Rubber and plastic metal magnetic suction sealing strip structure and manufacturing process
Through the rubber and plastic metal magnetic suction seal strip structure and extrusion process, the existing magnetic seal strips are easily deformed, aging and assembly time-consuming and labor-consuming, and simpler and faster assembly and higher sealing effects are achieved, reducing the number of times and more. Production costs and environmental pollution.
Patent Information
- Application Number
- CN202411514191.3
- Authority / Receiving Office
- CN · China
- Patent Type
- Applications(China)
- Current Assignee / Owner
- Filing Date
- 2024-10-29
- Publication Date
- 2024-11-26
AI Technical Summary
The existing magnetic seal strips are prone to deform and aging during use, which is time-consuming and labor-intensive to assemble, and the processing cost of metal-type materials is high, which makes them environmental pollution problems.
The rubber-plastic metal magnetic suction sealing strip structure is adopted, including a magnetic strip mount made of soft rubber, a glass fastener made of hard rubber and a metal connector. It is made by extrusion molding, which eliminates the step of making glass glue, and uses glass The elastic deformation of the fastener is directly clamped and installed, combining the cold rolling mill and rubber and plastic extruder processes to achieve integrated molding.
It simplifies the assembly process, improves the installation tightness of the seal strip, reduces production costs, extends service life, and reduces environmental pollution.
Smart Images

Figure CN119021572A_ABST
Abstract
Description
Technical Field
[0001] The invention relates to the technical field of shower door accessories, and in particular to a rubber-plastic-metal magnetic sealing strip structure and a manufacturing process. Background Art
[0002] Usually, a sealing strip is installed on the edge of the glass door of the shower room, and in order to achieve a better sealing effect, a magnetic sealing strip is generally used. The magnetic sealing strip can make the glass door firmly adsorbed on the metal door frame of the shower room during the closing process, thereby achieving a better sealing effect.
[0003] The existing magnetic sealing strips are PVC-type magnetic strips, which have the following defects: 1. The water retaining strips are easy to deform, resulting in loud noises when the glass door is opened and closed in the later period of use; 2. They are easy to age, usually yellowing and breaking in about three years, and cannot be used normally; 3. Metal profiles (such as stainless steel) are used to make the main frame of the shower room. Large laser machines, cutting machines, planing machines, and folding machines are required, which take a long time to process and have high production costs (machine costs, labor and material costs), and metal profiles are clamped on the outer edge of the glass. , glass glue is needed, and it takes 24 hours to dry before assembly; 4. Metal (stainless steel, aluminum profiles) profiles are easily compressed and deformed during transportation due to the internal cavity structure. At the same time, the profiles are hard and inconvenient to process and assemble; 5. Metal (stainless steel, aluminum profiles) U-slot cards are easy to fall off on the glass, so glass glue is indispensable. Assembly is time-consuming and labor-intensive, and glass glue contains potassium. Glass glue is prone to aging and mold after 5-6 months of use; 6. Aluminum needs to be oxidized and water-plated when making various colors, which pollutes the environment. Summary of the invention
[0004] In view of the defects existing in the prior art, the purpose of the present invention is to provide a rubber-plastic-metal magnetic sealing strip structure and a manufacturing process to solve the problem of time-consuming and labor-intensive assembly caused by the need to apply glass glue during the glass clamping process of the existing metal U-shaped card slot.
[0005] To achieve the above purpose, the technical solution adopted by the present invention is as follows: In a first aspect, the present application provides a rubber-plastic-metal magnetic sealing strip structure, the magnetic sealing strip structure comprising a magnetic strip, and the magnetic sealing strip structure further comprising: A magnetic stripe mounting seat made of soft rubber material, wherein a mounting groove is formed on one side of the outer side of the magnetic stripe mounting seat along its length direction, and the magnetic stripe is mounted in the mounting groove; A metal connector, one side of which is clamped and mounted on the bottom end of the magnetic strip mounting seat, and the other side of the metal connector is formed with a first U-shaped slot arranged in an inverted "U" shape, and the first U-shaped slot is arranged along the length direction of the metal connector; A glass clip is made of hard plastic material, and is formed with a second U-shaped slot for installing glass in an inverted "U" shape. The glass clip is fixedly installed in the slot of the first U-shaped slot, and the second U-shaped slot is arranged along the length direction of the glass clip.
[0006] Furthermore, clamping strip structures are formed on the inner walls on both sides of the second U-shaped slot respectively, and the clamping strip structures include a pair of clamping strips arranged in an eight-shaped shape and extending from the inner wall of the second U-shaped slot in opposite directions toward the center, and the pair of clamping strips are symmetrically arranged up and down.
[0007] Furthermore, the clamping strip structure and the glass clamping member are integrally formed.
[0008] Furthermore, the magnetic strip mounting seat is formed with a hollow inner cavity for buffering.
[0009] Furthermore, a pair of the clamping strip structures are symmetrically arranged on the side walls on opposite sides of the second U-shaped slot, and the clamping strip structures are set at the notch of the second U-shaped slot.
[0010] Furthermore, the magnetic strip mounting seat, the metal connector and the glass clip are integrally formed by extrusion molding.
[0011] In a second aspect, the present application also provides a manufacturing process for manufacturing a rubber-plastic-metal magnetic sealing strip structure as described above, the manufacturing process comprising the following steps: Cut the metal into required sizes and load it into the unwinding rack; Processed into a preset groove shape by a cold rolling mill; Start two rubber and plastic extruders and one modified PVC extruder, and insert the metal parts and magnetic strips processed into the preset groove shape into the precision extrusion mold at high temperature, and then extrude them together with the rubber and PVC in the two rubber extruders and the modified PVC extruder to form an integrated rubber-plastic-metal magnetic sealing strip structure product; The rubber-plastic-metal magnetic sealing strip structure product just out of the mold is introduced into the shaping mold for shaping; After the rubber-plastic-metal magnetic sealing strip structure product is finalized, it is cooled and dried; The rubber-plastic-metal magnetic sealing strip structure products are cut according to the preset size.
[0012] Furthermore, the rubber-plastic-metal magnetic sealing strip structure product that has just been molded is introduced into the molding mold for molding, and the dimensional accuracy of the rubber-plastic-metal magnetic sealing strip structure product is ensured through cooling, moisturizing and vacuuming processes.
[0013] The beneficial effects of the present invention are: 1. By fixing a glass clip made of hard plastic material in the first U-shaped slot of the metal connector, the elastic deformation characteristics of the glass clip can be used to directly clamp the glass in the second U-shaped slot of the glass clip when installing the glass, eliminating the step of gluing, making the assembly simpler and faster. At the same time, the inner wall of the first U-shaped slot of the metal connector limits the deformation of the glass clip to the outside, so that the glass clip is more closely attached to the outer surface of the glass, making it difficult for the glass to fall off; 2. A clamping strip structure is formed on the side walls of the second U-shaped slot of the glass clamping member on both sides. A pair of clamping strips arranged in an eight-shaped shape in the clamping strip structure can further enhance the installation fastness of the glass in the second U-shaped slot. The clamping strip is arranged in an eight-shaped shape, which ensures that the glass is clamped and facilitates the insertion of the glass into the second U-shaped slot. 3. The magnetic strip mounting base, metal connector and glass clip are integrally extruded and molded, which improves the use cost of the product, extends the use time of the product (saving labor and materials), and makes the product more concise and refined. BRIEF DESCRIPTION OF THE DRAWINGS
[0014] Figure 1 It is a schematic diagram of the three-dimensional structural state of glass installed in the rubber-plastic-metal magnetic sealing strip structure of the embodiment of the present application.
[0015] Figure 2 It is a schematic diagram of the three-dimensional structure of the rubber-plastic-metal magnetic sealing strip structure in the embodiment of the present application.
[0016] Figure 3 for Figure 2 Schematic diagram of the local enlarged structure at A in the figure.
[0017] Figure 4 It is a schematic diagram of the process of manufacturing the rubber-plastic-metal magnetic sealing strip structure according to the embodiment of the present application.
[0018] In the figure: 10- rubber-plastic-metal magnetic sealing strip structure, 20- glass, 100- magnetic strip mounting seat, 101- mounting slot, 102- hollow inner cavity, 200- magnetic strip, 300- metal connector, 400- glass clip, 401- clip strip, 402- second U-shaped clip slot. DETAILED DESCRIPTION
[0019] The present invention will be further described in detail below in conjunction with the accompanying drawings and specific implementation methods.
[0020] See attached Figure 1 To Attachment Figure 3 As shown, this embodiment provides a rubber-plastic-metal magnetic sealing strip structure 10 , which includes a magnetic strip 200 , a magnetic strip mounting seat 100 , a metal connector 300 and a glass clip 400 .
[0021] The magnetic stripe mounting seat 100 is made of soft rubber material, for example, silicone material. An installation groove 101 is formed on the outer side of the magnetic stripe mounting seat 100 (i.e., the side away from the metal connector 300), and the installation groove 101 is arranged along the length direction of the magnetic stripe mounting seat 100.
[0022] The magnetic stripe 200 is horizontally inserted into the mounting slot 101 of the magnetic stripe mounting seat 100. In order to ensure the installation tightness of the magnetic stripe 200 in the mounting slot 101, the slot opening size of the mounting slot 101 is equal to or slightly smaller than the outer size of the magnetic stripe 200. In this way, after the magnetic stripe 200 is inserted into the mounting slot 101, the magnetic stripe 200 will exert a certain amount of extrusion on the inner wall of the mounting slot 101, causing the mounting slot 101 to produce a certain amount of elastic deformation, so that the magnetic stripe 200 is installed more firmly in the mounting slot 101 and is not easy to fall off from the mounting slot 101.
[0023] At the same time, in order to improve the shock-absorbing and buffering effect of the magnetic stripe mounting seat 100, the magnetic stripe mounting seat 100 is formed with a hollow inner cavity 102 for buffering.
[0024] Refer to the attached Figure 2 and attached Figure 3 As shown, the upper end of the metal connector 300 in this embodiment is clamped and mounted on the bottom end of the magnetic strip mounting seat 100, and the bottom end of the metal connector 300 is formed with a first U-shaped slot arranged in an inverted "U" shape, and the first U-shaped slot is arranged along the length direction of the metal connector 300. In some embodiments, the metal connector 300 can be made of stainless steel and aluminum alloy.
[0025] Refer to the attached Figure 2 As shown, the glass clip 400 is fixedly installed in the first U-shaped slot of the metal connector 300. The glass clip 400 is used to fix the glass 20. To this end, a second U-shaped slot 402 is formed at the bottom end of the glass clip 400. The second U-shaped slot 402 is arranged along the length direction of the glass clip 400. When the glass 20 is installed, the glass 20 is directly inserted into the second U-shaped slot 402, and the glass 20 is fixedly installed in the second U-shaped slot 402 by the tight fit between the glass 20 and the second U-shaped slot 402. In this embodiment, the glass clip 400 is made of hard plastic material, such as rubber material. In this way, the glass clip 400 has a certain elastic deformation and a certain use strength.
[0026] By fixing a glass clip 400 made of hard plastic material in the first U-shaped groove of the metal connector 300, the elastic deformation characteristics of the glass clip 400 itself can be utilized when the glass 20 is installed. The glass 20 can be directly clamped and installed in the second U-shaped groove 402 of the glass clip 400, eliminating the step of gluing, and the assembly is simpler and faster. At the same time, the inner wall of the first U-shaped groove of the metal connector 300 limits the deformation of the glass clip 400 to the outside, so that the glass clip 400 is more closely attached to the outer surface of the glass 20, making it difficult for the glass 20 to fall off.
[0027] Refer to the attached Figure 2 and attached Figure 3 As shown, in order to further improve the installation fastness between the glass clip 400 and the glass 20, the inner walls on the opposite sides of the second U-shaped slot 402 are respectively formed with clamping strip structures, and a pair of clamping strip structures are symmetrically arranged. Each clamping strip structure includes a pair of clamping strips 401 arranged in an eight-shaped shape extending from the inner wall of the second U-shaped slot 402 to the center in the opposite direction, and the pair of clamping strips 401 are symmetrically arranged up and down. In addition, in order to facilitate the installation of the glass 20 in the second U-shaped slot 402 on the glass clip 400, a pair of clamping strip structures are arranged at the notch of the second U-shaped clamping slot. In some embodiments, the clamping strip structure and the glass clip 400 are integrally formed.
[0028] By forming a clamping strip structure on the opposite side walls of the second U-shaped groove 402 of the glass clamping piece 400, a pair of clamping strips 401 arranged in an eight-shaped shape in the clamping strip structure can further enhance the installation fastness of the glass 20 in the second U-shaped groove 402. The clamping strip 401 is arranged in an eight-shaped shape, which ensures that the glass 20 is clamped while also facilitating the insertion of the glass 20 into the second U-shaped groove 402.
[0029] In addition, in order to facilitate use, be more efficient and economical, the magnetic strip mounting base 100, the metal connector 300 and the glass clip 400 are integrally extruded and manufactured.
[0030] Refer to the attached Figure 4 As shown, this embodiment also provides a manufacturing process for manufacturing the rubber-plastic-metal magnetic sealing strip structure as described above, and the manufacturing process includes the following steps: S1. Cut the metal into required sizes and load it into the unwinding rack; S2, processing into a preset groove shape by a cold rolling mill; Use various metals (such as 304 or 326 stainless steel, aluminum coils, etc.) to cut into required sizes and load them into the unwinding rack, and use the cold rolling machine to roll out the preset groove shape. If there are more requirements, U-shaped grooves of different sizes can be processed; S3, start two rubber and plastic extruders and one modified PVC extruder, and successively insert the metal parts processed into the preset groove shape and the magnetic strip into the precision extrusion mold through high temperature, and then extrude them together with the rubber and PVC in the two rubber extruders and the modified PVC extruder to form an integrated rubber-plastic-metal magnetic sealing strip structure product; For example: in a modified PVC extruder, the temperature when processing and extruding the modified PVC material is set at 120℃ to 200℃; in two rubber and plastic extruders, the temperature of one is set at 200℃ to 300℃ when processing and extruding the rubber and plastic material, and the temperature of the other is set at 180℃ to 300℃ when processing and extruding the rubber and plastic material.
[0031] Since the two rubber extruders process two rubber and plastic materials with different hardness, for example, the hardness of the rubber material extruded by one rubber extruder is 80 to 90 degrees, and the extrusion temperature is set to 200°C to 300°C; the hardness of the rubber material extruded by the other rubber extruder is 60 to 70 degrees, which is slightly softer than the rubber material used by the above rubber extruder, so the extrusion temperature is set to 180°C to 280°C.
[0032] It should be noted here that the reason why the metal parts and magnetic strips need to be inserted into the precision extrusion mold in a high temperature environment is that during the process of integrally molding the metal parts and magnetic strips with the rubber, it is necessary to ensure that the barrel, screw and die head mold in the extruder are at a preset temperature so that the molten rubber and the metal parts and magnetic strips can be integrally molded; but since the screw, barrel and die head in the extruder are processed by electric heating, it takes a long time to heat them to the preset temperature, and the extrusion running time of the metal parts and magnetic strips in the extruder is short during extrusion molding. If the metal parts and magnetic strips are heated after being inserted into the extrusion mold, the temperature of the die head, screw and barrel is low, and the extrusion movement time of the metal parts and magnetic strips in the extruder is short, it is impossible to ensure the integral molding of the metal parts, magnetic strips and rubber. Therefore, the metal parts and magnetic strips need to be in a high temperature environment when they are inserted into the extrusion mold.
[0033] In addition, it is known that the magnetic strip itself has a certain heat resistance (200°C). The magnetic strip is in the extruder, and the extruder is equipped with an insulating cylinder. The magnetic strip is extruded forward in the insulating cylinder. In the internal environment of the insulating cylinder, the temperature actually borne by the magnetic strip is not high, and the magnetic strip stays in the extruder for a short time, that is, the time the magnetic strip stays from entering the extruder to being extruded from the extruder is generally 1-2 seconds. Therefore, the magnetic strip does not melt during the entire extrusion process.
[0034] For the sake of ease of description, the two rubber extruders are referred to as extruder No. 1 and extruder No. 2, and the modified PVC extruder is referred to as extruder No. 3. Then, extruder No. 1 corresponds to the above-mentioned glass clip 400 and clip strip 401; extruder No. 2 corresponds to the above-mentioned mounting groove 101; and extruder No. 3 corresponds to the above-mentioned magnetic strip mounting seat 100.
[0035] S4, introducing the rubber-plastic-metal magnetic sealing strip structure product just out of the mold into the shaping mold for shaping; The newly molded product is introduced into the shaping mold, and the shape is fixed to maintain the dimensional accuracy through water cooling, water moistening and vacuuming; Since the production process of extruded products is mainly divided into two steps, in addition to the extrusion mold, external cooling and shaping is also a key and indispensable step. According to the shrinkage characteristics of rubber and plastic materials, when the product is just extruded from the extrusion mold, it must be immediately introduced into the cooling and shaping mold for water cooling to ensure that the product just entered into the mold is quickly water-cooled and formed, thereby improving the water cooling accuracy of the product.
[0036] Water cooling and vacuuming complement each other. The product just extruded is in a high temperature state and must be cooled by water to set the shape. When the product moves in the shaping mold cavity, it cannot move without water. When the entire production line is running, the metal parts and rubber and plastic extrusion combination will not be able to complete the shaping process without water in the shaping mold when they are running and moving.
[0037] Because during the extrusion process, the shaping die and the high-temperature extrusion die are on the same horizontal line, and the distance between the two hot and cold dies is only 50-100mm. If the vacuum is not drawn, the cooling water will easily overflow and rush to the high-temperature extrusion die head, causing the die head to cool down rapidly and making it impossible to extrude normally.
[0038] When the product enters the inner cavity of the shaping mold, the water cooling allows the high-temperature product to quickly cool down and take shape. The water temperature can ensure that the product moves normally and smoothly in the mold cavity. In addition to ensuring that water does not overflow and rush to the die head, vacuuming can also allow the product to better adhere to the inner cavity of the shaping mold and run normally and smoothly, while also controlling the dimensional accuracy of the product.
[0039] S5. After the rubber-plastic-metal magnetic sealing strip structure product is finalized, it is cooled and dried; For example, after the product leaves the mold, it can be immersed in a cooling water tank and the water droplets can be blown away by a nozzle; S6. Cut the rubber-plastic-metal magnetic sealing strip structure products according to the preset size.
[0040] By adopting the above-mentioned production process, it can be achieved; 1. Plastic and metal alloys, stainless steel 304, 316 and other stainless steel alloys and plastic silicone, rubber, PVC and other plastics, bare magnetic strips, manufactured through one-piece extrusion process, so that a variety of materials with different properties are perfectly combined and integrated, and can be used on all shower room glass; 2. Plastics with the same or different properties and metal aluminum alloys, copper alloys, tin alloys, etc., bare magnetic strips, through precise extrusion manufacturing technology, make the above materials perfectly combined and integrated; 3. All U-shaped card slots of different sizes and shapes, metals, stainless steel 304, 316, etc., and plastics with the same or different properties such as rubber, silicone, PVC, PC, bare magnetic strips, etc., are perfectly combined and integrated through extrusion manufacturing processes such as metal forming equipment + extrusion equipment; 4. All different sizes and shapes, U-shaped slot metals, such as aluminum alloy, copper alloy and other metal alloys combined with plastics of different properties, and seals such as sealing water retaining strips, magnetic strips and other seals that are perfectly formed by the extrusion process; 5. Regardless of size, U-shaped grooves of different shapes, metal alloys and plastics with the same or different properties, such as PVC, rubber, silicone, etc., are integrally formed through extrusion technology; 6. All U-shaped card slots of different shapes, regardless of size and manufacturing process, including metal alloys, plastics, and bare magnetic strips, are made through precise extrusion process, allowing multiple types of materials with different properties to be perfectly combined into one.
[0041] Obviously, those skilled in the art can make various changes and modifications to the present invention without departing from the spirit and scope of the present invention. Thus, if these modifications and variations of the present invention fall within the scope of the claims of the present invention and their equivalents, the present invention is also intended to include these modifications and variations.
Claims
1. A rubber-plastic-metal magnetic sealing strip structure, the magnetic sealing strip structure comprising a magnetic strip, characterized in that: The magnetic sealing strip structure also includes: A magnetic stripe mounting seat made of soft rubber material, wherein a mounting groove is formed on one side of the outer side of the magnetic stripe mounting seat along its length direction, and the magnetic stripe is mounted in the mounting groove; A metal connector, one side of which is clamped and mounted on the bottom end of the magnetic strip mounting seat, and the other side of the metal connector is formed with a first U-shaped slot arranged in an inverted "U" shape, and the first U-shaped slot is arranged along the length direction of the metal connector; A glass clip is made of hard plastic material, and is formed with a second U-shaped slot for installing glass in an inverted "U" shape. The glass clip is fixedly installed in the slot of the first U-shaped slot, and the second U-shaped slot is arranged along the length direction of the glass clip.
2. A rubber-plastic-metal magnetic sealing strip structure according to claim 1, characterized in that: The inner walls on opposite sides of the second U-shaped slot are respectively formed with clamping strip structures, which include a pair of clamping strips arranged in an eight-shaped shape and extending from the inner wall of the second U-shaped slot in opposite directions toward the center, and the pair of clamping strips are symmetrically arranged up and down.
3. A rubber-plastic-metal magnetic sealing strip structure according to claim 2, characterized in that: The clamping strip structure and the glass clamping piece are integrally formed.
4. The rubber-plastic-metal magnetic sealing strip structure according to claim 1, characterized in that: The magnetic strip mounting seat is formed with a hollow inner cavity for buffering.
5. A rubber-plastic-metal magnetic sealing strip structure according to claim 2 or 3, characterized in that: A pair of the clamping strip structures are symmetrically arranged on the side walls of the second U-shaped slot on opposite sides, and the clamping strip structures are arranged at the notch of the second U-shaped slot.
6. The rubber-plastic-metal magnetic sealing strip structure according to claim 1, characterized in that: The magnetic strip mounting seat, the metal connector and the glass clip are integrally formed by extrusion molding.
7. A manufacturing process for manufacturing a rubber-plastic-metal magnetic sealing strip structure as claimed in claim 1, characterized in that: The manufacturing process comprises the following steps: Cut the metal into required sizes and load it into the unwinding rack; Processed into a preset groove shape by a cold rolling mill; Start two rubber and plastic extruders and one modified PVC extruder, and insert the metal parts and magnetic strips processed into the preset groove shape into the precision extrusion mold at high temperature, and then extrude them together with the rubber and PVC in the two rubber extruders and the modified PVC extruder to form an integrated rubber-plastic-metal magnetic sealing strip structure product; The rubber-plastic-metal magnetic sealing strip structure product just out of the mold is introduced into the shaping mold for shaping; After the rubber-plastic-metal magnetic sealing strip structure product is finalized, it is cooled and dried; The rubber-plastic-metal magnetic sealing strip structure products are cut according to the preset size.
8. The manufacturing process of a rubber-plastic-metal magnetic sealing strip structure according to claim 7, characterized in that: The rubber-plastic-metal magnetic sealing strip structure product that has just been molded is introduced into the molding mold for molding. During the molding process, the dimensional accuracy of the rubber-plastic-metal magnetic sealing strip structure product is ensured through cooling, moisturizing and vacuuming processes.
Citation Information
Patent Citations
Cloth-imitating type automobile door frame sealing strip and preparing technology thereof
CN110774559A
Vacuum glass panel
CN112424437A
Composite waterproof sealing rubber strip and manufacturing method thereof
CN116972168A
Shower room is to joint strip that opens door
CN207974744U
Integrally, Extrusion Blow Molded Container, Label and RFID Tag
US20190084722A1