Spraying control method and device for quick-setting rubber asphalt waterproof coating

Through intelligent spray control method, combined with the spray tube and paint attribute information, the injection speed and viscosity coefficient are dynamically adjusted, the problem of uneven spraying of fast-gel rubber asphalt waterproof coating is solved, and efficient waterproof construction and cost reduction are achieved.

CN119016227APending Publication Date: 2024-11-26河南新华五岳抽水蓄能发电有限公司 +1
View PDF 0 Cites 1 Cited by

Patent Information

Application Number
CN202411394301.7
Authority / Receiving Office
CN · China
Patent Type
Applications(China)
Current Assignee / Owner
Filing Date
2024-10-08
Publication Date
2024-11-26

AI Technical Summary

Technical Problem

During the construction of pumping dams, it is difficult for the existing technology to accurately control the spraying speed of fast-gel rubber asphalt waterproof coating with high viscosity, resulting in uneven spraying of the paint, unable to achieve reasonable waterproofing effects, and the existing control methods are inefficient and cannot achieve Reasonable jet operation.

Method used

Through intelligent spray control method, combined with the attribute information of the spray tube, coating and rapid detergent, the initial spray speed is calculated, and extreme empty defects and high-reverse defects are detected before spraying, and the nozzle diameter and rapid detergent viscosity coefficient are dynamically adjusted. , ensure accurate control of spray speed, achieve uniform distribution of paint and waterproofing effect.

Benefits of technology

The uniform distribution of the paint is achieved, the waterproofing effect and construction efficiency are improved, the cost is reduced, the rework and maintenance work is reduced, and the continuity and integrity of the waterproof coating is ensured.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure CN119016227A_ABST
    Figure CN119016227A_ABST
Patent Text Reader

Abstract

The invention discloses a spraying control method and device for quick-setting rubber asphalt waterproof paint, and relates to the field of spraying control. The method comprises the steps that in response to the received injection thickness input by a user, the first control injection amount on the unit area is calculated according to the injection thickness, detection information is obtained, and the detection information comprises injection pipe attribute information, rapid-hardening rubber asphalt waterproof coating attribute information and accelerator attribute information; calculating according to the first control injection amount and the detection information to obtain an initial injection speed; carrying out extreme vacant defect and high-reflection defect detection on the current test area; and when the extreme vacancy defect and the high reflection defect do not exist in the current test area, spraying the quick-setting rubber asphalt waterproof paint on the current test area according to the initial spraying speed. By implementing the technical scheme provided by the invention, the working quality and efficiency of the waterproof coating are guaranteed through reasonable spraying speed.
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] The present application relates to the technical field of spraying control, and in particular to a spraying control method and device for a quick-setting rubber asphalt waterproof coating. Background Art

[0002] Waterproofing is of vital importance in pumped dam construction projects. At present, a high-viscosity quick-setting rubber asphalt waterproof coating (referred to as mixed coating) is pumped into the dam area for waterproofing. This quick-setting rubber asphalt waterproof coating has high viscosity and contains a quick-setting agent. The spraying speed of this coating must be strictly controlled to ensure that the sprayed coating is continuous and has good low-reflection characteristics.

[0003] If the pump output spray speed is too fast, a large amount of paint will be sprayed out in a short time. At this time, the amount of spray waterproof paint cannot be accurately controlled. However, if the pump output spray speed is too slow, the spray paint will be continuously sprayed and have high-reflection characteristics, which will cause some areas of the sprayed surface to have no paint, and some areas of the sprayed surface to have too high a paint thickness. Then, too high a paint thickness will inevitably cause high-reflection characteristics. The main control method in the prior art is to set and adjust the spray speed based on experience, which will result in low efficiency of the spraying operation and fail to achieve reasonable control.

[0004] Therefore, a spraying control method capable of automatically regulating the spraying speed is needed. Summary of the invention

[0005] The present application provides a spray control method and device for quick-setting rubber asphalt waterproof coating, which fully considers the corresponding technical characteristics of quick-setting rubber asphalt waterproof coating spraying, such as viscosity, discontinuous spraying and high reflection, realizes intelligent coordinated control, and ultimately ensures the quality and efficiency of the continuous spraying operation of quick-setting rubber asphalt waterproof coating mixed coating.

[0006] In a first aspect of the present application, a spraying control method of a quick-setting rubber asphalt waterproof coating is provided, which is applied to a spraying control platform. The spraying control method comprises: In response to receiving the injection thickness input by the user, a first controlled injection amount per unit area is calculated according to the injection thickness, and detection information is acquired, wherein the detection information includes injection pipe attribute information, quick-setting rubber asphalt waterproof coating attribute information, and quick-setting agent attribute information; Calculating an initial injection speed according to the first controlled injection amount and the detection information; Conduct extreme empty defect and high reflection defect detection on the current test area; When there are no extreme empty defects and high reverse defects in the current test area, the quick-setting rubber asphalt waterproof coating is sprayed on the current test area according to the initial spraying speed.

[0007] By adopting the above technical solution, the first controlled injection amount per unit area is accurately calculated by responding to the injection thickness input by the user, and the injection speed is further optimized by combining the property information of the injection pipe, the coating and the quick-setting agent. This precise control method ensures the uniform distribution of the coating, avoids the waste and excessive use of the coating, and thus improves the utilization rate and waterproof effect of the coating. Before spraying, the current test area is tested for extreme empty defects and high-reflection defects to ensure that the spraying is carried out without any quality risks. This step effectively prevents coating defects caused by base problems and improves the overall quality of the waterproof coating. Through the automated spray control platform, the precise control of the spray speed and injection amount is achieved, reducing the dependence on manual operation and the interference of human factors. This not only improves the construction efficiency, but also reduces the construction cost and shortens the construction period. The embodiment of the present invention supports the adjustment of multiple spray thicknesses and coating properties, and can adapt to the needs of different construction environments and base conditions. At the same time, through the intelligent control platform, the spray parameters can be monitored and adjusted in real time to ensure the stability and reliability of the construction process.

[0008] Optionally, the calculating the initial injection speed according to the first controlled injection amount and the detection information includes: calculating the initial injection speed V according to the following formula: 初 : Among them, K1 is the variable proportional coefficient of the nozzle diameter, K1=d / D, K2 is the viscosity coefficient of the accelerator; d is the diameter of the injection pipe, D is the nozzle diameter, P is the outlet pressure of the injection pipe for spraying the quick-setting rubber asphalt waterproof coating, n is the rheological index of the quick-setting rubber asphalt waterproof coating, ρ is the density of the quick-setting rubber asphalt waterproof coating, m is the amount of accelerator, and Q is the first controlled injection amount.

[0009] By adopting the above technical solution, multiple factors affecting the injection speed are comprehensively considered, including the nozzle diameter variable proportional coefficient (K1), the viscosity coefficient of the accelerating agent (K2), the injection pipe diameter (d), the nozzle diameter (D), the outlet pressure (P), the rheological index (n), the coating density (ρ) and the amount of accelerating agent (m). This comprehensive consideration of multiple factors makes the calculated initial injection speed more accurate and can better adapt to the actual construction needs. The various parameters in the formula (such as nozzle diameter, outlet pressure, and amount of accelerating agent) are adjustable, which means that under different construction conditions, the injection speed can be optimized by adjusting these parameters to ensure uniform spraying and waterproofing effect of the coating. This flexibility improves the adaptability and practicality of the construction method. By accurately calculating the initial injection speed, it can be ensured that the utilization rate of the coating is maximized during the spraying process, reducing the waste of coating and the number of repeated spraying. This not only improves construction efficiency, but also reduces construction costs. Accurate injection speed control helps to form a uniform and continuous waterproof coating, avoiding coating defects and water leakage problems caused by uneven spraying. This is of great significance for improving the waterproof performance and service life of buildings.

[0010] Optionally, the detecting of extreme empty defects and high-reflection defects in the current test area includes: Capturing images of the current test area at intervals of a preset distance to obtain target image frames; Determine the similarity between the target image frame and the standard empty defect image, and when the similarity is greater than a similarity threshold, determine that the target image frame has an empty defect; When the ratio of the number of target image frames with empty defects to the total number of target image frames is greater than or equal to the standard number ratio threshold, it is determined that the current test area has an extreme empty defect; A flatness detection is performed on the current test area. If the flatness is less than or equal to a flatness threshold, it is determined that a high-reflection defect exists in the current test area.

[0011] By adopting the above technical solution, by collecting images of the current test area at each preset distance, the detailed information of the area can be fully covered and captured. Subsequently, the collected target image frame is compared with the standard empty defect image for similarity. This detection method based on image recognition has high accuracy and objectivity and can effectively identify empty defects. Furthermore, by counting the number of target image frames with empty defects and comparing them with the total number, the severity of the empty defects can be quantitatively evaluated. When the ratio exceeds the set standard number ratio threshold, it is determined to be an extreme empty defect. This method enhances the scientificity and accuracy of defect determination. Performing flatness detection on the current test area through the flatness detection method is an important part of evaluating construction quality. Flatness, as one of the important indicators of pavement or coating quality, directly affects its performance and durability. When the flatness is less than or equal to the flatness threshold, it is determined to be a high-reflection defect, which helps to promptly discover and correct possible problems in construction, thereby ensuring construction quality. By testing for extreme empty defects and high-reflective defects before spraying quick-setting rubber asphalt waterproof coatings, potential construction problems can be discovered and dealt with in advance to prevent these defects from adversely affecting subsequent construction and waterproofing effects. This helps to improve the overall construction quality control level and ensure the continuity and integrity of the waterproof coating. Through comprehensive testing of the test area, potential hazards that may affect construction safety can be discovered and dealt with in a timely manner. For example, empty defects may cause uneven coating thickness and easy breakage, which in turn affects the waterproofing effect and service life. High-reflective defects may cause safety hazards such as coating peeling and shedding.

[0012] Optionally, the spraying control method further includes: When an extreme empty defect and / or a high-reflection defect exists in the current test area, the nozzle diameter variable proportional coefficient and / or the quick-setting agent viscosity coefficient are adjusted until the extreme empty defect and / or the high-reflection defect are overcome, and the final nozzle diameter variable proportional coefficient and the final quick-setting agent viscosity coefficient are determined; The target injection speed is calculated according to the variable proportional coefficient of the final nozzle diameter and the viscosity coefficient of the final accelerating agent, and the quick-setting rubber asphalt waterproof coating is sprayed on the target test area according to the target injection speed.

[0013] By adopting the above technical solution, when an extreme empty defect or high reverse defect is detected, the nozzle diameter variable proportional coefficient (K1) and / or the viscosity coefficient of the quick-setting agent (K2) can be adjusted in real time. This dynamic adjustment capability makes the construction process more flexible, can quickly respond to changes in the base conditions, and ensure the uniform spraying of the coating and the integrity of the waterproof layer. By adjusting these key parameters, problems such as uneven surface of the base and poor fluidity of the coating can be overcome, thereby optimizing the spraying effect. For example, reducing the nozzle diameter or increasing the viscosity of the quick-setting agent may help reduce empty defects and improve the adhesion and flatness of the coating. By promptly discovering and handling defects, larger problems can be avoided in the subsequent construction process, thereby reducing rework and maintenance work. This not only improves construction efficiency, but also reduces construction costs. The optimized spraying parameters can ensure that the coating forms a continuous and uniform waterproof layer on the base, thereby improving waterproof performance and service life. The embodiment of the present invention applies intelligent technology to spraying control, and realizes precise spraying by automatically detecting and adjusting parameters. This intelligent control method reduces the interference of human factors and improves the controllability and stability of the construction process. After adjusting the parameters and determining the final spraying speed, the platform can automatically spray the target test area. This automated construction method not only improves construction efficiency, but also reduces the requirements for the skill level of construction personnel. By adjusting parameters such as nozzle diameter and viscosity coefficient of the quick-setting agent, the embodiment of the present invention can adapt to different types of base conditions (such as concrete, steel plate, masonry, etc.), thereby ensuring that the coating can form a good waterproof layer on various bases.

[0014] Optionally, the step of adjusting the nozzle diameter variable ratio coefficient and / or the quick-setting agent viscosity coefficient until overcoming the extreme empty defect and / or high-reverse defect comprises: When a high-reflection defect exists in the current test area, increasing the nozzle diameter variable proportional coefficient and / or the quick-setting agent viscosity coefficient; When an extreme empty defect exists in the current test area, the nozzle diameter variable proportional coefficient and / or the quick-setting agent viscosity coefficient are reduced.

[0015] By adopting the above technical solution, when there is a high-reflection defect in the test area, the fluidity and adhesion of the paint can be improved by increasing the nozzle diameter variable ratio coefficient (K1) and / or the accelerator viscosity coefficient (K2). The increased nozzle diameter allows more paint to be sprayed out in a shorter time, which helps to fill the tiny depressions or uneven parts on the surface of the base layer and improve the flatness of the coating. At the same time, increasing the accelerator viscosity coefficient can enhance the adhesion of the paint, reduce the splashing and loss of the paint during the spraying process, and further improve the flatness and density of the coating. On the contrary, when there is an extreme empty defect in the test area, reducing the nozzle diameter variable ratio coefficient (K1) and / or the accelerator viscosity coefficient (K2) is an effective solution. The reduced nozzle diameter can reduce the amount of paint sprayed in a single spray, make the paint more evenly distributed on the surface of the base layer, and reduce the empty area. At the same time, reducing the accelerator viscosity coefficient can make the paint easier to flow and penetrate into the tiny pores of the base layer, fill the empty part, and improve the density and waterproof performance of the coating. By precisely adjusting the nozzle diameter and the viscosity coefficient of the quick-setting agent, it is possible to ensure that the coating forms a uniform and continuous waterproof layer during the spraying process. This not only helps to improve the waterproof performance and service life of the coating, but also reduces rework and repair work caused by uneven coating, and improves construction efficiency and quality.

[0016] Optionally, the step of adjusting the nozzle diameter variable ratio coefficient and / or the quick-setting agent viscosity coefficient until the extreme empty defect and / or high-reverse defect is overcome further comprises: When the current test area has a high-reflection defect and an extreme empty defect, the viscosity coefficient of the quick-setting agent is kept unchanged and the variable proportional coefficient of the nozzle diameter is gradually changed, and a first defect detection is performed after each change of the variable proportional coefficient of the nozzle diameter; when all available variable proportional coefficients of the nozzle diameter have been used and there are still high-reflection defects and / or extreme empty defects, the target variable proportional coefficient of the nozzle diameter is determined according to the result of the first defect detection, the variable proportional coefficient of the nozzle diameter is kept as the target variable proportional coefficient of the nozzle diameter, and the viscosity coefficient of the quick-setting agent is gradually changed, and a second defect detection is performed after each change of the viscosity coefficient of the quick-setting agent; Until there is no high-reflection defect and / or extreme empty defect in the current test area, or the value adjustment of the viscosity coefficient of the quick-setting agent reaches the upper threshold limit and the lower threshold limit.

[0017] By adopting the above technical solution, the viscosity coefficient of the quick-setting agent is first kept unchanged, the variable proportional coefficient of the nozzle diameter is gradually changed, and the first defect detection is performed after each change. This step-by-step adjustment method helps to evaluate the influence of the nozzle diameter on the spraying effect separately, so as to find the key point to solve the problem more accurately. When all available variable proportional coefficients of the nozzle diameter have been tried and the problem is still not solved, the viscosity coefficient of the quick-setting agent is gradually changed and the second defect detection is performed. This comprehensive adjustment method ensures the comprehensive optimization of the spraying parameters from multiple angles and increases the possibility of solving the problem. By gradually changing the parameters and performing defect detection, the key factors causing the defects can be quickly identified, avoiding blind attempts and wasting resources. By carefully adjusting and optimizing the spraying parameters, the spraying effect can be significantly improved, and the uniformity, flatness and density of the coating can be improved. The optimized spraying parameters help to form a continuous and complete waterproof layer, improving the waterproof performance and service life of the building.

[0018] Optionally, the spraying control method further includes: When the numerical adjustment of the viscosity coefficient of the quick-setting agent reaches the upper and lower limits of the threshold, the target viscosity coefficient of the quick-setting agent is determined according to the result of the second defect detection, the nozzle diameter variable proportional coefficient is kept as the target nozzle diameter variable proportional coefficient and the quick-setting agent viscosity coefficient is kept as the target quick-setting agent viscosity coefficient, the power of the power pump is gradually adjusted to change the outlet pressure of the sprayed quick-setting rubber asphalt waterproof coating at the injection pipe, and a third defect detection is performed after each change in the outlet pressure until there is no high-reverse defect and / or extreme empty defect in the current test area; When the adjustment range of the outlet pressure reaches the preset adjustment range, the power pump is shut down.

[0019] By adopting the above technical solution and gradually adjusting the power of the power pump, the outlet pressure of the sprayed quick-setting rubber asphalt waterproof coating can be finely controlled. This precise adjustment helps to reduce spraying quality problems caused by pressure fluctuations, such as uneven coating thickness, sagging, pinholes, etc. Performing a third defect detection after each change in the outlet pressure can promptly detect and correct potential quality problems and ensure that the overall quality of the coating meets the expected standards. After the viscosity coefficient of the quick-setting agent and the variable proportional coefficient of the nozzle diameter reach the optimal value, the outlet pressure is further optimized by adjusting the power pump power, which is actually a comprehensive optimization of the spraying process parameters. This optimization helps to improve the utilization rate of the coating, reduce waste, and reduce construction costs.

[0020] In a second aspect of the present application, a spray control system for a quick-setting rubber asphalt waterproof coating is provided, comprising an information module, an initial module, a detection module and an execution module, wherein: An information module configured to calculate a first controlled injection amount per unit area according to the injection thickness in response to receiving the injection thickness input by a user, and to obtain detection information, wherein the detection information includes injection pipe attribute information, quick-setting rubber asphalt waterproof coating attribute information, and quick-setting agent attribute information; an initial module, configured to calculate an initial injection speed according to the first controlled injection amount and the detection information; An inspection module configured to inspect the current test area for extreme empty defects and high-reflection defects; The execution module is configured to spray the quick-setting rubber asphalt waterproof coating on the current test area according to the initial spraying speed when there are no extreme empty defects and high reverse defects in the current test area.

[0021] In the third aspect of the present application, an electronic device is provided, including a processor, a memory, a user interface and a network interface, the memory is used to store instructions, the user interface and the network interface are both used to communicate with other devices, and the processor is used to execute the instructions stored in the memory so that the electronic device executes any one of the methods described above.

[0022] In a fourth aspect of the present application, a computer-readable storage medium is provided, wherein the computer-readable storage medium stores instructions, and when the instructions are executed, any of the methods described above is executed.

[0023] In summary, one or more technical solutions provided in the embodiments of the present invention have at least the following technical effects or advantages: 1. By responding to the injection thickness input by the user, the first control injection amount per unit area is intelligently calculated. This step ensures the accuracy of the injection amount and avoids errors caused by human estimation or empirical judgment. In the calculation process, multiple factors such as the injection pipe property information, the quick-setting rubber asphalt waterproof coating property information and the quick-setting agent property information are also comprehensively considered, making the determination of the injection amount more scientific and reasonable; 2. Based on the first controlled spray volume and detection information, the platform can calculate the initial spray speed. This speed setting helps to achieve uniform and rapid spraying of the paint and improve construction efficiency. Before spraying, the current test area is tested for extreme empty defects and high-reflection defects. Only when there are no such defects in the area, the spraying operation is carried out. This real-time detection and adjustment mechanism ensures the efficiency and quality stability of the spraying operation. 3. Through the detection of extreme empty defects and high reflection defects, coating defects caused by uneven base or paint fluidity problems are effectively prevented, thereby ensuring the overall quality of the waterproof coating; precise spray volume control and appropriate spray speed enable the paint to be evenly distributed on the surface of the base, forming a continuous and dense waterproof layer, improving the waterproof effect and service life; 4. Avoiding the waste of paint due to excessive or insufficient spray volume, saving material costs; through strict quality control and defect prevention, reducing rework and maintenance work caused by coating quality problems, further reducing construction costs. BRIEF DESCRIPTION OF THE DRAWINGS

[0024] Figure 1 It is a flow chart of a spraying control method of a quick-setting rubber asphalt waterproof coating disclosed in an embodiment of the present invention; Figure 2 It is a structural schematic diagram of a spray control platform disclosed in an embodiment of the present invention from one perspective; Figure 3 is a structural schematic diagram of the spray control platform disclosed in an embodiment of the present invention from another perspective; Figure 4 It is a schematic diagram of a process of detecting extreme empty defects and high-reflection defects in a current test area disclosed in an embodiment of the present invention; Figure 5 It is a schematic diagram of a process for adjusting a nozzle diameter variable proportional coefficient and / or a quick-setting agent viscosity coefficient disclosed in an embodiment of the present invention; Figure 6 It is another schematic diagram of a process for adjusting the variable proportional coefficient of nozzle diameter and / or the viscosity coefficient of the quick-setting agent disclosed in an embodiment of the present invention; Figure 7 It is another schematic diagram of a process for adjusting the variable proportional coefficient of nozzle diameter and / or the viscosity coefficient of the quick-setting agent disclosed in an embodiment of the present invention; Figure 8 It is a schematic diagram of a flow chart of adjusting the outlet pressure disclosed in an embodiment of the present invention; Fig. 9 It is a module schematic diagram of a spraying control system of a quick-setting rubber asphalt waterproof coating disclosed in an embodiment of the present invention; Fig.10 It is a structural schematic diagram of an electronic device disclosed in an embodiment of the present invention.

[0025] Explanation of the reference numerals: 901, information module; 902, initial module; 903, detection module; 904, execution module; 1001, processor; 1002, communication bus; 1003, user interface; 1004, network interface; 1005, memory. DETAILED DESCRIPTION

[0026] In order to enable technicians in this field to better understand the technical solutions in this specification, the technical solutions in the embodiments of this specification will be clearly and completely described below in conjunction with the drawings in the embodiments of this specification. Obviously, the described embodiments are only part of the embodiments of this application, not all of the embodiments.

[0027] In the description of the embodiments of the present invention, words such as "for example" or "for example" are used to indicate examples, illustrations or explanations. Any embodiment or design described as "for example" or "for example" in the embodiments of the present invention should not be interpreted as being more preferred or more advantageous than other embodiments or designs. Specifically, the use of words such as "for example" or "for example" is intended to present related concepts in a specific way.

[0028] In the description of the embodiments of the present invention, the term "multiple" means two or more. For example, multiple systems refer to two or more systems, and multiple screen terminals refer to two or more screen terminals. In addition, the terms "first" and "second" are used for descriptive purposes only and cannot be understood as indicating or implying relative importance or implicitly indicating the indicated technical features. Thus, the features defined as "first" and "second" may explicitly or implicitly include one or more of the features. The terms "include", "comprise", "have" and their variations all mean "including but not limited to", unless otherwise specifically emphasized.

[0029] This embodiment discloses a spraying control method of a quick-setting rubber asphalt waterproof coating. Figure 1 : is a flow chart of a spraying control method of a quick-setting rubber asphalt waterproof coating disclosed in an embodiment of the present invention, such as Figure 1 As shown, the method comprises the following steps: S110, in response to receiving the injection thickness input by the user, calculating a first controlled injection amount per unit area according to the injection thickness, and acquiring detection information, the detection information including injection pipe attribute information, quick-setting rubber asphalt waterproof coating attribute information, and quick-setting agent attribute information; Figure 2 is a structural schematic diagram of a spray control platform disclosed in an embodiment of the present invention from one perspective, Figure 3 is a schematic diagram of the structure of the spray control platform disclosed in an embodiment of the present invention from another perspective, such as Figure 2 and Figure 3As shown, the spray control platform includes a mobile vehicle-mounted platform 201 and a support frame 202 installed on the mobile vehicle-mounted platform 201, a spray pipe 203, a nozzle 204 installed at the end of the spray pipe 203, a controller panel installed on the mobile vehicle-mounted platform 201 (not shown in the figure), an image acquisition detection unit 206, a power pump 207 and a paint stirring barrel 208. The power pump 207 is connected to the spray pipe 203. The power pump 207 is an original power output device, which is a common variable frequency power pump; wherein the main control system is the controller panel. Combined with Figure 2 and Figure 3 The embodiments of the present invention are described.

[0030] The controller panel receives the control command input by the user and parses the control command to obtain the required spraying thickness, and the preset model calculates the first control spraying amount per unit area according to the spraying thickness. The control command is parsed to obtain the property information of the quick-setting agent, the property information of the quick-setting rubber asphalt waterproof coating and the property information of the spray pipe, the property information of the quick-setting rubber asphalt waterproof coating includes the rheological index of the quick-setting rubber asphalt waterproof coating, and the property information of the spray pipe includes the diameter of the spray pipe, the diameter of the nozzle and the variable proportional coefficient of the nozzle diameter; at the same time, the detection command is executed to detect and obtain the property information of the spray pipe, and the property information of the spray pipe includes the outlet pressure of the spray pipe spraying the quick-setting rubber asphalt waterproof coating and the density of the quick-setting rubber asphalt waterproof coating.

[0031] Specifically, the injection pipe attribute information includes the injection pipe diameter d and the nozzle diameter D, the outlet pressure P of the injection pipe for spraying quick-setting rubber asphalt waterproof coating, and the variable proportional coefficient K1 of the nozzle diameter; the quick-setting rubber asphalt waterproof coating attribute information includes the quick-setting rubber asphalt waterproof coating rheological index n and the quick-setting rubber asphalt waterproof coating density ρ; the accelerator attribute information includes the accelerator dosage m and the accelerator viscosity coefficient K2.

[0032] Before obtaining the injection pipe property information, the quick-setting rubber asphalt waterproof coating property information and the quick-setting agent property information, it also includes: setting a pre-processing buffer time period through the controller panel 205, starting the power pump for power output, and starting the timing, and after the nozzle sprays the quick-setting rubber asphalt waterproof coating continuously within the pre-processing buffer time period, the injection pipe property information, the quick-setting rubber asphalt waterproof coating property information and the quick-setting agent property information are obtained.

[0033] S120, calculating an initial injection speed according to the first controlled injection amount and the detection information; Optionally, the calculating the initial injection speed according to the first controlled injection amount and the detection information includes: The initial injection velocity V is calculated according to the following formula 初 : Among them, K1 is the variable proportional coefficient of the nozzle diameter, K1=d / D, K2 is the viscosity coefficient of the accelerator; d is the diameter of the injection pipe, D is the nozzle diameter, P is the outlet pressure of the injection pipe for spraying the quick-setting rubber asphalt waterproof coating, n is the rheological index of the quick-setting rubber asphalt waterproof coating, ρ is the density of the quick-setting rubber asphalt waterproof coating, m is the amount of accelerator, and Q is the first controlled injection amount.

[0034] S130, performing extreme empty defect and high reflection defect detection on the current test area; High reflection defect is caused by too high injection speed, and extreme empty defect is caused by too low injection speed, so when high reflection defect and / or extreme empty defect occur, it is necessary to adjust the initial injection speed. Empty defect specifically refers to the fact that the nozzle nozzle sprays the paint not continuously due to other reasons such as too low injection speed, and there will be blank areas without paint in the area. This area is an empty defect. High reflection defect is the "high rebound amount" in the spraying operation of quick-setting rubber asphalt waterproof coating. Specifically, it means that during the spraying process, a large amount of quick-setting rubber asphalt waterproof coating rebounds from the base surface instead of being firmly attached to the base surface, causing the base surface to be uneven, affecting the waterproof effect of the waterproof coating. The high rebound phenomenon usually leads to the following problems: 1. Low spraying efficiency: a large amount of quick-setting rubber asphalt waterproof coating is not attached to the target base surface, but is wasted, reducing the overall efficiency of the operation; 2. Poor quality of the spray layer: the quick-setting rubber asphalt waterproof coating that bounces back does not have good embedding properties, which will cause problems such as roughness, looseness, and low strength of the spray layer surface; 3. Uneven spray surface: a large number of rebound objects will cause the surface of the spray layer to be uneven, affecting the subsequent leveling and decoration process. Through further research, the embodiments of the present invention found that the main reasons for the high rebound amount include: 1. Improper spraying parameters: such as excessive pressure, excessive outlet speed, etc., resulting in excessive spraying speed; 2. Improper base surface treatment: such as the base surface is too smooth, incomplete cleaning, etc.; 3. Unreasonable mix ratio of quick-setting rubber asphalt waterproof coating: such as too low viscosity, poor aggregate particle size distribution, etc. The embodiment of the present invention mainly adopts reasonable management and control of the spraying speed.

[0035] Optionally, the detecting of extreme empty defects and high-reflection defects in the current test area includes: Capturing images of the current test area at intervals of a preset distance to obtain target image frames; Determine the similarity between the target image frame and the standard empty defect image, and when the similarity is greater than a similarity threshold, determine that the target image frame has an empty defect; When the ratio of the number of target image frames with empty defects to the total number of target image frames is greater than or equal to the standard number ratio threshold, it is determined that the current test area has an extreme empty defect; A flatness detection is performed on the current test area. If the flatness is less than or equal to a flatness threshold, it is determined that a high-reflection defect exists in the current test area.

[0036] Figure 4 is a schematic diagram of a process for detecting extreme empty defects and high-reflection defects in the current test area disclosed in an embodiment of the present invention, such as Figure 4 As shown, the image acquisition and detection unit 206 is used to regularly acquire images of the current test area. For example, the image acquisition and detection unit 206 can be used to capture images at a preset distance to ensure that the test area can be fully covered and sufficient real-time image frames (i.e., target image frames) can be acquired. Real-time images of the test area are acquired for subsequent defect analysis. The acquired real-time image frames are compared with the empty defect images stored in the standard database. The similarity between the local image in the real-time image frame and the standard empty defect image is calculated by an algorithm. When the calculated similarity is greater than the preset similarity threshold, it is considered that there is an empty defect in the real-time image frame. The empty defect in the test area is identified to provide basic data for subsequent overall evaluation. All real-time image frames in the test area are continuously detected, and the number of real-time image frames with empty defects is counted and compared with the total number of real-time image frames. If the ratio of the number of real-time image frames with empty defects to the total number of image frames is greater than or equal to the preset standard number ratio threshold, it is determined that the entire test area has an extreme empty defect. The severity of the empty defect in the test area is evaluated to determine whether further remedial measures are needed. The flatness detection method is used to perform flatness detection on the current test area. Flatness is an important indicator to measure the smoothness of the surface, and is of great significance for detecting high-reflection defects. If the detected flatness is less than or equal to the preset flatness threshold, it is determined that there is a high-reflection defect in the test area. Identify the high-reflection problem caused by the uneven surface in the test area to ensure that the spraying quality meets the requirements.

[0037] The following methods can usually be used to detect high-reflection defects: Flatness detection method: During the spraying process, carefully observe the spraying surface to see if there are a large number of quick-setting rubber asphalt waterproof coating splashes and rebound objects; these large rebound objects will significantly reduce the flatness and density of the sprayed surface. Laser scanning flatness detection method can also be used: using laser scanning equipment to perform three-dimensional scanning of the surface can obtain more detailed flatness information.

[0038] Collect sample analysis method: collect rebound samples of a certain area and weight on the spray surface; by performing density testing and particle size analysis on the samples, the amount of rebound can be quantified.

[0039] Laser beam detection method: Use X-ray or gamma-ray imaging technology to scan the sprayed surface; it can clearly show the distribution of surface rebound objects.

[0040] High-speed camera image online monitoring method: Install sensors on the spray robot or manual spray gun; through video frame image detection, monitor the changes in the rebound amount during the spraying process in real time and provide data feedback.

[0041] Through these detection methods, high-rebound defect problems can be discovered in time, and then corresponding measures can be taken to optimize the spraying process, reduce the rebound amount, and improve the spraying quality. For this purpose, the embodiment of the present invention preferably uses a flatness detection method, a laser ray detection method, or a high-speed camera image online monitoring method, and the specific implementation process will not be repeated. As long as the rebound amount can be guaranteed to be low and the compressive strength of the sprayed quick-setting rubber asphalt waterproof coating will not be significantly reduced, the ultimate control purpose is sufficient.

[0042] Through the preset image acquisition interval and image processing algorithm, the test area is automatically inspected, avoiding the subjectivity and errors that may be caused by manual inspection. The image frames of the test area can be acquired in real time and compared with the standard database to quickly identify the empty defects, improving the inspection efficiency and accuracy. By calculating the ratio of the number of target image frames with empty defects to the total number of image frames, the severity of the empty defects in the test area is quantitatively evaluated. When the ratio exceeds the preset threshold, it can be determined as an extreme empty defect, providing a clear basis for subsequent improvement measures. The flatness detection method is used to quantitatively evaluate the surface quality of the test area, effectively identifying the surface unevenness that may cause high-reflection defects. The immediate feedback of the test results enables the operator to understand the problems in the spraying process in a timely manner, so as to adjust the spraying parameters, repair the nozzle problems or improve the substrate pretreatment process to ensure the quality of subsequent spraying operations. By accumulating test data, the spraying process can be continuously optimized to improve production efficiency and product quality.

[0043] Optionally, the spraying control method further includes: When an extreme empty defect and / or a high-reflection defect exists in the current test area, the nozzle diameter variable proportional coefficient and / or the quick-setting agent viscosity coefficient are adjusted until the extreme empty defect and / or the high-reflection defect are overcome, and the final nozzle diameter variable proportional coefficient and the final quick-setting agent viscosity coefficient are determined; The target injection speed is calculated according to the variable proportional coefficient of the final nozzle diameter and the viscosity coefficient of the final accelerating agent, and the quick-setting rubber asphalt waterproof coating is sprayed on the target test area according to the target injection speed.

[0044] The nozzle diameter is a key factor affecting the spray coverage and the uniformity of the coating distribution. By adjusting the variable ratio coefficient of the nozzle diameter, the effective spray area of ​​the nozzle can be changed to optimize the coating coverage. For example, increasing the nozzle diameter can improve the coating coverage and help reduce the void defects; while reducing the nozzle diameter may improve the coating distribution uniformity and reduce the risk of high-reflection defects. The viscosity of the accelerator has an important impact on the fluidity and adhesion of the coating. Adjusting the viscosity coefficient of the accelerator can change the fluidity and adhesion of the coating, thereby affecting the spraying effect. Appropriately reducing the viscosity of the accelerator can improve the fluidity of the coating, making it easier to penetrate the surface of the substrate and reduce void defects; while increasing the viscosity of the accelerator may enhance the adhesion of the coating, improve surface flatness, and reduce the risk of high-reflection defects. After the above adjustments, the system will gradually determine the final nozzle diameter variable ratio coefficient and the final accelerator viscosity coefficient that can overcome extreme void defects and / or high-reflection defects through multiple tests and tests. These final parameters will serve as the baseline parameters for subsequent spraying operations. Based on the finalized variable ratio coefficient of nozzle diameter and viscosity coefficient of quick-setting agent, the target spraying speed is recalculated. This new target spraying speed will ensure uniform and rapid spraying of the coating without defects in the test area. Finally, according to the recalculated target spraying speed, the platform will spray the quick-setting rubber asphalt waterproof coating on the target test area.

[0045] When an extreme empty defect or high-reflection defect is detected, the current spraying conditions are adapted by adjusting the nozzle diameter variable ratio coefficient and / or the viscosity coefficient of the accelerating agent. This real-time adjustment capability ensures the flexibility and accuracy of the spraying process. Through continuous trials and adjustments, the optimal nozzle diameter variable ratio coefficient and the viscosity coefficient of the accelerating agent are finally determined. These optimized parameters can more effectively cover the test area, reduce empty defects, and improve the flatness and glossiness of the coating, thereby overcoming the high-reflection defect. By adjusting the spraying parameters, the occurrence of extreme empty defects and high-reflection defects can be significantly reduced, and the spraying quality can be improved. This helps to ensure the uniformity, adhesion and durability of the coating, and meet the design requirements and usage requirements. The optimized spraying parameters can ensure consistent spraying effects between different test areas and batches, and improve the overall quality and consistency of the product. The embodiment of the present invention combines intelligent technologies such as image acquisition, defect recognition, and parameter adjustment to achieve automation and intelligent control of the spraying process. This helps to improve the intelligence level of the production line and reduce dependence on manual operation.

[0046] Optionally, the step of adjusting the nozzle diameter variable ratio coefficient and / or the quick-setting agent viscosity coefficient until overcoming the extreme empty defect and / or high-reverse defect comprises: When a high-reflection defect exists in the current test area, increasing the nozzle diameter variable proportional coefficient and / or the quick-setting agent viscosity coefficient; When an extreme empty defect exists in the current test area, the nozzle diameter variable proportional coefficient and / or the quick-setting agent viscosity coefficient are reduced.

[0047] Figure 5 is a schematic diagram of a process for adjusting the nozzle diameter variable ratio coefficient and / or the viscosity coefficient of the quick-setting agent disclosed in an embodiment of the present invention, such as Figure 5 As shown, if the detection finds that the current test area has a high-reflection defect, the injection speed of the current test area is adjusted to be reduced. Specifically, the nozzle with a larger nozzle diameter than the current one is gradually replaced to obtain the value of K1, and the value of K2 is gradually increased; after each adjustment, K1 and K2 are updated to obtain the latest value of the injection speed formula executed by the preset model, and the injection operation test of the new test area is performed for the latest value of the injection speed after each update to verify whether there are extreme empty defects and high-reflection defects.

[0048] Figure 6 is another flow chart of adjusting the nozzle diameter variable ratio coefficient and / or the viscosity coefficient of the quick-setting agent disclosed in the embodiment of the present invention, such as Figure 6 As shown, if the detection finds that the current test area has an extreme empty defect, the injection speed of the current test area is adjusted to increase the feedback. Gradually replace the nozzle with a smaller nozzle diameter than the current one to obtain the value of K1, and gradually reduce the value of K2; after each adjustment, update the latest value of the injection speed formula executed by the preset model, and perform the injection operation test of the new test area for the latest value of the injection speed after each update to verify whether there is an extreme empty defect and a high-reflection defect.

[0049] By adopting different adjustment strategies according to the defect type (high reflection or extreme empty), problems that occur during the spraying process can be solved more accurately and the spraying quality can be improved. After adjusting the nozzle diameter variable ratio coefficient and the quick-setting agent viscosity coefficient, the coating's coverage area, adhesion, and fluidity properties are optimized, making the spraying effect more uniform and smooth, and reducing the occurrence of defects. By real-time detection and adjustment of spraying parameters, rework and maintenance work caused by quality problems can be reduced, production efficiency can be improved, and costs can be reduced. At the same time, the optimized spraying parameters also help to improve the utilization rate of the coating and reduce waste.

[0050] Optionally, the step of adjusting the nozzle diameter variable ratio coefficient and / or the quick-setting agent viscosity coefficient until the extreme empty defect and / or high-reverse defect is overcome further comprises: When the current test area has a high-reflection defect and an extreme empty defect, the viscosity coefficient of the quick-setting agent is kept unchanged and the variable proportional coefficient of the nozzle diameter is gradually changed, and a first defect detection is performed after each change of the variable proportional coefficient of the nozzle diameter; when all available variable proportional coefficients of the nozzle diameter have been used and there are still high-reflection defects and / or extreme empty defects, the target variable proportional coefficient of the nozzle diameter is determined according to the result of the first defect detection, the variable proportional coefficient of the nozzle diameter is kept as the target variable proportional coefficient of the nozzle diameter, and the viscosity coefficient of the quick-setting agent is gradually changed, and a second defect detection is performed after each change of the viscosity coefficient of the quick-setting agent; Until there is no high-reflection defect and / or extreme empty defect in the current test area, or the value adjustment of the viscosity coefficient of the quick-setting agent reaches the upper threshold limit and the lower threshold limit.

[0051] You only need to change the nozzle diameter size to get a new K1 parameter. However, if you reduce or increase the viscosity (i.e. adjust K2), you need to re-stir the paint and mix a new proportion of the quick-setting rubber asphalt waterproof paint. Therefore, the embodiment of the present invention specifies K1 (nozzle diameter variable proportional coefficient) as the first priority adjustment parameter, and K2 (accelerator viscosity coefficient) as the second priority adjustment parameter. This means that during the adjustment process, you will first try to solve the problem by changing K1. Figure 7 is another flow chart of adjusting the nozzle diameter variable ratio coefficient and / or the viscosity coefficient of the quick-setting agent disclosed in the embodiment of the present invention, such as Figure 7 As shown, when a high-reflection defect and / or an extreme empty defect is detected in the current test area, K2 is kept unchanged, and a nozzle with a smaller nozzle diameter than the current one is gradually replaced to obtain different K1 values. After each replacement, a first defect detection is performed, that is, whether a high-reflection defect and / or an extreme empty defect still exists. If the defect-free condition cannot be met after trying all available nozzle diameters (that is, all K1 values), the second priority adjustment parameter K2 needs to be started at this time. This means that the adjustment of K1 has reached its limit, and the adjustment of K2 is needed to further improve the spraying effect. On the premise of keeping K1 as the current optimal value (that is, the variable proportional coefficient of the target nozzle diameter determined according to the first defect detection result), the value of K2 is gradually changed. After each change, a second defect detection is performed to verify whether the high-reflection defect and / or the extreme empty defect are resolved. The adjustment process will continue until there are no high-reflection defects and / or extreme empty defects in the current test area, or the numerical adjustment of K2 reaches the preset upper and lower threshold limits. This means that the adjustment process will stop when either of these two conditions is met.

[0052] By adjusting the nozzle diameter variable ratio coefficient (K1) first and then the accelerator viscosity coefficient (K2) priority setting, the system can more efficiently locate and solve defects in the spraying process. This step-by-step strategy avoids the inefficiency that may be caused by blindly adjusting multiple parameters. After each parameter adjustment, defect detection is performed to ensure that each adjustment accurately reflects the impact on the spraying effect. This immediate feedback mechanism helps to quickly find the optimal parameter combination to overcome high-reflection defects and extreme empty defects. When all available nozzle diameter variable ratio coefficients have been tried and still cannot solve the problem, the system can automatically switch to the stage of adjusting the accelerator viscosity coefficient. This comprehensive adjustment strategy ensures that an effective solution can be found even under complex and changing spraying conditions. The entire adjustment process can be automated through dynamic feedback from the controller panel, reducing the need for manual intervention. This not only improves production efficiency, but also reduces the risk of human error. The platform allows the adjustment to stop when the numerical adjustment of the accelerator viscosity coefficient reaches the upper and lower thresholds. This flexible adjustment range ensures that the platform can find the optimal solution within a reasonable parameter range and avoid other problems caused by excessive parameter adjustment. By precisely adjusting the nozzle diameter variable ratio coefficient and the accelerator viscosity coefficient, the platform can significantly improve the spraying effect and reduce the occurrence of high reflection defects and extreme empty defects. This helps to improve the spraying quality and product consistency and meet higher quality requirements.

[0053] Optionally, the spraying control method further includes: When the numerical adjustment of the viscosity coefficient of the quick-setting agent reaches the upper and lower limits of the threshold, the target viscosity coefficient of the quick-setting agent is determined according to the result of the second defect detection, the nozzle diameter variable proportional coefficient is kept as the target nozzle diameter variable proportional coefficient and the quick-setting agent viscosity coefficient is kept as the target quick-setting agent viscosity coefficient, the power of the power pump is gradually adjusted to change the outlet pressure of the sprayed quick-setting rubber asphalt waterproof coating at the injection pipe, and a third defect detection is performed after each change in the outlet pressure until there is no high-reverse defect and / or extreme empty defect in the current test area; When the adjustment range of the outlet pressure reaches the preset adjustment range, the power pump is shut down.

[0054] Figure 8 is a schematic diagram of a flow chart of adjusting the outlet pressure disclosed in an embodiment of the present invention, such as Figure 8As shown, when the value adjustment of the viscosity coefficient of the quick-setting agent (K2) reaches its upper threshold or lower threshold, a target viscosity coefficient of the quick-setting agent is determined according to the previous second defect detection result. At the same time, the nozzle diameter variable proportional coefficient (K1) is also maintained as the target nozzle diameter variable proportional coefficient determined previously. Under the premise of keeping K1 and K2 as their respective target values, the power of the power pump is gradually adjusted. This is achieved by a variable frequency power regulator to change the outlet pressure of the quick-setting rubber asphalt waterproof coating sprayed at the injection pipe. After each adjustment of the power pump power, the latest value of the injection speed formula is updated, and the injection operation test of the new test area is performed. At this time, the third defect detection is performed to verify whether there are still high-reverse defects and / or extreme empty defects in the current test area. The power pump power is adjusted and the third defect detection is performed continuously until there are no high-reverse defects and / or extreme empty defects in the current test area, or the adjustment range of the outlet pressure reaches the preset adjustment range threshold. If the adjustment range of the outlet pressure reaches the preset adjustment range threshold, but there are still defects in the current test area, the power pump should be shut down. This is to avoid possible damage to the equipment due to over-regulation, but also to save energy and reduce unnecessary wear. Or if a defect-free condition has been achieved, regulation can be stopped at this time.

[0055] When the value adjustment of the viscosity coefficient of the quick-setting agent (K2) reaches its upper threshold or lower threshold, a target viscosity coefficient of the quick-setting agent is determined according to the previous second defect detection result. At the same time, the nozzle diameter variable proportional coefficient (K1) is also maintained as the target nozzle diameter variable proportional coefficient determined previously. On the premise of maintaining K1 and K2 as their respective target values, the power of the power pump is gradually adjusted. This is achieved by a variable frequency power regulator to change the outlet pressure of the quick-setting rubber asphalt waterproof coating sprayed at the injection pipe. After each adjustment of the power pump power, the latest value of the injection speed formula is updated, and the injection operation test of the new test area is performed. At this time, the third defect detection is performed to verify whether the current test area still has high-reverse defects and / or extreme empty defects. The power pump power is adjusted and the third defect detection is performed continuously until the current test area no longer has high-reverse defects and / or extreme empty defects, or the adjustment range of the outlet pressure reaches the preset adjustment range threshold. If the adjustment range of the outlet pressure reaches the preset adjustment range threshold, but the current test area still has defects, or the defect-free condition has been achieved, the power pump should be shut down. This is to avoid possible damage to the equipment due to over-adjustment, as well as to save energy and reduce unnecessary wear.

[0056] S140. When there are no extreme empty defects and high-reflection defects in the current test area, spray the quick-setting rubber asphalt waterproof coating on the current test area according to the initial spraying speed.

[0057] If the current test area itself does not have extreme empty defects and high-reflection defects, or if the current test area does not have extreme empty defects and high-reflection defects after adjustment, this indicates that the current spraying parameter combination (including nozzle diameter, viscosity coefficient of quick-setting agent, and power pump power, etc.) can meet the spraying quality requirements of the area. After confirming the defect-free state, the quick-setting rubber asphalt waterproof coating can be sprayed on the current test area according to the initial spraying speed or the target spraying speed confirmed after adjustment. During the spraying process, it is necessary to ensure the stability of the spraying parameters to avoid reintroducing defects due to parameter fluctuations. Therefore, the operating status of the spraying equipment should be closely monitored to promptly detect and resolve possible abnormal situations.

[0058] This embodiment also discloses a spray control system for a quick-setting rubber asphalt waterproof coating. Fig. 9 Schematic diagram of a module of a spray control system for a quick-setting rubber asphalt waterproof coating disclosed in an embodiment of the present invention, such as Fig. 9 As shown, the system includes an information module, an initial module, a detection module and an execution module, wherein: An information module configured to calculate a first controlled injection amount per unit area according to the injection thickness in response to receiving the injection thickness input by a user, and to obtain detection information, wherein the detection information includes injection pipe attribute information, quick-setting rubber asphalt waterproof coating attribute information, and quick-setting agent attribute information; an initial module, configured to calculate an initial injection speed according to the first controlled injection amount and the detection information; An inspection module configured to inspect the current test area for extreme empty defects and high-reflection defects; The execution module is configured to spray the quick-setting rubber asphalt waterproof coating on the current test area according to the initial spraying speed when there are no extreme empty defects and high reverse defects in the current test area.

[0059] Optionally, the initial module is configured to: The initial injection velocity V is calculated according to the following formula 初 : Among them, K1 is the variable proportional coefficient of the nozzle diameter, K1=d / D, K2 is the viscosity coefficient of the accelerator; d is the diameter of the injection pipe, D is the nozzle diameter, P is the outlet pressure of the injection pipe spraying the quick-setting rubber asphalt waterproof coating, n is the rheological index of the quick-setting rubber asphalt waterproof coating, ρ is the density of the quick-setting rubber asphalt waterproof coating, and m is the amount of accelerator.

[0060] Optionally, the detection module is configured to: Capturing images of the current test area at intervals of a preset distance to obtain target image frames; Determine the similarity between the target image frame and the standard empty defect image, and when the similarity is greater than a similarity threshold, determine that the target image frame has an empty defect; When the ratio of the number of target image frames with empty defects to the total number of target image frames is greater than or equal to the standard number ratio threshold, it is determined that the current test area has an extreme empty defect; A flatness detection is performed on the current test area. If the flatness is less than or equal to a flatness threshold, it is determined that a high-reflection defect exists in the current test area.

[0061] Optionally, the spray control system further includes an adjustment module, and the adjustment module is configured to: When an extreme empty defect and / or a high-reflection defect exists in the current test area, the nozzle diameter variable proportional coefficient and / or the quick-setting agent viscosity coefficient are adjusted until the extreme empty defect and / or the high-reflection defect are overcome, and the final nozzle diameter variable proportional coefficient and the final quick-setting agent viscosity coefficient are determined; The target injection speed is calculated according to the variable proportional coefficient of the final nozzle diameter and the viscosity coefficient of the final accelerating agent, and the quick-setting rubber asphalt waterproof coating is sprayed on the target test area according to the target injection speed.

[0062] Optionally, the adjustment module is configured to: When a high-reflection defect exists in the current test area, increasing the nozzle diameter variable proportional coefficient and / or the quick-setting agent viscosity coefficient; When an extreme empty defect exists in the current test area, the nozzle diameter variable proportional coefficient and / or the quick-setting agent viscosity coefficient are reduced.

[0063] Optionally, the adjustment module is further configured to: When the current test area has a high-reflection defect and an extreme empty defect, the viscosity coefficient of the quick-setting agent is kept unchanged and the variable proportional coefficient of the nozzle diameter is gradually changed, and a first defect detection is performed after each change of the variable proportional coefficient of the nozzle diameter; when all available variable proportional coefficients of the nozzle diameter have been used and there are still high-reflection defects and / or extreme empty defects, the target variable proportional coefficient of the nozzle diameter is determined according to the result of the first defect detection, the variable proportional coefficient of the nozzle diameter is kept as the target variable proportional coefficient of the nozzle diameter, and the viscosity coefficient of the quick-setting agent is gradually changed, and a second defect detection is performed after each change of the viscosity coefficient of the quick-setting agent; Until there is no high-reflection defect and / or extreme empty defect in the current test area, or the value adjustment of the viscosity coefficient of the quick-setting agent reaches the upper threshold limit and the lower threshold limit.

[0064] Optionally, the spray control system further includes a pressure regulating module, which is configured to: when the numerical adjustment of the viscosity coefficient of the quick-setting agent reaches an upper threshold value and a lower threshold value, determine a target viscosity coefficient of the quick-setting agent according to a result of a second defect detection, maintain the nozzle diameter variable proportional coefficient as the target nozzle diameter variable proportional coefficient and maintain the viscosity coefficient of the quick-setting agent as the target viscosity coefficient of the quick-setting agent, gradually adjust the power of the power pump to change the outlet pressure of the sprayed quick-setting rubber asphalt waterproof coating at the injection pipe, and perform a third defect detection after each change in the outlet pressure until there are no high-reverse defects and / or extreme empty defects in the current test area; When the adjustment range of the outlet pressure reaches the preset adjustment range, the power pump is shut down.

[0065] It should be noted that: when the device provided in the above embodiment realizes its function, only the division of the above functional modules is used as an example. In actual application, the above functions can be assigned to different functional modules as needed, that is, the internal structure of the device is divided into different functional modules to complete all or part of the functions described above. In addition, the device and method embodiments provided in the above embodiment belong to the same concept, and the specific implementation process is detailed in the method embodiment, which will not be repeated here.

[0066] This embodiment also discloses an electronic device, referring to Fig.10 , the electronic device may include: at least one processor, at least one communication bus, a user interface, a network interface, and at least one memory.

[0067] The communication bus is used to realize the connection and communication between these components.

[0068] The user interface may include a display screen (Display) and a camera (Camera), and the optional user interface may also include a standard wired interface and a wireless interface.

[0069] The network interface may optionally include a standard wired interface or a wireless interface (such as a WI-FI interface).

[0070] Among them, the processor may include one or more processing cores. The processor uses various interfaces and lines to connect various parts within the entire server, and executes various functions of the server and processes data by running or executing instructions, programs, code sets or instruction sets stored in the memory, and calling data stored in the memory. Optionally, the processor can be implemented in at least one hardware form of digital signal processing (Digital Signal Processing, DSP), field programmable gate array (Field-Programmable Gate Array, FPGA), and programmable logic array (Programmable Logic Array, PLA). The processor can integrate one or a combination of a central processing unit (Central Processing Unit, CPU), a graphics processing unit (Graphics Processing Unit, GPU) and a modem. Among them, the CPU mainly processes the operating system, user interface and application programs; the GPU is responsible for rendering and drawing the content to be displayed on the display screen; the modem is used to process wireless communications. It can be understood that the above-mentioned modem may not be integrated into the processor, but implemented separately through a chip.

[0071] Among them, the memory may include a random access memory (Random Access Memory, RAM) and may also include a read-only memory (Read-Only Memory). Optionally, the memory includes a non-transitory computer-readable storage medium. The memory can be used to store instructions, programs, codes, code sets or instruction sets. The memory may include a program storage area and a data storage area, wherein the program storage area may store instructions for implementing an operating system, instructions for at least one function (such as a touch function, a sound playback function, an image playback function, etc.), instructions for implementing the above-mentioned method embodiments, etc.; the data storage area may store data involved in the above-mentioned method embodiments, etc. The memory may also be optionally at least one storage device located away from the aforementioned processor. As Fig.10 As shown, the memory as a computer storage medium may include an operating system, a network communication module, a user interface module, and an application program of a spraying control method of a quick-setting rubber asphalt waterproof coating.

[0072] exist Fig.10In the electronic device shown, the user interface is mainly used to provide an input interface for the user and obtain data input by the user; and the processor can be used to call the application program of the spraying control method of the quick-setting rubber asphalt waterproof coating stored in the memory. When executed by one or more processors, the electronic device executes one or more methods in the above-mentioned embodiments.

[0073] It should be noted that, for the aforementioned method embodiments, for the sake of simplicity, they are all described as a series of action combinations, but those skilled in the art should be aware that the present application is not limited by the order of the actions described, because according to the present application, certain steps can be performed in other orders or simultaneously. Secondly, those skilled in the art should also be aware that the embodiments described in the specification are all preferred embodiments, and the actions and modules involved are not necessarily required for the present application.

[0074] In the above embodiments, the description of each embodiment has its own emphasis. For parts that are not described in detail in a certain embodiment, reference can be made to the relevant descriptions of other embodiments.

[0075] In the several embodiments provided in this application, it should be understood that the disclosed devices can be implemented in other ways. For example, the device embodiments described above are only schematic, such as the division of units, which is only a logical function division. There may be other division methods in actual implementation, such as multiple units or components can be combined or integrated into another system, or some features can be ignored or not executed. Another point is that the mutual coupling or direct coupling or communication connection shown or discussed can be through some service interfaces, and the indirect coupling or communication connection of devices or units can be electrical or other forms.

[0076] The units described as separate components may or may not be physically separated, and the components shown as units may or may not be physical units, that is, they may be located in one place or distributed on multiple network units. Some or all of the units may be selected according to actual needs to achieve the purpose of the solution of this embodiment.

[0077] In addition, each functional unit in each embodiment of the present application may be integrated into one processing unit, or each unit may exist physically separately, or two or more units may be integrated into one unit. The above-mentioned integrated unit may be implemented in the form of hardware or in the form of software functional units.

[0078] If the integrated unit is implemented in the form of a software functional unit and sold or used as an independent product, it can be stored in a computer-readable memory. Based on this understanding, the technical solution of the present application, or the part that contributes to the prior art, or all or part of the technical solution can be embodied in the form of a software product, which is stored in a memory and includes several instructions for a computer device (which can be a personal computer, server or network device, etc.) to perform all or part of the steps of the various embodiments of the present application. The aforementioned memory includes: various media that can store program codes, such as USB flash drives, mobile hard drives, magnetic disks or optical disks.

[0079] The above is only an exemplary embodiment of the present disclosure and cannot be used to limit the scope of the present disclosure. That is, any equivalent changes and modifications made according to the teachings of the present disclosure are still within the scope of the present disclosure. After considering the disclosure of the specification, those skilled in the art will easily think of other embodiments of the present disclosure. This application is intended to cover any modification, use or adaptation of the present disclosure, which follows the general principles of the present disclosure and includes common knowledge or customary technical means in the technical field that are not recorded in the present disclosure. The description and examples are only regarded as exemplary, and the scope and spirit of the present disclosure are defined by the claims.

Claims

1. A spraying control method for a quick-setting rubber asphalt waterproof coating, characterized in that: Applied to a spraying control platform, the spraying control method includes: In response to receiving the injection thickness input by the user, a first controlled injection amount per unit area is calculated according to the injection thickness, and detection information is acquired, wherein the detection information includes injection pipe attribute information, quick-setting rubber asphalt waterproof coating attribute information, and quick-setting agent attribute information; Calculating an initial injection speed according to the first controlled injection amount and the detection information; Conduct extreme empty defect and high reflection defect detection on the current test area; When there are no extreme empty defects and high reverse defects in the current test area, the quick-setting rubber asphalt waterproof coating is sprayed on the current test area according to the initial spraying speed.

2. The spraying control method of the quick-setting rubber asphalt waterproof coating according to claim 1 is characterized in that: The calculating the initial injection speed according to the first controlled injection amount and the detection information comprises: The initial injection velocity V is calculated according to the following formula 初 : Among them, K1 is the variable proportional coefficient of the nozzle diameter, K1=d / D, K2 is the viscosity coefficient of the accelerator; d is the diameter of the injection pipe, D is the nozzle diameter, P is the outlet pressure of the injection pipe for spraying the quick-setting rubber asphalt waterproof coating, n is the rheological index of the quick-setting rubber asphalt waterproof coating, ρ is the density of the quick-setting rubber asphalt waterproof coating, m is the amount of accelerator, and Q is the first controlled injection amount.

3. The spraying control method of the quick-setting rubber asphalt waterproof coating according to claim 1 is characterized in that: The detection of extreme empty defects and high-reflection defects in the current test area includes: Capturing images of the current test area at intervals of a preset distance to obtain target image frames; Determine the similarity between the target image frame and the standard empty defect image, and when the similarity is greater than a similarity threshold, determine that the target image frame has an empty defect; When the ratio of the number of target image frames with empty defects to the total number of target image frames is greater than or equal to the standard number ratio threshold, it is determined that the current test area has an extreme empty defect; A flatness detection is performed on the current test area. If the flatness is less than or equal to a flatness threshold, it is determined that a high-reflection defect exists in the current test area.

4. The spraying control method of the quick-setting rubber asphalt waterproof coating according to claim 1 is characterized in that: The spraying control method also includes: When an extreme empty defect and / or a high-reflection defect exists in the current test area, the nozzle diameter variable proportional coefficient and / or the quick-setting agent viscosity coefficient are adjusted until the extreme empty defect and / or the high-reflection defect are overcome, and the final nozzle diameter variable proportional coefficient and the final quick-setting agent viscosity coefficient are determined; The target injection speed is calculated according to the variable proportional coefficient of the final nozzle diameter and the viscosity coefficient of the final accelerating agent, and the quick-setting rubber asphalt waterproof coating is sprayed on the target test area according to the target injection speed.

5. The spraying control method of the quick-setting rubber asphalt waterproof coating according to claim 4 is characterized in that: The adjusting of the nozzle diameter variable proportional coefficient and / or the quick-setting agent viscosity coefficient until the extreme empty defect and / or the high-reflection defect are overcome comprises: when the current test area has a high-reflection defect, increasing the nozzle diameter variable proportional coefficient and / or the quick-setting agent viscosity coefficient; When an extreme empty defect exists in the current test area, the nozzle diameter variable proportional coefficient and / or the quick-setting agent viscosity coefficient are reduced.

6. The spraying control method of the quick-setting rubber asphalt waterproof coating according to claim 5 is characterized in that: The adjusting of the nozzle diameter variable proportional coefficient and / or the quick-setting agent viscosity coefficient until the extreme empty defect and / or the high-reflection defect are overcome also includes: when the current test area has a high-reflection defect and an extreme empty defect, keeping the quick-setting agent viscosity coefficient unchanged and gradually changing the nozzle diameter variable proportional coefficient, and performing a first defect detection after each change of the nozzle diameter variable proportional coefficient; when all available nozzle diameter variable proportional coefficients have been used and the high-reflection defect and / or the extreme empty defect still exist, determining the target nozzle diameter variable proportional coefficient according to the result of the first defect detection, keeping the nozzle diameter variable proportional coefficient as the target nozzle diameter variable proportional coefficient and gradually changing the quick-setting agent viscosity coefficient, and performing a second defect detection after each change of the quick-setting agent viscosity coefficient; Until there is no high-reflection defect and / or extreme empty defect in the current test area, or the value adjustment of the viscosity coefficient of the quick-setting agent reaches the upper threshold limit and the lower threshold limit.

7. The spraying control method of the quick-setting rubber asphalt waterproof coating according to claim 6 is characterized in that: The spraying control method also includes: When the numerical adjustment of the viscosity coefficient of the quick-setting agent reaches the upper and lower limits of the threshold, the target viscosity coefficient of the quick-setting agent is determined according to the result of the second defect detection, the nozzle diameter variable proportional coefficient is kept as the target nozzle diameter variable proportional coefficient and the quick-setting agent viscosity coefficient is kept as the target quick-setting agent viscosity coefficient, the power of the power pump is gradually adjusted to change the outlet pressure of the sprayed quick-setting rubber asphalt waterproof coating at the injection pipe, and a third defect detection is performed after each change in the outlet pressure until there is no high-reverse defect and / or extreme empty defect in the current test area; When the adjustment range of the outlet pressure reaches the preset adjustment range, the power pump is shut down.

8. A spray control system for quick-setting rubber asphalt waterproof coating, characterized in that: It includes information module, initial module, detection module and execution module, among which: An information module configured to calculate a first controlled injection amount per unit area according to the injection thickness in response to receiving the injection thickness input by a user, and to obtain detection information, wherein the detection information includes injection pipe attribute information, quick-setting rubber asphalt waterproof coating attribute information, and quick-setting agent attribute information; an initial module, configured to calculate an initial injection speed according to the first controlled injection amount and the detection information; An inspection module configured to inspect the current test area for extreme empty defects and high-reflection defects; The execution module is configured to spray the quick-setting rubber asphalt waterproof coating on the current test area according to the initial spraying speed when there are no extreme empty defects and high reverse defects in the current test area.

9. An electronic device, characterized in that: It includes a processor, a memory, a user interface and a network interface, the memory is used to store instructions, the user interface and the network interface are both used to communicate with other devices, and the processor is used to execute the instructions stored in the memory so that the electronic device executes the method as described in any one of claims 1-7.

10. A computer-readable storage medium, characterized in that: The computer-readable storage medium stores instructions, and when the instructions are executed, the method according to any one of claims 1 to 7 is executed.

Citation Information

Cited By

  • Cable anti-corrosion grease coating control method, device and equipment

    CN119972463A