Heat-insulating and fire-resistant regenerated building wall polyphenyl material and preparation method thereof
By using styrene-vinyl triethoxysilane-zinc borate and styrene-glycidyl methacrylate-melamine polyphosphate copolymers in building wall materials, combined with regenerated polyphenylene plastics and other additives, the solution is solved The problem of insufficient thermal insulation and fire resistance performance of traditional materials is achieved, and high-performance thermal insulation and fire resistance effects and resource recycling are achieved to meet building safety and energy-saving needs.
Patent Information
- Application Number
- CN202411556587.4
- Authority / Receiving Office
- CN · China
- Patent Type
- Applications(China)
- Current Assignee / Owner
- Filing Date
- 2024-11-04
- Publication Date
- 2024-11-29
AI Technical Summary
Traditional building wall materials have limitations in thermal insulation and fire resistance, which is difficult to meet the needs of building safety and energy saving. Moreover, the performance of regenerated polystyrene materials is not as good as that of native materials, and it needs to be improved by adding special compounds.
Using styrene-vinyltriethoxysilane-zinc borate copolymer (P (St - VTEOS - ZB) and styrene-glycidyl methacrylate-melamine polyphosphate copolymer (P (St - GMA - MPP ) and other copolymers, combined with regenerated polystyrene plastics, plasticizers, stabilizers and flame retardants, prepare heat-insulating and refractory recycled building wall polystyrene materials through free radical polymerization and extrusion molding.
It significantly improves the heat insulation and fire resistance and mechanical properties of wall materials, extends the service life of the materials, realizes resource recycling and environmentally friendly and sustainable development, and meets the needs of different building structures and use environments.
Abstract
Description
Technical Field
[0001] The invention relates to the technical field of building wall materials, and in particular to a heat-insulating and fire-resistant recycled building wall polystyrene material and a preparation method thereof. Background Art
[0002] In modern buildings, the performance requirements of wall materials are becoming increasingly stringent. Not only do they need to have good thermal insulation to reduce energy consumption, but they must also have excellent fire resistance to ensure the safety of buildings in emergency situations such as fires. Traditional building wall materials have certain limitations in terms of thermal insulation and fire resistance, and it is difficult to meet people's needs for building safety and energy saving.
[0003] Polystyrene materials have been widely used in the field of building insulation due to their good thermal insulation properties. However, the flammability of polystyrene materials makes them have major defects in fire resistance. With the increasing requirements for building fire protection, the development of heat-insulating and fire-resistant polystyrene wall materials has become a research hotspot.
[0004] At the same time, the increasing awareness of resource recycling and environmental protection has prompted people to pay attention to the application of recycled polystyrene materials. The use of recycled polystyrene materials can not only reduce waste emissions, but also reduce the cost of raw materials. However, the performance of recycled polystyrene materials is often not as good as that of virgin materials, and special compounds need to be added to improve their performance. Summary of the invention
[0005] The present invention proposes a heat-insulating and fire-resistant recycled building wall polystyrene material and a preparation method thereof, specifically: A heat-insulating and fire-resistant recycled building wall polystyrene material comprises a styrene-vinyl triethoxysilane-zinc borate copolymer (P (St - VTEOS - ZB)), wherein the molar ratio of styrene, vinyl triethoxysilane and zinc borate is 4:1:1.
[0006] Furthermore, the wall polystyrene material also includes recycled polystyrene plastic, plasticizer, stabilizer and flame retardant. The plasticizer is dioctyl phthalate, accounting for 8% of the total mass; the stabilizer is zinc stearate, accounting for 3% of the total mass; and the flame retardant is magnesium hydroxide, accounting for 15% of the total mass.
[0007] The recycled polystyrene plastics are discarded polystyrene foams and polystyrene plastic products, which are common knowledge in the art and can be obtained through conventional channels.
[0008] Furthermore, the method for preparing the wall polystyrene material comprises the following steps: S1. Add styrene, vinyl triethoxysilane and zinc borate monomers into a reaction vessel, wherein the molar ratio of styrene, vinyl triethoxysilane and zinc borate is 4:1:1; then add dibenzoyl peroxide as an initiator in an amount of 1.5% of the total mass of the monomers, and xylene as a solvent; heat the reaction system to 90° C., and perform free radical polymerization under nitrogen protection for 6 hours; after the reaction is completed, cool to room temperature, pour the reaction product into ethanol for precipitation, filter and dry to obtain a P (St - VTEOS - ZB) copolymer; S2, mixing the prepared P (St - VTEOS - ZB) copolymer with recycled polystyrene plastic and additives; the additives include plasticizer dioctyl phthalate, stabilizer zinc stearate, and flame retardant magnesium hydroxide; the mixing process is carried out in a high-speed mixer to ensure that the components are fully mixed and uniform; then, the mixed materials are prepared into wall materials through an extrusion molding process.
[0009] On the other hand, the present invention also provides another high-performance heat-insulating and fire-resistant recycled building wall polystyrene material, comprising styrene-glycidyl methacrylate-melamine polyphosphate copolymer (P (St-GMA-MPP)), wherein the molar ratio of styrene, glycidyl methacrylate and melamine polyphosphate is 3:1:2.
[0010] Furthermore, the wall material also includes recycled polystyrene plastic, plasticizer, stabilizer and flame retardant. The plasticizer is tributyl citrate, accounting for 6% of the total mass; the stabilizer is barium laurate, accounting for 2.5% of the total mass; and the flame retardant is a mixture of aluminum hydroxide and magnesium hydroxide in a mass ratio of 1:1, accounting for 12% of the total mass.
[0011] Furthermore, the method for preparing the wall polystyrene material comprises: S1. Add styrene, glycidyl methacrylate and melamine polyphosphate monomers into a reaction vessel, wherein the molar ratio of styrene, glycidyl methacrylate and melamine polyphosphate is 3:1:2; then add azobisisoheptanenitrile as an initiator in an amount of 1.2% of the total mass of the monomers, and solvent toluene; heat the reaction system to 85° C., and perform free radical polymerization under nitrogen protection for 5.5 hours; after the reaction is completed, cool to room temperature, pour the reaction product into methanol for precipitation, filter and dry to obtain a P (St-GMA-MPP) copolymer; S2. The prepared P (St-GMA-MPP) copolymer is mixed with recycled polystyrene plastic and additives; the additives include a mixture of plasticizer tributyl citrate, stabilizer barium laurate, and flame retardants aluminum hydroxide and magnesium hydroxide; the mixing process is carried out in a high-speed mixer to ensure that the components are fully mixed and uniform; then, the mixed materials are prepared into wall materials through an extrusion molding process.
[0012] Furthermore, the styrene-vinyl triethoxysilane-zinc borate copolymer (P (St-VTEOS-ZB)) is used in the preparation of double-isolation recycled polystyrene plastic building wall materials.
[0013] Furthermore, the styrene-glycidyl methacrylate-melamine polyphosphate copolymer (P (St-GMA-MPP)) is used in the preparation of double-isolation recycled polystyrene plastic building wall materials. Beneficial technical effects:
[0014] 1. Improved thermal insulation and fire resistance By introducing copolymers such as styrene-vinyl triethoxysilane-zinc borate, the thermal insulation and fire resistance of wall materials are significantly improved. The synergistic effect of ethoxysilane groups and zinc borate groups effectively prevents the transfer of heat and oxygen, delays the combustion of materials, reduces the heat release rate, and enables wall materials to better withstand high temperature environments and meet building fire protection requirements.
[0015] (II) Enhanced mechanical properties The rigid structure provided by styrene and the good compatibility of copolymers with other components significantly improve the tensile strength, bending strength and other mechanical properties of the wall materials after adding P (St -VTEOS - ZB) copolymer. This helps to ensure the stability and durability of the wall materials during use and extend the service life of the building.
[0016] 3. Environmental protection and resource recycling The invention uses recycled polystyrene plastic as the main raw material, reduces the discharge of waste and realizes the recycling of resources. Meanwhile, the additives and copolymers used are environmentally friendly during production and use, and meet the requirements of sustainable development.
[0017] (IV) Comprehensive performance optimization The addition of new compounds not only improves the thermal insulation, fire resistance and mechanical properties of wall materials, but also improves the chemical stability and compatibility of materials. This comprehensive performance optimization makes wall materials have a wider application prospect in the construction field and can meet the needs of different building structures and use environments. DETAILED DESCRIPTION Example 1
[0018] The heat-insulating and fire-resistant recycled building wall polystyrene material of the present invention comprises styrene-vinyl triethoxysilane-zinc borate copolymer (P (St-VTEOS-ZB)), wherein the molar ratio of styrene, vinyl triethoxysilane and zinc borate is 4:1:1. In addition, the wall polystyrene material also includes recycled polystyrene plastic, plasticizer, stabilizer and flame retardant. The plasticizer is dioctyl phthalate, accounting for 8% of the total mass; the stabilizer is zinc stearate, accounting for 3% of the total mass; the flame retardant is magnesium hydroxide, accounting for 15% of the total mass. The recycled polystyrene plastic is discarded polystyrene foam and polystyrene plastic products, which are common knowledge in the art and can be obtained through conventional channels.
[0019] In a reaction vessel, styrene, vinyl triethoxysilane and zinc borate monomers are added, wherein the molar ratio of styrene, vinyl triethoxysilane and zinc borate is 4:1:1. Then, dibenzoyl peroxide initiator is added in an amount of 1.5% of the total mass of the monomers, and solvent xylene. The reaction system is heated to 90°C and free radical polymerization is carried out under nitrogen protection for 6 hours. After the reaction is completed, it is cooled to room temperature, and the reaction product is poured into ethanol for precipitation, filtered and dried to obtain P (St - VTEOS - ZB) copolymer.
[0020] The prepared P (St - VTEOS - ZB) copolymer is mixed with recycled polystyrene plastic and additives. The additives include plasticizer dioctyl phthalate, stabilizer zinc stearate, flame retardant magnesium hydroxide, etc. The mixing process is carried out in a high-speed mixer to ensure that the components are fully mixed and uniform. Then, the mixed materials are prepared into wall materials through an extrusion molding process. During the extrusion process, the extrusion temperature is controlled to be 200°C, the pressure is 10MPa, and the speed is 2m / min.
[0021] The P (St - VTEOS - ZB) copolymer is designed and synthesized based on the demand for thermal insulation and fire resistance. Styrene (St) provides the basic skeleton and physical properties of the material. The introduction of vinyl triethoxysilane (VTEOS) and zinc borate (ZB) is intended to improve the thermal insulation and fire resistance of the material. The benzene ring is a rigid structural unit that provides high strength and stability for the material. The conjugated structure of the benzene ring makes the electron cloud evenly distributed throughout the ring, giving the material good chemical corrosion resistance. When the wall material is corroded by external chemicals, the benzene ring can effectively resist chemical attacks and maintain the structural integrity of the material. At the same time, the presence of the benzene ring also helps to improve the thermal insulation performance of the material, because the benzene ring structure can hinder the transfer of heat. The ethoxysilane group will undergo hydrolysis and condensation reactions when heated to form a three-dimensional network structure of siloxane. This siloxane structure can effectively prevent the transfer of heat and gas, and improve the thermal insulation and fire resistance of the material. During the combustion process, the siloxane structure can form a dense protective layer on the surface of the material to prevent oxygen and heat from penetrating into the interior of the material, thereby slowing down the combustion rate of the material. In addition, the ethoxysilane group can also enhance the compatibility of the material with other components and improve the overall performance of the material. Zinc borate will decompose at high temperatures, releasing crystal water and absorbing a large amount of heat, thereby reducing the temperature of the material surface and playing a flame retardant and heat insulating role. At the same time, the zinc oxide and boron oxide produced by the decomposition of zinc borate can form a glass-like covering layer on the surface of the material. This covering layer can prevent the transfer of heat and oxygen and enhance the fire resistance of the material. In addition, zinc borate can also produce a synergistic effect with other flame retardants to further improve the flame retardant effect of the material. In order to more intuitively demonstrate the advantages of the heat-insulating and fire-resistant recycled building wall polystyrene material of the present invention over the prior art, The following comparative synergistic tests were conducted: The thermal conductivity of the wall material of the present invention (experimental group) and the common polystyrene wall material in the prior art (control group) were tested using a thermal conductivity tester. The test results show that the thermal conductivity of the control group is 0.055 W / (m・K), while the thermal conductivity of the experimental group is only 0.035 W / (m・K). This shows that the wall material of the present invention has better thermal insulation performance, can more effectively prevent the transfer of heat, maintain the stability of indoor temperature, and reduce the energy consumption of the building; The wall materials of the control group and the experimental group were made into samples of the same size and placed on a heating table to increase the surface temperature evenly. Then an infrared thermal imager was used to monitor the temperature distribution on the surface of the sample. The results showed that under the same heating conditions, the temperature distribution on the surface of the control group sample was uneven and the heat diffusion was fast, while the temperature distribution on the surface of the experimental group sample was relatively uniform and the heat diffusion was significantly slowed down. This further proves the excellent thermal insulation performance of the wall material of the present invention; The vertical combustion test was conducted in accordance with national standards. The ordinary polystyrene wall material in the control group burned rapidly under the action of the flame, with a burning time of up to 15 seconds, accompanied by a large amount of dripping, which easily caused a secondary fire. However, after adding P (St - VTEOS - ZB) copolymer to the wall material of the experimental group, the burning time was significantly shortened to 5 seconds, the dripping phenomenon was significantly reduced, and the flame propagation speed was effectively controlled; Thermogravimetric analysis was performed on the wall materials of the control group and the experimental group. The results showed that the initial decomposition temperature of the control group was 260°C, and the mass loss was rapid at high temperatures. The initial decomposition temperature of the experimental group was increased to 350°C, and the mass loss curve was relatively gentle during the entire thermal decomposition process, indicating that the wall material of the present invention has better thermal stability at high temperatures and can better resist flame erosion; The oxygen index is an important indicator for measuring the flame retardant properties of materials. The test results show that the oxygen index of the control group is 20%, which is a flammable material. The oxygen index of the wall material in the experimental group increased to 30%, indicating that it has better flame retardant properties and is more difficult to burn in the air; The tensile strength of the wall materials of the control group and the experimental group was tested using a universal material testing machine. The tensile strength of the control group was 12.5 MPa, while the tensile strength of the experimental group was increased to 16.8 MPa, indicating that the wall material of the present invention has a better ability to resist tensile deformation; The bending strength test showed that the bending strength of the control group was 18.2 MPa, while the bending strength of the experimental group reached 23.5 MPa. This shows that the wall material of the present invention has higher strength when subjected to bending load, and can better ensure the structural stability of the wall; The wall material samples of the control group and the experimental group were placed in a UV aging box to simulate UV irradiation in the natural environment. After a certain period of irradiation, the appearance changes and performance degradation of the samples were observed. The samples of the control group showed obvious fading, cracking and performance degradation, while the samples of the experimental group had less appearance changes and the degree of performance degradation was significantly lower than that of the control group due to the addition of additives such as stabilizers, indicating that the wall material of the present invention has better UV aging resistance; The samples were placed in a damp heat aging test chamber, and a certain temperature and humidity condition was set to conduct a damp heat aging test. The results showed that the wall materials in the control group were prone to deformation and mold in a damp heat environment, and the mechanical properties decreased significantly. However, the wall materials in the experimental group maintained good appearance and mechanical properties after damp heat aging, indicating that they have better resistance to damp heat aging. 1. Improved thermal insulation and fire resistance By introducing styrene-vinyl triethoxysilane-zinc borate copolymer, the thermal insulation and fire resistance of the wall material are significantly improved. The synergistic effect of the ethoxysilane group and the zinc borate group effectively prevents the transfer of heat and oxygen, delays the combustion of the material, reduces the heat release rate, and enables the wall material to better withstand high temperature environments and meet the requirements of building fire protection; (II) Enhanced mechanical properties The rigid structure provided by styrene and the good compatibility of copolymers with other components significantly improve the tensile strength, bending strength and other mechanical properties of the wall materials after adding P (St -VTEOS - ZB) copolymer. This helps to ensure the stability and durability of the wall materials during use and extend the service life of the building.
[0022] 3. Environmental protection and resource recycling The invention uses recycled polystyrene plastic as the main raw material, reduces the discharge of waste and realizes the recycling of resources. Meanwhile, the additives and copolymers used are environmentally friendly during production and use, and meet the requirements of sustainable development.
[0023] (IV) Comprehensive performance optimization The addition of new compounds not only improves the thermal insulation, fire resistance and mechanical properties of wall materials, but also improves the chemical stability and compatibility of materials. This comprehensive performance optimization makes wall materials have a wider application prospect in the construction field and can meet the needs of different building structures and use environments.
[0024] Table 1. Comparative synergistic experiment of P (St - VTEOS - ZB) copolymer Performance test items Existing wall materials (control group) Wall material of the present invention (experimental group) Efficiency data Thermal conductivity (W / (m・K)) 0.055 0.035 Reduced by 0.02 Vertical burning test burning time (s) 15 5 Shorten by 10 seconds Thermogravimetric analysis onset decomposition temperature (℃) 260 350 Increase 90℃ Oxygen index (%) 20 30 Increase by 10% Tensile strength (MPa) 12.5 16.8 Increase 4.3MPa Bending strength (MPa) 18.2 23.5 Increase 5.3MPa UV aging test appearance change degree Obvious fading and cracking Slight changes The degree of change has been significantly reduced UV aging test performance attenuation degree Significant decline Smaller The attenuation is significantly reduced Deformation degree of wet heat aging test Easy to deform Small deformation The degree of deformation is significantly reduced Moisture test of heat aging Prone to mold Less mold The mold condition has been significantly improved
[0025] Embodiment 2, The wall material of the present invention comprises styrene-glycidyl methacrylate-melamine polyphosphate copolymer (P (St-GMA-MPP)), wherein the molar ratio of styrene, glycidyl methacrylate and melamine polyphosphate is 3:1:2. In addition, the wall polystyrene material also comprises recycled polystyrene plastic, plasticizer, stabilizer and flame retardant. The plasticizer is tributyl citrate, accounting for 6% of the total mass; the stabilizer is barium laurate, accounting for 2.5% of the total mass; the flame retardant is a mixture of aluminum hydroxide and magnesium hydroxide (mass ratio 1:1), accounting for 12% of the total mass. The recycled polystyrene plastic is discarded polystyrene foam and polystyrene plastic products, which are common knowledge in the art and can be obtained through conventional channels.
[0026] Prepare raw materials such as styrene, glycidyl methacrylate, melamine polyphosphate, azobisisobutyronitrile, toluene, recycled polystyrene plastic, tributyl citrate, barium laurate, aluminum hydroxide, and magnesium hydroxide.
[0027] In a four-necked flask equipped with a stirrer, a thermometer, a reflux condenser and a nitrogen inlet device, a certain amount of styrene, glycidyl methacrylate and toluene are added. After stirring evenly, the four-necked flask is placed in an oil bath and heated to 85°C. Then, azobisisoheptanenitrile dissolved in a small amount of toluene is slowly added dropwise to the reaction system. Next, melamine polyphosphate monomer is added. Under nitrogen protection, the reaction is carried out for 5.5 hours. After the reaction is completed, the reaction product is poured into methanol for precipitation. The precipitate is filtered and placed in a vacuum drying oven to dry to constant weight to obtain P (St - GMA - MPP) copolymer.
[0028] The prepared P (St - GMA - MPP) copolymer, recycled polystyrene plastic, tributyl citrate, barium laurate, aluminum hydroxide and magnesium hydroxide were added to a high-speed mixer and stirred evenly. The mixed materials were added to an extruder, and the extrusion temperature was controlled to be 195°C, the pressure was 9MPa, and the speed was 2.5m / min. High-performance heat-insulating and fire-resistant recycled building wall polystyrene materials were obtained by extrusion molding.
[0029] P (St - GMA - MPP) copolymer is designed and synthesized based on the need to improve the thermal insulation and fire resistance of polystyrene materials. Styrene provides the basic framework and physical properties of the material, and the introduction of glycidyl methacrylate (GMA) and melamine polyphosphate (MPP) is intended to enhance the thermal insulation and fire resistance of the material.
[0030] The benzene ring has a rigid structure, which provides strength and stability for the material. Its conjugated structure makes the material have good chemical corrosion resistance, can effectively resist the erosion of external chemicals, and maintain the structural integrity of the wall material. At the same time, the benzene ring structure has a certain hindering effect on heat transfer, which helps to improve the thermal insulation performance of the material. The glycidyl group can undergo a cross-linking reaction when the material is heated to form a three-dimensional network structure, which enhances the structural stability of the material. This cross-linking structure can prevent the diffusion of heat and gas, and improve the thermal insulation and fire resistance of the material. In addition, the glycidyl group can also improve the compatibility of the copolymer with other components, making the components of the material more closely combined. Melamine polyphosphate decomposes at high temperatures and releases non-combustible gases, such as ammonia, which can dilute the concentration of combustible gases and reduce the intensity of the combustion reaction. At the same time, the phosphate ions produced by the decomposition can promote the formation of a carbon layer on the surface of the material, which can insulate heat and oxygen and prevent the spread of flames. In addition, melamine polyphosphate can also synergize with other flame retardants to further improve the flame retardant effect of the material.
[0031] Table 2. Comparative synergistic experiment of P (St - GMA - MPP) copolymer Performance test items Existing wall materials (control group) Wall material of the present invention (experimental group) Efficiency data Thermal conductivity (W / (m・K)) 0.050 0.030 Reduced by 0.02 Vertical burning test burning time (s) 12 4 Shorten 8s Thermogravimetric analysis onset decomposition temperature (℃) 250 330 Increase 80℃ Oxygen index (%) 22 32 Increase by 10% Tensile strength (MPa) 13.0 17.5 Increase 4.5MPa Bending strength (MPa) 19.0 25.0 Increase 6.0MPa Infrared thermal imaging test maximum temperature (℃) 80 50 Reduce by 30℃ Peak heat release rate measured by cone calorimeter (kW / m²) 350 200 Reduce 150kW / m² Cone calorimeter test total heat release (MJ / m²) 15 8 Reduce 7MJ / m²
[0032] 1. Significantly improved thermal insulation and fire resistance By introducing the P (St - GMA - MPP) copolymer, the thermal insulation and fire resistance of the wall material are significantly improved. The cross-linking effect of the glycidyl ester group and the flame retardant effect of the melamine polyphosphate group work together to effectively prevent the spread of heat and flames and improve the stability of the material at high temperatures.
[0033] (II) Enhanced mechanical properties The synergistic effect of the rigid structure of styrene and the copolymer significantly improves the mechanical properties of the wall material, such as tensile strength and bending strength, thus ensuring the reliability and durability of the wall material during use.
[0034] III) Environmental protection and resource recycling The use of recycled polystyrene plastic as the main raw material reduces waste emissions and achieves resource recycling. At the same time, the additives and copolymers used are environmentally friendly and meet the requirements of sustainable development.
[0035] (IV) Comprehensive performance optimization The addition of new compounds not only improves the thermal insulation, fire resistance and mechanical properties of wall materials, but also optimizes the chemical stability and processing properties of the materials, enabling them to better meet the diverse needs of building wall materials.
[0036] In summary, the high-performance heat-insulating and fire-resistant recycled building wall polystyrene material and its preparation method provided by the present invention achieve a comprehensive improvement in the performance of the wall material through innovative copolymer design and optimized preparation process, and provide a new type of wall material with broad application prospects for the construction industry.
Claims
1. A heat-insulating and fire-resistant recycled building wall polystyrene material, characterized in that: It comprises a styrene-vinyl triethoxysilane-zinc borate copolymer (P (St - VTEOS - ZB)), wherein the molar ratio of styrene, vinyl triethoxysilane and zinc borate is 4:1:
1.
2. The wall polystyrene material according to claim 1, characterized in that: The wall polystyrene material also includes recycled polystyrene plastic, plasticizer, stabilizer and flame retardant. The plasticizer is dioctyl phthalate, accounting for 8% of the total mass; the stabilizer is zinc stearate, accounting for 3% of the total mass; and the flame retardant is magnesium hydroxide, accounting for 15% of the total mass.
3. The method for preparing the wall polystyrene material according to claim 1, characterized in that: The method comprises the following steps: S1, adding styrene, vinyl triethoxysilane and zinc borate monomers into a reaction container; then adding an initiator dibenzoyl peroxide in an amount of 1.5% of the total mass of the monomers; heating the reaction system to 90°C, and carrying out a free radical polymerization reaction for 6 hours under nitrogen protection; after the reaction is completed, cooling to room temperature, pouring the reaction product into ethanol for precipitation, filtering and drying to obtain a P (St - VTEOS - ZB) copolymer; S2, mixing the prepared P (St - VTEOS - ZB) copolymer with recycled polystyrene plastic and additives; the additives include a plasticizer dioctyl phthalate, a stabilizer zinc stearate, and a flame retardant magnesium hydroxide; the mixing process is carried out in a high-speed mixer to ensure that the components are fully mixed and evenly mixed; then, the mixed materials are prepared into wall materials through an extrusion molding process.
4. Use of the styrene-vinyl triethoxysilane-zinc borate copolymer (P (St-VTEOS-ZB)) according to claim 1 in the preparation of double-insulated recycled polystyrene plastic building wall materials.
5. A building wall, characterized in that: Made of the recycled building wall polystyrene material as described in claim 1.
Citation Information
Patent Citations
Preparation method of thermotolerant high-elasticity halogen-free flame-resistant thermoplastic elastomer
CN101570618A
Polyphenylether / thermoplastic elastomer composition used for cables and preparation method thereof
CN102226031A
Halogen-free inflaming retarding type micro-foaming full-plastic wood-simulating material and preparation method thereof
CN102408640A
Regenerative highly-impact-resistant polystyrene material and preparation method thereof
CN109370138A
Preparing a copolymer, useful to produce e.g. plastics, comprises providing a cyclodextrin compound, providing a metallocene compound with double bonds and providing a styrene compound, adding an initiator and polymerizing components
DE102009020544A1