Composite heavy metal contaminated soil remediation agent and preparation method thereof
Through the modified chitosan and microbial agents in the composite repair agent, the problems of limited repair effects of soil heavy metal pollution and secondary pollution are solved, and the effect of efficiently reducing heavy metal ion concentration and improving soil structure is achieved.
Patent Information
- Application Number
- CN202411080851.1
- Authority / Receiving Office
- CN · China
- Patent Type
- Applications(China)
- Current Assignee / Owner
- Filing Date
- 2024-08-08
- Publication Date
- 2024-11-29
AI Technical Summary
The existing soil heavy metal pollution repair agent has limited repair effects and may cause secondary pollution.
Complex heavy metal contaminated soil repair agents, including montmorillonite powder, modified chitosan, inorganic fertilizers and microbial bacteria agents, improve adsorption capacity by modifying chitosan, and the metabolites of microbial bacteria react with heavy metal ions, and combine with high Molecular polymers and inorganic fertilizers improve soil structure and nutrient supplementation.
Effectively reduce the concentration of heavy metal ions in the soil, improve the repair effect, reduce secondary pollution, and improve soil structure and fertility.
Smart Images

Figure CN119040002A_ABST
Abstract
Description
Technical Field
[0001] The present invention relates to the technical field of soil remediation, and in particular to a composite heavy metal contaminated soil remediation agent and a preparation method thereof. Background Art
[0002] Heavy metal pollution in soil refers to excessive levels of trace metal elements in the soil that exceed the background value due to human activities, and excessive deposition causes excessive levels, which is collectively referred to as heavy metal pollution in soil. Heavy metal pollution in farmland soil is extremely harmful. Heavy metal pollution in soil not only leads to reduced crop yields and quality, but also enters the human body through the soil-plant system and the food chain, endangering human health and life safety.
[0003] At present, the methods for soil heavy metal remediation can be divided into three types: physical methods, chemical methods and biological methods. Physical methods include deep plowing method, soil import method, etc., chemical methods include leaching method, passivation method, etc., and biological methods include phytoremediation method and microbial remediation method. Among them, the passivation method achieves passivation or fixation by adding remediation agents. This method has become a promising soil heavy metal pollution remediation technology due to its advantages such as simple operation and short remediation cycle. However, the current soil remediation agents still have limited remediation effects on heavy metal contaminated soils, and the remediation agents themselves may cause secondary pollution and other problems. Summary of the invention
[0004] In order to solve the above problems, the present invention provides a composite heavy metal contaminated soil remediation agent and a preparation method thereof.
[0005] The technical scheme of the present invention is: a composite heavy metal contaminated soil repair agent, which comprises the following components by weight: 30-40 parts of montmorillonite powder, 4-8 parts of high molecular polymer, 20-30 parts of modified chitosan, 15-30 parts of inorganic fertilizer, 1-5 parts of sodium humate, and 2-6 parts of microbial agent;
[0006] The modified chitosan is prepared from the following raw materials in parts by weight: 3-6 parts of chitosan, 2-5 parts of ferrous sulfate, 6-8 parts of acetic acid, and 9-11 parts of deionized water.
[0007] Description: The above-mentioned repair agent improves the solubility of chitosan in alkaline and neutral environments and the adsorption capacity of chitosan for heavy metals by modifying chitosan, which can effectively reduce the concentration of heavy metal ions in the soil. The metabolites of microbial agents can react with heavy metal ions to further improve the repair effect, and the overall secondary pollution of the repair agent is relatively small.
[0008] Furthermore, the high molecular polymer is a mixture of any one or more of polyacrylamide and polyvinyl alcohol in any ratio.
[0009] Description: The above-mentioned high molecular polymer can effectively absorb heavy metals in the soil, improve soil structure and enhance soil water retention.
[0010] Furthermore, the inorganic fertilizer is a mixture of any one or more of calcium sulfate, calcium phosphate, magnesium sulfate, potassium nitrate, calcium oxide and zinc sulfate in any ratio.
[0011] Note: The above-mentioned inorganic fertilizers can add nutrients to the soil, improve soil fertility, adjust the pH value of the soil, and reduce the activity of heavy metals in the soil.
[0012] Furthermore, the microbial agent is a mixture of any one or more of Bacillus subtilis, Pseudomonas nitroreducens and Trichoderma in any ratio.
[0013] Description: The above-mentioned microbial agents can regulate soil nutrients, and their metabolites can provide a large number of active groups to adsorb heavy metal ions in the soil.
[0014] Furthermore, the preparation method of the modified chitosan comprises the following steps:
[0015] S1. Completely dissolving chitosan and ferrous sulfate in deionized water to obtain a first mixed solution;
[0016] S2, under stirring, gradually adding sodium hydroxide solution to the first mixed solution until the pH value of the mixed solution reaches 11-12, and stopping the addition of sodium hydroxide solution to obtain a second mixed solution;
[0017] S3, adding acetic acid once into the second mixed solution, stirring for 5 to 10 minutes, and during the stirring process, raising the temperature of the second mixed solution by 10 to 20° C.;
[0018] S4, repeating step S3 until all the acetic acid is added to the second mixed solution, stirring for 2 to 4 hours, and obtaining a third mixed solution; wherein the initial addition amount of acetic acid accounts for 15 to 25% of the total weight, and the subsequent addition amount of acetic acid is increased by 20 to 30% compared with the previous addition;
[0019] S5. Filtering the third mixed solution to obtain solid particles, and washing the solid particles to obtain modified chitosan.
[0020] Description: The above modification method improves the solubility of chitosan in alkaline and neutral environments by reacting chitosan with acetic acid. At the same time, ferric acetate is compounded on chitosan to increase the electrostatic interaction between chitosan and heavy metal ions, increase the hydroxyl functional groups on the surface of chitosan, and improve the chemical adsorption capacity of heavy metal ions.
[0021] Furthermore, in step S2, the mass concentration of the sodium hydroxide solution is 15-25%, and the dropping speed of the sodium hydroxide solution is 20-40 ml / min.
[0022] Note: By limiting the concentration and addition rate of the sodium hydroxide solution, the reaction rate of the sodium hydroxide and ferrous sulfate can be controlled, and the pH value of the first mixed solution can be prevented from rising too quickly.
[0023] Furthermore, in step S3, the initial temperature of the second mixed solution is 30-40°C, and the heating rate of the second mixed solution is 3-5°C / min.
[0024] Note: Limiting the initial temperature and heating rate of the second mixed solution can prevent the temperature from rising too quickly, which would result in acetic acid not being able to fully participate in the reaction.
[0025] Furthermore, in step S5, the cleaning uses anhydrous ethanol or methanol as a cleaning agent.
[0026] Note: The above cleaning agents will not dissolve modified chitosan, and have a good cleaning effect and can effectively remove residues on solid particles.
[0027] The present invention also provides a method for preparing a composite heavy metal contaminated soil remediation agent, which is used to prepare the above-mentioned soil remediation agent, comprising the following steps:
[0028] Step 1: uniformly mixing the montmorillonite powder, inorganic fertilizer and sodium humate to obtain a first mixture;
[0029] Step 2: crushing the modified chitosan, and then uniformly mixing it with a high molecular polymer to obtain a second mixture;
[0030] Step 3: Use a 80-120 mesh sieve to sieve the first mixture, and then gradually add the second mixture into the sieved first mixture under stirring. During the addition of the second mixture, the microbial agent is divided into 2-4 equal portions and added to the first mixture. The time interval for adding each portion of the microbial agent is 1-2 minutes, until the second mixture is added. The repair agent is obtained.
[0031] Note: The above preparation method ensures the particle size of the first mixture by sieving the first mixture, so that the first mixture and the second mixture can be evenly mixed, and the microbial agent can be evenly distributed in the repair agent by adding the microbial agent multiple times.
[0032] Furthermore, the amount of the second mixed material added per minute accounts for 8-12% of its total weight.
[0033] Note: Limiting the adding speed of the second mixture can ensure that the first mixture and the second mixture can be evenly mixed, so that the modified chitosan can be evenly distributed.
[0034] The beneficial effects of the present invention are:
[0035] (1) The repair agent of the present invention improves the solubility of chitosan in alkaline and neutral environments and the adsorption capacity of chitosan for heavy metals by modifying chitosan, which can effectively reduce the concentration of heavy metal ions in the soil. The metabolites of the microbial agent can react with heavy metal ions to further improve the repair effect, and the overall secondary pollution of the repair agent is relatively small.
[0036] (2) The preparation method of the present invention ensures the particle size of the first mixture by screening the first mixture, so that the first mixture and the second mixture can be evenly mixed, and the microbial agent can be evenly distributed in the repair agent by adding the microbial agent multiple times. BRIEF DESCRIPTION OF THE DRAWINGS
[0037] Figure 1 is a trend chart of the reduction rate of heavy metal content before and after restoration of Experimental Example 1 of the present invention;
[0038] Figure 2 is a trend chart of the reduction rate of heavy metal content before and after restoration of Experimental Example 2 of the present invention;
[0039] Figure 3 is a trend chart of the reduction rate of heavy metal content before and after restoration of Experimental Example 3 of the present invention;
[0040] Figure 4 is a trend chart of the reduction rate of heavy metal content before and after restoration of Experimental Example 4 of the present invention;
[0041] Figure 5 is a trend chart of the reduction rate of heavy metal content before and after restoration of Experimental Example 5 of the present invention;
[0042] Figure 6 is a trend chart of the reduction rate of heavy metal content before and after restoration of Experimental Example 6 of the present invention;
[0043] Figure 7 This is a trend chart of the reduction rate of heavy metal content before and after restoration of Experimental Example 7 of the present invention. DETAILED DESCRIPTION
[0044] In order to further illustrate the method adopted by the present invention and the effect achieved, the technical solution of the present invention will be clearly and completely described in combination with experiments below.
[0045] Example 1: A composite heavy metal contaminated soil remediation agent, the remediation agent comprises the following components by weight: 35 parts of montmorillonite powder, 6 parts of high molecular polymer, 25 parts of modified chitosan, 22 parts of inorganic fertilizer, 3 parts of sodium humate, and 4 parts of microbial agent; wherein the high molecular polymer is polyacrylamide, the inorganic fertilizer is calcium phosphate, and the microbial agent is Bacillus subtilis;
[0046] The modified chitosan is prepared from the following raw materials in parts by weight: 5 parts of chitosan, 3 parts of ferrous sulfate, 7 parts of acetic acid, and 10 parts of deionized water;
[0047] The preparation method of the modified chitosan comprises the following steps:
[0048] S1. Completely dissolving chitosan and ferrous sulfate in deionized water to obtain a first mixed solution;
[0049] S2. Under stirring, gradually dropwise adding sodium hydroxide solution to the first mixed solution until the pH value of the mixed solution reaches 11.5, and then stopping the dropwise addition of sodium hydroxide solution to obtain a second mixed solution; wherein the mass concentration of the sodium hydroxide solution is 20%, and the dropping speed of the sodium hydroxide solution is 30 ml / min;
[0050] S3, adding acetic acid once into the second mixed solution, stirring for 8 minutes, and during the stirring process, raising the temperature of the second mixed solution by 15°C; wherein the initial temperature of the second mixed solution is 35°C, and the heating rate of the second mixed solution is 4°C / min;
[0051] S4, repeating step S3 until all the acetic acid is added into the second mixed solution, stirring for 3 hours, and obtaining a third mixed solution; wherein the initial addition amount of acetic acid accounts for 20% of the total weight, and the subsequent addition amount of acetic acid is increased by 25% each time compared with the previous addition;
[0052] S5, filtering the third mixed solution to obtain solid particles, and washing the solid particles to obtain modified chitosan; wherein anhydrous ethanol is used as a washing agent for washing;
[0053] The preparation method of the above-mentioned repair agent comprises the following steps:
[0054] Step 1: uniformly mixing the montmorillonite powder, inorganic fertilizer and sodium humate to obtain a first mixture;
[0055] Step 2: crushing the modified chitosan, and then uniformly mixing it with a high molecular polymer to obtain a second mixture;
[0056] Step 3: Use a 100-mesh sieve to sieve the first mixture, and then gradually add the second mixture into the sieved first mixture under stirring. During the addition of the second mixture, the microbial agent is divided into 3 equal portions and added to the first mixture. The time interval for adding each portion of the microbial agent is 1.5 minutes, until the second mixture is added. After the repair agent is obtained, the amount of the second mixture added per minute accounts for 10% of its total weight.
[0057] Example 2: This example is basically the same as Example 1, except that the repair agent includes the following ingredients by weight: 30 parts of montmorillonite powder, 4 parts of high molecular polymer, 20 parts of modified chitosan, 15 parts of inorganic fertilizer, 1 part of sodium humate, and 2 parts of microbial agent.
[0058] Example 3: This example is basically the same as Example 1, except that the repair agent includes the following ingredients by weight: 40 parts of montmorillonite powder, 8 parts of high molecular polymer, 30 parts of modified chitosan, 30 parts of inorganic fertilizer, 5 parts of sodium humate, and 6 parts of microbial agent.
[0059] Example 4: This example is basically the same as Example 1, except that the modified chitosan is made of the following raw materials in parts by weight: 3 parts of chitosan, 2 parts of ferrous sulfate, 6 parts of acetic acid, and 9 parts of deionized water.
[0060] Example 5: This example is basically the same as Example 1, except that the modified chitosan is made of the following raw materials in parts by weight: 6 parts of chitosan, 5 parts of ferrous sulfate, 8 parts of acetic acid, and 11 parts of deionized water.
[0061] Example 6: This example is basically the same as Example 1, except that acetic acid is added once to the second mixed solution, stirred for 5 minutes, and during the stirring process, the temperature of the second mixed solution is increased by 10°C.
[0062] Example 7: This example is basically the same as Example 1, except that acetic acid is added once to the second mixed solution, stirred for 10 minutes, and during the stirring process, the temperature of the second mixed solution is increased by 20°C.
[0063] Example 8: This example is basically the same as Example 1, except that the initial temperature of the second mixed solution is 30°C, and the heating rate of the second mixed solution is 3°C / min.
[0064] Example 9: This example is basically the same as Example 1, except that the initial temperature of the second mixed solution is 40°C, and the heating rate of the second mixed solution is 5°C / min.
[0065] Example 10: This example is substantially the same as Example 1, except that the initial addition amount of acetic acid is 15% of the total weight, and the subsequent addition amount of acetic acid is increased by 20% each time compared with the previous addition amount.
[0066] Example 11: This example is substantially the same as Example 1, except that the initial addition amount of acetic acid is 25% of the total weight, and the subsequent addition amount of acetic acid is increased by 30% each time compared with the previous addition amount.
[0067] Example 12: This example is basically the same as Example 1, except that the microbial agent is divided into two equal portions and added to the first mixed material, and the time interval for adding each portion of the microbial agent is 1 minute.
[0068] Example 13: This example is basically the same as Example 1, except that the microbial agent is divided into 4 equal portions and added to the first mixed material, and the time interval for adding each portion of the microbial agent is 2 minutes.
[0069] Example 14: This example is basically the same as Example 1, except that the amount of the second mixed material added per minute accounts for 8% of its total weight.
[0070] Example 15: This example is basically the same as Example 1, except that the amount of the second mixture added per minute accounts for 12% of its total weight.
[0071] Comparative Example 1: This example is substantially the same as Example 1, except that ordinary chitosan is used instead of the modified chitosan in Example 1.
[0072] Comparative Example 2: This example is substantially the same as Example 1, except that hydroxy-modified chitosan is used to replace the modified chitosan in Example 1.
[0073] Comparative Example 3: This example is substantially the same as Example 1, except that the temperature of the second mixed solution does not increase after acetic acid is added to the second mixed solution.
[0074] Comparative Example 4: This example is substantially the same as Example 1, except that the amount of acetic acid added each time is the same.
[0075] Comparative Example 5: This embodiment is basically the same as Example 1, except that the microbial agent is added all at once.
[0076] Experimental example: In order to explore the influence of the parameters of each embodiment on the performance of the repair agent, soil samples from the same area were taken, and the soil repair agent of each embodiment was applied to each soil sample at a ratio of 100g of soil repair per kilogram of soil. Deionized water was added to each soil sample at a water content of 60%. After 30 days, the heavy metal content in each soil sample was measured, and the reduction rate of Cd, Hg, and Pb content before and after repair by the repair agent of each embodiment was obtained by calculation. The specific exploration is as follows:
[0077] 1. Explore the influence of the ingredients of the repair agent on the performance of the repair agent
[0078] like Figure 1 As shown, by comparing Examples 1, 2, and 3, it can be seen that the reduction rate of Cd, Hg, and Pb contents in the soil sample of Example 1 is the highest, indicating that the repair agent of Example 1 has the best performance and the repair agent component selected in Example 1 is optimal; by comparing Example 1 with Comparative Examples 1 and 2, it can be seen that the reduction rate of Cd content in the soil sample of Example 1 is 11% higher than that of Comparative Example 1 and 8% higher than that of Comparative Example 2; the reduction rate of Hg content is 13% higher than that of Comparative Example 1 and 10% higher than that of Comparative Example 2; the reduction rate of Pb content is 11% higher than that of Comparative Example 1 and 5% higher than that of Comparative Example 2; this shows that the use of the modified chitosan of Example 1 can effectively improve the performance of the repair agent, because the modified chitosan of Example 1 introduces ferric acetate, which itself has the ability to adsorb heavy metal ions, and ferric acetate changes the charge properties of the chitosan surface, increases the electrostatic interaction between chitosan and heavy metal ions, and at the same time, ferric acetate increases the hydroxyl functional groups on the surface of chitosan, provides more adsorption sites, and improves the chemical adsorption capacity for heavy metal ions.
[0079] 2. Explore the effect of modified chitosan raw material components on the performance of the repair agent
[0080] like Figure 2 As shown, by comparing Examples 1, 4, and 5, it can be seen that the reduction rate of Cd, Hg, and Pb contents in the soil sample of Example 1 is the highest, indicating that the repair agent of Example 1 has the best performance. This is because the raw material ratio in Example 1 reacts more fully, the conversion rate of modified chitosan is higher, and more hydroxyl functional groups can be provided to chitosan. Therefore, the chitosan raw material component selected in Example 1 is optimal.
[0081] 3. Investigate the effect of the temperature change of the second mixed solution on the performance of the repair agent
[0082] like Figure 3As shown, by comparing Examples 1, 6, and 7, it can be seen that the reduction rate of Cd, Hg, and Pb contents in the soil sample of Example 1 is the highest, indicating that the repair agent of Example 1 has the best performance. This is because the temperature change amount selected in Example 1 can ensure the reaction rate of the second mixed solution and avoid the temperature rising too fast and exceeding the optimal reaction temperature range. Therefore, the temperature change amount of the second mixed solution selected in Example 1 is optimal; by comparing Example 1 with Comparative Example 3, it can be seen that the reduction rates of Cd, Hg, and Pb contents in the soil sample of Comparative Example 3 are all lower than those in Example 1. This is because the temperature of the second mixed solution does not change, resulting in a too low reaction rate, and the reaction in the second mixed solution cannot be fully carried out. Therefore, the temperature change method of the second mixed solution selected in Example 1 is better.
[0083] 4. Investigate the effect of the heating rate of the second mixed solution on the performance of the repair agent
[0084] like Figure 4 As shown, by comparing Examples 1, 8, and 9, it can be seen that the reduction rate of Cd, Hg, and Pb contents in the soil sample of Example 1 is the highest, and the repair agent of Example 1 has the best performance, but the overall data variation range is small, indicating that the heating rate of the second mixed solution has little effect on the performance of the repair agent.
[0085] 5. Investigate the effect of the amount of acetic acid added on the performance of the repair agent
[0086] like Figure 5 As shown, by comparing Examples 1, 10, and 11, it can be seen that the reduction rate of Cd, Hg, and Pb contents in the soil sample of Example 1 is the highest, indicating that the repair agent of Example 1 has the best performance. This is because the change in the amount of acetic acid added in Example 1 can ensure that the second mixed solution reacts fully with acetic acid and improves the conversion rate of modified chitosan. Therefore, the change in the amount of acetic acid added selected in Example 1 is optimal; by comparing Example 1 with Comparative Example 4, it can be seen that the reduction rates of Cd, Hg, and Pb contents in the soil sample of Comparative Example 4 are all lower than those in Example 1. This is because as the reaction of the second mixed solution proceeds, the amount of acetic acid added needs to be increased to ensure the conversion rate of modified chitosan, and unreacted acetic acid is also easy to remove. Therefore, the change in the amount of acetic acid added selected in Example 1 is better.
[0087] 6. Explore the effect of the time interval of adding microbial agents on the performance of the repair agent
[0088] like Figure 6As shown, by comparing Examples 1, 12, and 13, it can be seen that the reduction rate of Cd, Hg, and Pb contents in the soil sample of Example 1 is the highest, indicating that the remediation agent of Example 1 has the best performance. This is because the microbial agent is evenly distributed in the remediation agent. Therefore, the addition time interval of the microbial agent selected in Example 1 is optimal. By comparing Example 1 with Comparative Example 5, it can be seen that the reduction rates of Cd, Hg, and Pb contents in the soil sample of Comparative Example 5 are all lower than those in Example 1. This is because the addition method of the microbial agent in Example 1 can reduce the microbial aggregation phenomenon and make the microbial agent evenly distributed. Therefore, the addition method of the microbial agent selected in Example 1 is better.
[0089] 7. Investigate the effect of the second mixture addition rate on the performance of the repair agent
[0090] like Figure 7 As shown, by comparing Examples 1, 14, and 15, it can be seen that the reduction rate of Cd, Hg, and Pb contents in the soil sample of Example 1 is the highest, indicating that the repair agent of Example 1 has the best performance. This is because the second mixture is evenly mixed with the first mixture, and the repair agent composition is uniform, but the overall data variation range is small, indicating that the addition speed of the second mixture has little effect on the performance of the repair agent.
Claims
1. A composite heavy metal contaminated soil remediation agent, characterized in that: The repair agent includes the following components by weight: 30-40 parts of montmorillonite powder, 4-8 parts of high molecular polymer, 20-30 parts of modified chitosan, 15-30 parts of inorganic fertilizer, 1-5 parts of sodium humate, and 2-6 parts of microbial agent; The modified chitosan is prepared from the following raw materials in parts by weight: 3-6 parts of chitosan, 2-5 parts of ferrous sulfate, 6-8 parts of acetic acid, and 9-11 parts of deionized water.
2. A composite heavy metal contaminated soil remediation agent according to claim 1, characterized in that: The high molecular polymer is a mixture of any one or more of polyacrylamide and polyvinyl alcohol in any ratio.
3. A composite heavy metal contaminated soil remediation agent according to claim 1, characterized in that: The inorganic fertilizer is a mixture of any one or more of calcium sulfate, calcium phosphate, magnesium sulfate, potassium nitrate, calcium oxide and zinc sulfate in any ratio.
4. A composite heavy metal contaminated soil remediation agent according to claim 1, characterized in that: The microbial agent is a mixture of any one or more of Bacillus subtilis, Pseudomonas nitroreducens and Trichoderma in any ratio.
5. The composite heavy metal contaminated soil remediation agent according to claim 1, characterized in that: The preparation method of the modified chitosan comprises the following steps: S1. Completely dissolving chitosan and ferrous sulfate in deionized water to obtain a first mixed solution; S2, under stirring, gradually adding sodium hydroxide solution to the first mixed solution until the pH value of the mixed solution reaches 11-12, and stopping the addition of sodium hydroxide solution to obtain a second mixed solution; S3, adding acetic acid once into the second mixed solution, stirring for 5 to 10 minutes, and during the stirring process, raising the temperature of the second mixed solution by 10 to 20° C.; S4, repeating step S3 until all the acetic acid is added to the second mixed solution, stirring for 2 to 4 hours, and obtaining a third mixed solution; wherein the initial addition amount of acetic acid accounts for 15 to 25% of the total weight, and the subsequent addition amount of acetic acid is increased by 20 to 30% compared with the previous addition; S5. Filtering the third mixed solution to obtain solid particles, and washing the solid particles to obtain modified chitosan.
6. A composite heavy metal contaminated soil remediation agent according to claim 5, characterized in that: In step S2, the mass concentration of the sodium hydroxide solution is 15-25%, and the dropping speed of the sodium hydroxide solution is 20-40 ml / min.
7. The composite heavy metal contaminated soil remediation agent according to claim 5, characterized in that: In step S3, the initial temperature of the second mixed solution is 30-40°C, and the heating rate of the second mixed solution is 3-5°C / min.
8. The composite heavy metal contaminated soil remediation agent according to claim 5, characterized in that: In step S5, the cleaning adopts anhydrous ethanol or methanol as a cleaning agent.
9. A method for preparing a composite heavy metal contaminated soil remediation agent, used for preparing a composite heavy metal contaminated soil remediation agent according to any one of claims 1 to 8, characterized in that: The following steps are involved: Step 1: uniformly mixing the montmorillonite powder, inorganic fertilizer and sodium humate to obtain a first mixture; Step 2: crushing the modified chitosan, and then uniformly mixing it with a high molecular polymer to obtain a second mixture; Step 3: Use a 80-120 mesh sieve to sieve the first mixture, and then gradually add the second mixture into the sieved first mixture under stirring. During the addition of the second mixture, the microbial agent is divided into 2-4 equal portions and added to the first mixture. The time interval for adding each portion of the microbial agent is 1-2 minutes, until the second mixture is added. The repair agent is obtained.
10. The method for preparing a composite heavy metal contaminated soil remediation agent according to claim 9, characterized in that: The amount of the second mixed material added per minute accounts for 8-12% of its total weight.