Super-hydrophobic surface machining method and system and material piece

By forming a micron-order hydrophobic concave and convex structure on the surface of the power grid equipment, the existing power grid anti-icing methods are solved in low efficiency and high energy consumption in high humidity and extremely cold environments, and effective anti-icing on the surface of the energy equipment is achieved and improved The power supply reliability of the power grid.

CN119024651APending Publication Date: 2024-11-26CHONGQING UNIV
View PDF 0 Cites 0 Cited by

Patent Information

Application Number
CN202411174301.6
Authority / Receiving Office
CN · China
Patent Type
Applications(China)
Current Assignee / Owner
Filing Date
2024-08-23
Publication Date
2024-11-26

AI Technical Summary

Technical Problem

The existing power grid anti-icing methods are low in efficiency, high energy consumption, complex maintenance in high humidity and extremely cold environments, and require power outage operations, making it difficult to effectively prevent energy equipment from being covered with ice.

Method used

Using superhydrophobic surface processing method, the photoresist layer is coated on the surface of the material, photolithography pattern layer formed at the micrometer order by photolithography, and plasma bombardment etching is used to form a hydrophobic concave-convex structure at the micrometer order to form Superhydrophobic material parts are used to prevent ice from being frozen on the surface of the grid equipment.

Benefits of technology

It significantly improves the anti-ice effect of the power grid, reduces the difficulty of the power grid, avoids ice-cold surfaces of energy equipment, and improves the power supply reliability of the power grid.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure CN119024651A_ABST
    Figure CN119024651A_ABST
Patent Text Reader

Abstract

The invention discloses a super-hydrophobic surface processing method, a super-hydrophobic surface processing system and a material piece with a super-hydrophobic surface. The processing method comprises the following steps: coating a photoresist layer on the surface of the material piece to be processed; performing photoetching on the photoresist layer to remove the photoresist layer in a set area on the surface of the to-be-processed material piece so as to form a photoetching pattern layer of a photoresist area and a non-photoresist area, wherein the sizes of the photoresist area and the non-photoresist area in at least one direction are micron-scale; and performing bombardment etching on the surface of the to-be-processed material piece by using plasma, and processing a non-photoresist area on the to-be-processed material piece to form a groove, so that a micron-scale hydrophobic concave-convex structure is formed on the surface of the to-be-processed material piece. The to-be-machined material piece machined through the machining method has the super-hydrophobic surface, the to-be-machined material piece is used for preparing wind power equipment, photovoltaic equipment and other energy equipment, it can be avoided that the surfaces of various power grid equipment are frozen to a great extent, and the ice resistance difficulty of a power grid is reduced.
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] The present invention relates to the technical field of material processing, and in particular to a super-hydrophobic surface processing method and system, and a material part with a super-hydrophobic surface. Background Art

[0002] In recent years, the wind and solar energy power generation industry has developed rapidly, but when using wind and solar energy in high-altitude mountainous areas, there is the problem of icing of power generation energy equipment in the high humidity and extreme cold environment in autumn and winter. Icing of power generation energy equipment seriously threatens the safe and stable operation of the power grid, and is very likely to cause disasters such as line breakage, tower collapse, flashover tripping, and wind turbine shutdown, which in turn causes large-scale power outages and causes huge losses to the national economy.

[0003] For a long time, continuous research has been carried out at home and abroad on the defense of power grid icing, and certain breakthroughs have been made in the fields of mechanics, electromagnetism, heat, new materials, etc., and power grid anti-icing solutions have been formed, including mechanical deicing, airbag deicing, short-circuit current ice melting, electromagnetic pulse deicing, expanded-diameter conductor anti-icing, orthogonal double pendulum hammer anti-icing, coating of super-hydrophobic coatings and heating coatings. However, the various current power grid icing defense methods have certain limitations to a greater or lesser extent, and are restricted by factors such as the use environment. Taking DC ice melting technology as an example, this technology requires power outages, is complex and time-consuming to operate, and has shortcomings such as large and bulky equipment.

[0004] Based on the analysis of existing power grid anti-icing and de-icing schemes, there are not many power grid anti-icing methods that can be applied to actual engineering projects, and basically they need to be implemented under power outage conditions. They generally have shortcomings such as high energy consumption, low efficiency, and complex maintenance. Summary of the invention

[0005] The purpose of the present invention is to provide a super-hydrophobic surface processing method and system, and a material part with a super-hydrophobic surface, which can be used to process the surface of the material part to form a super-hydrophobic surface. The surface of the material part is applied to energy equipment in a power grid, which can effectively inhibit the formation and development of ice on the surface of the energy equipment, significantly improve the anti-icing effect of the power grid, and reduce the difficulty of anti-icing the power grid.

[0006] In order to solve the above technical problems, the present invention provides a super-hydrophobic surface processing method, comprising:

[0007] Coating a photoresist layer on the surface of the material to be processed;

[0008] Performing photolithography on the photoresist layer to remove the photoresist layer in a set area on the surface of the material piece to be processed, so as to form a photoresist pattern layer having photoresist areas and non-photoresist areas with sizes in the micrometer range in at least one direction;

[0009] The surface of the material to be processed is bombarded and etched by plasma, and grooves are formed in the non-photoresist area on the material to be processed, so that a hydrophobic concave-convex structure of micrometer level is formed on the surface of the material to be processed.

[0010] In an optional embodiment of the present application, the material to be processed is any one of a silicon material, a silicon dioxide material, an aluminum material or a copper material.

[0011] In an optional embodiment of the present application, coating a photoresist layer on the surface of the material to be processed includes:

[0012] Coating the photoresist layer with a thickness of 10 μm to 25 μm on the surface of the material to be processed;

[0013] The photoresist layer is photolithographically removed from a set area on the surface of the material to be processed to form a photoresist pattern layer having photoresist areas and non-photoresist areas with sizes in the micrometer range in at least one direction, including:

[0014] Performing photolithography on the photoresist layer to form the photoresist pattern layer in which the photoresist region and the non-photoresist region are alternately distributed on the surface of the material to be processed; wherein the photoresist region and the non-photoresist region are parallel to each other in strip shape, and the width of the photoresist region is 2 μm to 5 μm; and the width of the non-photoresist region is 4 μm to 7 μm;

[0015] The surface of the material to be processed is bombarded and etched by plasma to form a groove in the non-photoresist area on the material to be processed, including:

[0016] The non-photoresist area on the surface of the material to be processed is bombarded and etched by plasma to form a groove with a depth of 7 μm to 11 μm.

[0017] In an optional embodiment of the present application, before coating the surface of the material to be processed with a photoresist layer, the method further includes:

[0018] Placing the material to be processed in a mixed cleaning solution of ethanol and deionized water;

[0019] Applying ultrasonic vibration to the mixed cleaning liquid to clean the material to be processed;

[0020] The cleaned material to be processed is dried.

[0021] In an optional embodiment of the present application, bombarding and etching the surface of the material to be processed by plasma to form a groove in the non-photoresist area on the material to be processed includes:

[0022] Determining plasma parameters in advance according to the physical and chemical property parameters of the material to be processed;

[0023] Placing the material to be processed on a first electrode plate in a plasma generating device;

[0024] Filling the cavity of the plasma generator with a reaction gas and an inert gas, and controlling and adjusting the working parameters of the plasma generator so that the reaction gas generates plasma satisfying the plasma parameters in the cavity of the plasma generator;

[0025] The plasma is driven by the electric field between the first electrode plate and the second electrode plate to bombard the non-photoresist area on the material piece to be processed to form the groove.

[0026] In an optional embodiment of the present application, the physical and chemical property parameters at least include material hardness parameters;

[0027] The plasma parameters include plasma density, plasma temperature and active species content;

[0028] The plasma parameters are determined in advance according to the physical and chemical property parameters of the material to be processed, including:

[0029] The plasma parameters are determined in advance according to the fact that the plasma density, the plasma temperature and the active species content are all proportional to the material hardness parameter.

[0030] In an optional embodiment of the present application, the plasma parameters are determined in advance according to the physical and chemical property parameters of the material to be processed, including:

[0031] When the material hardness parameter is within a high hardness range and / or the material to be processed is a metal material, it is determined that the plasma density is within a high density range and the plasma temperature is within a high temperature range;

[0032] Wherein, the high hardness range is greater than or equal to 800 Pascal;

[0033] The high density range is 10 11 cm -3 ~10 12 cm -3 ;

[0034] The high temperature range is 5eV~10eV.

[0035] In an optional embodiment of the present application, the reaction gas includes at least one of oxygen, active chlorine gas or fluorine-based gas.

[0036] A material piece with a super-hydrophobic surface, wherein the surface of the material piece is formed by processing using any of the super-hydrophobic surface processing methods described above.

[0037] A super-hydrophobic surface processing system is used to implement the super-hydrophobic surface processing method as described in any of the above items, and the processing system includes a lithography device for etching the surface of a material to be processed to form a lithography pattern layer; a plasma generating device; a reaction gas supply device connected to the plasma generating device; and a vacuum pumping device connected to the plasma generating device.

[0038] The present invention provides a super-hydrophobic surface processing method, system, and material piece with super-hydrophobic surface. The processing method comprises: coating a photoresist layer on the surface of the material piece to be processed; performing photolithography on the photoresist layer to remove the photoresist layer in a set area on the surface of the material piece to be processed, so as to form a photolithography pattern layer of photoresist areas and non-photoresist areas with sizes in at least one direction of micrometer order; bombarding and etching the surface of the material piece to be processed by plasma, processing the non-photoresist area on the material piece to be processed to form grooves, so that a hydrophobic concave-convex structure in the micrometer order is formed on the surface of the material piece to be processed.

[0039] In the present application, the surface of the material to be processed is first coated with photoresist and the photoresist layer in a specific area is removed by photolithography to form a photolithography pattern layer; the photolithography pattern layer is equivalent to a mask layer, and when the surface of the material to be processed is bombarded and etched by plasma, the plasma can only etch the non-photoresist area in the photolithography pattern layer to form a groove with a certain depth, so that the etched area (i.e., groove) and the non-etched area of ​​the entire material to be processed form a micron-level concave-convex structure together, and this concave-convex structure is also a structural layer with super-hydrophobic function. Therefore, when the material to be processed after being processed by the processing method in the present application also has a super-hydrophobic surface, this material to be processed is used to prepare wind power, photovoltaic and other energy equipment, and it can also largely avoid the surface icing of various power grid equipment, reducing the difficulty of anti-icing of the power grid. BRIEF DESCRIPTION OF THE DRAWINGS

[0040] In order to more clearly illustrate the embodiments of the present invention or the technical solutions of the prior art, the drawings required for use in the embodiments or the description of the prior art will be briefly introduced below. Obviously, the drawings described below are only some embodiments of the present invention. For ordinary technicians in this field, other drawings can be obtained based on these drawings without paying creative work.

[0041] Figure 1 A schematic diagram of a process for processing a super-hydrophobic surface provided in an embodiment of the present application;

[0042] Figure 2 A schematic cross-sectional structure diagram of a processing flow of a material to be processed provided in an embodiment of the present application;

[0043] Figure 3 This is a schematic diagram of the structure of a plasma generating device provided in an embodiment of the present application. DETAILED DESCRIPTION

[0044] At present, coating with super-hydrophobic coating and heating coating is a common way to make the surface of power grid equipment hydrophobic. However, as the use time of power grid equipment increases, especially in outdoor environments, no matter what kind of coating layer is used, it will inevitably fall off, thereby reducing the anti-icing effect of the power grid.

[0045] For plates or other material structures with rough structures on the micron scale on the surface, they all have a certain degree of hydrophobicity. Water droplets on the superhydrophobic surface are in a Cassie-Baxter state (similar to the state where the surface of a lotus leaf is not wet). Because water droplets cannot adhere to the surface of the material structure, the material structure is obviously not easy to freeze.

[0046] To this end, this application considers that if a plate or material structure with a rough structure at the micron scale is used to prepare wind power, photovoltaic and other energy equipment in the power grid, it can obviously greatly reduce the possibility of icing on the surface of the energy equipment in the power grid, which can also reduce the difficulty of the power grid's anti-icing to a certain extent and improve the reliability of the power supply of the power grid.

[0047] In order to enable those skilled in the art to better understand the scheme of the present invention, the present invention is further described in detail below in conjunction with the accompanying drawings and specific implementation methods. Obviously, the described embodiments are only part of the embodiments of the present invention, rather than all of the embodiments. Based on the embodiments of the present invention, all other embodiments obtained by ordinary technicians in this field without making creative work are within the scope of protection of the present invention.

[0048] like Figure 1 and Figure 2 As shown, Figure 1 A schematic diagram of a process for processing a super-hydrophobic surface provided in an embodiment of the present application; Figure 2 A schematic cross-sectional structure diagram of a processing flow of a material to be processed provided in an embodiment of the present application.

[0049] In a specific embodiment of the present application, the super-hydrophobic surface processing method may include:

[0050] S1: Coat a photoresist layer on the surface of the material to be processed.

[0051] Firstly, the material to be processed in the present application can be of various different material types.

[0052] For example, the material to be processed may be a material plate used to prepare semiconductor devices, and the material to be processed may be a silicon material; it may also be a silicon dioxide material, specifically, it may be tempered glass used as a glass plate in a photovoltaic module.

[0053] The material to be processed may be a metal material, such as an aluminum material or a copper material, in addition to the non-metal material mentioned above.

[0054] In addition, before coating the surface of the material to be processed with a photoresist layer, the surface of the material to be processed can be cleaned and pre-treated. Specifically, the material to be processed can be placed in a mixed cleaning liquid of ethanol and deionized water, and then the mixed cleaning liquid can be ultrasonically vibrated to clean the material to be processed. After the cleaning of the material to be processed is completed, the material to be processed can be further dried.

[0055] After the cleaning pretreatment of the material to be processed is completed, a photoresist layer may be further coated on the surface of the material to be processed.

[0056] In practical applications, the thickness of the photoresist layer coated on the surface of the material to be processed may be 10 μm to 25 μm.

[0057] S2: performing photolithography on the photoresist layer to remove the photoresist layer in a set area on the surface of the material piece to be processed, so as to form a photoresist pattern layer having photoresist areas and non-photoresist areas with sizes in micrometers in at least one direction.

[0058] Reference Figure 2 When the photoresist layer 11 in a set area on the surface of the material piece 10 to be processed is actually exposed and removed, the shape and size of the set area can be pre-set; after the photoresist layer 11 in the set area is removed by exposure photolithography, a photoresist pattern layer including a photoresist area and a non-photoresist area can be formed on the side surface of the material piece 10 to be processed; wherein the photoresist area is the area covered by the photoresist, and the non-photoresist area is the area not covered by the photoresist, which corresponds to the set area.

[0059] On this basis, when actually determining the set area, it should be ensured that the size of the photoresist area and the non-photoresist area is in the micron order at least in one direction; for example, the size of the photoresist area and the non-photoresist area in the set direction is in the micron order, that is to say, the distance in the set direction between any boundary line segment of the photoresist area and another adjacent boundary line segment that is closest in the set direction is in the micron order. In practical applications, the photoresist area on the surface of the entire material to be processed can be a completely connected complete area, and the non-photoresist area can also be a completely connected area, for example, the photoresist area and the non-photoresist area can be mutually nested spiral-shaped areas. The photoresist area and the non-photoresist area on the surface of the material to be processed can also include multiple, and each photoresist area and the non-photoresist area are mixed and alternately distributed, for example, the photoresist area and the non-photoresist area are both in the shape of multiple concentric rings, and the photoresist area and the non-photoresist area are alternately arranged in circles, which can also realize the technical solution of the present application.

[0060] Reference Figure 2 In another optional implementation of the present embodiment, after the photoresist layer 11 of the material piece 10 to be processed is photolithographically processed, a photoresist pattern layer in which photoresist areas and non-photoresist areas are alternately distributed is formed on the surface of the material piece to be processed; and the photoresist areas and non-photoresist areas are strip areas parallel to each other, and the width of the photoresist areas is 2μm~5μm; the width of the non-photoresist areas is 4μm~7μm.

[0061] It can be understood that, in practical applications, the width of the photoresist region should be slightly larger than the width of the non-photoresist region.

[0062] S3: bombarding and etching the surface of the material to be processed by plasma, and forming grooves in the non-photoresist area on the material to be processed, so that a hydrophobic concave-convex structure of micrometer level is formed on the surface of the material to be processed.

[0063] After the photoresist layer in a set area on the material to be processed is exposed, etched and removed, the photoresist layer in the photoresist area is equivalent to forming a mask on the surface of the material to be processed; when the surface of the material to be processed is bombarded with plasma, the photoresist area on the surface of the material to be processed covered with the photoresist layer is blocked and covered, and the high-energy ions in the plasma hit the non-photoresist area on the surface of the material to be processed that is not covered by the photoresist, causing atoms of the material to be processed to be sputtered out from the surface. As the plasma continues to bombard and etch, the number of atoms sputtered on the surface of the material to be processed gradually increases, that is, grooves of a certain depth are gradually formed in the bombarded non-photoresist area. This process is purely physical etching and does not involve chemical reactions.

[0064] In an optional implementation of this embodiment, plasma is used to bombard and etch the non-photoresist area on the surface of the workpiece, and the depth of the formed groove can be 7μm~11μm; specifically, the groove can be 7μm, 8μm, 9μm, 10μm, 11μm. It should be noted that in actual applications, if the width of the photolithography area and the non-photolithography area is relatively larger, the depth of the corresponding groove can be relatively smaller; conversely, when the width of the photolithography area and the non-photolithography area is relatively small, the depth of the groove can be relatively larger.

[0065] Further optionally, in this embodiment, the process of bombarding and etching the surface of the material to be processed by plasma may further include:

[0066] S31: Determine the plasma parameters in advance according to the physical and chemical property parameters of the material to be processed.

[0067] It should be noted that, in this embodiment, the physical and chemical property parameters of the material to be processed may include material hardness parameters, material chemical composition type, etc.; and the plasma parameters may include plasma density, plasma temperature, active particle content, etc. For different physical and chemical property parameters, the corresponding plasma parameters are not the same. In general, plasma density, plasma temperature, active particle content, etc. should be related to the physical and chemical property parameters of the material to be processed.

[0068] (1) The relationship between the material hardness parameters of the material to be etched and the plasma parameters is as follows:

[0069] ① If the material hardness parameter is a low hardness material (Vickers hardness HV<200), then:

[0070] Plasma density: medium to low (10 9 cm -3 ~10 10 cm -3 );

[0071] Plasma temperature: low (1eV~3eV);

[0072] Active particle content: low;

[0073] Reason: Low hardness materials can be effectively etched at low plasma density and plasma temperature, avoiding excessive damage or decomposition of the material due to high temperature.

[0074] ② If the material hardness parameter is medium hardness material (200≤HV<800), then:

[0075] Plasma density: medium (10 10 cm -3 ~10 11cm -3 );

[0076] Plasma temperature: medium (3eV~5eV);

[0077] Active particle content: medium;

[0078] Reason: Medium hardness materials require moderate plasma density and plasma temperature to achieve uniform and effective etching; too high plasma density and plasma temperature may cause the etching rate to be too fast and damage the material surface.

[0079] ③ If the material hardness parameter is high hardness material (HV ≥ 800), then:

[0080] Plasma Density: High (10 11 cm -3 ~10 12 cm ^-3 );

[0081] Plasma temperature: high (5eV~10eV);

[0082] Active particle content: high;

[0083] Reason: High-hardness materials require high-density and high-temperature plasma to provide sufficient energy and active particles to overcome the hardness of the material and achieve effective etching.

[0084] (2) The relationship between the chemical composition of the material to be etched and the plasma parameters is as follows:

[0085] ① When the material to be etched is a metal material,

[0086] Plasma Density: High (10 11 cm -3 ~10 12 cm -3 );

[0087] Plasma temperature: high (5eV~10eV);

[0088] Active particle content: high (especially active etching gases such as chlorine or fluorine);

[0089] Reason: Metal materials are usually chemically inert and require high-energy plasma and high concentrations of active particles to break metal bonds and form volatile products.

[0090] ② When the material to be etched is a semiconductor material (such as silicon, gallium arsenide), then:

[0091] Plasma Density: Medium to High (10 10 cm -3~10 11 cm -3 );

[0092] Plasma temperature: medium (3eV~5eV);

[0093] Active particle content: medium;

[0094] Reason: Semiconductor materials require moderate plasma parameters to ensure etching uniformity while avoiding damage to the material's mechanical properties.

[0095] ③ When the material to be etched is an oxide material (such as SiO2):

[0096] Plasma density: medium (10 10 cm -3 ~10 11 cm -3 );

[0097] Plasma temperature: medium (3eV~5eV);

[0098] Active particle content: medium (especially fluorine-based etching gases);

[0099] Reason: Oxide materials are chemically stable and require plasma with moderate parameters to effectively etch and form volatile products.

[0100] On this basis, in a specific implementation of this embodiment, when the material hardness parameter is within the high hardness range and / or the material to be processed is a metal material, it is determined that the plasma density is within the high density range and the plasma temperature is within the high temperature range; obviously, the high hardness range is greater than or equal to 800 Pascals; the high density range is 10 11 cm -3 ~10 12 cm -3 The high temperature range is 5eV to 10eV. It should be noted that in this embodiment, the Kelvin temperature of the plasma is characterized by electron volts.

[0101] S32: placing the material to be processed on the first electrode plate in the plasma generating device.

[0102] Reference Figure 3In the plasma generating device, a reaction chamber 20 is included, in which a first electrode plate 21 and a second electrode plate 22 are arranged; the first electrode plate 21 and the second electrode plate 22 are powered by a radio frequency power supply, so that an electric field is formed between the first electrode plate 21 and the second electrode plate 22; the electric field can ionize the reaction gas in the reaction chamber 20 to generate plasma, and the electric field force applied by the electric field to the plasma can drive the plasma to bombard the surface of the workpiece 10 to be processed on the first electrode plate 21.

[0103] In practical applications, the first electrode plate 21 and the second electrode plate 22 can be two semi-cylindrical electrode plates; the two electrode plates have the same radius, and the specific size can be determined according to the requirements of the material to be processed for plasma density.

[0104] S33: Filling the cavity of the plasma generator with reaction gas and inert gas, and controlling and adjusting the working parameters of the plasma generator so that the reaction gas generates plasma satisfying the plasma parameters in the cavity of the plasma generator; utilizing the electric field between the first electrode plate and the second electrode plate to drive the plasma to bombard the non-photoresist area on the workpiece to form a groove.

[0105] It is understandable that the reaction gas may also be different based on the different physical and chemical property parameters of the material to be processed. As shown in Table 1, Table 1 lists the types of reaction gases corresponding to the material to be processed of several different materials.

[0106] Table 1:

[0107] The type of material to be etched Reaction gas silicon <![CDATA[O2 / Ar / C4F8 / C l2 / SF6]]> Silicon dioxide <![CDATA[CF4 / CH2 / NF3]]> copper <![CDATA[C l2 / CF4]]> aluminum <![CDATA[C l2 / BC l3 ]]>

[0108] Based on Table 1, it can be seen that the reaction gas in this embodiment can be at least one of oxygen, active chlorine gas or fluorine-based gas; in actual applications, the reaction gas can contain only one type of gas or a mixed gas containing multiple different types of gases.

[0109] It can be understood that in the present embodiment, when using a plasma generator to perform groove etching on the surface of a workpiece to be processed, based on the different requirements of the workpiece to be processed for plasma parameters, it is necessary to make different adjustments to the working parameters of the plasma generator; the working parameters of the plasma generator include: RF power, chamber pressure, gas type, gas flow rate, radius of the cylindrical flat plate electrode, and distance between the plates.

[0110] To further facilitate understanding, the correlation between plasma parameters and operating parameters of the plasma generating device will be specifically described below.

[0111] (1) RF power

[0112] Plasma density: As the RF power increases, the plasma density increases; higher power can provide more energy to ionize gas molecules and generate more electrons and ions.

[0113] Plasma temperature: As the RF power increases, both the electron temperature and the ion temperature increase because higher power provides more energy to the plasma particles.

[0114] Active Species Content: As the RF power increases, the generation rate of active species (such as free radicals and ions) also increases because more gas molecules are ionized and excited.

[0115] (2) Cavity pressure

[0116] Plasma density: At low pressure, the plasma density is low; as the pressure increases, the plasma density also increases.

[0117] Plasma temperature: At low pressure, the RF power temperature is high; as the pressure increases, the electron temperature decreases because the collision frequency increases and the energy is dispersed at high pressure.

[0118] Active particle content: Moderate pressure is conducive to the generation of more active particles; too high or too low pressure may be unfavorable for the generation of active particles.

[0119] (3) Gas type

[0120] Plasma density: Different reactive gases have different ionization energies, which affect the plasma density. For example, helium and hydrogen are easier to form high-density plasmas due to their low ionization energies, while oxygen and nitrogen form lower-density plasmas due to their high ionization energies.

[0121] Plasma temperature: Different gases have different ionization and excitation characteristics, which affect the plasma temperature. For example, hydrogen plasma has a higher temperature, while argon plasma has a relatively low temperature.

[0122] Active particle content: Different gases generate different active particles. For example, active oxygen atoms (O) generated by oxygen and fluorine atoms (F) generated by fluorine gas play a key role in the etching process.

[0123] (4) Gas flow

[0124] Plasma Density: As the gas flow rate increases, the plasma density increases because more gas molecules are available for ionization.

[0125] Plasma temperature: Excessive gas flow may cause the plasma temperature to drop as the cold gas enters the chamber and absorbs energy.

[0126] Active particle content: A moderate gas flow rate helps to generate more active particles, while too high or too low a gas flow rate may be detrimental to the generation and maintenance of active particles.

[0127] (5) Radius of cylindrical plate electrode

[0128] Plasma density: When the electrode radius is larger, the plasma volume is larger and the density is lower; when the electrode radius is smaller, the plasma volume is smaller and the density is higher.

[0129] Plasma temperature: The effect of electrode radius on temperature is more complex and needs to be considered in combination with other parameters.

[0130] Active particle content: The electrode radius affects the uniformity of the plasma and thus the distribution of active particles.

[0131] (6) Distance between boards

[0132] Plasma density: When the distance between the plates is small, the electric field strength is high, and high-density plasma is easily formed; when the distance between the plates is large, the electric field strength is low and the plasma density decreases.

[0133] Plasma temperature: When the distance between the plates is small, the electron temperature is higher; when the distance between the plates is large, the electron temperature is lower.

[0134] Active species content: The distance between the plates affects the plasma generation area and the uniformity of active species.

[0135] In summary, in this application, the surface of the material to be processed is first coated with photoresist and the photoresist layer in a specific area is photolithographically removed to form a photolithographic pattern layer; the photolithographic pattern layer is equivalent to a mask layer, and when the surface of the material to be processed is bombarded and etched by plasma, the plasma can only etch the non-photoresist area in the photolithographic pattern layer to form a groove with a certain depth, thereby making the etched area (i.e., groove) and the non-etched area of ​​the entire material to be processed form a micron-level concave-convex structure together, and this concave-convex structure is also a structural layer with super-hydrophobic function. Therefore, when the material to be processed after being processed by the processing method in this application also has a super-hydrophobic surface, this material to be processed is used to prepare wind power, photovoltaic and other energy equipment, and it can also avoid icing on the surface of various power grid equipment to a large extent, reducing the difficulty of anti-icing of the power grid.

[0136] The present application also provides an embodiment of a material piece having a super-hydrophobic surface, wherein the surface of the material piece is formed by processing using any of the super-hydrophobic surface processing methods described above.

[0137] The present application also provides an embodiment of a super-hydrophobic surface processing system, which is used to implement the super-hydrophobic surface processing method as described in any of the above items. The processing system may include a lithography device for etching the surface of a material to be processed to form a lithography pattern layer; a plasma generating device; a reaction gas supply device connected to the plasma generating device; and a vacuum pumping device connected to the plasma generating device.

[0138] It should be noted that, in this article, relational terms such as first and second, etc. are only used to distinguish one entity or operation from another entity or operation, and do not necessarily require or imply that there is any such actual relationship or order between these entities or operations. Moreover, the term "includes", "comprising" or any other variant thereof is intended to cover non-exclusive inclusion, so that the process, method, article or equipment comprising a series of elements are inherent to the elements. In the absence of more restrictions, the elements limited by the sentence "comprising one..." do not exclude the presence of other identical elements in the process, method, article or equipment comprising the elements. In addition, the above-mentioned technical solution provided in the embodiment of the present application is consistent with the corresponding technical solution in the prior art in principle, and the part is not described in detail, so as to avoid too much redundancy.

[0139] The principles and implementation methods of the present invention are described in this article using specific examples. The description of the above embodiments is only used to help understand the method and core ideas of the present invention. It should be pointed out that for ordinary technicians in this technical field, several improvements and modifications can be made to the present invention without departing from the principles of the present invention, and these improvements and modifications also fall within the scope of protection of the claims of the present invention.

Claims

1. A super-hydrophobic surface processing method, characterized in that: include: Coating a photoresist layer on the surface of the material to be processed; Performing photolithography on the photoresist layer to remove the photoresist layer in a set area on the surface of the material piece to be processed, so as to form a photoresist pattern layer having photoresist areas and non-photoresist areas with sizes in the micrometer range in at least one direction; The surface of the material to be processed is bombarded and etched by plasma, and grooves are formed in the non-photoresist area on the material to be processed, so that a hydrophobic concave-convex structure of micrometer level is formed on the surface of the material to be processed.

2. The super-hydrophobic surface processing method as claimed in claim 1, wherein The material to be processed is any one of a silicon material, a silicon dioxide material, an aluminum material or a copper material.

3. The super-hydrophobic surface processing method as claimed in claim 1, wherein A photoresist layer is coated on the surface of the material to be processed, including: Coating the photoresist layer with a thickness of 10 μm to 25 μm on the surface of the material to be processed; The photoresist layer is photolithographically removed from a set area on the surface of the material to be processed to form a photoresist pattern layer having photoresist areas and non-photoresist areas with sizes in the micrometer range in at least one direction, including: Performing photolithography on the photoresist layer to form the photoresist pattern layer in which the photoresist region and the non-photoresist region are alternately distributed on the surface of the material to be processed; wherein the photoresist region and the non-photoresist region are parallel to each other in strip shape, and the width of the photoresist region is 2 μm to 5 μm; and the width of the non-photoresist region is 4 μm to 7 μm; The surface of the material to be processed is bombarded and etched by plasma to form a groove in the non-photoresist area on the material to be processed, including: The non-photoresist area on the surface of the material to be processed is bombarded and etched by plasma to form a groove with a depth of 7 μm to 11 μm.

4. The super-hydrophobic surface processing method as claimed in claim 1, wherein Before coating the photoresist layer on the surface of the material to be processed, the method also includes: Placing the material to be processed in a mixed cleaning solution of ethanol and deionized water; Applying ultrasonic vibration to the mixed cleaning liquid to clean the material to be processed; The cleaned material to be processed is dried.

5. The super-hydrophobic surface processing method according to any one of claims 1 to 4, characterized in that, The surface of the material to be processed is bombarded and etched by plasma to form a groove in the non-photoresist area on the material to be processed, including: Determining plasma parameters in advance according to the physical and chemical property parameters of the material to be processed; Placing the material to be processed on a first electrode plate in a plasma generating device; Filling the cavity of the plasma generator with a reaction gas and an inert gas, and controlling and adjusting the working parameters of the plasma generator so that the reaction gas generates plasma satisfying the plasma parameters in the cavity of the plasma generator; The plasma is driven by the electric field between the first electrode plate and the second electrode plate to bombard the non-photoresist area on the material piece to be processed to form the groove.

6. The super-hydrophobic surface processing method as claimed in claim 5, characterized in that, The physical and chemical property parameters at least include material hardness parameters; The plasma parameters include plasma density, plasma temperature and active species content; The plasma parameters are determined in advance according to the physical and chemical property parameters of the material to be processed, including: The plasma parameters are determined in advance according to the fact that the plasma density, the plasma temperature and the active species content are all proportional to the material hardness parameter.

7. The super-hydrophobic surface processing method according to claim 6, wherein: The plasma parameters are determined in advance according to the physical and chemical property parameters of the material to be processed, including: When the material hardness parameter is within a high hardness range and / or the material to be processed is a metal material, it is determined that the plasma density is within a high density range and the plasma temperature is within a high temperature range; Wherein, the high hardness range is greater than or equal to 800 Pascal; The high density range is 10 11 cm -3 ~10 12 cm -3 ; The high temperature range is 5eV~10eV.

8. The super-hydrophobic surface processing method according to claim 6, wherein: The reaction gas includes at least one of oxygen, active chlorine gas or fluorine-based gas.

9. A material having a super-hydrophobic surface, characterized in that: The surface of the material piece is formed by processing using the super-hydrophobic surface processing method as described in any one of claims 1 to 8.

10. A super-hydrophobic surface processing system, characterized in that: Used to implement the super-hydrophobic surface processing method as described in any one of claims 1 to 8, the processing system includes a lithography device for etching the surface of a material to be processed to form a lithography pattern layer; a plasma generating device; a reaction gas supply device connected to the plasma generating device; and a vacuum pumping device connected to the plasma generating device.