Multi-filtering cigarette holder and preparation method thereof
By using polylactic fibers with a skin core structure and electrospinned fibers in cigarette filter materials to combine fat-linked branch cellulose microspheres, the problem that the prior art cannot effectively remove tobacco carcinogens is solved, and the adsorption effect is significantly improved. Improved air quality and environmental protection.
Patent Information
- Application Number
- CN202411157331.6
- Authority / Receiving Office
- CN · China
- Patent Type
- Applications(China)
- Current Assignee / Owner
- Filing Date
- 2024-08-22
- Publication Date
- 2024-11-26
Abstract
Description
Technical Field
[0001] The invention relates to the technical field of rolled tobacco, and in particular to a multiple-filter cigarette holder and a preparation method thereof. Background Art
[0002] The development of cigarette filters has been going on for quite a long time. Soon after the appearance of cigarettes, cigarette filters came into being. From the initial paper wrapped with fiber floss, it was gradually updated to paper and cellulose flexible filling, and then to paper wrapped with cotton, and then to filter tips with asbestos as filter materials, and then to activated carbon with adsorption function as filter materials. It was not until the 1960s that the first acetate filter tip came out, and then the United States invented the filter tip with polypropylene as the filling material. It was not until the 1980s that my country imported and gradually used and participated in the use and research of cigarette filters for the first time. Today, cigarette filters have been well known to the public in the cigarette market. In addition to traditional filter materials such as cotton fiber and acetate fiber, its development has also introduced new cellulose materials such as Lyocell. It is well known that some components in the smoke produced by tobacco combustion are extremely harmful to human health and the environment. There are at least a dozen carcinogens in tar alone. Although the above materials can have a certain filtering effect on harmful substances such as tar produced when tobacco burns, some harmful substances will still remain. Summary of the invention
[0003] Technical problem to be solved: The purpose of the present invention is to provide a multi-filter cigarette holder, which adopts the combination of skin-core structure polylactic acid fiber and electrostatically spun polylactic acid fiber bundle to achieve better filtering effect.
[0004] Technical solution: A multiple filter cigarette holder, the filter cigarette holder is formed by a combination of melt-spun polylactic acid fibers and electrospun polylactic acid fiber bundles, the core-sheath structure polylactic acid fibers and electrospun polylactic acid fiber bundles are arranged alternately, and the electrospun polylactic acid fiber bundles are bent in an "S" shape. Preferably, the preparation method of the electrospun polylactic acid fiber bundle comprises the following steps: S11. Adding polylactic acid to dichloromethane and stirring to dissolve to obtain a 5.5-7wt% electrospinning solution; S12. The electrospinning solution was electrospun using a multi-needle classical spinning device to obtain an electrospinning fiber bundle, the voltage was 15 kV, the flow rate was 0.5-1 mL / h, and the receiving distance was 20 cm; S13. Heat-treating the electrospun fiber bundle in an "S"-structured mold to obtain an "S"-structured polylactic acid fiber bundle. Preferably, the wavelength of the "S"-structured polylactic acid fiber bundle in step S3 is 0.7-1.5 cm, the wave height is 0.3-0.6 cm, the heat setting temperature is 105-120° C., and the time is 10-30 seconds. The method for preparing the above-mentioned multiple filter cigarette holder comprises the following steps: S1. Using low melting point polylactic acid as the cortex material and high melting point polylactic acid as the core material, the cortex material and the core material are dried and melted to obtain a cortex spinning solution and a core spinning solution, and fat chain grafted cellulose microspheres are added to the cortex spinning solution for spinning to obtain a sheath-core structure polylactic acid fiber; S2. The polylactic acid fibers and polylactic acid fiber bundles of the sheath-core structure are arranged alternately to obtain a cigarette holder tow, and then the cigarette holder is obtained by thermal bonding. Preferably, the method for preparing the fat chain grafted cellulose microspheres comprises the following steps: S21. The cellulose was added to 1-butyl-3-methylimidazole chloride, stirred to dissolve, and a cellulose solution having a concentration of 6-8wt% was obtained; S22. Nano-copper oxide particles were added to the cellulose solution, stirred evenly, and a mixed solution was obtained; S23. Span80, Tween 80 and liquid paraffin are mixed in a mass ratio of 1:1:100, stirred and mixed evenly, and then the mixed solution prepared in step S2 is added dropwise to the above solution, stirred vigorously for emulsification, and then water is added to the suspension, and the cellulose microspheres are separated by cooling; S24. Adding the cellulose microspheres to a 0.05-0.1 mol / L hydrochloric acid solution, stirring to dissolve the copper oxide particles contained in the cellulose microspheres, and directly filtering to obtain porous cellulose microspheres; S25. Add the porous cellulose microspheres into the melted lauric acid so that the microspheres are completely immersed in the lauric acid liquid, then ultrasonically oscillate for 30-60 minutes to allow the solid microspheres to absorb fatty acids as much as possible, then vacuum filter and dry to obtain the fat-linked cellulose microspheres. Preferably, in step S1, the mass ratio of low-melting point polylactic acid to high-melting point polylactic acid is 50-70:30-50, the melting point of low-melting point polylactic acid is 115-130°C, the melting point of high-melting point polylactic acid is 150-170°C, and the mass fraction of fat chain grafted cellulose microspheres in the sheath spinning solution is 5-8wt%, and the fineness of the sheath-core structure polylactic acid fiber is 11-22dtex. Preferably, the ratio of the polylactic acid fibers of the sheath-core structure and the electrospun polylactic acid fiber bundles in the cigarette holder fiber bundle is 55-70:30-45. Preferably, in step S22, the content of copper oxide in the mixed solution is 1-2 wt %. Preferably, the rotation speed of the vigorous stirring in step S22 is 800-1200 r / min. Beneficial effects: The multi-filter cigarette holder of the present invention has the following advantages: 1. The present invention uses two fibers with different oriented structures for composite, one is a polylactic acid fiber with a skin-core structure, and the other is a polylactic acid nanofiber bundle prepared by electrospinning. The arrangement of the polylactic acid with the skin-core structure is conventionally longitudinally parallel. The polylactic acid nanocellulose is first heat-treated to obtain an "S"-shaped structure. The skin-core polylactic acid fiber and the electrospun polylactic acid fiber bundle are arranged alternately to obtain a composite cigarette holder bundle with a "$" structure. The polylactic acid nanofiber bundle prepared by electrospinning is itself a nanofiber. The harmful substances in the cigarette will greatly increase the contact area and improve the adsorption effect. After the heat treatment to form an "S" result, it has a larger area and can adsorb more harmful substances. 2. The polylactic acid fibers of the sheath-core structure of the present invention are spun and woven using two polylactic acid raw materials with different melting points, and fat chain grafted cellulose microspheres are added to the sheath. During the thermal bonding process, the polylactic acid fibers added to the sheath will melt to a certain extent, so that the polylactic acid fibers are bonded to each other, and the polylactic acid fibers and the polylactic acid electrospun fiber bundles are bonded to each other. At the same time, more fat chain grafted cellulose microspheres in the sheath can be exposed, thereby improving the filtering effect of the filter cigarette holder; 3. In the present invention, the cortex is filled with fat chain grafted cellulose microspheres, which have a porous structure and some Cu 2+ , as well as long fat chains, can improve the filtering and adsorption effect of the cigarette holder. DETAILED DESCRIPTION The present invention will be further described below in conjunction with embodiments, which are explanations of the present invention and are not limited to the following embodiments: Example 1 The preparation method of electrospun polylactic acid fiber bundles comprises the following steps: S11. adding polylactic acid to dichloromethane and stirring to dissolve to obtain a 5.5 wt % electrospinning solution; S12. The electrospinning solution was electrospun using a two-needle classical spinning device to obtain an electrospinning fiber bundle, with a voltage of 15 kV, a flow rate of 1 mL / h, and a receiving distance of 20 cm; S13. Heat-treating the electrospun fiber bundle in an "S"-structured mold to obtain an "S"-structured polylactic acid fiber bundle. Preferably, the wavelength of the "S"-structured polylactic acid fiber bundle in step S3 is 0.7 cm, the wave height is 0.3 cm, the heat setting temperature is 105° C., and the time is 30 seconds. Example 2 The preparation method of electrospun polylactic acid fiber bundles comprises the following steps: S11. adding polylactic acid to dichloromethane and stirring to dissolve to obtain a 7 wt % electrospinning solution; S12. The electrospinning solution was electrospun using a three-needle classical spinning device to obtain an electrospinning fiber bundle, with a voltage of 15 kV, a flow rate of 0.5 mL / h, and a receiving distance of 20 cm; S13. Heat-treating the electrospun fiber bundle in an "S"-structured mold to obtain an "S"-structured polylactic acid fiber bundle. Preferably, the wavelength of the "S"-structured polylactic acid fiber bundle in step S3 is 1.5 cm, the wave height is 0.6 cm, the heat setting temperature is 120° C., and the time is 10 s. Example 3 The preparation method of electrospun polylactic acid fiber bundles comprises the following steps: S11. adding polylactic acid to dichloromethane and stirring to dissolve to obtain a 6 wt % electrospinning solution; S12. The electrospinning solution was electrospun using a two-needle classical spinning device to obtain an electrospun fiber bundle, with a voltage of 15 kV, a flow rate of 85-1 mL / h, and a receiving distance of 20 cm; S13. Heat-treating the electrospun fiber bundle in an "S"-structured mold to obtain an "S"-structured polylactic acid fiber bundle. Preferably, the wavelength of the "S"-structured polylactic acid fiber bundle in step S3 is 1.2 cm, the wave height is 0.5 cm, the heat setting temperature is 110° C., and the time is 20 seconds. Example 4 A method for preparing a multiple filter cigarette holder, the method comprising the following steps: S1. Using low-melting-point polylactic acid with a melting point of 115°C as the skin material, and high-melting-point polylactic acid with a melting point of 150°C as the core material, the mass ratio of low-melting-point polylactic acid to high-melting-point polylactic acid is 7:3, the skin material and the core material are dried and melted to obtain skin spinning solution and core spinning solution respectively, and fat chain grafted cellulose microspheres are added to the skin spinning solution for spinning, the mass fraction of fat chain grafted cellulose microspheres in the skin spinning solution is 8wt%, and a skin-core structured polylactic acid fiber with a fineness of 22dtex is obtained; S2. The skin-core structured polylactic acid fibers and the polylactic acid fiber bundles prepared in Example 1 are arranged alternately to obtain a cigarette holder tow, the skin-core structured polylactic acid fibers and the electrospun polylactic acid fiber bundles account for 55:45 in the cigarette holder tow, and then a filter cigarette holder is obtained through thermal bonding; The method for preparing the fat chain grafted cellulose microspheres comprises the following steps: S21. The cellulose was added to 1-butyl-3-methylimidazole chloride, stirred to dissolve, and a cellulose solution having a concentration of 6 wt% was obtained; S22. Nano-copper oxide particles were added to the cellulose solution, the content of copper oxide in the mixed solution was 1 wt%, and stirred to obtain a mixed solution; S23. Span80, Tween 80 and liquid paraffin were mixed in a mass ratio of 1:1:100, stirred and mixed evenly, and then the mixed solution prepared in step S2 was added dropwise to the above solution, stirred vigorously at a speed of 800 r / min for emulsification, and then water was added to the suspension, and the cellulose microspheres were separated by cooling; S24. Adding the cellulose microspheres to a 0.05 mol / L hydrochloric acid solution, stirring to dissolve the copper oxide particles contained in the cellulose microspheres, and directly filtering to obtain porous cellulose microspheres; S25. Add the porous cellulose microspheres into the melted lauric acid so that the microspheres are completely immersed in the lauric acid liquid, then ultrasonically oscillate for 30 minutes to allow the solid microspheres to absorb fatty acids as much as possible, then vacuum filter and dry to obtain the fat-linked cellulose microspheres. Example 5 A method for preparing a multiple filter cigarette holder, the method comprising the following steps: S1. Using low-melting-point polylactic acid with a melting point of 130°C as the skin material, and high-melting-point polylactic acid with a melting point of 170°C as the core material, the mass ratio of low-melting-point polylactic acid to high-melting-point polylactic acid is 5:3, the skin material and the core material are dried and melted to obtain skin spinning solution and core spinning solution respectively, and fat chain grafted cellulose microspheres are added to the skin spinning solution for spinning, the mass fraction of fat chain grafted cellulose microspheres in the skin spinning solution is 5wt%, and a skin-core structured polylactic acid fiber with a fineness of 11dtex is obtained; S2. The skin-core structured polylactic acid fibers and the polylactic acid fiber bundles prepared in Example 2 are arranged alternately to obtain a cigarette holder tow, the skin-core structured polylactic acid fibers and the electrospun polylactic acid fiber bundles account for 70:30 in the cigarette holder tow, and then a filter cigarette holder is obtained through thermal bonding; The method for preparing the fat chain grafted cellulose microspheres comprises the following steps: S21. The cellulose was added to 1-butyl-3-methylchloroimidazole, stirred to dissolve, and a cellulose solution having a concentration of 8 wt% was obtained; S22. Nano-copper oxide particles were added to the cellulose solution, the content of copper oxide in the mixed solution was 1 wt%, and stirred to obtain a mixed solution; S23. Span80, Tween 80 and liquid paraffin were mixed in a mass ratio of 1:1:100, stirred and mixed evenly, and then the mixed solution prepared in step S2 was added dropwise to the above solution, stirred vigorously at a speed of 1200 r / min for emulsification, and then water was added to the suspension, and the cellulose microspheres were separated by cooling; S24. Adding the cellulose microspheres to a 0.1 mol / L hydrochloric acid solution, stirring to dissolve the copper oxide particles contained in the cellulose microspheres, and directly filtering to obtain porous cellulose microspheres; S25. Add the porous cellulose microspheres into the melted lauric acid so that the microspheres are completely immersed in the lauric acid liquid, then ultrasonically oscillate for 60 minutes to allow the solid microspheres to absorb fatty acids as much as possible, then vacuum filter and dry to obtain the fat-linked cellulose microspheres. Example 6 A method for preparing a multiple filter cigarette holder, the method comprising the following steps: S1. Using low-melting-point polylactic acid with a melting point of 120°C as the skin material, and high-melting-point polylactic acid with a melting point of 160°C as the core material, the mass ratio of low-melting-point polylactic acid to high-melting-point polylactic acid is 6:4, the skin material and the core material are dried and melted to obtain skin spinning solution and core spinning solution respectively, and fat chain grafted cellulose microspheres are added to the skin spinning solution for spinning, the mass fraction of fat chain grafted cellulose microspheres in the skin spinning solution is 6-wt%, and a skin-core structured polylactic acid fiber with a fineness of 14 dtex is obtained; S2. The skin-core structured polylactic acid fibers and the polylactic acid fiber bundles prepared in Example 3 are arranged alternately to obtain a cigarette holder tow, the skin-core structured polylactic acid fibers and the electrospun polylactic acid fiber bundles account for 60:35 in the cigarette holder tow, and then a filter cigarette holder is obtained through thermal bonding; The method for preparing the fat chain grafted cellulose microspheres comprises the following steps: S21. The cellulose was added to 1-butyl-3-methylimidazole chloride, stirred to dissolve, and a cellulose solution having a concentration of 6.5 wt% was obtained; S22. Nano-copper oxide particles were added to the cellulose solution, the content of copper oxide in the mixed solution was 1.8 wt%, and stirred to obtain a mixed solution; S23. Span80, Tween 80 and liquid paraffin were mixed in a mass ratio of 1:1:100, stirred and mixed evenly, and then the mixed solution prepared in step S2 was added dropwise to the above solution, stirred vigorously at a speed of 900 r / min for emulsification, and then water was added to the suspension, and the cellulose microspheres were separated by cooling; S24. Adding the cellulose microspheres to a 0.09 mol / L hydrochloric acid solution, stirring to dissolve the copper oxide particles contained in the cellulose microspheres, and directly filtering to obtain porous cellulose microspheres; S25. Add the porous cellulose microspheres into the melted lauric acid so that the microspheres are completely immersed in the lauric acid liquid, then ultrasonically oscillate for 50 minutes to allow the solid microspheres to absorb fatty acids as much as possible, then vacuum filter and dry to obtain the fat-linked cellulose microspheres. Example 7 A method for preparing a multiple filter cigarette holder, the method comprising the following steps: S1. Using low-melting-point polylactic acid with a melting point of 125°C as the skin material and high-melting-point polylactic acid with a melting point of 165°C as the core material, the mass ratio of low-melting-point polylactic acid to high-melting-point polylactic acid is 55:40, drying and melting the skin material and the core material to obtain skin spinning solution and core spinning solution, respectively, adding fat chain grafted cellulose microspheres to the skin spinning solution, spinning, the mass fraction of fat chain grafted cellulose microspheres in the skin spinning solution is 7wt%, and obtaining a skin-core structure polylactic acid fiber with a fineness of 18dtex; S2. The polylactic acid fibers of the sheath-core structure and the polylactic acid fiber bundle prepared in Example 3 are arranged alternately to obtain a cigarette holder tow, wherein the polylactic acid fibers of the sheath-core structure and the electrospun polylactic acid fiber bundle account for 65:40 in the cigarette holder tow, and then a filter cigarette holder is obtained by thermal bonding; The method for preparing the fat chain grafted cellulose microspheres comprises the following steps: S21. The cellulose was added to 1-butyl-3-methylimidazole chloride, stirred and dissolved to obtain a cellulose solution with a concentration of 67.5wt%; S22. Nano-copper oxide particles were added to the cellulose solution, the content of copper oxide in the mixed solution was 1.2wt%, and stirred to obtain a mixed solution; S23. Span80, Tween 80 and liquid paraffin were mixed in a mass ratio of 1:1:100, stirred and mixed evenly, and then the mixed solution prepared in step S2 was added dropwise to the above solution, stirred vigorously at a speed of 1100 r / min for emulsification, and then water was added to the suspension, and the cellulose microspheres were separated by cooling; S24. Adding the cellulose microspheres to a 0.06 mol / L hydrochloric acid solution, stirring to dissolve the copper oxide particles contained in the cellulose microspheres, and directly filtering to obtain porous cellulose microspheres; S25. Add the porous cellulose microspheres into the melted lauric acid so that the microspheres are completely immersed in the lauric acid liquid, then ultrasonically oscillate for 45 minutes to allow the solid microspheres to absorb fatty acids as much as possible, then vacuum filter and dry to obtain the fat-linked cellulose microspheres. Example 8 A method for preparing a multiple filter cigarette holder, the method comprising the following steps: S1. Using low-melting-point polylactic acid with a melting point of 115-120°C as the skin material and high-melting-point polylactic acid with a melting point of 160°C as the core material, the mass ratio of low-melting-point polylactic acid to high-melting-point polylactic acid is 6:4, drying and melting the skin material and the core material to obtain skin spinning solution and core spinning solution, respectively, adding fat chain grafted cellulose microspheres to the skin spinning solution, spinning, the mass fraction of fat chain grafted cellulose microspheres in the skin spinning solution is 6.5wt%, and obtaining a skin-core structure polylactic acid fiber with a fineness of 16dtex; S2. The polylactic acid fibers of the sheath-core structure and the polylactic acid fiber bundle prepared in Example 3 are arranged alternately to obtain a cigarette holder tow, wherein the polylactic acid fibers of the sheath-core structure and the electrospun polylactic acid fiber bundle account for 65:35 in the cigarette holder tow, and then a filter cigarette holder is obtained by thermal bonding; The method for preparing the fat chain grafted cellulose microspheres comprises the following steps: S21. The cellulose was added to 1-butyl-3-methylimidazole chloride, stirred to dissolve, and a cellulose solution having a concentration of 7 wt% was obtained; S22. Nano-copper oxide particles were added to the cellulose solution, the content of copper oxide in the mixed solution was 1.5 wt%, and stirred to obtain a mixed solution; S23. Span80, Tween 80 and liquid paraffin were mixed in a mass ratio of 1:1:100, stirred and mixed evenly, and then the mixed solution prepared in step S2 was added dropwise to the above solution, stirred vigorously at a speed of 1000 r / min for emulsification, and then water was added to the suspension, and the cellulose microspheres were separated by cooling; S24. Adding the cellulose microspheres to a 0.1 mol / L hydrochloric acid solution, stirring to dissolve the copper oxide particles contained in the cellulose microspheres, and directly filtering to obtain porous cellulose microspheres; S25. Add the porous cellulose microspheres into the melted lauric acid so that the microspheres are completely immersed in the lauric acid liquid, then ultrasonically oscillate for 45 minutes to allow the solid microspheres to absorb fatty acids as much as possible, then vacuum filter and dry to obtain the fat-linked cellulose microspheres. Comparative Example 1 The preparation method of electrospun polylactic acid fiber bundles comprises the following steps: S11. adding polylactic acid to dichloromethane and stirring to dissolve to obtain a 6 wt % electrospinning solution; S12. The electrospinning solution was electrospun using a two-needle classical spinning device to obtain an electrospun fiber bundle, with a voltage of 15 kV, a flow rate of 85-1 mL / h, and a receiving distance of 20 cm; S13. Heat-treating the electrospun fiber bundle in an "S"-structured mold to obtain an "S"-structured polylactic acid fiber bundle. Preferably, the wavelength of the "S"-structured polylactic acid fiber bundle in step S3 is 2 cm, the wave height is 0.3 cm, the heat setting temperature is 110° C., and the time is 20 seconds. Comparative Example 2 The preparation method of electrospun polylactic acid fiber bundles comprises the following steps: S11. adding polylactic acid to dichloromethane and stirring to dissolve to obtain a 6 wt % electrospinning solution; S12. The electrospinning solution was electrospun using a two-needle classical spinning device to obtain an electrospun fiber bundle, with a voltage of 15 kV, a flow rate of 85-1 mL / h, and a receiving distance of 20 cm; S13. Heat-treating the electrospun fiber bundle in an "S"-structured mold to obtain an "S"-structured polylactic acid fiber bundle. Preferably, the wavelength of the "S"-structured polylactic acid fiber bundle in step S3 is 0.5 cm, the wave height is 0.5 cm, the heat setting temperature is 110° C., and the time is 20 seconds. Comparative Example 3 A method for preparing a multiple filter cigarette holder, the method comprising the following steps: S1. Using low-melting-point polylactic acid with a melting point of 115-120°C as the skin material and high-melting-point polylactic acid with a melting point of 160°C as the core material, the mass ratio of low-melting-point polylactic acid to high-melting-point polylactic acid is 6:4, drying and melting the skin material and the core material to obtain skin spinning solution and core spinning solution, respectively, adding fat chain grafted cellulose microspheres to the skin spinning solution, spinning, the mass fraction of fat chain grafted cellulose microspheres in the skin spinning solution is 6.5wt%, and obtaining a skin-core structure polylactic acid fiber with a fineness of 16dtex; S2. The polylactic acid fibers of the sheath-core structure and the polylactic acid fiber bundles prepared in Comparative Example 1 are arranged alternately to obtain a cigarette holder tow, wherein the polylactic acid fibers of the sheath-core structure and the electrospun polylactic acid fiber bundles account for 65:35 in the cigarette holder tow, and then a filter cigarette holder is obtained by thermal bonding; The method for preparing the fat chain grafted cellulose microspheres comprises the following steps: S21. The cellulose was added to 1-butyl-3-methylimidazole chloride, stirred to dissolve, and a cellulose solution having a concentration of 7 wt% was obtained; S22. Nano-copper oxide particles were added to the cellulose solution, the content of copper oxide in the mixed solution was 1.5 wt%, and stirred to obtain a mixed solution; S23. Span80, Tween 80 and liquid paraffin were mixed in a mass ratio of 1:1:100, stirred and mixed evenly, and then the mixed solution prepared in step S2 was added dropwise to the above solution, stirred vigorously at a speed of 1000 r / min for emulsification, and then water was added to the suspension, and the cellulose microspheres were separated by cooling; S24. Adding the cellulose microspheres to a 0.1 mol / L hydrochloric acid solution, stirring to dissolve the copper oxide particles contained in the cellulose microspheres, and directly filtering to obtain porous cellulose microspheres; S25. Add the porous cellulose microspheres into the melted lauric acid so that the microspheres are completely immersed in the lauric acid liquid, then ultrasonically oscillate for 45 minutes to allow the solid microspheres to absorb fatty acids as much as possible, then vacuum filter and dry to obtain the fat-linked cellulose microspheres. Comparative Example 4 A method for preparing a multiple filter cigarette holder, the method comprising the following steps: S1. Using low-melting-point polylactic acid with a melting point of 115-120°C as the skin material and high-melting-point polylactic acid with a melting point of 160°C as the core material, the mass ratio of low-melting-point polylactic acid to high-melting-point polylactic acid is 6:4, drying and melting the skin material and the core material to obtain skin spinning solution and core spinning solution, respectively, adding fat chain grafted cellulose microspheres to the skin spinning solution, spinning, the mass fraction of fat chain grafted cellulose microspheres in the skin spinning solution is 6.5wt%, and obtaining a skin-core structure polylactic acid fiber with a fineness of 16dtex; S2. The polylactic acid fibers of the sheath-core structure and the polylactic acid fiber bundles prepared in Comparative Example 2 are arranged alternately to obtain a cigarette holder tow, wherein the polylactic acid fibers of the sheath-core structure and the electrospun polylactic acid fiber bundles account for 65:35 in the cigarette holder tow, and then a filter cigarette holder is obtained by thermal bonding; The method for preparing the fat chain grafted cellulose microspheres comprises the following steps: S21. The cellulose was added to 1-butyl-3-methylimidazole chloride, stirred to dissolve, and a cellulose solution having a concentration of 7 wt% was obtained; S22. Nano-copper oxide particles were added to the cellulose solution, the content of copper oxide in the mixed solution was 1.5 wt%, and stirred to obtain a mixed solution; S23. Span80, Tween 80 and liquid paraffin were mixed in a mass ratio of 1:1:100, stirred and mixed evenly, and then the mixed solution prepared in step S2 was added dropwise to the above solution, stirred vigorously at a speed of 1000 r / min for emulsification, and then water was added to the suspension, and the cellulose microspheres were separated by cooling; S24. Adding the cellulose microspheres to a 0.1 mol / L hydrochloric acid solution, stirring to dissolve the copper oxide particles contained in the cellulose microspheres, and directly filtering to obtain porous cellulose microspheres; S25. Add the porous cellulose microspheres into the melted lauric acid so that the microspheres are completely immersed in the lauric acid liquid, then ultrasonically oscillate for 45 minutes to allow the solid microspheres to absorb fatty acids as much as possible, then vacuum filter and dry to obtain the fat-linked cellulose microspheres. Filter rod section weight (g) Absorption resistance(kPa) Filter rod ventilation rate (%) Example 4 0.15 1.32 35.12 Example 5 0.15 1.31 35.42 Example 6 0.15 1.32 35.29 Example 7 0.15 1.30 34.96 Example 8 0.15 1.32 36.18 Comparative Example 3 0.15 1.26 40.45 Comparative Example 4 0.17 1.37 28.26 Note: GB / T 22838 test is adopted, the cigarette specification is 84mm in length (54mm tobacco material section + 30mm filter rod section, the cigarette circumference is 17.0mm, and the weight of the tobacco material section in the cigarette is 0.40±0.1g. Comparative Example 5 A method for preparing a multiple filter cigarette holder, the method comprising the following steps: S1. Using low-melting-point polylactic acid with a melting point of 115-120°C as the skin material and high-melting-point polylactic acid with a melting point of 160°C as the core material, the mass ratio of the low-melting-point polylactic acid to the high-melting-point polylactic acid being 6:4, drying and melting the skin material and the core material to obtain a skin spinning solution and a core spinning solution, respectively, and spinning to obtain a skin-core structure polylactic acid fiber with a fineness of 16 dtex; S2. The polylactic acid fibers with a sheath-core structure and the polylactic acid fiber bundles prepared in Example 3 are arranged alternately to obtain a cigarette holder tow, wherein the polylactic acid fibers with a sheath-core structure and the electrospun polylactic acid fiber bundles account for 65:35 in the cigarette holder tow, and then a filter cigarette holder is obtained by thermal bonding. Comparative Example 6 A method for preparing a multiple filter cigarette holder, the method comprising the following steps: S1. Using low-melting-point polylactic acid with a melting point of 115-120°C as the skin material and high-melting-point polylactic acid with a melting point of 160°C as the core material, the mass ratio of low-melting-point polylactic acid to high-melting-point polylactic acid is 6:4, drying and melting the skin material and the core material to obtain skin spinning solution and core spinning solution, respectively, adding fat chain grafted cellulose microspheres to the skin spinning solution, spinning, the mass fraction of fat chain grafted cellulose microspheres in the skin spinning solution is 6.5wt%, and obtaining a skin-core structure polylactic acid fiber with a fineness of 16dtex; S2. The polylactic acid fibers and polylactic acid fiber bundles of the sheath-core structure are arranged alternately to obtain a cigarette holder tow, wherein the polylactic acid fibers of the sheath-core structure and the electrospun polylactic acid fiber bundles account for 65:35 in the cigarette holder tow, and then a filter cigarette holder is obtained by thermal bonding; wherein the preparation method of the fat chain grafted cellulose microspheres comprises the following steps: S21. The cellulose was added to 1-butyl-3-methylimidazole chloride, stirred to dissolve, and a cellulose solution having a concentration of 7 wt% was obtained; S22. Nano-copper oxide particles were added to the cellulose solution, the content of copper oxide in the mixed solution was 1.5 wt%, and stirred to obtain a mixed solution; S23. Span80, Tween 80 and liquid paraffin were mixed in a mass ratio of 1:1:100, stirred and mixed evenly, and then the mixed solution prepared in step S2 was added dropwise to the above solution, stirred vigorously at a speed of 1000 r / min for emulsification, and then water was added to the suspension, and the cellulose microspheres were separated by cooling; S24. Adding the cellulose microspheres to a 0.1 mol / L hydrochloric acid solution, stirring to dissolve the copper oxide particles contained in the cellulose microspheres, and directly filtering to obtain porous cellulose microspheres; S25. The porous cellulose microspheres were added to the melted lauric acid so that the microspheres were completely immersed in the lauric acid liquid, and then ultrasonically vibrated for 45 minutes to allow the solid microspheres to absorb fatty acids as much as possible, and then vacuum filtered and dried to obtain fat-linked cellulose microspheres; The preparation method of electrospun polylactic acid fiber bundles comprises the following steps: S11. adding polylactic acid to dichloromethane and stirring to dissolve to obtain a 6 wt % electrospinning solution; S12. The electrospinning solution was electrospun using a two-needle classical spinning device to obtain an electrospinning fiber bundle with a voltage of 15 kV, a flow rate of 85-1 mL / h, and a receiving distance of 20 cm. Comparative Example 7 A method for preparing a multiple filter cigarette holder, the method comprising the following steps: S1. Using low-melting-point polylactic acid with a melting point of 115-120°C as the skin material and high-melting-point polylactic acid with a melting point of 160°C as the core material, the mass ratio of low-melting-point polylactic acid to high-melting-point polylactic acid is 6:4, drying and melting the skin material and the core material to obtain skin spinning solution and core spinning solution, respectively, adding fat chain grafted cellulose microspheres to the skin spinning solution, spinning, the mass fraction of fat chain grafted cellulose microspheres in the skin spinning solution is 6.5wt%, and obtaining a skin-core structure polylactic acid fiber with a fineness of 16dtex; S2. The polylactic acid fibers of the sheath-core structure and the polylactic acid fiber bundle prepared in Example 3 are arranged alternately to obtain a cigarette holder tow, wherein the polylactic acid fibers of the sheath-core structure and the electrospun polylactic acid fiber bundle account for 65:35 in the cigarette holder tow, and then a filter cigarette holder is obtained by thermal bonding; The method for preparing the fat chain grafted cellulose microspheres comprises the following steps: S21. Add cellulose to 1-butyl-3-methylimidazole chloride, stir to dissolve, and obtain a cellulose solution with a concentration of 7 wt%; S22. Span80, Tween 80 and liquid paraffin are mixed in a mass ratio of 1:1:100, and stirred to mix evenly, and then the mixed solution prepared in step S2 is added dropwise to the above solution, and vigorously stirred at a speed of 1000 r / min for emulsification, and then water is added to the suspension, and the cellulose microspheres are separated by cooling; S23. Add cellulose microspheres into melted lauric acid so that the microspheres are completely immersed in the lauric acid liquid, then ultrasonically oscillate for 45 minutes to allow the solid microspheres to absorb fatty acids as much as possible, then vacuum filter and dry to obtain fat-linked cellulose microspheres. Comparative Example 8 A method for preparing a multiple filter cigarette holder, the method comprising the following steps: S1. Using low-melting-point polylactic acid with a melting point of 115-120°C as the skin material and high-melting-point polylactic acid with a melting point of 160°C as the core material, the mass ratio of low-melting-point polylactic acid to high-melting-point polylactic acid is 6:4, drying and melting the skin material and the core material to obtain skin spinning solution and core spinning solution, respectively, adding porous cellulose microspheres to the skin spinning solution, spinning, the mass fraction of porous cellulose microspheres in the skin spinning solution is 6.5wt%, and obtaining a skin-core structure polylactic acid fiber with a fineness of 16dtex; S2. The polylactic acid fibers of the sheath-core structure and the polylactic acid fiber bundle prepared in Example 3 are arranged alternately to obtain a cigarette holder tow, wherein the polylactic acid fibers of the sheath-core structure and the electrospun polylactic acid fiber bundle account for 65:35 in the cigarette holder tow, and then a filter cigarette holder is obtained by thermal bonding; The method for preparing the porous cellulose microspheres comprises the following steps: S21. The cellulose was added to 1-butyl-3-methylimidazole chloride, stirred to dissolve, and a cellulose solution having a concentration of 7 wt% was obtained; S22. Nano-copper oxide particles were added to the cellulose solution, the content of copper oxide in the mixed solution was 1.5 wt%, and stirred to obtain a mixed solution; S23. Span80, Tween 80 and liquid paraffin were mixed in a mass ratio of 1:1:100, stirred and mixed evenly, and then the mixed solution prepared in step S2 was added dropwise to the above solution, stirred vigorously at a speed of 1000 r / min for emulsification, and then water was added to the suspension, and the cellulose microspheres were separated by cooling; S24. Add the cellulose microspheres into 0.1 mol / L hydrochloric acid solution, stir to dissolve the copper oxide particles contained in the cellulose microspheres, and directly filter to obtain porous cellulose microspheres. Performance Testing: The interception rate of tar and total particulate matter in the sample cigarette was determined according to the method of GB / T19609-2004; Tar per mouthful (mg / mouthful) Total particle retention rate (%) Example 8 0.04 39.15 Comparative Example 3 0.09 35.62 Comparative Example 4 0.04 39.21 Comparative Example 5 0.09 34.52 Comparative Example 6 0.11 32.65 Comparative Example 7 0.09 33.98 Comparative Example 8 0.1 33.25 Cigarettes of the same specifications available on the market 0.12-0.15 28-33 Testing the filtration efficiency of components such as PAHs using gas chromatography-mass spectrometry; Benzoanthracene (%) phenol(%) Example 8 39.6 79.5 Comparative Example 3 37.1 73.6 Comparative Example 4 39.5 78.9 Comparative Example 5 33.6 72.6 Comparative Example 6 29.6 70.5 Comparative Example 7 32.4 66.8 Comparative Example 8 33.9 75.8 Cigarettes of the same specifications available on the market 15-29 45-70 Obviously, the above embodiments are merely examples for the purpose of clear explanation, and are not intended to limit the implementation methods. For those skilled in the art, other different forms of changes or modifications can be made based on the above description. It is not necessary and impossible to list all the implementation methods here. The obvious changes or modifications derived therefrom are still within the scope of protection of the invention.
Claims
1. A multiple filter cigarette holder, characterized in that: The filter cigarette holder is formed by a collection of melt-spun polylactic acid fibers and electrostatically spun polylactic acid fiber bundles. The core-sheath structure polylactic acid fibers and electrostatically spun polylactic acid fiber bundles are arranged alternately, and the electrostatically spun polylactic acid fiber bundles are bent in an "S" shape.
2. The multi-filter cigarette holder according to claim 1, characterized in that: The preparation method of the electrospun polylactic acid fiber bundle comprises the following steps: S11. Adding polylactic acid to dichloromethane and stirring to dissolve to obtain a 5.5-7wt% electrospinning solution; S12. The electrospinning solution was electrospun using a multi-needle classical spinning device to obtain an electrospinning fiber bundle, the voltage was 15 kV, the flow rate was 0.5-1 mL / h, and the receiving distance was 20 cm; S13. The electrospun fiber bundle is heat-treated in an "S"-structured mold to obtain an "S"-structured polylactic acid fiber bundle.
3. The multi-filter cigarette holder according to claim 2, characterized in that: In the step S3, the wavelength of the polylactic acid fiber bundle with "S" structure is 0.7-1.5 cm, the wave height is 0.3-0.6 cm, the heat setting temperature is 105-120° C., and the time is 10-30 s.
4. The method for preparing a multiple filter cigarette holder according to claim 1, characterized in that: The preparation method of the filter cigarette holder comprises the following steps: S1. Using low melting point polylactic acid as the cortex material and high melting point polylactic acid as the core material, the cortex material and the core material are dried and melted to obtain a cortex spinning solution and a core spinning solution, and fat chain grafted cellulose microspheres are added to the cortex spinning solution for spinning to obtain a sheath-core structure polylactic acid fiber; S2. The polylactic acid fibers and polylactic acid fiber bundles of the sheath-core structure are arranged alternately to obtain a cigarette holder tow, and then the cigarette holder is obtained by thermal bonding.
5. The method for preparing a multi-filter cigarette holder according to claim 4, characterized in that: The method for preparing the fat chain grafted cellulose microspheres comprises the following steps: S21. Add cellulose to 1-butyl-3-methylimidazole chloride, stir and dissolve to obtain a cellulose solution having a concentration of 6-8wt%; S22. Adding nano copper oxide particles to the cellulose solution and stirring to obtain a mixed solution; S23. Span80, Tween 80 and liquid paraffin are mixed in a mass ratio of 1:1:100, stirred and mixed evenly, and then the mixed solution prepared in step S2 is added dropwise to the above solution, stirred vigorously for emulsification, and then water is added to the suspension, and the cellulose microspheres are separated by cooling; S24. Adding the cellulose microspheres to a 0.05-0.1 mol / L hydrochloric acid solution, stirring to dissolve the copper oxide particles contained in the cellulose microspheres, and directly filtering to obtain porous cellulose microspheres; S25. Add the porous cellulose microspheres into the melted lauric acid so that the microspheres are completely immersed in the lauric acid liquid, then ultrasonically oscillate for 30-60 minutes to allow the solid microspheres to absorb fatty acids as much as possible, then vacuum filter and dry to obtain the fat-linked cellulose microspheres.
6. The method for preparing a multiple filter cigarette holder according to claim 4, characterized in that: In the step S1, the mass ratio of low-melting point polylactic acid to high-melting point polylactic acid is 50-70:30-50, the melting point of low-melting point polylactic acid is 115-130°C, the melting point of high-melting point polylactic acid is 150-170°C, the mass fraction of fat chain grafted cellulose microspheres in the sheath spinning solution is 5-8wt%, and the fineness of the sheath-core structure polylactic acid fiber is 11-22dtex.
7. The method for preparing a multiple filter cigarette holder according to claim 4, characterized in that: The ratio of the polylactic acid fibers of the sheath-core structure and the electrospun polylactic acid fiber bundles in the cigarette holder fiber bundle is 55-70:30-45.
8. The method for preparing a multiple filter cigarette holder according to claim 5, characterized in that: In step S22, the content of copper oxide in the mixed solution is 1-2 wt %.
9. The method for preparing a multiple filter cigarette holder according to claim 5, characterized in that: The rotation speed of the vigorous stirring in step S22 is 800-1200 r / min.
Citation Information
Patent Citations
Preparation method of titanium dioxide nano hollow ball
CN102786083A
Sheath-core polylactic acid tobacco tow and filter stick and preparation method thereof
CN103074716A
Filter tip bar including spiral absorption lines or spice lines and preparation method thereof
CN103156278A
Ultrahigh-adhesion fiber cigarette filter
CN103720043A
Lithium ion battery silica carbon-based cathode material and preparation method thereof
CN108899495A