Phase change memory and preparation method thereof
By growing nanowires as lower electrodes on the second metal layer and wrapping them in the second dielectric layer, the problems of complex processes and high cost in the prior art are solved, and effective control of the size and contact area of the lower electrode are achieved, thereby improving the improvement of The performance and preparation efficiency of phase change memory are achieved.
Patent Information
- Application Number
- CN202310600384.X
- Authority / Receiving Office
- CN · China
- Patent Type
- Applications(China)
- Current Assignee / Owner
- Filing Date
- 2023-05-25
- Publication Date
- 2024-11-26
AI Technical Summary
The existing phase change memory preparation process is complex and costly, making it difficult to effectively control the size and contact area of the electrode, affecting the performance of the memory.
By selectively growing on the second metal layer, nanowires are formed as lower electrodes and wrapping the lower electrodes in the second dielectric layer, the through-hole width is controlled to determine the lower electrode width, avoiding the formation of smaller holes in multiple etching processes , simplify the process and reduce costs.
The process simplification and cost savings are achieved, while the electrode size and contact area are effectively controlled, improving the performance of the memory.
Smart Images

Figure CN119031825A_ABST
Abstract
Description
Technical Field
[0001] The present invention relates to the field of semiconductor technology, and in particular to a phase change memory and a preparation method thereof. Background Art
[0002] Phase change memory is a new type of non-volatile memory. It has great advantages over flash memory in terms of read and write speed, read and write times, data retention time, unit area, multi-value realization, etc., and has become the focus of current non-volatile memory technology research. Phase change memory uses the difference in conductivity of phase change materials when they transform between crystalline and amorphous states to store data.
[0003] In phase change memory, the commonly used phase change materials are mainly tellurium-based materials. Phase change materials are used to form a storage layer, which is directly connected to the lower electrode. In the existing preparation process, multiple photolithography processes are generally used to reduce the size of the hole, and then the hole is filled to form the lower electrode. Reducing the size of the hole indirectly means reducing the size of the lower electrode, and reducing the size of the lower electrode can reduce the contact area between the lower electrode and the storage layer, thereby reducing the phase change area of the memory. However, using multiple photolithography processes is complicated, or more advanced photolithography machines are required to prepare smaller holes, which has a high preparation cost. Summary of the invention
[0004] The object of the present invention is to provide a phase change memory and a preparation method thereof, which has a simple process and is easy to control, and can save preparation costs.
[0005] In order to achieve the above object, the present invention provides a method for preparing a phase change memory, comprising:
[0006] Providing a substrate, wherein a first dielectric layer is formed on the substrate, and a through hole is formed in the first dielectric layer extending longitudinally therethrough;
[0007] sequentially forming a first metal layer and a second metal layer to fill the through hole, wherein the second metal layer is located on the first metal layer;
[0008] Selectively growing nanowires on the second metal layer as a lower electrode;
[0009] forming a second dielectric layer on the first dielectric layer, wherein the second dielectric layer wraps the lower electrode, and a top surface of the second dielectric layer is higher than a top surface of the lower electrode; and,
[0010] A groove is formed in the second dielectric layer, the bottom of the groove exposes the lower electrode, and the groove is filled to form a storage layer.
[0011] Optionally, the step of sequentially forming a first metal layer and a second metal layer to fill the through hole includes:
[0012] Forming the first metal layer to fill up a portion of the height of the through hole;
[0013] The second metal layer is formed to fill the top of the through hole.
[0014] Optionally, the first metal layer includes tungsten, and the second metal layer includes copper or zinc.
[0015] Optionally, before the first metal layer and the second metal layer are formed in sequence and filled in the through hole, the method further includes forming a first barrier layer on the inner wall of the through hole.
[0016] Optionally, the material of the first barrier layer includes titanium or titanium nitride.
[0017] Optionally, before forming the second metal layer, a second barrier layer is formed on the inner wall of the remaining height of the through hole.
[0018] Optionally, the material of the second barrier layer includes tantalum or tantalum nitride.
[0019] Optionally, the lower electrode is formed by a CVD process, and a process gas of the CVD process chemically reacts with the second metal layer to grow and form the nanowire.
[0020] Optionally, the conductivity of the lower electrode is greater than 2770 S / M.
[0021] The present invention also provides a phase change memory, comprising:
[0022] A substrate, wherein a first dielectric layer is formed on the substrate, and a through hole is formed in the first dielectric layer extending longitudinally therethrough;
[0023] A first metal layer and a second metal layer are filled in the through hole, and the second metal layer is located on the first metal layer;
[0024] A lower electrode, located on the second metal layer;
[0025] A second dielectric layer, located on the first dielectric layer, the second dielectric layer wraps the lower electrode, and a top surface of the second dielectric layer is higher than a top surface of the lower electrode;
[0026] A storage layer is formed in the second dielectric layer, a groove is formed in the second dielectric layer, the bottom of the groove exposes the lower electrode, and the storage layer is filled in the groove.
[0027] In the phase change memory and its preparation method provided by the present invention, a substrate is provided, a first dielectric layer is formed on the substrate, a through hole is formed in the first dielectric layer which penetrates longitudinally; a first metal layer and a second metal layer are formed in sequence to fill in the through hole, the second metal layer is located on the first metal layer; a nanowire is selectively grown on the second metal layer as a lower electrode; a nanowire is formed as a lower electrode and is located on the second metal layer; a second dielectric layer is formed on the first dielectric layer, the second dielectric layer wraps the lower electrode, and the top surface of the second dielectric layer is higher than the top surface of the lower electrode; and a groove is formed in the second dielectric layer, the bottom of the groove exposes the lower electrode, and a storage layer is filled in the groove. In the present invention, nanowires are first grown on the second metal layer as the lower electrode, and then a second dielectric layer is formed to wrap the lower electrode, the width of the lower electrode is related to the width of the second metal layer, the width of the second metal layer is controlled by controlling the width of the through hole, and the width of the lower electrode is controlled, so as to avoid using multiple etching processes to form a smaller hole to form a lower electrode in the hole, and a more advanced photolithography machine is not required to prepare a smaller hole, the process is simple and easy to control, and the preparation cost can be saved. BRIEF DESCRIPTION OF THE DRAWINGS
[0028] Figure 1 A flow chart of a method for preparing a phase change memory provided by an embodiment of the present invention;
[0029] Figures 2A to 2H A schematic cross-sectional view of corresponding steps in a method for preparing a phase change memory provided by an embodiment of the present invention.
[0030] in, Figures 2A to 2H The accompanying drawings are:
[0031] 10 - substrate; 21 - first dielectric layer; 22 - second dielectric layer; 30 - through hole; 41 - first barrier layer; 42 - second barrier layer; 51 - first metal layer; 52 - second metal layer; 60 - lower electrode; 70 - groove; 80 - storage layer. DETAILED DESCRIPTION
[0032] In order to make the purpose, advantages and features of the present invention clearer, the present invention is further described in detail below in conjunction with the accompanying drawings and specific embodiments. It should be noted that the drawings are all in a very simplified form and are not drawn to scale, and are only used to conveniently and clearly assist in explaining the purpose of the embodiments of the present invention. In addition, the structure shown in the drawings is often a part of the actual structure. In particular, the emphasis of each drawing is different, and sometimes different scales are used.
[0033] As used in the present invention, the singular forms "one", "an", and "the" include plural objects, the term "or" is generally used to include the meaning of "and / or", the term "several" is generally used to include the meaning of "at least one", and the term "at least two" is generally used to include the meaning of "two or more". In addition, the terms "first", "second", and "third" are used for descriptive purposes only and cannot be understood as indicating or implying relative importance or implicitly indicating the number of technical features indicated. Therefore, the features defined as "first", "second", and "third" may explicitly or implicitly include one or at least two of the features, "one end" and "the other end" as well as "proximal end" and "distal end" generally refer to two corresponding parts, which include not only endpoints, and the terms "installed", "connected", and "connected" should be understood in a broad sense. In addition, as used in the present invention, an element disposed on another element generally only indicates that there is a connection, coupling, or cooperation relationship between the two elements, and the connection, coupling, or cooperation between the two elements may be direct or indirect through an intermediate element, and cannot be understood as indicating or implying a spatial position relationship between the two elements, that is, an element may be in any orientation such as inside, outside, above, below, or on one side of another element, unless otherwise clearly indicated in the content. For those of ordinary skill in the art, the specific meanings of the above terms in the present invention can be understood according to specific circumstances.
[0034] Figure 1 This is a flow chart of the method for preparing the phase change memory provided in this embodiment. Please refer to Figure 1 This embodiment provides a method for preparing a phase change memory, comprising:
[0035] Step S1: providing a substrate, on which a first dielectric layer is formed, and in which a through hole is formed that runs vertically through the first dielectric layer;
[0036] Step S2: forming a first metal layer and a second metal layer in sequence to fill the through hole, wherein the second metal layer is located on the first metal layer;
[0037] Step S3: selectively growing nanowires on the second metal layer as a lower electrode;
[0038] Step S4: forming a second dielectric layer on the first dielectric layer, wherein the second dielectric layer wraps the lower electrode, and a top surface of the second dielectric layer is higher than a top surface of the lower electrode;
[0039] Step S5: forming a groove in the second dielectric layer, with the bottom of the groove exposing the lower electrode, and filling the groove to form a storage layer.
[0040] Figures 2A to 2H The cross-sectional schematic diagram of the corresponding steps in the preparation method of the phase change memory provided in this embodiment is shown below in combination with Figures 2A to 2HThe preparation method of the phase change memory provided in this embodiment is described in detail.
[0041] Please refer to Figure 2A and 2B , performing step S1: providing a substrate 10, in which a plurality of device structures, such as CMOS device structures, are formed. A first dielectric layer 21 is formed on the substrate 10, in which a through hole 30 is formed that runs vertically through the first dielectric layer 21, and the bottom of the through hole 30 exposes the substrate 10. In this embodiment, the material of the first dielectric layer 21 includes silicon oxide or silicon nitride, but is not limited to the above materials.
[0042] Please refer to Figure 2C and 2D , perform step S2: before sequentially forming the first metal layer 51 and the second metal layer 52 to fill the through hole 30, a first barrier layer 41 is formed on the inner wall of the through hole 30 by using a PVD process (physical vapor deposition process). When forming the first barrier layer 41, the first barrier layer 41 will extend to cover the surface of the first dielectric layer 21 (not shown in the figure). In this embodiment, the material of the first barrier layer 41 includes titanium or titanium nitride, but is not limited to the above materials.
[0043] Then, the first metal layer 51 is formed to fill part of the height of the through hole 30, for example, the first metal layer 51 is filled to half the height of the through hole 30. When the first metal layer 51 is formed, the first metal layer 51 will extend to cover the surface of the first barrier layer 41 (not shown in the figure). The first metal layer and the first barrier layer on the surface of the first dielectric layer 21 are removed by dry etching to expose the surface of the first dielectric layer 21, and the first barrier layer 41 on the inner wall of the through hole 30 and the first metal layer 51 in the through hole 30 (such as Figure 2C ), since the through hole 30 has a large aspect ratio, when the dry etching process is used to vertically etch downward, the etching effect on the first barrier layer 41 and the first metal layer 51 in the through hole 30 is small, and the first barrier layer 41 on the inner wall of the through hole 30 and the first metal layer 51 in the through hole 30 can be retained. In this embodiment, the material of the first metal layer 51 includes tungsten, but is not limited to the above material.
[0044] After the first metal layer and the first barrier layer on the surface of the first dielectric layer 21 are removed by dry etching, before the second metal layer 52 is formed, a second barrier layer 42 is formed on the inner wall of the remaining height of the through hole 30 by PVD process (the second barrier layer 42 covers the top of the first metal layer 51 and part of the surface of the first barrier layer 41). When the second barrier layer 42 is formed, the second barrier layer 42 will extend to cover the surface of the first dielectric layer 21 (not shown in the figure). In this embodiment, the material of the second barrier layer 42 includes tantalum or tantalum nitride, but is not limited to the above materials.
[0045] Further, an ECP process (electrochemical plating process) is used to form a second metal layer 52 to fill the top of the through hole 30. When the second metal layer 52 is formed, the second metal layer 52 will extend to cover the surface of the second barrier layer 42 (not shown in the figure), and the second metal layer 52 also covers the top of the through hole 30 (not shown in the figure); then, a grinding process is used to grind and remove the second metal layer and the second barrier layer on the surface of the first dielectric layer 21 to expose the surface of the first dielectric layer 21. After grinding, the top of the second metal layer 52 is flush with the surface of the first dielectric layer 21. In this embodiment, the material of the second metal layer 52 includes copper or zinc, but is not limited to the above materials.
[0046] Please refer to Figure 2E , step S3 is performed: a CVD process (chemical vapor deposition process) is used to form a nanowire as the lower electrode 60. Since the materials of the first dielectric layer 21, the first barrier layer 41, the second barrier layer 42 and the second metal layer 52 are different, when the CVD process is used, the process gas provided by the CVD process is only for the second metal layer 52, and the process gas of the CVD process reacts chemically with the second metal layer 52 to grow on the second metal layer 52 to form a nanowire (lower electrode 60), wherein the process gas of the CVD process reacts chemically with the second metal layer 52, indicating that a small part of the metal ions in the second metal layer 52 are freed and react with the process gas of the CVD process to form a metal compound, and the metal compound grows in layers on the second metal layer 52 to form a nanowire, and the metal compounds are connected to each other, so that the nanowire is located on the second metal layer 52. In this embodiment, the conductivity of the lower electrode 60 is greater than 2770S / M to meet the electrical requirements of the phase change memory. In this embodiment, if the material of the second metal layer 52 is preferably copper, the process gas of the CVD process includes hydrogen sulfide and oxygen, and hydrogen sulfide and oxygen chemically react with copper to form cuprous sulfide. At this time, the material of the lower electrode 60 is cuprous sulfide, and the electrical conductivity of cuprous sulfide is 10400 S / M.
[0047] Please refer to Figure 2F , step S4 is performed: forming a second dielectric layer 22 on the first dielectric layer 21, the second dielectric layer 22 wraps the lower electrode 60, and the top surface of the second dielectric layer 22 is higher than the top surface of the lower electrode 60. In this embodiment, the material of the second dielectric layer 22 includes silicon oxide or silicon nitride, but is not limited to the above materials.
[0048] Please refer to Figure 2G and 2H , perform step S5: form a groove 70 in the second dielectric layer 22, the bottom of the groove 70 exposes the top of the lower electrode 60; then, fill the groove 70 to form a storage layer 80, the storage layer 80 is in contact with the lower electrode 60, and the contact area is a phase change area; in this embodiment, the material of the storage layer 80 includes Ge-Sb-Te phase change material, but is not limited to the above material.
[0049] In the prior art, multiple etching processes are used to form smaller holes and then form lower electrodes in the holes. The multiple etching processes are complicated and it is difficult to control the size of the holes, that is, it is difficult to control the size of the lower electrode, or a more advanced photolithography machine is required to prepare smaller holes, and the preparation cost is high. In the present embodiment, the lower electrode 60 is first grown on the second metal layer 52, and then the second dielectric layer 22 is formed to wrap the lower electrode 60, rather than first etching to form a through hole (hole) and then filling the through hole to form the lower electrode. The width of the lower electrode 60 is related to the width of the second metal layer 22. The width of the second metal layer 52 can be controlled by controlling the width of the through hole 30, so as to control the width of the lower electrode 60. The process is simple and easy to control, and the preparation cost can be saved.
[0050] Further, after the storage layer is formed by filling the groove, an upper electrode is formed on the storage layer, and the upper electrode contacts the storage layer.
[0051] Figure 2H is a cross-sectional schematic diagram of corresponding steps in the method for preparing the phase change memory provided in this embodiment, Figure 2H This is also a cross-sectional schematic diagram of the phase change memory provided in this embodiment. Figure 2H This embodiment further provides a phase change memory, including: a substrate 10, a first dielectric layer 21, a second dielectric layer 22, a first metal layer 51, a second metal layer 52, a lower electrode 60 and a storage layer 80. The first dielectric layer 21 is formed on the substrate 10, a through hole 30 is formed in the first dielectric layer 21 and runs vertically through the first dielectric layer 21, the bottom of the through hole 30 exposes the substrate 10, and the material of the first dielectric layer 21 includes silicon oxide or silicon nitride, but is not limited to the above materials.
[0052] A first barrier layer 41 is formed on the inner wall of the through hole 30. The material of the first barrier layer 41 includes titanium or titanium nitride, but is not limited to the above materials. The first metal layer 51 fills part of the height of the through hole 30. The material of the first metal layer 51 includes tungsten, but is not limited to the above materials. A second barrier layer 42 is formed on the inner wall of the remaining height of the through hole 30 (the second barrier layer 42 covers the top of the first metal layer 51 and part of the surface of the first barrier layer 41). The material of the second barrier layer 42 includes tantalum or tantalum nitride, but is not limited to the above materials. The second metal layer 52 fills the top of the through hole 30. The second metal layer 52 is located on the first metal layer 51. The material of the second metal layer 52 includes copper or zinc, but is not limited to the above materials.
[0053] The lower electrode 60 is located on the second metal layer 52. The material of the lower electrode 60 is related to the material of the second metal layer 52. Some metal ions in the second metal layer 52 are freed and react with the process gas of the CVD process to form a metal compound (lower electrode 60). The conductivity of the lower electrode 60 is greater than 2770S / M to meet the electrical requirements of the phase change memory. In this embodiment, if the material of the second metal layer 52 is preferably copper, the process gas of the CVD process includes hydrogen sulfide and oxygen, and hydrogen sulfide and oxygen chemically react with copper to form cuprous sulfide. At this time, the material of the lower electrode 60 is cuprous sulfide, and the conductivity of cuprous sulfide is 10400S / M.
[0054] The second dielectric layer 22 is located on the first dielectric layer 21 , and the second dielectric layer 22 wraps the lower electrode 60 . The top surface of the second dielectric layer 22 is higher than the top surface of the lower electrode 60 . The material of the second dielectric layer 22 includes silicon oxide or silicon nitride, but is not limited to the above materials.
[0055] A groove 70 is formed in the second dielectric layer 22, and the bottom of the groove 70 exposes the top of the lower electrode 60; the storage layer 80 is filled in the groove 70, and the storage layer 80 contacts the lower electrode 60, and the contact area is a phase change area. The material of the storage layer 80 includes Ge-Sb-Te phase change material, but is not limited to the above materials. An upper electrode (not shown in the figure) is also formed on the storage layer 80, and the upper electrode contacts the storage layer 80.
[0056] In summary, in the phase change memory and its preparation method provided by the present invention, a substrate is provided, a first dielectric layer is formed on the substrate, and a through hole is formed in the first dielectric layer that penetrates longitudinally; a first metal layer and a second metal layer are formed in sequence to fill in the through hole, and the second metal layer is located on the first metal layer; a nanowire is selectively grown on the second metal layer as a lower electrode; a nanowire is formed as a lower electrode and is located on the second metal layer; a second dielectric layer is formed and is located on the first dielectric layer, the second dielectric layer wraps the lower electrode, and the top surface of the second dielectric layer is higher than the top surface of the lower electrode; and a groove is formed in the second dielectric layer, the bottom of the groove exposes the lower electrode, and a storage layer is filled in the groove. In the present invention, nanowires are first grown on the second metal layer as the lower electrode, and then a second dielectric layer is formed to wrap the lower electrode. The width of the lower electrode is related to the width of the second metal layer. The width of the second metal layer is controlled by controlling the width of the through hole, so as to control the width of the lower electrode, avoid using multiple etching processes to form a smaller hole to form a lower electrode in the hole, and do not need a more advanced photolithography machine to prepare a smaller hole. The process is simple and easy to control, which can save preparation costs.
[0057] The above is only a preferred embodiment of the present invention and does not limit the present invention in any way. Any technician in the relevant technical field, without departing from the scope of the technical solution of the present invention, makes any form of equivalent replacement or modification to the technical solution and technical content disclosed in the present invention, which does not depart from the content of the technical solution of the present invention and still falls within the protection scope of the present invention.
Claims
1. A method for preparing a phase change memory, It is characterized in that include: Providing a substrate, wherein a first dielectric layer is formed on the substrate, and a through hole is formed in the first dielectric layer extending longitudinally therethrough; sequentially forming a first metal layer and a second metal layer to fill the through hole, wherein the second metal layer is located on the first metal layer; Selectively growing nanowires on the second metal layer as a lower electrode; forming a second dielectric layer on the first dielectric layer, wherein the second dielectric layer wraps the lower electrode, and a top surface of the second dielectric layer is higher than a top surface of the lower electrode; and, A groove is formed in the second dielectric layer, the bottom of the groove exposes the lower electrode, and the groove is filled to form a storage layer.
2. The method for preparing a phase change memory according to claim 1, It is characterized in that The steps of sequentially forming a first metal layer and a second metal layer to fill the through hole include: Forming the first metal layer to fill up a portion of the height of the through hole; The second metal layer is formed to fill the top of the through hole.
3. The method for preparing a phase change memory according to claim 1, It is characterized in that The first metal layer includes tungsten, and the second metal layer includes copper or zinc.
4. The method for preparing a phase change memory according to claim 1, It is characterized in that Before the first metal layer and the second metal layer are sequentially formed and filled in the through hole, the method further includes forming a first barrier layer on the inner wall of the through hole.
5. The method for preparing a phase change memory according to claim 4, It is characterized in that The material of the first barrier layer includes titanium or titanium nitride.
6. The method for preparing a phase change memory according to claim 2, It is characterized in that Before forming the second metal layer, a second barrier layer is formed on the inner wall of the remaining height of the through hole.
7. The method for preparing a phase change memory according to claim 6, It is characterized in that The material of the second barrier layer includes tantalum or tantalum nitride.
8. The method for preparing a phase change memory according to claim 1, It is characterized in that The lower electrode is formed by a CVD process, and a process gas of the CVD process chemically reacts with the second metal layer to grow and form the nanowire.
9. The method for preparing a phase change memory according to claim 1, It is characterized in that The electrical conductivity of the lower electrode is greater than 2770 S / M.
10. A phase change memory, It is characterized in that include: A substrate, wherein a first dielectric layer is formed on the substrate, and a through hole is formed in the first dielectric layer extending longitudinally therethrough; A first metal layer and a second metal layer are filled in the through hole, and the second metal layer is located on the first metal layer; A lower electrode, located on the second metal layer; A second dielectric layer is located on the first dielectric layer, the second dielectric layer wraps the lower electrode, and a top surface of the second dielectric layer is higher than a top surface of the lower electrode; A storage layer is formed in the second dielectric layer, a groove is formed in the second dielectric layer, the bottom of the groove exposes the lower electrode, and the storage layer is filled in the groove.