the present invention can be implemented without one or more of these details. In other examples, in order to avoid confusion with the present invention, some technical features well known in the art are not described.
[0021] The applicant believes that the existing technology has problems such as uneven singeing effect, high energy consumption, and large equipment footprint, which not only affects production efficiency but also may cause damage to the fabric.
[0022] To this end, the applicant has designed a process for treating the wool feel of the surface layer of a textile fabric, comprising the following steps: S1: Fabric pre-treatment, including: cleaning, drying and finishing; S2: Fabric pretreatment, including: pre-stretching and brushing; S3: Singeing, including: gas singeing, laser singeing, the singeing process uses a gas and laser integrated fabric singeing device for processing; S4: Fabric post-processing, including cooling, washing, drying and finishing.
[0023] Among them, in step S1, the cleaning adopts hot alkaline solution to desizing and softening, which can effectively remove the sizing on the fabric and improve the softness of the fabric; the drying process adopts a dryer at 120°C for 15 minutes to completely dry the fabric, which can ensure that the fabric reaches an ideal humidity state before singeing and avoid poor singeing effect caused by uneven humidity; the finishing process adopts a resin finishing method to further enhance the durability and comfort of the fabric.
[0024] In step S2, the fabric is pre-stretched in both the longitudinal and transverse directions by using a cloth-pulling machine, so that the fabric reaches the best tension and stability before singeing; the bristles are brushed by using a machine to drive a short-hair brush to comb up the excess hair on the surface of the fabric in a linear direction to facilitate subsequent singeing.
[0025] In step S3, during the singeing process, both the gas and the laser singe the front and back sides of the fabric, and the singeing rate is 2 m / s, which not only greatly improves the production efficiency but also ensures the uniformity and consistency of the singeing effect.
[0026] In step S4, the fabric is washed with water at a rate of 0.5 m / s during the cooling process; the fabric is washed with alkaline water at 60°C and then rinsed with warm water at 30°C with a pH value of 7 during the cleaning process; the temperature of the dryer is adjusted to 80°C for drying during the drying process, and the drying time is controlled within 20 minutes; the fabric is ironed at 120°C for finishing, and the edges of the fabric are trimmed neatly.
[0027] like Figure 1-2 The gas and laser integrated fabric singeing device shown is used for the fabric singeing treatment in step S3, and includes a treatment device body, and the treatment device body also includes: Roller 101 assembly, roller 101 assembly is used to transport fabrics to each singeing treatment station, and at least four groups of roller 101 assemblies are arranged, and the positions are staggered up and down; The gas singeing component includes: a burner 201, the burner 201 is tangent to the roller 101 component, and the burner 201 is aligned with the direction of rotation of the roller 101 component; an air inlet pipe 202, the air inlet pipe 202 is connected to the burner 201, and is used to provide combustible gas. The temperature and flame size of the gas singeing component can be adjusted; The laser singeing component includes: a laser transmitter 301 and a laser receiver 302. The laser transmitter 301 and the laser receiver 302 are installed at absolutely horizontal positions. The position where the laser is emitted is infinitely close to the roller 101 component. The temperature of the laser singeing component is adjustable.
[0028] The roller 101 assembly includes: a roller 102 and a rotating shaft, and the rotation directions of the roller 102 assemblies from top to bottom are opposite to each other.
[0029] Principle of use: After the fabric pretreatment is completed, it is laid flat on the roller 101 assembly in the main body of the processing device, and the roller 101 assembly is opened to make the fabric move at a uniform speed in the main body of the processing device. The gas singeing assembly is respectively arranged on the two roller 101 assemblies arranged vertically and staggered at the lower end, and the installation position is tangent to the roller 101 assembly. The laser singeing assembly is arranged on the two roller 101 assemblies arranged vertically and staggered at the upper end, and the installation position is tangent to the roller 101 assembly. The rotation direction of the roller 101 assembly is from top to bottom in the opposite direction. The laser transmitter 301 and the laser receiver 302 used in this application adopt the transmitter and receiver commonly used in the laser engraving device for fabrics in the prior art. The gas singeing assembly is a prior art, so this application will not be repeated in detail.
[0030] It will be apparent to those skilled in the art that the invention is not limited to the details of the exemplary embodiments described above and that the invention can be implemented in other specific forms without departing from the spirit or essential features of the invention. Therefore, the embodiments should be considered exemplary and non-limiting in all respects, and the scope of the invention is defined by the appended claims rather than the foregoing description, and it is intended that all variations falling within the meaning and scope of the equivalent elements of the claims be included in the invention. Any reference numeral in a claim should not be considered as limiting the claim to which it relates.
Claims
1. A process for treating the wooly feel of the surface layer of textile fabrics. It is characterized in that The steps include: S1: Fabric pre-treatment, including: cleaning, drying and finishing; S2: Fabric pretreatment, including: pre-stretching and brushing; S3: Singeing, including: gas singeing, laser singeing, the singeing process uses a gas and laser integrated fabric singeing device for processing; S4: Fabric post-processing, including cooling, washing, drying and finishing.
2. A process for treating the wooly feel of the surface layer of a textile fabric according to claim 1, It is characterized in that In step S1, hot alkali solution is used for desizing and softening during cleaning; a dryer is used for complete drying at 120° C. for 15 minutes during the drying process; and a resin finishing method is used for the finishing process.
3. A process for treating the wooly feel of the surface layer of a textile fabric according to claim 1, It is characterized in that In step S2, the fabric is pre-stretched by using a cloth drawing machine to stretch the fabric in both the longitudinal and transverse directions; the bristles are brushed by using a machine to drive a short-hair brush to comb up the excess hair on the surface of the fabric along a linear direction to facilitate subsequent singeing.
4. A process for treating the wooly feel of the surface layer of a textile fabric according to claim 1, It is characterized in that In step S3, during the singeing process, both the gas and the laser perform singeing treatment on the front and back sides of the fabric, and the singeing rate is 2 m / s.
5. The process for treating the surface layer of a textile fabric to give it a wooly feel according to claim 1, It is characterized in that In step S4, the fabric is washed with water at a rate of 0.5 m / s during the cooling process; the fabric is washed with alkaline water at 60°C and then rinsed with warm water at 30°C with a pH value of 7 during the cleaning process; the temperature of the dryer is adjusted to 80°C for drying during the drying process, and the drying time is controlled within 20 minutes; the fabric is ironed at 120°C for finishing, and the edges of the fabric are trimmed neatly.
6. A gas and laser integrated fabric singeing device, used for the fabric singeing treatment in step S3 of claim 1, It is characterized in that The processing device comprises a main body, wherein the main body of the processing device further comprises: Roller assembly, the roller assembly is used to transport the fabric to each singeing treatment station, the roller assembly is provided with at least four groups, and the positions are staggered up and down; A gas singeing component, the gas singeing component comprising: a burner, the burner is tangent to the roller component, and the burner is aligned with the direction of rotation of the roller component; an air inlet pipe, the air inlet pipe is connected to the burner and is used to provide combustible gas, and the temperature and flame size of the gas singeing component can be adjusted; A laser singeing component, comprising: a laser transmitter and a laser receiver, the laser transmitter and the laser receiver are installed at absolutely horizontal positions, the laser emission position is infinitely close to the roller component, and the temperature of the laser singeing component is adjustable.
7. A gas and laser integrated fabric singeing device according to claim 6, It is characterized in that The roller assembly comprises: a roller and a rotating shaft, and the rotating directions of the roller assemblies from top to bottom are opposite to each other.