Metal sandwich panel laser welding method and device based on laser pulse swing
By using laser pulse swing technology and argon protection tooling in laser welding, the problems of small welds and low connection strength when the welding thickness increases are solved, and efficient smelting and strength improvement of welds are achieved. It is suitable for large-thick sandwich plates welding.
Patent Information
- Application Number
- CN202411545603.X
- Authority / Receiving Office
- CN · China
- Patent Type
- Applications(China)
- Current Assignee / Owner
- Filing Date
- 2024-11-01
- Publication Date
- 2024-11-29
- Estimated Expiration
- 2044-11-01
AI Technical Summary
When the existing laser welding technology is used to weld the sandwich plate with increased thickness, the effective melting area of the weld is small, the connection strength is low, and the laser power control accuracy is poor, which is prone to pore defects and insufficient applicability.
Using a welding method based on laser pulse swing, the laser power pulse frequency and laser beam space swing frequency are accurately adjusted through the controller, so that they are at the same frequency and phase, forming a "U"-shaped weld, increasing welding energy, and passing parallel to the weld seam The protective tooling achieves argon protection.
Significantly increase the effective smelting area and strength of the weld, reduce welding deformation, improve welding accuracy and joint strength, is suitable for substrate welding with increased thickness, and effectively protects the welding area and reduces pore defects.
Smart Images

Figure CN119035764A_ABST
Abstract
Description
Technical Field
[0001] The invention relates to the technical field of welding, and in particular to a laser welding method and device for metal sandwich panels based on laser pulse swing. Background Art
[0002] Sandwich panels usually have a multi-layer structure. Due to the special nature of their structure, the traditional conventional welding process is relatively complicated and difficult to implement, and will cause large welding deformation. As an advanced welding manufacturing method, laser welding has the advantages of high welding efficiency, small welding deformation, high weld quality, and one-time deep penetration welding, making it an effective means to quickly and efficiently manufacture sandwich panel structures.
[0003] At present, conventional laser welding can achieve the welding of sandwich panel joints of 2mm and below. However, as the thickness of the sandwich panel substrate increases, the weld will present a "T" shape due to the concentrated energy density of the conventional laser, resulting in a smaller effective melting area of the weld and reduced welding strength. By increasing the swing of the laser beam, the spot energy density of the laser beam is reduced, but because the energy distribution of the conventional swing laser is uniform, the welding energy on both sides of the weld is insufficient, resulting in an insignificant increase in the effective melting area of the weld.
[0004] CN111037099A discloses a laser welding method and system for the end faces of copper and its alloy plates of unequal thickness, and proposes that the laser beam power, laser beam swing amplitude and swing frequency can be set according to the thickness of the first plate and the second plate to be welded, so as to stably weld copper and its alloy plates of unequal thickness, ensure that the end faces are fully covered, and the surface weld transition is smooth. However, the following problems still exist: 1. The laser beam swing is a sine wave, while the laser power is a linear wave, and the synergistic effect of the two is poor, and effective time-space coupling cannot be achieved, resulting in unsatisfactory welding effect; 2. The precise control of the laser power at each swing position is not achieved, and only a simple linear change at different deviations is used to control the laser power in each area, with poor accuracy; 3. The laser power control accuracy is poor, there is no gas protection device, and welding defects such as pores are prone to occur, and the applicability to the equal-thickness end face welding or sandwich panels of closed active metals is poor. Summary of the invention
[0005] In view of this, the present invention aims to propose a metal sandwich panel laser welding method and device based on laser pulse oscillation to solve the problem of small effective melting area and low connection strength of lap welds.
[0006] To achieve the above object, the technical solution of the present invention is achieved as follows: On the one hand, the present invention proposes a laser welding method for metal sandwich panels based on laser pulse swing, using a laser welding device, the laser welding device includes a laser head, a controller and a laser, the laser head and the laser are connected to the controller respectively, the laser is used to output laser light and transmit it to the laser head through an optical fiber, the laser head is used to focus the laser light output by the laser to form a guide laser beam, the laser beam swings left and right on the weld of the metal sandwich panel, and is used to weld the metal sandwich panel, the controller collects and receives the swing parameters of the laser beam, and controls the output power and the output pulse waveform of the laser to be a sine wave through the controller, the output power changes, thereby changing the energy of the laser beam at different swinging positions, so that the laser power pulse frequency and the laser beam spatial swing frequency are the same frequency and phase. The present invention utilizes the high-precision coupling control of the two in time and space, and the differentiated distribution of the laser beam energy increases the welding energy on both sides of the weld, and the morphology of the lap weld is "U" shaped, which increases the effective melting area of the weld. The coupling of laser power pulse frequency and laser beam spatial oscillation frequency can better control the laser beam energy distribution on the laser beam oscillation trajectory, realize accurate control of weld heat input, obtain the expected weld profile size, meet different connection strength requirements, and can be used for welding of substrates with increased thickness.
[0007] Furthermore, the laser pulse waveform is a sine wave, and the laser beam swings to the two sides, namely the leftmost position and the rightmost position of the laser beam, and the corresponding powers are P1 and P3 respectively. At this time, the laser power is at the peak value P 峰 When it swings to the middle position, the corresponding power is P2. At this time, the laser power is at the base value P 基 .
[0008] Furthermore, the laser power output by the laser is determined by the following formula:
[0009] Wherein, P is the instantaneous power of the laser output by the laser, in W; P 峰 is the peak power, in W; P 基 is the base power, in W; t is time, in seconds; T1 is the thickness of the upper layer of the metal sandwich panel, in mm; S is the depth of the weld, in mm; k is the phase coordination repair coefficient, in s; D is the distance of laser beam swing, in mm.
[0010] Furthermore, the laser welding method is used to weld a metal sandwich panel, wherein the metal sandwich panel comprises an upper substrate, an interlayer plate and a lower substrate in sequence, and the laser welding method specifically comprises the following steps: Step 1: Pickle the upper substrate, the interlayer plate and the lower substrate, wherein the upper substrate has a first weld, and then clean the first weld area within a range of 20 to 40 mm; Step 2: Assemble and spot weld the upper base plate, sandwich plate and lower base plate, and the assembly gap should be less than 0.5mm; Step 3: Fix the workpiece to be welded with a tool, adjust the trajectory of the laser beam, so that the spot formed by the laser beam is exactly in the middle of the area to be welded, and the offset error of the spot is less than 0.3mm; Step 4: Set the spatial swing amplitude, swing frequency and welding speed of the laser beam according to the process requirements; Step 5, set the laser pulse power output to a sine wave, set the laser power pulse frequency and the laser beam spatial swing frequency to be consistent and have the same phase through the controller, and set the peak power P1 and P3 and the base power P2, so that when the laser beam swings to the left and right sides of the first weld, the power is at P1 or P3, and when it swings to the middle of the first weld, the power is at P2; Step 6: Introduce argon gas to ensure that the first weld area and the heat-affected area are in an argon atmosphere from the beginning to the end of welding; Step 7: Start welding, the laser beam will swing horizontally, and the laser beam will move at the set welding speed, showing a wave-like swinging trajectory on the first weld; Step 8: After reaching the welding end point, the laser output stops, and the welding of the upper substrate and the sandwich panel is completed; Step 9, flip the metal sandwich panel so that the lower base plate is located at the uppermost side, and the lower base plate has a second welding seam; Step 10: Repeat the operations from step 3 to step 7. After reaching the welding end point, the laser output stops, and the welding of the lower base plate and the sandwich plate is completed through the second weld to obtain a welded metal sandwich panel.
[0011] Further, when the upper base plate and the sandwich plate are welded, T1 is the thickness of the upper base plate, and when the lower base plate and the sandwich plate are welded, T1 is the thickness of the lower base plate.
[0012] On the other hand, the present invention also proposes a laser welding device, which adopts the above-mentioned laser welding method for metal sandwich panels based on laser pulse swing, and includes two protective fixtures, which are arranged on the upper plate of the metal sandwich panel, and the two protective fixtures are arranged parallel to the two sides of the weld, and a cavity is formed between the two protective fixtures to form a welding area. By setting the protective fixtures relatively, argon gas can diffuse in the cavity between the protective fixtures, effectively protecting the weld.
[0013] Furthermore, the protective tooling includes an air inlet pipe and an air hole, the air hole is opened on one end face of the protective tooling facing the weld, and the air hole is arranged at the lower part of the end face, one end of the air inlet pipe is connected to the argon gas source, and the other end is connected to the protective tooling. Argon gas enters the protective tooling through the air inlet pipe, overflows into the cavity through the air hole, and evenly sinks to the area to be welded. Due to the high density of argon gas, the air in the upper area of the cavity can be discharged upward until the argon gas diffuses into the entire cavity area, thereby achieving effective gas protection and ensuring the strength of the welded joint.
[0014] Compared with the prior art, the metal sandwich panel laser welding method and device based on laser pulse oscillation described in the present invention has the following advantages: 1. The laser power pulse frequency and the laser beam spatial swing frequency are of the same frequency and phase, so that the two are coupled in time and space, which is beneficial to increase the output power on both sides of the weld, making the appearance of the lap weld "U" shape with adjustable width, increasing the effective melting area and strength of the weld; low power is used in the middle of the weld to reduce the overall heat input and further reduce welding deformation; 2. By controlling the laser energy distribution on the laser beam swing trajectory, the heat input of the weld can be accurately controlled, and the expected weld profile size can be obtained to meet the requirements of different connection strengths; 3. The use of pulse and swing time-space coupled laser welding can reduce the requirements of traditional laser welding on assembly clearance; 4. The protective tooling set parallel to both sides of the weld can achieve effective argon gas protection and ensure the strength of the welded joint. BRIEF DESCRIPTION OF THE DRAWINGS
[0015] The accompanying drawings constituting a part of the present invention are used to provide a further understanding of the present invention. The exemplary embodiments of the present invention and their descriptions are used to explain the present invention and do not constitute an improper limitation of the present invention. In the accompanying drawings: Figure 1 It is a structural schematic diagram of a metal sandwich panel laser welding device based on laser pulse swing according to the present invention; Figure 2 It is a corresponding diagram of the laser power curve, the swing trajectory of the laser beam on the weld, and the cross-sectional diagram of the metal sandwich panel and the weld of the present invention; Figure 3 It is a structural schematic diagram of the protective tooling of the present invention; Figure 4 A schematic diagram of the flow path of the argon shielding gas according to the present invention; Figure 5 This is a metallographic cross-sectional view of a laser-welded sandwich panel according to Example 1 of the present invention; Figure 6This is a metallographic cross-sectional view of a laser welded sandwich panel according to comparative example 1 of the present invention.
[0016] Description of reference numerals: 1. Laser head; 2. Middle position; 3. Leftmost position; 4. Rightmost position; 5. Area to be welded; 6. Swinging trajectory; 7. Welding seam; 8. Upper substrate; 9. Interlayer board; 10. Lower substrate; 11. Controller; 12. Laser; 13. Optical fiber; 14. Protective tooling; 15. Laser power curve; 16. Inlet pipe; 17. Air hole. DETAILED DESCRIPTION
[0017] The present invention will be further described below in conjunction with specific embodiments. It should be noted that the data in the following experimental examples are obtained by the inventor through a large number of experiments. Due to space limitations, only a part of them is shown in the specification, and those of ordinary skill in the art can understand and implement the present invention under these data. These embodiments are only used to illustrate the present invention and are not intended to limit the scope of the present invention. In addition, it should be understood that after reading the content of the present invention, those skilled in the art can make various changes or modifications to the present invention, and these changes or modifications also fall within the scope protected by the present application.
[0018] It should be noted that, in the absence of conflict, the embodiments of the present invention and the features in the embodiments may be combined with each other.
[0019] The present invention will be described in detail below with reference to the accompanying drawings and in conjunction with embodiments.
[0020] The present invention provides a laser welding method for metal sandwich panels based on laser pulse oscillation, using a laser welding device such as Figure 1 As shown, the laser welding device includes a laser head 1, a controller 11 and a laser 12, the laser head 1 and the laser 12 are connected to the controller 11 respectively, the laser head 1 and the laser 12 are connected through an optical fiber 13, the laser 12 is used to output laser light, and transmit it to the laser head 1 through the optical fiber 13, the laser head 1 is used to focus the laser light output by the laser 12 to form a guide laser beam, the laser beam swings left and right on the weld 7 of the metal sandwich panel, and is used to weld the metal sandwich panel, the controller 11 collects and receives the swing parameters of the laser beam, and controls the output power and the output pulse waveform of the laser 12 to be a sine wave through the controller 11, the output power changes, thereby changing the energy of the laser beam at different swing positions, so that the laser power pulse frequency and the laser beam spatial swing frequency are the same frequency and phase.
[0021] The output power of the laser 12 is the power of the laser beam formed by the laser head 1. The present invention adjusts the laser 12 to differentiate and set the energy of each phase of the swing track 6 formed by the laser beam, realizes the differentiated distribution of the laser beam energy at different swing positions, and achieves high-precision coupling control of the laser power pulse frequency output by the laser 12 and the spatial swing frequency of the laser beam focused by the laser head 1 in time and space. The differentiated distribution of the laser beam energy increases the welding energy on both sides of the weld 7, and the morphology of the lap weld 7 is "U"-shaped, which increases the effective melting area of the weld 7. It avoids the situation that after the laser beam swings, the energy distribution is uniform, resulting in insufficient welding energy in the areas on both sides of the weld 7. The coupling of the laser power pulse frequency and the laser beam spatial swing frequency can better control the laser beam energy distribution on the laser beam swing track 6, realize accurate control of the weld heat input, and obtain the expected cross-sectional dimensions of the weld 7, meet different connection strength requirements, and can be used for welding substrates with increased thickness.
[0022] The laser 12 of the present invention can control the laser power pulse frequency under the action of the controller 11. The laser head 1 can control the laser beam spatial oscillation frequency under the action of the controller 11. The specific control method can refer to the prior art and will not be described in detail here.
[0023] A rotating lens is provided in the laser head 1. By adjusting the rotational posture of the lens, the laser beam can be caused to swing in space perpendicular to the welding direction. The main swinging parameters include the swinging frequency and the swinging amplitude. The swinging amplitude is determined according to the width of the weld 7 and the operator's experience. Within a swinging interval, the laser beam swings left and right at a specific swinging amplitude. The high-frequency swinging makes the laser beam form a linear heat source. The laser beam at the leftmost position 3 and the laser beam at the rightmost position 4 can increase the heated area and increase the heat input on both sides of the weld 7, thereby increasing the heated width of the weld 7.
[0024] Furthermore, the laser pulse waveform is a sine wave, and the laser beam swings to the two sides, namely the leftmost position 3 and the rightmost position 4, and the corresponding powers are P1 and P3 respectively. At this time, the laser power is at the peak value P 峰 When it swings to the middle position 2, the corresponding power is P2. At this time, the laser power is at the base value P 基 , the laser power output by the laser 12 is determined by the following formula:
[0025] Wherein, P is the instantaneous power of the laser output by the laser 12, in W; P 峰 is the peak power, in W; P 基 is the base power, in W; t is time, in seconds; T1 is the thickness of the upper layer of the metal sandwich panel, in mm; S is the depth of weld 7, in mm; k is the phase coordination repair coefficient, in s; D is the distance of laser beam swing, in mm.
[0026] During welding, the laser beam oscillates perpendicular to the welding direction. Figure 2 As shown, from top to bottom, the laser power curve 15, the swing trajectory 6 of the laser beam on the weld 7, and the cross-sectional view of the metal sandwich panel and the weld 7 are represented in sequence. The laser pulse power output is a sine wave, and the swing trajectory 6 of the laser beam on the weld 7 is wavy. The determination of the laser power output by the laser 12 is related to the swing position of the laser beam. When the laser beam swings to the left and right sides, the power is at the peak value of P1 or P3. The high-power laser on both sides of the weld 7 can increase the heated width, and the morphology of the lap weld 7 changes from a "T" shape or a "V" shape to a "U" shape with adjustable width. The effective melting area of the weld 7 is significantly increased, and the strength of the lap weld 7 is significantly improved. When the laser beam swings to the middle position 2, the power is at the base value of P2, which can reduce the energy in the central area of the weld 7, reduce the overall heat input, and control welding deformation. Through the formula of the laser power P output by the laser 12 of the present invention, the laser power at each swing position can be accurately controlled, and the control accuracy of the pulsed laser is high, so as to achieve accurate control and improvement of the effective melting area of the weld.
[0027] exist Figure 2 In the cross-sectional view of the metal sandwich panel and the weld 7, C is the width of the weld 7, S is the depth of the weld 7, Y is the width of the effective melting area, T1 is the thickness of the upper base plate 8, and T2 is the thickness of the sandwich panel 9.
[0028] A laser welding method for metal sandwich panels based on laser pulse oscillation of the present invention is used to weld metal sandwich panels, wherein the metal sandwich panels sequentially include an upper substrate 8, an interlayer plate 9 and a lower substrate 10. The welding method specifically includes the following steps: Step 1: pickling the upper substrate 8, the interlayer plate 9 and the lower substrate 10, wherein the upper substrate 8 has a first weld, and then cleaning the first weld area within a range of 20 to 40 mm; Specifically, when cleaning the area near the first weld, either a hard grinding head or laser cleaning is used.
[0029] Step 2: Assemble and spot weld the upper base plate 8, the sandwich plate 9 and the lower base plate 10, and the assembly gap should be less than 0.5mm; Step 3: Fix the workpiece to be welded with a tool, adjust the trajectory of the laser beam, so that the spot formed by the laser beam is located exactly in the middle of the area to be welded 5, and the offset error of the spot is less than 0.3mm; Step 4: Set the spatial swing amplitude, swing frequency and welding speed of the laser beam according to the process requirements; Specifically, the swing amplitude is the distance from the leftmost position 3 to the rightmost position 4, the distance of the laser beam at the leftmost position 3 is D1, the distance at the rightmost position 4 is D3, and the distance at the middle position 2 is D2. The welding speed is 0.1~0.3mm / s.
[0030] Step 5, setting the laser pulse power output to a sine wave, setting the laser power pulse frequency and the laser beam spatial swing frequency to be consistent and have the same phase through the controller 11, and setting the peak power P1 and P3 and the base power P2, so that when the laser beam swings to the left and right sides of the first weld, the power is at P1 or P3, and when it swings to the middle of the first weld, the power is at P2; Step 6: Introduce argon gas to ensure that the first weld area and the heat-affected area are in an argon atmosphere from the beginning to the end of welding; Step 7: Start welding, the laser beam produces a lateral swing, and the laser beam moves at a set welding speed, presenting a wave-like swing trajectory 6 on the first weld; The laser energy of each phase on the oscillating trajectory 6 is controlled by the controller 11. Therefore, the laser energy at each position of the wave trajectory can be accurately controlled, and the heat input in the first weld area is rationally distributed, which is conducive to controlling the size of the first weld and reducing welding deformation.
[0031] Step 8: After reaching the welding end point, the laser output stops, and the welding of the upper substrate 8 and the sandwich plate 9 is completed; Step nine, flip the metal sandwich panel so that the lower base plate 10 is located at the uppermost side, and the lower base plate 10 has a second welding seam; Step 10: Repeat the operations from step 3 to step 7. After reaching the welding end point, the laser output stops, and the welding of the lower base plate 10 and the sandwich plate 9 is completed through the second weld to obtain a welded metal sandwich panel.
[0032] Regarding the determination of the instantaneous power P of the laser output by the laser 12, when welding the upper substrate 8 and the sandwich plate 9, T1 is the thickness of the upper substrate 8, and when welding the lower substrate 10 and the sandwich plate 9, T1 is the thickness of the lower substrate 10.
[0033] The present invention also provides a laser welding device, the laser welding device includes two protective tools 14, such as Figure 3~4As shown, the protective tooling 14 is arranged on the upper plate of the metal sandwich panel, and two protective toolings 14 are arranged parallel to the two sides of the weld 7, and there is a cavity between the two protective toolings 14 to form a welding area 5. The weld 7 is located in the cavity. When the metal sandwich panel laser welding method based on laser pulse swing is used to weld the lap joint of the metal sandwich panel, due to the large heated area, the protection difficulty is also greater, and oxidation at the joint is likely to cause a decrease in welding strength. The use of traditional mobile drag hoods for protection is inconvenient to operate. By setting relatively arranged protective toolings 14, argon gas can diffuse in the cavity between the protective toolings 14, and the weld 7 is effectively protected. Figure 4 The arrow in the figure shows the flow direction of the argon gas after it escapes from the protective tooling 14 .
[0034] As a preferred embodiment of the present invention, the protective tooling 14 includes an air inlet pipe 16 and an air hole 17. The air hole 17 is opened on one end face of the protective tooling 14 facing the weld 7, and the air hole 17 is arranged at the lower part of the end face. One end of the air inlet pipe 16 is connected to the argon gas source, and the other end is connected to the protective tooling 14. Argon gas enters the protective tooling 14 through the air inlet pipe 16, overflows into the cavity through the air hole 17, and evenly sinks to the area to be welded 5. Due to the high density of argon gas, the air in the upper area of the cavity can be discharged upward until the argon gas diffuses into the entire cavity area, thereby achieving effective gas protection, reducing pore defects, preventing weld oxidation, improving weld forming quality, and ensuring the strength of the welded joint.
[0035] The metal sandwich panel laser welding method and device based on laser pulse oscillation of the present invention has the following advantages: 1. The laser power pulse frequency and the laser beam spatial swing frequency are of the same frequency and phase, so that the two are coupled in time and space, which is conducive to increasing the output power on both sides of the weld 7, making the appearance of the lap weld 7 into a "U" shape with adjustable width, and increasing the effective melting area and strength of the weld 7; low power is used in the middle of the weld 7 to reduce the overall heat input and further reduce welding deformation; 2. By controlling the laser energy distribution on the laser beam swing trajectory 6, the heat input of the weld 7 can be accurately controlled, and the expected cross-sectional dimensions of the weld 7 can be obtained to meet the requirements of different connection strengths; 3. The use of pulse and swing time-space coupled laser welding can reduce the requirements of traditional laser welding on assembly clearance; 4. The protective tooling 14 is arranged parallel to both sides of the weld 7 to achieve effective argon gas protection and ensure the strength of the weld joint; 5. It can realize efficient welding of active metal sandwich panels such as titanium alloy or zirconium alloy.
[0036] Example 1
[0037] The metal sandwich panel of the present invention can be a titanium alloy sandwich panel. As a light-weight, high-specific stiffness and high-specific strength structure, the titanium alloy sandwich panel structure has outstanding advantages in fire resistance, shock absorption, fatigue resistance and impact resistance.
[0038] This embodiment takes titanium alloy as an example. The parent material is an upper substrate 8 with a thickness of 3 mm, a lower substrate 10, and a sandwich plate 9 with a thickness of 3 mm. The metal sandwich panel laser welding method and welding device based on laser pulse swing of the present invention are used to weld the upper substrate 8, the sandwich plate 9 and the lower substrate 10. During the welding process, the laser 12 and the laser head 1 are controlled by the controller 11 so that the laser power pulse frequency and the laser beam spatial swing frequency are the same frequency and phase. The laser power output by the laser 12 is determined by the following formula: .
[0039] like Figure 5 As shown, the morphology of the weld 7 obtained in Example 1 is "U"-shaped, and the width Y of the effective melting area of the weld 7 is 2.6 mm.
[0040] Comparative Example 1 Titanium alloy is selected as the workpiece to be welded, and the selection of the parent material is the same as in Example 1, and the conventional laser welding method is adopted. Figure 6 As shown, the morphology of the weld 7 obtained in Comparative Example 1 is in the shape of a letter T, and the width Y of the effective melting area of the weld 7 is 1.2 mm.
[0041] Compared with comparative example 1, by using example 1 of the present invention, the effective melting area width D of the weld 7 is increased, and the strength of the lap weld 7 is more than doubled, which is suitable for high-quality welding of thick metal sandwich panels.
[0042] The above description is only a preferred embodiment of the present invention and is not intended to limit the present invention. Any modifications, equivalent substitutions, improvements, etc. made within the spirit and principle of the present invention should be included in the protection scope of the present invention.
Claims
1. A laser welding method for metal sandwich panels based on laser pulse oscillation, It is characterized in that A laser welding device is used, comprising a laser head (1), a controller (11) and a laser (12), wherein the laser head (1) and the laser (12) are respectively connected to the controller (11), wherein the laser (12) is used to output laser light and transmit the laser light to the laser head (1) via an optical fiber (13), wherein the laser head (11) is used to focus the laser light output by the laser (12) to form a guide laser beam, wherein the laser beam swings left and right on a weld seam (7) of a metal sandwich panel and is used to weld the metal sandwich panel, wherein the controller (11) collects and receives swing parameters of the laser beam, and controls the output power and output pulse waveform of the laser (12) to be a sine wave through the controller (11), wherein the output power changes, thereby changing the energy of the laser beam at different swing positions, so that the laser power pulse frequency and the laser beam spatial swing frequency have the same frequency and phase.
2. The metal sandwich panel laser welding method based on laser pulse oscillation according to claim 1, It is characterized in that The laser pulse waveform is a sine wave. The laser beam swings to the leftmost position (3) and the rightmost position (4). The corresponding powers are P1 and P3 respectively. At this time, the laser power is at the peak value P 峰 When it swings to the middle position (2), the corresponding power is P2. At this time, the laser power is at the base value P 基 .
3. The metal sandwich panel laser welding method based on laser pulse oscillation according to claim 2, It is characterized in that The laser power output by the laser (12) is determined by the following formula: , Wherein, P is the instantaneous power of the laser output by the laser (12), in W; P 峰 is the peak power, in W; P 基 is the base power, in W; t is time, in seconds; T 1 is the thickness of the upper layer of the metal sandwich panel, in mm; S is the depth of the weld (7), in mm; k is the phase coordination repair coefficient, in s; D is the distance of laser beam swing, in mm.
4. The metal sandwich panel laser welding method based on laser pulse oscillation according to any one of claims 1 to 3, It is characterized in that The laser welding method is used to weld a metal sandwich panel, wherein the metal sandwich panel comprises an upper base plate (8), a sandwich plate (9) and a lower base plate (10) in sequence, and the laser welding method specifically comprises the following steps: Step 1: pickling the upper substrate (8), the sandwich plate (9) and the lower substrate (10), wherein the upper substrate (8) has a first weld, and then cleaning the first weld area within a range of 20 to 40 mm; Step 2: Assemble and spot weld the upper base plate (8), the sandwich plate (9) and the lower base plate (10), and the assembly gap should be less than 0.5 mm; Step 3: Fix the workpiece to be welded with a tool, and adjust the trajectory of the laser beam so that the spot formed by the laser beam is exactly in the middle of the area to be welded (5), and the offset error of the spot is less than 0.3 mm; Step 4: Set the spatial swing amplitude, swing frequency and welding speed of the laser beam according to the process requirements; Step 5, setting the laser pulse power output to a sine wave, setting the laser power pulse frequency and the laser beam spatial swing frequency to be consistent and have the same phase through the controller (11), and setting the peak power P1 and P3 and the base power P2, so that when the laser beam swings to the left and right sides of the first weld, the power is at P1 or P3, and when it swings to the middle position (2) of the first weld, the power is at P2; Step 6: Introduce argon gas to ensure that the first weld area and the heat-affected area are in an argon atmosphere from the beginning to the end of welding; Step 7: Start welding, the laser beam generates a lateral swing, and the laser beam moves at a set welding speed, presenting a wave-like swing trajectory on the first weld (6); Step 8: After reaching the welding end point, the laser output stops, and the welding of the upper substrate (8) and the sandwich plate (9) is completed; Step nine, turning over the metal sandwich panel so that the lower base plate (10) is located at the uppermost side, and the lower base plate (10) has a second weld seam; Step 10: Repeat the operations of step 3 to step 7. After reaching the welding end point, the laser output stops, and the welding of the lower base plate (10) and the sandwich plate (9) is completed through the second weld seam to obtain a welded metal sandwich panel.
5. The metal sandwich panel laser welding method based on laser pulse oscillation according to claim 4, It is characterized in that When the upper base plate (8) and the sandwich plate (9) are welded, T1 is the thickness of the upper base plate (8), and when the lower base plate (10) and the sandwich plate (9) are welded, T1 is the thickness of the lower base plate (10).
6. A laser welding device, It is characterized in that The laser welding device adopts the metal sandwich panel laser welding method based on laser pulse oscillation according to any one of claims 1 to 5, and the laser welding device comprises two protective fixtures (14), the protective fixtures (14) are arranged on the upper plate of the metal sandwich panel, and the two protective fixtures (14) are arranged parallel to the two sides of the weld (7), and a cavity is provided between the two protective fixtures (14) to form a welding area (5).
7. The laser welding device according to claim 6, It is characterized in that The protective tooling (14) comprises an air inlet pipe (16) and an air hole (17); the air hole (17) is formed on an end surface of the protective tooling (14) facing the weld (7), and the air hole (17) is arranged at the lower part of the end surface; one end of the air inlet pipe (16) is connected to an argon gas source, and the other end is connected to the protective tooling (14).
Citation Information
Patent Citations
Multilayer combination hollow sandwich plate structure for protection and welding method
CN107672248A
Method for remote laser welding with superposed oscillating movement of the laser beam
CN107949453A
Laser welding method and system for end faces of copper and copper alloy plates with different thicknesses
CN111037099A
Laser welding system, laser welding control method and device and storage medium
CN113182686A
Aluminum alloy and stainless steel welding method capable of obtaining high-strength welding joint
CN113414494A
Cited By
Handheld laser welding method and welding machine based on laser swing energy control
CN120828198A