Application method of micro-aperture TGV on folding display screen supporting component BKT
By setting up micro-through holes in the bending area of the folding display support structure component and filling with foldable liquid glue, the problem of through-hole morphology transfer during bending is solved, and the bending performance and service life are improved.
Patent Information
- Application Number
- CN202411321530.6
- Authority / Receiving Office
- CN · China
- Patent Type
- Applications(China)
- Current Assignee / Owner
- Filing Date
- 2024-09-23
- Publication Date
- 2024-11-26
AI Technical Summary
The existing folding display supporting structural parts are poorly displayed due to dust accumulation and deformation in the large hole area during bending, and the through-hole morphology is easily transferred to the display screen, which affects the service life.
Micro-through holes arranged in parallel (diameter 0.02mm~0.1mm) are used to arrange micro-through holes in parallel to the bending area of the supporting structure, and fill the micro-through holes with foldable liquid glue. After the liquid glue is cured, it absorbs bending deformation to avoid through holes. Transfer the morphology to the display.
Effectively disperse bending deformation, reduce single-through hole deformation, avoid the through hole morphology transfer to the folding display, and improve bending performance and service life.
Smart Images

Figure CN119028229A_ABST
Abstract
Description
Technical Field
[0001] The present invention relates to the technical field of non-film-printed folding display screens, and in particular to an application method of a micro-aperture TGV on a folding display screen support component BKT. Background Art
[0002] Folding displays have attracted widespread attention from users because of their advantages of both large screens and portability. The supporting structure, as the main supporting component of the folding display, can meet the bendability of the folding display while improving the compression resistance of the folding display, avoiding damage to the folding display due to compression, and effectively increasing the service life of the folding display.
[0003] The supporting structure of the folding display screen is evenly punched in the bending area through the punching technology to achieve foldability; the traditional folding display screen supporting structure uses 0.1~0.2mm stainless steel plate (P-SUS) and adopts hollowing technology in the folding area. The through-hole size is 0.15-0.4mm wide and 3.5-6.5mm long. Such a large hole area is prone to dust accumulation during the bending process, resulting in poor display in the bending area. In addition, the large hole area is greatly deformed during the bending process, which easily transfers the through-hole morphology to the display screen and causes obvious film printing. Summary of the invention
[0004] The purpose of the present invention is to address the deficiencies of the prior art and provide a folding display screen support structure. By reducing the through-hole diameter of the folding zone of the support structure and increasing the number of through-holes, the deformation during the bending process is dispersed over more micro-through-holes, the deformation of a single through-hole is reduced, and the transfer of the through-hole morphology to the folding display screen during the bending process is avoided. At the same time, for different micro-through-hole diameters, a matching micro-through-hole processing method is provided. For support structures with micro-through-hole diameters above 0.1 mm, after punching, a foldable liquid glue is filled in the micro-through-holes. After the liquid glue is cured, it can absorb the deformation of the micro-through-holes during the bending process, thereby avoiding the transfer of the through-hole morphology to the folding screen.
[0005] To achieve the above-mentioned purpose, the present invention first provides a folding display screen supporting structure, wherein the folding display screen comprises a supporting structure, a protective film, a display screen and a foldable liquid adhesive layer from bottom to top, and the bending area of the supporting structure is processed with multiple rows of parallelly arranged micro-through holes, the micro-through holes are circular and evenly distributed in the bending area of the supporting structure, the diameter of the micro-through holes is 0.02mm~0.1mm, and the spacing between the micro-through holes is 0.5~5mm.
[0006] The supporting structure is made of glass, and the thickness of the supporting structure is 0.1-0.3 mm.
[0007] The protective film is a U-Film protective film, and the U-Film protective film is fixedly arranged between the supporting structure and the display screen.
[0008] The material of the foldable liquid adhesive layer is acrylic polymer, silicone resin, epoxy resin or polyurethane resin.
[0009] The present invention also provides a method for applying the micro-aperture TGV to the folding display screen support member BKT, comprising the following steps:
[0010] Step S1, cleaning the supporting structure to be processed;
[0011] Step S2, uniformly punching holes in the bending area of the supporting structure;
[0012] Step S3, cleaning the punched support structure again;
[0013] Step S4, sequentially covering the punched and cleaned support structure with a U-Film protective film and a display screen, filling with foldable liquid glue, and performing a curing process to obtain a foldable display screen without film marks;
[0014] Step S5: performing a bending test on the obtained foldable display screen to verify its performance.
[0015] Specifically, in step S2, the bending area of the supporting structure is evenly punched, and the punching method is TGV punching, laser punching, or etching punching.
[0016] Specifically, the punching method is TGV punching, and the punching hole diameter is 0.02-0.1 mm; the punching method is laser punching or etching punching, and the punching hole diameter is greater than 0.1 mm.
[0017] Specifically, the curing treatment in step S4 is heat curing, moisture curing or UV curing.
[0018] Specifically, the bending test in step S5 has the following test conditions: bending 200,000 times at R1.0-20°C & 60°C / 90% RH & 70°C without breakage.
[0019] Compared with the prior art, the present invention has the following beneficial effects:
[0020] 1. The present invention reduces the diameter of the through holes in the folding area of the supporting structure and increases the number of through holes, thereby dispersing the deformation during the bending process on more micro-through holes, reducing the deformation of a single through hole, and avoiding the transfer of the through hole morphology to the folding display screen during the bending process.
[0021] 2. The present invention provides a matching micro-through hole processing method for different micro-through hole diameters. For supporting structural parts with micro-through hole diameters above 0.1 mm, foldable liquid glue is filled in the micro-through hole after punching. After the liquid glue is cured, it can absorb the deformation of the micro-through hole during the bending process, thereby avoiding the transfer of the through hole morphology to the folding screen display. BRIEF DESCRIPTION OF THE DRAWINGS
[0022] Figure 1 This is a structural diagram of the folding display screen of the present invention;
[0023] Figure 2 A schematic diagram of filling the foldable liquid glue of the present invention;
[0024] Figure 3 This is a morphology diagram of the through holes in the bending area of the supporting structure of a traditional folding display screen.
[0025] In the figure: 1. Support structure; 2. Protective film; 3. Display screen; 4. Foldable liquid adhesive layer; 5. Micro-through hole. DETAILED DESCRIPTION
[0026] In order to better reflect the advantages and innovations of the present invention and clearly demonstrate the technical solution of the present invention, the present invention will be further described in detail below in conjunction with specific embodiments.
[0027] Example
[0028] The present invention provides a folding display screen supporting structure, such as Figure 1 As shown, the foldable display screen is composed of a supporting structure, a protective film, a display screen and a foldable liquid adhesive layer from bottom to top. The bending area of the supporting structure is processed with multiple rows of parallel micro-through holes. The micro-through holes are circular and evenly distributed in the bending area of the supporting structure. The diameter of the micro-through holes is 0.02mm~0.1mm, and the spacing between the micro-through holes is 0.5~5mm.
[0029] The supporting structure is made of glass, and the thickness of the supporting structure is 0.1-0.3 mm.
[0030] The protective film is a U-Film protective film, and the U-Film protective film is fixedly arranged between the supporting structure and the display screen.
[0031] The material of the foldable liquid adhesive layer is acrylic polymer, silicone resin, epoxy resin or polyurethane resin.
[0032] In this embodiment, a method for applying a micro-aperture TGV to the folding display screen support member BKT is also provided, comprising the following steps:
[0033] Step S1, cleaning the supporting structure to be processed;
[0034] Step S2, uniformly punching holes in the bending area of the supporting structure;
[0035] Step S3, cleaning the punched support structure again;
[0036] Step S4, sequentially covering the punched and cleaned support structure with a U-Film protective film and a display screen, filling with foldable liquid glue, and performing a curing process to obtain a foldable display screen without film marks;
[0037] Step S5: performing a bending test on the obtained foldable display screen to verify its performance.
[0038] Specifically, in step S2, the bending area of the supporting structure is evenly punched, and the punching method is TGV punching, laser punching, or etching punching.
[0039] Specifically, the punching method is TGV punching, and the punching hole diameter is 0.02-0.1 mm; the punching method is laser punching or etching punching, and the punching hole diameter is greater than 0.1 mm.
[0040] It should be noted that if Figure 2 As shown, when the aperture of the through hole is above 0.1 mm, it is necessary to fill the through hole of the supporting structure with foldable liquid glue after punching. After the foldable liquid glue is cured, it will absorb the deformation of the through hole during the bending process, further preventing the through hole morphology from being transferred to the folding screen display.
[0041] Specifically, the curing treatment in step S4 is heat curing, moisture curing or UV curing.
[0042] Specifically, the bending test in step S5 has the following test conditions: bending 200,000 times at R1.0-20°C & 60°C / 90% RH & 70°C without breakage.
[0043] The performance of the folding display screen support structure provided by the present invention is further tested and explained through comparative tests.
[0044] 1. Appearance inspection
[0045] 20 observers were randomly selected to observe the folding display screen made of the support structure provided by the present invention and the folding display screen made of the traditional support structure. The through hole morphology of the folding zone of the traditional support structure is as follows: Figure 3 As shown, statistical observers observed obvious hole marks in the bending area when the folding display was in a bent state. The results are shown in Table 1 below.
[0046] Table 1. Appearance test results
[0047]
[0048]
[0049] Note: "0" indicates no obvious film mark was observed; "1" indicates obvious film mark was observed.
[0050] It can be seen from the results in the above table that the present invention reduces the aperture of the through holes in the folding area of the supporting structure and increases the number of through holes, thereby dispersing the deformation in the bending process over more micro-through holes, reducing the deformation of a single through hole, and avoiding the transfer of the through hole morphology to the folding display screen during the bending process.
[0051] 2. Drop ball test
[0052] A 35g steel ball is used for dropping. The ball-dropping jig is made of stainless steel, with a smooth surface and no scratches, dents, bumps or other surface defects. The steel ball is dropped from a height of 5cm at the center of the hole-dropping area. Each height is tested 5 times. After the test is completed, it is confirmed that the product appearance is not broken. The height is increased at intervals of 1cm until it breaks, and the height value before breaking is recorded.
[0053] The above method was used to perform a ball drop test on the TGV glass, the supporting structure of the present invention, the folding display screen made by using the supporting structure of the present invention, and the traditional supporting structure. The results are shown in Table 2 below.
[0054] Table 2. Ball drop test results
[0055]
[0056]
[0057] It can be seen from the results in the above table that the support structure provided by the present invention can avoid the transfer of the through-hole morphology to the folding display screen during the bending process. Compared with traditional support structures, the ball drop strength of the bending zone of the support structure provided by the present invention is basically the same as that of traditional support structures.
[0058] 3. Bending test of foldable glass cover after hole filling protection
[0059] As shown in Table 3 below, the fracture conditions of the bending area of a folding display screen made of the supporting structure of the present invention and a folding display screen made of a traditional supporting structure after being bent 200,000 times at R1.0.
[0060] Table 3. Bending test results
[0061]
[0062] Note: “ / ” indicates that the sample did not break after being bent 200,000 times; “*” indicates that the sample broke after being bent 200,000 times.
[0063] It can be seen from the above table that the bending performance of the bending zone of the foldable glass cover plate after hole filling and protection according to the method of the present invention is not significantly different from that of the traditional foldable glass, and the bending performance is not reduced.
[0064] In summary, the present invention reduces the diameter of the through holes in the folding area of the supporting structure and increases the number of through holes, thereby dispersing the deformation in the bending process onto more micro-through holes. Under the premise of ensuring the ball drop strength and bending performance, the deformation of a single through hole is reduced, and the transfer of the through hole morphology to the folding display screen to produce film marks can be effectively avoided during the bending process, thereby affecting the user experience of the folding display screen product.
[0065] It should be understood that the above description of the preferred embodiment is relatively detailed and cannot be regarded as limiting the scope of patent protection of the present invention. Under the enlightenment of the present invention, ordinary technicians in this field can also make substitutions or modifications without departing from the scope of protection of the claims of the present invention, which all fall within the scope of protection of the present invention. The scope of protection requested for the present invention shall be based on the attached claims.
Claims
1. A folding display screen supporting structure, characterized in that: The foldable display screen comprises, from bottom to top, a supporting structure (1), a protective film (2), a display screen (3) and a foldable liquid adhesive layer (4); the supporting structure (1) has a bending region processed with a plurality of rows of micro-through holes (5) arranged in parallel; the micro-through holes (5) are circular and evenly distributed in the bending region of the supporting structure (1); the diameter of the micro-through holes (5) is 0.02 mm to 0.1 mm, and the spacing between the micro-through holes (5) is 0.5 to 5 mm.
2. A folding display screen supporting structure according to claim 1, characterized in that: The supporting structure (1) is made of glass, and the thickness of the supporting structure (1) is 0.1-0.3 mm.
3. The folding display screen supporting structure according to claim 1, characterized in that: The protective film (2) is a U-Film protective film, and the U-Film protective film is fixedly arranged between the supporting structure (1) and the display screen (3).
4. The folding display screen supporting structure according to claim 1, characterized in that: The material of the foldable liquid adhesive layer (4) is acrylic polymer, silicone resin, epoxy resin or polyurethane resin.
5. A method for applying a micro-aperture TGV to a folding display screen support structure BKT, corresponding to the folding display screen support structure as described in claims 1-4, characterized in that: The following steps are involved: Step S1, cleaning the supporting structure to be processed (1); Step S2, uniformly punching holes in the bending area of the supporting structure (1); Step S3, cleaning the punched support structure (1) again; Step S4, sequentially covering the punched and cleaned support structure (1) with a U-Film protective film and a display screen, filling with foldable liquid glue, and performing a curing treatment to obtain a foldable display screen without film marks; Step S5: performing a bending test on the obtained foldable display screen to verify its performance.
6. The method for applying the micro-aperture TGV to the folding display screen support member BKT according to claim 5, characterized in that: In step S2, the bending area of the supporting structure (1) is evenly punched, and the punching method is TGV punching, laser punching or etching punching.
7. The method for applying the micro-aperture TGV to the folding display screen support member BKT according to claim 6, characterized in that: The punching method is TGV punching, and the punching hole diameter is 0.02-0.1 mm; the punching method is laser punching or etching punching, and the punching hole diameter is above 0.1 mm.
8. The method for applying the micro-aperture TGV to the folding display screen support member BKT according to claim 5, characterized in that: The curing treatment in step S4 is heat curing, moisture curing or UV curing.
9. The method for applying the micro-aperture TGV to the folding display screen support member BKT according to claim 5, characterized in that: The bending test in step S5 is conducted under the following test conditions: 200,000 bends at -20°C & 60°C / 90%RH & 70°C without breakage.
Citation Information
Patent Citations
Support plate and display device
CN114333601A
Supporting piece, preparation method of supporting piece, display module and electronic equipment
CN115171528A
Display device
CN118135896A
Folding display device
CN210627726U
Supporting backboard, flexible display module and display device
CN216249792U