Molding structure of low-modulus nodular cast iron box hub casting
By setting cold iron and exhaust plates in ductile iron box hub castings and adopting an open casting system, the shrinkage defects and high waste rate of low-modulus ductile iron parts are solved, and no riser casting is achieved, and production costs are reduced. And improve product quality.
Patent Information
- Application Number
- CN202411449541.2
- Authority / Receiving Office
- CN · China
- Patent Type
- Applications(China)
- Current Assignee / Owner
- Filing Date
- 2024-10-17
- Publication Date
- 2024-11-26
AI Technical Summary
During the trial production process of low-module ductile iron box hub castings, the waste defect rate is high, the product quality is low, and traditional processes require multiple shrinkage risers to increase production costs, resulting in shrinkage defects and high waste rate inside the castings.
Design a molding structure of low-modulus ductile iron box hub castings, including the installation of cylindrical cold iron and exhaust plates on multiple tables on the outer side of the box hub, and an open casting system using ceramic runner pipes and filters. The retraction riser is cancelled, and the solidification speed and gas discharge are adjusted through the design of cold iron and exhaust plates to ensure that the molten iron is poured and filled evenly.
Effectively eliminate shrinkage defects, reduce production costs, improve casting quality, reduce waste defective rate, and achieve no rise casting, which has changed the concept that low-module ductile iron castings cannot be rise casting in traditional processes, significantly improving product quality and Production efficiency.
Smart Images

Figure CN119016683A_ABST
Abstract
Description
Technical Field
[0001] The invention relates to a casting molding structure, in particular to a low-modulus ductile iron box hub casting molding structure, belonging to the casting field. Background Art
[0002] In the field of casting, when producing ductile iron parts, thick-walled ductile iron parts with a casting modulus greater than 2.5cm can produce qualified castings without setting shrinkage risers, while ductile iron parts with a modulus less than 2.5cm generally need to set shrinkage risers to produce qualified castings. For ductile iron parts of important equipment with complex shapes, to produce high-quality castings with no shrinkage defects inside, larger and more shrinkage risers are required, which will undoubtedly increase the production cost. The ductile iron box hub produced by our company is one of them. Its characteristics are that the modulus is less than 2.5cm, it has dispersed multiple heat nodes, and medium wall thickness. During the trial production, according to the traditional process, multiple shrinkage risers were set. As a result, there were shrinkage defects inside the castings, the scrap rate was high, exceeding the normal scrap rate, and many qualified products were on the edge of defective products, with almost no profit.
[0003] In order to improve the quality of hub castings and meet the needs of the high-end equipment industry, research on low-cost hub castings has become a major issue for the company. Summary of the invention
[0004] In view of the current situation that ductile iron box hub castings have a high scrap rate and low product quality during the trial production process, the present invention provides a modeling structure of a low modulus ductile iron box hub casting, the purpose of which is to reduce or cancel the riser setting, reduce or eliminate shrinkage defects, improve the manufacturing quality of low modulus ductile iron box hub castings, reduce production costs, and meet customer needs.
[0005] The technical scheme of the present invention is: a molding of a low modulus ductile iron box hub casting, the box hub comprises a center hole and a rim, a spoke connected between the center hole on the outer side of the box hub and the rim, and an outer rim on the outer side of the rim 014. When molding the box hub casting, the box hub casting is a vertical molding pouring with the outer side of the box hub facing upward, a plurality of bosses facing upward are arranged on the outer side of the box hub close to the outer rim, a plurality of bosses are respectively provided with a chill on the table of every other boss in the circumferential direction, a plurality of outer peripheral exhaust fins are uniformly arranged on the table of the plurality of bosses in the intervals provided with the chill, a plurality of inner peripheral exhaust fins less in number than the outer peripheral exhaust fins are uniformly arranged on the convex edge surface of the center hole in the same direction as the table of the boss, a straight runner is arranged in the center hole of the box hub, The pouring cup at the top of the sprue is set above the casting. The sprue adopts a ceramic sprue tube. A molten iron ceramic filter is set at the bottom of the sprue. An endogate consisting of multiple ceramic sprue tubes connected to the rim is radially arranged below the filter. The endogate is a form of molten iron pouring that injects molten iron into the cavity from its bottom in the reverse direction upward. The box hub casting is not provided with a shrinkage feeder. Furthermore, the cold iron disposed on the boss on the outer side of the box hub is in the shape of a cylindrical cold iron, and the cold iron is made of iron, steel, copper or graphite, and a magnet is disposed in the mold below the cold iron; Furthermore, the length of the connection portion between the bottom of the outer peripheral exhaust sheet and the inner peripheral exhaust sheet and the table top of the boss is 30 to 70 mm, the width is 3 to 12 mm, the height of the outer peripheral exhaust sheet and the inner peripheral exhaust sheet exceeds the height of the upper sand box, and the inner peripheral exhaust sheet and the peripheral exhaust sheet are in a wedge-shaped structure with a larger upper part and a smaller lower part in the height direction; Furthermore, in the pouring system, the cross-sectional area ratio of the sprue to the ingode is: A 直 : A 内 =1:1.25, which is an open pouring system; Furthermore, the number of the outer peripheral exhaust plates (003) is between 3 and 6, the number of the inner peripheral exhaust plates (002) is between 2 and 4, the inner diameter of the sprue ceramic tube is between Ø35 and 60 mm, and the inner diameter of the endocastor ceramic tube is between Ø15 and 25 mm; Further, the hub casting has a medium wall thickness and a modulus of less than 2.5 cm; Furthermore, the size of the cylindrical cold iron is between Ø30 and 60 mm and the height is between 50 and 150 mm.
[0006] The present invention has the following positive effects: by arranging a cold iron on the table surface of every other boss in the circumferential direction of the outer side surface of the box hub, it is to artificially create a difference in the solidification speed of adjacent boss positions after pouring molten iron, so as to utilize the expansion of graphite precipitated when the molten iron solidifies to compensate for the shrinkage caused by the cooling of the molten iron, thereby creating conditions for eliminating shrinkage defects and breaking the traditional structure of setting a riser during casting; by designing the box hub casting into a vertical molding and pouring structure with the outer side of the box hub facing upward, and arranging the sprue in the center hole of the box hub casting, and arranging a filter at the bottom of the sprue, the outer size of the sand box can be reduced, thereby reducing the amount of molding sand and saving production costs; by designing the pouring system into a pouring form in which molten iron enters the bottom of the center hole from the sprue, and then the molten iron enters the mold cavity from the bottom in the reverse direction upward, and the cross-sectional area ratio of the sprue to the inner pouring channel is designed to be A 直 : A 内 =1:1.25 opening form, when molten iron falls from the sprue to the bottom of the filter, the impact force brought by the molten iron is greatly reduced by bending 180 degrees, so that the molten iron can flow smoothly into the cavity without being involved in gas and slag, and there will be no molten iron sand washing defects. At the same time, the molten iron is gradually filled from the bottom of the casting upward, and the molten iron filling direction is consistent with the exhaust direction in the cavity, which is conducive to exhaust and slag removal, and avoids slag holes and pore defects in the casting; by evenly arranging radial dispersed ingates under the filter, the molten iron and heat are evenly distributed everywhere after the molten iron enters the cavity, avoiding local overheating, thereby ensuring the consistency of the metallographic structure everywhere inside the casting. A plurality of outer venting fins are evenly arranged on the table surface of a plurality of spaced bosses of the box hub casting facing upward on the outer side of the box hub, and a plurality of inner venting fins are evenly arranged on the circumferential direction of the convex edge surface of the center hole, so that the pouring direction and the venting direction are in the same direction, which is conducive to the smooth discharge of gas in the mold cavity when molten iron is filled, ensuring that the casting does not produce pore defects, reducing defects caused by poor venting, and improving the product quality of the casting. The length of the connection between the bottom of the inner venting fin and the outer venting fin and the convex table surface of the casting is 30-70 mm, the width is 3-12 mm, and the height exceeds the height of the upper sand box, which is conducive to smooth venting and demolding in the height direction; the use of the present invention to cast low modulus ductile iron box hubs realizes riser-free casting, which changes the traditional theory and process method that low modulus ductile iron parts cannot be cast without risers. The use of the process of the present invention to produce box hub castings not only improves the quality of castings and reduces the scrap rate, but also reduces the production cost. The present invention creates a more scientific process method for the production of similar ductile iron parts, and the effect is that the castings are of better quality and the production cost is lower. BRIEF DESCRIPTION OF THE DRAWINGS
[0007] Figure 1 This is a schematic diagram of the box hub casting structure of the present invention Figure 1 .
[0008] Figure 2 This is a schematic diagram of the box hub casting structure of the present invention Figure 2 .
[0009] Figure 3 It is a structural diagram of the box hub casting.
[0010] Explanation of reference numerals: 001—hub casting, 002—inner exhaust plate, 003—outer exhaust plate, 004—chill, 005—pouring cup, 006—sprue, 007—filter, 008—introducing channel, 009—magnet, 010—boss, 011—center hole, 012—outer rim, 013—spoke, 014—rim, 015—convex edge. DETAILED DESCRIPTION
[0011] The specific implementation of the invention is further described in detail below with reference to the accompanying drawings. In the following description, the outer side of the hub refers to the side of the hub arranged on the equipment facing the outside of the equipment, that is, the side close to the end of the equipment shaft, and the inner side of the rim refers to the opposite side of the hub arranged on the equipment facing the outside of the equipment.
[0012] A low modulus ductile iron box hub casting. Figure 1 This is a schematic diagram of the box hub casting structure of the present invention Figure 1 , Figure 2 This is a schematic diagram of the box hub casting structure of the present invention Figure 2 , Figure 3 : is a schematic diagram of the structure of a box hub casting, the box hub comprises a center hole 011 and a rim 014, a spoke 013 connected between the center hole 011 and the rim 014, an outer rim 012 on the outer side of the rim 014, and an inner rim on the inner side of the rim 014. When the box hub casting 001 is molded, the outer side of the box hub casting 001 is vertically molded and poured with the outer side of the box hub casting 001 facing upward. A plurality of bosses facing upward are arranged on the outer side of the box hub near the outer rim. A chill 004 is arranged on the surface of each of the plurality of bosses 010 in the circumferential direction. A plurality of outer peripheral exhaust fins 003 are uniformly arranged on the surfaces of the plurality of bosses 010 in the intervals provided with the chill 004 in the circumferential direction. A plurality of inner peripheral exhaust fins 002 whose number is less than the outer peripheral exhaust fins 003 are uniformly arranged on the surface of the convex edge 015 of the center hole 011 in the same direction as the surface of the boss 010 in the circumferential direction. A straight runner 006 is arranged in the center hole 011 of the box hub. The pouring cup 005 of the straight runner 006 is arranged above the casting. The straight runner 006 adopts a ceramic runner tube. A molten iron ceramic filter 007 is arranged at the bottom of the straight runner 006. An endogate 008 composed of multiple ceramic runner tubes connected to the bottom surface of the rim 014 is radially arranged below the filter 007. The endogate 008 is a form of molten iron pouring that is injected upward from the bottom of the rim. The box hub casting 001 is not provided with a shrinkage feed riser.
[0013] Reference Figure 1 , Figure 2 The chiller 004 provided on the boss 010 on the outer side of the hub is in the shape of a cylindrical chiller 004. The chiller 004 is made of iron, steel, copper metal material or graphite material, etc. A magnet 009 is provided in the mold below the chiller. In this embodiment, in order to reduce costs, gray cast iron material is used to make the chiller.
[0014] Reference Figure 1 , Figure 2 The length of the connecting part between the bottom of the inner peripheral exhaust plate 002 and the outer peripheral exhaust plate 003 and the table top of the boss 010 is 30-70 mm, and the width is 3-12 mm. The height of the inner peripheral exhaust plate 002 and the outer peripheral exhaust plate 003 exceeds the height of the upper sand box. The inner peripheral exhaust plate 002 and the outer peripheral exhaust plate 003 are wedge-shaped structures with a larger upper part and a smaller lower part in the height direction.
[0015] In the pouring system, the cross-sectional area ratio of the sprue 006 to the ingode 008 is: 直 : A 内 =1:1.25, which is an open pouring system.
[0016] The number of the outer peripheral exhaust plates 003 is between 3 and 6, the number of the inner peripheral exhaust plates 002 is between 2 and 4, the inner diameter of the sprue 006 ceramic tube is between Ø35 and 60 mm, and the inner diameter of the endocastor 006 ceramic tube is between Ø15 and 25 mm.
[0017] The hub casting 001 has a medium wall thickness, and the modulus of the hub casting 001 is less than 2.5 cm.
[0018] The cylindrical cold iron 004 has a diameter of 30 to 60 mm and a height of 50 to 150 mm.
[0019] Specific implementation steps: ① First, according to the structural characteristics of the ductile iron castings produced, carry out process analysis and evaluation to determine the preliminary process plan; ② Design and draw casting production process diagrams; including designing sand boxes and drawing sand box diagrams; designing chillers and drawing chiller diagrams; designing pouring risers and exhaust plates; ③Design and draw mold drawings for modeling; ④ Purchase the sand box, chiller, mold and various materials needed for production; ⑤ Make molds for modeling, make sand boxes, make chillers, and inspect whether the molds, sand boxes, and chillers are qualified; ⑥ Molding and core making, painting, drying, core lowering and box packing; ⑦ Melting the molten iron while carrying out step ⑥; ⑧ Molten iron is discharged from the furnace and spheroidized; ⑨ Pouring: Pour the molten iron that has passed the spheroidization treatment into the mold after it comes out of the furnace; ⑩ After natural cooling to below 300℃, unpack and remove sand; ⑪ Polishing and inspection: Finally, qualified hub castings are obtained. Specific embodiments
[0020] Our company actually produces a box hub, which is made of QT450-10, weighs 293kg, has a casting modulus of Mc=1.98cm, and a main wall thickness of 35mm. In the past, according to the traditional theoretical design process, during the molding, whether the outer side of the box hub is facing up or down during pouring, a larger shrinkage feed riser is required. The process yield is 75%, and the internal shrinkage defect scrap rate is 10%. Even the qualified castings have slight shrinkage inside. According to the process method of the present invention, the casting is vertically molded and poured vertically, the outer side of the box hub faces upward, and there is no need to set a shrinkage feeder. On the boss 010 on the outer side of the box hub, 12 Ø50×100 cylindrical chillers 004 are set on every other boss 010, and the chillers 004 are evenly distributed in the circumferential direction. In this embodiment, 6 5×60 outer peripheral exhaust fins 003 are evenly set on the circumference of the boss 010; 4 4×40 inner peripheral exhaust fins 002 are evenly set on the surface of the convex edge 015 of the center hole 011. The design form of the pouring system is that the pouring cup 005 is higher than The sand box enters the sprue 006 after passing through the upper runner. The sprue 006 is set in the center hole of the box hub cast iron 001. The sprue 006 is formed by a ceramic sprue pipe with an inner diameter of Ø40. A molten iron ceramic filter 007 is set at the bottom of the sprue 006. There are 6 Ø18 ceramic sprue pipes below the filter 007. The sprue 008 is connected to the rim 014 (specifically the bottom outer edge in the molding) in a radial form. After passing through the sprue 008, the molten iron turns 180 degrees and is injected into the sand mold cavity from the bottom of the casting rim. Due to the reduction of the sand box, 480kg less molding sand is used for each box hub produced, saving 60 yuan in costs. In addition, 33kg less molten iron is used for each piece without shrinkage feeder, saving 10 yuan in costs. A total of 43 yuan can be saved per piece, and 146 yuan per ton. The production process yield rate has increased from 75% to 86%, and the qualified rate is over 98%. The waste and defective products are other casting defects, there are no internal shrinkage defects, and the quality has always been good.
[0021] The above embodiments are only preferred embodiments of the present invention and are not intended to limit the scope of implementation of the present invention. The present invention can be applied to similar casting production.
[0022] The present invention has the following positive effects: by arranging a chill 004 on the surface of every other boss 010 on the outer surface of the hub, the solidification speed difference between adjacent bosses 010 after pouring molten iron is artificially caused, so as to utilize the expansion of graphite precipitated during the solidification of molten iron to compensate for the shrinkage caused by the cooling of molten iron, thereby creating conditions for avoiding shrinkage defects and breaking the traditional structure of setting risers during casting; by designing the hub casting 001 to be a vertical molding casting with the outer surface of the hub facing upward, and arranging the sprue 006 in the center hole 011 of the hub cast iron 001, and arranging a filter 007 at the bottom of the sprue 006, this molding structure can reduce the outer dimensions of the sand box, thereby reducing the amount of molding sand and saving production costs; the cross-sectional area ratio of the sprue 006 to the ingrow 008 is designed to be A 直 : A 内 =1:1.25 open form, the pouring system is designed so that the molten iron enters the bottom of the casting from the sprue 006, and then pours upward from the bottom of the sprue 006 through the inner gate into the cavity. When the molten iron falls from the sprue 006 to the bottom of the filter 007, it will be bent 180 degrees to greatly reduce the impact of the molten iron, so that the molten iron can flow smoothly into the sand mold cavity without involving gas and slag, and will not cause molten iron sand washing defects. At the same time, the molten iron gradually fills up from the bottom of the casting, and the molten iron filling is convenient The exhaust direction is consistent with that in the cavity, which is beneficial to exhaust and slag removal, avoiding slag holes and pore defects in the casting; by evenly arranging radial dispersed ingates 008 on the filter 007, the molten iron and heat can be evenly distributed everywhere after the molten iron enters the cavity, avoiding local overheating, thereby ensuring the consistency of the metallographic structure everywhere inside the casting; by evenly arranging a plurality of peripheral exhaust plates 003 on the surface of the upward boss 010 on the outer side of the box hub, the circumferential surface of the convex edge 015 of the center hole 011 is evenly A plurality of inner circumference exhaust plates 002 are arranged so that the pouring direction and the exhaust direction are in the same direction, which is beneficial to the smooth exhaust of the gas in the mold cavity when the molten iron is filled, and ensures that the casting does not produce pore defects, can reduce the defects caused by poor exhaust, and can improve the product quality of the casting; by controlling the connection length between the bottom of the inner circumference exhaust plate 002 and the outer circumference exhaust plate 003 and the table top of the casting boss 010 to be 30-70 mm, the width is 3-12 mm, and the height exceeds the height of the upper sand box, it is beneficial to smooth exhaust and to demolding in the height direction; the use of the present invention to cast low modulus ductile iron box hubs can achieve riser-free casting, which changes the traditional theory and process method that low modulus ductile iron parts cannot be cast without risers. The use of the process of the present invention to produce box hub castings not only improves the quality of the castings, but also reduces the scrap rate from 10% in the past to 2%, and also reduces the production cost. The present invention creates a more scientific process method for the production of similar ductile iron parts, and the effect is that the castings are of better quality and the production cost is lower.
Claims
1. A molding structure of a low modulus ductile iron hub casting, the hub comprising a center hole (011) and a rim 014, a spoke (013) connected between the center hole (011) and the rim (014), and an outer rim (012) outside the rim, Features: When the box hub casting is molded, the box hub casting is a vertical casting mold with the outer side of the box hub facing upward, a plurality of bosses with the table surface facing upward are arranged on the outer side of the box hub near the outer wheel rim, a chill (004) is arranged on the table surface of each of the plurality of bosses in the circumferential direction, a plurality of peripheral exhaust fins (003) are evenly arranged on the table surfaces (010) of the plurality of bosses in the intervals provided with the chill (004) in the circumferential direction, a plurality of inner peripheral exhaust fins (002) whose number is less than the outer peripheral exhaust fins (003) are evenly arranged on the surface of the convex edge (015) of the center hole in the same direction as the table surface of the boss, and a straight runner (006) is arranged in the center hole of the box hub, The top pouring cup of the sprue (006) is arranged above the casting. The sprue (006) adopts a ceramic sprue tube. A molten iron ceramic filter (007) is arranged at the bottom of the sprue. An endogate (008) composed of multiple ceramic sprue tubes connected to the rim is radially arranged below the filter. The endogate (008) is a form of molten iron pouring that injects molten iron into the mold cavity from the bottom of the rim in the reverse direction upward. The box hub casting is not provided with a shrinkage feed riser.
2. The molding of a low modulus ductile iron hub casting according to claim 1, Features: The cold iron arranged on the boss on the outer side of the box hub is in the shape of a cylindrical cold iron, and the cold iron is made of iron, steel, copper or graphite. A magnet (009) is arranged in the mold below the cold iron.
3. The molding structure of a low modulus ductile iron hub casting according to claim 1, Features: The bottom of the outer peripheral exhaust plate (003) and the inner peripheral exhaust plate (002) are connected to the table top of the boss in length of 30 to 70 mm and width of 3 to 12 mm. The height of the outer peripheral exhaust plate (003) and the inner peripheral exhaust plate (002) exceeds the height of the upper sand box. The outer peripheral exhaust plate (003) and the inner peripheral exhaust plate (002) are in a wedge-shaped structure with a larger top and a smaller bottom in the height direction.
4. The molding structure of a low modulus ductile iron hub casting according to claim 1, Features: In the pouring system, the cross-sectional area ratio of the sprue (006) to the ingode (008) is: A 直 : A 内 =1:1.25, which is an open pouring system.
5. The molding structure of a low modulus ductile iron hub casting according to claim 1, Features: The number of the outer peripheral exhaust plates (003) is between 3 and 6, the number of the inner peripheral exhaust plates (002) is between 2 and 4, the inner diameter of the sprue ceramic tube is between Ø35 and 60 mm, and the inner diameter of the endocastor ceramic tube is between Ø15 and 25 mm.
6. The molding structure of a low modulus ductile iron hub casting according to claim 1, Features: The hub casting has a medium wall thickness and a modulus of less than 2.5 cm.
7. The molding structure of a low modulus ductile iron hub casting according to claim 2, Features: The cylindrical cold iron has a diameter of 30 to 60 mm and a height of 50 to 150 mm.