Culvert roadbed filling method
Through the filling test and layered filling method of high-fill culvert roadbeds, the problem of unreasonable calculation of soil pressure in culvert construction in mountainous expressways is solved, and the efficient use of filler resources is achieved to ensure construction safety and economicality.
Patent Information
- Application Number
- CN202411128516.4
- Authority / Receiving Office
- CN · China
- Patent Type
- Applications(China)
- Current Assignee / Owner
- Filing Date
- 2024-08-16
- Publication Date
- 2024-11-22
AI Technical Summary
In mountainous expressway projects, the construction of culverts in high-fill roadbeds has the problem of unreasonable calculation of soil pressure, which leads to an increase in project cost and construction difficulty, and the consumption of filling resources is large, affecting the environment.
By conducting filler tests on high-fill culvert roadbeds, construction parameters and data are obtained, filling materials are selected reasonably, and layered filling and monitoring methods are adopted to ensure the stability of the fill quality and structure, reduce the abandonment of the square, and improve the soil arch effect.
Effectively utilize soil and stone mixed materials to reduce environmental damage, ensure the safety of high-fill culvert roadbeds, reduce construction and maintenance costs, and improve project efficiency.
Smart Images

Figure CN118996935A_ABST
Abstract
Description
Technical Field
[0001] The invention relates to the field of roadbed filling construction, in particular to a culvert roadbed filling method. Background Art
[0002] Culverts are the infrastructure of transportation projects. They account for a large proportion of highway projects and are an important part of highway projects. They have important engineering economic value. The main purpose of culverts is to serve as transverse passages for highways, railways, rainwater, sewage, and pipelines. According to statistics, there are about 4 to 6 culverts per kilometer of highway in mountainous and hilly areas; in mountainous highways, the number of culverts accounts for about 60% to 70% of the total number of bridges and culverts. Culverts can be either rigid or flexible; rigid culverts are made of prefabricated reinforced concrete or cast on site, while flexible culverts can be made of general steel, cast iron, aluminum and corrugated steel. Usually, culvert projects in transportation projects only need to be selected according to standard drawings without special design.
[0003] With the increasing number of highway construction projects in the mountainous areas of western my country, the high-fill roadbed derived from the construction of high-grade highways in mountainous and hilly areas can reach tens of meters high, and the roadbed filling materials are mostly soil-rock mixed filling materials. The soil-rock mixed roadbed of mountain highways has the characteristics of high economic cost, tight construction period, large filling resource consumption, large filling height, and great social impact. During the construction process, it is inevitable to bury culverts across the highway at the bottom of the high-fill section for lateral drainage, vehicle or pedestrian passage. In addition, the high-fill embankment will cause the geometric length and load of the culvert to be very large. If the calculation of the soil pressure on the culvert is unreasonable, it will bring many problems to the culvert engineering design, engineering cost and construction application.
[0004] Therefore, conducting systematic research on the construction methods of culverts in high-fill earth-rock mixture embankments in mountainous areas can not only provide a deep understanding of the stress mechanism of high-fill culverts, improve the calculation theory of the stress on culvert structures, and provide a reference for culvert design under different foundation conditions, different filling materials and different boundary conditions, but also provide a prerequisite for the prevention and control of culvert diseases and flood control and discharge of culverts in the construction of transportation, water conservancy, energy and other projects. It has important theoretical, practical and scientific research significance. Summary of the invention
[0005] The objective of the present invention is achieved through the following technical solutions:
[0006] A culvert roadbed filling method comprises the following steps:
[0007] S1. Conduct filler test for high fill culvert roadbed, obtain parameters and data for culvert roadbed construction based on filler test, and reasonably select filler for filling construction based on these parameters and data;
[0008] S2. According to the design requirements, construct the main body of the culvert, maintain it and after it has passed the acceptance inspection, fill the area around the culvert to the required range according to the design requirements;
[0009] S3, carry out the construction of high fill culvert roadbed above the culvert, and use the construction parameters, data and selected fillers obtained from the S1 filler test to guide the basis for the high fill culvert roadbed;
[0010] S4. Monitor the high fill culvert roadbed under construction.
[0011] Preferably, the filler test in S1 includes: compaction test; filler mechanical property test; indoor model test.
[0012] Preferably, the compaction test step comprises:
[0013] S11. Selection of filler: Select soil-rock mixture that can meet the requirements as filler for culvert roadbed;
[0014] S12. Selection of particle gradation: According to the requirements of roadbed filling, the selected fillers are scaled down to obtain the data and parameters before and after scaling, so as to select the appropriate filler particle size;
[0015] S13. Filler compaction test: Conduct a standard compaction test on the selected filler to obtain the parameters and data of the compaction test; after the compaction test, screen the filler and analyze the change pattern of the filler.
[0016] Preferably, the step of testing the mechanical properties of the filler comprises: performing a shear test on the filler in the filler, and performing a shear test on the selected filler by using a shear instrument to determine the mechanical parameters of the filler.
[0017] Preferably, the indoor model test includes: using similarity theory to ensure that the model test is similar to the culvert prototype during construction and filling in terms of geometry and boundary conditions, and meets the requirements of physical equations.
[0018] Preferably, the construction requirements for filling the area around the culvert in S2 are:
[0019] S21. Fill the culvert with fillers on both sides at the same time, in layers, and the height difference of the fillers on both sides shall not exceed 300mm;
[0020] S22. When the filling materials on both sides are 1m away from the culvert vault vertically, a pull plate is arranged at each layer and every horizontal distance of 0.8-1m for each layer of filling materials on both sides. One end of the pull plate is connected to the side wall of the culvert, and the other end is at least 1m away from the side wall of the culvert and is rolled and buried in the filling materials of the side wall.
[0021] S23. After the filling materials on both sides are flush with the culvert vault, EPS boards are laid on the culvert vault, and stretchable geogrids are laid on the top of the filling materials on both sides of the culvert. The geogrids are laid on one side close to the EPS board and under the EPS board, and the overlap length of the two is 150 to 200 mm.
[0022] Preferably, the S3 culvert roadbed construction steps are as follows:
[0023] S31. Lay the first layer of culvert roadbed filler mixture selected through filler test on the laid EPS board to 0.5m above the culvert arch, and use small machinery with manual assistance for rolling. And on both sides of the layer of mixed filler, 2m horizontally away from the culvert arch foot, construct a drainage blind ditch along the longitudinal direction of the culvert;
[0024] S32, when the second layer of culvert embankment mixed filler is laid out on the first layer of mixed filler along the longitudinal direction of the culvert to the center line of the culvert, and the center line is separated by a partition, and the second layer of culvert embankment mixed filler is laid to the designed height, and the second layer of culvert embankment mixed filler is compacted;
[0025] S33. Before laying the embankment mixture on the second layer of culvert embankment, take out the partition in S32, pour medium-coarse sand into the gap after the partition is taken out, and compact the filling. Lay a layer of geogrid above the gap after the partition is taken out of the second layer of embankment mixture, and then lay and fill the upper culvert roadbed on the second layer of embankment mixture to the designed elevation.
[0026] Preferably, the monitoring of the high fill culvert roadbed in S4 includes monitoring deformation of the high fill culvert roadbed and monitoring uneven settlement of the high fill culvert roadbed.
[0027] The beneficial effects of the present invention are as follows: the purpose of the present invention is to provide a culvert roadbed filling method, which uses test data and parameters as a basis and reference to guide the roadbed (embankment) construction of a high-fill culvert. Through this construction method, the excavated soil-rock mixture material can be fully utilized to reduce the damage to the environment caused by abandoned soil; this construction method takes into account and improves the soil arch effect of the vertical soil pressure and lateral soil pressure on the roadbed at the top of the culvert, thereby ensuring the safety of the high-fill culvert roadbed and saving the cost of reinforcing and repairing the culvert and the culvert roadbed. BRIEF DESCRIPTION OF THE DRAWINGS
[0028] Figure 1 The present invention is a schematic diagram of the construction process of a culvert roadbed filling method. DETAILED DESCRIPTION
[0029] In order to make the purpose, technical solutions and advantages of the present invention more clearly understood, the present invention is further described in detail below in conjunction with the accompanying drawings and embodiments.
[0030] like Figure 1 As shown, a method for filling culvert roadbed, before construction and filling, first conducts a filling material test of the high fill culvert roadbed, and obtains the parameters and data of the culvert roadbed construction based on the filling material test. Based on these parameters and data, the filling material for filling construction is reasonably selected to guide the construction of the high fill culvert roadbed. These filling material tests include: compaction test, filling material mechanical property test, indoor model test, etc.; these filling material tests also determine the quality requirements of the filling material for the later filling construction; therefore, these filling material test parameters and data are crucial. The following is an example of the steps of these filling material tests.
[0031] 1. Compaction test
[0032] (1) Selection of filler: Select soil-rock mixture that can meet the requirements for culvert roadbed filler;
[0033] The test materials are road embankment fillers from highway and culvert projects, which mainly include shale and shale soil, and some also contain sandstone and limestone. In the later indoor model test, a mixture of shale, sandstone and limestone is used as the "stone" (particle size greater than 5mm) in the soil-rock mixture road embankment-culvert filler, and shale soil is selected as the "soil" (particle size less than 5mm) in the filler, in preparation for analyzing the soil arch effect at the top of the culvert and the vertical settlement change law;
[0034] (2) Selection of filler particle size distribution: According to the requirements of roadbed filling, the selected fillers are scaled down to obtain the data and parameters before and after scaling, so as to select the appropriate filler particle size;
[0035] The maximum particle size of the filler used for highway roadbed filling is between 400 and 500 mm. Considering the limitation of the maximum particle size of the filler by the test equipment, the filler on site was scaled down. In this embodiment, the mixing method is selected to scale down the filler gradation. The specific operation steps of the mixing method to scale down the filler gradation are as follows: first, the filler is proportionally scaled to 1 / 4 times of the original size according to the geometric similarity method, and then, in order to ensure that the content of the particle size less than 5 mm remains unchanged, the large-particle "stone" larger than 40 mm is proportionally replaced with the small-particle "stone" of 5 to 40 mm, and the soil-rock mixture filler gradation curve before and after the scale-down can be obtained. In addition, according to the soil-rock mixture filler gradation curve, five kinds of test fillers with stone content (10%, 30%, 50%, 70%, 90%), the gradation curves of fillers with different stone contents, and the corresponding soil-rock mixture filler particle gradation table with different stone contents (Table 1) are designed:
[0036] Table 1 Representative grading table of soil-rock mixture fillers with different stone contents
[0037]
[0038] Note: 1) The actual roadbed filler (stone content of 33.1%) test model parameters are used to replace the filler model parameters with a stone content of 30%;
[0039] 2) P5 means that particles with a diameter ≥ 5 mm are defined as stone.
[0040] According to the test data, the conclusion is: the particle grading curve of the original soil material is close to the particle grading curve with a stone content of 30%, and each level of distribution curve meets the requirements of good particle grading. Therefore, the original soil-stone mixture filler is used instead of the filler with a stone content of 30% for subsequent tests.
[0041] After scaling down the soil-rock mixture fillers with various stone contents, the designed unevenness coefficient of each stone content filler is guaranteed to be greater than 5, and the curvature coefficient is between 1 and 3. The specific particle size characteristic values are shown in Table 2.
[0042] Table 2 Grain size characteristics of soil-rock mixtures with different stone contents
[0043]
[0044] According to the Highway Geotechnical Test Code (JTG E40-2007), the on-site fill was screened to obtain fills with different particle sizes. The standard vibrating screen machine used in the test was used for screening samples.
[0045] Five kinds of stone content fillers were prepared according to Table 1. Six groups of tests were conducted for each stone content filler, with each group weighing 3 kg, a total of 18 kg, and each stone content filler was weighed.
[0046] In order to prevent particles of different sizes from sticking together due to excessive moisture content, which in turn affects the particle grading, the selected on-site fillers are heated in a drying oven with the temperature controlled at 100°C ~ 105°C for 12 hours. After drying, each group of fillers is loaded and the initial moisture content of the soil-rock mixture fillers with each stone content is calculated. The moisture content results obtained from the three groups of tests are averaged to determine the initial moisture content of the fillers with each stone content.
[0047] (3) Filler compaction test: Conduct standard compaction test on selected fillers to obtain parameters and data of compaction test; after compaction test, screen the fillers and analyze the change law of fillers;
[0048] The standard heavy compaction test II-1 should be carried out on the soil-rock mixture filler. Therefore, a multifunctional electric compactor was used to carry out compaction tests on five kinds of soil-rock mixture fillers with different stone contents. The hammer weight of the electric compactor was 2.5-4.5 kg, the diameter of the test mold was 100-152 mm, the drop height was 300-450 mm, and the number of hammer strikes was 30-32 times / minute. The compaction tests were carried out on the original soil and the fillers with stone contents (10%, 30%, 50%, 70%, 90%) of the designed gradation, and the compaction test results are shown in Table 3.
[0049] Table 2 Maximum dry bulk density and optimum moisture content of different stone contents
[0050] Stone content (%) <![CDATA[Maximum dry unit weight (kg / m 3 )]]> Optimum moisture content (%) 10 2100 7.8 30 2146 7.4 50 2190 7.2 70 2230 6.5 90 2067 6
[0051] From the compaction curves of different stone contents of soil-rock mixture fillers in Table 3, it can be concluded that:
[0052] (1) The maximum dry density shows different trends with the increase of stone content. When the stone content is 10%, 30%, 50% and 70%, the maximum dry density increases with the increase of stone content; and when the stone content is 90%, the maximum dry density is the smallest. The main reasons are: ① When the stone content increases from 10% to 30%, the proportion of stone in the soil-rock mixture increases. Since the density of stone is greater than that of soil, the greater the stone content of the filler, the greater the corresponding maximum dry density. At this time, the filler belongs to the suspended-dense structure; ② When the stone content increases from 30% to 70%, the proportion of stone in the soil-rock mixture is greater, and the maximum dry density of the filler also increases. At this time, the filler belongs to the skeleton-dense structure; ③ When the stone content is greater than 90%, the proportion of stone in the soil-rock mixture is greater, but because the proportion of soil is less, the soil fails to fill the gaps between the skeleton structure formed by the stone, resulting in a larger porosity of the filler and a smaller maximum dry density. At this time, the filler belongs to the skeleton-void structure.
[0053] (2) As the stone content increases, the optimum moisture content of the soil-rock mixture with each stone content decreases. It should be noted that due to the long cycle of the indoor model test, the optimum moisture content of the soil-rock mixture with each stone content needs to be increased by 1% to 2% during the test.
[0054] After the compaction test, the soil-rock mixture fillers with different stone contents were screened, and the variation law and influencing factors of the crushing rate of the soil-rock mixture were analyzed. The main reasons for the particle crushing of the soil-rock mixture filler are: the particles of different particle sizes in the filler are often in point contact, which causes the "stones" in the skeleton of the soil-rock mixture filler to squeeze each other during the compaction process. When the squeezing force is greater than the pressure it can resist, the particles will break; when the large-sized particles are split into multiple small particles with uneven particle sizes, coupled with the defects of the particle structure itself, the particles themselves will fall off to form smaller particles, causing the large particles to gradually become smaller, and then break and crush; when there is mechanical bite between the particles, shear force will be generated on the surface of each particle, resulting in the large particles to be crushed by particle grinding. The particle crushing is roughly rupture, crushing, and grinding.
[0055] In order to reflect the change value of each particle size content before and after the filler is compacted, and to characterize the degree of crushing of particles of each particle size, B g The calculation method is as follows:
[0056] B g =∑|W ki -W kf |
[0057] Where: B g W is the sum of the positive values of the differences in mass fractions of each particle size component before and after the test, which is used as a measure of the degree of particle breakage; ki is the mass fraction corresponding to a certain particle size before compaction test; W kf is the mass fraction corresponding to the same particle size after compaction. The particle breakage rate of fillers with different stone contents in Table 4 was statistically analyzed, and its relationship with water content was established.
[0058] Table 4 Mechanical indexes of soil-rock mixture materials with different stone contents
[0059]
[0060] Note: 1) Considering the uncertainty of the change of moisture content of the roadbed on site, direct shear test of coarse-grained soil at different moisture contents was not carried out;
[0061] 2) Due to the size limitation of the direct shear test of coarse-grained soil and the indoor filler-culvert model test, the shear parameters of the original particle size of the soil-rock mixture were not analyzed, and therefore the influence of replacing large-size aggregates larger than 40 mm on the shear parameters was not considered.
[0062] When the water content is the same, the crushing rate of the soil-rock mixture filler with a high stone content is greater, and when the stone content is greater than 50%, the filler crushing rate increases significantly. According to the corresponding values of the filler crushing rate and water content relationship curve, it is found that the stone content and water content are two important factors affecting the particle crushing rate.
[0063] Further analysis of the influence of stone content and water content on the crushing rate of soil-rock mixture filler
[0064] (1) When considering the influence of moisture content, the filler moisture content of 2.18% is taken as the baseline value, and the moisture contents of 4.18%, 6.18%, 8.18%, and 10.18% are taken as comparison values. When the stone content is 10%, the maximum increase in the crushing rate when the moisture content increases from 2.18% to 10.18% is 44.90%. Similarly, when the stone content is 30%, 50%, 70%, and 90%, the maximum increase in the crushing rate is 154.60%, 113%, 54.87%, and 34.66%, respectively.
[0065] (2) When discussing the influence of stone content, the filler stone content is 10%, and the moisture content is 2.18%, 4.18%, 6.18%, 8.18%, and 10.18% as the benchmark values. When the stone content is 30%, 50%, 70%, and 90% and the moisture content is 2.18%, the increase in crushing rate is 234.7%, 810%, 1629%, and 2756%, with the maximum value being 2756%. Similarly, when the stone content is 30%, 50%, 70%, and 90% and the moisture content is 4.18%, 6.18%, 8.18%, and 10.18%, the maximum increase in crushing rate is 2792%, 2946%, 2580%, and 2554%.
[0066] Analysis of the above data shows that the effect of stone content on crushing rate is more significant than that of water content.
[0067] 2. Test of mechanical properties of packing
[0068] The mechanical parameters of fillers with different stone contents were determined by using a coarse-grained soil direct shear compression dual-purpose instrument. During the test, four dial gauges with a range of 10 mm were placed on the top of the pressure transmission plate, and a horizontal dial gauge with a range of 50 mm was installed on the left and right sides of the lower shear box. The vertical and horizontal displacement results of the specimens were taken as the average of the dial gauge results. A total of 33 groups of coarse-grained soil were conducted. When the stone content was 10%, 50%, 70%, and 90%, 5 groups of coarse-grained soil direct shear tests with different normal stresses were conducted for each stone content; 13 groups were conducted when the stone content was 30%, of which 5 groups were coarse-grained soil direct shear tests with different normal stresses, and the other 8 groups were coarse-grained soil direct shear tests to determine the influence of compaction on shear strength parameters (internal friction angle and cohesion).
[0069] During the shear process, there is mutual extrusion, interlocking, embedding and friction between the clay particles in the filler and the stones inside the filler, and there is a "stone-around effect"; the shear deformation caused by the shear strain of the soil-rock mixture filler is small at the beginning of the shear, and then gradually produces plastic deformation, and finally shear failure with the shear surface penetrating occurs; at the beginning of the shear, microcracks first appear near the stone blocks. As the shear test progresses, the microcracks gradually expand into the "soil", and finally form a penetrating shear zone at the interface of the upper and lower soil pressure shear boxes.
[0070] According to the direct shear test results of coarse-grained soil with various stone content fillers, the relationship curve between shear strength S and vertical pressure P is drawn, and the following can be obtained through analysis:
[0071] The soil-rock mixture fillers with different stone contents all show the following rules: in the initial stage, the greater the normal stress applied to the upper shear box, the greater the elastic ratio of the shear stress τ and horizontal displacement △S relationship curve; the greater the normal stress applied to the upper shear box, the greater the maximum value of the shear stress corresponding to the shear stress τ and horizontal displacement △S relationship curve; when the shear stress reaches the maximum value, there is no obvious shear stress softening phenomenon in the shear stress τ and horizontal displacement △S relationship curve.
[0072] The shear stress τ of soil-rock mixture fillers with various stone contents shows a certain degree of step-like increase with the increase of horizontal displacement △S. Specifically, the greater the normal stress applied to the upper shear box, the more obvious the step-like phenomenon caused by the rising curve (increase in shear stress τ) during the increase of horizontal displacement △S.
[0073] According to the relationship curve between shear strength S and vertical pressure P and the calculation internal friction angle specified in the Highway Geotechnical Test Code The stress circle of the cohesion c value and the Mohr envelope of the shear strength were related to the fitting curve of the relationship between the shear strength and the vertical pressure of each stone content. Based on the fitting curve of the relationship between the shear strength and the vertical pressure of each stone content, the internal friction angle of the soil-rock mixture filler with different stone contents was obtained by reverse calculation. The specific values of cohesion c are shown in Table 5. As can be seen from Table 5, the shear strength of the fillers of soil-rock mixtures with different stone contents mainly comes from the internal friction angle and cohesion, which shows that: with the increase of stone content, the cohesion of the filler decreases and the internal friction angle increases.
[0074] Table 5 Mechanical indexes of soil-rock mixture materials with different stone contents
[0075]
[0076] Note: 1) Considering the uncertainty of the change of moisture content of the roadbed on site, direct shear test of coarse-grained soil at different moisture contents was not carried out;
[0077] 2) Due to the size limitation of the direct shear test of coarse-grained soil and the indoor filler-culvert model test, the shear parameters of the original particle size of the soil-rock mixture were not analyzed, and therefore the influence of replacing large-size aggregates larger than 40 mm on the shear parameters was not considered.
[0078] Through the direct shear test of coarse-grained soil, the relationship curve between the filler compaction degree and the filler internal friction angle and cohesion when the filler stone content is 30% is obtained.
[0079] Finally, we can conclude that:
[0080] When the filler stone content is 30% and the filler moisture content is the optimal moisture content of 7.4%, with the increase of compaction degree, the filler internal friction angle increases nonlinearly. According to the exponential form equation, the change value of the filler internal friction angle under different compaction degrees is fitted, and the correlation coefficient of the fitting equation is 0.9927.
[0081] With the increase of compaction degree, the cohesion of the filler increases roughly linearly. The change of cohesion of the filler under different compaction degrees is fitted according to the exponential equation, and the correlation coefficient of the fitting equation is 0.9994.
[0082] These test parameters provide parameter basis for the later high culvert roadbed filling construction, especially the influence of culvert side fill compaction on the vertical friction between culvert and side fill.
[0083] 3. Indoor model test
[0084] According to similarity theory, in order to ensure that the model test can more accurately reflect the test results of the prototype, it is necessary to ensure that the model and the prototype are similar in geometry and boundary conditions and meet the requirements of the physical equations.
[0085] (1) Geometric similarity
[0086] To make the model similar to the prototype, the geometric dimensions of the corresponding parts of the model and the prototype must be proportional and the geometric shapes must be similar. The geometric dimension ratio of the model is the geometric similarity constant C. L ,Right now
[0087]
[0088] In the formula, l p —Geometric dimensions of the prototype (length, width, height, thickness, etc.); m —Geometric dimensions corresponding to the model, subscript p and subscript m represent the prototype and model respectively. In order for the model to meet the material weight similarity between the model and the prototype, the material weight similarity constant C must be met. γ The requirement is
[0089]
[0090] In the formula, γ p , γ m Represent the bulk density of model and prototype fillers respectively.
[0091] (2) Physical equations
[0092] In order for the model to meet stress similarity with the prototype, the stress similarity constant C must be satisfied. σ The requirement is
[0093]
[0094] From formula (2.4), we can get the physical equation, namely:
[0095]
[0096] All fillings in model and prototype tests are on-site fillings.
[0097] According to similarity theory, the stress value σ at a point on the prototype p for
[0098] σ p =σ m C L (3.5)
[0099] The deformation of the prototype can be directly converted from the model deformation according to the similarity theory, that is,
[0100] u p =u m C L (3.6)
[0101] At this time, convert equation (3.3) and assume that the strain similarity constant C ε Similarity constant C to Poisson's ratio v If both are 1, we can get the vertical earth pressure coefficient of the culvert top during the indoor model test, which is the earth pressure coefficient of the culvert top during the prototype test, that is,
[0102]
[0103] In the formula, F ep With F em They represent the earth pressure coefficient at the top of the culvert for the prototype and model respectively (the ratio of the vertical earth pressure at the top of the culvert to the theoretical deadweight earth pressure).
[0104] (3) Similar boundary conditions
[0105] Ensure that the model and the prototype are similar in terms of support conditions, constraints, and force conditions on the boundary, that is, the various conditions of contact with the outside world are similar. For the high embankment culvert test model, it is recommended to use the geometric similarity constant CL =20~50, so the geometric similarity constant C used in this indoor model test is determined L is 20.
[0106] 2.3.2 Model box design
[0107] The model test was carried out in a self-made model box with a length × width × height = 1.4m × 1.0m × 1.5m. The model box was made of welded rectangular steel and reinforced on the outside with longitudinal and transverse rectangular steels. The strength and rigidity of the model box could meet the test requirements.
[0108] The maximum fill height of the indoor test model is 0.9m, and the simulated actual fill height is 18m. During the test, the fill load is applied by paving fill on both sides of the culvert and above the culvert. The weight of each layer of fill is calculated according to the volume method, where the compaction degree of the test fill is first determined by formula (3.8), and then the actual weight of each layer of fill is calculated by formula (3.9). The model test did not consider the force response of the culvert when vibration load and incremental cyclic load were applied to the fill surface.
[0109] ρ ds =ρ x ·ρ dmax (3.8)
[0110] G=ρ ds ·L·B·h d (3.9)
[0111] Where: x is the compaction degree; ρ dmax is the maximum dry density of the filler (g / cm 3 );ρ ds is the dry density of the filler during the test (g / cm 3 ); L is the net length of the inner side of the two wooden templates of the model box; B is the net width of the model box; h d is the height of each layer of packing; G is the weight of each layer of packing.
[0112] Considering the stress conditions of five kinds of soil-rock mixture fillers-culverts with different rock contents, five indoor model tests were completed. The specific conditions of the model tests are shown in Table 2.7. Wooden templates were added to the left and right sides of the model box and the rear side of the box, and a transparent tempered glass with a total thickness of 2.5 cm was placed vertically on the front side; in order to facilitate deformation observation, a square grid of 10 cm × 10 cm was drawn on the glass surface; the roadbed filler was filled in a layer every 10 cm in height (equivalent to the actual 2 m), and spread evenly. After the filler was filled, the data of the micro-earth pressure box was observed for 30 to 45 minutes. When the data of the earth pressure box did not change for 10 minutes or the change value was negligible, the earth pressure data on each micro pressure box was read and the displacement value of the filler point was recorded. Then the next level of filler was filled, and so on until 9 layers of filler were filled. One indoor model test lasted about 24 hours from filling to taking the filler out of the model box. Micro-earth pressure box layout.
[0113] Table 3 Indoor soil-rock mixture filler-culvert model test conditions
[0114]
[0115]
[0116] Channel steel is laid at the bottom of the model box, 5 cm thick coarse sand is filled on the channel steel, and a high-rigidity wooden formwork is laid on the coarse sand to simulate a rigid foundation. The culvert is arranged on the wooden formwork in the model box and placed in the center of the box. The distance between the edges of the two sides of the culvert and the left and right inner formworks is 52.5 cm. The culvert is placed and filled with soil on the side of the culvert. In order to more accurately monitor the actual stress characteristics of the culvert structure, the indoor test uses a reinforced concrete cover culvert cast according to the scaled size.
[0117] The scaled model is explained as follows:
[0118] The actual culvert structure is calculated according to the geometric similarity constant C L The culvert model was scaled down to 20, and the length of the scaled culvert model was 90cm. The culvert model was made by casting in situ.
[0119] During the casting of the scaled culvert, longitudinal stress-bearing steel bars and distribution bars are arranged at the bottom of the cover culvert body and inside the side wall of the culvert to ensure that the side wall and the culvert bottom are stressed together, and the culvert model is maintained at room temperature for 90 days; the length of the longitudinal reinforcement of the side wall and the bottom plate is 80cm, ensuring that the thickness of the longitudinal reinforcement protection layer is 5cm, and the diameters of the longitudinal stress-bearing steel bars on the side wall and the bottom plate are 5.5cm and 8.25cm respectively; the transverse reinforcement is connected to the longitudinal reinforcement on the side wall and the bottom plate; the longitudinal and transverse reinforcements are both round steel bars with a diameter of 6mm and a spacing of 20cm. Specific cross-section and reinforcement arrangement of the scaled culvert model. Since the designed cover plate thickness of the cover culvert top is 1.6cm, it is difficult to cast concrete after tying the reinforcement. Therefore, no reinforcement is arranged in the top plate of the cover culvert, and only plain concrete is cast in place. In addition, epoxy resin concrete is poured between the concrete cover plate and the side wall to simulate the hinged connection between the cover plate and the side wall. The specific culvert production process is similar to the complete cover culvert model.
[0120] In summary, through the above-mentioned filling material test of high fill culvert roadbed, the parameters and data of culvert roadbed construction are obtained. Based on these parameters and data, the filling material for filling construction is reasonably selected to guide the construction of high fill culvert roadbed.
[0121] Furthermore, according to the design requirements, the main body of the culvert is constructed, maintained and accepted, and then, according to the design requirements, the area around the culvert is filled with soil to the required range of the design.
[0122] During the construction of the culvert body and surrounding fill:
[0123] (1) The two sides of the culvert are filled with fillers at the same time, layered and compacted, and the height difference of the fillers on both sides cannot exceed 300mm. Depending on the type of culvert construction and the mixed fillers selected based on the filler test, the layered compaction thickness of the fillers on both sides will also be different.
[0124] (2) During the construction of high fill culvert roadbed, when the filling materials on both sides are 1m away from the culvert arch vertically, a pull plate is arranged at each layer and every horizontal distance of 0.8 to 1m for each layer of filling materials on both sides. One end of the pull plate is connected to the side wall of the culvert, and the other end is at least 1m away from the side wall of the culvert and is rolled and buried in the filling materials of the side wall. In this way, at a vertical distance of 1m from the culvert arch, a layer of several pull plates is arranged for each layer of culvert side wall filling materials, forming a "mixed sandwich layer"; and during construction, one end of each pull plate of each layer is connected to the side wall of the culvert, thereby preventing and slowing down the uneven settlement of the culvert side wall filling materials in the later stage through the "friction tension" between the several pull plates of each layer and the upper and lower layers of filling materials.
[0125] (3) When the filling materials on both sides are flush with the culvert vault, EPS boards are laid on the culvert vault, and stretchable geogrids are laid on the top of the filling materials on both sides of the culvert. The geogrids are laid under the EPS boards on the side close to the EPS boards, and the overlap length of the two is 150 to 200 mm. The stretchable geogrids here are different from the geogrids used in normal construction. The geogrids are connected in a "diamond" form to form a mesh (similar to honeycombs), which has high strength and can adapt to the "large-scale tensile deformation" of the filling materials on both sides of the culvert in both the horizontal and vertical directions. In addition, in combination with several "mixed sandwich layers" under the filling materials on both sides of the culvert vault, it can effectively reduce the uneven stress in the longitudinal direction of the culvert (the slope sections on both sides of the roadbed and the horizontal section between the highest points of the slope sections on both sides) and the uneven settlement. The EPS board (expandable polystyrene foam board) is used in conjunction with the geogrid mesh overlapped on both sides of the lower end. When the vertical earth pressure on the culvert top is reduced, the geogrid mesh can be freely stretched to prevent excessive uneven settlement in the longitudinal direction of the culvert structure.
[0126] Furthermore, after the EPS board constructed on the top of the culvert is accepted, the high fill culvert roadbed construction above the culvert will be carried out, and the construction parameters, data and selected fillers obtained from the filler test will serve as the basis for guiding the high fill culvert roadbed.
[0127] The steps of the high fill culvert roadbed are as follows:
[0128] (1) The first layer of culvert roadbed filler mixture selected through filler test is laid on the laid EPS board to 0.5m above the culvert arch, and small machinery is used with manual assistance to roll it to avoid the impact of large machinery and equipment on the culvert arch;
[0129] In addition, on both sides of this layer of mixed filler, a drainage blind ditch is constructed along the longitudinal direction of the culvert at a horizontal distance of 2m from the culvert arch foot, so as to facilitate the longitudinal drainage of the upper filling roadbed in the later stage and reduce the impact of seepage on the roadbed, and the water damage caused by seepage of the fill above the culvert top and the fill on both sides of the culvert.
[0130] (2) When laying the second layer of mixed filler for culvert embankment, on the first layer of mixed filler (the first layer of mixed filler is laid out in one go along the direction of the road), the center line of the culvert is laid out along the longitudinal direction of the culvert, and the second layer of mixed filler for culvert embankment is laid to the designed height and compacted by partitions along the center line of the laid out line. The second layer of mixed filler for culvert embankment is constructed by "dividing sides" (both sides are along the center of the culvert); because the center line position of the first layer above the top of the culvert is separated by partitions, that is, the two sides are filled toward the center to the center line partition position "separated from each other", so that it is disconnected at this position, so as to adapt to the later stage, the uniform settlement caused by the fillers on both sides of the culvert is reduced to reduce the "reflection cracks" on the road surface above.
[0131] (3) Before laying the embankment mixture on the second layer of the culvert embankment, take out the partition in the first layer of mixed filler above the culvert (the second layer of mixed filler roadbed is disconnected and separated at the center of the culvert), pour medium-coarse sand into the gap after the partition is taken out, and compact the filling, lay a layer of geogrid above the gap after the partition of the second layer of embankment mixture is taken out, and then lay the upper culvert roadbed to the design elevation on the second layer of embankment mixture. Since the "middle layer" of the roadbed of the culvert is disconnected in this embodiment (the middle layer of the roadbed is separated); even if the fillers on both sides of the culvert settle unevenly, the road surface above, due to the "middle disconnection", can also adapt to the uneven settlement of the roadbed and road surface on the "left and right" sides, and reduce the disease of "reflective cracks".
[0132] (4) After the construction of the top layer of the roadbed is completed, the high fill culvert roadbed is monitored, including the deformation monitoring of the high fill culvert roadbed and the uneven settlement monitoring of the high fill culvert roadbed. Then, based on the monitoring feedback data, the safety of the culvert and the culvert roadbed is judged to facilitate the subsequent construction.
[0133] In summary, this method uses test data and parameters as a basis and reference to guide the construction of the roadbed (embankment) of high fill culverts. Through this construction method, the excavated soil-rock mixture material can be fully utilized to reduce the damage to the environment caused by abandoned soil; this construction method takes into account and improves the soil arch effect of the vertical earth pressure and lateral earth pressure on the roadbed at the top of the culvert, thereby ensuring the safety of the high fill culvert roadbed and saving the cost of reinforcing and maintaining the culvert and the culvert roadbed.
[0134] The preferred embodiments of the present invention are described in detail above in conjunction with the accompanying drawings. However, the present invention is not limited to the specific details in the embodiments in the above description. Within the technical concept of the present invention, a variety of simple modifications can be made to the technical solution of the present invention, and these simple modifications all belong to the protection scope of the present invention.
Claims
1. A culvert roadbed filling method, It is characterized in that The steps include: S1. Conduct filler test for high fill culvert roadbed, obtain parameters and data for culvert roadbed construction based on filler test, and reasonably select filler for filling construction based on these parameters and data; S2. According to the design requirements, construct the main body of the culvert, maintain it and after it has passed the acceptance inspection, fill the area around the culvert to the required range according to the design requirements; S3, carry out the construction of high fill culvert roadbed above the culvert, and use the construction parameters, data and selected fillers obtained from the S1 filler test to guide the basis for the high fill culvert roadbed; S4. Monitor the high fill culvert roadbed under construction.
2. A culvert roadbed filling method according to claim 1, It is characterized in that The filler test of S1 includes: compaction test; filler mechanical property test; indoor model test.
3. A culvert roadbed filling method according to claim 2, It is characterized in that The compaction test steps include: S11. Selection of filler: Select soil-rock mixture that can meet the requirements as filler for culvert roadbed; S12. Selection of particle gradation: According to the requirements of roadbed filling, the selected fillers are scaled down to obtain the data and parameters before and after scaling, so as to select the appropriate filler particle size; S13. Filler compaction test: Conduct a standard compaction test on the selected filler to obtain the parameters and data of the compaction test; after the compaction test, screen the filler and analyze the change pattern of the filler.
4. A culvert roadbed filling method according to claim 3, It is characterized in that The step of testing the mechanical properties of the filler comprises: performing a shear test on the filler in the filler, performing a shear test on the selected filler by using a shear instrument, and determining the mechanical parameters of the filler.
5. A culvert roadbed filling method according to claim 4, It is characterized in that The indoor model test includes: using similarity theory to ensure that the model test is similar to the culvert prototype during construction and filling in terms of geometry and boundary conditions, and meets the requirements of physical equations.
6. A culvert roadbed filling method according to claim 4, It is characterized in that The construction requirements of S2 for filling around the culvert are: S21. Fill the culvert with fillers on both sides at the same time, in layers, and the height difference of the fillers on both sides shall not exceed 300mm; S22. When the filling materials on both sides are 1m away from the culvert vault vertically, a pull plate is arranged at each layer and every horizontal distance of 0.8~1m for each layer of filling materials on both sides. One end of the pull plate is connected to the side wall of the culvert, and the other end is at least 1m away from the side wall of the culvert and is rolled and buried in the filling materials of the side wall. S23. After the filling materials on both sides are flush with the culvert vault, EPS boards are laid on the culvert vault, and stretchable geogrids are laid on the top of the filling materials on both sides of the culvert. The geogrids are laid under the EPS boards on one side close to the EPS boards, and the overlap length of the two is 150~200mm.
7. A culvert roadbed filling method according to claim 6, It is characterized in that The S3 culvert roadbed construction steps are as follows: S31. Lay the first layer of culvert roadbed filler mixture selected through filler test on the laid EPS board to 0.5m above the culvert arch, and use small machinery with manual assistance for rolling. And on both sides of the layer of mixed filler, 2m horizontally away from the culvert arch foot, construct a drainage blind ditch along the longitudinal direction of the culvert; S32, when the second layer of culvert embankment mixed filler is laid out on the first layer of mixed filler along the longitudinal direction of the culvert to the center line of the culvert, and the center line is separated by a partition, and the second layer of culvert embankment mixed filler is laid to the designed height, and the second layer of culvert embankment mixed filler is compacted; S33. Before laying the embankment mixture on the second layer of culvert embankment, take out the partition in S32, pour medium-coarse sand into the gap after the partition is taken out, and compact the filling. Lay a layer of geogrid above the gap after the partition is taken out of the second layer of embankment mixture, and then lay and fill the upper culvert roadbed on the second layer of embankment mixture to the designed elevation.
8. A culvert roadbed filling method according to claim 7, It is characterized in that The monitoring of the high fill culvert roadbed in S4 includes monitoring the deformation of the high fill culvert roadbed and monitoring the uneven settlement of the high fill culvert roadbed.