Pavement paving method
By setting a baffle in the paver hopper to form a transition section, the problems of low efficiency and poor flatness in asphalt paving construction are solved, uninterrupted paving is achieved and the durability and service performance of the pavement are improved.
Patent Information
- Application Number
- CN202411312966.9
- Authority / Receiving Office
- CN · China
- Patent Type
- Applications(China)
- Current Assignee / Owner
- Filing Date
- 2024-09-20
- Publication Date
- 2024-11-22
- Estimated Expiration
- 2044-09-20
AI Technical Summary
In the prior art, the alternating construction efficiency of the two asphalt mixtures during asphalt pavement construction is low and the flatness at the joints is poor, resulting in early water loss and peeling, affecting the durability and service performance of the pavement.
By installing a baffle in the hopper of the paver, the hopper is divided into two bins, and a transition section is formed by using the angle of the baffle, so that the first and second laying materials form an oblique drainage interface during the paving process. , realize uninterrupted paving, improve construction efficiency and flatness.
The uninterrupted process of asphalt pavement construction is realized, the construction time is shortened, the overall construction efficiency is improved, and the flatness at the joints is effectively improved, the risk of early water loss peeling is reduced, and the durability and performance of the pavement are improved. .
Smart Images

Figure CN118996962A_ABST
Abstract
Description
Technical Field
[0001] The invention relates to the technical field of road construction, and in particular to a road surface paving method. Background Art
[0002] With the rapid growth of traffic volume, environmental protection tasks have become increasingly arduous, and the requirements for highway pavement performance have been increasing. my country's highway pavement construction has gradually moved towards thickening, specialization, and diversification. Expressways have designed various asphalt pavement structures such as AC, PAC, SMA, and SUP for different climates, terrains, and usage requirements. The paving methods of asphalt pavements with different structural forms directly affect the flatness and durability of the asphalt pavement. Improper handling can easily lead to early water damage and peeling of the asphalt pavement layer, so higher requirements are placed on the paving technology of asphalt mixtures.
[0003] At present, in road construction, for the alternating construction of two asphalt mixtures, the most commonly used transverse joint treatment measures are mainly the following: manual shoveling method, at the end of the construction, the paver lifts the flat plate near the end, manually shovels the end mixture and then rolls it. Then check the flatness, and vertically plane off the part of the end layer with insufficient thickness before it cools down, so that it can be connected at a right angle during the next construction. Square wood or steel support method, first spread a thin layer of sand belt at the end of the predetermined paving section, and after paving the mixture, dig a gap in the paving layer while it is hot. The gap is located at the junction of the sanded and unsanded layers, and a wooden board or steel with the same thickness as the compacted layer is embedded in the gap. After compaction, the sanded part is shoveled off, the sand is swept away, the wooden board or steel is removed, and a tack coat of asphalt is applied to the end and then paved. Mechanical cutting method: first lay a layer of burlap or kraft paper (or a thin layer of abrasive belt) at the end of the predetermined paving section, spread and roll it into a slope, and before the mixture is completely cooled and hardened, cut off the part covered with burlap or kraft paper or a thin layer of abrasive belt with a cutting machine.
[0004] However, the above-mentioned existing technical solutions have obvious technical defects. On the one hand, downtime and waiting are inevitable during the construction process, which affects the construction efficiency, easily leads to material waste, increases construction costs, and waste materials need to be handled separately due to environmental protection requirements. On the other hand, the flatness construction quality of the joints is difficult to ensure, which easily leads to early water damage and peeling of the asphalt surface layer, affecting the durability and performance of the road surface. Summary of the invention
[0005] The purpose of the present invention is to provide a road paving method to solve the technical problems in the prior art of low efficiency and poor flatness at the joints when two asphalt mixtures are alternately constructed.
[0006] As conceived above, the technical solution adopted by the present invention is:
[0007] A road paving method, comprising:
[0008] Step 1: Prepare the first paving material and the second paving material;
[0009] Step 2: unloading the first paving material into a hopper of a paver, and driving the paver to pave the first paving material along an extension direction of the road surface to be paved;
[0010] Step 3: When the amount of the first paving material remaining in the hopper reaches a critical value, a baffle is installed in the hopper, the baffle is arranged at a first angle with the axis of the road surface to be paved, and the baffle separates the hopper into a first bin body and a second bin body, the first bin body is close to the paving end of the paver, the remaining first paving material is distributed into the first bin body, and the second paving material is unloaded into the second bin body;
[0011] Step 4: Continue to drive the paver to pave the first paving material. After the first paving material is paved, remove the baffle and continue to pave the second paving material onto the road surface to be paved; thereby forming a transition section between the first paving material and the second paving material on the road surface to be paved.
[0012] Preferably, in step 4, the paving speed of the paver is first reduced, and after the paving of the first paving material is completed and the paving of the second paving material begins, the initial paving speed is restored.
[0013] Preferably, the paving speed is greater than or equal to 2 m / min and less than or equal to 3 m / min.
[0014] Preferably, during actual construction, in step 4, when paving the transition section between the first paving material and the second paving material, the paver adjusts the loose paving thickness every time it travels a first distance value.
[0015] Preferably, the first angle is greater than or equal to 30 degrees and less than or equal to 80 degrees.
[0016] Preferably, before step 1, the road surface to be paved is cleaned.
[0017] Preferably, before step 1, the road surface to be paved is waterproofed, and a waterproof adhesive layer is sprayed on the road surface to be paved.
[0018] Preferably, during the transportation of the first paving material and the second paving material, the first paving material and the second paving material are covered with a heat-insulating tarpaulin.
[0019] Preferably, the transition section is arranged outside the drainage surface range of the road surface to be paved.
[0020] Preferably, after step 4, the first paving material and the second paving material that have been paved are rolled.
[0021] Beneficial effects of the present invention:
[0022] The pavement paving method proposed by the present invention, during the construction process, firstly prepare the first paving material and the second paving material, then unload the first paving material into the hopper of the paver, and drive the paver to pave the first paving material along the extension direction of the pavement to be paved; when the amount of the first paving material remaining in the hopper reaches a critical value, a baffle is installed in the hopper, the baffle is set at a first angle to the axis of the pavement to be paved, the baffle separates the hopper into a first bin body and a second bin body, the first bin body is close to the paving end of the paver, the remaining first paving material is manually shoveled into the first bin body, and then the second paving material is unloaded into the second bin body by a transport vehicle; then , continue to drive the paver to pave the first paving material, and after the first paving material is paved, remove the baffle and continue to pave the second paving material to the road surface to be paved; because the baffle is set at the first angle, the first paving material and the second paving material also form a transition section along the inclination of the baffle during the paving process. Through the formation of the transition section, an obvious oblique drainage interface is formed after the first paving material and the second paving material are paved, which completes the transition between the two paving materials and makes the construction uninterrupted, avoiding the downtime and waiting when the two paving materials are alternating, and can achieve uninterrupted paving, shortening the construction time and improving the overall construction efficiency. In addition, the formation of the transition section effectively improves the flatness of the joints between the two different paving materials, reduces the risk of early water damage and peeling of the paving layer due to poor flatness, and improves the durability and performance of the road surface. BRIEF DESCRIPTION OF THE DRAWINGS
[0023] Figure 1 is a flow chart of a road paving method provided by an embodiment of the present invention;
[0024] Figure 2 It is a schematic diagram of the structure of a paver provided by an embodiment of the present invention.
[0025] In the figure:
[0026] 1. First paving material; 2. Second paving material; 3. Paving machine; 31. Hopper; 32. Baffle; 4. Transition section. DETAILED DESCRIPTION
[0027] Embodiments of the present invention are described in detail below, examples of which are shown in the accompanying drawings, wherein the same or similar reference numerals throughout represent the same or similar elements or elements having the same or similar functions. The embodiments described below with reference to the accompanying drawings are exemplary and are intended to be used to explain the present invention, and should not be construed as limiting the present invention.
[0028] In the description of the present invention, unless otherwise clearly specified and limited, the terms "connected", "connected", and "fixed" should be understood in a broad sense, for example, it can be a fixed connection, a detachable connection, or an integral connection; it can be a mechanical connection or an electrical connection; it can be a direct connection or an indirect connection through an intermediate medium, it can be the internal connection of two elements or the interaction relationship between two elements. For ordinary technicians in this field, the specific meanings of the above terms in the present invention can be understood according to specific circumstances.
[0029] In the present invention, unless otherwise clearly specified and limited, a first feature being "above" or "below" a second feature may include that the first and second features are in direct contact, or may include that the first and second features are not in direct contact but are in contact through another feature between them. Moreover, a first feature being "above", "above" and "above" a second feature includes that the first feature is directly above and obliquely above the second feature, or simply indicates that the first feature is higher in level than the second feature. A first feature being "below", "below" and "below" a second feature includes that the first feature is directly below and obliquely below the second feature, or simply indicates that the first feature is lower in level than the second feature.
[0030] The technical solution of the present invention is further described below with reference to the accompanying drawings and through specific implementation methods.
[0031] See also Figure 1 and Figure 2 The pavement paving method provided by the embodiment of the present invention includes step 1: preparing the first paving material 1 and the second paving material 2; step 2: unloading the first paving material 1 into the hopper 31 of the paver 3, and driving the paver 3 to pave the first paving material 1 along the extension direction of the pavement to be paved; step 3: when the amount of the remaining first paving material 1 in the hopper 31 reaches a critical value, installing a baffle 32 in the hopper 31, the baffle 32 is set at a first angle with the axis of the pavement to be paved, and the baffle 32 separates the hopper 31 into a first bin body and a second bin body, the first bin body is close to the paving end of the paver 3, and the remaining first paving material 1 is distributed into the first bin body, and the second paving material 2 is unloaded into the second bin body; step 4: continue to drive the paver 3 to pave the first paving material 1, after the paving of the first paving material 1 is completed, remove the baffle 32, and continue to pave the second paving material 2 to the pavement to be paved; thereby, a transition section 4 is formed between the first paving material 1 and the second paving material 2 on the pavement to be paved.
[0032] In this embodiment, the first paving material 1 is made of AC-13 asphalt, and the second paving material 2 is made of PAC-13 asphalt. In other embodiments, the first paving material 1 and the second paving material 2 can also be made of other materials such as gravel and concrete, which are not limited here.
[0033] The pavement paving method proposed by the present invention forms a clear oblique drainage interface after the first paving material 1 and the second paving material 2 are paved through the formation of the transition section 4 during the construction process, thus completing the transition between the two paving materials and making the construction uninterrupted, avoiding downtime and waiting when the two paving materials are switched, and can achieve uninterrupted paving, shortening the construction time and improving the overall construction efficiency. In addition, the formation of the transition section 4 effectively improves the flatness of the joint between the two different paving materials, reduces the risk of early water damage and peeling of the paving layer due to poor flatness, and improves the durability and performance of the pavement.
[0034] It is understandable that the paver 3 is a mechanical device previously available in the art, and its working principle and specific structure are not described in detail here.
[0035] The specific steps of the road paving method are described in detail below.
[0036] First, the porosity of PAC-13 asphalt is between 18% and 25%, and the porosity of AC-13 asphalt is between 3% and 6%. Therefore, the drainage performance of the two paving materials is different. Considering that the drainage facilities of PAC-13 asphalt pavement sections are different from those of ordinary asphalt pavement sections, in order to ensure smooth lateral drainage of PAC-13 asphalt pavement, transition section 4 is set outside the drainage pavement range of the road to be paved.
[0037] Before step 1, in order to ensure the performance of the paving material after paving, the road surface to be paved is first cleaned. Specifically, cleaning equipment is used for cleaning, and then air blowing equipment is used for dust removal or other effective measures are used to clean the road surface.
[0038] In addition, before step 1, the pavement to be paved needs to be waterproofed and a waterproof adhesive layer is sprayed on the pavement to be paved. Since the materials of the first paving material 1 and the second paving material 2 are different, the treatment methods for the pavement to be paved of the two paving materials are also different. For the road section of PAC-13 asphalt, in order to avoid the flow of SBS modified emulsified asphalt during spreading, SBS modified emulsified asphalt should be spread in two times, with the first spreading amount being about 0.4kg / m2 and the second spreading amount being about 0.4kg / m2. When spreading, the spreader should maintain a constant speed and a stable rotation speed to ensure uniform spreading. During the spreading process of SBS modified emulsified asphalt, attention should be paid to the construction treatment of the joints, which are specifically divided into transverse joints and longitudinal joints. At the location of the transverse joint, when constructing again, it is necessary to closely connect with the previous construction while also avoiding overlapping with the previous construction section. For AC-13 asphalt sections, the amount of pure asphalt in the SBS modified emulsified asphalt inter-layer tack coat oil spray emulsion should be greater than 0.3kg / ㎡. The specific spraying amount should be determined after trial spraying. The sprayed tack coat oil must be uniformly misted and evenly distributed in the full width of the road surface to form a film. There must be no leakage or strips, and no accumulation. Insufficient spraying should be supplemented, and excessive spraying should be scraped off. After spraying the tack coat oil, it is strictly forbidden for material transport vehicles and pedestrians to pass.
[0039] It is worth noting that the tack coat oil should be spread on the same day. After the SBS modified emulsified asphalt is demulsified and the water evaporates, the next layer of paving material should be laid immediately to ensure that the tack coat is not contaminated.
[0040] Step 1 is the preparation process of the first paving material 1 and the second paving material 2. The paving parameters need to be adjusted and stirred according to the actual working conditions. Specifically, the stirring time is determined by trial mixing, so that the mixture is evenly mixed and all the mineral particles are covered with asphalt. During the mixing process, the operator should observe the color of the finished material, the approximate proportion of the gradation, measure the oil temperature, the amount of asphalt, and the surface of the mixed material is black with a slightly brown luster, not dry, and does not collapse or segregate when loaded on the vehicle.
[0041] After the preparation of the first paving material 1 and the second paving material 2 is completed, they need to be transported to the construction site. In order to reduce the frequent change of vehicles and unloading in front of the paver 3, a large dump truck is used. The car should have a tight, clean, smooth metal bottom plate and be cleaned. Apply a layer of oil-water mixture on the side panels and bottom of the car. Use a sprayer to apply the diesel-water mixture to ensure that it is evenly sprayed without residual liquid. When loading, the car should move back and forth in the order of front, back, middle, front, and back to avoid segregation of the mixture. The material transport vehicle should have good coverage and insulation to avoid pollution. In order to avoid the shutdown of the paver 3 due to insufficient supply to the site, the finished product storage bin of the mixing plant stores enough mixture. During construction, at least four trucks of paving materials are always kept in front of the paver 3 to ensure continuous paving.
[0042] In order to prevent the paving material from losing temperature and causing crusting and contamination on the surface of the mixture, the first paving material 1 and the second paving material 2 are covered with thermal insulation tarpaulin during transportation. To reduce the temperature loss of the paving material during transportation, the material truck driving to the paving site shall not stop midway, and the paving material that has been transported to the site should be paved as soon as possible to avoid temperature loss and agglomeration.
[0043] After the material preparation is completed, step 2 is performed, and the first paving material 1 is first spread on the road surface to be paved. Then, step 3 is performed, and when the amount of the remaining first paving material 1 in the hopper 31 reaches a critical value, a baffle 32 is installed in the hopper 31, and the baffle 32 is set at a first angle with the axis of the road surface to be paved. The baffle 32 separates the hopper 31 into a first bin and a second bin. The first bin is close to the paving end of the paver 3, and the remaining first paving material 1 is distributed into the first bin, and the second paving material 2 is unloaded into the second bin, wherein the paving end is used to pave the paving material in the hopper 31 on the road surface to be paved.
[0044] The first angle is greater than or equal to 30 degrees and less than or equal to 80 degrees. Within this angle range, it is helpful to better control the distribution and connection of the first paving material 1 and the second paving material 2 in the transition section 4, thereby further improving the flatness of the road paving, so that the distribution of the first paving material 1 and the second paving material 2 in the alternating process is more accurate and efficient.
[0045] In step 4, during the paving process of the paver 3, the paving speed of the paver 3 is first reduced, and after the first paving material 1 is laid and the second paving material 2 begins to be laid, the initial paving speed is restored, which helps to more finely control the paving of the transition section 4, making the connection between the two paving materials more stable, thereby improving the construction quality of the transition section 4. Reducing the paving speed can reduce the material segregation phenomenon that may be caused by excessive speed when the paving materials are alternated, ensure the uniformity of the materials in each part of the road surface, and improve the overall performance of the road surface. By adjusting the speed, the paving thickness and uniformity of the paving materials can be better controlled, thereby further improving the flatness of the road surface and reducing the possibility of bumps and uneven settlement.
[0046] Specifically, the paving speed is greater than or equal to 2m / min and less than or equal to 3m / min. The frequency of folding the hopper should be reduced as much as possible to avoid flaky segregation of paving materials. When folding the hopper, the previous material transport vehicle has just left after unloading, and the next material transport vehicle has not yet arrived. The hopper 31 must be folded before the scraper in the receiving hopper 31 is exposed and there is about 50cm thick hot paving material, so as to ensure continuous feeding and avoid segregation of coarse aggregate.
[0047] It is worth noting that the paver 3 must spread slowly, evenly, continuously and uninterruptedly, and must not change speed or stop in the middle at will, so as to improve the flatness and reduce the segregation of the mixture. The screed plate should be preheated to above 120℃ in advance, and medium-strong tamping grade should be used to make the initial compaction of the pavement not less than 85%. The paving temperature shall not be lower than 160℃.
[0048] In addition, considering that the loose laying coefficients of the first paving material 1 and the second paving material 2 are different during actual construction, in step 4, when paving the transition section 4 between the first paving material 1 and the second paving material 2, the paver 3 adjusts the loose laying thickness every time it travels the first distance value. The laying thickness of each paving material can be accurately controlled to ensure the accuracy and quality of paving. Timely and frequent thickness adjustments help eliminate the unevenness caused by the difference in loose laying coefficients, making the transition between the first paving material 1 and the second paving material 2 smoother, thereby improving the flatness of the road surface.
[0049] After step 4, the first paving material 1 and the second paving material 2 that have been paved are rolled. By rolling the first paving material 1 and the second paving material 2 that have been paved, the voids in the mixture can be effectively reduced, the density of the road surface can be increased, and the bearing capacity and stability of the road surface can be improved. In addition, rolling can make the paving materials more evenly distributed, eliminate the minor ups and downs and unevenness that may occur during the paving process, further improve the flatness of the road surface, and provide a more comfortable driving experience.
[0050] Specifically, in this embodiment, four double steel wheel rollers and two rubber wheel rollers are selected for rolling. Compaction should be carried out according to the principles of initial compaction, repeated compaction, supplementary compaction and final compaction, following the principle of "closely following, slow compaction, uniform speed and less water", that is, the roller must closely follow the paver 3 and move forward to roll, in the order of light first, heavy later, and from low to high. The rolling direction is parallel to the center line of the road, and static pressure should be used during rolling, and the length of the rolling area is controlled at 20-40m.
[0051] The above embodiments are only to illustrate the basic principles and characteristics of the present invention. The present invention is not limited by the above embodiments. Without departing from the spirit and scope of the present invention, the present invention may be subject to various changes and modifications, which are within the scope of the present invention. The scope of protection of the present invention is defined by the attached claims and their equivalents.
Claims
1. A road paving method, characterized in that: include: Step 1: preparing the first paving material (1) and the second paving material (2); Step 2: unloading the first paving material (1) into the hopper (31) of the paver (3), and driving the paver (3) to pave the first paving material (1) along the extension direction of the road surface to be paved; Step 3: When the amount of the first paving material (1) remaining in the hopper (31) reaches a critical value, a baffle (32) is installed in the hopper (31), the baffle (32) is arranged at a first angle with the axis of the road surface to be paved, and the baffle (32) separates the hopper (31) into a first bin and a second bin, the first bin being close to the paving end of the paver (3), and the remaining first paving material (1) is distributed into the first bin, and the second paving material (2) is discharged into the second bin; Step 4: Continue to drive the paver (3) to pave the first paving material (1). After the first paving material (1) is paved, remove the baffle (32) and continue to pave the second paving material (2) onto the road surface to be paved; thereby forming a transition section (4) between the first paving material (1) and the second paving material (2) on the road surface to be paved.
2. The road paving method according to claim 1, characterized in that: In step 4, the paving speed of the paver (3) is first reduced, and after the paving of the first paving material (1) is completed and the paving of the second paving material (2) begins, the initial paving speed is restored.
3. The road paving method according to claim 2, characterized in that: The paving speed is greater than or equal to 2 m / min and less than or equal to 3 m / min.
4. The road paving method according to claim 1, characterized in that: During actual construction, in step 4, when paving the transition section (4) between the first paving material (1) and the second paving material (2), the paver (3) adjusts the loose paving thickness every time it travels a first distance value.
5. The road paving method according to claim 1, characterized in that: The first angle is greater than or equal to 30 degrees and less than or equal to 80 degrees.
6. The road paving method according to any one of claims 1 to 5, characterized in that: Before step 1, the road surface to be paved is cleaned.
7. The road paving method according to any one of claims 1 to 5, characterized in that: Before step 1, the road surface to be paved is waterproofed, and a waterproof adhesive layer is sprayed on the road surface to be paved.
8. The road paving method according to any one of claims 1 to 5, characterized in that: During the transportation of the first paving material (1) and the second paving material (2), the first paving material (1) and the second paving material (2) are covered with a heat-insulating tarpaulin.
9. The road paving method according to any one of claims 1 to 5, characterized in that: The transition section (4) is arranged outside the drainage surface range of the road surface to be paved.
10. The road paving method according to any one of claims 1 to 5, characterized in that: After step 4, the first paving material (1) and the second paving material (2) that have been paved are rolled.
Citation Information
Patent Citations
Pumping distributor of pavement paver
CN113026482A
Treatment method for construction joints in paving process of steel slag asphalt mixture pavement
CN115012271A
Paver and construction process of new and old asphalt concrete pavement
CN115522435A
Miniature paver
CN115787423A
Hopper insert for an asphalt paving machine
US9702095B1