Preparation method of composite film, cutting die structure and composite film
By integrating the functional film and protective film into the composite film preparation method, the low production efficiency problem caused by shape differences is solved, and more efficient processing and better user experience is achieved.
Patent Information
- Application Number
- CN202411112762.0
- Authority / Receiving Office
- CN · China
- Patent Type
- Applications(China)
- Current Assignee / Owner
- Filing Date
- 2024-08-14
- Publication Date
- 2024-11-26
AI Technical Summary
In the prior art, the functional film and the protective film are inefficient in the production process due to shape differences, which increases production costs.
By adopting the composite film preparation method, by applying the first diaphragm to the second diaphragm and synchronously forming both shapes by using a punching device, ensuring that the second outer contour does not exceed the first outer contour, thereby realizing integrated molding and improving processing Efficiency and product stability.
Improves the processing and forming efficiency of functional films and protective films, enhances the durability of the product, and simplifies the operation process, providing a better feel and user experience.
Smart Images

Figure CN119017481A_ABST
Abstract
Description
Technical Field
[0001] The present invention relates to the technical field of composite film production, and in particular to a composite film preparation method, a knife die structure and a composite film. Background Art
[0002] In order to improve the safety and functionality of the cover glass, a functional film (such as explosion-proof film or optical film, etc.) will be applied to the cover glass as required before the cover glass is assembled. In order to further protect the functional film and prevent it from being damaged during transportation and assembly of the cover glass, a protective film will be attached to the surface of the functional film.
[0003] The current process of coating the functional film and the protective film on the cover glass is to first process and shape the functional film and the protective film according to the shape and size of the cover glass, then coat the functional film on the surface of the cover glass by a film laminating machine, then coat the protective film on the surface of the functional film, and then package the cover glass after two film laminating processes for subsequent processing, and finally install the cover glass on the vehicle, and tear off the protective film to expose the functional film.
[0004] However, in the process of implementing the present invention, the inventors found that since it is necessary to design protruding tear strips at the edges of some parts of the protective film to facilitate the subsequent tearing off of the protective film, this leads to differences in the shapes of the functional film and the protective film. The two need to be produced and processed separately during the production process, which not only affects the production efficiency, but also greatly increases the production cost. Summary of the invention
[0005] A technical problem to be solved by the present disclosure is that the functional film and the protective film with different shapes cannot be processed synchronously, resulting in low work efficiency.
[0006] In order to solve the above technical problems, the present disclosure provides a method for preparing a composite film in a first aspect, comprising:
[0007] Step S1, attaching the first film to the second film;
[0008] Step S2, using a punching device to punch out to simultaneously form a first outer contour of the first diaphragm and a second outer contour of the second diaphragm, wherein the second outer contour as a whole does not exceed the first outer contour.
[0009] In some embodiments, before step S1, the method further includes:
[0010] Step S101, obtaining a first diaphragm roll and a second diaphragm roll;
[0011] Step S102, processing the first film roll to form a plurality of first films with a third outer contour, the first outer contour being located inside the third outer contour; processing the second film roll to form a plurality of second films with a fourth outer contour, the second outer contour being located inside the fourth outer contour.
[0012] In some embodiments, before step S102, the method further includes:
[0013] Draw a first boundary of the rectangle, where the length of the first boundary is the farthest straight-line distance between two sides of the first outer contour along the first direction, and the width of the first boundary is the farthest straight-line distance between two sides of the first outer contour along the second direction, and the first direction is perpendicular to the second direction; take the first boundary as a reference, and expand the first preset distance as a whole to obtain a third outer contour, where the first preset distance is greater than 10 mm, for example, the first preset distance may be 11 mm, 13 mm, 15 mm, 17 mm, 19 mm, etc.;
[0014] Draw a second boundary of the rectangle, where the length of the second boundary is the farthest straight-line distance between the two sides of the second outer contour along the first direction, and the width of the second boundary is the farthest straight-line distance between the two sides of the second outer contour along the second direction; based on the second boundary, the second preset distance is extended equidistantly as a whole to obtain a fourth outer contour, where the second preset distance is greater than 10 mm, for example, the second preset distance can be 11 mm, 13 mm, 15 mm, 17 mm, 19 mm, etc.
[0015] In some embodiments, the punching method using the punching device is:
[0016] In some embodiments, the first cutter and the second cutter of the punching device are used to punch synchronously from the second film sheet to the first film sheet; the first cutter and the second cutter have a height difference, and the height difference is calculated by the formula:
[0017] H=dA
[0018] Where, H, height difference, mm;
[0019] d, thickness of the first diaphragm, mm;
[0020] A, constant, 5-10, mm, for example, A can be 5mm, 6mm, 7mm, 8mm, 9mm or 10mm, etc.
[0021] In some embodiments, a portion of the first outer contour completely overlaps with the second outer contour, and another portion of the first outer contour exceeds the second outer contour to form a tear strip.
[0022] In some embodiments, step S2 includes:
[0023] Punching with a punching device to simultaneously form an outer contour of a first sub-film layer of the first diaphragm, an outer contour of a second sub-film layer of the first diaphragm, and a second outer contour of the second diaphragm;
[0024] Among them, the first sub-membrane layer is located between the second sub-membrane layer and the second membrane sheet, the outer contour of the second sub-membrane layer forms the first outer contour, the second outer contour does not exceed the outer contour of the first sub-membrane layer, and the outer contour of the first sub-membrane layer does not exceed the first outer contour.
[0025] In some embodiments, the second outer contour can be located inside the edge of the object to be bonded and has a third preset distance from the edge of the object to be bonded.
[0026] The second aspect of the present application provides a knife die structure, which is applied to a punching device in the preparation method of the composite film of the first aspect, comprising:
[0027] Mounting frame;
[0028] a first annular cutter, disposed on a mounting frame; and,
[0029] The second tool is located inside the first tool. The second tool is arranged on the mounting frame. The first tool and the second tool together form two annular structures. The first tool can be close to the composite film relative to the second tool. The first tool and the second tool are punched synchronously and can cooperate to form a tear strip on part of the composite film.
[0030] The third aspect of the present application provides a composite membrane obtained by the preparation method of the composite membrane of the first aspect, comprising:
[0031] The first film sheet comprises a first sub-film layer and a second sub-film layer; the first sub-film layer and the second sub-film layer are adsorbed by electrostatic attraction;
[0032] A first sub-tear strip is integrally formed with the first sub-film layer; and,
[0033] The second sub-tear strip overlaps with the first sub-tear strip, and the second sub-tear strip is integrally formed with the second sub-film layer;
[0034] The second membrane sheet, the first sub-membrane layer is attached to the second membrane sheet.
[0035] In some embodiments, the second membrane comprises:
[0036] A first release base film layer, an optically transparent adhesive layer and a functional film layer are stacked in sequence; and a first sub-film layer is attached to the functional film layer.
[0037] Through the above technical scheme, the preparation method of the composite film provided by the present invention improves the processing efficiency of the first film and the second film by attaching the first film to the second film to form a composite film, and then using a punching device to punch to synchronously form the shapes of the two films; since the first film and the second film are both integrally formed during the punching process, the stability of the structures of the two is ensured and the durability of the product is enhanced; and since the shape of the first outer contour is different from the shape of the second outer contour, and the second outer contour as a whole does not exceed the first outer contour, that is, at least part of the first outer contour exceeds the second outer contour, the first film is easier to be identified and grasped by the operator, which helps to provide a better feel and operational convenience when tearing off the first film, making the tearing process smoother, reducing the difficulty of operation, and improving user experience. BRIEF DESCRIPTION OF THE DRAWINGS
[0038] In order to more clearly illustrate the embodiments of the present disclosure or the technical solutions in the prior art, the drawings required for use in the embodiments or the description of the prior art will be briefly introduced below. Obviously, the drawings described below are only some embodiments of the present disclosure. For ordinary technicians in this field, other drawings can be obtained based on these drawings without paying any creative work.
[0039] Figure 1 is a schematic structural diagram of a first diaphragm of the present invention from a first viewing angle;
[0040] Figure 2 is a schematic structural diagram of the first diaphragm of the present invention from a second viewing angle;
[0041] Figure 3 is a schematic structural diagram of a second diaphragm of the present invention from a first viewing angle;
[0042] Figure 4 is a schematic structural diagram of a second diaphragm of the present invention from a second viewing angle;
[0043] Figure 5 is a schematic structural diagram of a composite film disclosed in the present invention from a first perspective;
[0044] Figure 6 is a schematic structural diagram of the composite film disclosed in the present invention from a second viewing angle;
[0045] Figure 7 is a schematic diagram of the structure of the composite film and cover glass disclosed in the present invention;
[0046] Figure 8 It is a structural schematic diagram of the knife die structure disclosed in the present invention;
[0047] Fig. 9 It is a partial cross-sectional view of the first cutting tool and the second cutting tool of the cutting die structure disclosed in the present invention.
[0048] Description of reference numerals:
[0049] 1. First film; 11. First outer contour; 12. Tear strip; 13. First sub-film layer; 131. First sub-tear strip; 14. Second sub-film layer; 141. Second sub-tear strip; 15. Antistatic adhesive layer; 16. Second release bottom film layer; 2. Second film; 21. Second outer contour; 22. Functional film layer; 23. Optically transparent adhesive layer; 24. First release bottom film layer; 25. Initial PET film layer; 3. Composite film; 4. Knife die structure; 41. Mounting frame; 42. First tool; 43. Second tool; 5. Cover glass. DETAILED DESCRIPTION
[0050] The following is a further detailed description of the embodiments of the present disclosure in conjunction with the accompanying drawings and examples. The detailed description of the following embodiments and the accompanying drawings are used to exemplarily illustrate the principles of the present disclosure, but cannot be used to limit the scope of the present disclosure. The present disclosure can be implemented in many different forms and is not limited to the specific embodiments disclosed herein, but includes all technical solutions that fall within the scope of the claims.
[0051] The present disclosure provides these embodiments to make the present disclosure thorough and complete, and to fully express the scope of the present disclosure to those skilled in the art. It should be noted that unless otherwise specifically stated, the relative arrangement of the parts and steps, the composition of the materials, the numerical expressions and the numerical values set forth in these embodiments should be interpreted as being merely exemplary, and not as limiting.
[0052] It should be noted that, in the description of the present disclosure, unless otherwise specified, the meaning of "multiple" is greater than or equal to two; the terms "upper", "lower", "left", "right", "inner", "outer", etc., indicating the orientation or positional relationship, are only for the convenience of describing the present disclosure and simplifying the description, and do not indicate or imply that the device or element referred to must have a specific orientation, be constructed and operated in a specific orientation, and therefore cannot be understood as a limitation of the present disclosure. When the absolute position of the object being described changes, the relative positional relationship may also change accordingly.
[0053] In addition, the words "first", "second" and similar words used in the present disclosure do not indicate any order, quantity or importance, but are only used to distinguish different parts. "Vertical" does not mean vertical in the strict sense, but is within the tolerance range. "Parallel" does not mean parallel in the strict sense, but is within the tolerance range. "Include" or "comprising" and similar words mean that the elements before the word include the elements listed after the word, and do not exclude the possibility of including other elements.
[0054] It should also be noted that in the description of the present disclosure, unless otherwise clearly specified and limited, the terms "installed", "connected", and "connected" should be understood in a broad sense. For example, it can be a fixed connection, a detachable connection, or an integral connection; it can be directly connected or indirectly connected through an intermediate medium. For ordinary technicians in this field, the specific meanings of the above terms in the present disclosure can be understood according to the specific circumstances. When a specific device is described as being located between a first device and a second device, there may or may not be an intermediate device between the specific device and the first device or the second device.
[0055] All terms used in the present disclosure have the same meanings as those understood by those of ordinary skill in the art to which the present disclosure belongs, unless otherwise specifically defined. It should also be understood that terms defined in general dictionaries, for example, should be interpreted as having meanings consistent with their meanings in the context of the relevant technology, and should not be interpreted in an idealized or extremely formal sense, unless explicitly defined as such herein.
[0056] Technologies, methods, and equipment known to ordinary technicians in the relevant art may not be discussed in detail, but where appropriate, the technologies, methods, and equipment should be considered part of the specification.
[0057] In the production process of the cover glass 5, it is necessary to first process and shape the rolled functional film and the rolled protective film separately, and then transport the processed functional film and protective film to the cover glass 5 processing workshop for film laminating, and finally transport the film laminating cover glass 5 to the assembly workshop for assembly of the cover glass 5.
[0058] The inventors noticed that since the protective film needs to be prepared with a tear strip 12 , the shape of the protective film is different from that of the functional film, and the two need to be processed and formed separately, which greatly reduces the production efficiency.
[0059] After in-depth research, the inventors found that the first film 1 can be attached to the second film 2 to form a composite film 3, and then a punching device can be used to punch to simultaneously form the first outer contour 11 of the first film 1 and the second outer contour 21 of the second film 2 to improve processing efficiency.
[0060] The composite film 3 prepared in the present application is suitable for being attached to cover glass 5, smart phone screen, laptop screen, furniture decoration, etc. The material of the composite film 3 can be specifically selected according to the application field.
[0061] Example 1
[0062] like Figure 1-Figure 9 As shown, Example 1 of the present application provides a method for preparing a composite film, comprising:
[0063] Step S1 , attaching the first film 1 to the second film 2 .
[0064] Specifically, the first film 1 may be a polyethylene terephthalate (PET) film with an antistatic function, or a polyethylene film with a protective function.
[0065] The second film 2 may be a functional film, such as an explosion-proof film, an anti-glare film, an anti-fingerprint film, etc. The first film 1 may be laminated to the second film 2 by a laminating machine.
[0066] In some embodiments, before step S1, the method further includes:
[0067] Step S101, obtaining a first diaphragm roll and a second diaphragm roll;
[0068] Step S102, processing the first film roll to form a plurality of first film sheets 1 having a third outer contour, wherein the first outer contour 11 is located inside the third outer contour; processing the second film roll to form a plurality of second film sheets 2 having a fourth outer contour, wherein the second outer contour 21 is located inside the fourth outer contour.
[0069] Specifically, the first film roll can be processed into a plurality of first film sheets 1 having a third outer contour by punching, cutting, etc. The shape of the third outer contour can be the same as that of the first outer contour 11; or, the shape of the third outer contour can also be different from that of the first outer contour 11. The first outer contour 11 can be located on the inner side of the third outer contour as a whole; or, part of the first outer contour 11 can be located on the inner side of the third outer contour, and another part of the first outer contour 11 can overlap with the third outer contour. In the present application, it is preferred that the first outer contour 11 is located on the inner side of the third outer contour as a whole, so as to facilitate the subsequent lamination of the first film sheet 1 and the second film sheet 2, reduce the accuracy requirements during the lamination process, and leave a margin for the subsequent punching of the punching device to ensure the accuracy of the punching.
[0070] The second film roll can be processed into a plurality of first films 1 with a fourth outer contour by punching, cutting, etc. The shape of the fourth outer contour can be the same as the shape of the second outer contour 21; or, the shape of the fourth outer contour can also be different from the shape of the second outer contour 21. The second outer contour 21 can be located on the inner side of the fourth outer contour as a whole; or, part of the second outer contour 21 can be located on the inner side of the fourth outer contour, and another part of the second outer contour 21 overlaps with the fourth outer contour. In the present application, it is preferred that the second outer contour 21 is located on the inner side of the fourth outer contour as a whole, so as to facilitate the subsequent lamination of the first film 1 and the second film 2, reduce the accuracy requirements during the lamination process, and leave a margin for the subsequent punching of the punching device to ensure the accuracy of the punching.
[0071] In some embodiments, before step S102, the method further includes:
[0072] Draw a first boundary of the rectangle, where the length of the first boundary is the farthest straight-line distance between the two sides of the first outer contour 11 along the first direction, and the width of the first boundary is the farthest straight-line distance between the two sides of the first outer contour 11 along the second direction, and the first direction is perpendicular to the second direction; and the first preset distance is extended equidistantly based on the first boundary to obtain a third outer contour, and the first preset distance is greater than 10 mm;
[0073] Draw the second boundary of the rectangle, the length of the second boundary is the farthest straight-line distance on both sides of the second outer contour 21 along the first direction, and the width of the second boundary is the farthest straight-line distance on both sides of the second outer contour 21 along the second direction; based on the second boundary, the second preset distance is extended equidistantly as a whole to obtain the fourth outer contour, and the second preset distance is greater than 10 mm.
[0074] Specifically, the first outer contour 11 can be a regular shape; the first outer contour 11 can also be a special shape. After the first outer contour 11 is drawn by professional drawing software (such as SolidWorks or AutoCAD, etc.), the first boundary and the third outer contour can be drawn by the drawing software; wherein, the length direction of the first boundary is the first direction, and the width direction of the first boundary is the second direction. Designing the third contour as a rectangle is more conducive to the processing of the first diaphragm roll. When the first diaphragm 1 is a rectangle, the first boundary is the first outer contour 11.
[0075] The shape of the second outer contour 21 may refer to the first outer contour 11. The shape of the second outer contour 21 may be the same as the first outer contour 11, or the shape of the second outer contour 21 may be different from the first outer contour 11. The fourth outer contour may be drawn in the manner described above with reference to the third outer contour.
[0076] Step S2 , using a punching device to punch out to simultaneously form a first outer contour 11 of the first diaphragm 1 and a second outer contour 21 of the second diaphragm 2 , wherein the shape of the first outer contour 11 is different from the shape of the second outer contour 21 , and the second outer contour 21 as a whole does not exceed the first outer contour 11 .
[0077] Specifically, the punching device may be a mechanical punching device or a laser cutting machine, etc. When a laser cutting machine is used, in order to simultaneously cut the first diaphragm 1 and the second diaphragm 2, the laser cutting machine may be configured with a first light beam and a second light beam of two different cutting depths, and the two light beams together constitute a ring-shaped beam path to synchronously form a first outer contour 11 and a second outer contour 21 of different shapes. When a mechanical punching device is used, in some embodiments, the punching method using the punching device is:
[0078] The first cutter 42 and the second cutter 43 of the punching device are used to punch synchronously from the second diaphragm 2 to the first diaphragm 1; the first cutter 42 and the second cutter 43 have a height difference, and the height difference is calculated as follows:
[0079] H=dA
[0080] Where, H, height difference, mm;
[0081] d, thickness of the first membrane 1, mm;
[0082] A, constant, 5~10, mm.
[0083] Specifically, the die structure 4 of the punching device is equipped with a first tool 42 and a second tool 43. The second outer contour 21 may be entirely located inside the first outer contour 11; or, part of the second outer contour 21 may be located inside the first outer contour 11, and another part of the second outer contour 21 may overlap with the first outer contour 11.
[0084] When a glue layer is provided on a side of the first diaphragm 1 close to the second diaphragm 2 , the thickness of d may be the thickness of the first diaphragm 1 minus the thickness of the glue layer.
[0085] When the second outer contour 21 is entirely located on the inner side of the first outer contour 11, taking the first tool 42 being close to the second diaphragm 2 relative to the second tool 43 as an example, during the punching process: due to the height difference between the first tool 42 and the second tool 43, the first tool 42 first punches the second diaphragm 2, and as the punching depth increases, the first tool 42 punches the first diaphragm 1; due to the height difference design, the second tool 43 punches the second diaphragm 2 at this time, and when the punching stops, the second diaphragm 2 is completely punched by the second mold, while the first diaphragm 1 is not completely punched by the second tool 43, so that the first diaphragm 1 and the second diaphragm 2 have first outer contours 11 and second outer contours 21 of different shapes.
[0086] When part of the second outer contour 21 is located on the inner side of the first outer contour 11, another part of the second outer contour 21 overlaps with the first outer contour 11. For example, in some embodiments, part of the first outer contour 11 completely overlaps with the second outer contour 21, and another part of the first outer contour 11 exceeds the second outer contour 21 to form a tear strip 12. Taking the first cutter 42 approaching the second film 2 relative to the second cutter 43 as an example, during the punching process: due to the height difference between the first cutter 42 and the second cutter 43, the first cutter 42 punches the second film 2 first, and as the punching depth increases, the first cutter 42 punches the first film 1, that is, the first cutter 42 forms the first outer contour 11 and part of the second outer contour 21; due to the height difference design, the second cutter 43 punches the second film 2, that is, the second cutter 43 forms another part of the second outer contour 21, and the other part of the second outer contour 21 is opposite to the edge of the tear strip 12, so that the first film 1 and the second film 2 have first outer contours 11 and second outer contours 21 of different shapes.
[0087] By setting the constant A, it can be ensured that the second diaphragm 2 can be completely punched, that is, the second diaphragm 2 is completely cut off, while protecting the integrity of the first diaphragm 1. During the punching process, the pressure can be adjusted to adjust the punching depth.
[0088] In some embodiments, step S2 includes:
[0089] Punching by a punching device to simultaneously form an outer contour of the first sub-film layer 13 of the first diaphragm 1, an outer contour of the second sub-film layer 14 of the first diaphragm 1, and a second outer contour 21 of the second diaphragm 2;
[0090] Among them, the first sub-membrane layer 13 is located between the second sub-membrane layer 14 and the second membrane 2, the outer contour of the second sub-membrane layer 14 forms the first outer contour 11, the second outer contour 21 does not exceed the outer contour of the first sub-membrane layer 13, and the outer contour of the first sub-membrane layer 13 does not exceed the first outer contour 11.
[0091] Specifically, the first sub-film layer 13 can be a PET film layer or a polypropylene film layer (PP) film layer, etc., and the second sub-film layer 14 can be a PE film layer or a copolymer polyethylene film layer (CPE) film layer, etc., and specific selection can be made according to needs.
[0092] The second outer contour 21 may be located entirely inside the outer contour of the first sub-membrane layer 13; or, part of the second outer contour 21 may be located inside the outer contour of the first sub-membrane layer 13, and another part of the second outer contour 21 may overlap with the outer contour of the first sub-membrane layer 13. The outer contour of the first sub-membrane layer 13 may be located entirely inside the first outer contour 11; or, part of the outer contour of the first sub-membrane layer 13 may be located inside the first outer contour 11, and another part of the second outer contour 21 may overlap with the outer contour of the first sub-membrane layer 13.
[0093] At this time, the punching device can be equipped with three cutting dies with height differences between each other. The working method of the three cutting dies with height differences between each other can refer to the working method of the first cutting tool 42 and the second cutting tool 43.
[0094] When the composite film 3 prepared in the present application is applied to the cover glass 5 of a vehicle, the first sub-film layer 13 of the present application can be an antistatic PET film layer, and the second sub-film layer 14 can be a PE film layer, and the PE film layer protects the PET film layer.
[0095] For example, the present application can obtain a first film roll by purchasing, and the first film roll may include a PE film layer (i.e., the second sub-film layer 14), a PET film layer (i.e., the first sub-film layer 13), an antistatic adhesive layer 15, and a second release bottom film layer 16 stacked in sequence, and after processing, a plurality of first film sheets 1 stacked in the above sequence are formed; the present application can obtain a second film roll by purchasing, and the second film roll may include an initial PET film 25 layer, a functional film layer 22, an adhesive layer, and a first release bottom film layer 24 stacked in sequence, and after processing, a plurality of second film sheets 2 stacked in the above sequence are formed. Since the initial PET film layer 25 in the second film roll has a poor antistatic effect, the initial PET film layer 25 is replaced with the first film 1 in the actual production process to achieve a better antistatic function. Among them, the antistatic effect of the PET film layer is greater than the antistatic effect of the initial PET film 25 layer.
[0096] During the laminating process, the initial PET film 25 layer of the second film sheet 2 is first torn off, and then the second release bottom film layer 16 of the first film sheet 1 is torn off, and then the PET film layer is laminated on the functional film layer 22 through the antistatic adhesive layer 15 and the laminating machine to achieve lamination of the first film layer and the second film layer. After lamination, the composite film 3 is formed by punching and forming, and the thickness of d is the sum of the thickness of the PE film layer and the thickness of the first sub-film layer 13 and the second sub-film layer 14. For example, the thickness of the first sub-film layer 13 can be 75 μm, the thickness of the second sub-film layer 14 can be 20 μm, and the thickness of d is 100 μm.
[0097] Next, clean the cover glass 5, and laminate the composite film 3 onto the cover glass 5 through a laminating machine. After laminating, perform a degassing treatment to remove air bubbles between the film layer and the glass. Then perform a random inspection to check the lamination quality between the composite film 3 and the cover glass 5. Finally, assemble the cover glass 5 to complete the assembly of the entire product. After the assembly is completed, tear off the PE film layer.
[0098] Since the present application performs punching and forming after forming the composite film 3, the loss caused by laminating the two types of film sheets separately is reduced, the planning link of production materials is reduced, the production process is simplified, and the production efficiency is improved.
[0099] In some embodiments, the second outer contour 21 can be located inside the edge of the object to be bonded and has a third preset distance from the edge of the object to be bonded.
[0100] Specifically, the object to be bonded may be a cover glass 5, a mobile phone screen, etc. Taking the cover glass 5 as an example, the second outer contour 21 as a whole may be located inside the edge of the cover glass 5, and the second outer contour 21 as a whole may have a third preset distance from the edge of the cover glass 5 to facilitate the installation of the cover glass 5, and part of the tear strip 12 may extend out of the cover glass 5 to facilitate the tearing of the tear strip 12. The third preset distance may be designed according to actual conditions, for example, it may be 0.4 mm, 0.5 mm, or 0.6 mm, etc.
[0101] The preparation method of the composite film provided in Example 1 of the present application improves the processing efficiency of the first film sheet 1 and the second film sheet 2 by attaching the first film sheet 1 to the second film sheet 2 to form a composite film 3, and then using a punching device to punch to synchronously form the shapes of the two films; since the first film sheet 1 and the second film sheet 2 are both integrally formed during the punching process, the stability of the structures of the two is ensured and the durability of the product is enhanced; and since the shape of the first outer contour 11 is different from the shape of the second outer contour 21, and the second outer contour 21 as a whole does not exceed the first outer contour 11, that is, at least part of the first outer contour 11 exceeds the second outer contour 21, the first film sheet 1 is easier to be identified and grasped by the operator, which helps to provide a better feel and operational convenience when tearing off the first film sheet 1, making the tearing process smoother, reducing the difficulty of operation, and improving the user experience.
[0102] Example 2
[0103] like Figure 8 and Fig. 9 As shown, Example 2 of the present application provides a knife die structure, which is applied to the punching device in the preparation method of the composite film in Example 1, including:
[0104] Mounting frame 41;
[0105] A first annular cutter 42 is disposed on the mounting frame 41; and
[0106] The second tool 43 is located on the inner side of the first tool 42. The second tool 43 is set on the mounting frame 41. The first tool 42 and the second tool 43 together form two annular structures. The first tool 42 can be close to the composite film 3 relative to the second tool 43. The first tool 42 and the second tool 43 are synchronously punched and can cooperate to form a tear strip 12 on part of the composite film 3.
[0107] Specifically, the mounting frame 41 serves as a fixed base for the cutting die, ensuring that the cutting die remains stable during the punching process.
[0108] The first cutter 42 is used to form the first outer contour 11 of the first membrane 1 in the composite membrane 3. The first cutter 42 can be set on the mounting frame 41 by bolts or clamping. The shape of the first cutter 42 is the same as the shape of the first outer contour 11 of the first membrane 1 in the composite membrane 3.
[0109] The second cutter 43 is used to cut the second membrane 2 in the composite membrane 3. The second cutter 43 can be set on the mounting frame 41 by bolts or clamping. The shape of the second cutter 43 can be annular, in which case the second cutter 43 is located inside the first cutter 42, and the outer peripheral side of the second cutter 43 can be arranged at equal intervals from the inner peripheral side of the first cutter 42. In this case, the two annular structures are formed by the first cutter 42 and the second cutter 43 itself, respectively, and the second cutter 43 is used to form the outer contour of the second membrane 2; or, the second cutter 43 can be plate-shaped or other non-closed shapes, in which case the second cutter 43 contacts the first cutter 42 to divide the annular first cutter 42 into two annular structures.
[0110] The first tool 42 and the second tool 43 have a height difference. The specific design of the height difference between the first tool 42 and the second tool 43 can refer to Example 1.
[0111] The knife die structure 4 of Example 2 of the present application forms two annular structures through the first tool 42 and the second tool 43. Since the first tool 42 can be close to the composite film 3 relative to the second tool 43, that is, the two tools have a height difference, the first film sheet 1 and the second film sheet 2 in the composite film 3 can be formed into different shapes at the same time, that is, the first film sheet 1 forms a tear strip 12, which improves the processing efficiency, and the tear strip 12 is easier for the operator to identify and grasp, which helps to provide a better feel and operational convenience when tearing off the protective film, making the tearing process smoother, reducing the difficulty of operation, and improving the user experience; at the same time, the two annular structures ensure that the first film sheet 1 and the second film sheet 2 of the composite film 3 are integrally formed during the punching process, ensuring the stability of the two structures and enhancing the durability of the product.
[0112] Example 3
[0113] like Figure 1-Figure 6 As shown, a composite membrane according to Example 3 of the present application is obtained by the preparation method of the composite membrane according to Example 1, comprising:
[0114] The first membrane 1 includes a first sub-membrane layer 13 and a second sub-membrane layer 14; the first sub-membrane layer 13 and the second sub-membrane layer 14 are adsorbed by electrostatic attraction;
[0115] The first sub-tear strip 131 is integrally formed with the first sub-film layer 13; and,
[0116] The second sub-tear strip 141 overlaps with the first sub-tear strip 131, and the second sub-tear strip 141 is integrally formed with the second sub-film layer 14;
[0117] The second membrane 2 , and the first sub-membrane layer 13 are attached to the second membrane 2 .
[0118] Specifically, the first sub-film layer 13 can be a PET film layer or a polypropylene film layer (PP) film layer, etc., and the second sub-film layer 14 can be a PE film layer or a copolymer polyethylene film layer (CPE) film layer, etc. In the present application, the first sub-film layer 13 is preferably a PET film layer and the second sub-film layer 14 is a PE film layer.
[0119] The first tear strip 131 and the second tear strip 141 can completely overlap; or, the first tear strip 131 can partially overlap with the second tear strip 141 (in this case, the outer contour of the first tear strip 131 does not exceed the outer contour of the second tear strip 141). For the convenience of processing, the present application preferably completely overlaps the first tear strip 131 and the second tear strip 141. The first sub-film layer 13 can be attached to the second film sheet 2 by an antistatic adhesive layer 15 and an attaching machine.
[0120] In the composite film 3 of Example 3 of the present application, the first sub-film layer 13 and the second sub-film layer 14 are combined together by electrostatic adsorption, and the structure is relatively stable, which is also conducive to the subsequent tearing off of the second sub-film layer 14; the first sub-tear strip 131 is integrally formed with the first sub-film layer 13, and the second sub-tear strip 141 is integrally formed with the second sub-film layer 14 and overlaps with the first sub-tear strip 131, thereby improving the stability of the structure and improving the durability during use; the second sub-tear strip 141 overlaps with the first sub-tear strip 131, and the overlapping part of the tear strip 12 can provide additional strength and protection, thereby improving the durability of the composite film 3 during actual use.
[0121] In some embodiments, the second membrane 2 includes:
[0122] The functional film layer 22 , the optically transparent adhesive layer 23 and the first release base film layer 24 are stacked in sequence; the first sub-film layer 13 is attached to the functional film layer 22 .
[0123] Specifically, when the composite film 3 is attached to the cover glass 5 , it is only necessary to tear off the first release bottom film layer 24 , and then the attachment can be achieved through the optically transparent adhesive layer 23 , which is easy to operate.
[0124] So far, various embodiments of the present disclosure have been described in detail. In order to avoid obscuring the concept of the present disclosure, some details known in the art are not described. Based on the above description, those skilled in the art can fully understand how to implement the technical solution disclosed here.
[0125] Although some specific embodiments of the present disclosure have been described in detail by way of examples, it should be understood by those skilled in the art that the above examples are for illustration only and are not intended to limit the scope of the present disclosure. It should be understood by those skilled in the art that the above embodiments may be modified or some technical features may be replaced by equivalents without departing from the scope and spirit of the present disclosure. In particular, the various technical features mentioned in the various embodiments may be combined in any manner as long as there is no structural conflict.
Claims
1. A method for preparing a composite film, It is characterized in that include: Step S1, attaching the first film (1) to the second film (2); Step S2, using a punching device to punch out to simultaneously form a first outer contour (11) of the first diaphragm (1) and a second outer contour (21) of the second diaphragm (2), wherein the shape of the first outer contour (11) is different from the shape of the second outer contour (21), and the second outer contour (21) as a whole does not exceed the first outer contour (11).
2. The method for preparing the composite film according to claim 1, It is characterized in that Before step S1, the following steps are also included: Step S101, obtaining a first diaphragm roll and a second diaphragm roll; Step S102, processing the first diaphragm roll to form a plurality of the first diaphragms (1) having a third outer contour, wherein the first outer contour (11) is located on the inner side of the third outer contour; processing the second diaphragm roll to form a plurality of the second diaphragms (2) having a fourth outer contour, wherein the second outer contour (21) is located on the inner side of the fourth outer contour.
3. The method for preparing the composite film according to claim 2, It is characterized in that Before step S102, the following steps are also included: Draw a first boundary of a rectangle, wherein the length of the first boundary is the longest straight-line distance between two sides of the first outer contour (11) along a first direction, and the width of the first boundary is the longest straight-line distance between two sides of the first outer contour (11) along a second direction, wherein the first direction is perpendicular to the second direction; and the third outer contour is obtained by extending the first preset distance as a whole with the first boundary as a reference, wherein the first preset distance is greater than 10 mm; A second boundary of the rectangle is drawn, wherein the length of the second boundary is the farthest straight-line distance between the two sides of the second outer contour (21) along the first direction, and the width of the second boundary is the farthest straight-line distance between the two sides of the second outer contour (21) along the second direction; and the second preset distance is extended equidistantly based on the second boundary to obtain the fourth outer contour, wherein the second preset distance is greater than 10 mm.
4. The method for preparing the composite membrane according to claim 1, It is characterized in that The punching method using the punching device is: The first cutter (42) and the second cutter (43) of the punching device are used to synchronously punch from the second membrane (2) to the first membrane (1); the first cutter (42) and the second cutter (43) have a height difference, and the height difference is calculated as follows: H=dA Where, H, height difference, mm; d, thickness of the first diaphragm (1), mm; A, constant, 5~10, mm.
5. The method for preparing the composite film according to claim 1, It is characterized in that Part of the first outer contour (11) completely overlaps with the second outer contour (21), and another part of the first outer contour (11) exceeds the second outer contour (21) to form a tear strip (12).
6. The method for preparing the composite film according to claim 1, It is characterized in that The step S2 comprises: Using the punching device to punch to simultaneously form the outer contour of the first sub-film layer (13) of the first diaphragm (1), the outer contour of the second sub-film layer (14) of the first diaphragm (1), and the second outer contour (21) of the second diaphragm (2); Wherein, the first sub-membrane layer (13) is located between the second sub-membrane layer (14) and the second membrane sheet (2), the outer contour of the second sub-membrane layer (14) forms the first outer contour (11), the second outer contour (21) does not exceed the outer contour of the first sub-membrane layer (13), and the outer contour of the first sub-membrane layer (13) does not exceed the first outer contour (11).
7. The method for preparing the composite film according to claim 1, It is characterized in that The second outer contour (21) can be located inside the edge of the object to be bonded and has a third preset distance from the edge of the object to be bonded.
8. A die cutter structure, used in a punching device in a method for preparing a composite film according to any one of claims 1 to 7, include: Mounting frame (41); A first annular cutter (42) is arranged on the mounting frame (41); and, The second tool (43) is located on the inner side of the first tool (42). The second tool (43) is arranged on the mounting frame (41). The first tool (42) and the second tool (43) together form two annular structures. The first tool (42) can be closer to the composite film (3) relative to the second tool (43). The first tool (42) and the second tool (43) can perform synchronous punching and can cooperate to form a tear strip (12) on a part of the composite film (3).
9. A composite film obtained by the method for preparing a composite film according to any one of claims 1 to 7, It is characterized in that include: The first membrane (1) comprises a first sub-membrane layer (13) and a second sub-membrane layer (14); the first sub-membrane layer (13) and the second sub-membrane layer (14) are adsorbed by electrostatic attraction; a first sub-tear strip (131), formed integrally with the first sub-film layer (13); and, A second sub-tear strip (141) overlaps with the first sub-tear strip (131), and the second sub-tear strip (141) and the second sub-film layer (14) are integrally formed; A second membrane (2), wherein the first sub-membrane layer (13) is adhered to the second membrane (2).
10. The composite film according to claim 9, It is characterized in that The second membrane (2) comprises: A first release base film layer (24), an optically transparent adhesive layer (23) and a functional film layer (22) are stacked in sequence; the first sub-film layer (13) is adhered to the functional film layer (22).
Citation Information
Patent Citations
Diaphragm integrated punching method
CN107561603A
High-reliability sheet type die cutting part tool for preventing too many materials on handle
CN108237590A
Manufacturing method of protection film
TW202031454A