Optical lens and manufacturing method thereof

By using raw materials such as quartz sand for smelting and mixing, and forming a protective layer of potassium nitrate in the optical lens, the bubbles and strength problems of the optical lens are solved, and the efficient compressive strength and transparency of the lens are improved.

CN119001932APending Publication Date: 2024-11-22南京荣达光学仪器有限公司
View PDF 0 Cites 0 Cited by

Patent Information

Application Number
CN202411233293.8
Authority / Receiving Office
CN · China
Patent Type
Applications(China)
Current Assignee / Owner
Filing Date
2024-09-04
Publication Date
2024-11-22

AI Technical Summary

Technical Problem

Optical lenses are prone to bubbles and have low strength and are prone to damage when used.

Method used

Use quartz sand, oxides, hydroxides, nitrates, carbonates, phosphates, lens resins, plastics, cosolvents, clarifiers and potassium nitrate to be melted and mixed. After thorough smelting and mixing, it is in the mold Add potassium nitrate solution to form a protective layer to improve the strength and transparency of the lens.

Benefits of technology

Effectively reduce the internal bubbles of the lens, enhance the strength and service life of the lens, improve the compressive strength and reduce the mirror bubbles, forming a more glossy and stable optical lens.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure CN119001932A_ABST
    Figure CN119001932A_ABST
Patent Text Reader

Abstract

The invention discloses an optical lens and a manufacturing method thereof. The optical lens is prepared from the following raw materials in parts by weight: 10-20 parts of quartz sand, 5-10 parts of oxide, 5-10 parts of hydroxide, 5-10 parts of nitrate, 5-10 parts of carbonate, 5-10 parts of phosphate, 1-5 parts of lens resin, 1-5 parts of plastic, 1-5 parts of a cosolvent, 1-5 parts of a clarifying agent, 1-5 parts of a decolorizing agent and 1-5 parts of potassium nitrate. A manufacturing method of an optical lens comprises the following steps that S1, quartz sand, hydroxide, nitrate, carbonate and phosphate are added into a smelting furnace to be smelted, and a first mixture is obtained after smelting; s2, the resin and the plastic are added into a smelting furnace to be smelted, and a second mixture is obtained through smelting; s3, at the moment, the first mixture and the second mixture are added into a smelting furnace to be smelted; the optical lens has the effect of effectively reducing bubbles in the lens, meanwhile, the strength of the optical lens can be effectively guaranteed, and the optical lens is convenient to produce and popularize.
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] The present invention relates to the technical field of optical lenses, and in particular to an optical lens and a method for manufacturing the optical lens. Background Art

[0002] In the prior art, an optical lens is a transparent material with one or more curved surfaces made of optical materials such as glass or resin. It is often assembled with eyeglass frames to form glasses, which are used to correct the user's vision and obtain a clear field of vision. There are various types of lenses, including but not limited to anti-reflective protective lenses, colored lenses, tinted lenses, polarized lenses and photochromic lenses. These lenses have their own characteristics. For example, anti-reflective protective lenses prevent strong light reflection by coating a thin layer of magnesium fluoride on the surface. Colored lenses and tinted lenses add chemicals during the production process to make the lenses appear colored. Polarized lenses are used to filter light in a specific direction, and photochromic lenses change color under strong light to provide protection. The materials of optical lenses include resin and glass. Glass lenses are made of high-purity oxides of silicon, boron, sodium, potassium, zinc, lead, magnesium, calcium, barium, etc., mixed according to a specific formula, melted at high temperature in a platinum crucible, and made after a series of process treatments. They have high transparency and refractive index. The difference between optical glass and other glasses is that as a component of the optical system, it must meet the requirements of optical imaging. Therefore, the determination of optical glass quality also includes some special and strict indicators. There are the following requirements for optical glass: 1. Specific optical constants and consistency of optical constants of the same batch of glass. Each type of optical glass has a specified standard refractive index value for different wavelengths of light, which serves as the basis for optical designers to design optical systems. Therefore, the optical constants of optical glass produced by the factory must be within a certain allowable deviation range of these values, otherwise the actual imaging quality will not be consistent with the expected results during design, affecting the quality of optical instruments. At the same time, since the same batch of instruments are often made of the same batch of optical glass, in order to facilitate the unified calibration of the instruments, the allowable deviation of the refractive index of the same batch of glass must be stricter than their deviation from the standard value. 2. High transparency. The brightness of the image of the optical system is proportional to the transparency of the glass. The transparency of optical glass to a certain wavelength of light is expressed by the light absorption coefficient Kλ. After the light passes through a series of prisms and lenses, part of its energy is lost in the interface reflection of the optical parts and the other part is absorbed by the medium (glass) itself. The former increases with the increase of the refractive index of the glass. This value is very large for high refractive index glass, such as the light reflection loss of one surface of heavy flint glass is about 6%. Therefore, for an optical system containing multiple thin lenses, the main way to improve transmittance is to reduce the reflection loss on the lens surface, such as coating the surface with an anti-reflection film. For large-sized optical parts such as the objective lens of an astronomical telescope, due to its large thickness, the transmittance of the optical system is mainly determined by the light absorption coefficient of the glass itself. By improving the purity of the glass raw materials and preventing any coloring impurities from mixing in the entire process from batching to melting, the light absorption coefficient of the glass can generally be made less than 0.01 (that is, the light transmittance of glass with a thickness of 1 cm is greater than 99%).

[0003] In the prior art, when an optical lens is in use, bubbles are generated inside the optical lens, and the optical lens has low strength and is easily damaged.

[0004] Therefore, the present application proposes an optical lens and a method for manufacturing an optical lens to solve the above problems. Summary of the invention

[0005] Based on the technical problems that bubbles are generated inside the optical lens when it is in use and the optical lens has low strength and is easily damaged, the present invention proposes an optical lens and a method for manufacturing the optical lens.

[0006] The optical lens proposed by the present invention comprises the following raw materials in parts by weight: 10-20 parts of quartz sand, 5-10 parts of oxide, 5-10 parts of hydroxide, 5-10 parts of nitrate, 5-10 parts of carbonate, 5-10 parts of phosphate, 1-5 parts of lens resin, 1-5 parts of plastic, 1-5 parts of co-solvent, 1-5 parts of clarifier, 1-5 parts of decolorizer and 1-5 parts of potassium nitrate.

[0007] A method for manufacturing an optical lens comprises the following steps: S1: adding quartz sand, hydroxide, nitrate, carbonate and phosphate into a furnace for smelting to obtain a first mixture; S2: adding the resin and the plastic into a melting furnace for melting, and obtaining a second mixture by melting; S3: At this time, the first mixture and the second mixture are added into the furnace for smelting; S4: adding a solvent into the melting furnace during the melting process, and obtaining a lens mixture after sufficient melting; S5: adding the obtained lens mixture into a mixer, adding a clarifying agent and a decolorizing agent into the mixer, and then fully mixing them through the mixer; S6: The mixed material is then squeezed into a mold by an extruder, and pressed into shape by a press, and potassium nitrate solution is added into the mold to fully contact with the material; S7: After the final shaping, the material is polished by a grinder to form an optical lens.

[0008] Preferably, the auxiliary solvent is prepared by mixing sodium oxide, potassium oxide, lead oxide, calcium oxide and barium oxide.

[0009] Preferably, the clarifier is prepared by mixing arsenic oxide, antimony oxide and nitrifying salt.

[0010] Preferably, the decolorizing agent is made of sodium hypochlorite and potassium permanganate.

[0011] Preferably, the resin is made by mixing polycarbonate, polystyrene, polyurethane, epoxy resin and polymethyl methacrylate.

[0012] Preferably, the raw materials include the following parts by weight: 10-14 parts of quartz sand, 5-6 parts of oxides, 5-7 parts of hydroxides, 5-6 parts of nitrates, 5-6 parts of carbonates, 5-6 parts of phosphates, 1-4 parts of lens resins, 1-2 parts of plastics, 1-3 parts of co-solvents, 1-3 parts of clarifiers, 1-1 parts of decolorizers, and 1-5 parts of potassium nitrate.

[0013] A method for making an optical lens, the preparation process of which comprises the following steps: adding quartz sand, hydroxide, nitrate, carbonate and phosphate into a furnace and smelting them at 1400-2000 degrees for 5-10 minutes to obtain a first mixture after smelting, adding resin and plastic into the furnace and smelting them at 1500-2000 degrees for 1-5 minutes to obtain a second mixture, adding the first mixture and the second mixture into the furnace and smelting them at 1600-3000 degrees for 5-10 minutes, adding a solvent into the smelting furnace and smelting them for 10-20 minutes, and then fully smelting the mixture. After refining, a lens mixture is obtained. The sodium oxide in the solvent can reduce the viscosity of the glass during formation, making the glass easy to melt and playing a good fluxing role; tin oxide can increase the chemical stability and mechanical strength of the glass; lead oxide can increase the density and have a special luster; lead can make the glass have a large refractive index and a small scattering rate for light, making the glass more shiny and stable. The obtained lens mixture is added to a mixer, and a clarifier and a decolorizer are added to the mixer at the same time. Some bubbles will appear in the process of glass making, and the bubbles can be removed by a clarifier. A clarifier is an industrial material used to improve transparency or clarity. Its function and usage vary depending on the application field. In glass manufacturing, clarifying agents such as ethanol and propylene glycol are used to maintain or improve the transparency of transparent shampoo. In the glass melting process, clarifying agents such as sulfates, multivalent oxides and halides achieve the effect of clarifying the glass by promoting the rise and discharge of bubbles. They are mainly used to eliminate the undesirable color brought to the glass by impurities in the raw materials, so that the glass appears colorless and transparent. At this time, the mixer is used to mix for 10-20 minutes at a speed of 10-50 revolutions per minute, and then the mixed material is squeezed into the mold by an extruder, and pressed by a press for 10-30 minutes to achieve pressing and forming. At the same time, potassium nitrate solution is added to the inside of the mold to fully contact with the material. Potassium nitrate can make the glass surface harder and more wear-resistant, thereby improving the service life and aesthetics of the glass. A layer of potassium nitrate film is formed on the glass surface, and it is combined with the glass surface through the process of heating and cooling, thereby forming a hard protective layer to ensure the strength of the lens. After the final molding, the material is polished by a grinder at a speed of 200-300 revolutions per minute for 5-10 minutes to form an optical lens.

[0014] Beneficial effects of the present invention: 1. Optical lenses can be obtained by melting and mixing quartz sand, oxides, hydroxides, nitrates, carbonates, phosphates, lens resins and plastics; 2. By adding clarifier and potassium nitrate into the optical lens, the bubbles inside the lens can be effectively reduced. At the same time, potassium nitrate forms a protective layer on the surface of the optical lens, which can effectively protect the optical lens, increase its strength and ensure its service life. The optical lens of the present invention has the effect of effectively reducing bubbles in the lens, and can effectively ensure the strength of the optical lens, and is easy to produce and popularize. BRIEF DESCRIPTION OF THE DRAWINGS

[0015] Figure 1 The working flow chart proposed by the present invention. DETAILED DESCRIPTION

[0016] The present invention will be further explained below in conjunction with specific embodiments.

[0017] Reference Figure 1 , Embodiment 1 In this embodiment, an optical lens is proposed, comprising the following raw materials in parts by weight: 10 parts of quartz sand, 5 parts of oxide, 5 parts of hydroxide, 5 parts of nitrate, 5 parts of carbonate, 5 parts of phosphate, 1 part of lens resin, 1 part of plastic, 1 part of solvent, 1 part of clarifier, 1 part of decolorizer, and 1 part of potassium nitrate.

[0018] The preparation process includes the following steps: adding quartz sand, hydroxide, nitrate, carbonate and phosphate into a furnace and smelting them at 1400 degrees for 5 minutes to obtain a first mixture, and adding resin and plastic into the furnace and smelting them at 1500 degrees for 1 minute to obtain a second mixture. The lens resin is a polymer composite material with strong impact resistance. At this time, the first mixture and the second mixture are added into the furnace and smelted at 1600 degrees for 5 minutes. At the same time, a solvent is added into the smelting furnace during the smelting process and smelted for 10 minutes. At this time, the lens is obtained after sufficient smelting. The mixture, sodium oxide in the solvent can reduce the viscosity of the glass during formation, making the glass easier to melt and playing a good fluxing role; tin oxide can increase the chemical stability and mechanical strength of the glass; lead oxide can increase the density and have a special luster; lead can make the glass have a large refractive index and a small scattering rate for light, making the glass more shiny and stable. The obtained lens mixture is added to the mixer, and clarifiers and decolorizers are added to the mixer at the same time. Some bubbles will appear in the process of glass making, which can be removed by clarifiers. Clarifiers are an industrial material used to improve transparency or clarity, and their functions and usage vary depending on the application field. In glass manufacturing, clarifying agents such as ethanol and propylene glycol are used to maintain or improve the transparency of transparent shampoos. In the glass melting process, clarifying agents such as sulfates, multivalent oxides and halides achieve the effect of clarifying the glass by promoting the rise and discharge of bubbles. They are mainly used to eliminate the undesirable color brought to the glass by impurities in the raw materials, so that the glass appears colorless and transparent. At this time, the mixer is used to mix for 10 minutes at a speed of 10 revolutions per minute, and then the mixed material is squeezed into the mold by an extruder, and pressed by a press for 10 minutes to achieve pressing molding. At the same time, potassium nitrate solution is added to the inside of the mold to fully contact with the material. Potassium nitrate can make the glass surface harder and more wear-resistant, thereby improving the service life and aesthetics of the glass. A layer of potassium nitrate film is formed on the glass surface, and it is combined with the glass surface through a heating and cooling process to form a hard protective layer to ensure the strength of the lens. After the final molding, the material is polished for 5 minutes at a speed of 200 revolutions per minute by a grinder to form an optical lens.

[0019] Reference Figure 1 , Embodiment 2 In this embodiment, an optical lens is proposed, comprising the following raw materials in parts by weight: 14 parts of quartz sand, 7 parts of oxide, 7 parts of hydroxide, 8 parts of nitrate, 7 parts of carbonate, 9 parts of phosphate, 2 parts of lens resin, 3 parts of plastic, 1 part of co-solvent, 2 parts of clarifier, 2 parts of decolorizer, and 4 parts of potassium nitrate.

[0020] A method for making an optical lens comprises the following steps: adding quartz sand, hydroxide, nitrate, carbonate and phosphate into a furnace and smelting them at 1600 degrees for 7 minutes to obtain a first mixture after smelting, and adding resin and plastic into the furnace and smelting them at 1700 degrees for 2 minutes to obtain a second mixture by smelting, wherein the lens resin is a polymer composite material with strong impact resistance, and at this time, the first mixture and the second mixture are added into the furnace and smelted at 2500 degrees for 6 minutes, and at the same time, a solvent is added into the smelting furnace during the smelting process and smelted for 12 minutes, and at this time, after sufficient smelting, a second mixture is obtained. To the lens mixture, sodium oxide in the solvent can reduce the viscosity of the glass during formation, making the glass easier to melt and playing a good fluxing role; tin oxide can increase the chemical stability and mechanical strength of the glass; lead oxide can increase the density and have a special luster; lead can make the glass have a large refractive index and a small scattering rate for light, making the glass more shiny and stable. The obtained lens mixture is added to the mixer, and clarifiers and decolorizers are added to the mixer at the same time. Some bubbles will appear in the process of glass making, which can be removed by clarifiers. Clarifiers are an industrial material used to improve transparency or clarity. Their functions and usage vary depending on the application field. In glass manufacturing, clarifying agents such as ethanol and propylene glycol are used to maintain or improve the transparency of transparent shampoos. In the glass melting process, clarifying agents such as sulfates, multivalent oxides and halides achieve the effect of clarifying the glass by promoting the rise and discharge of bubbles. They are mainly used to eliminate the undesirable color brought to the glass by impurities in the raw materials, so that the glass appears colorless and transparent. At this time, the mixer is used to mix for 16 minutes at a speed of 40 revolutions per minute, and then the mixed material is squeezed into the mold by an extruder, and pressed by a press for 21 minutes to achieve pressing and molding. At the same time, potassium nitrate solution is added to the inside of the mold to fully contact with the material. Potassium nitrate can make the glass surface harder and more wear-resistant, thereby improving the service life and aesthetics of the glass. A layer of potassium nitrate film is formed on the glass surface, and it is combined with the glass surface through a heating and cooling process to form a hard protective layer to ensure the strength of the lens. After the final molding, the material is polished for 8 minutes at a speed of 260 revolutions per minute by a grinder to form an optical lens.

[0021] Reference Figure 1 , Embodiment 3 In this embodiment, an optical lens is proposed, comprising the following raw materials in parts by weight: 11 parts of quartz sand, 6 parts of oxide, 6 parts of hydroxide, 9 parts of nitrate, 8 parts of carbonate, 8 parts of phosphate, 3 parts of lens resin, 2 parts of plastic, 3 parts of solvent, 4 parts of clarifier, 5 parts of decolorizer, and 1 part of potassium nitrate.

[0022] The preparation process includes the following steps: adding quartz sand, hydroxide, nitrate, carbonate and phosphate into a furnace and smelting them at 1800 degrees for 7 minutes to obtain a first mixture, and adding resin and plastic into the furnace and smelting them at 1600 degrees for 2 minutes to obtain a second mixture. The lens resin is a polymer composite material with strong impact resistance. At this time, the first mixture and the second mixture are added into the furnace and smelted at 2000 degrees for 8 minutes. At the same time, a solvent is added into the smelting furnace during the smelting process and smelted for 17 minutes. At this time, the lens is obtained after sufficient smelting. The mixture, sodium oxide in the solvent can reduce the viscosity of the glass during formation, making the glass easier to melt and playing a good fluxing role; tin oxide can increase the chemical stability and mechanical strength of the glass; lead oxide can increase the density and have a special luster; lead can make the glass have a large refractive index and a small scattering rate for light, making the glass more shiny and stable. The obtained lens mixture is added to the mixer, and clarifiers and decolorizers are added to the mixer at the same time. Some bubbles will appear in the process of glass making, which can be removed by clarifiers. Clarifiers are an industrial material used to improve transparency or clarity, and their functions and usage vary depending on the application field. In glass manufacturing, clarifying agents such as ethanol and propylene glycol are used to maintain or improve the transparency of transparent shampoos. In the glass melting process, clarifying agents such as sulfates, multivalent oxides and halides achieve the effect of clarifying the glass by promoting the rise and discharge of bubbles. They are mainly used to eliminate the undesirable color brought to the glass by impurities in the raw materials, so that the glass appears colorless and transparent. At this time, the mixer is used to mix for 19 minutes at a speed of 20 revolutions per minute, and then the mixed material is squeezed into the mold by an extruder, and pressed by a press for 25 minutes to achieve pressing molding. At the same time, potassium nitrate solution is added to the inside of the mold to fully contact with the material. Potassium nitrate can make the glass surface harder and more wear-resistant, thereby improving the service life and aesthetics of the glass. A layer of potassium nitrate film is formed on the glass surface, and it is combined with the glass surface through a heating and cooling process to form a hard protective layer to ensure the strength of the lens. After the final molding, the material is polished for 8 minutes at a speed of 2400 revolutions per minute by a grinder to form an optical lens.

[0023] Reference Figure 1 , Embodiment 4 In this embodiment, an optical lens is proposed, comprising the following raw materials in parts by weight: 17 parts of quartz sand, 9 parts of oxides, 9 parts of hydroxides, 9 parts of nitrates, 6 parts of carbonates, 6 parts of phosphates, 3 parts of lens resins, 1 part of plastics, 1 part of solvents, 2 parts of clarifiers, 4 parts of decolorizers, and 5 parts of potassium nitrate.

[0024] The preparation process includes the following steps: adding quartz sand, hydroxide, nitrate, carbonate and phosphate into a furnace and smelting them at 1800 degrees for 7 minutes to obtain a first mixture, and adding resin and plastic into the furnace and smelting them at 1500 degrees for 2 minutes to obtain a second mixture. The lens resin is a polymer composite material with strong impact resistance. At this time, the first mixture and the second mixture are added into the furnace and smelted at 2900 degrees for 8 minutes. At the same time, a solvent is added into the smelting furnace during the smelting process and smelted for 15 minutes. At this time, the lens is obtained after sufficient smelting. The mixture, sodium oxide in the solvent can reduce the viscosity of the glass during formation, making the glass easier to melt and playing a good fluxing role; tin oxide can increase the chemical stability and mechanical strength of the glass; lead oxide can increase the density and have a special luster; lead can make the glass have a large refractive index and a small scattering rate for light, making the glass more shiny and stable. The obtained lens mixture is added to the mixer, and clarifiers and decolorizers are added to the mixer at the same time. Some bubbles will appear in the process of glass making, which can be removed by clarifiers. Clarifiers are an industrial material used to improve transparency or clarity, and their functions and usage vary depending on the application field. In glass manufacturing, clarifying agents such as ethanol and propylene glycol are used to maintain or improve the transparency of transparent shampoos. In the glass melting process, clarifying agents such as sulfates, multivalent oxides and halides achieve the effect of clarifying the glass by promoting the rise and discharge of bubbles. They are mainly used to eliminate the undesirable color brought to the glass by impurities in the raw materials, so that the glass appears colorless and transparent. At this time, the mixer is used to mix for 16 minutes at a speed of 21 revolutions per minute, and then the mixed material is squeezed into the mold by an extruder, and pressed by a press for 30 minutes to achieve pressing molding. At the same time, potassium nitrate solution is added to the inside of the mold to fully contact with the material. Potassium nitrate can make the glass surface harder and more wear-resistant, thereby improving the service life and aesthetics of the glass. A layer of potassium nitrate film is formed on the glass surface, and it is combined with the glass surface through a heating and cooling process to form a hard protective layer to ensure the strength of the lens. After the final molding, the material is polished for 8 minutes at a speed of 2600 revolutions per minute by a grinder to form an optical lens.

[0025] Reference Figure 1 Embodiment 5 In this embodiment, an optical lens is proposed, comprising the following raw materials in parts by weight: 20 parts of quartz sand, 10 parts of oxide, 10 parts of hydroxide, 10 parts of nitrate, 10 parts of carbonate, 10 parts of phosphate, 5 parts of lens resin, 5 parts of plastic, 5 parts of solvent, 5 parts of clarifier, 5 parts of decolorizer, and 5 parts of potassium nitrate.

[0026] The preparation process comprises the following steps: adding quartz sand, hydroxide, nitrate, carbonate and phosphate into a furnace and smelting them at 2000 degrees for 10 minutes to obtain a first mixture, and adding resin and plastic into the furnace and smelting them at 2000 degrees for 5 minutes to obtain a second mixture. Lens resin is a polymer composite material with strong impact resistance. At this time, the first mixture and the second mixture are added into the furnace and smelted at 3000 degrees for 10 minutes. At the same time, a solvent is added into the smelting furnace during the smelting process and smelted for 20 minutes. At this time, the lens is obtained after sufficient smelting. The lens mixture, sodium oxide in the solvent can reduce the viscosity during glass formation, making the glass easier to melt and playing a good fluxing role; tin oxide can increase the chemical stability and mechanical strength of the glass; lead oxide can increase the density and have a special luster; lead can make the glass have a large refractive index and a small scattering rate for light, making the glass more shiny and stable. The obtained lens mixture is added to the mixer, and clarifiers and decolorizers are added to the mixer at the same time. Some bubbles will appear in the process of glass making, which can be removed by clarifiers. Clarifiers are an industrial material used to improve transparency or clarity. Their functions and usage vary depending on the application field. In glass manufacturing, clarifying agents such as ethanol and propylene glycol are used to maintain or improve the transparency of transparent shampoos. In the glass melting process, clarifying agents such as sulfates, multivalent oxides and halides achieve the effect of clarifying the glass by promoting the rise and discharge of bubbles. They are mainly used to eliminate the undesirable color brought to the glass by impurities in the raw materials, so that the glass appears colorless and transparent. At this time, the mixer is used to mix for 20 minutes at a speed of 50 revolutions per minute, and then the mixed material is squeezed into the mold by an extruder, and pressed by a press for 30 minutes to achieve pressing molding. At the same time, potassium nitrate solution is added to the inside of the mold to fully contact with the material. Potassium nitrate can make the glass surface harder and more wear-resistant, thereby improving the service life and aesthetics of the glass. A layer of potassium nitrate film is formed on the glass surface, and it is combined with the glass surface through a heating and cooling process to form a hard protective layer to ensure the strength of the lens. After the final molding, the material is polished by a grinder at a speed of 300 revolutions per minute for 10 minutes to form an optical lens.

[0027] Comparing the conventional premixed mortar with the optical lenses prepared in Examples 1 to 5, the optical lenses prepared in Examples 1 to 5 are as follows: Example one two three Four five Increased compressive strength 20% 36% 41% 33% 50% Mirror bubble reduction 80% 80% 20% 60% 90% It can be seen from the above table that the optical lens proposed by the present invention has obvious improvements, and implementation five is the best implementation example.

[0028] The above description is only a preferred specific implementation manner of the present invention, but the protection scope of the present invention is not limited thereto. Any technician familiar with the technical field can make equivalent replacements or changes according to the technical scheme and inventive concept of the present invention within the technical scope disclosed by the present invention, which should be covered by the protection scope of the present invention.

Claims

1. An optical lens, characterized in that: The invention comprises the following raw materials in parts by weight: 10-20 parts of quartz sand, 5-10 parts of oxide, 5-10 parts of hydroxide, 5-10 parts of nitrate, 5-10 parts of carbonate, 5-10 parts of phosphate, 1-5 parts of lens resin, 1-5 parts of plastic, 1-5 parts of co-solvent, 1-5 parts of clarifier, 1-5 parts of decolorizer and 1-5 parts of potassium nitrate.

2. The method for manufacturing an optical lens according to claim 1, characterized in that: The following steps are involved: S1: adding quartz sand, hydroxide, nitrate, carbonate and phosphate into a furnace for smelting to obtain a first mixture; S2: adding the resin and the plastic into a melting furnace for melting, and obtaining a second mixture by melting; S3: At this time, the first mixture and the second mixture are added into the furnace for smelting; S4: adding a solvent into the melting furnace during the melting process, and obtaining a lens mixture after sufficient melting; S5: adding the obtained lens mixture into a mixer, adding a clarifying agent and a decolorizing agent into the mixer, and then fully mixing them through the mixer; S6: The mixed material is then squeezed into a mold by an extruder, and pressed into shape by a press, and potassium nitrate solution is added into the mold to fully contact with the material; S7: After the final shaping, the material is polished by a grinder to form an optical lens.

3. An optical lens according to claim 1, characterized in that: The auxiliary solvent is prepared by mixing sodium oxide, potassium oxide, lead oxide, calcium oxide and barium oxide.

4. An optical lens according to claim 1, characterized in that: The clarifier is prepared by mixing arsenic oxide, antimony oxide and nitrate salt.

5. An optical lens according to claim 1, characterized in that: The decolorizing agent is made of tin oxide, antimony oxide and phosphate.

6. An optical lens according to claim 1, characterized in that: The resin is prepared by mixing polycarbonate, polystyrene, polyurethane, epoxy resin and polymethyl methacrylate.

7. An optical lens according to claim 1, characterized in that: The invention comprises the following raw materials in parts by weight: 10-14 parts of quartz sand, 5-6 parts of oxide, 5-7 parts of hydroxide, 5-6 parts of nitrate, 5-6 parts of carbonate, 5-6 parts of phosphate, 1-4 parts of lens resin, 1-2 parts of plastic, 1-3 parts of co-solvent, 1-3 parts of clarifier, 1-1 parts of decolorizer and 1-5 parts of potassium nitrate.

8. The method for manufacturing an optical lens according to claim 1, characterized in that: The preparation process comprises the following steps: adding quartz sand, hydroxide, nitrate, carbonate and phosphate into a furnace and smelting them at 1400-2000 degrees for 5-10 minutes to obtain a first mixture, adding resin and plastic into the furnace and smelting them at 1500-2000 degrees for 1-5 minutes to obtain a second mixture, adding the first mixture and the second mixture into the furnace and smelting them at 1600-3000 degrees for 5-10 minutes, and adding a solvent into the smelting furnace during the smelting process and smelting for 10-20 minutes. Refining, at this time, after sufficient melting, a lens mixture is obtained, the obtained lens mixture is added into a mixer, and a clarifier and a decolorizer are added into the mixer at the same time, and the mixer is used to mix for 10-20 minutes at a speed of 10-50 revolutions per minute, and then the mixed material is squeezed into a mold by an extruder, and pressed by a press for 10-30 minutes to achieve compression molding, and potassium nitrate solution is added inside the mold to fully contact with the material, and finally after molding, the material is polished by a grinder at a speed of 200-300 revolutions per minute for 5-10 minutes to form an optical lens.