Shape memory hydrogel biological material as well as preparation method and application thereof

Through the design of multi-layer shape memory hydrogel biological materials, the problem of poor binding of implanted materials to human tissues in the treatment of lumbar disc herniation is solved, and good combination with fibrous annulus and rapid recovery of patients is achieved, reducing the pain of patients .

CN119034014AActive Publication Date: 2024-11-29HARBIN INST OF TECH
View PDF 7 Cites 0 Cited by

Patent Information

Application Number
CN202411193250.1
Authority / Receiving Office
CN · China
Patent Type
Applications(China)
Current Assignee / Owner
Filing Date
2024-08-28
Publication Date
2024-11-29
Estimated Expiration
2044-08-28

AI Technical Summary

Technical Problem

Existing treatment methods for lumbar disc herniation, such as discectomy and artificial nucleus pulposus replacement, have palliative and high complications, and the implanted materials cannot effectively meet the biomechanical needs of human tissues, resulting in abnormal fibrous annulus bulging inward and Poor fit.

Method used

Using multi-layer shape memory hydrogel biomaterials, the elastic modulus of changing gradient along the vertical direction is combined with graft monomers, shape memory materials, and light Initiators, antibacterial agents and natural polymer materials are prepared by cross-linking reactions to form materials with shape memory properties for nucleus pulposus replacement.

Benefits of technology

This material can regulate cell growth, meet the needs of human biomechanical, achieve good combination with surrounding tissues, promote patient recovery, and achieve minimally invasive implantation through shape memory performance, reducing patient pain.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure CN119034014A_ABST
    Figure CN119034014A_ABST
Patent Text Reader

Abstract

The invention provides shape memory hydrogel as well as a preparation method and application thereof. The hydrogel biological material comprises shape memory hydrogel layers and adhesive hydrogel layers which are sequentially and alternately arranged in the vertical direction, wherein the number of the shape memory hydrogel layers is larger than that of the adhesion hydrogel layers, and the elasticity moduli of the shape memory hydrogel layers are different from one another; the shape memory hydrogel comprises a temporary shape and an initial shape, the size of the temporary shape is smaller than that of the initial shape, and the shape memory hydrogel can be converted into the initial shape from the temporary shape under the action of external stimulation. The shape memory hydrogel disclosed by the invention can well meet the biomechanical requirements of human tissues and organs, and can be well combined with a surrounding tissue structure to promote rapid recovery of an affected part.
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] The invention relates to the technical field of hydrogels, and in particular to a shape memory hydrogel biomaterial and a preparation method and application thereof. Background Art

[0002] Lumbar disc herniation (LDH) is a disease characterized by low back pain and a series of radicular symptoms, caused by degeneration of the lumbar disc and external force damage, which causes partial rupture of the annulus fibrosus. The nucleus pulposus bulges outward from the defect in the annulus fibrosus and compresses the spinal nerve roots or cauda equina.

[0003] Currently, the main treatments for lumbar disc herniation are discectomy and artificial nucleus pulposus replacement. However, discectomy and fusion are palliative in nature and may not restore the baseline motion and mechanical load characteristics of adult intervertebral discs. In addition, the complication rate of artificial nucleus pulposus replacement is very high, which is caused by extrusion or displacement due to poor integration of the implant with the surrounding structure. At the same time, the current implant materials cannot meet the biomechanical requirements of human tissues and organs well, so it is impossible to ensure that the nucleus pulposus replacement materials can inhibit the abnormal inward bulging of the annulus fibrosus after the removal of the nucleus pulposus and fit the biomechanical properties of the native tissue.

[0004] Therefore, based on the above problems, there is an urgent need to provide a shape memory hydrogel biomaterial and a preparation method and application thereof. Summary of the invention

[0005] The embodiment of the present invention provides a shape memory hydrogel biomaterial and a preparation method and application thereof. The shape memory hydrogel can well meet the biomechanical requirements of human tissues and organs, and can be well integrated with surrounding tissue structures to promote rapid recovery of the diseased area.

[0006] In a first aspect, the present invention provides a shape memory hydrogel, wherein the hydrogel biomaterial comprises shape memory hydrogel layers and adhesion hydrogel layers alternately arranged from top to bottom; wherein the number of the shape memory hydrogel layers is greater than the number of the adhesion hydrogel layers, and the elastic modulus of each shape memory hydrogel layer is different from each other;

[0007] The shape memory hydrogel comprises a temporary shape and an initial shape, the size of the temporary shape is smaller than the size of the initial shape, and the shape memory hydrogel can be transformed from the temporary shape to the initial shape under external stimulation.

[0008] Preferably, the number of the shape memory hydrogel layers is at least three; and the elastic modulus of each shape memory hydrogel layer changes gradually in the vertical direction.

[0009] Preferably, the change in elastic modulus between two adjacent shape memory gel layers is 50-100 KPa.

[0010] Preferably, each shape memory gel layer is prepared by a cross-linking reaction using a grafting monomer, a shape memory material, a photoinitiator, an antibacterial agent and water as reaction raw materials.

[0011] More preferably, the shape memory material is gelatin, the photoinitiator is 2-hydroxy-2-methyl-1-[4-(2-hydroxyethoxy)phenyl]-1-propanone or phenylbis(2,4,6-trimethylbenzoyl)phosphine oxide, and the antibacterial agent is tannic acid or silver nanoparticles.

[0012] Preferably, in parts by weight, the contents of the various reaction raw materials in the preparation process of the shape memory gel layer are as follows: 10-50 parts of grafting monomer, 10-20 parts of shape memory material, 0.1-0.5 parts of photoinitiator, 5-10 parts of antibacterial agent, and 50-100 parts of water.

[0013] Preferably, the adhesive gel layer is prepared by cross-linking reaction using natural polymer materials, grafting monomers, thermal initiators and water as reaction raw materials.

[0014] More preferably, the natural polymer material is hyaluronic acid, and the thermal initiator is ammonium persulfate or sodium persulfate.

[0015] More preferably, the grafting monomer is prepared by reacting glycineamide hydrochloride, potassium carbonate, an organic solvent and acryloyl chloride.

[0016] Preferably, the contents of the reaction raw materials in the preparation process of the adhesive gel layer are as follows, in parts by weight: 5-10 parts of natural polymer material, 1-5 parts of grafting monomer, 0.1-1 parts of thermal initiator, and 100-150 parts of water.

[0017] In a second aspect, the present invention provides a method for preparing the shape memory hydrogel biomaterial as described in any one of the first aspects above, the preparation method comprising the following steps:

[0018] (1) adding grafted monomers, shape memory materials, photoinitiators and antibacterial agents to water in different proportions and stirring to react, thereby obtaining shape memory gel layers with different elastic moduli; wherein the content of grafted monomers in each shape memory gel layer is different;

[0019] (2) adding the natural polymer material, the grafting monomer and the thermal initiator into water and stirring the reaction to obtain an adhesive gel layer;

[0020] (3) Alternately placing the shape memory gel layer and the adhesion gel layer in a mold for compounding to obtain the shape memory hydrogel biomaterial.

[0021] Preferably, in step (1), the reaction is carried out under ultraviolet light conditions, and the illumination time is 30-60 minutes.

[0022] Preferably, in step (2), the reaction temperature is 50-60°C and the reaction time is 30-60 min.

[0023] In a third aspect, the present invention further provides a use of the shape memory hydrogel biomaterial described in any one of the first aspect or the shape memory hydrogel biomaterial prepared by any preparation method described in the second aspect as a nucleus pulposus replacement material.

[0024] Compared with the prior art, the present invention has at least the following beneficial effects:

[0025] In the present invention, a multi-layer shape memory hydrogel layer structure is prepared, and two adjacent shape memory hydrogel layers are bonded by an adhesive hydrogel layer, and the elastic modulus of each shape memory gel layer in the vertical direction is different, so that the shape memory hydrogel biomaterial has different responses to different cells in the annulus fibrosus, thereby regulating the growth of cells so that it meets the needs of human biomechanics and is well combined with the surrounding tissues of the human body to promote the recovery of the diseased part. At the same time, the hydrogel biomaterial prepared in the present invention has shape memory properties. During use, the prepared shape memory hydrogel is regulated from the initial shape to a temporary shape that is easy to implant. After implantation, external stimulation is applied to restore it to the initial shape, thereby achieving a minimally invasive effect and alleviating the pain of the patient. BRIEF DESCRIPTION OF THE DRAWINGS

[0026] In order to more clearly illustrate the embodiments of the present invention or the technical solutions in the prior art, the drawings required for use in the embodiments or the description of the prior art will be briefly introduced below. Obviously, the drawings described below are some embodiments of the present invention. For ordinary technicians in this field, other drawings can be obtained based on these drawings without paying creative work.

[0027] Figure 1 is a schematic structural diagram of a shape memory hydrogel biomaterial provided by one embodiment of the present invention;

[0028] Figure 2 is a schematic diagram of the initial shape of a shape memory hydrogel biomaterial provided by one embodiment of the present invention;

[0029] Figure 3 It is a schematic diagram of a mold structure used in a process of preparing a shape memory hydrogel biomaterial provided by an embodiment of the present invention;

[0030] Figure 4This is a schematic diagram of the structure of a shape memory hydrogel biomaterial that changes from an initial shape to a temporary shape provided by one embodiment of the present invention;

[0031] Figure 5 This is a schematic structural diagram of a shape memory hydrogel biomaterial provided by one embodiment of the present invention, which is used as a nucleus pulposus replacement material after being implanted into a lumbar shoulder disc; in the figure, 100 is a shape memory hydrogel layer, and 200 is an adhesion gel layer. DETAILED DESCRIPTION

[0032] In order to make the purpose, technical solutions and advantages of the embodiments of the present invention clearer, the technical solutions in the embodiments of the present invention will be clearly and completely described below in conjunction with the drawings in the embodiments of the present invention. Obviously, the described embodiments are part of the embodiments of the present invention, rather than all the embodiments. Based on the embodiments in the present invention, all other embodiments obtained by ordinary technicians in this field without making creative work are within the scope of protection of the present invention.

[0033] like Figure 1 and Figure 4 As shown, the present invention provides a shape memory hydrogel biomaterial, which includes shape memory hydrogel layers 100 and adhesion hydrogel layers 200 alternately arranged in a vertical direction; wherein the number of the shape memory hydrogel layers is greater than the number of the adhesion hydrogel layers, and the elastic modulus of each shape memory hydrogel layer is different; the shape memory hydrogel includes a temporary shape and an initial shape, the size of the temporary shape is smaller than the size of the initial shape, and the shape memory hydrogel can be transformed from the temporary shape to the initial shape under external stimulation.

[0034] In the embodiment of the present invention, a multi-layer shape memory hydrogel layer structure is prepared, and two adjacent shape memory hydrogel layers are bonded by an adhesive hydrogel layer, and the elastic modulus of each shape memory gel layer in the vertical direction is different, so that the shape memory hydrogel biomaterial has different responses to different cells in the annulus fibrosus, thereby regulating the growth of cells so that it meets the needs of human biomechanics and is well combined with the surrounding tissues of the human body to promote the recovery of the diseased part. At the same time, the hydrogel biomaterial prepared in the present invention has shape memory properties. During use, the prepared shape memory hydrogel is regulated from the initial shape to a temporary shape that is easy to implant. After implantation, external stimulation is applied to restore it to the initial shape, thereby achieving a minimally invasive effect and reducing the pain of the patient.

[0035] According to some preferred embodiments, the number of the shape memory hydrogel layers is at least three; and the elastic modulus of each shape memory hydrogel layer changes gradually in the vertical direction.

[0036] Taking into account the large differences between the artificial nucleus pulposus materials in the related art and human tissues and organs, the artificial nucleus pulposus materials cannot meet the biomechanical needs of human tissues and organs after implantation into the human body, and are poorly integrated with the tissue structure around the human annulus fibrosus, which is not conducive to the recovery of the diseased part. The inventors have found through research that the main reason for the above-mentioned problem is that the annulus fibrosus and the nucleus pulposus in the intervertebral disc have different biomechanical properties, and the annulus fibrosus is highly heterogeneous in terms of cell phenotype, biomechanics, biochemistry and microstructure, and has typical gradient characteristics along the radial direction. Therefore, in the embodiment of the present invention, the shape memory hydrogel biomaterial that can be used as a nucleus pulposus substitute material is designed as a multilayer structure in combination with the above reasons, and the elastic modulus of each shape memory gel layer changes gradiently in the vertical direction in sequence. In this way, the cells in different gradient layers of the annulus fibrosus respond to the physical signal gradient in the shape memory hydrogel biomaterial and migrate along the direction of the signal change, so that it can meet the needs of human biomechanics to regulate cell growth and better achieve the purpose of good integration with the surrounding tissues of the human body to promote the recovery of the diseased part.

[0037] It should be noted that the number of shape memory gel layers in the embodiment of the present invention can be specifically 3-25 layers. At the same time, the overall thickness of the shape memory hydrogel biomaterial can be determined according to the thickness of the fiber ring during actual application, and the thickness of each shape memory gel layer is the same.

[0038] According to some preferred embodiments, the variation in elastic modulus of two adjacent shape memory gel layers is 50-100 KPa (for example, it may be 50 KPa, 60 KPa, 70 KPa, 80 KPa, 90 KPa or 100 KPa).

[0039] In the embodiment of the present invention, by further controlling the change in the elastic modulus of two adjacent shape memory gel layers, it is beneficial to better achieve controllable growth of cells, thereby facilitating better integration of cells with surrounding tissues of the human body to achieve better therapeutic effects.

[0040] According to some preferred embodiments, each shape memory gel layer is prepared by a cross-linking reaction using a grafted monomer, a shape memory material, a photoinitiator, an antibacterial agent and water as reaction raw materials; the shape memory material is gelatin, the photoinitiator is 2-hydroxy-2-methyl-1-[4-(2-hydroxyethoxy)phenyl]-1-propanone or phenylbis(2,4,6-trimethylbenzoyl)phosphine oxide, and the antibacterial agent is tannic acid or silver nanoparticles.

[0041] In an embodiment of the present invention, in the process of preparing the shape memory gel layer, a grafted monomer is first obtained by self-production, and the grafted monomer has good mechanical properties and biocompatibility. Then, it is grafted and cross-linked with a shape memory material having good biocompatibility and shape memory properties under the action of a photoinitiator, thereby obtaining a shape memory gel layer having excellent mechanical properties and shape memory properties. At the same time, a certain amount of antibacterial agent is also added in the process of preparing the shape memory gel layer, which can give the shape memory gel layer good antibacterial properties, thereby effectively avoiding the problem of bacterial growth during postoperative recovery.

[0042] According to some preferred embodiments, the grafted monomer is prepared by reacting glycineamide hydrochloride, potassium carbonate, an organic solvent and acryloyl chloride; the preparation method of the grafted monomer is as follows: glycineamide hydrochloride, potassium carbonate and an organic solvent are added to water and mixed to obtain a mixed solution; acryloyl chloride dissolved in an organic solvent is added dropwise to the mixed solution and mixed to obtain a reaction product after reaction; the reaction product is sequentially pH adjusted, extracted, freeze-dried, dissolved and rotary evaporated to obtain the grafted monomer; wherein the organic solvent is ether.

[0043] According to some preferred embodiments, in the mixed solution, the mass ratio of glycinamide hydrochloride and potassium carbonate is (6-7):(9-10), the volume ratio of the organic solvent and water is 3:1; the mass volume ratio of acryloyl chloride and the organic solvent is (5-6) g:(20-30) mL.

[0044] In the embodiment of the present invention, the above raw materials are used and reacted by controlling their contents, thereby preparing a grafted monomer with excellent mechanical properties, which is grafted and cross-linked with a shape memory material to obtain a shape memory hydrogel biomaterial with the ability to regulate cell growth.

[0045] It should be noted that, in the embodiment of the present invention, the above-mentioned mixing process is carried out under ice water bath conditions, and the reaction temperature of glycinamide hydrochloride and acryloyl chloride is 20-30°C, and the reaction time is 4-5h. Further, after obtaining the reaction product, the pH value of the reaction product solution can be adjusted to 2.0 using a 6mol / L HCl solution, and ether is used as an extractant to extract and remove the organic phase in the reaction solution, and then, a mixed solvent (methanol and ethanol in a volume ratio of 4:1) is further used to wash and remove inorganic salts in the reaction product, and finally, the solution is rotary evaporated at 40°C, and the precipitate is placed in a vacuum drying oven to dry, thereby obtaining a powdered grafting monomer.

[0046] According to some preferred embodiments, the content of each reaction raw material in the preparation process of the shape memory gel layer is as follows, in parts by weight: 10-50 parts of grafting monomer (for example, 10 parts, 20 parts, 30 parts, 40 parts or 50 parts), 10-20 parts of shape memory material (for example, 10 parts, 12 parts, 14 parts, 16 parts, 18 parts or 20 parts), 0.1-0.5 parts of photoinitiator (for example, 0.1 parts, 0.2 parts, 0.3 parts, 0.4 parts or 0.5 parts), 5-10 parts of antibacterial agent (for example, 5 parts, 6 parts, 7 parts, 8 parts, 9 parts or 10 parts), and 50-100 parts of water (for example, 50 parts, 60 parts, 70 parts, 80 parts, 90 parts or 100 parts).

[0047] In the embodiment of the present invention, by controlling the content of the above-mentioned reaction raw materials, it is beneficial to prepare a shape memory gel layer with excellent mechanical properties and shape memory shape. It is confirmed by the experiment of the present invention that by adjusting the content of the grafted monomer and the shape memory material in each layer of the shape memory gel layer, the elastic modulus of each layer of the shape memory gel layer can be controlled. Under the condition of the same content of shape memory material, as the content of the grafted monomer increases, the elastic modulus of the shape memory gel layer also increases. However, when the content of the grafted monomer is too high, it is not only not conducive to improving the elastic modulus of the shape memory gel layer, but also reduces the shape memory performance of the shape memory gel layer. At the same time, it is confirmed by the experiment of the present invention that the content of the antibacterial agent is positively correlated with the antibacterial performance of the shape memory gel layer, but if the content of the antibacterial agent is too much, it is not only not conducive to significantly enhancing the antibacterial performance of the shape memory gel layer, but also causes waste of the antibacterial agent.

[0048] According to some preferred embodiments, the adhesive gel layer is prepared by a cross-linking reaction using natural polymer materials, grafting monomers, thermal initiators and water as reaction raw materials; the natural polymer material is hyaluronic acid, and the thermal initiator is ammonium persulfate or sodium persulfate.

[0049] In the embodiment of the present invention, the adhesive gel layer is prepared by using natural polymer materials and grafted monomers as reaction raw materials. The above-mentioned types of natural polymer materials are naturally degradable and have good compatibility with the human body, and can better adjust the adhesion properties of the adhesive gel layer. The grafted monomers can not only form hydrogen bonds with the natural polymer materials and water, thereby further enhancing the adhesion properties of the adhesive gel layer, but also the grafted monomers can give the adhesive gel layer better mechanical properties. At the same time, the use of the same grafted monomers in the adhesive gel layer as those in the shape memory gel layer is conducive to maximizing the guarantee of good bonding performance of the two adjacent shape memory gel layers.

[0050] According to some preferred embodiments, the contents of the reaction raw materials in the preparation process of the adhesive gel layer are as follows, in parts by weight: 5-10 parts of natural polymer material (for example, 5 parts, 6 parts, 7 parts, 8 parts, 9 parts or 10 parts), 1-5 parts of grafting monomer (for example, 1 part, 2 parts, 3 parts, 4 parts or 5 parts), 0.1-1 part of thermal initiator (for example, 0.1 part, 0.2 parts, 0.4 parts, 0.5 parts, 0.8 parts or 1 part), and 100-150 parts of water (for example, 100 parts, 110 parts, 120 parts, 130 parts, 140 parts or 150 parts).

[0051] In the embodiment of the present invention, by using an appropriate ratio of natural polymer materials and grafted monomers to initiate grafting crosslinking via a thermal initiator, it is beneficial to prepare an adhesive gel layer with excellent adhesion and mechanical properties, which is beneficial to ensure the integrity of the shape memory hydrogel biomaterial; if the content of the natural polymer material or the grafted monomer is too high or too low, it is not conducive to ensuring the good adhesion and mechanical properties of the adhesive gel layer.

[0052] The embodiment of the present invention further provides a method for preparing the shape memory hydrogel biomaterial as described in any one of the above items, the preparation method comprising the following steps:

[0053] (1) adding grafted monomers, shape memory materials, photoinitiators and antibacterial agents to water in different proportions and stirring to react, thereby obtaining shape memory gel layers with different elastic moduli; wherein the content of grafted monomers in each shape memory gel layer is different;

[0054] (2) adding the natural polymer material, the grafting monomer and the thermal initiator into water and stirring the reaction to obtain an adhesive gel layer;

[0055] (3) Alternately placing the shape memory gel layer and the adhesion gel layer in a mold for compounding to obtain the shape memory hydrogel biomaterial.

[0056] In the embodiment of the present invention, the shape memory hydrogel biomaterial includes an initial shape and a temporary shape. The initial shape and the temporary shape have the same structure but different sizes. In the embodiment of the present invention, there is no particular restriction on the initial shape and the temporary shape of the shape memory hydrogel biomaterial. Specifically, the shape memory hydrogel biomaterial can be prepared into different shapes (such as Figure 2 or Figure 4 shown).

[0057] It should be noted that, in order to ensure good antibacterial properties of the shape memory gel layer, different types of antibacterial agents are used, and different methods for preparing the shape memory gel layer are used in the embodiments of the present invention. Specifically, when the antibacterial agent is tannic acid, the grafted monomer, shape memory material and photoinitiator are added to water to react, and the gel obtained is immersed in an aqueous solution of the antibacterial agent to obtain a shape memory gel layer with antibacterial properties; when the antibacterial agent is silver nanoparticles, the grafted monomer, shape memory material, antibacterial agent and photoinitiator are added to water to react, thereby obtaining a shape memory gel layer with antibacterial properties.

[0058] At the same time, in order to ensure that the two adjacent shape memory gel layers have a good connection effect, in an embodiment of the present invention, when preparing a shape memory hydrogel biomaterial, the grafted monomer and the shape memory material, the photoinitiator and the antibacterial agent can be first added to water in different proportions and stirred to obtain a gel precursor solution with different elastic moduli, and the natural polymer material, the grafted monomer and the thermal initiator are added to the water and stirred to obtain an adhesion gel precursor solution; then, the gel precursor solution is poured into the mold in sequence and then light-cured to obtain a shape memory gel layer, and then the adhesion gel precursor solution is poured on the surface of the shape memory gel layer, and heated and cured to obtain an adhesion hydrogel layer, and this cycle is repeated until a shape memory gel layer is obtained.

[0059] According to some preferred embodiments, in step (1), the reaction is carried out under ultraviolet illumination, and the illumination time is 30-60 min (for example, it can be 30 min, 40 min, 50 min or 60 min); in step (2), the reaction temperature is 50-60°C (for example, it can be 50°C, 55°C or 60°C), and the reaction time is 30-60 min (for example, it can be 30 min, 40 min, 50 min or 60 min).

[0060] For example, using Figure 3 When a rectangular shape memory hydrogel biomaterial is prepared using a mold in the invention, a hydrogel precursor solution formed by a grafted monomer, a shape memory material, a photoinitiator, an antibacterial agent and water is first added to the mold, and then it is reacted and cured by ultraviolet light of 365 nm to obtain a shape memory gel layer; then an adhesion hydrogel precursor solution formed by a natural polymer material, a grafted monomer, a thermal initiator and water is added to the surface of the mold, and it is reacted and cured after heating to obtain an adhesion gel layer; then a hydrogel precursor solution formed by a grafted monomer, a shape memory material, a photoinitiator, an antibacterial agent and water in different proportions is placed on the surface of the adhesion hydrogel layer, and this cycle is repeated to prepare an integrated rectangular shape memory hydrogel biomaterial.

[0061] An embodiment of the present invention further provides a use of the shape memory hydrogel biomaterial described in any one of the above items as a nucleus pulposus replacement material.

[0062] In the embodiment of the present invention, when the shape memory hydrogel biomaterial is used as a nucleus pulposus replacement material to treat lumbar shoulder disc herniation, the specific method of use is as follows: the prepared shape memory hydrogel biomaterial is heated to above the glass transition temperature. Considering the comfort and tolerance of the human body, the glass transition temperature of the hydrogel biomaterial in the embodiment of the present invention is 40 degrees; and an external force is applied to it to transform it into a temporary shape with a smaller size (which can be as follows Figure 4 As shown in the figure, it is then placed at room temperature for fixation to obtain a temporary shape of the shape memory hydrogel biomaterial; thereafter, it is placed in the defect of the intervertebral disc, and external stimulation is applied again (for example, a certain amount of hot water can be added) to restore it to its larger initial shape. Thereafter, the shape memory hydrogel biomaterial can regulate the growth and proliferation of surrounding tissue cells, thereby tightly integrating with the surrounding tissue structure, thereby promoting healing faster.

[0063] In the embodiment of the present invention, the shape memory hydrogel biomaterial in the embodiment of the present invention has directionality. The inventors further considered that the composition of vascular adventitial fibroblasts is different, the inner region is mainly composed of type II collagen and proteoglycan PGs, and the outer region mainly contains type I collagen. Different types of collagen in bone marrow mesenchymal stem cells have different expression rates on materials with different mechanical properties. Therefore, when using the shape memory hydrogel biomaterial prepared as above as a nucleus pulposus substitute material to treat lumbar disc herniation, Figure 5 As shown, in the embodiment of the present invention, the end with a lower elastic modulus in the shape memory hydrogel biomaterial can be controlled to contact the outer cells of the annulus fibrosus, and the end with a higher elastic modulus can contact the inner cells of the annulus fibrosus. This is conducive to guiding the growth of cells in different areas of the annulus fibrosus and making them tightly combined with the shape memory hydrogel biomaterial, thereby achieving effective blocking of the defects in the annulus fibrosus and promoting disease recovery.

[0064] In order to more clearly illustrate the technical solution and advantages of the present invention, a shape memory hydrogel and a preparation method thereof are described in detail below through several embodiments.

[0065] In the following examples, the masses of the grafting monomer, shape memory material, photoinitiator, antibacterial agent, natural polymer material, thermal initiator and water are expressed in parts by weight;

[0066] In the following examples, the grafted monomers were prepared by the following method:

[0067] Under ice-water bath conditions, 6.3 g of glycineamide hydrochloride, 9.27 g of potassium carbonate and 18 mL of organic solvent (ether) were added to 6 mL of deionized water and mixed to obtain a mixed solution; 5.7 g of acryloyl chloride was dissolved in 24 mL of organic solvent (ether), and then added dropwise to the mixed solution and mixed. After reacting at room temperature of 25°C for 5 hours to obtain a reaction product, the pH of the reaction product solution was adjusted to 2.0 with a hydrochloric acid solution, and the solution after the pH adjustment was extracted three times with 150 mL of ether to remove the organic phase, and the pH of the remaining solution was adjusted to neutral with sodium hydroxide, and the solution was washed with 150 mL of a mixed solvent (ethanol and methanol in a volume ratio of 4:1), and finally, it was recrystallized after rotary evaporation at 40°C, and the precipitate was dried to obtain a grafted monomer powder.

[0068] Embodiment 1:

[0069] (1) adding 10 parts of grafting monomer, 10 parts of shape memory material (gelatin), and 0.1 parts of photoinitiator (2-hydroxy-2-methyl-1-[4-(2-hydroxyethoxy)phenyl]-1-propanone) to 50 parts of deionized water, and stirring to obtain a first hydrogel precursor solution; adding 30 parts of grafting monomer, 10 parts of shape memory material (gelatin), and 0.3 parts of photoinitiator (2-hydroxy-2-methyl-1-[4-(2-hydroxyethoxy)phenyl]-1-propanone) to 80 parts of deionized water, and stirring to obtain a second hydrogel precursor solution; adding 50 parts of grafting monomer, 10 parts of shape memory material (gelatin), and 0.5 parts of photoinitiator (2-hydroxy-2-methyl-1-[4-(2-hydroxyethoxy)phenyl]-1-propanone) to 100 parts of deionized water, and stirring to obtain a third hydrogel precursor solution;

[0070] (2) adding 8 parts of natural polymer material (hyaluronic acid), 3 parts of grafting monomer and 0.5 parts of thermal initiator (ammonium sulfate) into 120 parts of deionized water, stirring and mixing to obtain an adhesive hydrogel precursor solution;

[0071] (3) placing the first hydrogel precursor liquid in a cylindrical mold, irradiating it with 365nm ultraviolet light for 30min and then curing it to obtain a first shape memory gel layer; then pouring the above-mentioned adhesion hydrogel precursor liquid on its surface, and curing it at 50°C to obtain an adhesion hydrogel layer; then pouring the second hydrogel precursor liquid on the surface of the adhesion hydrogel layer, irradiating it with 365nm ultraviolet light for 30min and then curing it to obtain a second shape memory gel layer; then pouring the above-mentioned adhesion hydrogel precursor liquid on the surface of the second shape memory gel layer, and curing it at 50°C to obtain an adhesion hydrogel layer; finally, pouring the third hydrogel precursor liquid on the surface of the adhesion hydrogel layer, irradiating it with 365nm ultraviolet light for 30min and then curing it to obtain a third shape memory gel layer; immersing the gel formed after the above curing in an antibacterial aqueous solution for 72h, and taking it out to obtain a shape memory hydrogel biomaterial; wherein the antibacterial agent is 30 parts and the water is 300 parts.

[0072] Embodiment 2:

[0073] (1) adding 15 parts of grafted monomer, 20 parts of shape memory material (gelatin), 0.1 parts of photoinitiator (2-hydroxy-2-methyl-1-[4-(2-hydroxyethoxy)phenyl]-1-propanone) and 10 parts of silver nanoparticles to 60 parts of deionized water, and stirring to obtain a first hydrogel precursor solution; adding 35 parts of grafted monomer, 20 parts of shape memory material (gelatin), 0.3 parts of photoinitiator (2-hydroxy-2-methyl-1-[4-(2-hydroxyethoxy)phenyl]-1-propanone) and 10 parts of silver nanoparticles to 80 parts of deionized water, and stirring to obtain a second hydrogel precursor solution; adding 50 parts of grafted monomer, 20 parts of shape memory material (gelatin), 0.5 parts of photoinitiator (2-hydroxy-2-methyl-1-[4-(2-hydroxyethoxy)phenyl]-1-propanone) and 10 parts of silver nanoparticles to 100 parts of deionized water, and stirring to obtain a third hydrogel precursor solution;

[0074] (2) adding 10 parts of natural polymer material (hyaluronic acid), 5 parts of grafting monomer and 1 part of thermal initiator (ammonium sulfate) into 150 parts of deionized water, stirring and mixing to obtain an adhesive hydrogel precursor solution;

[0075] (3) placing the first hydrogel precursor liquid in a cylindrical mold, irradiating it with 365nm ultraviolet light for 30 minutes and then curing it to obtain a first shape memory gel layer; then pouring the above-mentioned adhesion hydrogel precursor liquid on its surface, reacting and curing it at 50°C to obtain an adhesion hydrogel layer; then, pouring the second hydrogel precursor liquid on the surface of the adhesion hydrogel layer, irradiating it with 365nm ultraviolet light for 30 minutes and then curing it to obtain a second shape memory gel layer; then pouring the above-mentioned adhesion hydrogel precursor liquid on the surface of the second shape memory gel layer, and reacting and curing it at 50°C to obtain an adhesion hydrogel layer; finally, pouring the third hydrogel precursor liquid on the surface of the adhesion hydrogel layer, irradiating it with 365nm ultraviolet light for 30 minutes and then curing it to obtain a shape memory hydrogel biomaterial.

[0076] Comparative Example 1:

[0077] (1) 10 parts of grafted monomer, 10 parts of shape memory material (gelatin), and 0.1 parts of photoinitiator (2-hydroxy-2-methyl-1-[4-(2-hydroxyethoxy)phenyl]-1-propanone) were added to 50 parts of deionized water, and stirred to obtain a hydrogel precursor solution, and three groups of hydrogel precursor solutions were prepared using the same ratio; the above hydrogel precursor solutions were placed in cylindrical molds, irradiated with ultraviolet light for reaction and then cured, and the gels formed after curing were immersed in an antibacterial agent aqueous solution for 72 hours, and three identical shape memory gel layers were obtained after taking out; wherein the antibacterial agent was 10 parts and the water was 100 parts;

[0078] (2) adding 8 parts of natural polymer material (hyaluronic acid), 3 parts of grafting monomer and 0.5 parts of thermal initiator (ammonium sulfate) into 120 parts of deionized water, stirring and mixing to obtain an adhesive hydrogel precursor solution;

[0079] (3) placing one of the shape memory gel layers in a cylindrical mold, then pouring the above-mentioned adhesion hydrogel precursor solution on its surface, and reacting and curing at 50°C to obtain an adhesion hydrogel layer; then, placing a shape memory gel layer on the surface of the adhesion hydrogel layer, then pouring the above-mentioned adhesion hydrogel precursor solution on it, and reacting and curing at 50°C to obtain an adhesion hydrogel layer; finally, placing a shape memory gel layer again on the surface of the adhesion hydrogel layer to obtain a shape memory hydrogel biomaterial.

[0080] Comparative Example 2:

[0081] Comparative Example 2 is basically the same as Example 1, except that step (2) is removed, and in step (3), the first shape memory gel layer is directly placed in a cylindrical mold, and then the second shape memory gel layer and the third shape memory gel layer are placed on the surface thereof in sequence to obtain a shape memory hydrogel biomaterial.

[0082] During the preparation process of Examples 1 to 2 and Comparative Examples 1 to 2, the first shape memory gel layer, the second shape memory gel layer and the third shape memory gel layer were prepared according to the same ratio of raw materials in the Examples and Comparative Examples, respectively, and the hydrogel samples were made into a dumbbell shape of 2.5 mm x 4 mm x 2 mm, and a tensile test was carried out at room temperature using an electronic universal tensile tester-UTM4101; the stretching speed was 50 mm / min, and the sensor was 100 N; the test results of each layer are shown in Table 1.

[0083] Table 1

[0084]

[0085] Note: The elastic moduli of the first, second and third layers correspond to the elastic moduli of the first, second and third shape memory gel layers in the hydrogel biomaterial, respectively.

[0086] It can be seen from Table 1 that, compared with the comparative example, the shape memory hydrogel biomaterial prepared in the embodiment of the present invention is integrated and has excellent mechanical properties. At the same time, its elastic modulus changes gradiently in the thickness direction. When used as a nucleus pulposus replacement material, it can well regulate the differentiation and proliferation of tissue cells around the lumbar disc, thereby being able to combine well with the surrounding tissue cells and promote rapid recovery of wounds.

[0087] Finally, it should be noted that the above embodiments are only used to illustrate the technical solutions of the present invention, rather than to limit it. Although the present invention has been described in detail with reference to the aforementioned embodiments, those skilled in the art should understand that they can still modify the technical solutions described in the aforementioned embodiments, or make equivalent replacements for some of the technical features therein. However, these modifications or replacements do not deviate the essence of the corresponding technical solutions from the spirit and scope of the technical solutions of the embodiments of the present invention.

Claims

1. A shape memory hydrogel biomaterial, characterized in that: The hydrogel biomaterial comprises shape memory hydrogel layers and adhesion hydrogel layers which are alternately arranged in sequence along the vertical direction; wherein the number of the shape memory hydrogel layers is greater than the number of the adhesion hydrogel layers, and the elastic modulus of each shape memory hydrogel layer is different from each other; The shape memory hydrogel comprises a temporary shape and an initial shape, the size of the temporary shape is smaller than the size of the initial shape, and the shape memory hydrogel can be transformed from the temporary shape to the initial shape under external stimulation.

2. The biomaterial according to claim 1, characterized in that The number of the shape memory hydrogel layers is at least three; the elastic modulus of each shape memory hydrogel layer changes gradually in the vertical direction.

3. The biomaterial according to claim 2, characterized in that The change in elastic modulus of two adjacent shape memory gel layers is 50-100 KPa.

4. The biomaterial according to claim 1, characterized in that Each shape memory gel layer is prepared by cross-linking reaction using grafted monomers, shape memory materials, photoinitiators, antibacterial agents and water as reaction raw materials; the shape memory material is gelatin, the photoinitiator is 2-hydroxy-2-methyl-1-[4-(2-hydroxyethoxy)phenyl]-1-propanone or phenylbis(2,4,6-trimethylbenzoyl)phosphine oxide, and the antibacterial agent is tannic acid or silver nanoparticles.

5. The biomaterial according to claim 4, characterized in that In parts by weight, the contents of various reaction raw materials in the preparation process of the shape memory gel layer are as follows: 10-50 parts of grafting monomer, 10-20 parts of shape memory material, 0.1-0.5 parts of photoinitiator, 5-10 parts of antibacterial agent, and 50-100 parts of water.

6. The biomaterial according to claim 1, characterized in that The adhesive gel layer is prepared by cross-linking reaction using natural polymer material, grafting monomer, thermal initiator and water as reaction raw materials; the natural polymer material is hyaluronic acid, and the thermal initiator is ammonium persulfate or sodium persulfate; and / or The grafting monomer is prepared by reacting glycineamide hydrochloride, potassium carbonate, an organic solvent and acryloyl chloride.

7. The biomaterial according to claim 6, characterized in that In parts by weight, the contents of the reaction raw materials in the preparation process of the adhesive gel layer are as follows: 5-10 parts of natural polymer material, 1-5 parts of grafting monomer, 0.1-1 parts of thermal initiator, and 100-150 parts of water.

8. A method for preparing a shape memory hydrogel biomaterial according to any one of claims 1 to 7, characterized in that: The preparation method comprises the following steps: (1) adding grafted monomers, shape memory materials, photoinitiators and antibacterial agents to water in different proportions and stirring to react, thereby obtaining shape memory gel layers with different elastic moduli; wherein the content of grafted monomers in each shape memory gel layer is different; (2) adding the natural polymer material, the grafting monomer and the thermal initiator into water and stirring the reaction to obtain an adhesive gel layer; (3) Alternately placing the shape memory gel layer and the adhesion gel layer in a mold for compounding to obtain the shape memory hydrogel biomaterial.

9. The preparation method according to claim 8, characterized in that: In step (1), the reaction is carried out under ultraviolet light conditions, and the illumination time is 30-60 minutes; and / or In step (2), the reaction temperature is 50-60°C and the reaction time is 30-60 minutes.

10. Use of the shape memory hydrogel biomaterial according to any one of claims 1 to 7 or the shape memory hydrogel biomaterial prepared by the preparation method according to any one of claims 8 to 9 in nucleus pulposus replacement materials.

Citation Information

Patent Citations

  • Photo-curing hydrogel for multi-cell sorting and stem cell area-selecting differentiation and preparation method thereof

    CN105294955A

  • Double-network hydrogel based on poly-N-acrylylglycinamide and sodium alginate, and preparation method thereof

    CN110885524A

  • Concentration / modulus bidirectional gradient hydrogel capable of being used for high-throughput screening of biological materials and preparation method of concentration / modulus bidirectional gradient hydrogel

    CN111607046A

  • Shape memory hydrogel with high strength and multistable state as well as preparation method and application of shape memory hydrogel

    CN114605666A

  • Gel layer and implantable flexible brain-computer interface electrode with same

    CN116763318A