Appearance restoration method of historical building bare brick wall

Through the color adjustment and polishing technology of new clay bricks, combined with the use of transparent water-based alkali-resistant coatings, the specifications and color consistency of old bricks in the restoration of clean water brick walls in historical buildings have been solved, reducing costs and improving the aesthetics after repairs. Weather resistance.

CN118997537AActive Publication Date: 2024-11-22SHANGHAI BUILDING DECORATION ENG GRP CO LTD
View PDF 4 Cites 0 Cited by

Patent Information

Application Number
CN202411225707.2
Authority / Receiving Office
CN · China
Patent Type
Applications(China)
Current Assignee / Owner
Filing Date
2024-09-03
Publication Date
2024-11-22
Estimated Expiration
2044-09-03

AI Technical Summary

Technical Problem

When the existing technology repairs the clean water brick walls of historical buildings, it is difficult to find old bricks with the same specifications and colors, and the large-area flat color process is costly and affects the natural feeling of the original brick wall.

Method used

New clay bricks are used, manufactured according to the specifications of old bricks, and their color is consistent with the old bricks by color adjustment and polishing. They are sealed and protected with transparent water-based alkali-resistant coatings, reducing flat color technology and improving aesthetics.

Benefits of technology

There is no need to purchase old bricks, which reduces procurement costs, avoids the problem of insufficient number of old bricks, ensures overall color coordination and aesthetics, and improves weather resistance after repair.

✦ Generated by Eureka AI based on patent content.
Patent Text Reader

Abstract

The invention discloses a method for repairing the appearance of a clear water brick wall of a historical building. The method comprises the following steps: S1, newly manufacturing clay bricks according to the old brick specification of the clear water brick wall; s2, determining the position of a newly-manufactured clay brick, and determining an exposed surface corresponding to the newly-manufactured clay brick according to the position; s3, sealing six surfaces of the newly-manufactured clay brick; s4, preparing a pigment, brushing the pigment on the newly-made clay brick to enable the color of the newly-made clay brick to be consistent with that of the old brick, and recording the proportion for subsequent use; s5, building or cutting and pasting new clay bricks in the to-be-repaired area of the bare brick wall until the repair is complete, and cleaning the building mortar and the adhesive mortar with polluted surfaces; s6, preparing pigments according to the proportion obtained in the step S4, and spraying and brushing all the newly-made clay bricks needing to be subjected to color matching for coloring; and S7, after the pigment is dried, confirming that the overall color impression is correct, and finishing repairing. According to the invention, the purchasing problem of old bricks is solved, the cost of unnecessary flat color process is reduced, and the aesthetic degree is improved.
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] The invention relates to the field of historical building repair, and in particular to a method for repairing the appearance of a plain brick wall of a historical building. Background Art

[0002] When the exposed brick walls of historical buildings deteriorate over time, the existing technology uses methods such as digging out and replacing new bricks, patching the surface with brick slices, and partially patching with brick powder. The above existing technologies have the following problems:

[0003] 1) If the renovation method of hollowing and brick slabs is adopted, old bricks need to be purchased. The specifications, colors and glaze texture of the purchased old bricks will be very different from those of the historical buildings to be repaired. And the number of old bricks purchased is limited.

[0004] 2) For bricks with color difference, the flat color process is used for the plain brick wall, but the flat color needs to be done on the whole brick wall. For large areas of brick walls with the same color and only a small part of the wall needs to be repaired, the cost of large-area flat color is too high, and the brick wall after flat color also loses the natural feeling of the original brick wall. Summary of the invention

[0005] In order to solve the deficiencies in the above-mentioned prior art, the present invention provides a method for repairing the appearance of the exposed brick wall of a historical building, which not only solves the problem of difficulty in purchasing old bricks, but also reduces the cost of unnecessary flat color process and improves the appearance. In order to achieve the above-mentioned invention purpose, the present invention provides the following technical solutions:

[0006] A method for repairing the appearance of a plain brick wall of a historical building, the method comprising the following steps:

[0007] S1. Make new clay bricks according to the specifications of old bricks in the exposed brick wall, and the color of the new clay bricks is lighter than that of the old bricks;

[0008] S2. According to the area to be repaired of the exposed brick wall, the position of the newly made clay brick is determined, and the exposed surface of the newly made clay brick corresponding to the position is determined, wherein the exposed surface refers to the exposed part of each newly made clay brick after the exposed brick wall repair is completed;

[0009] S3. The newly made clay bricks are sealed on six sides by applying a primer coat of exterior paint once;

[0010] S4. Color mixing: Mix the colorant and apply it on the new clay bricks so that the color of the new clay bricks is consistent with the color of the old bricks, and record the ratio for subsequent use;

[0011] S5. Lay new clay bricks or cut patches in the area to be repaired of the exposed brick wall until the repair is complete, and clean the contaminated masonry mortar and bonding mortar on the surface;

[0012] S6. Prepare the colorant according to the ratio obtained in step S4, and spray or brush the color on all the newly made clay bricks that need to be colored; S7. After the colorant is dry, confirm that the overall color appearance is correct and the repair is completed.

[0013] Furthermore, in step S2, after the exposed surface is determined, the exposed surface is polished until the appearance of the exposed surface is the same as that of the intact exposed part of the old brick.

[0014] Furthermore, the method for grinding the exposed surface is to first use 120-grit sandpaper for coarse grinding, then use 120-grit sandpaper for fine grinding, and finally use 320-grit sandpaper for polishing.

[0015] Furthermore, after polishing, the dust and garbage remaining on the surface are cleaned.

[0016] Furthermore, in step S3, the exterior wall primer coating is a transparent water-based alkali-resistant coating.

[0017] Furthermore, in step S4, the colorant is prepared by mixing water-based color paste and acrylic organic dye.

[0018] Furthermore, in step S6, after coloring is completed, a transparent water-based protective agent is applied.

[0019] Furthermore, in step S7, after the pigment is dried, the exposed surface of the newly made clay brick is sealed with a transparent water-based alkali-resistant paint for a second time, and finally a transparent matte topcoat of an exterior wall water-based paint is applied.

[0020] Based on the above technical solution, compared with the prior art, the technical solution of the present invention has the following advantages:

[0021] 1. There is no need to purchase old bricks, which saves procurement costs and avoids the problem of difficulty in timely procurement due to insufficient number of old bricks.

[0022] 2. Use transparent water-based anti-alkali exterior wall paint primer to seal the six faces of the newly made clay bricks, which can not only prevent the alkaline penetration of masonry mixed mortar or bonding mixed mortar, but also prevent the surface density of the newly made clay bricks from being uneven, resulting in different shades of color on the brick surface when coloring.

[0023] 3. After coloring is completed, apply a transparent water-based protective agent to increase the weather resistance of the antique color.

[0024] 4. After the exposed brick wall is finally repaired by the present invention, the overall color is more coordinated and more beautiful. DETAILED DESCRIPTION

[0025] The present invention is further described in detail below in conjunction with specific examples in order to provide a clearer understanding of its structural types and usage, but this should not be used to limit the protection scope of the patent of the present invention.

[0026] A method for repairing the appearance of a plain brick wall of a historical building, the method comprising the following steps:

[0027] S1. Use newly made clay bricks that are consistent with the specifications of the bricks used in the historical buildings being repaired. The color of the newly made bricks should be lighter than the color of the old bricks of the historical buildings being repaired, so as to facilitate color adjustment later.

[0028] S2. Determine the exposed surface of the newly made clay bricks after laying and pasting, and polish the exposed surface. Use a disc grinder to grind with 120-grit sandpaper first, then use 180-grit sandpaper, and finally polish with 320-grit sandpaper. The degree of grinding and polishing should be the same as the original intact and beautiful old brick surface of the historical building being repaired without modification.

[0029] Clean the dust and garbage remaining on the surface after polishing.

[0030] S3. Use a transparent water-based anti-alkali exterior wall paint primer to lightly apply once to seal the six sides of the brick. Sealing has two functions: one is to prevent the alkaline penetration of masonry mixed mortar or bonding mixed mortar; the other is to prevent the surface density of the newly made clay brick from being uneven, resulting in different shades of color on the brick surface when coloring.

[0031] S4. Use water-based color paste, acrylic organic dye and transparent water-based protective agent. In view of the difference between the base color of the newly made clay bricks on site and the color of the bricks of the historical building being repaired, on-site color matching is carried out. The purpose is to make the color of the new clay bricks consistent with that of the old bricks. After color matching, color the surface of the new clay bricks, make samples of different shades of color around the color of the exterior wall of the historical building being repaired, and record the ratio of colorants of different samples. Select the ratio of the color of the new clay brick surface dye after drying and the color of the old bricks as the formula of the colorant for large-scale construction.

[0032] Apply a transparent water-based protective agent on the surface of newly made clay tiles after the color has dried. Its function is to increase the weather resistance of the antique color.

[0033] S5. Lay or cut new clay bricks on the exterior walls of the historical buildings being repaired, and clean the contaminated masonry mortar and bonding mortar on the surface;

[0034] S6. Spray or brush color on all newly made clay bricks that need to be colored according to the final color matching formula.

[0035] S7. After the coloring dye on the large surface is dry, it is compared with the color of the specific historical building bricks to be repaired. After the acceptance parties confirm that the color quality of the large surface is correct, the transparent water-based anti-alkali exterior wall paint primer is sealed on the clay brick surface for the second time, and the final exterior wall water-based paint transparent matte topcoat. The number and thickness of primer and topcoat are based on the comparison of the appearance of the specific historical building bricks to be repaired.

[0036] Undoubtedly, the present invention has other similar structural compositions and usage modes besides the above-mentioned embodiments. In summary, the present invention also includes other obvious changes and substitutions for those skilled in the art.

Claims

1. A method for restoring the appearance of a plain brick wall of a historical building, characterized in that: The method comprises the following steps: S1. Make new clay bricks according to the specifications of old bricks in the exposed brick wall, and the color of the new clay bricks is lighter than that of the old bricks; S2. According to the area to be repaired of the exposed brick wall, the position of the newly made clay brick is determined, and the exposed surface of the newly made clay brick corresponding to the position is determined, wherein the exposed surface refers to the exposed part of each newly made clay brick after the exposed brick wall repair is completed; S3. The newly made clay bricks are sealed on six sides by applying a primer coat of exterior paint once; S4. Color mixing: Mix the colorant and apply it on the new clay bricks so that the color of the new clay bricks is consistent with the color of the old bricks, and record the ratio for subsequent use; S5. Lay new clay bricks or cut patches in the area to be repaired of the exposed brick wall until the repair is complete, and clean the contaminated masonry mortar and bonding mortar on the surface; S6. Modulate the colorant according to the ratio obtained in step S4, and spray or brush the newly made clay bricks that need color matching; S7. After the pigment is dry, confirm that the overall color appearance is correct and the repair is complete.

2. The method for repairing the appearance of a historic building's exposed brick wall according to claim 1, characterized in that: In step S2, after the exposed surface is determined, the exposed surface is polished until the appearance of the exposed surface is the same as that of the intact exposed part of the old brick.

3. The method for repairing the appearance of a historic building's exposed brick wall according to claim 2, characterized in that: The method for grinding the exposed surface is to use 120-grit sandpaper for rough grinding, then use 120-grit sandpaper for fine grinding, and finally use 320-grit sandpaper for polishing.

4. The method for repairing the appearance of a bare brick wall of a historical building according to claim 3, characterized in that: After polishing, clean the dust and garbage remaining on the surface.

5. The method for repairing the appearance of a historic building's exposed brick wall according to claim 1, characterized in that: In step S3, the exterior wall primer coating is a transparent water-based alkali-resistant coating.

6. The method for repairing the appearance of a historic building's exposed brick wall according to claim 1, characterized in that: In step S4, the colorant is prepared by mixing water-based color paste and acrylic organic dye.

7. The method for repairing the appearance of a historic building's exposed brick wall according to claim 1, characterized in that: In step S6, after coloring is completed, a transparent water-based protective agent is applied.

8. The method for repairing the appearance of a bare brick wall of a historical building according to claim 5, characterized in that: In step S7, after the pigment is dried, the exposed surface of the newly made clay brick is sealed with a transparent water-based alkali-resistant paint for a second time, and finally a transparent matte topcoat of an exterior wall water-based paint is applied.

Citation Information

Patent Citations

  • Quick-drying water-based seal primer

    CN105670405A

  • Historical building plain brick wall repair construction method

    CN109653529A

  • Repair process for brick wall of cultural insurance building

    CN116220415A

  • Old chamotte brick decorations face mould piece

    CN206205347U