Trench gate device and preparation method thereof

By forming doped regions and communication regions on the substrate in the trench gate device and transferring high electric fields to the PN junction region, the problem of early breakdown of gate dielectric layer during the device withstand voltage is solved, and the long-term reliability of the device is improved.

CN119008671APending Publication Date: 2024-11-22ALKAIDSEMI (SHANGHAI) TECHNOLOGIES CORP
View PDF 5 Cites 0 Cited by

Patent Information

Application Number
CN202411108349.7
Authority / Receiving Office
CN · China
Patent Type
Applications(China)
Current Assignee / Owner
Filing Date
2024-08-13
Publication Date
2024-11-22

AI Technical Summary

Technical Problem

During the withstand voltage process of the trench gate device, the gate dielectric layer is prone to premature breakdown, affecting the long-term reliability of the device.

Method used

The surface layer on the substrate forms a spaced trench gate structure, and a doping region is formed between two adjacent trench gate structures. The bottom surface of the doping region is lower than the bottom surface of the trench gate structure and extends to the trench gate along the side wall. Below the structure, the well region and the doped region are connected through the communication region and electrically connected to the upper electrode, transferring the high electric field at the bottom of the trench gate structure to the PN junction region between the doped region and the substrate.

Benefits of technology

It effectively reduces the electric field strength at the bottom of the trench gate structure, avoids early breakdown of the gate dielectric layer during the device withstand voltage, and improves the long-term reliability of the device.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure CN119008671A_ABST
    Figure CN119008671A_ABST
Patent Text Reader

Abstract

The invention provides a trench gate device and a preparation method thereof, the trench gate device comprises a substrate, a trench gate structure, a doped region, a well region, a source region, an interlayer dielectric layer, a communication region, a contact region, an upper / lower electrode and a gate, the trench gate structure is located on the upper surface layer of the substrate; the doped region is located in the substrate between two adjacent trench gate structures, and the bottom surface of the doped region is lower than the bottom surfaces of the trench gate structures; the well region is located on the upper surface of the substrate; the source region is located on the well region upper surface layer; the interlayer dielectric layer covers the substrate and the upper surface of the trench gate structure; an upper electrode contact hole penetrating through the interlayer dielectric layer is formed right above the doped region, and the bottom surface of the upper electrode contact hole is exposed out of the source region; the communicating region communicates the doped region with the well region; the contact region penetrates through the source region; the upper electrode is filled in the upper electrode contact hole, the gate is electrically connected with the trench gate structure, and the lower electrode is located on the back of the substrate. The side wall of the trench gate structure extends to the lower part of the trench gate structure, and the doped region is communicated with the well region through the communication region, so that the gate dielectric layer is prevented from being broken down in advance, and the reliability of the device is improved.
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] The invention belongs to the field of semiconductor integrated circuit manufacturing and relates to a trench gate device and a preparation method thereof. Background Art

[0002] Power MOSFET (metal-oxide semiconductor field effect transistor, MOS for short) and IGBT (insulated gate bipolar transistor) devices are widely used in power electronics due to their fast switching speed and low driving loss, and act as switching components. As an important component of power devices, trench gate power MOS and IGBT devices change the conductive channel in the device from horizontal to vertical, which effectively saves the device area and improves the power density of the device. At the same time, due to the setting of the trench gate, the JFET effect of the device can be eliminated, the input capacitance of the device can be reduced, the switching rate of the device can be increased, and the switching loss of the device can be reduced. However, due to the structural limitations of the trench gate, when the trench gate is drawn out in the device, the bottom of the trench gate will have a high electric field during the device withstand voltage process, which is easy to cause the gate oxide layer at the bottom of the trench gate to break down prematurely, and then the device fails, affecting the long-term reliability of the device.

[0003] Therefore, there is an urgent need to find a method for preparing a trench gate device that can prevent the gate dielectric layer at the bottom of the trench gate structure from being broken down prematurely during the device withstand voltage period. Summary of the invention

[0004] In view of the above-mentioned shortcomings of the prior art, an object of the present invention is to provide a trench gate device and a method for preparing the same, so as to solve the problem in the prior art that the gate dielectric layer at the bottom of the trench gate of the trench gate device is easily broken down prematurely due to the influence of high electric field.

[0005] To achieve the above object and other related objects, the present invention provides a method for preparing a trench gate device, comprising the following steps:

[0006] A first conductive type substrate is provided, a plurality of trench gate structures are formed on the upper surface of the substrate, and a second conductive type doped region is formed in the substrate between two adjacent trench gate structures, wherein the doped region is spaced from the trench gate structure by a preset distance, and the bottom surface of the doped region is lower than the bottom surface of the trench gate structure;

[0007] A second conductive type well region and a first conductive type source region located on the upper surface layer of the well region are formed on the upper surface layer of the substrate between two adjacent trench gate structures, and the doped region is spaced a preset distance from the well region;

[0008] forming an interlayer dielectric layer covering the substrate and the upper surface of the trench gate structure, and forming an upper electrode contact hole penetrating the interlayer dielectric layer and exposing the source region at the bottom, wherein the upper electrode contact hole is located directly above the doped region;

[0009] A second conductive type connection region connecting the doped region and the well region and a second conductive type contact region penetrating the source region are formed based on the upper electrode contact hole, and the contact region is spaced a preset distance from the trench gate structure;

[0010] An upper electrode is formed to fill the upper electrode contact hole and is electrically connected to the source region and the contact region, a gate is formed to be electrically connected to the trench gate structure, and a lower electrode is formed on the back side of the substrate.

[0011] Optionally, the trench gate structure includes a gate trench, a gate dielectric layer covering the bottom surface and inner wall of the gate trench, and a gate conductive layer filling the gate trench, the gate dielectric layer wraps the side walls and bottom surface of the gate conductive layer, the gate trench is embedded in the substrate, and the gate conductive layer is electrically connected to the gate.

[0012] Optionally, after forming the interlayer dielectric layer and before forming the upper electrode, the method further includes forming a gate contact hole penetrating the interlayer dielectric layer, wherein the bottom surface of the gate contact hole exposes the gate conductive layer.

[0013] Optionally, an upper surface of the doped region is higher than a bottom surface of the trench gate structure.

[0014] Optionally, the sidewalls of the doped region extend to below the trench gate structure.

[0015] Optionally, a preset distance is provided between a sidewall of the connecting region and the trench gate structure.

[0016] Optionally, the contact region is connected to the well region and has a bottom surface no lower than a bottom surface of the well region.

[0017] Optionally, after forming the upper electrode and the gate and before forming the lower electrode, the method further includes forming a first conductive type buffer zone on the lower surface layer of the substrate, and the lower electrode is electrically connected to the buffer zone.

[0018] Optionally, after forming the upper electrode and the gate and before forming the lower electrode, the method further includes forming a first conductive type buffer region and a second conductive type collector region in sequence on the lower surface layer of the substrate, wherein the collector region is located on the lower surface layer of the buffer region, and the lower electrode is at least electrically connected to the collector region.

[0019] The present invention also provides a trench gate device, comprising:

[0020] a first conductive type substrate;

[0021] A plurality of trench gate structures arranged at intervals are located on the upper surface layer of the substrate;

[0022] A second conductive type doped region, located in the substrate between two adjacent trench gate structures and spaced apart from the trench gate structure by a preset distance, wherein a bottom surface of the doped region is lower than a bottom surface of the trench gate structure;

[0023] A second conductive type well region is located on the upper surface layer of the substrate between two adjacent trench gate structures;

[0024] A first conductive type source region is located on the upper surface of the well region, and the doped region is spaced a preset distance from the well region;

[0025] an interlayer dielectric layer, covering the substrate and the upper surface of the trench gate structure, wherein the interlayer dielectric layer is provided with an upper electrode contact hole penetrating the interlayer dielectric layer and exposing the source region at the bottom, and the upper electrode contact hole is located directly above the doped region;

[0026] A second conductive type connection region is located in the substrate between the well region and the doping region and connects the doping region and the well region;

[0027] A second conductive type contact region, extending through the source region;

[0028] An upper electrode, a gate and a lower electrode, wherein the upper electrode fills the upper electrode contact hole and is electrically connected to the source region and the contact region, the gate is electrically connected to the trench gate structure, and the lower electrode is located on the back side of the substrate.

[0029] As described above, the trench gate device and the preparation method thereof of the present invention form the doping region in the substrate between two adjacent trench gate structures after forming the trench gate structure on the upper surface layer of the substrate, wherein the doping region is spaced apart from the trench gate structure by a preset distance and has a bottom surface lower than the bottom surface of the trench gate structure, and the sidewalls of the doping region along the arrangement direction extend to the bottom of the trench gate structure, and the well region is connected to the doping region by using the connecting region. Since the contact region electrically connected to the upper electrode and having the same conductivity type is connected to the well region, the high electric field at the bottom of the trench gate structure can be transferred to the PN junction region between the doping region and the substrate, thereby effectively reducing the electric field strength at the bottom of the trench gate structure, so that the bottom of the trench gate structure is protected by the doping region, avoiding premature breakdown of the gate dielectric layer at the bottom of the trench gate structure during the device withstand voltage period, improving the long-term reliability of the device, and having high industrial utilization value. BRIEF DESCRIPTION OF THE DRAWINGS

[0030] Figure 1Shown is a process flow chart of a method for preparing a trench gate device of the present invention.

[0031] Figure 2 The cross-sectional structure schematic diagram shows a substrate in the method for preparing a trench gate device of the present invention.

[0032] Figure 3 It is a schematic diagram of the cross-sectional structure after forming the doping region in the method for preparing the trench gate device of the present invention.

[0033] Figure 4 It is a schematic diagram showing the cross-sectional structure after forming the source region in the method for preparing the trench gate device of the present invention.

[0034] Figure 5 It is a schematic diagram showing the cross-sectional structure of the method for preparing the trench gate device of the present invention after forming the upper electrode contact hole.

[0035] Figure 6 It is a schematic diagram showing the cross-sectional structure after forming the connection area in the method for preparing the trench gate device of the present invention.

[0036] Figure 7 It is a schematic diagram showing the cross-sectional structure after forming the contact region in the method for preparing the trench gate device of the present invention.

[0037] Figure 8 It is a schematic diagram showing the cross-sectional structure of the method for preparing the trench gate device of the present invention after forming the upper electrode.

[0038] Fig. 9 It shows a schematic cross-sectional structure diagram of the method for preparing the trench gate device of the present invention after forming the lower electrode.

[0039] Fig.10 Another schematic diagram of a cross-sectional structure after forming a lower electrode in the method for preparing a trench gate device of the present invention is shown.

[0040] Description of Figure Numbers

[0041] 1 Substrate

[0042] 11 Doping region

[0043] 12 Well region

[0044] 13 Source area

[0045] 14 Connected Area

[0046] 15 Contact area

[0047] 16a, 16b buffer

[0048] 17 Collector area

[0049] 2 Trench Gate Structure

[0050] 21 Gate trench

[0051] 22. Gate dielectric layer

[0052] 23. Gate conductive layer

[0053] 3 Interlayer dielectric layer

[0054] 31 Upper electrode contact hole

[0055] 4 Upper electrode

[0056] 5 Lower electrode DETAILED DESCRIPTION

[0057] The following describes the embodiments of the present invention through specific examples, and those skilled in the art can easily understand other advantages and effects of the present invention from the contents disclosed in this specification. The present invention can also be implemented or applied through other different specific embodiments, and the details in this specification can also be modified or changed in various ways based on different viewpoints and applications without departing from the spirit of the present invention.

[0058] See also Figures 1 to 10 It should be noted that the illustrations provided in this embodiment are only used to illustrate the basic concept of the present invention in a schematic manner, and the drawings only show components related to the present invention rather than being drawn according to the number, shape and size of components in actual implementation. In actual implementation, the type, quantity and proportion of each component may be changed arbitrarily, and the component layout may also be more complicated.

[0059] Embodiment 1

[0060] This embodiment provides a method for preparing a trench gate device, such as Figure 1 FIG. 1 is a process flow chart of the method for preparing the trench gate device, comprising the following steps:

[0061] S1: providing a first conductive type substrate, forming a plurality of trench gate structures spaced apart on an upper surface layer of the substrate, and forming a second conductive type doped region in the substrate between two adjacent trench gate structures, wherein the doped region is spaced apart from the trench gate structure by a preset distance, and a bottom surface of the doped region is lower than a bottom surface of the trench gate structure;

[0062] S2: forming a second conductive type well region and a first conductive type source region located on the upper surface layer of the well region between two adjacent trench gate structures, wherein the doped region is spaced a preset distance from the well region;

[0063] S3: forming an interlayer dielectric layer covering the substrate and the upper surface of the trench gate structure, and forming an upper electrode contact hole penetrating the interlayer dielectric layer and exposing the source region at the bottom, wherein the upper electrode contact hole is located directly above the doped region;

[0064] S4: forming a second conductive type connection region connecting the doped region and the well region and a second conductive type contact region penetrating the source region based on the upper electrode contact hole, and the contact region is spaced a preset distance from the trench gate structure;

[0065] S5: forming an upper electrode filling the upper electrode contact hole and electrically connected to the source region and the contact region, forming a gate electrically connected to the trench gate structure, and forming a lower electrode on the back side of the substrate.

[0066] See also Figures 2 to 4 , performing step S1 and step S2: providing a first conductive type substrate 1, forming a plurality of trench gate structures 2 spaced apart on the upper surface of the substrate 1, and forming a second conductive type doping region 11 in the substrate 1 between two adjacent trench gate structures 2, wherein the doping region 11 is spaced apart from the trench gate structure 2 by a preset distance, and the bottom surface of the doping region 11 is lower than the bottom surface of the trench gate structure 2; forming a second conductive type well region 12 and a first conductive type source region 13 located on the upper surface of the well region 12 on the upper surface of the substrate 1 between two adjacent trench gate structures 2, wherein the doping region 11 is spaced apart from the well region 12 by a preset distance.

[0067] Specifically, the first conductivity type includes one of N type or P type, the second conductivity type includes one of N type or P type, and the first conductivity type is opposite to the second conductivity type. In this embodiment, the first conductivity type is N type, and the second conductivity type is P type.

[0068] Specifically, Figure 2 As shown, it is a schematic diagram of the cross-sectional structure of the substrate 1. Under the condition of ensuring the device performance, the size, shape, thickness and doping concentration of the substrate 1 can be selected according to actual conditions and are not limited here.

[0069] Specifically, under the condition of ensuring the device performance, the number of the trench gate structures 2 and the distance between two adjacent trench gate structures 2 can be selected according to actual conditions and are not limited here.

[0070] As an example, the trench gate structure 2 includes a gate trench 21, a gate dielectric layer 22 covering the bottom surface and inner wall of the gate trench 21, and a gate conductive layer 23 filling the gate trench 21, the gate dielectric layer 22 wraps the side walls and bottom surface of the gate conductive layer 23, the gate trench 21 is embedded in the substrate 1, and the gate conductive layer 23 is electrically connected to the gate.

[0071] Specifically, forming the gate trench 21 includes the following steps: forming a patterned first shielding layer on the upper surface of the substrate 1 , and forming the gate trench 21 based on the patterned first shielding layer.

[0072] Specifically, the material of the first shielding layer includes photoresist or other suitable photoresist materials; the method of forming the patterned first shielding layer is the commonly used photoresist coating, drying, exposure, and development process, which will not be repeated here.

[0073] Specifically, the method of forming the gate trench 21 includes dry etching, wet etching or other suitable methods.

[0074] Specifically, the method of forming the gate dielectric layer 22 includes thermal oxidation, chemical vapor deposition, physical vapor deposition or other suitable methods.

[0075] Specifically, under the condition of ensuring the device performance, the thickness of the gate dielectric layer 22 can be selected according to actual conditions and is not limited here.

[0076] Specifically, the method of forming the gate conductive layer 23 includes chemical vapor deposition, physical vapor deposition or other suitable methods.

[0077] Specifically, Figure 3 , which is a schematic diagram of a cross-sectional structure after the doping region 11 is formed, and the method for forming the doping region 11 includes ion implantation or other suitable methods. In this embodiment, ion implantation is performed in the substrate 1 between two adjacent trench gate structures 2, and the position of the upper surface of the region doped with ions is not lower than the bottom surface of the gate trench 21. After the ion implantation is completed, the doped substrate 1 is treated for a preset time using a high temperature well-driving process to form the doping region 11.

[0078] As an example, the sidewall of the doping region 11 extends to below the trench gate structure 2 to protect the bottom of the trench gate structure 2. In this embodiment, the sidewall of the doping region 11 along the arrangement direction extends to below the trench gate structure 2.

[0079] Specifically, while ensuring device performance, the distance between the doping region 11 and the well region 12 can be selected according to actual conditions and is not limited here; the distance between two adjacent doping regions 11 can be selected according to actual conditions and is not limited here.

[0080] As an example, the upper surface of the doped region 11 is higher than the bottom surface of the trench gate structure 2 .

[0081] Specifically, under the condition of ensuring device performance, the upper surface of the doped region 11 may also be lower than the bottom surface of the trench gate structure 2 .

[0082] Specifically, Figure 4 , which is a schematic diagram of the cross-sectional structure after the source region 13 is formed, the method for forming the well region 12 includes ion implantation or other suitable methods; the method for forming the source region 13 includes ion implantation or other suitable methods.

[0083] Please see again Figures 5 to 10 , performing the step S3, the step S4 and the step S5: forming an interlayer dielectric layer 3 covering the upper surface of the substrate 1 and the trench gate structure 2, and forming an upper electrode contact hole 31 penetrating the interlayer dielectric layer 3 and exposing the source region 13 on the bottom surface, wherein the upper electrode contact hole 31 is located directly above the doped region 11; based on the upper electrode contact hole 31, a second conductive type connecting region 14 connecting the doped region 11 and the well region 12 and a second conductive type contact region 15 penetrating the source region 13 are formed, and the contact region 15 is spaced a preset distance from the trench gate structure 2; forming an upper electrode 4 filling the upper electrode contact hole 31 and electrically connected to the source region 13 and the contact region 15, forming a gate (not shown) electrically connected to the trench gate structure 2, and forming a lower electrode 5 on the back side of the substrate 1.

[0084] Specifically, the method of forming the interlayer dielectric layer 3 includes chemical vapor deposition, physical vapor deposition or other suitable methods.

[0085] Specifically, under the condition of ensuring the device performance, the thickness of the interlayer dielectric layer 3 can be selected according to actual conditions and is not limited here.

[0086] Specifically, Figure 5 , which is a schematic diagram of the cross-sectional structure after the upper electrode contact hole 31 is formed. The method of forming the upper electrode contact hole 31 includes dry etching, wet etching or other suitable methods.

[0087] Specifically, the depth of the upper electrode contact hole 31 is not less than the thickness of the interlayer dielectric layer 3 and the bottom surface is higher than the bottom surface of the source region 13, that is, the bottom surface of the upper electrode contact hole 31 can be flush with the upper surface of the substrate 1, or can extend into the source region 13. The depth here refers to the distance from the bottom surface of the upper electrode contact hole 31 to the opening of the upper electrode contact hole 31 (that is, the upper surface of the interlayer dielectric layer 3). In this embodiment, the bottom surface of the upper electrode contact hole 31 extends into the source region 13.

[0088] As an example, Figure 6 As shown, it is a schematic diagram of the cross-sectional structure after the connection area 14 is formed, and the side wall of the connection area 14 is spaced from the trench gate structure 2 by a preset distance so that the device can be turned on through the gap between the connection area 14 and the trench gate structure 2 and the conductive channel controlled by the trench gate structure 2.

[0089] Specifically, the method for forming the connection region 14 includes ion implantation or other suitable methods. In this embodiment, boron ions with a preset energy and a preset dose are implanted into the substrate 1 based on the upper electrode contact hole 31 to form the connection region 14 .

[0090] Specifically, Figure 7 FIG. 1 is a schematic diagram of a cross-sectional structure after forming the contact area 15. The method for forming the contact area 15 includes ion implantation or other suitable methods. In this embodiment, a preset dose of BF is implanted into the substrate 1 based on the upper electrode contact hole 31. 2+ To form the contact hole 15 .

[0091] As an example, the contact region 15 is connected to the well region 12 and has a bottom surface no lower than a bottom surface of the well region 12 .

[0092] Specifically, the contact type between the contact region 15 and the upper electrode 4 is ohmic contact, and the doping concentration of the contact region 15 is greater than the doping concentration of the well region 12 .

[0093] Specifically, Figure 8 As shown, it is a schematic diagram of the cross-sectional structure after the upper electrode 4 is formed. The method of forming the upper electrode 4 includes magnetron sputtering, physical vapor deposition, chemical vapor deposition, metal compound vapor deposition, molecular beam epitaxy, atomic vapor deposition, atomic layer deposition or other suitable methods.

[0094] As an example, after forming the interlayer dielectric layer 3 and before forming the upper electrode 4, a step of forming a gate contact hole (not shown) penetrating the interlayer dielectric layer 3 is also included, and the bottom surface of the gate contact hole exposes the gate conductive layer 23.

[0095] Specifically, the method of forming the gate contact hole includes dry etching, wet etching or other suitable methods.

[0096] Specifically, the gate fills the gate contact hole to achieve electrical connection between the gate conductive layer 23 and the gate.

[0097] Specifically, the method of forming the gate includes magnetron sputtering, physical vapor deposition, chemical vapor deposition, metal compound vapor deposition, molecular beam epitaxy, atomic vapor deposition, atomic layer deposition or other suitable methods.

[0098] As an example, Fig. 9 As shown, it is a schematic diagram of a cross-sectional structure after forming the lower electrode 5. After forming the upper electrode 4 and the gate and before forming the lower electrode 5, it also includes the step of forming a first conductive type buffer zone 16a on the lower surface layer of the substrate 1. The lower electrode 5 is electrically connected to the buffer zone 16a, that is, the manufactured device is a trench gate MOS device.

[0099] Specifically, when the manufactured device is a trench gate MOS device, the contact type between the buffer region 16a and the lower electrode 5 is an ohmic contact, the lower electrode 5 is the drain of the device, and the upper electrode 4 is the source of the device.

[0100] Specifically, the method of forming the buffer region 16 a includes ion implantation or other suitable methods.

[0101] As an example, Fig.10 As shown, it is another schematic diagram of the cross-sectional structure after the lower electrode 5 is formed. After the upper electrode 4 and the gate are formed and before the lower electrode 5 is formed, it also includes the steps of sequentially forming a first conductive type buffer region 16b and a second conductive type collector region 17 on the lower surface layer of the substrate 1. The collector region 17 is located on the lower surface layer of the buffer region 16a. The lower electrode 5 is at least electrically connected to the collector region 17, that is, the manufactured device is a trench gate IGBT device.

[0102] Specifically, when the manufactured device is a trench gate IGBT device, the upper electrode 4 is the emitter of the device, the lower electrode 5 is the collector of the device, and the contact type between the collector region 17 and the lower electrode 5 is an ohmic contact.

[0103] Specifically, under the condition of ensuring the device performance, the trench gate IGBT device can be a common IGBT device or a reverse conducting IGBT device.

[0104] Specifically, the method of forming the buffer region 16 b includes ion implantation or other suitable methods; the method of forming the collector region 17 includes ion implantation or other suitable methods.

[0105] Specifically, the back side of the lower electrode 5 located in the substrate 1 refers to the side opposite to the formed interlayer dielectric layer 3, and the method of forming the lower electrode 5 includes magnetron sputtering, physical vapor deposition, chemical vapor deposition, metal compound vapor deposition, molecular beam epitaxy, atomic vapor deposition, atomic layer deposition or other suitable methods.

[0106] Specifically, the doping region 11 is formed in the substrate 1 between two adjacent trench gate structures, and the doping region 11 is connected to the well region 12 through the connecting region 14. The sidewall of the doping region 11 along the arrangement direction extends to the bottom of the trench gate structure 2. Since the contact region 15 is electrically connected to the upper electrode 4 and connected to the well region 12, the high electric field at the bottom of the trench gate structure 2 is transferred to the PN junction region between the doping region 11 and the substrate 1, thereby effectively reducing the electric field strength at the bottom of the trench gate structure 2, alleviating the influence of the high electric field on the gate dielectric layer 22, avoiding the premature breakdown of the gate dielectric layer 22 at the bottom of the trench gate structure 2 during the device withstand voltage period, and improving the long-term reliability of the device.

[0107] The preparation method of the trench gate device of the present embodiment improves the manufacturing process of the trench gate device. After the trench gate structure 2 is formed, the doping region 11 is formed in the substrate 1 between two adjacent trench gate structures 2. The doping region 11 is spaced apart from the trench gate structure 2 by a preset distance. The bottom surface of the trench gate structure 2 is higher than the bottom surface of the doping region 11, and the sidewall of the doping region 11 along the arrangement direction extends to the bottom of the trench gate structure 2. Then, the well region 12 and the doping region 11 are connected through the connecting region 14, and the contact region 15 is connected to the well region 12 and electrically connected to the upper electrode 4. Then, the high electric field at the bottom of the trench gate structure 2 is transferred to the PN junction region between the doping region 11 and the substrate 1, thereby effectively reducing the electric field strength at the bottom of the trench gate structure 2, avoiding the premature breakdown of the gate dielectric layer 22 at the bottom of the trench gate structure 2 during the withstand voltage period, and improving the long-term reliability of the device.

[0108] Embodiment 2

[0109] This embodiment provides a trench gate device, such as Fig. 9 and Fig.10As shown, there are schematic diagrams of a cross-sectional structure of the trench gate device and another schematic diagram of a cross-sectional structure of the trench gate device, respectively, including a first conductive type substrate 1, a trench gate structure 2, a second conductive type doped region 11, a second conductive type well region 12, a first conductive type source region 13, an interlayer dielectric layer 3, a second conductive type connection region 14, a second conductive type contact region 15, an upper electrode 4, a gate and a lower electrode 5, wherein a plurality of the trench gate structures 2 arranged at intervals are located on the upper surface layer of the substrate 1; the doped region 11 is located in the substrate 1 between two adjacent trench gate structures 2 and is spaced from the trench gate structure 2 by a preset distance, and the bottom surface of the doped region 11 is lower than the bottom surface of the trench gate structure 2; the well region 12 is located on the upper surface layer of the substrate 1 between two adjacent trench gate structures 2 ; The source region 13 is located on the upper surface of the well region 12, and the doping region 11 is spaced from the well region 12 by a preset distance; the interlayer dielectric layer 3 covers the substrate 1 and the upper surface of the trench gate structure 2, and an upper electrode contact hole 31 is provided in the interlayer dielectric layer 3, which penetrates the interlayer dielectric layer 3 and exposes the source region 13 on the bottom surface, and the upper electrode contact hole 31 is located directly above the doping region 11; the connecting region 14 is located in the substrate 1 between the well region 12 and the doping region 11 and connects the doping region 11 and the well region 12; the contact region 15 penetrates the source region 13; the upper electrode 4 fills the upper electrode contact hole 31 and is electrically connected to the source region 13 and the contact region 15, the gate is electrically connected to the trench gate structure 2, and the lower electrode 5 is located on the back side of the substrate 1.

[0110] Specifically, the substrate 1 is made of silicon, silicon germanium, silicon carbide or other suitable semiconductor materials.

[0111] Specifically, the trench gate structure 2 includes a gate trench 21, a gate dielectric layer 22 covering the bottom surface and inner wall of the gate trench 21, and a gate conductive layer 23 filling the gate trench 21, the gate dielectric layer 22 wraps the side walls and bottom surface of the gate conductive layer 23, the gate trench 21 is embedded in the substrate 1, and the gate conductive layer 23 is electrically connected to the gate.

[0112] Specifically, under the condition of ensuring device performance, the opening size, opening shape and depth of the gate trench 21 can be selected according to actual conditions, and are not limited here. The depth here is the distance from the bottom surface of the gate trench 21 to the opening of the gate trench 21 (i.e., the upper surface of the substrate 1).

[0113] Specifically, the gate dielectric layer 22 is made of silicon oxide, silicon nitride, silicon oxynitride or other suitable dielectric materials.

[0114] Specifically, the gate conductive layer 23 is made of polysilicon or other suitable conductive materials.

[0115] Specifically, while ensuring device performance, the distance between the doping region 11 and the gate trench 21 can be selected according to actual conditions and is not limited here; the doping concentration, shape, size and thickness of the doping region 11 can be selected according to actual conditions and are not limited here.

[0116] Specifically, the sidewall of the doped region 11 extends to below the trench gate structure 2 .

[0117] Specifically, the side wall of the connecting area 14 is spaced apart from the trench gate structure 2. While ensuring the device performance, the doping concentration and shape of the connecting area 14 can be selected according to actual conditions and are not restricted here. The distance between the connecting area 14 and the trench gate structure 2 can be selected according to actual conditions and is not restricted here.

[0118] Specifically, the contact type between the source region 13 and the upper electrode 4 is an ohmic contact. Under the condition of ensuring the device performance, the doping concentration and thickness of the well region 12 can be selected according to the actual situation, and are not limited here; the doping concentration and thickness of the source region 13 can be selected according to the actual situation, and are not limited here. The thickness here refers to the distance from the bottom surface of the well region 12 (the source region 13) to the upper surface of the well region 12 (the source region 13), wherein the upper surface of the source region 13 is equivalent to the upper surface of the substrate 1.

[0119] Specifically, the contact type between the contact region 15 and the upper electrode 4 is ohmic contact. Under the condition of ensuring the device performance, the doping concentration of the contact region 15 can be selected according to actual conditions and is not limited here.

[0120] Specifically, the material of the interlayer dielectric layer 3 includes silicon oxide, silicon nitride, silicon oxynitride or other suitable dielectric materials.

[0121] Specifically, the upper electrode 4 fills the upper electrode contact hole 31. Under the condition of ensuring the device performance, the opening size and opening shape of the upper electrode contact hole 31 can be selected according to actual conditions and are not limited here.

[0122] Specifically, a gate contact hole penetrating the interlayer dielectric layer 3 is further provided in the interlayer dielectric layer 3 , the gate conductive layer 23 is exposed from the bottom surface of the gate contact hole, and the gate fills the gate contact hole.

[0123] Specifically, under the condition of ensuring device performance, the opening size, opening shape and depth of the gate contact hole can be selected according to actual conditions, and are not limited here. The depth here refers to the distance between the bottom surface of the gate contact hole and the upper surface of the interlayer dielectric layer 3.

[0124] Specifically, the lower surface layer of the substrate 1 is also provided with a first conductive type buffer zone 16a of a preset thickness, and the lower electrode 5 is electrically connected to the buffer zone 16a, that is, the device is a trench gate MOS device, the upper electrode 5 is the source of the trench gate MOS device, the source region 13 is the source region of the trench gate MOS device, the well region 12 is the body region of the trench gate MOS device, and the lower electrode 5 is the drain of the device.

[0125] Specifically, when the device is a trench gate MOS device, the doping concentration and thickness of the buffer region 16a can be selected according to actual conditions while ensuring the device performance, and are not limited here. The thickness here is the distance between the upper surface of the buffer region 16a and the lower surface of the buffer region 16a (i.e., the lower surface of the substrate 1).

[0126] Specifically, the lower surface layer of the substrate 1 is also provided with a first conductive type buffer region 16b of a preset thickness and a second conductive type collector region 17 located on the lower surface layer of the buffer region 16b, and the lower electrode 5 is electrically connected to the collector region 17, that is, the device is a trench gate IGBT device, the upper electrode 5 is the emitter of the trench gate IGBT device, the source region 13 is the emitter region of the trench gate IGBT device, the well region 12 is the base region of the trench gate IGBT device, and the lower electrode 5 is the collector of the trench gate IGBT device.

[0127] Specifically, when the manufactured device is a trench gate IGBT device, the doping concentration and thickness of the buffer region 16b can be selected according to actual conditions while ensuring the device performance, and are not limited here; the doping concentration and thickness of the collector region 17 can be selected according to actual conditions, and are not limited here. The thickness of the buffer region 16b here refers to the distance between the upper surface of the buffer region 16b and the upper surface of the collector region 17, and the thickness of the collector region 17 refers to the distance between the upper surface of the collector region 17 and the lower surface of the collector region 17 (i.e., the lower surface of the substrate 1).

[0128] Specifically, the material of the upper electrode 4 includes titanium, titanium nitride, silver, gold, copper, aluminum, nickel, tungsten, platinum, aluminum or other suitable conductive materials; the material of the gate includes titanium, titanium nitride, silver, gold, copper, aluminum, nickel, tungsten, platinum, aluminum or other suitable conductive materials; the material of the lower electrode 5 includes titanium, titanium nitride, silver, gold, copper, aluminum, nickel, tungsten, platinum, aluminum or other suitable conductive materials.

[0129] Specifically, by setting the doping region 11 in the substrate 1, whose bottom surface is not higher than the trench gate structure 2 and whose sidewalls extend to the bottom of the trench gate structure 2, and using the connecting region 14 to connect the well region 12 and the doping region 11, and the contact region 15 electrically connected to the upper electrode 4 is also connected to the well region 12, the high electric field at the bottom of the trench gate structure 2 is transferred to the PN junction region between the doping region 11 and the substrate 1, thereby achieving protection of the bottom of the trench gate structure 2, avoiding premature breakdown of the gate dielectric layer 22 during the device withstand voltage period, and improving the long-term reliability of the device.

[0130] The trench gate device of this embodiment improves the structure of the device, and sets the doping region 11 with the opposite doping type to the substrate 1 in the substrate 1 between two adjacent trench gate structures 2. The sidewall of the doping region 11 extends to the bottom of the trench gate structure 2 and the bottom surface is lower than the bottom of the trench gate structure 2. The connecting region 14 is used to connect the doping region with the well region 12 connected to the upper electrode 4 through the contact region 15, and then the high electric field at the bottom of the trench gate structure 2 is transferred to the PN junction region between the doping region 11 and the substrate 1, thereby avoiding the premature breakdown of the gate dielectric layer 22 during the device withstand voltage period, thereby improving the long-term reliability of the device.

[0131] In summary, the trench gate device and its preparation method of the present invention form a doping region spaced by a preset distance from the trench gate structure and having a bottom surface lower than the bottom surface of the trench gate structure in the substrate between two adjacent trench gate structures after forming the trench gate structure, and the sidewall of the doping region along the arrangement direction extends to the bottom of the trench gate structure, and then the well region and the doping region are connected through the connecting region, and the contact region electrically connected to the upper electrode is connected to the well region, and then the high electric field at the bottom of the trench gate structure can be transferred to the PN junction region between the doping region and the substrate, effectively reducing the electric field strength at the bottom of the trench gate structure, avoiding the premature breakdown of the gate dielectric layer at the bottom of the trench gate structure during the device withstand voltage, and improving the long-term reliability of the device. Therefore, the present invention effectively overcomes various shortcomings in the prior art and has a high industrial utilization value.

[0132] The above embodiments are merely illustrative of the principles and effects of the present invention, and are not intended to limit the present invention. Anyone familiar with the art may modify or alter the above embodiments without departing from the spirit and scope of the present invention. Therefore, all equivalent modifications or alterations made by a person of ordinary skill in the art without departing from the spirit and technical concept disclosed by the present invention shall still be covered by the claims of the present invention.

Claims

1. A method for preparing a trench gate device, characterized in that: The following steps are involved: A first conductive type substrate is provided, a plurality of trench gate structures are formed on the upper surface of the substrate, and a second conductive type doped region is formed in the substrate between two adjacent trench gate structures, wherein the doped region is spaced from the trench gate structure by a preset distance, and the bottom surface of the doped region is lower than the bottom surface of the trench gate structure; A second conductive type well region and a first conductive type source region located on the upper surface layer of the well region are formed on the upper surface layer of the substrate between two adjacent trench gate structures, and the doped region is spaced a preset distance from the well region; forming an interlayer dielectric layer covering the substrate and the upper surface of the trench gate structure, and forming an upper electrode contact hole penetrating the interlayer dielectric layer and exposing the source region at the bottom, wherein the upper electrode contact hole is located directly above the doped region; A second conductive type connection region connecting the doped region and the well region and a second conductive type contact region penetrating the source region are formed based on the upper electrode contact hole, and the contact region is spaced a preset distance from the trench gate structure; An upper electrode is formed to fill the upper electrode contact hole and is electrically connected to the source region and the contact region, a gate is formed to be electrically connected to the trench gate structure, and a lower electrode is formed on the back side of the substrate.

2. The method for preparing a trench gate device according to claim 1, characterized in that: The trench gate structure includes a gate trench, a gate dielectric layer covering the bottom surface and inner wall of the gate trench, and a gate conductive layer filling the gate trench, the gate dielectric layer wraps the sidewall and bottom surface of the gate conductive layer, the gate trench is embedded in the substrate, and the gate conductive layer is electrically connected to the gate.

3. The method for preparing a trench gate device according to claim 2, characterized in that: After forming the interlayer dielectric layer and before forming the upper electrode, the method further includes forming a gate contact hole penetrating the interlayer dielectric layer, wherein the bottom surface of the gate contact hole exposes the gate conductive layer.

4. The method for preparing a trench gate device according to claim 1, wherein: The upper surface of the doped region is higher than the bottom surface of the trench gate structure.

5. The method for preparing a trench gate device according to claim 1, characterized in that: The sidewall of the doped region extends to below the trench gate structure.

6. The method for preparing a trench gate device according to claim 1, characterized in that: A preset distance is provided between the sidewall of the communication region and the trench gate structure.

7. The method for preparing a trench gate device according to claim 1, characterized in that: The contact region is connected to the well region and has a bottom surface no lower than a bottom surface of the well region.

8. The method for preparing a trench gate device according to claim 1, characterized in that: After forming the upper electrode and the gate and before forming the lower electrode, the method further includes forming a first conductive type buffer zone on the lower surface layer of the substrate, wherein the lower electrode is electrically connected to the buffer zone.

9. The method for preparing a trench gate device according to claim 1, characterized in that: After forming the upper electrode and the gate and before forming the lower electrode, the method further includes forming a first conductive type buffer region and a second conductive type collector region in sequence on the lower surface of the substrate. The collector region is located on the lower surface of the buffer region, and the lower electrode is at least electrically connected to the collector region.

10. A trench gate device, characterized in that: include: a first conductive type substrate; A plurality of trench gate structures arranged at intervals are located on the upper surface layer of the substrate; A second conductive type doped region, located in the substrate between two adjacent trench gate structures and spaced apart from the trench gate structure by a preset distance, wherein a bottom surface of the doped region is lower than a bottom surface of the trench gate structure; A second conductive type well region is located on the upper surface layer of the substrate between two adjacent trench gate structures; A first conductive type source region is located on the upper surface of the well region, and the doped region is spaced a preset distance from the well region; an interlayer dielectric layer, covering the substrate and the upper surface of the trench gate structure, wherein the interlayer dielectric layer is provided with an upper electrode contact hole penetrating the interlayer dielectric layer and exposing the source region at the bottom, and the upper electrode contact hole is located directly above the doped region; A second conductive type connection region is located in the substrate between the well region and the doping region and connects the doping region and the well region; A second conductive type contact region, extending through the source region; An upper electrode, a gate and a lower electrode, wherein the upper electrode fills the upper electrode contact hole and is electrically connected to the source region and the contact region, the gate is electrically connected to the trench gate structure, and the lower electrode is located on the back side of the substrate.

Citation Information

Patent Citations

  • Super junction trench gate MOSFET and preparation method thereof

    CN114447104A

  • Semiconductor device and manufacturing method thereof

    CN115966611A

  • Semiconductor device, integrated circuit, and electronic apparatus

    CN116779673A

  • Semiconductor device

    US20080099837A1

  • Semiconductor device and manufacturing method thereof

    US20170062556A1