Zero-gap membrane electrode electrocatalysis CO2 reduction electrolytic tank based on non-ion exchange membrane

By using a non-ion exchange membrane in a zero-gap membrane electrode electrolytic cell, the salt extraction and hydrogen evolution problems in traditional technology are solved, efficient and stable operation of CO2 reduction and efficient collection of liquid products are achieved, and the overall performance of the device is improved.

CN119040927APending Publication Date: 2024-11-29NANKAI UNIV
View PDF 0 Cites 0 Cited by

Patent Information

Application Number
CN202411517182.X
Authority / Receiving Office
CN · China
Patent Type
Applications(China)
Current Assignee / Owner
Filing Date
2024-10-29
Publication Date
2024-11-29

AI Technical Summary

Technical Problem

In the electrocatalytic CO2 reduction of traditional zero-gap film electrodes, salt and hydrogen evolution phenomena exist, and liquid products are difficult to collect, resulting in low device efficiency and low product utilization.

Method used

A non-ion exchange membrane is used as a separator to allow the relative free diffusion of anions and cations, avoid salt decomposition and water seepage, and form a solid-liquid-gas interface through the microporous structure to achieve efficient collection of liquid products.

Benefits of technology

The stability of the device and CO2 reduction efficiency are improved, and efficient and stable operation is achieved under acidic, neutral and alkaline electrolytes are solved, solving the product collection problem.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure FT_1
    Figure FT_1
  • Figure FT_2
    Figure FT_2
  • Figure FT_3
    Figure FT_3
Patent Text Reader

Abstract

According to the zero-gap membrane electrode electro-catalysis CO2 reduction electrolytic tank based on the non-ion exchange membrane, the non-ion exchange membrane is adopted for separating the cathode and the anode, short circuit is prevented, a solid-liquid-gas three-phase interface is formed through the pore structure and the infiltration characteristic of the membrane, and electro-catalysis CO2 reduction reaction is facilitated. Under the action of an electric field and a concentration field, anion and cation transmission reaches balance, the phenomenon of salt precipitation caused by too high local ion concentration is avoided, and high product Faraday efficiency, high energy efficiency and long-term operation stability can be obtained. The non-ion exchange membrane is used for improving mass transfer of a membrane electrode system, the reaction efficiency and stability of the electrode are improved, and the non-ion exchange membrane has a wide industrial application prospect in the aspect of electrocatalytic CO2 reduction.
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] Traditional zero-gap membrane electrode electrocatalytic CO2 reduction electrolyzers usually use ion exchange membranes to separate the anode and cathode to prevent short circuits within the system, and use the powerful ion transmission capacity of the ion exchange membrane to ensure the smooth progress of the electrocatalytic CO2 reduction process. However, the use of ion exchange membranes limits the transmission direction and flux of substances. Under the reaction conditions of high-concentration hydrogen ions and high-concentration salts, hydrogen precipitation and salt precipitation will occur due to the directional transmission of ions, and the liquid products in the electrocatalytic CO2 reduction are not easy to collect due to the material permeability of the ion exchange membrane. The present invention relates to a novel zero-gap membrane electrode electrolytic cell composition design, specifically, a non-ion exchange membrane is used for the zero-gap membrane electrode electrocatalytic CO2 reduction reaction, replacing the ion exchange membrane to achieve stable and highly selective CO2 reduction, and at the same time, efficient collection of liquid products can be achieved. Background Art

[0002] At present, zero-gap membrane electrode electrocatalytic CO2 reduction usually uses anion exchange membrane for reaction. However, due to the alkaline environment of the catalyst surface area during the reaction, it is very easy to combine with metal cations to produce carbonates, causing blockage of the carbon paper pores and failure of the entire system. Although the use of cation exchange membranes and acidic electrolytes can theoretically reduce the salt precipitation phenomenon and increase the CO2 utilization rate, the use of cation exchange membranes has serious hydrogen evolution reaction problems. If a high concentration of metal cation electrolyte is used, it can promote electrocatalytic CO2 reduction, but there will also be serious salt precipitation problems, and the liquid product is difficult to collect, analyze and utilize. Although the use of bipolar membranes can simultaneously increase the CO2 utilization rate and maintain the stability of the electrode surface microenvironment, its complex structure will lead to low energy efficiency of the overall device. Therefore, designing a new zero-gap membrane electrode assembly scheme for electrocatalytic CO2 reduction has become an effective strategy to achieve high-efficiency and stable production. Summary of the invention

[0003] The present invention adopts non-ion exchange membrane and designs a novel zero-gap membrane electrode assembly method for electrocatalytic CO2 reduction, such as Figure 1 (The illustrations of the present invention are only schematic diagrams, which are intended to help understand the embodiments of the present invention. The shapes, proportions and details may vary, and the actual design is not limited thereto) The core ideas of the present invention include: (1) using a non-ion exchange membrane to achieve the relatively free diffusion of anions and cations in the electric field and concentration field in the entire system, without serious salt precipitation and water seepage; (2) the membrane is non-conductive, can effectively separate the cathode and anode regions, and has partial solution wettability; (3) the membrane has a microporous structure, can form a solid-liquid-gas three-phase interface in the zero-gap membrane electrode, which is conducive to the CO2 reduction reaction; (4) the membrane will not block the liquid products produced by the reaction, and can achieve efficient collection of the liquid products.

[0004] In the zero-gap membrane electrode electrolytic cell, the cathode is flowing CO2 gas, the anode is flowing electrolyte, and there is a diaphragm between the anode and the cathode. The diaphragm used is a non-ion exchange membrane, which can be a nylon membrane, a polytetrafluoroethylene membrane, a polyvinylidene fluoride membrane, polyphenylene sulfide, polyetheretherketone, Zirmbrane, Zirfon and other wettable porous membranes.

[0005] The gas product is CO, CH4 or (and) C 2+ Products, etc.

[0006] The electrolyte can be an acidic electrolyte, a neutral electrolyte or an alkaline electrolyte.

[0007] The cathode catalyst can be any material having the function of catalyzing the CO2 reaction, including but not limited to gold, silver, copper and the like.

[0008] The anode catalyst may be any material that undergoes an oxidation reaction, including but not limited to iridium oxide, ruthenium oxide and the like. Technical Effects

[0009] Compared with the prior art, the present invention mainly addresses the application limitations of traditional zero-gap membrane electrode assembled electrolytic cells for electrocatalytic reduction of CO2, such as salt precipitation, hydrogen evolution and product collection problems, and cleverly uses non-ion exchange membranes to achieve balanced transmission of internal ions and molecules, improve device stability, and achieve efficient and stable operation of zero-gap membrane electrode electrocatalytic CO2 reduction in acidic, neutral and alkaline electrolytes. BRIEF DESCRIPTION OF THE DRAWINGS

[0010] Figure 1 It is a schematic diagram of the assembly of the zero-gap membrane electrode for electrocatalytic CO2 reduction of the non-ion exchange membrane designed by the present invention.

[0011] Figure 2 This is a physical picture of the non-ion exchange membrane used in the present invention (taking nylon membrane as an example).

[0012] Figure 3 The present invention is 100 mA cm –2 Faradaic efficiency diagram of CO2 reduction catalyzed by acidic zero-gap membrane electrode electrolyzer for 30 h under current conditions.

[0013] Figure 4 The present invention is 100 mA cm –2 Faradaic efficiency diagram of CO2 reduction catalyzed by neutral zero-gap membrane electrode electrolyzer for 25 h under current conditions.

[0014] Figure 5 The present invention is 100 mA cm –2Faradaic efficiency diagram of CO2 reduction catalyzed by alkaline zero-gap membrane electrode electrolyzer for 10 h under current conditions. DETAILED DESCRIPTION

[0015] In order to more clearly and completely describe the purpose, technical solutions and advantages of the present invention, the present invention is further described in detail below in conjunction with the accompanying drawings in the embodiments of the present invention. The embodiments described below are only part of the embodiments of the present invention, not all of the embodiments, and the specific embodiments described here are only used to explain the present invention and are not used to limit the present invention. Example 1

[0016] This embodiment specifically designs a non-ion exchange membrane ( Figure 2 ) as a separator, a sputtered silver electrode as a cathode, and commercial iridium oxide as an anode, specifically comprising the following steps: Step 1) Sputter a layer of nanosilver on the hydrophobic carbon paper by magnetron sputtering. The specific operation is as follows: put the carbon paper or other material substrate into the magnetron sputtering instrument, and sputter a layer of nanosilver. The sputtering time is 0-30 min, and the sputtering thickness is in the range of 0-500 nm. The magnetron sputtering conditions are: sputtering power 0-100 W; hydrogen flow rate 50-100 sccm; pre-sputtering pressure 0-2.0 Pa; pre-sputtering time 0-2 min; sputtering pressure 0-0.5 Pa. After sputtering, Ag electrodes of different thicknesses are obtained.

[0017] Step 2) Assemble the carbon paper, gasket, membrane, gasket, and iridium oxide electrode into an electrolytic cell in sequence, connect the gas path, circulate the electrolyte, and perform the electrocatalytic CO2 reduction reaction.

[0018] Step 3) Connect the liquid flow channel to the electrolyte and the gas flow channel to the CO2 gas, and operate the acidic electrocatalytic CO2 reduction electrolytic cell with a current density of 100 mA cm –2 The reaction time is 30 h. Figure 3 . Example 2

[0019] This embodiment specifically designs a non-ion exchange membrane ( Figure 2 ) as a separator, a sputtered silver electrode as a cathode, and commercial iridium oxide as an anode, specifically comprising the following steps: Step 1) Sputter a layer of nanosilver on the hydrophobic carbon paper by magnetron sputtering. The specific operation is as follows: put the carbon paper or other material substrate into the magnetron sputtering instrument, and sputter a layer of nanosilver. The sputtering time is 0-30 min, and the sputtering thickness is in the range of 0-500 nm. The magnetron sputtering conditions are: sputtering power 0-100 W; hydrogen flow rate 50-100 sccm; pre-sputtering pressure 0-2.0 Pa; pre-sputtering time 0-2 min; sputtering pressure 0-0.5 Pa. After sputtering, Ag electrodes of different thicknesses are obtained.

[0020] Step 2) Assemble the carbon paper, gasket, membrane, gasket, and iridium oxide electrode into an electrolytic cell in sequence, connect the gas path, circulate the electrolyte, and perform the electrocatalytic CO2 reduction reaction.

[0021] Step 3) Connect the liquid flow channel to the electrolyte and the gas flow channel to the CO2 gas, and operate the neutral electrocatalytic CO2 reduction electrolytic cell with a current density of 100 mA cm –2 The reaction time is 25 h. Figure 4 . Example 3

[0022] This embodiment specifically designs a non-ion exchange membrane ( Figure 2 ) as a separator, a sputtered silver electrode as a cathode, and commercial iridium oxide as an anode, specifically comprising the following steps: Step 1) Sputter a layer of nanosilver on the hydrophobic carbon paper by magnetron sputtering. The specific operation is as follows: put the carbon paper or other material substrate into the magnetron sputtering instrument, and sputter a layer of nanosilver. The sputtering time is 0-30 min, and the sputtering thickness is in the range of 0-500 nm. The magnetron sputtering conditions are: sputtering power 0-100 W; hydrogen flow rate 50-100 sccm; pre-sputtering pressure 0-2.0 Pa; pre-sputtering time 0-2 min; sputtering pressure 0-0.5 Pa. After sputtering, Ag electrodes of different thicknesses are obtained.

[0023] Step 2) Assemble the carbon paper, gasket, membrane, gasket, and iridium oxide electrode into an electrolytic cell in sequence, connect the gas path, circulate the electrolyte, and perform the electrocatalytic CO2 reduction reaction.

[0024] Step 3) Connect the liquid flow channel to the electrolyte and the gas flow channel to the CO2 gas, and operate the alkaline electrocatalytic CO2 reduction electrolytic cell with a current density of 100 mA cm –2 The reaction time is 10 h. Figure 5 .

[0025] The above contents are merely examples and explanations of the concept of the present invention. The technicians in this technical field may make various modifications or additions to the specific embodiments described or replace them in a similar manner. As long as they do not deviate from the concept of the invention or exceed the scope defined by the claims, they should all fall within the protection scope of the present invention.

Claims

1. A zero-gap membrane electrode electrocatalytic CO2 reduction electrolytic cell based on a non-ion exchange membrane, characterized in that: The device comprises an end plate, an anode plate, an anode catalyst, a gasket, a diaphragm, a gasket, a cathode catalyst, a cathode plate and an end plate. During the reaction process, CO2 gas is supplied to the cathode side and electrolyte is supplied to the anode side.

2. The method according to claim 1, characterized in that: The diaphragm used is a non-ion exchange membrane, has no conductivity, is a wettable porous material, has a suitable porosity, and can be any material that meets the above requirements, such as polytetrafluoroethylene, nylon, polyvinylidene fluoride, polyphenylene sulfide, polyetheretherketone, Zirmbrane, Zirfon, etc.

3. The method according to claim 1, characterized in that: The anolyte may be neutral, alkaline or acidic.

4. The method according to claim 1, characterized in that: The cathode catalyst is any catalyst that can cause CO2 reduction reaction; the anode catalyst can be any material that catalyzes oxidation reaction.

5. The method according to claim 1, characterized in that: A fuel cell stack composed of the above-mentioned electrolytic cell device.